Silicon-carbon negative pole piece and lithium ion battery using same

By constructing a three-dimensional graphene-encapsulated silicon carbon negative electrode sheet in situ on the current collector, the problems of volume changes and low conductivity of silicon materials are solved, and the energy density and rate performance of lithium-ion batteries are improved.

CN222015432UActive Publication Date: 2024-11-15ANHUI GLANCO NEW MATERIAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420379832.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-29
Publication Date
2024-11-15
Estimated Expiration
2034-02-28

AI Technical Summary

Technical Problem

Silicon materials have poor stability due to volume changes and low conductivity in lithium-ion batteries, making it difficult to form a stable solid electrolyte interface, affecting capacity and rate performance.

Method used

A silicon carbon negative electrode sheet wrapped in three-dimensional graphene is constructed directly on the current collector in situ to avoid adding conductive agents and binders to ensure the structural integrity of the graphene network.

Benefits of technology

It improves the energy density and first-time Coulomb efficiency of lithium-ion batteries, reduces the loss of lithium-ion, and enhances the circulation and rate performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222015432U_ABST
    Figure CN222015432U_ABST
Patent Text Reader

Abstract

The utility model discloses a silicon-carbon negative pole piece and a lithium ion battery applying the same, the silicon-carbon negative pole piece comprises a current collector and an active material layer directly constructed on one side of the current collector, and the active material layer is formed by wrapping a plurality of silicon-based materials which are arranged side by side through three-dimensional graphene. According to the lithium ion battery, additional adhesives and conductive agents do not need to be added, the energy density of the lithium ion battery is effectively improved, and a silicon-based / graphene composite material does not need to be scraped, so that the integrity of a graphene three-dimensional network structure can be effectively ensured; the complete three-dimensional network graphene framework can relieve volume fluctuation of the silicon-based material during circulation, prevent pulverization of the electrode material and avoid loss of a large amount of lithium ions, so that the first effect is improved; and the particles are prevented from falling off from the electrode, and charge transfer is promoted, so that the cycle and rate performance of the lithium ion battery is comprehensively improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of lithium ion batteries, and particularly relates to a silicon-carbon negative electrode sheet directly constructed in situ on a current collector. Background Art

[0002] As global environmental pollution and energy crisis intensify, the research and development of clean and renewable energy has become one of the important topics of global concern. Lithium-ion batteries, with their advantages such as high operating voltage, long cycle life and low environmental pollution, dominate the portable device market and become the most promising candidate for electric vehicles and large-scale energy storage systems.

[0003] Among many negative electrode materials, silicon is recognized as the most promising negative electrode material due to its high theoretical specific capacity, moderate operating voltage, rich content and environmental friendliness. However, there are still two key problems that limit the development of silicon materials: (1) During the alloying / de-alloying process, silicon undergoes a huge volume change (300% to 400%), which causes the silicon material to break and pulverize, making it difficult to form a stable solid electrolyte interface (SEI) film, resulting in rapid capacity decay and low initial efficiency of silicon negative electrodes; (2) The intrinsic conductivity of silicon is poor, which limits the rate performance of silicon negative electrodes.

[0004] To solve the above problems, researchers have done a lot of research on suppressing the volume effect of silicon-based materials, forming a stable solid electrolyte interface film (SEI film), and improving its conductivity. Traditional electrode sheets are prepared by a wet slurry method. The addition of a binder can maintain the structural stability of the active material during the charge and discharge process, and ensure good electrical contact between the conductive agent and the current collector. However, these inactive components will trigger side reactions with the electrolyte, and even hinder the transfer of charge, resulting in deterioration of the cycle performance. At the same time, these inactive components will also reduce the overall energy density of the battery and increase the cost. In addition, the rolling process in the wet electrode preparation process damages the structure of the electrode material. Therefore, if a self-integrated electrode material can be developed that is directly constructed in situ on the current collector, it will effectively improve the initial efficiency and cycle performance of the battery. Utility Model Content

[0005] The utility model aims to provide a silicon-carbon negative electrode sheet directly constructed in situ on a current collector. This in-situ preparation method can ensure the integrity of the three-dimensional graphene network structure. At the same time, this self-integrated negative electrode does not require the addition of conductive agents and binders, effectively reducing the side reactions caused by inactive components that do not contribute to the capacity, thereby improving the overall energy density and first coulomb efficiency of the battery.

[0006] In order to achieve the above-mentioned utility model purpose, the utility model adopts the following technical solutions:

[0007] A silicon-carbon negative electrode sheet comprises a current collector and an active material layer directly constructed on one side of the current collector, wherein the active material layer is composed of a plurality of silicon-based materials arranged side by side and wrapped by three-dimensional graphene.

[0008] Further technology of the utility model:

[0009] The silicon-based material is one or more of elemental silicon, silicon / carbon composite, silicon oxygen carbon, silicon carbide, lithium silicon alloy, and silicon oxide;

[0010] Preferably, the size of the silicon-based material is 1 nm to 200 μm.

[0011] The current collector is one or more of continuous copper foil, continuous carbon-coated copper foil, nickel foil, copper wire woven copper mesh, foam nickel, foam copper, carbon cloth, stainless steel sheet, three-dimensional nanoporous copper foil, and three-dimensional nanoporous carbon-coated copper foil;

[0012] Preferably, the current collector has a thickness of 1 to 100 μm.

[0013] Preferably, the loading amount of the silicon-based material in the active material layer is 0.1% to 99.9%.

[0014] The utility model also provides a lithium ion battery using the silicon-carbon negative electrode plate.

[0015] The beneficial effects of the utility model are:

[0016] The utility model has a simple structure and reasonable design. It uses active materials of the silicon-carbon active material layer without adding additional adhesives and conductive agents, which can effectively improve the energy density of lithium-ion batteries. By directly constructing the active material layer in situ on the negative electrode current collector, there is no need to scrape the silicon-based / graphene composite material, thereby effectively ensuring the integrity of the three-dimensional network structure of the graphene, reducing the volume change of the silicon-based material, effectively avoiding the pulverization of the electrode material, and reducing the loss of lithium ions, thereby improving the initial efficiency of the lithium-ion battery. Moreover, the laser-induced three-dimensional graphene can produce a buffering effect between the current collector and the active material, especially in the process of high-rate discharge, it is not easy to produce polarization, which solves the problem of low conductivity of silicon-carbon active materials, thereby comprehensively improving the cycle and rate performance of lithium-ion batteries, and meeting the practicality of electrode plates made of silicon-carbon materials in lithium batteries. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0018] Figure 1 It is a structural schematic diagram of the utility model.

[0019] Figure 2 It is the first charge and discharge curve diagram of Example 1 and Comparative Example 1 of the utility model.

[0020] In the attached figure: 1. current collector; 2. active material layer; 3. three-dimensional graphene; 4. silicon-based material. DETAILED DESCRIPTION

[0021] In order to make the purpose, technical solution and advantages of the embodiment of the utility model clearer, the technical solution in the embodiment of the utility model will be further described in detail below in conjunction with the drawings in the embodiment of the utility model. Obviously, the described embodiment is a part of the embodiment of the utility model but not all. Based on the embodiment of the utility model, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the utility model.

[0022] like Figure 1 As shown, the utility model provides a silicon-carbon negative electrode sheet, including a current collector 1 and an active material layer 2 directly constructed on one side of the current collector, wherein the active material layer is composed of a plurality of silicon-based materials 4 arranged side by side and wrapped by three-dimensional graphene 3.

[0023] The silicon base is silicon oxide with a size of 200nm, the current collector is a single-sided copper foil of 3μm, silicon oxide: graphene = 10:1 (mass ratio), the thickness of the active material layer is 5μm, and the loading amount of silicon oxide in the active material layer is 90.9%.

[0024] Comparative Example 1

[0025] In this comparative example, a negative electrode sheet was prepared by using a conventional wet slurry method to prepare an electrode sheet. The specific scheme is as follows:

[0026] The silicon dioxide / graphene active material layer in Example 1 was scraped off, and mixed and stirred for 7 hours according to the ratio of active material: Super P (conductive agent): PVDF (binder) = 8:1:1, and evenly coated on a single-sided copper foil and vacuum dried to obtain an active material layer with a thickness of 5 μm and a loading amount of silicon dioxide in the active material layer of 90.9%.

[0027] The obtained electrode pieces were cut into 12 mm discs, each disc was weighed, and the discs were put into a glove box filled with argon for assembly. The battery case used was CR2032, the diaphragm was polypropylene cegard2500, the counter electrode was a metal lithium sheet, and 1M LiPF6 was dissolved in a mixture of ethylene carbonate and diethyl carbonate (volume ratio 1:1) as the electrolyte.

[0028] The voltage range of the battery test is 0.01-3V, and the charge and discharge current is 0.1C, 0.25C, 0.5C, 1C. The first discharge specific capacity (mAh / g) and first efficiency (%) of the battery assembled above are tested. The results are as follows: Figure 2 As shown, it is the first charge and discharge curve of Example 1 and Comparative Example 1. It can be seen from the figure that the attenuation rate of the first charge and discharge capacity of Example 1 and Comparative Example 1 at a current density of 500mA / g. The attenuation rates of Example 1 and Comparative Example 1 are 14.71% and 30.12% respectively, and the corresponding first coulomb efficiencies are 85.29% and 69.88% respectively. It can be seen that the pole piece provided by the utility model can effectively improve the first coulomb efficiency of the silicon-carbon negative electrode.

[0029] The above contents are merely examples and explanations of the structure of the utility model. The technicians in this technical field may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the structure of the utility model or exceed the scope defined in the claims, they should all fall within the protection scope of the utility model.

Claims

1. A silicon-carbon negative electrode plate, characterized in that , including a current collector and an active material layer directly constructed on one side of the current collector, wherein the active material layer is composed of a plurality of silicon-based materials arranged side by side and wrapped by three-dimensional graphene.

2. A silicon-carbon negative electrode according to claim 1, characterized in that: The thickness of the current collector is 1 to 100 μm.

3. A silicon-carbon negative electrode according to claim 1, characterized in that: The active material layer has a thickness of 1 to 900 μm.

4. A lithium ion battery, characterized in that: A silicon-carbon negative electrode sheet as described in any one of claims 1 to 3 is used.