Vehicle-mounted PFC boost inductor

By using a combination of a ring magnetic core and a thermosetting resin frame in the vehicle-mounted PFC boost inductor, the problems of high production costs of potted inductors and bubble hazards are solved, and higher heat dissipation and reliability are achieved, which is suitable for new energy vehicles. application.

CN221946944UActive Publication Date: 2024-11-01SHENZHEN JINHAODE TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420497622.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-14
Publication Date
2024-11-01
Estimated Expiration
2034-03-14

AI Technical Summary

Technical Problem

The existing potted integrated inductors have high production costs and are prone to bubbles, resulting in major hidden dangers in the insulation safety performance of boost inductors and is not suitable for large-scale automated production, especially in high-humidity environments of automobiles.

Method used

The intermediate core and the end core are fixed by a plastic insulated skeleton to form an annular magnetic core, and are fixedly installed on the base with a thermosetting resin skeleton. The injection molding process is adopted to ensure that there are no pores and good thermal conductivity, suitable for fully automated production, and reduce costs. .

Benefits of technology

It realizes a lower working temperature, improves the heat dissipation and reliability of the inductor, shortens the safe distance between the coil and the magnetic core, reduces production costs, is suitable for the on-board power drive module of new energy vehicles, and enhances the safety and heat dissipation effect of the inductor. .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221946944U_ABST
    Figure CN221946944U_ABST
Patent Text Reader

Abstract

The utility model discloses a vehicle-mounted power factor correction (PFC) boost inductor, which belongs to the technical field of vehicle-mounted PFC boost inductors, and comprises a base, a magnetic core and a coil, the magnetic core comprises two middle magnetic cores arranged in parallel and two end magnetic cores arranged at the two ends of the two middle magnetic cores, the middle magnetic core and the end magnetic core are arranged in an end-to-end connection manner and are fixed through a plastic insulating framework to form an annular magnetic core; a thermosetting resin framework is sleeved outside the annular magnetic core, and the annular magnetic core is fixedly arranged on the base through the thermosetting resin framework; and the coils are respectively arranged on the thermosetting resin framework at positions corresponding to the two middle magnetic cores. The annular magnetic core has the advantages that the middle magnetic core and the end magnetic cores are fixed through the plastic insulation framework to form the annular magnetic core, the annular magnetic core is fixedly installed on the base through the thermosetting resin framework, the working temperature is low, and the annular magnetic core can be used in a vehicle-mounted power driving module of a new energy automobile.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of vehicle-mounted PFC boost inductors, and in particular to a vehicle-mounted PFC boost inductor. Background Art

[0002] The existing DC fast charging infrastructure is basically for 400V cars. If we want to complete the ecological construction of the 800V platform, in addition to upgrading the in-vehicle accessories, we also need to provide corresponding external charging facilities. The in-vehicle accessories include the core three-electric system, air conditioning compressor, DCDC (DC transformer), OBC (on-board charger) and other components, and the external accessories include charging piles and charging stations.

[0003] In order to realize the energy storage function of the supercharging station, the boost inductor needs to consider that in the inverter mode, it will encounter a higher current impact, that is, it is necessary to improve the high saturation capacity of the inductor. At the same time, in order to improve the economic benefits of the charging station, there are also higher requirements for the efficiency improvement of the boost inductor module.

[0004] The production cost of traditional potted integrated inductors is high. Since the magnetic glue used for potting must have high insulation, high thermal conductivity, and high fluidity, the material requirements are extremely high, which will increase the preparation cost of the inductor. The complex structure is not conducive to mass automated production, and it is easy to produce bubbles, which also poses a great hidden danger in the insulation safety performance of the boost inductor. The high humidity application environment of the car will have a great impact on the reliability of the inductor. For example, the utility model patent with announcement number CN215868906U discloses a water-cooled inductor, including a shell, provided with multiple side panels, the multiple side panels are connected in sequence, and enclosed to form a mounting groove; a magnetic core, which is provided with a coil and installed in the mounting groove; the coil is wound around the magnetic core in sequence, and extends two connection ends, the two connection ends pass through the same side panel in the horizontal direction, and are in the same plane; the thermal conductive silica gel is potted in the mounting groove along the opening of the mounting groove, and covers the magnetic core and the coil, and is flush with the shell. It also easily produces bubbles, which poses a great hidden danger in the insulation safety performance of the boost inductor.

[0005] In view of this, the inventor conducted in-depth research on this demand, and thus the present case was produced. Utility Model Content

[0006] In order to overcome the problems in the prior art that the encapsulated integrated inductor has high production cost, is easy to generate bubbles, and has great hidden dangers in terms of the insulation safety performance of the boost inductor, the utility model provides a vehicle-mounted PFC boost inductor, including a base, a magnetic core and a coil, wherein the magnetic core includes two parallel middle magnetic cores and two end magnetic cores arranged at both ends of the two middle magnetic cores, and the middle magnetic cores and the end magnetic cores are arranged end to end and fixed by a plastic insulating frame to form a ring-shaped magnetic core;

[0007] The annular magnetic core is covered with a thermosetting resin frame and is fixedly mounted on the base through the thermosetting resin frame; the coils are respectively arranged at positions on the thermosetting resin frame corresponding to the two middle magnetic cores.

[0008] The middle magnetic core and the end magnetic cores are fixed by a plastic insulating skeleton to form a ring-shaped magnetic core, and are fixed on the base by a thermosetting resin skeleton. It has a low operating temperature and can be used in the on-board power drive module of new energy vehicles.

[0009] Here, the thermosetting resin skeleton adopts the resin glue of hot injection molding, which has excellent thermal conductivity. In particular, there are no air holes between the coil and the magnetic core during molding, so the safety is more guaranteed. It is also suitable for full automation and facilitates the mass production of inductors, reducing the production cost.

[0010] Preferably, the cross section of the middle magnetic core is square. When in use, the inductor is fixed on the base. During use, part of the heat generated by the inductor will be dissipated through the inductor itself, and the heat dissipation pad and the base will also dissipate heat. The square design structure of the coil increases the heat dissipation area of ​​the inductor body compared to the ring design, and the heat dissipation effect is better. The effective area of ​​the core column will also increase, which can increase its inductance and further reduce the design size.

[0011] Preferably, the magnetic core is a magnetic core formed by pressing iron silicon powder, sendust powder or carbonyl iron powder, and of course, it can also be a magnetic core formed by pressing after mixing these powders. One or more of low-loss iron silicon, sendust powder or iron nickel is used as the magnetic core, and the injection molding resin has good heat dissipation, and the operating temperature can be below 125°C under high current and high voltage conditions.

[0012] Preferably, the middle magnetic core is composed of a number of magnetic core blocks, and an air gap is formed between the two adjacent magnetic core blocks and between the magnetic core blocks and the end magnetic cores, and a ceramic sheet is arranged between the air gaps. The flat vertically wound coils of the inductor are neatly arranged and symmetrically arranged on the middle magnetic cores on both sides of the magnetic core. The middle magnetic core is in a strip shape and has an air gap. The magnetic cores at both ends are in a U-shaped structure, and the arc surface is located on the outer circular contour of a toroidal inductor of the same size. Therefore, the effective cross-sectional area of ​​the inductor magnetic core will be significantly increased, and the space occupancy rate of the coil will be greatly improved, so that the space utilization rate of the inductor coil and the magnetic core will be greatly increased, which far exceeds the space utilization rate of the toroidal vertically wound inductor magnetic core material and winding coil. Therefore, the inductance of the inductor is also greater than the inductance of the toroidal inductor.

[0013] Preferably, the thermosetting resin skeleton is also provided with a connecting copper bar and a lead-out copper bar for connecting the connecting ends of two adjacent coils.

[0014] Preferably, the connecting copper busbar and the lead-out copper busbar are welded by argon arc welding, and the weld surface is bright and burr-free, there are no black spots at the weld, there is no blackening at the unpainted parts of the pins, and the welding depth is greater than 1.0-3.0 mm.

[0015] Preferably, an NTC temperature sensor is further provided between the magnetic core and the coil.

[0016] Preferably, the thermosetting resin skeleton is made of one of PBS resin, phenolic resin, epoxy resin, polyimide resin, polytetrafluoroethylene and BT resin, and the processing temperature is 140-260°C.

[0017] Preferably, the thermosetting resin frame is fixedly mounted on the base by fixing nuts and bolts.

[0018] Preferably, a thermal pad is provided between the base and the thermosetting resin frame.

[0019] Beneficial effects:

[0020] The beneficial effects produced by adopting the technical solution of the utility model are as follows:

[0021] (1) The middle magnetic core and the end magnetic core are fixed by a plastic insulating frame to form a ring-shaped magnetic core, and the ring-shaped magnetic core is fixed on the base by a thermosetting resin frame. The ring-shaped magnetic core has a low operating temperature and can be used in the on-board power drive module of new energy vehicles.

[0022] (2) Compared with the boost inductor prepared by potting, the injection molded insulation layer is denser and has no pores. Under the premise of meeting safety requirements, the safe distance between the coil and the magnetic core can be shortened, thereby reducing the volume of the inductor, improving reliability and heat dissipation.

[0023] (3) The vehicle-mounted boost inductor skeleton prepared by the one-piece injection molding process has high structural strength. It is fixed to the vehicle system through the injection molding skeleton, which can meet the working environment of the vehicle with strong vibrations. In addition, the process is simple and easier to automate, which can reduce its production cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] In order to more clearly illustrate the technical solution of the implementation mode of the utility model, the drawings required for use in the implementation mode will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the utility model and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other relevant drawings can be obtained based on these drawings without paying creative work.

[0025] Figure 1 This is a three-dimensional structural diagram of a preferred vehicle-mounted PFC boost inductor of the utility model;

[0026] Figure 2 This is a three-dimensional exploded view of a preferred vehicle-mounted PFC boost inductor of the utility model;

[0027] Figure 3 This is a partial three-dimensional exploded view of a preferred vehicle-mounted PFC boost inductor of the utility model;

[0028] Figure 4 This is a three-dimensional structural diagram of a preferred magnetic core of the utility model;

[0029] Figure 5 This is a three-dimensional structural diagram of a preferred plastic insulation frame of the utility model. DETAILED DESCRIPTION

[0030] In order to make the purpose, technical solutions and advantages of the embodiments of the utility model clearer, the technical solutions in the embodiments of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiments of the utility model. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Therefore, the following detailed description of the embodiments of the utility model provided in the drawings is not intended to limit the scope of the utility model for which protection is sought, but merely represents the selected embodiments of the utility model. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the utility model.

[0031] This embodiment uses a middle magnetic core and an end magnetic core fixed by a plastic insulating skeleton to form a ring-shaped magnetic core, and uses a thermosetting resin skeleton to fix it on the base. It has a lower operating temperature and can be used in the on-board power drive module of new energy vehicles. The specific implementation is as follows:

[0032] like Figure 1-4 As shown, a vehicle-mounted PFC boost inductor comprises a base 1, a magnetic core 2 and a coil 3, wherein the magnetic core 2 comprises two parallel intermediate magnetic cores 21 and two end magnetic cores 22 arranged at both ends of the two intermediate magnetic cores 21, and the intermediate magnetic cores 21 and the end magnetic cores 22 are arranged end to end and fixed by a plastic insulating frame 4 to form a ring-shaped magnetic core;

[0033] The annular magnetic core is covered with a thermosetting resin skeleton 5 and is fixedly mounted on the base 1 through the thermosetting resin skeleton 5 ; the coils 3 are arranged on the thermosetting resin skeleton 5 at positions corresponding to the two middle magnetic cores 21 .

[0034] Here, the thermosetting resin skeleton 5 adopts a resin glue formed by hot injection molding, which has excellent thermal conductivity. In particular, there are no pores between the coil and the magnetic core during molding, so the safety is more guaranteed. It is also suitable for full automation and facilitates the mass production of inductors, reducing the production cost.

[0035] As a preferred embodiment, the cross section of the middle magnetic core 21 is square. When in use, the inductor is fixed on the base. During use, part of the heat generated by the inductor will be dissipated through the inductor itself, and the heat dissipation pad and the base will also dissipate heat. The square design structure of the coil increases the heat dissipation area of ​​the inductor body compared to the ring design, and the heat dissipation effect is better. The effective area of ​​the core column will also increase, which can increase its inductance and further reduce the design size.

[0036] As a preferred embodiment, the magnetic core 2 is a magnetic core formed by pressing iron silicon powder, sendust powder or carbonyl iron powder, and of course, it can also be a magnetic core formed by mixing these powders and pressing them. One or more of low-loss iron silicon, sendust powder or iron nickel is used as the magnetic core, and the injection molding resin has good heat dissipation, and the operating temperature can be below 125°C under high current and high voltage conditions.

[0037] As a preferred embodiment, Figure 3 and 4 As shown, the middle magnetic core 21 is composed of a number of magnetic core blocks 211, and an air gap is formed between the two adjacent magnetic core blocks 211 and between the magnetic core block 211 and the end magnetic core 22, and a ceramic sheet 23 is arranged between the air gaps. The flat vertical winding coils of the inductor are neatly arranged and symmetrically arranged on the middle magnetic cores on both sides of the magnetic core. The middle magnetic core is in strip shape and has an air gap. The magnetic cores at both ends are in a U-shaped structure, and the arc surface is located on the outer circular contour of the toroidal inductor of the same size. Therefore, the effective cross-sectional area of ​​the inductor magnetic core will be significantly increased, and the space occupancy rate of the coil is greatly improved, so that the space utilization rate of the coil and the magnetic core of the inductor is greatly increased, which far exceeds the space utilization rate of the magnetic core material and the winding coil of the toroidal vertical winding inductor. Therefore, the inductance of the inductor is also greater than the inductance of the toroidal inductor.

[0038] As a preferred embodiment, the thermosetting resin skeleton 5 is further provided with a connecting copper bar 31 and a lead-out copper bar 32 for connecting the connecting ends of two adjacent coils 3 .

[0039] As a preferred embodiment, the connecting copper busbar 31 and the lead-out copper busbar 32 are welded by argon arc welding, and the weld surface is bright and burr-free, there are no black spots, there is no blackening at the unpainted parts of the pins, and the welding depth is greater than 1.0-3.0 mm.

[0040] As a preferred implementation, an NTC temperature sensor 6 is further provided between the magnetic core 2 and the coil 3 .

[0041] As a preferred embodiment, the thermosetting resin skeleton 5 is made of one of PBS resin, phenolic resin, epoxy resin, polyimide resin, polytetrafluoroethylene and BT resin, and the processing temperature is 140-260°C.

[0042] As a preferred embodiment, the thermosetting resin skeleton 5 is fixedly mounted on the base 1 by means of fixing nuts 11 and bolts, and a thermal conductive pad 7 is provided between the base 1 and the thermosetting resin skeleton 5 .

[0043] As a preferred embodiment, Figure 5 As shown, the plastic insulating skeleton 4 includes two main fixing skeletons 41 which are relatively arranged on the end magnetic cores 22. The main fixing skeletons 41 are sleeved on the end magnetic cores 22 and each of the main fixing skeletons 41 is limited by a limiting rod 42 with respect to the length direction edges of the two intermediate magnetic cores 21.

[0044] Two openings 43 for the end magnetic cores 22 to pass through are formed on the plastic insulating frame 4 at positions corresponding to the end magnetic cores 22 .

[0045] The limiting rod 42 includes a limiting fixing portion 421 and a limiting main rod portion 422; the limiting fixing portion 421 is integrally arranged at the edge of the opening 43 and the width of the corner guard formed by its extension to both sides is greater than the width of the limiting main rod portion 422; the width of the corner guard at the free end of the limiting main rod portion 422 gradually narrows to form a main rod head 423.

[0046] The method for preparing the boost inductor for vehicle-mounted boost power drive comprises the following steps:

[0047] Step S100: Select a magnetic core made of iron silicon powder, sendust powder or carbonyl iron powder or several of them, the magnetic permeability of the powder core is between 25-90, and the magnetic loss is between 3000-4000kw / m 3 (100mT@50kHz), the conductor is a coil wound with flat copper wire.

[0048] Step S200, the process preparation steps include: winding → magnetic core glue dispensing assembly baking → frame fixing coil and magnetic core → assembly and nut mold → mold flow injection molding → copper bar welding → air shower ultrasonic cleaning and drying → NTC assembly → test packaging;

[0049] Among them, the preheating temperature of the assembled inductor before injection molding is 130℃, the resin molding processing temperature is 140-260℃, the injection pressure is 45-90Mpa, and the holding time is 12-18s;

[0050] The welding requirements of copper busbars using argon arc welding technology are as follows: 1. The surface of the welding area is bright and free of burrs; 2. There are no black spots at the welding area; 3. There is no blackening at the unpainted parts of the pins; 4. The welding depth is greater than 1.0-3.0mm.

[0051] Air shower ultrasonic cleaning steps: ① Ultrasonic cleaning of the copper busbar inductor assembly for 3-5 minutes; ② Blow dry for 1 minute; ③ Dry at 80±10℃ for 30 minutes; ④ Cool to room temperature.

[0052] After the boost inductor is installed with the NTC temperature sensor, it is tested and qualified and packaged.

[0053] The above description is only the preferred implementation of the utility model, and is not intended to limit the utility model. For those skilled in the art, the utility model can have various modifications and changes. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the utility model shall be included in the protection scope of the utility model.

Claims

1. A vehicle-mounted PFC boost inductor, characterized in that: It comprises a base, a magnetic core and a coil, wherein the magnetic core comprises two parallel intermediate magnetic cores and two end magnetic cores arranged at both ends of the two intermediate magnetic cores, the intermediate magnetic cores and the end magnetic cores are arranged end to end and fixed by a plastic insulating frame to form a ring-shaped magnetic core; The annular magnetic core is covered with a thermosetting resin frame and is fixedly mounted on the base through the thermosetting resin frame; the coils are respectively arranged at positions on the thermosetting resin frame corresponding to the two middle magnetic cores.

2. The vehicle-mounted PFC boost inductor according to claim 1, characterized in that: The cross section of the middle magnetic core is square.

3. The vehicle-mounted PFC boost inductor according to claim 1, characterized in that: The magnetic core is a magnetic core formed by pressing silicon iron powder, aluminum sendust powder or carbonyl iron powder.

4. The vehicle-mounted PFC boost inductor according to claim 1, characterized in that: The middle magnetic core is composed of a plurality of magnetic core blocks, and air gaps are formed between two adjacent magnetic core blocks and between the magnetic core blocks and the end magnetic cores, and ceramic sheets are arranged between the air gaps.

5. The vehicle-mounted PFC boost inductor according to claim 1, characterized in that: The thermosetting resin skeleton is also provided with a connecting copper bar and a lead-out copper bar for connecting the connecting ends of two adjacent coils.

6. The vehicle-mounted PFC boost inductor according to claim 5, characterized in that: The connecting copper bar and the lead-out copper bar are welded by argon arc welding, and the weld surface is bright and burr-free, there are no black spots, there is no blackening at the unpainted pins, and the welding depth is greater than 1.0-3.0 mm.

7. The vehicle-mounted PFC boost inductor according to claim 1, characterized in that: An NTC temperature sensor is also arranged between the magnetic core and the coil.

8. The vehicle-mounted PFC boost inductor according to claim 1, characterized in that: The thermosetting resin skeleton is made of one of PBS resin, phenolic resin, epoxy resin, polyimide resin, polytetrafluoroethylene and BT resin.

9. The vehicle-mounted PFC boost inductor according to claim 1, characterized in that: The thermosetting resin frame is fixedly mounted on the base by fixing nuts and bolts.

10. The vehicle-mounted PFC boost inductor according to claim 1, characterized in that: A heat-conducting pad is arranged between the base and the thermosetting resin frame.