Press fitting type rapid fuse
By setting pillars in the press-fit fast fuse to evenly share the pressure of the conductive plate, combined with quartz sand solidification treatment and high-strength screw connection, the problem of uneven pressure distribution of the conductive plate is solved, and the stability and safety of the fuse are improved. properties, and reduces power consumption and contact resistance.
Patent Information
- Application Number
- CN202420600240.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-26
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2034-03-26
AI Technical Summary
The conductive plate of the existing press-mounted fast fuse has uneven pressure distribution when it is pressed, causing dents and increasing safety risks. Moreover, the water-cooled conductive plate of the traditional solution can only share the pressure through the end of the porcelain bottle, which cannot effectively solve the problem of high power consumption. and poor stability issues.
A pillar is set in the porcelain bottle. The pillar connects the upper conductive plate and the lower conductive plate to bear the pressure. Instead, the end face of the porcelain bottle and the pillar bear the pressure. Combined with quartz sand curing treatment and high-strength screw connection, the stability and safety of the conductive plate are improved.
Through the design of the pillar, the fuse can withstand greater extrusion force without causing deformation of the conductive plate, which improves stability and safety, while reducing power consumption and contact resistance, and enhancing conductivity.
Smart Images

Figure CN221927950U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of press-fit fast fuses, and in particular relates to a press-fit fast fuse. Background Art
[0002] Conventional press-fit fast fuses and the silicon components they protect are usually connected in the equipment through a water-cooled copper busbar. Although this can effectively solve the heat dissipation problem of the press-fit fast fuse during operation and improve its operating stability, it also increases the cost of equipment manufacturing and increases power consumption during operation.
[0003] The utility model patent with authorization announcement number CN209658122U discloses a high-power water-cooled press-fit fast fuse, which uses a process method in which left and right water-cooled conductive plates, quartz sand curing treatment, and silver foil is added between the conductive plate and the inner contact knife for extrusion connection through high-strength screws. It solves the problems of high power consumption, poor stability, and poor heat transfer capacity of traditional fuses. However, the fuse in the scheme of this utility model is also a crimped fuse, but the left and right water-cooled conductive plates can only share the pressure through a circle at the end of the porcelain bottle, resulting in uneven pressure distribution on the left and right water-cooled conductive plates, depression in the middle, and other problems, causing great safety hazards when the press-fit fast fuse is used. Utility Model Content
[0004] In order to solve the problem that the conductive plate of the existing fuse is unevenly pressed and thus dented, the utility model provides a press-fit fast fuse.
[0005] In order to achieve the above purpose, the utility model provides the following technical solutions:
[0006] A press-fit fast fuse comprises: a porcelain bottle which passes through from top to bottom and an upper conductive plate and a lower conductive plate which are sealed and connected to both ends of the porcelain bottle;
[0007] A pillar coaxial with the center line of the porcelain bottle is provided in the porcelain bottle, one end of the pillar is fixedly connected to an inner contact knife provided in the porcelain bottle and located on one side of the upper conductive plate, and the other end of the pillar is fixedly connected to the lower conductive plate;
[0008] It also includes a filler arranged between the inner contact blade and the lower conductive plate, and a plurality of melts welded between the inner contact blade and the lower conductive plate.
[0009] Furthermore, tin foil is arranged between the upper conductive plate and the inner contact blade.
[0010] Furthermore, the lower conductive plate is provided with a mounting hole for mounting the support column.
[0011] Furthermore, the filler is quartz sand and a curing agent.
[0012] Furthermore, the upper conductive plate and the lower conductive plate match the sizes of the corresponding end faces of the porcelain bottle.
[0013] Furthermore, the porcelain bottle is a 95 alumina high-strength porcelain bottle.
[0014] Furthermore, two ends of the porcelain bottle are sealed and connected to the upper conductive plate and the lower conductive plate respectively through high-strength screws.
[0015] The press-fit fast-acting fuse provided by the utility model has the following beneficial effects: in the press-fit fast-acting fuse of the utility model, a pillar supported between the upper conductive plate and the lower conductive plate is arranged in the porcelain bottle, so that the object bearing the pressure of the upper conductive plate and the lower conductive plate is changed from the original porcelain bottle end face to the porcelain bottle end face and the pillar, so that the fuse can withstand a greater extrusion pressure while ensuring that the upper conductive plate and the lower conductive plate will not be deformed due to the greater extrusion pressure, thereby causing safety problems, thereby improving the stability and safety of the press-fit fast-acting fuse. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the embodiment of the utility model and its design scheme, the following is a brief introduction to the drawings required for the embodiment. The drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0017] Figure 1 This is a side internal view of the fuse of the utility model;
[0018] Figure 2 This is a top view of the fuse of the utility model;
[0019] Figure 3 This is a side external view of the fuse of the utility model;
[0020] Figure 4 This is a top view of the external appearance of the fuse of the utility model.
[0021] In the figure: 1. upper conductive plate; 2. inner contact knife; 3. porcelain bottle; 4. filler; 5. melt; 6. support; 7. lower conductive plate. DETAILED DESCRIPTION
[0022] In order to enable those skilled in the art to better understand the technical solution of the utility model and implement it, the utility model is described in detail below in conjunction with the accompanying drawings and specific embodiments. The following embodiments are only used to more clearly illustrate the technical solution of the utility model, and cannot be used to limit the protection scope of the utility model.
[0023] Device Example 1:
[0024] A fuse of the utility model, such as Figure 1 As shown, it includes an upper conductive plate 1 and a lower conductive plate 7, a 95 aluminum oxide high-strength porcelain bottle 3 is sealed between the upper conductive plate 1 and the lower conductive plate 7, and the 95 aluminum oxide high-strength porcelain bottle 3 runs through from top to bottom; a filler 4 is arranged inside the 95 aluminum oxide high-strength porcelain bottle 3, an inner touch knife 2 is arranged between the upper conductive plate 1 and the lower conductive plate 7; the inner touch knife 2 is close to the upper conductive plate 1, and a pillar 6 is arranged between the inner touch knife 2 and the lower conductive plate 7, which is coaxial with the center line of the porcelain bottle 3 and is used to support the upper conductive plate 1 and the lower conductive plate 7. The height of the pillar 6 does not exceed the height of the 95 aluminum oxide high-strength porcelain bottle 3. In fact, the middle pillar 6 must ensure that the distance between the upper conductive plate 1 and the lower conductive plate 7 must be consistent with the height of the 95 aluminum oxide high-strength porcelain bottle 3 and can have a prescribed adjustable tolerance. A plurality of melts 5 are welded between the inner touch knife 2 and the lower conductive plate 7.
[0025] The utility model provides a press-fit fast-acting fuse with a pillar supported between an upper conductive plate and a lower conductive plate in a porcelain bottle. Thus, the object bearing the pressure of the upper conductive plate and the lower conductive plate is changed from the original porcelain bottle end face to the porcelain bottle end face and the pillar. Thus, the fuse can withstand a greater extrusion pressure while ensuring that the upper conductive plate and the lower conductive plate will not be deformed due to the greater extrusion pressure, thereby causing safety problems. The stability and safety of the press-fit fast-acting fuse are improved.
[0026] Device Example 2:
[0027] Based on device embodiment 1, Figure 1 As shown, tin foil for welding is also provided between the upper conductive plate 1 and the inner contact blade 2. The tin foil is provided to facilitate the subsequent fixing of the upper conductive plate 1, the lower conductive plate 7 and the 95 alumina high-strength porcelain bottle 3, and then use a high-frequency welding machine to melt the tin foil at high temperature, thereby improving the tightness of the connection between the upper conductive plate 1 and the inner contact blade 2, reducing the contact resistance, thereby reducing the power consumption during the operation of the fast fuse, and improving the stability of the fast fuse operation.
[0028] Device Example 3:
[0029] Based on device embodiment 1, Figure 1 As shown, the lower conductive plate 7 is also provided with a mounting hole for installing the pillar 6. The pillar 6 is firmly adhered to the mounting hole by a sealant. This arrangement makes the installation of the pillar 6 more convenient and quick, and facilitates the subsequent welding and installation of other components of the press-fit fast fuse.
[0030] Device Example 4:
[0031] On the basis of the device embodiment 1, the filler 4 is quartz sand and a curing agent. The quartz sand is filled inside and cured, thereby improving the breaking capacity and heat transfer capacity of the press-fit fast fuse.
[0032] Device Example 5:
[0033] Based on device embodiment 1, Figure 1-4 As shown, the upper conductive plate 1 has the same size as the corresponding end faces of the lower conductive plate 7 and the 95 alumina high-strength porcelain bottle 3. This arrangement can make the resistance of the conductive plate smaller, the current passing through larger, the power greater, the fuse can be disconnected faster, and the availability of the fuse is improved.
[0034] Device Example 6:
[0035] Based on device embodiment 1, Figure 2-4 As shown, the upper conductive plate 1 is firmly fixed to one end face of the 95 aluminum oxide high-strength porcelain bottle 3 with high-strength screws, and the lower conductive plate 7 is firmly fixed to the other end face of the 95 aluminum oxide high-strength porcelain bottle 3 with high-strength screws to form a sealed environment. Fixing the upper conductive plate 1, the lower conductive plate 7 and the 95 aluminum oxide high-strength porcelain bottle 3 with high-strength screws is more secure and convenient for subsequent welding.
[0036] In addition: Figure 1 As shown, a gap is left between the inner contact knife 2 and the inner surface of the 95 alumina high-strength porcelain bottle 3, and the gap is used to make the installation of the internal melt 5 more convenient and quick.
[0037] When installing:
[0038] like Figure 1 , 2 As shown, one end of the pillar 6 is installed in the mounting hole on the lower conductive plate 7 with a mounting hole on one side, and is firmly bonded with a sealant. The other end is supported on the inner contact blade 2 and is firmly bonded with a sealant. Then, one end of the folded line melt 5 is welded to the lower conductive plate 7, and the other end is welded to the inner contact blade 2. Then, a tin sheet is placed between the conductive plate 1 and the inner contact blade 2, and the inner contact blade 2 and the tin sheet are bonded with a sealant. A tin sheet is placed between the upper conductive plate 1 and the inner contact blade 2, and then a high-frequency welding machine is used to melt the tin sheet at high temperature, and at the same time, the screws on the upper conductive plate 1 are tightened to weld it, and then the fuse is placed in a vacuum tank and injected with a curing agent, and then placed in a drying box for curing. Since the conductive plate is the same size as the end face of the porcelain bottle, and there is a pillar in the middle, when the two conductive water bags are stacked and connected in series with the fuse, the pressure on the conductive plate in the vertical direction will be evenly shared on the end face of the porcelain bottle and the pillar, which will not only not cause deformation of the conductive plate, but also because there is enough pressure, its contact resistance will become smaller and the conductivity will be improved.
[0039] It should be noted that the above specific implementation methods can enable those skilled in the art to more fully understand the invention of the utility model, but do not limit the invention of the utility model in any way. Therefore, although the invention of the utility model has been described in detail in this specification and embodiments, those skilled in the art should understand that the invention of the utility model can still be modified or replaced by equivalents; and all technical solutions and improvements that do not deviate from the spirit and scope of the invention of the utility model are included in the protection scope of the patent of the invention of the utility model. Any figure mark in the claims should not be regarded as limiting the claims involved.
Claims
1. A press-fit fast fuse, It is characterized in that include: A porcelain bottle (3) that penetrates from top to bottom, and an upper conductive plate (1) and a lower conductive plate (7) that are sealed and connected to both ends of the porcelain bottle (3); The porcelain bottle (3) is provided with a support (6) coaxial with the center line of the porcelain bottle (3), one end of the support (6) is fixedly connected to an inner contact knife (2) provided in the porcelain bottle (3) and located on one side of the upper conductive plate (1), and the other end of the support (6) is fixedly connected to the lower conductive plate (7); It also includes a filler arranged between the inner contact blade (2) and the lower conductive plate (7), and a plurality of melts (5) welded between the inner contact blade (2) and the lower conductive plate (7).
2. The press-fit fast fuse according to claim 1, It is characterized in that Tin foil is arranged between the upper conductive plate (1) and the inner contact knife (2).
3. The press-fit fast fuse according to claim 1, It is characterized in that The lower conductive plate (7) is provided with a mounting hole for mounting the support column (6).
4. The press-fit fast fuse according to claim 1, It is characterized in that The filler (4) is quartz sand and a curing agent.
5. The press-fit fast fuse according to claim 1, It is characterized in that The upper conductive plate (1) and the lower conductive plate (7) match the sizes of the end faces of the corresponding porcelain bottles (3).
6. The press-fit fast fuse according to claim 1, It is characterized in that The porcelain bottle (3) is a 95% alumina high-strength porcelain bottle.
7. The press-fit fast fuse according to claim 1, It is characterized in that The two ends of the porcelain bottle (3) are sealedly connected to the upper conductive plate (1) and the lower conductive plate (7) respectively through high-strength screws.