Cigarette filter stick
By twisting the "test tube brush-shaped" cigarette filter rod composed of core wire and fiber fuzz, the problem of large suction resistance in heating and non-combust cigarettes is solved, and the effect of low suction resistance, low smoke retention and cooling is achieved, simplifying the production process , reduces costs.
Patent Information
- Application Number
- CN202323431552.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-15
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2033-12-15
AI Technical Summary
When existing cigarette filter rods are suitable for heating and non-combust cigarettes, they have a large suction resistance, which affects the smoking experience, and have high production costs, complex structures and cumbersome preparation steps.
A cord-wool structure consisting of a twisted core wire as the axis, with neatly arranged and outwardly stretched outwardly, forming a special form of a cigarette filter rod with a "test tube brush-shaped" shape. The fiber fluff is in an axial direction. Externally scattered, spiral or annularly connected, the outer wrapping material is in contact with the fiber velvet, and is prepared by the integrated spinning technology of "fleece cutting-core wire twisting".
It achieves low suction resistance and low flue gas interception, has good cooling effect, fast production speed, low cost, and stable structure. It is suitable for 14-20mm circumference fine cigarettes.
Smart Images

Figure CN221931277U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the field of cigarettes and relates to a cigarette filter rod. Background Art
[0002] With the development of society, smokers are paying more and more attention to their own health, and the market's requirements for cigarette filter rods are getting higher and higher. As the main part of reducing harmful components such as tar and nicotine in smoke, cigarette filter rods play an important role in filtering smoke and improving taste. In recent years, with the upgrading of consumption and the enhancement of people's health awareness, new tobacco products (heat-not-burn cigarettes) have attracted widespread attention in domestic and foreign markets. When smoking, the tobacco is in a non-burning state, and nicotine and flavor substances are mainly released by volatilization through heating (about 400°C) to meet the needs of smokers. The amount of smoke is small and the smoke temperature is high (the highest temperature of the first three puffs exceeds 60°C). Therefore, the corresponding filter rods are required to have low smoke retention, low suction resistance and improved cooling. The traditional acetate or polypropylene fiber bundle filter rods have a complex network structure formed by thousands of fibers arranged along the axial direction, which will lead to a large suction resistance and obvious smoke interception and filtration effect, affecting the smoker's experience. Therefore, there is an urgent need to develop a new type of cigarette filter rod suitable for new tobacco products (heat-not-burn cigarettes), which can effectively reduce the smoke temperature and maintain low smoke retention and low inhalation resistance at the smoke concentration as much as possible.
[0003] At present, for new tobacco products (heat-not-burn tobacco), some new filter rods have been developed at home and abroad. By designing new filter rods, structural innovations are made to the filter rods, or by adjusting the pore distribution of the filter rods to achieve low suction resistance, or by embedding a section of empty tube structure in the filter rod, or by using porous firmware. Philip Morris INC. of the United States (US11300583) discloses a segmented filter rod structure, which consists of a wrapping paper, a porous mesh, and gaps, etc., and is applied to heat-not-burn tobacco products. Its suction resistance is significantly reduced, and the traditional experience of smokers is retained to a large extent. Chinese patent CN202020118955.8 discloses a rolled spiral cooling filter structure, which is woven into a flat textile by one of the yarns such as polylactic acid, natural cellulose, and acetate fiber, and then rolled into a filter rod with multiple grid holes to achieve the purpose of cooling and reducing suction resistance, but the rolling molding process is relatively complicated, and the roundness of the filter tip is difficult to control during the rolling process. Chinese utility model patent CN201922458233.7 discloses a low-suction resistance, low-filtration and cooling composite cigarette mouthpiece, which is composed of ultra-high single-denier cellulose acetate tow and a structure that can reduce the temperature of cigarette smoke (including non-woven fabrics with gaps, fiber aggregates, empty tubes or particles), achieving low adsorption, low suction resistance and moderate cooling filtering effects. Chinese utility model patent CN201910502277.7 discloses an ultra-low adsorption cooling function filter rod suitable for new heat-not-burn cigarettes, in which the hollow core circular tube of the filter rod is provided with 2 to 6 layers of intercepting baffles perpendicular to the axial direction, and the baffles can be made of resin, plastic, nylon, wood, plexiglass, metal, paper and other materials, and each layer of intercepting baffle is independently provided with at least one throttling hole, achieving the purpose of low adsorption and temperature control. Chinese utility model patents CN201820988160 and CN201820988243 also describe similar structures, in which porous hardware is usually made of ceramics or polymer materials, with a porous structure in the center and chamfered or grooved structures on the periphery. Not only is the structure complex, but most of them are processed by injection molding, which increases production costs, and the safety of the selected materials remains to be verified. In summary, although the existing technology can meet the requirements of "reducing suction resistance" and / or cooling, it is either complex in structure, inconvenient to produce, or a non-uniform filter medium, or a segmented structure, with cumbersome preparation steps and high costs. Utility Model Content
[0004] In view of the above-mentioned deficiencies in the prior art, the purpose of the present utility model is to provide a cigarette filter rod, which is suitable for new tobacco products (heat-not-burn cigarettes) and has the characteristics of low smoke retention and low draw resistance.
[0005] The technical solution of the utility model to solve the technical problem is:
[0006] A cigarette filter rod comprises a filter core part and an outer layer wrapping material, wherein the filter core part comprises at least one or more chenille yarn materials; optionally, the chenille yarn material comprises a core yarn and fiber fluff extending outwardly along the axis of the core yarn.
[0007] Optionally, the core line coincides with or is parallel to the axis of the outer layer of wrapping material.
[0008] Optionally, the three-dimensional appearance of the chenille yarn may be similar to a "test tube brush", with the fiber fluff scattering outward from the axis, or forming a fixed angle with the axial direction of the core wire, preferably in the range of 45-135°, more preferably 80-100°.
[0009] Optionally, the fiber fluff is fixedly arranged on the section from the core axis to form but not limited to a flat straight structure, a Y-shaped structure, a cross structure, or a snowflake structure. The "Y-shaped structure, cross structure, or snowflake structure" refers to a pattern formed by the radial projection of the fiber fluff on a sufficiently long section of chenille material on the core.
[0010] Optionally, the connection point between the fiber fluff and the core wire is spiral or ring-shaped along the axis of the core wire. Optionally, the ring-shaped means that, like a ring, a ring of fiber fluff is placed on the core wire at a certain distance, and the rings are not connected; the spiral structure has a pitch of 0.2-50mm, preferably 1.2-5mm.
[0011] Optionally, the central thickness of the thread-shaped structure corresponds to the diameter of the core material, the thread thickness is proportional to the diameter of the fiber fluff, and the thread pitch corresponds to the inverse of the twist of the chenille yarn.
[0012] Optionally, the fiber fluff is arranged in a periodic structure along the axial direction of the core wire, including one or more combinations of cones, cylinders, truncated cones, etc. The circumferential spacing is 0.5-80 mm, preferably 5-30 mm.
[0013] Optionally, the ends of the fiber fluff are in contact with the inner wall of the outer layer wrapping material. The ends of the fiber fluff can be in contact with the inner wall of the outer layer wrapping material through physical action, preferably, they can be in contact with each other through an adhesive.
[0014] Optionally, the fiber fluff can be cut in a certain oblique direction through the outer circle to form a periodic structure similar to a cone or a truncated cone. Optionally, the fiber fluff can also be cut to form a pagoda-like, wave-like, gourd-like, or special-shaped structure with different diameters.
[0015] Optionally, the fiber fluff is periodically, evenly and neatly distributed inside the outer wrapping material.
[0016] Optionally, the fiber fluff can be composed of fluff of different lengths distributed inside the outer wrapping material. Optionally, the fluff of different lengths is formed by fibers containing at least two different properties, which produce different expansion and contraction changes through physical effects such as tension and heat. Optionally, acetate fiber and high shrinkage polyester fiber are used as fiber fluff at the same time. When heated to 100°C, the polyester fiber curls while the acetate fiber remains basically unchanged, thereby forming a fiber arrangement of different lengths. Optionally, acetate fiber mixed with a single denier of 2.0 dtex and a single denier of 22 dtex is selected as the fiber fluff material. After cutting, the difference in resilience caused by the difference in single denier can cause the final two fibers to shrink to different degrees, so that the fiber fluff of the resulting lanyard yarn presents different lengths.
[0017] Optionally, the piles of different lengths can also be formed by twisting two or more chenille yarns with different pile lengths. For example, two chenille yarns can be further arranged in parallel or twisted together into one. At this time, if the fiber lengths of the two chenille yarns are different, the resulting chenille yarn will have piles of two lengths alternately distributed.
[0018] Optionally, the cigarette filter rod has a diameter of 4-9 mm and a porosity of 20-99%, preferably 50-99.5%, and more preferably 90-99%.
[0019] Optionally, the fiber fluff is a polymer fiber or a cellulose fiber, including but not limited to cellulose, regenerated cellulose, cellulose derivatives, starch-based thermoplastic resins, cellulose acetate, polylactic acid, chitosan and its derivatives, alginate, polyhydroxybutyrate, poly-ε-caprolactone, polyglycolic acid, polyhydroxyalkanoate, polypropylene, polyethylene, polyvinyl alcohol, polyester fiber, polyamide fiber, polyurethane, polyacrylonitrile, and combinations thereof. The fiber fluff has a fiber fineness of 0.5-133 dtex, preferably 2.2-22 dtex.
[0020] Optionally, the fiber fluff has a fiber fineness of 0.5-133 dtex, preferably a fiber fineness of 2.0-22 dtex.
[0021] Optionally, the core wire includes but is not limited to polyester fiber, polyamide fiber, polyethylene fiber, polypropylene fiber, cotton yarn, linen yarn, viscose fiber, chitosan fiber, seaweed fiber, acetate fiber, polylactic acid fiber, seaweed fiber, polyacrylonitrile fiber and any one of their modified fibers, metal wires, and composite wires of two or more of them. The core wire has a fineness of at least 2tex and a strength of at least 2N, preferably a strength greater than or equal to 10N.
[0022] Optionally, the core wire is made of a degradable or recyclable material.
[0023] Optionally, the core wire has a fineness of at least 2 tex, preferably 5-80 tex; a strength of at least 2N, optionally, a strength of at least 10N.
[0024] Optionally, the metal wire includes stainless steel wire or copper wire.
[0025] Optionally, in certain embodiments, when the fiber is in a single shape and not in a yarn state, such as a single polymer fiber polyethylene fiber, a single metal wire stainless steel, its fineness is calculated by diameter, and the fineness is at least 0.01 mm. Preferably, the strength is at least 10N.
[0026] The outer wrapping material includes but is not limited to sheet material with a thickness of no more than 4 mm, preferably no more than 2 mm, preferably 0.02-0.5 mm.
[0027] Optionally, the sheet material may be cellulose paper, which is mainly made of plant fibers such as wood, grass, hemp, reed, cotton, etc., preferably cigarette paper, preferably with a thickness of 0.02mm-0.5mm.
[0028] Optionally, the sheet material can be plastic, preferably with a thickness of 0.01-1 mm; optionally, the sheet material is rolled into a tube (thickness 0.05-0.7 mm). The plastic includes one or a mixture of polyolefins, polyesters, polyamides, polyimides, polyaldehydes, cellulose esters, cellulose ethers, polysaccharide-based materials, any derivatives thereof, or any copolymers thereof. Among them, polyolefins include vinyls, propenyls, olefins, styrenes, acrylates, and fluorine-containing olefins; polyesters include polylactic acid, polycarbonate, polyurethane, polyhydroxyalkanoate, polyglycolic acid, poly-ε-caprolactone, polyethylene terephthalate, polybutylene terephthalate, polycyclohexanedimethylene terephthalate, polypropylene terephthalate, acrylonitrile-butadiene-styrene, styrene-acrylonitrile, styrene-butadiene, and styrene-maleic acid styrene copolymers; cellulose esters include cellulose acetate, cellulose acetate butyrate, plasticized cellulose plastics, cellulose propionate, and any derivatives thereof; cellulose ethers include methyl cellulose, ethyl cellulose, benzyl cellulose, phenyl cellulose, and any derivatives thereof; polysaccharide-based materials include starch-based, glycogen, heteropolysaccharides, lignin plastic materials, and modified materials thereof.
[0029] Optionally, the sheet material may be a fabric or non-woven material made of natural fibers or chemical fibers, or may be a hollow tube formed from acetate fiber bundles.
[0030] Optionally, the sheet material may be metal, ceramic, or glass.
[0031] The method for preparing the cigarette filter rod comprises the following steps:
[0032] (1) Any fiber bundle is selected as the velvet yarn, any one of filament, single yarn and ply yarn is used as the core yarn, a gauge with different neck width is selected, the rotating head speed, twist direction, spindle speed and roller speed are adjusted, and the rope velvet yarn is obtained by the integrated spinning technology of "velvet yarn cutting-core yarn twisting";
[0033] It should be noted that for chenille yarns where the connection points between the fiber pile and the core wire form a spiral line with the core wire as the axis: the diameter of the column core is proportional to the fineness of the core material. The thread thickness is approximately proportional to the fiber denier / density, mainly due to the different cross-sectional shapes of the fibers. The thread pitch is proportional to the roller speed / spindle speed.
[0034] Optionally, the chenille yarn may be core-wrapped in a bundling-like manner on the periphery of the chenille yarn to improve the firmness of the fiber fluff in the chenille yarn.
[0035] In other words, according to step (1), the fiber is clamped between two core wires, and then a core material can be wrapped around the formed chenille yarn. At this time, the fiber bundle can be used as a yarn-wrapped material to form a nearly annular contact point.
[0036] In addition, there are other processes that can achieve the embedding of fibers in loops, and then the nesting of loops to form long chenille yarns, which will not be discussed here.
[0037] (2) After the spun chenille yarn or at least one chenille yarn of different thicknesses is combined and twisted, it is cut into chenille yarn segments of different lengths according to needs, and packaged into the outer layer wrapping material of the filter rod to obtain the cigarette filter rod.
[0038] Optionally, the fiber bundle in step (1) is a polymer fiber or a cellulose fiber, including but not limited to one or more of cellulose, regenerated cellulose, cellulose derivatives, starch-based thermoplastic resins, cellulose acetate, polylactic acid, polyhydroxybutyrate, poly-ε-caprolactone, polyglycolic acid, polyhydroxyalkanoate, polypropylene, polyethylene, polyvinyl alcohol, polyester fiber, polyamide fiber, polyurethane, and polyacrylonitrile.
[0039] Optionally, the fiber tow in step (1) has a fiber fineness of 0.5-133 dtex, preferably a fiber fineness of 2.2-22 dtex.
[0040] Optionally, the core wire in step (1) includes but is not limited to polyester fiber, polyamide fiber, polyethylene fiber, polypropylene fiber, cotton yarn, linen yarn, viscose fiber, acetate fiber, polylactic acid fiber, polyacrylonitrile fiber and any one of their modified fibers and metal wires, and composite wires of two or more of them.
[0041] Optionally, the core wire in step (1) is made of a degradable or recyclable material.
[0042] Optionally, the yarn core wire fineness of step (1) is at least 2 tex, preferably between 5 and 80 tex.
[0043] Optionally, the metal wire comprises stainless steel wire or copper wire, and optionally has a fineness of at least 0.01 mm, preferably 0.1-0.3 mm.
[0044] Optionally, the width of the gauge neck in step (1) is 0.8-10 mm, preferably 1.5-4.5 mm; or, the rotating head speed in step (1) is between 4000 and 30000 r / min, preferably 12000-15000 r / min; or, the twist direction in step (1) may be S twist or Z twist; or, the spindle speed in step (1) is 50-12000 r / min, preferably 100-4000 r / min, preferably 400-3000 r / min; or, the roller speed in step (1) is set between 4 and 20 m / min.
[0045] Optionally, the merging and twisting in step (2) is parallel arrangement or twisting together. Optionally, in the twisting method, the twisting direction is opposite to the twisting direction in step (1).
[0046] Optionally, the merging and twisting described in step (2) is to combine at least two rope velvet yarns with different fiber velvet lengths (corresponding to different selections of gauge neck widths) to obtain a fiber velvet structure with different lengths extending outward from the axis and arranged as the core wire.
[0047] Furthermore, the velvet yarn can be subjected to heat treatment or chemical reaction to shrink and curl the fiber fluff, making the surface rough, and can be modified by coating it with functional additives such as flavors and fragrances, phase change materials, etc., to construct filter rods with different structures and effects.
[0048] Optionally, the chenille yarn is a two-dimensional "flat straight line", and the fiber fluff is distributed on both sides of the core material axis. The initial test tube brush-shaped chenille yarn can be processed by yarn wrapping and compaction to form a two-dimensional plane structure. Further, a three-dimensional spiral structure can be formed by secondary twisting, such as a spiral structure with a pitch of 5 mm.
[0049] Application of the cigarette filter rod in cigarettes and heated cigarettes.
[0050] Compared with the prior art, the utility model has the following advantages:
[0051] The utility model provides a cigarette filter rod in a special "test tube brush shape". The cigarette filter rod in a special "test tube brush shape" adopts a rope velvet structure composed of a twisted core wire as an axis and diacetate cellulose fiber fluff arranged neatly and extending outwards. It has the characteristics of small fiber usage, small suction resistance, fast production speed, low cost, stable product structure quality, etc. It is an economical new method for preparing cigarette filter rods. In addition, the obtained filter rod has a novel structure, so that the diacetate fibers that are orderly arranged in a scattered shape from the axis are arranged perpendicular to the direction of smoke flow, which changes the current situation of the traditional diacetate fiber tow in the filter tip being arranged axially for filtering, and has excellent low suction resistance and low smoke interception effects. In addition, the large amount of fluff radially distributed on the cross section and the continuous structure formed with the outer layer of the wrapping material are conducive to the heat absorption and heat conduction of the high-temperature smoke flowing through, showing a good cooling effect. The cigarette filter rod of the utility model can also be used to replace the traditional cigarette filter rod of diacetate cellulose tow, especially the filter rod for medium and thin cigarettes with a circumference of 14-20mm, which can provide a low suction resistance effect. BRIEF DESCRIPTION OF THE DRAWINGS
[0052] Figure 1 This is a schematic diagram of an embodiment of a cigarette filter rod of the utility model.
[0053] Figure 2 It is a longitudinal schematic diagram of an embodiment of the chenille yarn filter rod of the utility model.
[0054] Figure 3 It is a schematic diagram of the spiral structure of one embodiment of the chenille yarn of the utility model.
[0055] Figure 4 Schematic diagram of the principle of preparing a chenille yarn structure for the utility model Figure 1 .
[0056] Figure 5 Schematic diagram of the principle of preparing a chenille yarn structure for the utility model Figure 2 .
[0057] Fig. 6A It is a longitudinal schematic diagram of an embodiment of the "straight-line" chenille yarn of the utility model.
[0058] Figure 6B It is a horizontal schematic diagram of an embodiment of the "straight-line" chenille yarn of the utility model.
[0059] Fig. 7A It is a transverse schematic diagram of an embodiment of the "Y-shaped" chenille yarn of the utility model.
[0060] Figure 7B It is a transverse schematic diagram of an embodiment of a "cross-shaped" chenille yarn of the utility model.
[0061] Figure 7CIt is a transverse schematic diagram of an embodiment of the "snowflake-shaped" chenille yarn of the utility model.
[0062] Figure 8 It is an axial schematic diagram of an embodiment of the chenille yarn of the utility model with a "truncated cone" type structure arrangement.
[0063] Markings in the figure: 1, rotating head; 2, velvet yarn; 4, gauge; 5, chenille yarn; 6, blade;
[0064] 10, filter rod; 10-1, fiber fluff; 10-2, core wire; 10-3, outer wrapping material. DETAILED DESCRIPTION
[0065] The utility model discloses a cigarette filter rod, comprising a filter core part and an outer layer wrapping material, wherein the filter core part comprises a chenille thread, wherein the chenille thread comprises a core thread and fiber fluff arranged along the core thread and extending outward from the axis; the core thread coincides with or is parallel to the axis of the outer layer wrapping material. The fiber fluff of the chenille thread is scattered outward from the axis; the ends of the fiber fluff are in contact with the inner wall of the outer layer wrapping material; the connection point between the fiber fluff and the core thread is spiral or annular along the axis of the core thread.
[0066] Specifically, a cigarette filter rod 10 is composed of an inner chenille yarn composed of fiber fluff 10-1, a core yarn 10-2 and an outer layer of a wrapping material 10-3. The chenille yarn can be a special form similar to a "test tube brush shape". It is a special form of chenille yarn composed of a twisted core yarn 10-2 as an axis and a fiber fluff 10-1 is arranged on the chenille yarn on a fancy spinning machine, including but not limited to diacetate fiber as the fluff yarn and ordinary yarn as the core yarn. Please refer to Figure 1 Its internal pore structure is mainly determined by the spatial distribution of the fiber villi of the chenille yarn.
[0067] Optionally, the connection points between the fiber fluff and the core wire form a spiral line or a ring with the core wire as the axis; further, the extension direction of the spiral line diverges in a spiral (spiral) toward the outer circumference, showing a periodic, uniform and regular distribution.
[0068] Optionally, the fiber fluff is arranged in a periodic structure along the axial direction of the core wire, including one or more combinations of cones, cylinders, truncated cones, etc.
[0069] Optionally, the ends of the fiber fluff are in contact with the inner wall of the outer layer wrapping material. Optionally, the two can be in contact with each other through physical action, preferably, the contact between the two can be achieved by using an adhesive.
[0070] The filter rod of the utility model can provide a new smoke flow channel. The main factors include the materials used for the core wire and fiber fluff, fiber denier, and fiber root number, which affect the main physical indicators of the filter rod including porosity, and then produce different effects on smoke components, cooling and suction resistance.
[0071] The selection of fiber materials of the present invention may consider whether it needs to have phase change heat absorption performance. Among them, acetate fiber (no obvious heat absorption and melting within 200°C) and polylactic acid (melting temperature around 160°C) are representative, and both are green and degradable materials. Acetate fiber has always been the first choice for tobacco materials and has high safety.
[0072] The selection of the core wire material of the utility model can consider the following factors: providing better clamping, axial support, degradable materials, green raw materials, low cost, etc., which can be represented by polyester cotton, polylactic acid, metal wire, etc.
[0073] A method for preparing the cigarette filter rod may include the following steps:
[0074] (1) Selecting cellulose diacetate fiber tow as velvet yarn, with a fineness of 1.3-22 dtex and a fiber number of 100-800. Using any one of filaments, single yarns, and ply yarns with a fineness of 5-80 tex as the core yarn, selecting gauges with different neck widths, adjusting the parameters such as the rotating head speed, twist direction, spindle speed, and roller speed, and obtaining the lanyard yarn through the integrated spinning technology of "velvet yarn cutting-core yarn twisting" (see Figure 6);
[0075] Preferably, the width of the gauge neck is 0.8-4.5 mm, the length of the spun rope velvet yarn is 1.2-9 mm, and the circumference of the cross-sectional circle outer contour is between 3.7 and 28 mm; the width of the gauge neck determines the length of the velvet after cutting and the corresponding circumferential contour to adapt to the circumferential specifications.
[0076] It should be noted that the number of fibers in the fiber bundle used in (1) can affect the number of hairs in a single bundle after shearing, and thus affect the suction resistance of the filter rod.
[0077] The choice of core material has an impact on the shape stability of the velvet sample. As the modulus of the selected core material increases, the clamping of the core material on the fiber fluff is enhanced, and the axial support of the obtained velvet sample is enhanced.
[0078] The single polyester-cotton yarn has low modulus (softness) and insufficient support. The single polymer fiber such as polyethylene fiber and stainless steel wire are selected, which have a large modulus and can provide better clamping and axial support.
[0079] The rotating head speed is between 4000 and 30000 r / min; the twist direction can be S twist or Z twist; the spindle speed is between 100 and 4000 r / min; the roller speed is set between 4 and 20 m / min. This part of the process parameter range interval ensures that the sample can be obtained. The pitch of the obtained chenille yarn is determined by the ratio of the roller speed to the spindle speed.
[0080] (2) The spun chenille yarns can be combined and twisted into chenille yarns of different thicknesses.
[0081] Here is a single chenille thread, but at least 1 thread can be added to the filter rod, and it can be 2 or more threads. This is mainly the outer layer wrapping molding process, which can be 2 threads in parallel and twisted into a whole thread during the traction process (similar to twisting hemp rope).
[0082] The chenille segments are cut into different lengths according to the requirements and packaged into the outer layer wrapping material of the specified filter rod to obtain a cigarette filter rod of a special form; the merging and twisting can be simply arranged in parallel or twisted together. If the twisting method is adopted, the twist direction must be opposite to the twist direction of step (1).
[0083] The utility model achieves the specified requirements through the process to adapt to the inner cavity size of the filter rod with a circumference of 14-28mm and prevent it from moving freely in the outer wrapping material (such as a cardboard tube); at least one lanyard yarn containing a core wire and fiber fluff is used.
[0084] Furthermore, when the fluff fiber used in the chenille yarn material of the present invention has a low denier, such as 2.0 dtex acetate fiber, the overall structure is relatively soft. Therefore, a casing material, such as a paper tube, plastic tube, film tube, etc. with a certain hardness, can be wrapped around the chenille yarn to obtain a cylindrical rod-shaped structure with a stable structure, that is, Figure 1 The cigarette filter rod shown provides a cylindrical shape with satisfactory hardness / roundness / structural stability. The chenille yarn processed by the outer wrapping sleeve process not only maintains the uniform and stable distribution of the fluff in the cylindrical cavity, but also meets the downstream composite filter rod forming process requirements (such as circumference, roundness, hardness), and can be effectively operated on existing cigarette machine equipment, reducing processing costs.
[0085] Furthermore, an adhesive can be added between the fiber fluff of the velvet yarn and the outer wrapping material to improve the adhesion between the two, enhance the overall structural stability, avoid changes in the spatial distribution of the velvet structure in the casing during storage, transportation and use, reduce the possibility of fiber fluff falling when the filter rod is cut short, and reduce the cleaning and maintenance of the filter rod forming process.
[0086] The adhesives used include but are not limited to one or more of the following:
[0087] Polysaccharides and derivatives, including but not limited to starch and starch-based derivatives, dextrin, gum arabic, methyl cellulose, ethyl cellulose, carboxymethyl cellulose, hydroxypropyl methyl cellulose, cellulose acetate and other cellulose derivatives, chitosan and derivatives;
[0088] Polyolefins, including but not limited to polyvinyl acetate (PVAC), vinyl acetate-ethylene copolymers (EVA), acrylic copolymers, polyvinyl pyrrolidone (PVP) and derivatives, polyvinyl pyridine derivatives, styrene maleic acid copolymers, polyvinyl alcohol (PVA);
[0089] Polyethylene terephthalate (PET) and other polyesters, polyurethane (PU), polyamide (PA), polyimide (PI), polyethylene glycol (PEG), polypropylene glycol, ethylene glycol propylene glycol copolymers;
[0090] Gelatin and derivatives, corn starch, paraffin, glycerides, citrates, acetylcitrates, epoxidized vegetable oil esters and other fatty acid esters. Preferably, the adhesive used is food grade.
[0091] A production process of a chenille yarn embodiment: two core wires are passed through Twisting Hundreds of short fibers are clamped, and the fibers actually present a certain spiral arrangement between each node; similar to the arrangement of spiraling stairs, similar to the process of twisting hemp rope, certain fibers are clamped in the nodes, and the spatial arrangement of the fibers also presents a certain rotation with the curvature of the hemp rope (caused by twisting), which may not be in the same plane, but is a periodic extension and divergent arrangement in the cylinder along the axis of the core material.
[0092] Please refer to the attached picture, Fig. 6A , Figure 6B In the figure, the core wire 10-2 is composed of two or more core materials twisted with each other, the fiber fluff 10-1 is fiber fluff and fiber fluff clusters, an angle α is formed between the fiber fluff 10-1 and the core wire 10-2, and the nearly circular diameter of the lanyard is d.
[0093] Fig. 7A , Figure 7B and Figure 7C The chenille yarn with any transverse cross section shown in the figure can be obtained by die extruding the chenille yarn with the corresponding radial transverse cross section.
[0094] Figure 8 The chenille yarn with the "truncated cone" structure shown in the figure can be obtained by cutting the cylindrical chenille yarn, wherein the circular cross-sectional diameters corresponding to the fiber fluffs of different lengths at both ends are (respectively d1 and d2). When d1=d2, the fiber fluffs on the chenille yarn are arranged in a cylindrical periodic manner along the axis of the core material (same Figure 2), when d1 is greater than d2, a truncated cone-shaped structure is presented. When d2 is equal to 0, that is, there is a section of the core material in the middle without fiber fluff clamped, and the periodic change presents a nearly conical structure. The periodic arrangement on the axis can be one or more combinations of the above structures. The above-mentioned cylindrical, truncated cone and conical rope wool yarns are wrapped and limited to obtain a filter rod, which can further increase the porosity of the filter rod and reduce the suction resistance of the filter rod. A periodic interval is 0.5-80mm.
[0095] It is particularly important to emphasize that the drawings of the present invention are for the purpose of facilitating understanding and schematically illustrating the basic structure and principle of the present invention. The scope of the present invention is not limited to the structures shown in the drawings. While meeting basic requirements, the core wires, fiber fluffs, and periodic structures of the present invention are not all absolutely regular and orderly.
[0096] The present invention is further described below in conjunction with specific embodiments.
[0097] like Figures 1 to 8 As shown, a cigarette filter rod 10 comprises a filter core part and an outer layer wrapping material 10-3, wherein the filter core part comprises at least one or more chenille yarn materials.
[0098] The lanyard yarn comprises a core yarn 10-2 and fiber fluff 10-1 extending outwardly along the axis of the core yarn; the axis of the core yarn 10-2 coincides with or is parallel to the axis of the outer layer wrapping material 10-3.
[0099] The three-dimensional appearance of the chenille yarn may be similar to a "test tube brush", and the fiber fluff 10-1 may be scattered outward from the axis, or may form a fixed angle with the axial direction of the core wire 10-2, preferably in the range of 45-135°, more preferably 80-100°.
[0100] In one embodiment, the fiber fluff 10-1 is fixedly arranged on a section from the axis of the core line 10-2 to form, but not limited to, a flat straight-line structure, a Y-shaped structure, a cross structure, or a snowflake structure. The "Y-shaped structure, cross structure, or snowflake structure" refers to a pattern formed by the radial projection of the fiber fluff 10-1 on a sufficiently long section of velvet material on the core line 10-2.
[0101] In one embodiment, the connection point between the fiber fluff 10-1 and the core wire 10-2 is spiral or ring-shaped along the axis of the core wire 10-2. Optionally, the ring-shaped means that, like a ring, a ring of fiber fluff is placed on the core wire 10-2 at a certain distance, and the rings are not connected; the spiral structure has a pitch of 0.2-50mm, preferably 1.2-5mm.
[0102] In one embodiment, the central thickness of the thread-shaped structure corresponds to the diameter of the core material, the thread thickness is proportional to the diameter of the fiber pile 10 - 1 , and the thread pitch corresponds to the inverse of the twist of the chenille yarn.
[0103] In one embodiment, the fiber fluff 10-1 is arranged periodically along the axial direction of the core wire 10-2, including one or more combinations of cones, cylinders, truncated cones, etc. The circumferential spacing is 0.5-80 mm, preferably 5-30 mm.
[0104] In one embodiment, the ends of the fiber fluff 10-1 are in contact with the inner wall of the outer wrapping material 10-3. The ends of the fiber fluff 10-1 can be in contact with the inner wall of the outer wrapping material 10-3 through physical action, preferably, through an adhesive therebetween.
[0105] In one embodiment, the fiber fluff 10-1 can be cut obliquely to form a periodic structure similar to a cone or a truncated cone. Optionally, the fiber fluff 10-1 can also be cut to form a pagoda-like, wave-like, gourd-like, or other special-shaped structures of different diameters.
[0106] In one embodiment, the fiber fluff 10 - 1 is periodically, evenly and neatly distributed inside the outer wrapping material 10 - 3 .
[0107] In one embodiment, the fiber fluff 10-1 can be composed of fluff of different lengths distributed inside the outer wrapping material 10-3. Optionally, the fluff of different lengths is formed by fibers containing at least two different properties, which produce different expansion and contraction changes through physical effects such as tension and heat. Optionally, acetate fiber and high shrinkage polyester fiber are heated to 100°C as fiber fluff at the same time, the polyester fiber curls while the acetate fiber remains basically unchanged, thereby forming a fiber arrangement of different lengths. Optionally, acetate fiber mixed with a single denier of 2.0 dtex and a single denier of 22 dtex is selected as the fiber fluff material. After cutting, the difference in resilience caused by the difference in single denier can cause the final two fibers to shrink to different degrees, so that the fiber fluff of the resulting lanyard yarn presents different lengths.
[0108] In one embodiment, the piles of different lengths can also be formed by twisting two or more chenille yarns with different pile lengths. For example, two chenille yarns can be further arranged in parallel or twisted together into one. At this time, if the fiber lengths of the two chenille yarns are different, the resulting chenille yarn will have two lengths of piles alternately distributed.
[0109] In one embodiment, the cigarette filter rod 11 has a diameter of 4-9 mm and a porosity of 20-99%, preferably 50-99.5%, and more preferably 90-99%.
[0110] Example 1
[0111] (1) 2.2dtex / 430f diacetate cellulose filaments were selected as the fleece yarn, 2 strands of 35tex cotton yarn were used as the core yarn, a gauge with a neck width of 1.8mm was selected, the rotary head speed was set to 15000r / min, the twist direction was Z twist, the spindle speed was 2000r / min, and the roller speed was 8m / min. The yarn was spun on an integrated spinning machine of "fleece yarn cutting-core twisting", and two "test tube brush-shaped" rope fleece yarns were obtained at the same time; the weight was 1100tex, and the fleece length was approximately 3.4mm.
[0112] (2) According to the demand, two spun chenille yarns are paralleled and combined together, and packaged in a hollow paper tube with a circumference of 22.0 mm and a wall thickness of 0.25 mm. After being cut into short pieces, a cigarette filter rod with embedded chenille yarn is obtained. The suction resistance of the 120 mm filter rod is 260 Pa.
[0113] The merging and packaging steps need to reach a specified circumference thickness to prevent the tube from moving at will. In this embodiment, two tubes are merged to meet the filling needs of an empty tube with a circumference of 21.5 mm.
[0114] According to the filling weight of a single velvet material, the filling amount of the filter rod is calculated to be 260 mg, and the porosity is 95.8%.
[0115] For comparison, a single denier 22 dtex acetate fiber tow was selected and opened in a KDF2 / AF2 (Hauni) opening and forming machine at 120-200 m / min to prepare a conventional filter rod A of ultra-high single denier cellulose acetate tow, with a triacetin application amount of 10 wt%, a length of 120 mm, a circumference of 22.0 mm, a filter rod pressure drop of 1000 Pa, a tow filter rod (excluding the outer layer forming paper) weight of 580 mg, and a porosity of about 92%.
[0116] A conventional filter rod B made of cellulose acetate tow prepared with a 6.4 dtex specification tow, a triglyceride application amount of 9.5%, a pressure drop of 2800 Pa, a tow filter rod weight of 560 mg, and a porosity of about 91.4%.
[0117] Comparing the filter rod of the utility model with the above-mentioned two conventional filter rods A and B made of cellulose acetate tow, it can be found that the suction resistance of the filter rod of the utility model prepared by the velvet sample is significantly reduced, which is reduced by 74% and 91% respectively, and the reduction is greater than 70%. The filling weight is reduced by at least 50%, and the corresponding porosity is increased by 4 percentage points.
[0118] Example 2
[0119] (1) 35 tex cotton yarn and 0.2 mm stainless steel wire were used as core yarns, diacetate cellulose tow (2.2 dtex / 430f) was used as velvet yarn, and a gauge with a neck width of 4.0 mm was selected. The rotary head speed was set to 15000 r / min, the twist direction was Z twist, the spindle speed was 3000 r / min, and the roller speed was 6 m / min. The yarn was spun on an integrated spinning machine of "velvet yarn cutting-core twisting". A rope velvet yarn with a gram weight of 1700 tex and a velvet length of approximately 8 mm was obtained at the same time.
[0120] (2) As in Example 1, a single chenille yarn was placed in a hollow paper tube with a circumference of 22.0 mm and a wall thickness of 0.25 mm through a casing process, and a 120 mm chenille yarn-embedded cigarette filter rod was obtained after cutting, with a suction resistance of 130 Pa, a filling amount of 200 mg, and a porosity of 97%.
[0121] Compared with the conventional filter rod B made of 6.4 dtex cellulose acetate tow, the filter rod prepared in this embodiment has a suction resistance reduced by 95%, a filling amount reduced by 65%, and a porosity increased by about 6 percentage points.
[0122] Compared with Example 1, in order to improve the shape stability of the rope velvet yarn, a stainless steel core material is selected to enhance the twisting ability with another core material, thereby improving the fixation and clamping stability of the fluff in the two core material nodes, and meeting the technical requirements of improving axial straightness and supporting performance; the fluff length is increased to 8mm, which can meet the filling requirements of a 22.0mm circular filter rod with a single strand, and is in direct physical contact with the inside of a paper tube with an inner diameter of approximately 6.9mm.
[0123] Example 3
[0124] (1) 28 tex polylactic acid and 0.2 mm copper wire were used as core wires, diacetate cellulose tow (2.2 dtex / 430f) was used as velvet yarn, and a gauge with a neck width of 4.2 mm was selected. The rotary head speed was set to 12000 r / min, the twist direction was Z twist, the spindle speed was 2500 r / min, and the roller speed was 5 m / min. The yarn was spun on an integrated spinning machine of "velvet yarn cutting-core twisting". Two rope velvet yarns with a gram weight of 1500 tex and a velvet of approximately 8.4 mm were obtained at the same time.
[0125] (2) As in Example 1, a single chenille yarn was placed in a hollow paper tube with a circumference of 22.0 mm and a wall thickness of 0.25 mm through a sleeve, and a filter rod with a 120 mm chenille yarn embedded therein was obtained by cutting, with a suction resistance of 260 Pa, a filling amount of 180 mg, and a porosity of 97.2%.
[0126] In contrast to Example 1, polylactic acid and copper wire were selected as core materials, wherein polylactic acid has degradation properties and phase change endothermic cooling properties at 160°C-180°C, polylactic acid and copper wire improve the twisting ability and axial supporting performance of the core material, and the gram weight of the rope velvet can be regulated by controlling the process parameters, thereby changing the filling amount, porosity and other indicators of the obtained filter rod.
[0127] Example 4
[0128] (1) 32 tex polyester / cotton yarn and 0.25 mm polyethylene were used as core yarns, diacetate cellulose tow (2.2 dtex / 430 f) was used as velvet yarn, a gauge with a neck width of 4.5 mm was selected, the rotary head speed was set to 15000 r / min, the twist direction was Z twist, the spindle speed was 3000 r / min, and the roller speed was 6 m / min. The spinning was carried out on a spinning machine integrated with "velvet yarn cutting-core twisting", and two rope velvet yarns were obtained at the same time; the gram weight was 2400 tex, and the velvet length was approximately 9.0 mm.
[0129] (2) As in Example 1, a single chenille yarn was placed in a hollow paper tube with a circumference of 22.0 mm and a wall thickness of 0.25 mm through a sleeve, and a filter rod with a 120 mm chenille yarn embedded therein was obtained by cutting. The filter rod had a pressure drop of 290 Pa, a filling weight of 290 mg, and a porosity of 95%.
[0130] Compared with the conventional 6.4 dtex acetate fiber tow nozzle B, the filter rod pressure drop of this embodiment is reduced by 89%, and the porosity is increased by about 4 percentage points. In addition, this embodiment uses a single polymer polyethylene wire as the core material to meet the technical requirements of improving the twisting, clamping and supporting performance of the core material, and the material has low cost, high safety, easy cutting, low requirements for equipment and machinery, and is conducive to industrialization.
[0131] Example 5
[0132] (1) 32 tex polyester / cotton yarn and 0.25 mm polyethylene were used as core yarns, diacetate cellulose tow (9.0 dtex / 100 f) was used as velvet yarn, a gauge with a neck width of 4.0 mm was selected, the rotary head speed was set to 12000 r / min, the twist direction was Z twist, the spindle speed was 2500 r / min, and the roller speed was 5 m / min. The spinning was carried out on a spinning machine integrated with "velvet yarn cutting-core twisting", and two rope velvet yarns were obtained at the same time; the gram weight was 900 tex and the velvet length was about 8 mm.
[0133] (2) As in Example 1, a single chenille yarn was placed in a hollow paper tube with a circumference of 22.0 mm and a wall thickness of 0.25 mm through a sleeve, and a filter rod with a 120 mm chenille yarn embedded therein was obtained by cutting. The obtained filter rod had a pressure drop of 110 Pa, a filling amount of 110 mg, and a porosity of 98.5%.
[0134] Example 6
[0135] The filter rod is made of two chenille yarns twisted and wrapped, the weight of the obtained chenille yarn is 1800tex, and the rest is basically the same as in Example 5, which will not be repeated here.
[0136] The obtained filter rod had a pressure drop of 230 Pa, a filling amount of 225 mg, and a porosity of 97%.
[0137] Compared with the above-mentioned Examples 1-4, the denier of the acetate fiber in Example 6 and Example 5 was increased to 9.0 dtex, and the filter rod suction resistance was further reduced, the filling amount was reduced, and the porosity was increased to 98.5%. After twisting the two chenille yarns, the filter rod suction resistance still maintained a low pressure drop and porosity.
[0138] Example 7
[0139] Triacetin was used as the adhesive to form a strong physical bond between the chenille pile and the outer paper tube; the rest was basically the same as in Example 5, which will not be repeated here. The pressure drop and porosity of the obtained filter rod were the same as in Example 5, with a pressure drop of 110 Pa and a porosity of 98.5%.
[0140] Example 8
[0141] Polylactic acid (specification 1.8dtex / 50f) was selected as the fluff material, and the obtained rope fleece yarn was twisted with two warps, with a gram weight of 900tex. The rest was basically the same as in Example 5 and will not be repeated here. The obtained filter rod had a suction resistance of 110Pa, a filling amount of 108mg, and a porosity of 98%.
[0142] Example 9
[0143] Ultra-high single-denier cellulose diacetate tow (specification 22.2dtex / 100f) was selected, and the obtained lanyard yarn weight was 900tex. The rest was basically the same as in Example 5 and will not be repeated here. The obtained filter rod had a suction resistance of 60Pa, a filling amount of 110mg, and a porosity of about 98.7%.
[0144] Example 10
[0145] The velvet sample obtained in Example 7 was selected and a polyester-cotton yarn was used as the core wire for wire pressing treatment. The cross-section of the velvet wire formed a two-dimensional plane structure, that is, a flat straight shape (as shown in Figure 7). It can be found that the fiber fluff is distributed on both sides of the core material axis with an angle of 80°. The filter rod obtained by wrapping the molding paper has an absorption resistance of 50Pa, a filling amount of 100mg, and a porosity of about 98.7%.
[0146] Compared with the conventional filter rods A and B made of cellulose acetate tow mentioned above, the velvet structure filter rods prepared in embodiments 1-10 of the utility model exhibit the characteristics of low absorption resistance, high porosity and low filling amount. The absorption resistance is reduced by more than 70%, the filling amount is reduced by more than 50%, the porosity is higher than 95%, and the characteristic of low smoke retention is shown.
[0147] Flue gas analysis:
[0148] The 23 mm Example 5, acetate filter rod A and acetate filter rod B were added to the heated cigarettes for use as mouthpieces. According to the national standard GB / T19609-2004, the smoke temperature and emission of the trial cigarettes were tested using the Canadian deep smoking mode (HCI). The results are shown in Table 1.
[0149] It can be found that compared with conventional acetate filter rods, the nicotine release in the mainstream smoke of heated cigarettes using the chenille filter rod of the utility model increased by 160%, and the maximum smoke temperature did not increase due to the increase in smoke volume, but decreased by about 2°C. This is mainly due to the special spatial arrangement of the chenille hairs in the filter rod, and the pore structure characteristics formed are conducive to heat transfer and reduce the interception of smoke.
[0150] Table 1 Smoke data of heated cigarettes using 23mm different mouthpiece materials
[0151]
[0152] At present, the market mainly adopts the longitudinal channel structure formed by PLA pleated film (for related content, see the published Chinese patent CN104203015B) as the cooling section. The utility model chenille filter rod has low smoke retention, cooling, low filling amount and high porosity.
[0153] The following investigates the effects of the velvet filter rod's absorption resistance, single denier, porosity, and adhesive on flue gas.
[0154] Examples 1-9 respectively verify the effects of denier, fluff length, and filling weight on the porosity and suction resistance of the filter rod. In view of experience, the pressure drop, denier, and porosity (filling amount) of the filter rod have obvious effects on the flue gas. Taking the above factors into consideration, Examples 4-8 are selected to cover technical features such as 1.8-9.0 dtex denier, 95-98.5% porosity, 110-290 Pa pressure drop, application of adhesive, and non-acetate fiber as fluff.
[0155] The 15 mm samples of Examples 4-8 were added to the heated cigarettes for use as cooling sections, and a longitudinal channel structure cooling section formed by a 15 mm PLA corrugated film (weight about 150-200 mg, porosity 75%) was selected as comparison sample C. The smoke temperature and release amount of the trial cigarettes were tested. The results are shown in Table 2.
[0156] Table 2 Smoke data of heated cigarettes using different cooling section mouthpiece materials
[0157]
[0158]
[0159] Compared with the C cooling section, when the chenille structure filter rod of the utility model is used as the cooling section, the maximum temperature of the smoke is reduced, and the nicotine release amount remains basically the same or increases, which mainly increases with the reduction of the suction resistance of the chenille filter rod and the increase of the denier of the fluff, increasing by 0.2-0.3 mg / cig.
[0160] Comparing the preparation method example 5 and the preparation method example 7, triacetin was added as an adhesive, and the porosity of the filter rod was consistent at 98.5%, the nicotine release in the smoke was consistent at 1.93 mg / cig, and the maximum smoke temperature of the mainstream smoke was about 59°C. Within the SD deviation (±1°C), the smoke temperature was basically consistent, indicating that by applying the adhesive on the paper tube and the end of the fiber fluff, the key indicators of the velvet filter rod were not changed, and the nicotine and temperature in the smoke were not significantly affected. The triacetin adhesive mainly plays a fixing role.
[0161] In summary, the cigarette filter rod prepared by the utility model adopts the lanyard yarn structural material, which changes the arrangement mode of the traditional diacetate fiber tow in the filter tip, and has the characteristics of novel structure, small fiber dosage, low suction resistance, large porosity, low smoke adsorption, good cooling effect, etc., and has the advantages of simple preparation process, high production efficiency, low cost, stable product structure quality, and is very easy to industrialize.
[0162] The above-mentioned related explanations and descriptions of the embodiments are for the convenience of ordinary technicians in the technical field to understand and apply the utility model. It is obvious that those familiar with the technology in the field can easily make various modifications to these contents and apply the general principles described here to other embodiments without creative work. Therefore, the utility model is not limited to the above-mentioned related explanations and descriptions of the embodiments. Improvements and modifications made by technicians in the field based on the disclosure of the utility model without departing from the scope of the utility model should be within the scope of protection of the utility model.
Claims
1. A cigarette filter rod, comprising a filter core part and an outer layer of wrapping material, characterized in that: The filter element part comprises at least one or more chenille yarn materials, and the chenille yarn materials comprise a core yarn and fiber fluff extending outwardly along the axis of the core yarn.
2. The cigarette filter rod according to claim 1, characterized in that: The core line is coincident with or parallel to the axis of the outer layer of wrapping material.
3. The cigarette filter rod according to claim 1, characterized in that: The fiber fluff is freely scattered outward from the axis of the core wire or forms a fixed angle with the axial direction of the core wire.
4. The cigarette filter rod according to claim 3, characterized in that: The angle range is 45-135°.
5. The cigarette filter rod according to claim 3, characterized in that: The angle range is 80-100°.
6. The cigarette filter rod according to claim 1, characterized in that: The fiber fluff is fixedly arranged on the axial section of the core wire to form but not limited to a straight-line structure, a Y-shaped structure, a cross structure, and a snowflake structure.
7. The cigarette filter rod according to claim 1, characterized in that: The connection point between the fiber fluff and the core wire is spiral or ring-shaped along the axis of the core wire.
8. The cigarette filter rod according to claim 7, characterized in that: The central thickness of the spiral corresponds to the diameter of the core material, the spiral thickness is proportional to the diameter of the fiber fluff, and the spiral pitch corresponds to the inverse of the twist of the chenille yarn.
9. The cigarette filter rod according to claim 7, characterized in that: The pitch of the spiral is 0.2-50 mm.
10. The cigarette filter rod according to claim 7, characterized in that: The pitch of the spiral is 1.2-5 mm.
11. The cigarette filter rod according to claim 1, characterized in that: The fiber fluff is arranged periodically along the axial direction of the core wire, including one or more combinations of cones, cylinders, and truncated cones.
12. The cigarette filter rod according to claim 11, characterized in that: The circumferential spacing of the periodically arranged structure is 0.5-80 mm.
13. The cigarette filter rod according to claim 11, characterized in that: The circumferential spacing of the periodically arranged structure is 5-30 mm.
14. The cigarette filter rod according to claim 1, characterized in that: The ends of the fiber pile are in contact with the inner wall of the outer wrapping material.
15. The cigarette filter rod according to claim 14, characterized in that: The ends of the fiber pile can be in physical contact with the inner wall of the outer wrapping material.
16. The cigarette filter rod according to claim 14, characterized in that: The ends of the fiber pile may contact the inner wall of the outer wrapping material via an adhesive.
17. The cigarette filter rod according to claim 1, characterized in that: The fiber fluff has a fiber fineness of 0.5-133 dtex.
18. The cigarette filter rod according to claim 1, characterized in that: The fiber fluff has a fiber fineness of 2.2-22 dtex.
19. The cigarette filter rod according to claim 1, characterized in that: The core wire has a fineness of at least 2tex and a strength of at least 2N.
20. The cigarette filter rod according to claim 19, characterized in that: The strong force is greater than or equal to 10N.
21. The cigarette filter rod according to claim 1, characterized in that: The outer wrapping material includes but is not limited to a sheet material, and the thickness of the sheet material is not greater than 4 mm.
22. The cigarette filter rod according to claim 21, characterized in that: The thickness of the sheet material is no more than 2 mm.
23. The cigarette filter rod according to claim 21, characterized in that: The thickness of the sheet material is 0.02-0.5 mm.
24. The cigarette filter rod according to claim 1, characterized in that: The cigarette filter rod has a diameter of 4-9 mm.
25. The cigarette filter rod according to claim 1, characterized in that: The porosity of the cigarette filter rod is 20%-99.9%.
26. The cigarette filter rod according to claim 1, characterized in that: The porosity of the cigarette filter rod is 50%-99.5%.
27. The cigarette filter rod according to claim 1, characterized in that: The porosity of the cigarette filter rod is 90%-99%.
Citation Information
Cited By
Cigarette filter stick and preparation method thereof
CN117814526A