Piston ring with DLC (Diamond Like Carbon) coating with soft and hard two-phase hardness

By adopting a DLC coating structure with soft and hardness on the piston ring, combining the hard phase layer and the soft phase layer, the wear resistance and processing difficulty of the DLC coating in the piston ring is solved, and high wear resistance is achieved. Low friction piston ring.

CN221942581UActive Publication Date: 2024-11-01NANJING FAYN PISTON RING
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323642421.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-29
Publication Date
2024-11-01
Estimated Expiration
2033-12-29

AI Technical Summary

Technical Problem

The existing DLC ​​coatings have problems of poor wear resistance and difficult processing in the piston ring. DLC coatings with high hardness are difficult to process smoothly, while DLC coatings with low hardness are easy to process but lack wear resistance.

Method used

DLC coating structure with soft and hard two-phase hardness is adopted, including a matrix, DLC coating and transition layer. The DLC coating consists of a hard phase layer and a soft phase layer. The hardness of the hard phase layer is 2000-3000HV0.025, and the soft phase layer is The hardness is 800-1600HV0.025, and the bond strength between the substrate and the DLC coating is increased through the chromium layer transition layer.

Benefits of technology

It achieves high wear resistance and low friction performance of the piston ring and improves processing performance, which is significantly better than traditional single-phase DLC coatings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221942581U_ABST
    Figure CN221942581U_ABST
Patent Text Reader

Abstract

The utility model discloses a piston ring with a hard and soft DLC (Diamond Like Carbon) coating. The piston ring comprises a base body, the DLC coating and a transition layer, the transition layer is arranged between the base body and the DLC coating, and the DLC coating comprises a hard phase layer and a soft phase layer. According to the utility model, the excellent use performance of high wear resistance and low friction of the DLC coating is completely maintained, and compared with the traditional single-phase DLC coating, the DLC coating has obvious advantages.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of internal combustion engine piston rings, in particular to a piston ring with a DLC coating having soft and hard two-phase hardness. Background Art

[0002] DLC (Diamond-Like Carbon), as a coating with low friction coefficient and high hardness, plays an increasingly important role in the development of energy saving, emission reduction and service life extension technology for internal combustion engines, and its application is becoming more and more extensive. For piston rings, DLC coating is mainly applied to the outer cylindrical working surface of the piston ring. Compared with traditional coatings, it can reduce the wear of the piston ring and the cylinder, and reduce the friction power consumption between the two.

[0003] According to different application fields, there are high-hardness DLC coating and low-hardness DLC coating. The former improves the wear resistance of the piston ring due to its high hardness, while the latter improves the running-in performance of the piston ring due to its low hardness. However, high-hardness DLC brings the problem of processing difficulties, that is, it is difficult to process the surface smoothly. Although low-hardness DLC has good running-in performance and processing performance, it does not help with wear resistance. Utility Model Content

[0004] Purpose of the utility model: The utility model provides a piston ring with a DLC coating having a soft and hard two-phase hardness, which solves the problem that the existing DLC ​​coating is not wear-resistant or difficult to process.

[0005] Technical solution: The utility model proposes a piston ring with a DLC coating having soft and hard two-phase hardness, comprising a substrate, a DLC coating, and a transition layer; the transition layer is arranged between the substrate and the DLC coating, and the DLC coating comprises a hard phase layer and a soft phase layer.

[0006] Preferably, the DLC coating has a thickness of 0.01 to 0.040 mm.

[0007] Preferably, the transition layer is a chromium layer with a thickness of 0.001 to 0.005 mm.

[0008] Preferably, the hardness of the hard phase layer is 2000-3000 HV0.025, and the thickness is 0.010-0.025 mm.

[0009] Preferably, the hardness of the soft phase layer is 800-1600 HV0.025, and the thickness is 0.002-0.007 mm.

[0010] Preferably, the soft phase layer is located at the outermost layer, and the roughness of the outer cylindrical surface meets the requirement of Rz2.

[0011] Preferably, the surface of the hard phase layer is a rough surface, and the surface of the soft phase layer (5) is a smooth surface.

[0012] Beneficial effects: The utility model fully maintains the excellent performance of the DLC coating, which is high wear resistance and low friction, and has obvious advantages over the traditional single-phase DLC coating. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 This is a schematic diagram of the DLC coating structure of the utility model;

[0014] Figure 2 This is a schematic diagram of the DLC coating morphology of the utility model. DETAILED DESCRIPTION

[0015] The utility model proposes a piston ring with a DLC coating having a soft and hard two-phase hardness, comprising a substrate 1, a DLC coating 2, and a transition layer 3; the transition layer 3 is arranged between the substrate 1 and the DLC coating 2, and the DLC coating 2 comprises a hard phase layer 4 and a soft phase layer 5.

[0016] ①. The total thickness of the DLC coating 2 is 0.010 to 0.040 mm, preferably 0.015 to 0.030 mm.

[0017] ②, the junction of the DLC coating 2 and the substrate has a transition layer 3, the purpose of preparing the transition layer 3 is to ensure the bonding strength between the coating and the substrate 1. The transition layer 3 is a chromium layer, and its thickness is 0.001-0.005mm, preferably 0.001-0.003mm.

[0018] ③. Outside the transition layer 3 is a hard phase layer 4, whose hardness is 2000-3000 HV0.025. Its thickness is selected differently depending on the application field, preferably 0.010-0.025 mm.

[0019] ④. Outside the hard phase layer 4 is the soft phase layer 5, which is also the outermost layer of the coating, and has a hardness of 800-1600 HV0.025, preferably 800-1400 HV0.025, and a thickness of 0.002-0.007 mm, preferably 0.003-0.006 mm.

[0020] ⑤. In the finished product state, the roughness of the outer cylindrical surface meets the requirement of Rz2, preferably Rz1.

[0021] The utility model fully maintains the excellent performance of the DLC coating, which is high wear resistance and low friction, and has obvious advantages over the traditional single-phase DLC coating.

[0022] Compare Projects This patent Single hard phase layer Single soft phase layer Wear resistance good good not good Easy running-in performance good not good good Damage to the cylinder good not good good Outer circle finish good not good good Easy processing performance good not good good

Claims

1. A piston ring having a DLC coating with soft and hard two-phase hardness, It is characterized in that It comprises a substrate (1), a DLC coating (2), and a transition layer (3); the transition layer (3) is arranged between the substrate (1) and the DLC coating (2), and the DLC coating (2) comprises a hard phase layer (4) and a soft phase layer (5).

2. The piston ring having a DLC coating with a soft and hard two-phase hardness according to claim 1, It is characterized in that The DLC coating (2) has a thickness of 0.01 to 0.040 mm.

3. The piston ring having a DLC coating with a soft and hard two-phase hardness according to claim 1, It is characterized in that The transition layer (3) is a chromium layer, and its thickness is 0.001-0.005 mm.

4. The piston ring having a DLC coating with a soft and hard two-phase hardness according to claim 1, It is characterized in that The hardness of the hard phase layer (4) is 2000-3000 HV0.025, and the thickness is 0.010-0.025 mm.

5. The piston ring having a DLC coating with a soft and hard two-phase hardness according to claim 1, It is characterized in that The hardness of the soft phase layer (5) is 800-1600 HV0.025, and the thickness is 0.002-0.007 mm.

6. The piston ring having a DLC coating with a soft and hard two-phase hardness according to claim 1, It is characterized in that The soft phase layer (5) is located at the outermost layer, and the roughness of the outer cylindrical surface meets the requirement of Rz2.

7. The piston ring having a DLC coating with a soft and hard dual-phase hardness according to claim 1, It is characterized in that The surface of the hard phase layer (4) is a rough surface, and the surface of the soft phase layer (5) is a smooth surface.