Thinning structure of Hybrid glass

Through the thinning structure of Hybrid glass, the first adhesive layer with a thickness exceeding twice the thickness of the display structure is used to connect the substrate glass, combined with the edge connection of the second adhesive layer, to solve the glass resistance when the 0.5mm panel is thinned to 0.2mm Weakness and transportation fragmentation problems are eliminated, productivity and stability are improved, and production costs and fragmentation risks are reduced.

CN221917827UActive Publication Date: 2024-10-29EVERDISPLAY OPTRONICS (SHANGHAI) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420043715.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-08
Publication Date
2024-10-29
Estimated Expiration
2034-01-08

AI Technical Summary

Technical Problem

Existing technology is difficult to effectively solve the problems of weak glass resistance, brittleness, high production costs, and fragmentation during transportation when the 0.5mm panel is thinned to 0.2mm.

Method used

Using the thin structure of Hybrid glass, it is connected to the first adhesive layer through two layers of substrate glass. The thickness of the first adhesive layer exceeds 2 times the thickness of the display structure, and the width is less than the width between the display structures. It is installed on adjacent displays of the substrate glass. Between the structures, a second glue layer is combined for edge connection to improve the strength and stability of the glass.

Benefits of technology

It significantly increases the thinning capacity, reduces the risk of fragmentation of Hybrid panels during transportation and handling, avoids contact damage to the display structure, and maintains high yield and low production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221917827U_ABST
    Figure CN221917827U_ABST
Patent Text Reader

Abstract

The utility model relates to a thinning structure of Hybrid glass. The thinning structure comprises two layers of substrate glass and a display structure arranged on the substrate glass, the substrate glass is connected through a first adhesive layer; the display structures on the two layers of substrate glass are oppositely arranged; the first adhesive layer is arranged between the adjacent display structures of the single piece of substrate glass; at least two first adhesive layers are arranged; the thickness of the first adhesive layer is larger than two times of the thickness of the display structure; the width of the first adhesive layer is smaller than the width between the adjacent display structures. According to the thinning structure provided by the utility model, the two pieces of glass can be synchronously thinned to be less than 0.2 mm, so that the thinning capacity is obviously improved, and meanwhile, the fragment risk of a Hybrid panel in the processes of transportation, carrying and the like is also reduced; furthermore, the contact of the display structure can be avoided in the processing process, so that the probability of damaging the display structure when the display screen is laminated is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of glass processing and manufacturing, and in particular to a hybrid glass thinning structure. Background Art

[0002] At present, as the market demand for tablet / laptop products is becoming increasingly lighter and thinner, the current trend is to combine the respective advantages of flexible and hard screens to create a new form of ultra-light and thin hybrid panel.

[0003] Currently, 0.5mm panels are usually thinned to 0.2mm, and market feedback shows that they are still relatively thick. However, due to technical and manufacturing limitations, the thinning of a single display can only achieve 0.2mm.

[0004] For example, CN106746705A discloses a single-sided glass thinning method and glass thinning equipment, which includes the following steps: S1, detachably fixing the glass on the fixed surface of the acrylic plate, with the acid-resistant film surface of the glass facing the fixed surface of the acrylic plate; S2, moving the acrylic plate fixed with the glass into an etching tank to thin the glass; S3, separating the glass from the acrylic plate.

[0005] CN106082687A discloses a glass thinning method and a glass thinning device, including step S1, providing a glass to be thinned; S2, using an acidic corrosive liquid to corrode the surface of the glass to be thinned, and while corroding the glass, using a friction mechanism that moves relative to the glass to flatten the surface of the glass to be thinned.

[0006] However, the current trend of thinning single 0.5mm panels further leads to the following bottlenecks:

[0007] (1) The G6 large panels currently produced, whether cut or quartered, are still relatively large in size. After being thinned to 0.2mm, if they are thinned further, the resistance of the large thin glass will be weaker, and the risk of breakage will increase during the thinning process, reducing the yield rate.

[0008] (2) If the production line is modified to produce panels less than 0.2 mm, the equipment modification cost will increase;

[0009] (3) Large thin panels are prone to floating during transportation, and a carrier plate is required to carry the panels for transportation, which increases production costs;

[0010] (4) When the panel thickness is less than 0.3 mm, the panel is more likely to bend and deform when the robot is processing a large thin panel, and the large thin panel is more likely to break during transportation and handling. Utility Model Content

[0011] In view of the problems existing in the prior art, the purpose of the present invention is to provide a hybrid glass thinning structure to solve the problem of glass breakage during the thinning process of glass less than 0.2 mm and during transportation.

[0012] To achieve this purpose, the utility model adopts the following technical solutions:

[0013] The utility model provides a hybrid glass thinning structure, the hybrid glass thinning structure comprising:

[0014] 2 layers of substrate glass, and a display structure disposed on the substrate glass;

[0015] The substrate glasses are connected via a first adhesive layer;

[0016] The display structures on the two layers of substrate glass are arranged relatively;

[0017] The first adhesive layer is disposed between adjacent display structures of a single substrate glass;

[0018] The first adhesive layer is provided at least at two locations;

[0019] The thickness of the first adhesive layer is greater than twice the thickness of the display structure;

[0020] The width of the first adhesive layer is less than the width between adjacent display structures.

[0021] The thinning structure provided by the utility model can simultaneously thin the two pieces of glass to less than 0.2mm, significantly improving the thinning capacity, while also reducing the risk of breakage of the hybrid panel during transportation and handling; further, contact with the display structure can be avoided during processing to avoid the possibility of damage to the display structure when the display screen is stacked.

[0022] As a preferred technical solution of the present utility model, the thickness of the first adhesive layer is 3-50 μm.

[0023] As a preferred technical solution of the present utility model, the thickness of the substrate glass is greater than 0.2 mm.

[0024] As a preferred technical solution of the utility model, the first adhesive layer is arranged between each adjacent display structure of a single substrate glass.

[0025] As a preferred technical solution of the utility model, the first adhesive layer is arranged around the display structure of a single substrate glass.

[0026] As a preferred technical solution of the present utility model, the distance between the first adhesive layer and the display structure is 0.1-30 mm.

[0027] As a preferred technical solution of the present utility model, the thickness of the display structure is 1-25 μm.

[0028] As a preferred technical solution of the present utility model, the edges of the thinned structure of the Hybrid glass are connected by a second adhesive layer.

[0029] As a preferred technical solution of the present invention, the distance between the second adhesive layer and the display structure is 0.1-30 mm.

[0030] As a preferred technical solution of the present utility model, the thickness of the second adhesive layer is equal to the thickness of the first adhesive layer.

[0031] Compared with the existing technical solutions, the utility model has the following beneficial effects:

[0032] The thinning structure provided by the utility model not only meets the thinning process of the substrate glass on the basis of the existing technology, but also meets the strength requirements of subsequent processing and transportation, and additionally realizes double output; specifically, without reducing the yield and increasing the production cost, a Hybrid panel with a thickness of less than 0.2mm can be produced, which can improve the thinning capacity and reduce the risk of ultra-thin Hybrid panels being broken during transportation and handling. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 It is a schematic diagram of the thinning structure of Hybrid glass provided in an embodiment of the utility model;

[0034] Figure 2 It is a schematic diagram of a first adhesive layer partially disposed in the thinning structure of the Hybrid glass provided by an embodiment of the utility model;

[0035] Figure 3 It is a schematic diagram of a first adhesive layer disposed around the thinning structure of the Hybrid glass provided in an embodiment of the present utility model.

[0036] In the figure, 1-substrate glass, 2-display structure, 3-first adhesive layer, 4-second adhesive layer.

[0037] The utility model is further described in detail below. However, the following examples are only simple examples of the utility model and do not represent or limit the scope of protection of the utility model. The scope of protection of the utility model shall be subject to the claims. DETAILED DESCRIPTION

[0038] In order to better illustrate the present invention and facilitate understanding of the technical solution of the present invention, typical but non-limiting embodiments of the present invention are as follows:

[0039] This embodiment provides a hybrid glass thinning structure, such as Figure 1and Figure 2 As shown, the thinning structure of the Hybrid glass includes:

[0040] 2 layers of substrate glass 1, and a display structure 2 disposed on the substrate glass 1;

[0041] The substrate glass 1 is connected via a first adhesive layer 3;

[0042] The display structures 2 on the two layers of substrate glass 1 are arranged opposite to each other;

[0043] The first adhesive layer 3 is disposed between adjacent display structures 2 of a single substrate glass 1;

[0044] The first adhesive layer 3 is provided at least at two locations;

[0045] The thickness of the first adhesive layer 3 is greater than twice the thickness of the display structure 2;

[0046] The width of the first adhesive layer 3 is smaller than the width between adjacent display structures 2 .

[0047] Specifically, the first adhesive layer 3 is provided at least at two locations, such as two locations, three locations, four locations or five locations, but is not limited to the listed values, and other listed values ​​within the range also meet the requirements.

[0048] Specifically, the number of locations is reasonably configured according to the area of ​​the glass substrate and the number of display structures 2 .

[0049] Specifically, the thickness of the first adhesive layer 3 is greater than twice the thickness of the display structure 2, such as 2.1 times, 2.2 times, 2.3 times, 2.4 times, 2.5 times, 2.6 times, 2.7 times, 2.8 times, 2.9 times, 3 times, 3.2 times, 3.4 times, 3.6 times, 3.8 times or 4 times, but is not limited to the listed values, and other listed values ​​within the range also meet the requirements.

[0050] The thickness of the first adhesive layer 3 is 3-50 μm, for example, 3 μm, 5 μm, 10 μm, 15 μm, 20 μm, 30 μm, 35 μm, 40 μm, 45 μm or 50 μm, but is not limited to the listed values, and other listed values ​​within the range also meet the requirements.

[0051] Among them, the thickness of the substrate glass 1 is >0.2mm, for example, it can be 0.21mm, 0.22mm, 0.24mm, 0.26mm, 0.28mm, 0.3mm, 0.32mm, 0.34mm, 0.36mm, 0.38mm, 0.4mm, 0.42mm, 0.44mm, 0.46mm, 0.48mm or 0.5mm, but is not limited to the listed values, and other listed values ​​within the range also meet the requirements.

[0052] Among them, the thickness of the display structure 2 is 1-25μm, for example, it can be 1μm, 2μm, 4μm, 6μm, 8μm, 10μm, 12μm, 14μm, 16μm, 18μm, 20μm, 22μm, 24μm or 25μm, but is not limited to the listed values, and other listed values ​​within the range also meet the requirements.

[0053] The first adhesive layer 3 is disposed between each adjacent display structure 2 of a single substrate glass 1 .

[0054] The first adhesive layer 3 is arranged around the display structure 2 of the single substrate glass 1. Figure 3 shown.

[0055] In this example, when the first adhesive layer 3 is disposed around the display structure 2 of a single substrate glass 1, the adhesive layers between adjacent display structures 2 may be shared or disposed separately to avoid interference in certain circumstances.

[0056] Among them, the spacing between the first adhesive layer 3 and the display structure 2 is 0.1-30mm, for example, it can be 0.1mm, 0.2mm, 0.4mm, 0.6mm, 0.8mm, 1mm, 2mm, 4mm, 6mm, 8mm, 10mm, 12mm, 14mm, 16mm, 18mm, 20mm, 22mm, 24mm, 26mm, 28mm or 30mm, but is not limited to the listed values, and other listed values ​​within the range also meet the requirements.

[0057] Wherein, the edges of the thinned structure of the Hybrid glass are connected by using a second adhesive layer 4 .

[0058] Among them, the spacing between the second adhesive layer 4 and the display structure 2 is 0.1-30mm, for example, it can be 0.1mm, 0.2mm, 0.4mm, 0.6mm, 0.8mm, 1mm, 2mm, 4mm, 6mm, 8mm, 10mm, 12mm, 14mm, 16mm, 18mm, 20mm, 22mm, 24mm, 26mm, 28mm or 30mm, but is not limited to the listed values, and other listed values ​​within the range also meet the requirements.

[0059] The thickness of the second adhesive layer 4 is equal to the thickness of the first adhesive layer 3 .

[0060] In this example, the display structure 2 includes precision structures such as TFT, OLED, TFE, TOE, COE, etc., which can be designed based on existing technologies and will not be described in detail in this example.

[0061] In this example, the first and second adhesive layers 3 and 4 are only used to distinguish the positions of the two adhesive layers, and there is no difference in composition. Specifically, the adhesive layer can be a glue commonly used in the field to play a dividing and supporting role, such as a single-component glue or a two-component glue. For example, glass powder glue such as frit glue, or light-curing glue, such as ultraviolet light-curing glue, infrared light-curing glue, natural light-curing glue, etc.

[0062] Exemplarily, the first adhesive layer 3 may be made of frit adhesive, the second adhesive layer 4 may be made of UV curing adhesive, or both the first adhesive layer 3 and the second adhesive layer 4 may be made of UV curing adhesive, or both the first adhesive layer 3 and the second adhesive layer 4 may be made of frit adhesive, or the first adhesive layer 3 may be made of light curing adhesive and the second adhesive layer 4 may be made of frit adhesive.

[0063] The frit glue in this example is a colloid made of various metal oxide powders, supporting particles, adhesives and solvents according to a certain formula.

[0064] Among them, the UV light curing glue is a single-component, low-viscosity, high-strength organic adhesive, which can be cured by ultraviolet irradiation with a wavelength of 365nm, and has a fast curing speed, good transparency, excellent weather resistance, and good heat and chemical resistance.

[0065] Furthermore, UF glue is a type of UV glue, also known as peelable blue glue, which can be directly torn off by hand after curing. UF glue not only serves as a bonding and supporting function during the thinning process of the Hybrid panel, but also plays a temporary protective role during the transportation of the Hybrid panel. After curing, UF glue can play an insulating, moisture-proof and protective role. It is non-toxic, non-volatile, and has excellent moisture resistance. The cured UF glue layer has good elasticity and toughness, good adhesion to the panel, and is easy to peel off, complete, and without leaving any residue, and has no effect on the bottom layer.

[0066] In this example, the first adhesive layer 3 and the second adhesive layer 4 can be arranged on one of the glass substrates 1 by dispensing, coating, etc. according to the design size and then buckled, or they can be arranged on two substrates according to the size and buckled.

[0067] In this example, the first adhesive layer 3 and the second adhesive layer 4 can be set continuously or discontinuously; the continuous setting means a continuous setting without breakpoints, and the discontinuous setting means there are gaps in the adhesive layer. The specific setting method can be reasonably selected while meeting the needs.

[0068] In this example, the first adhesive layer 3 plays a supporting role, and the coating position is located outside the cutting path of the large glass panel display structure 2 to be cut, and then the two large panels are laminated. If the display structure 2 is small and there are many of them, more display structures 2 can be sealed together, and a small amount of Frit glue can be applied in the middle to play a supporting role.

[0069] Furthermore, a protective gas layer may be provided between the closed thinned structures formed after buckling, such as air, nitrogen, carbon dioxide, helium, neon, argon and other gases.

[0070] Furthermore, after the thinning structure is obtained, a thinning process can be performed. The specific process may be, for example, that the thinned structure obtained by buckling is processed according to a conventional thinning process in the field, such as etching and thinning using an etching liquid. It should be noted that the thinning function achieved by the thinning structure in the utility model is an advantage of the thinning structure, and is not related to the operating parameters in the etching and thinning process, that is, the glass thinning of <0.2mm can be achieved in the etching and thinning process, and does not affect the thinning effect of the thinning structure. Even if the thinning structure provided by the utility model cannot achieve glass thinning of <0.2mm through the etching and thinning process, the glass thinning of <0.2mm can still be guaranteed.

[0071] Furthermore, after the thinning process, the large display screen can be directly packaged and transported, or according to the needs of subsequent manufacturing, the large display screen can be cut along the adhesive layer and the display structure 2 to be divided into several small display screens; the first adhesive layer 3 and the second adhesive layer 4 are removed together with the cutting, and the two display screens are separated to achieve the thinning of the double-layer display screen and double the output of the small display structure 2.

[0072] Using the above-mentioned thinning process, the two pieces of glass can be simultaneously thinned to less than 0.2mm, which significantly improves the thinning capacity and also reduces the risk of breakage of the hybrid panel during transportation and handling.

[0073] It is stated that the utility model uses the above embodiments to illustrate the detailed structural features of the utility model, but the utility model is not limited to the above detailed structural features, that is, it does not mean that the utility model must rely on the above detailed structural features to be implemented. Those skilled in the art should understand that any improvement to the utility model, equivalent replacement of the components selected by the utility model, addition of auxiliary components, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the utility model.

[0074] The preferred embodiments of the present invention are described in detail above. However, the present invention is not limited to the specific details in the above embodiments. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, and these simple modifications all belong to the protection scope of the present invention.

[0075] It should also be noted that the various specific technical features described in the above specific embodiments can be combined in any suitable manner without contradiction. In order to avoid unnecessary repetition, the present utility model will not further describe various possible combinations.

[0076] In addition, various embodiments of the present invention may be arbitrarily combined, and as long as they do not violate the concept of the present invention, they should also be regarded as the contents disclosed by the present invention.

Claims

1. A hybrid glass thinning structure, characterized in that: The thinning structure of the hybrid glass includes: 2 layers of substrate glass, and a display structure disposed on the substrate glass; The substrate glasses are connected via a first adhesive layer; The display structures on the two layers of substrate glass are arranged relatively; The first adhesive layer is disposed between adjacent display structures of a single substrate glass; The first adhesive layer is provided at least at two locations; The thickness of the first adhesive layer is greater than twice the thickness of the display structure; The width of the first adhesive layer is less than the width between adjacent display structures.

2. The hybrid glass thinning structure according to claim 1, characterized in that: The thickness of the first adhesive layer is 3-50 μm.

3. The hybrid glass thinning structure according to claim 1 or 2, characterized in that: The thickness of the substrate glass is greater than 0.2 mm.

4. The hybrid glass thinning structure as claimed in claim 3, characterized in that: The first adhesive layer is disposed between each adjacent display structure of a single substrate glass.

5. The hybrid glass thinning structure according to claim 1 or 4, characterized in that: The first adhesive layer is disposed around the display structure of a single substrate glass.

6. The hybrid glass thinning structure as claimed in claim 5, characterized in that: The distance between the first adhesive layer and the display structure is 0.1-30 mm.

7. The hybrid glass thinning structure according to claim 1 or 6, characterized in that: The display structure has a thickness of 1-25 μm.

8. The hybrid glass thinning structure according to claim 1, characterized in that: The edges of the thinned structure of the Hybrid glass are connected by using a second adhesive layer.

9. The hybrid glass thinning structure according to claim 8, characterized in that: The distance between the second adhesive layer and the display structure is 0.1-30 mm.

10. The hybrid glass thinning structure according to claim 8 or 9, characterized in that: The thickness of the second adhesive layer is equal to the thickness of the first adhesive layer.