Low-volatility wave-absorbing shielding sponge adhesive tape

By adding low-volatilization absorbing materials and PET double-sided adhesive to the conductive sponge, combining polyurethane sponge and nickel structure, the shortcomings of existing conductive sponges in high shielding requirements and high temperature environments are solved, and double electromagnetic wave shielding and low volatility are achieved , suitable for places such as car smart windows.

CN221956018UActive Publication Date: 2024-11-05HANPIN (KUNSHAN) ELECTRONIC CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420588969.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-26
Publication Date
2024-11-05
Estimated Expiration
2034-03-26

AI Technical Summary

Technical Problem

Existing conductive sponges are not enough to meet the needs in some places with high shielding requirements, especially in vehicle-mounted smart windows and other high-temperature environments, which are difficult to effectively control volatile electromagnetic waves, affecting the normal operation of the equipment.

Method used

The electromagnetic wave shielding effect is enhanced through the combination of the low-volatilization absorbing material and the conductive sponge through the two shielding methods of absorption and reflection. The first and second wave absorbing materials and the low-volatilization PET double-sided adhesive are used to enhance the electromagnetic wave shielding effect, and the polyurethane sponge and Nickel structure improves conductivity.

Benefits of technology

Double protection is achieved to minimize electromagnetic interference, and due to its low volatility, it is suitable for high-temperature environments and window applications, improving the application compatibility and overall performance of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221956018U_ABST
    Figure CN221956018U_ABST
Patent Text Reader

Abstract

The utility model discloses a low-volatility wave-absorbing shielding sponge adhesive tape which comprises a conductive shielding sponge, a first wave-absorbing material is arranged on one side of the conductive shielding sponge, the first wave-absorbing material and the conductive shielding sponge are bonded through a first low-volatility PET double-sided adhesive tape, and a second wave-absorbing material is arranged on the other side of the conductive shielding sponge. According to the structure, the conductive shielding sponge serves as a main body, the low-volatility wave-absorbing material adhesive tape with the protective adhesive tape is attached to the single face of the conductive shielding sponge, then the low-volatility wave-absorbing material double-faced adhesive tape is attached to the other face of the conductive shielding sponge, and therefore the conductive shielding sponge is attached to the low-volatility wave-absorbing material adhesive tape with the protective adhesive tape, and the low-volatility wave-absorbing material double-faced adhesive tape is attached to the other face of the conductive shielding sponge. The wave-absorbing layer is added on the basis of the traditional conductive sponge, two shielding modes of wave absorption and reflection are integrated, double protection is achieved, electromagnetic interference can be reduced to the maximum extent, meanwhile, the sponge is suitable for window application due to low volatility, and application compatibility of the sponge is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of adhesive tapes, in particular to a low-volatile wave-absorbing shielding sponge adhesive tape. Background Art

[0002] At present, the conventional conductive sponge structure on the market is mostly polyurethane sponge electroplated with conductive particles to achieve conductive shielding function, which can meet the requirements in most application scenarios, but in some places with special high shielding requirements, this ordinary shielding solution is not enough to meet the application requirements. In addition, with the increasing requirements for vehicle-mounted components, high-standard control requirements are imposed on the high-temperature volatile visible substances of functional materials in vehicle-mounted smart windows, display components, and other lens parts. Therefore, a low-volatile absorbing shielding sponge that combines low volatility and absorbs electromagnetic waves, and can perform secondary reflection and purification of interfering electromagnetic waves through shielding conductive sponges to ensure the good operation of components is particularly important. This low-volatile absorbing shielding sponge tape uses absorbing materials with low-volatile glue and composite conductive sponges. The overall combination integrates two shielding methods, absorption and reflection of electromagnetic waves, as well as low volatility, to fully meet the performance requirements of vehicle-mounted components and further enhance the user experience of vehicle-mounted users. Utility Model Content

[0003] The technical problem solved by the utility model is to provide a low-volatile wave-absorbing shielding sponge tape, which integrates wave-absorbing and reflection shielding methods into one, provides double protection, and can reduce electromagnetic interference to the greatest extent. At the same time, due to its low volatility, it can also be suitable for window applications, thereby increasing the application compatibility of the product.

[0004] The technical solution adopted by the utility model to solve its technical problems is: a low-volatile absorbing shielding sponge tape, comprising a conductive shielding sponge, wherein a first absorbing material is arranged on one side of the conductive shielding sponge, and the first absorbing material and the conductive shielding sponge are bonded by a first low-volatile PET double-sided adhesive, and a second absorbing material is arranged on the other side of the conductive shielding sponge, and the second absorbing material and the conductive shielding sponge are bonded by a second low-volatile PET double-sided adhesive.

[0005] Furthermore, a first low-volatile PET single-sided adhesive is arranged on the side of the first absorbing material away from the first low-volatile PET double-sided adhesive.

[0006] Furthermore, a third low-volatile PET double-sided adhesive tape is arranged on the side of the second absorbing material away from the second low-volatile PET double-sided adhesive tape.

[0007] Furthermore, the conductive shielding sponge comprises a polyurethane sponge, and a nickel structure is electroplated on the surface of the polyurethane sponge.

[0008] Furthermore, the first absorbing material and the second absorbing material are Sendust magnetic powder.

[0009] Furthermore, the overall thickness of the first absorbing material, the first low-volatile PET double-sided adhesive and the first low-volatile PET single-sided adhesive is 0.05 mm to 0.1 mm.

[0010] Furthermore, the overall thickness of the second low-volatile PET double-sided adhesive tape and the third low-volatile PET double-sided adhesive tape of the second absorbing material is 0.05 mm to 0.1 mm.

[0011] The beneficial effect of the utility model is as follows: the structure takes the conductive shielding sponge as the main body, firstly, a low-volatile absorbing material tape with a protective tape is adhered to one side, and then a low-volatile absorbing material double-sided tape is adhered to the other side of the sponge. The final product is a single-sided adhesive absorbing shielding sponge. An absorbing layer is added to the traditional conductive sponge, integrating the two shielding methods of absorption and reflection into one, with double protection, which can minimize electromagnetic interference. At the same time, due to its low volatility, it can also be suitable for window applications, thereby increasing the application compatibility of the product. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 This is a schematic structural diagram of a low-volatile wave-absorbing and shielding sponge tape according to an embodiment of the present application.

[0013] Marked in the figure: 1. first low-volatile PET single-sided adhesive; 2. first absorbing material; 3. first low-volatile PET double-sided adhesive; 4. conductive shielding sponge; 5. second low-volatile PET double-sided adhesive; 6. second absorbing material; 7. third low-volatile PET double-sided adhesive. DETAILED DESCRIPTION

[0014] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific implementation methods of the present invention are described in detail below with reference to the accompanying drawings.

[0015] like Figure 1 As shown, an embodiment of the present application discloses a low-volatile absorbing shielding sponge tape, comprising a conductive shielding sponge 4, wherein a first absorbing material 2 is arranged on one side of the conductive shielding sponge 4, and the first absorbing material 2 and the conductive shielding sponge 4 are bonded to each other through a first low-volatile PET double-sided adhesive 3; a second absorbing material 6 is arranged on the other side of the conductive shielding sponge 4, and the second absorbing material 6 and the conductive shielding sponge 4 are bonded to each other through a second low-volatile PET double-sided adhesive 5.

[0016] Specifically, in this structure, the first absorbing material 2 and the second absorbing material 6 are attached to both sides of the conductive shielding sponge 4, so that the structure has excellent electromagnetic absorption and shielding effects. The characterization parameter magnetic permeability of this product can be in the range of μ'@3MHZ: 120H / m~250H / m.

[0017] The structure is based on the conductive shielding sponge 4. First, a low-volatile absorbing material tape with a protective tape is attached to one side, and then a low-volatile absorbing material double-sided tape is attached to the other side of the sponge. The final product is a single-sided adhesive absorbing shielding sponge. An absorbing layer is added to the traditional conductive sponge, integrating the two shielding methods of absorbing and reflecting into one. The double protection can minimize electromagnetic interference. At the same time, due to its low volatility, it can also be applied to windows, increasing the application compatibility of the product.

[0018] In this embodiment, a first low-volatile PET single-sided adhesive 1 is provided on the side of the first absorbing material 2 away from the first low-volatile PET double-sided adhesive 3, and a third low-volatile PET double-sided adhesive 7 is provided on the side of the second absorbing material 6 away from the second low-volatile PET double-sided adhesive 5. The first absorbing material 2 and the second absorbing material 6 are sendust magnetic powder.

[0019] Specifically, due to long-term use in a high-temperature vehicle operating environment, the sendust magnetic powder is prone to powder shedding. Therefore, the use of the first low-volatile PET single-sided adhesive 1 and the third low-volatile PET double-sided adhesive 7 in this structure can avoid the risk of powder shedding and ensure the overall quality of the product. To ensure the overall softness of the product, the thickness of the first low-volatile PET single-sided adhesive is ≤0.01mm. At the same time, the setting of the third low-volatile PET double-sided adhesive can also make the tape convenient to be attached to the product for use.

[0020] It should be explained that the method of determining low volatility is mainly to cut the product into fixed specifications, place it in a heating container, cover the surface with a glass plate and a black PC plastic sheet, bake it on a heating table at 130°C for 48 hours, then take it out and visually inspect and test the haze at the most serious volatility point. A haze value of <1.0 means low volatility. If droplets appear on the test piece, it is directly determined to be NG. Low volatility is mainly achieved by the carbon-carbon double bonds in the glue raw materials, which are easily broken by heat and react with other components or decompose themselves to produce volatile substances. Therefore, in order to ensure the low volatility of each layer structure in this structure, the low-volatile PET double-sided adhesive and the low-volatile PET single-sided adhesive will pre-volatize the volatile substances through high-temperature baking, thereby ensuring the low volatility of the overall product. The above method is an existing method, and therefore, the above-mentioned low-volatile tape can be purchased on the market or processed by itself.

[0021] In this embodiment, the conductive shielding sponge 4 includes a polyurethane sponge, and a nickel structure is electroplated on the surface of the polyurethane sponge.

[0022] Specifically, the structure adopts the form of polyurethane sponge plus electroplated nickel structure, so that the shielding effectiveness of the conductive shielding sponge 4 30MHZ~1.5GHZ can be greater than 60dB. At the same time, it also has the characteristics of low stress, can be die-cut into any shape, and has excellent filling adaptability for parts, making up for the defect of the single shape of the wrapped foam.

[0023] In this embodiment, the overall thickness of the first absorbing material 2, the first low-volatile PET double-sided adhesive and the first low-volatile PET single-sided adhesive (1) is 0.05mm-0.1mm, and the overall thickness of the second absorbing material 6, the second low-volatile PET double-sided adhesive and the third low-volatile PET double-sided adhesive 7 is 0.05mm-0.1mm.

[0024] Specifically, in this structure, the thickness of the above material is controlled between 0.05 mm and 0.1 mm, thereby preventing the absorbing material from being too thick and causing wrinkles and stratification on the surface of the product.

[0025] The specific embodiments described above further illustrate the purpose, technical solutions and beneficial effects of the present invention. It should be understood that the above description is only a specific embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A low-volatile wave-absorbing shielding sponge tape, characterized in that: The conductive shielding sponge (4) comprises a first absorbing material (2) arranged on one side of the conductive shielding sponge (4), the first absorbing material (2) and the conductive shielding sponge (4) being bonded together via a first low-volatile PET double-sided adhesive (3), a second absorbing material (6) arranged on the other side of the conductive shielding sponge (4), the second absorbing material (6) and the conductive shielding sponge (4) being bonded together via a second low-volatile PET double-sided adhesive (5), and a third low-volatile PET double-sided adhesive (7) being arranged on the side of the second absorbing material (6) away from the second low-volatile PET double-sided adhesive (5).

2. The low-volatile wave-absorbing shielding sponge tape according to claim 1, characterized in that: A first low-volatile PET single-sided adhesive (1) is provided on the side of the first absorbing material (2) away from the first low-volatile PET double-sided adhesive (3).

3. The low-volatile wave-absorbing shielding sponge tape according to claim 1, characterized in that: The conductive shielding sponge (4) comprises a polyurethane sponge, and a nickel structure is electroplated on the surface of the polyurethane sponge.

4. The low-volatile wave-absorbing shielding sponge tape according to claim 1, characterized in that: The first absorbing material (2) and the second absorbing material (6) are sendust magnetic powder.

5. The low-volatile wave-absorbing shielding sponge tape according to claim 2, characterized in that: The overall thickness of the first absorbing material (2), the first low-volatile PET double-sided adhesive and the first low-volatile PET single-sided adhesive (1) is 0.05 mm to 0.1 mm.

6. The low-volatile wave-absorbing shielding sponge tape according to claim 3, characterized in that: The overall thickness of the second absorbing material (6), the second low-volatile PET double-sided adhesive tape and the third low-volatile PET double-sided adhesive tape (7) is 0.05 mm to 0.1 mm.