Dry-method chip making device for bipolar polar plate of nickel-metal hydride battery

By compounding the positive electrode and negative electrode mixture on the conductive substrate through rolling and hot pressing in a dry production device for bipolar plates of nickel-metal hydride batteries, the problems of poisoning of conductive skeleton materials and low processing efficiency in the existing technology are solved. , improving the battery performance and cycle life of nickel-metal hydride batteries.

CN221928134UActive Publication Date: 2024-10-29SHENZHEN TEV ENERGY CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420292174.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-09
Publication Date
2024-10-29
Estimated Expiration
2034-02-09

AI Technical Summary

Technical Problem

The existing bipolar plate production methods for nickel-metal hydride batteries have problems such as poisoning of conductive skeleton materials, poor charge retention, poor storage performance, low processing efficiency, short cycle life, and low high-current discharge platform.

Method used

Design a dry production device for bipolar plates of nickel-metal hydride batteries. Feeders and pressure rollers are provided on both sides of the conductive substrate. The positive electrode mixture and the negative electrode mixture are compounded on the front and back sides of the conductive substrate through rolling processing, and Improve bonding strength through hot pressing and rolling treatments.

Benefits of technology

It improves the processing efficiency and battery performance of nickel-metal hydride batteries, extends the cycle life, and improves high-current charge and discharge characteristics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221928134U_ABST
    Figure CN221928134U_ABST
Patent Text Reader

Abstract

The utility model discloses a dry-method sheet making device for a bipolar plate of a nickel-metal hydride battery, and belongs to the technical field of nickel-metal hydride battery preparation, two feeders, two first compression rollers and two second compression rollers are sequentially arranged on two sides of a conductive substrate from top to bottom, and the feeders, the first compression rollers and the second compression rollers are symmetrically arranged on two sides of the conductive substrate; the device is high in processing efficiency, simple in structure, ingenious in design and capable of simultaneously compounding the positive electrode mixture and the negative electrode mixture on the front and back surfaces of the conductive substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of nickel-hydrogen battery preparation, and in particular relates to a dry-process film-making device for a nickel-hydrogen battery bipolar plate. Background Art

[0002] At present, there are two methods for making negative electrode sheets of nickel-hydrogen batteries: one is to use dry embedding technology for powder coating and rolling. The defect of this method is that the negative electrode uses copper mesh as the conductive skeleton, and copper is toxic in the positive electrode of nickel-hydrogen batteries, which makes the manufactured battery have problems of poor charge retention and storage performance. The other is to use wet sheet drawing, using nickel strip, nickel-plated strip, titanium-plated strip as the conductive skeleton, attaching the binder and hydrogen storage alloy powder to the base strip and then rolling and forming. The negative electrode sheet drawn by this method has a binder in the electrode sheet, which easily causes defects such as short battery cycle life and low high current discharge platform when making high-capacity batteries or high-power batteries.

[0003] The manufacturing method of the positive electrode plate of the nickel-hydrogen battery mainly adopts the dry process. The positive electrode dry process adopts the positive electrode active material Ni(OH)2, the conductive agent and the adhesive to be mechanically mixed, and then it is made into a positive electrode plate after the steps of dry powder coating and rolling molding with foamed nickel on a special dry equipment, and then assembled into a nickel-hydrogen battery with the negative electrode plate, diaphragm paper, electrolyte, container, etc.

[0004] In the prior art, a step-by-step method is generally used to process bipolar plates, that is, positive electrode active material / negative electrode active material is first coated on one side of a conductive substrate, and then negative electrode active material / positive electrode active material is coated on the other side. The processing efficiency is low, and the resulting nickel-hydrogen battery has poor high current discharge characteristics, and the surface active material is easy to fall off, which affects the cycle life of the nickel-hydrogen battery. Utility Model Content

[0005] In order to solve the problems in the prior art, the utility model aims to provide a dry-process film-making device for bipolar plates of nickel-hydrogen batteries.

[0006] The technical solution of the utility model is as follows:

[0007] A dry film making device for bipolar plates of nickel-hydrogen batteries, wherein a feeder, a first pressing roller, and a second pressing roller are arranged on both sides of the conductive substrate from top to bottom in sequence, and the feeder, the first pressing roller, and the second pressing roller are all two in number and symmetrically arranged on both sides of the conductive substrate.

[0008] In a preferred solution, the conductive substrate and the feeder are arranged vertically, and a discharge port is provided at the bottom of the feeder to facilitate the transfer of the positive electrode mixture and the negative electrode mixture to the roller gap between the conductive substrate and the first pressing roller.

[0009] In a preferred solution, the discharge port is a slit parallel to the width direction of the conductive substrate, and the width of the discharge port is smaller than the width of the conductive substrate.

[0010] In a more preferred solution, the spacing between the discharge ports is adjustable.

[0011] Furthermore, the discharge port is provided with a valve for opening or closing the discharge port.

[0012] Furthermore, an air-inflating and pressurizing mechanism is provided on the upper part of the feeder to promote the downward transmission of the viscous mixture.

[0013] Furthermore, a feeding port is provided on the top of the feeder.

[0014] Beneficial technical effects of the utility model:

[0015] The utility model provides a dry-process film-making device for bipolar plates of nickel-hydrogen batteries. A feeder, a first pressing roller and a second pressing roller are arranged on both sides of a conductive substrate from top to bottom in sequence. The number of the feeder, the first pressing roller and the second pressing roller are two, which are symmetrically arranged on both sides of the conductive substrate. The device has high processing efficiency, simple structure and ingenious design, and can compound a positive electrode mixture and a negative electrode mixture on the front and back sides of the conductive substrate at the same time. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to more clearly illustrate the technical solution implemented by the utility model, the following drawings are briefly introduced. The following drawings are only some implementation examples of the utility model, and those skilled in the art can use them according to the drawings and actual production conditions without paying creative labor.

[0017] Figure 1 The device is used in the dry film making process of bipolar plates for nickel-hydrogen batteries;

[0018] Figure 2 It is a structural schematic diagram of the feeder;

[0019] Figure 3 This is the power density diagram of the square 7.2V-6.5Ah NiMH bipolar battery;

[0020] Figure 4 This is a high current charge and discharge diagram for a square 7.2V-6.5Ah NiMH bipolar battery;

[0021] Figure 5 This is the cycle performance diagram of the square 7.2V-6.5Ah nickel-metal hydride bipolar battery;

[0022] Explanation of reference numerals: 1-conductive substrate, 2-feeder, 3-first pressing roller, 4-second pressing roller, 5-discharging port, 6-valve, 7-inflating and pressurizing mechanism, 8-positive electrode active material layer, 9-negative electrode active material layer, 10-feeding port. DETAILED DESCRIPTION

[0023] The present invention will be further described in detail below with reference to the accompanying drawings and specific embodiments:

[0024] It should be noted that the "upper", "lower", "left", "right", "front" and "back" mentioned in this article to describe the direction do not refer to the direction unless otherwise specified, but are only for the convenience of description. The description of the product will be different if it is placed in a different direction. Any direction that can be understood by ordinary technicians in this field without making creative work belongs to the protection scope of this utility model.

[0025] Example 1

[0026] A dry-process sheeting device for bipolar plates of nickel-hydrogen batteries, wherein a feeder 2, a first pressing roller 3, and a second pressing roller 4 are sequentially arranged on both sides of a conductive substrate 1 from top to bottom, and the number of the feeder 2, the first pressing roller 3, and the second pressing roller 4 are all two, and they are symmetrically arranged on both sides of the conductive substrate 1;

[0027] The conductive substrate 1 and the feeder 2 are arranged vertically, and a discharge port 5 is provided at the bottom of the feeder 2 to facilitate the conveying of the positive electrode mixture and the negative electrode mixture to the roller gap between the conductive substrate and the first pressing roller.

[0028] Specifically, the discharge port 5 is a gap parallel to the width direction of the conductive substrate, the width of the discharge port 5 is smaller than the width of the conductive substrate 1, and the spacing of the discharge ports 5 is adjustable.

[0029] Specifically, the discharge port 5 is provided with a valve 6, and the discharge port can be opened or closed by adjusting the valve 6.

[0030] Specifically, an air-filling and pressurizing mechanism 7 is provided above the interior of the feeder 2 to promote the downward transmission of the viscous positive and negative electrode mixture.

[0031] Specifically, a feeding port 10 is provided on the top of the feeder 2 .

[0032] Example 2

[0033] A dry process for preparing bipolar plates for nickel-hydrogen batteries comprises the following steps:

[0034] (1) mixing the positive electrode active material and the binder uniformly to obtain a positive electrode mixed powder, and subjecting the positive electrode mixed powder to high-speed shearing to obtain a viscous positive electrode mixture;

[0035] (2) mixing the negative electrode active material and the binder uniformly to obtain a negative electrode mixed powder, and subjecting the negative electrode mixed powder to high-speed shearing to obtain a viscous negative electrode mixture;

[0036] (3) coating a conductive layer on the front and back surfaces of the conductive substrate, wherein the thickness of the conductive layer is 0.1 to 5 μm, placing the viscous positive electrode mixture obtained in step (1) and the viscous negative electrode mixture obtained in step (2) on both sides of the pretreated conductive substrate, respectively, and subjecting the positive electrode mixed powder and the negative electrode mixed powder to a rolling process so as to bond the conductive substrate to obtain a bipolar plate after rolling;

[0037] (4) hot pressing the roll-pressed bipolar plate obtained in step (3) to compound the positive electrode mixed powder and the negative electrode mixed powder on the front and back surfaces of the conductive substrate to obtain a hot pressed bipolar plate;

[0038] (5) The hot-pressed bipolar plate is immersed in a binder solution containing a conductive agent for 5 seconds to 30 minutes, and then dried and rolled at a rolling pressure of 10 MPa and a roller gap of 0.1 mm to obtain the nickel-hydrogen battery bipolar plate.

[0039] In this embodiment, the conductive substrate is a nickel-plated steel plate, and the thickness of the conductive substrate is 200 μm.

[0040] In this embodiment, the binder is a polytetrafluoroethylene (PTFE) solution with a concentration of 35 wt %.

[0041] In this embodiment, the positive electrode formula is: nickel hydride: cobalt: conductive agent: binder (PTFE) = 94-96: 1-5: 0.5-3: 0.1-3.

[0042] The negative electrode formula is: hydrogen storage alloy powder: conductive agent: binder (PTFE): catalyst = 94-97: 0.5-3: 0.1-3: 0.1-1.

[0043] In this embodiment, the cobalt is one or more of cobalt hydroxide, cobaltous oxide, and cobalt powder; the conductive agent is one or more of carbon black, acetylene black, carbon nanotubes, and graphene; and the catalyst is potassium borohydride or sodium borohydride.

[0044] In this embodiment, a high-speed mixer is used to mix to obtain a mixed powder; a spiral stirrer is used to prepare a viscous mixture.

[0045] In this embodiment, in step (3), the pressure of the roller pressing treatment is 40 MPa; the roller pressing temperature is 40° C.; and the roller gap is 0.1 mm.

[0046] In this embodiment, in step (4), the pressure of the hot pressing treatment is 30 MPa; the hot pressing temperature is 100° C.; and the roller gap is 0.1 mm.

[0047] In this embodiment, in step (5), the binder solution of the conductive agent is a PTFE solution of carbon black, and the mass concentration of the carbon black is 1 to 20 wt%.

[0048] The nickel-hydrogen battery bipolar plates prepared in Example 2 were assembled into square 7.2V-6.5Ah nickel-hydrogen batteries. The assembly process of the nickel-hydrogen battery was the prior art. The electrical performance test results were as follows: energy density was 108Wh / kg, high current charge and discharge characteristics 100C>80%, cycle performance 0.5C 80% DOD, and capacity retention rate of 8000 cycles was greater than 80%. Figures 3 to 5 shown.

[0049] The above is only a preferred embodiment of the present invention, and the protection scope of the present invention is not limited to the above embodiments. For those skilled in the art, improvements and changes obtained without departing from the technical concept of the present invention should also be regarded as the protection scope of the present invention.

Claims

1. A dry process for preparing bipolar plates for nickel-hydrogen batteries, characterized in that: A feeder (2), a first pressing roller (3), and a second pressing roller (4) are sequentially arranged on both sides of the conductive substrate (1) from top to bottom, and the number of the feeder (2), the first pressing roller (3), and the second pressing roller (4) is two, and they are symmetrically arranged on both sides of the conductive substrate (1); The conductive substrate (1) and the feeder (2) are arranged vertically, and a discharge port (5) is provided at the bottom of the feeder (2) to facilitate the conveying of the positive electrode mixture and the negative electrode mixture to the roller gap between the conductive substrate and the first pressing roller.

2. A dry process for preparing bipolar plates for nickel-hydrogen batteries according to claim 1, characterized in that: The discharge port (5) is a slit parallel to the width direction of the conductive substrate, and the width of the discharge port (5) is smaller than the width of the conductive substrate (1).

3. The dry process film making device for bipolar plates of nickel-hydrogen batteries according to claim 1, characterized in that: The spacing between the discharge ports (5) is adjustable.

4. The dry process film making device for bipolar plates of nickel-hydrogen batteries according to claim 1, characterized in that: The discharge port (5) is provided with a valve (6).

5. The dry process film making device for bipolar plates of nickel-hydrogen batteries according to claim 1, characterized in that: An air charging and pressurizing mechanism (7) is provided above the interior of the feeder (2).

6. The dry process film making device for bipolar plates of nickel-hydrogen batteries according to claim 1, characterized in that: The top of the feeder (2) is provided with a feeding port (10).

Citation Information

Cited By

  • Dry-method chip making process for bipolar plate of nickel-metal hydride battery

    CN117954581A