Double-layer screen structure of wearing product matched with brightness enhancement film

By adding a brightening film and optical adhesive layer between the STN display and the second display, the problem of low reflectivity of the STN display is solved, significantly improving the display effect, and enhancing the anti-glare and wear resistance.

CN221977241UActive Publication Date: 2024-11-08TRULY OPTO ELECTRONICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420688487.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-03
Publication Date
2024-11-08
Estimated Expiration
2034-04-03

AI Technical Summary

Technical Problem

The reflectivity of the STN display is low, resulting in poor display effect and affecting the user's experience.

Method used

Add a brightening film between the STN display screen and the second display screen, and improve the reflectance of the STN display screen through the brightening film. The DBEF film and OCA optical adhesive layer are used for bonding and fixing, combining AG anti-glare coating layer and DLC coating layer to improve display effect.

Benefits of technology

The reflectivity of the STN display is significantly improved from 4.8% to 16.4%, improving the display effect and enhancing anti-glare and wear resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221977241U_ABST
    Figure CN221977241U_ABST
Patent Text Reader

Abstract

The utility model discloses a double-layer screen structure with a wearing product matched with a brightness enhancement film, which comprises an STN display screen, a first optical adhesive layer, a brightness enhancement film, a second optical adhesive layer and a second display screen which are sequentially stacked from top to bottom, the first optical adhesive layer is used for bonding and fixing the STN display screen and the brightness enhancement film, and the second optical adhesive layer is used for bonding and fixing the brightness enhancement film and the second display screen. According to the double-layer screen structure of the wearable product matched with the brightness enhancement films, the brightness enhancement films are increased or decreased between the STN display screen and the second display screen, the reflectivity of the surface of the STN display screen is improved through the brightness enhancement films, and therefore the display effect of the STN display screen is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of display technology, in particular to a double-layer screen structure of a wearable product with a brightness enhancement film. Background Art

[0002] With the development of science and technology, intelligence can be seen everywhere in people's lives, such as smart watches, bracelets and other smart wearable products. In order to improve the convenience of using smart wearable products, wearable products with a double-layer screen structure have become popular. The double-layer screen has two screens, the upper layer is an AMOLED display, and the lower layer is an STN display. Since the STN display is a semi-transparent and semi-reflective screen, it can achieve a double-layer screen display, but the reflectivity of the STN display has certain limitations. For example, when the STN screen is displayed (the AMOLED display is in the off state), due to the low reflectivity, the display effect is poor, and sometimes it is difficult to see the display screen of the STN display, which affects the user's use effect. Utility Model Content

[0003] The purpose of the utility model is to overcome the shortcomings of the prior art and provide a wearable product with a double-layer screen structure with a brightness enhancement film that can improve the display effect of an STN display screen.

[0004] The purpose of this utility model is achieved through the following technical solutions:

[0005] A double-layer screen structure of a wearable product with a brightness enhancement film, comprising: an STN display screen, a first optical adhesive layer, a brightness enhancement film, a second optical adhesive layer and a second display screen, wherein the STN display screen, the first optical adhesive layer, the brightness enhancement film, the second optical adhesive layer and the second display screen are stacked in sequence from top to bottom, the first optical adhesive layer is used for bonding and fixing the STN display screen and the brightness enhancement film, and the second optical adhesive layer is used for bonding and fixing the brightness enhancement film and the second display screen.

[0006] In one embodiment, the brightness enhancement film is a DBEF film.

[0007] In one embodiment, the DBEF film has a thickness of 3 mm.

[0008] In one embodiment, the second display screen is an AMOLED display screen.

[0009] In one embodiment, the first optical adhesive layer is a first OCA optical adhesive layer.

[0010] In one embodiment, the thickness of the first OCA optical adhesive layer is 0.25 mm.

[0011] In one embodiment, the second optical adhesive layer is a second OCA optical adhesive layer.

[0012] In one embodiment, the thickness of the second OCA optical adhesive layer is 0.25 mm.

[0013] In one embodiment, an AG anti-glare coating layer is provided on the surface of the STN display screen.

[0014] In one embodiment, a DLC coating is disposed on the surface of the STN display screen.

[0015] Compared with the prior art, the utility model has at least the following advantages:

[0016] The double-layer screen structure of the wearable product with a brightness enhancement film of the utility model increases the reflectivity of the surface of the STN display screen by adding a layer of brightness enhancement film between the STN display screen and the second display screen, thereby improving the display effect of the STN display screen. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] In order to more clearly illustrate the technical solutions of the embodiments of the present utility model, the drawings required for use in the embodiments are briefly introduced below.

[0018] Figure 1 It is a schematic diagram of the stacking structure of a double-layer screen structure of a wearable product with a brightness enhancement film in one embodiment of the utility model;

[0019] Figure 2 for Figure 1 A schematic diagram of the structure of the second display screen of the double-layer screen structure of the wearable product with a brightness enhancement film;

[0020] Figure 3 for Figure 1 Schematic diagram of the display effect of the STN display screen with a double-layer screen structure and a brightness enhancement film in a wearable product. DETAILED DESCRIPTION

[0021] In order to facilitate the understanding of the present invention, the present invention will be described more comprehensively below with reference to the relevant drawings.

[0022] See also Figure 1 , Figure 2 and Figure 3As shown, a double-layer screen structure 10 of a wearable product with a brightness enhancement film includes: an STN (Super Twisted Nematic) display screen 100, a first optical adhesive layer 200, a brightness enhancement film 300, a second optical adhesive layer 400 and a second display screen 500. The STN display screen 100, the first optical adhesive layer 200, the brightness enhancement film 300, the second optical adhesive layer 400 and the second display screen 500 are stacked in sequence from top to bottom, respectively. The first optical adhesive layer 200 is used to bond and fix the STN display screen 100 and the brightness enhancement film 300, and the second optical adhesive layer 400 is used to bond and fix the brightness enhancement film 300 and the second display screen 500.

[0023] It should be noted that, under the conventional double-layer screen structure, the surface reflectivity of the STN display screen is 4.8%, and the display effect is not good. Therefore, in the present invention, by adding a layer of brightness enhancement film 300 between the STN display screen 100 and the second display screen 500, the surface reflectivity of the STN display screen 100 is made to reach about 16.4% by the brightness enhancement film 300, thereby significantly improving the display effect.

[0024] Preferably, the brightness enhancement film 300 is a DBEF (Dual Brightness Enhancement Film) film. The DBEF film is a thin film reflective polarizer that can provide brightness in the entire viewing range of the liquid crystal display. In this way, even if the second display screen 500 is in the off state, the display effect of the STN display screen can be ensured.

[0025] Preferably, the thickness of the DBEF film is 3 mm.

[0026] In one embodiment, the second display screen 500 is an AMOLED (Active-matrix organic light-emitting diode) display screen. The AMOLED display screen has thin screen, high resolution, wide color gamut and self-luminous characteristics. Therefore, the wearable product can be thinned and the display effect of the wearable product can be improved. Specifically, the structure of the AMOLED display screen includes a glass cover plate, an LTPS (low temperature polycrystalline silicon) layer, an OLED (organic light emitting semiconductor) vapor deposition layer and a glass substrate.

[0027] Preferably, the first optical adhesive layer 200 is a first OCA (Optically Clear Adhesive, special adhesive) optical adhesive layer. The first OCA optical adhesive layer is a special adhesive used for bonding transparent optical elements, and has the characteristics of being colorless and transparent, having high light transmittance and good bonding strength. Preferably, the thickness of the first OCA optical adhesive layer is 0.25 mm.

[0028] Preferably, the second optical adhesive layer 400 is a second OCA optical adhesive layer. Similarly, the OCA optical adhesive layer has the advantages of being colorless and transparent, having high light transmittance and good bonding strength. Preferably, the thickness of the second OCA optical adhesive layer is 0.25 mm.

[0029] In one embodiment, an AG anti-glare coating layer is provided on the surface of the STN display screen 100. By coating a layer of AG anti-glare coating layer on the surface of the STN display screen, an anti-glare effect is achieved, thereby improving the user experience. In addition, an anti-fingerprint AF coating layer can be added above the AG anti-glare coating layer to further improve the anti-fouling and anti-fingerprint effects.

[0030] In one embodiment, a DLC (diamond-like carbon) coating is provided on the surface of the STN display screen 100. Since wearable products frequently come into contact with external objects during use and are prone to wear and tear, a layer of DLC coating is provided on the outer surface of the STN display screen to improve the wear resistance.

[0031] The above-mentioned embodiments only express several implementation methods of the utility model, and the description is relatively specific and detailed, but it cannot be understood as limiting the scope of the utility model patent. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the utility model, which all belong to the protection scope of the utility model. Therefore, the protection scope of the utility model patent shall be based on the attached claims.

Claims

1. A double-layer screen structure of a wearable product with a brightness enhancement film, characterized in that: include: An STN display screen, a first optical adhesive layer, a brightness enhancement film, a second optical adhesive layer and a second display screen, wherein the STN display screen, the first optical adhesive layer, the brightness enhancement film, the second optical adhesive layer and the second display screen are stacked in sequence from top to bottom, wherein the first optical adhesive layer is used for bonding and fixing the STN display screen and the brightness enhancement film, and the second optical adhesive layer is used for bonding and fixing the brightness enhancement film and the second display screen.

2. The double-layer screen structure of the wearable product with a brightness enhancement film according to claim 1, characterized in that: The brightness enhancement film is a DBEF film.

3. The double-layer screen structure of the wearable product with a brightness enhancement film according to claim 2, characterized in that: The thickness of the DBEF film is 3 mm.

4. The double-layer screen structure of the wearable product with a brightness enhancement film according to claim 1, characterized in that: The second display screen is an AMOLED display screen.

5. The double-layer screen structure of the wearable product with a brightness enhancement film according to claim 1, characterized in that: The first optical adhesive layer is a first OCA optical adhesive layer.

6. The double-layer screen structure of the wearable product with a brightness enhancement film according to claim 5, characterized in that: The thickness of the first OCA optical adhesive layer is 0.25 mm.

7. The double-layer screen structure of the wearable product with a brightness enhancement film according to claim 1, characterized in that: The second optical adhesive layer is a second OCA optical adhesive layer.

8. The double-layer screen structure of the wearable product with a brightness enhancement film according to claim 7, characterized in that: The thickness of the second OCA optical adhesive layer is 0.25 mm.

9. The double-layer screen structure of a wearable product with a brightness enhancement film according to claim 1, characterized in that: An AG anti-glare coating layer is arranged on the surface of the STN display screen.

10. The double-layer screen structure of a wearable product with a brightness enhancement film according to claim 1, characterized in that: A DLC coating is arranged on the surface of the STN display screen.