Perovskite photovoltaic module

Through the combination of inner and outer edge sealant and high barrier gap filler, a multi-layer sealing structure is formed, which solves the problem of perovskite photovoltaic modules being sensitive to water vapor, significantly improves its resistance ability, extends service life and expands the scope of application.

CN222017142UActive Publication Date: 2024-11-15CHINT NEW ENERGY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420155146.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-22
Publication Date
2024-11-15
Estimated Expiration
2034-01-22

AI Technical Summary

Technical Problem

Perovskite photovoltaic modules are sensitive to water vapor, and the invasion of water vapor leads to the failure of the module, limiting their wide application.

Method used

Using inner and outer edge sealant and high barrier gap filler, a multi-layer sealing structure is formed to block water vapor, including inner edge sealant filling the gap between the front plate glass and the back plate, and outer edge sealant extends to the lower surface of the back plate , and a high barrier gap filler is provided at the border to enhance the sealing effect.

Benefits of technology

It significantly improves the resistance of perovskite photovoltaic modules to water vapor, extends the service life of the module and expands its application range.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222017142U_ABST
    Figure CN222017142U_ABST
Patent Text Reader

Abstract

The utility model discloses a perovskite photovoltaic module, which comprises front plate glass, a battery layer, a packaging adhesive film and a back plate which are sequentially stacked, a frame; an inner edge sealant and an outer edge sealant; wherein the inner edge sealant is filled in grooves formed between the lower surface of the edge part of the front plate glass, the upper surface of the edge part of the back plate and the side surfaces of the battery layer and the packaging adhesive film; the outer edge sealant extends from the upper surface of the edge part of the front plate glass to the lower surface of the edge part of the back plate through the side surface of the front plate glass and the side surface of the back plate so as to form a glue layer with a U-shaped cross section; the cross section of the frame is in a U shape, and the outer edge of the frame is wrapped with the sealant. Through the combined action of the two layers of sealing structures of the inner edge sealant and the outer edge sealant, the water vapor blocking capability of the perovskite assembly is ensured to a great extent, and wide application of the perovskite assembly is facilitated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of photovoltaic components, in particular to a perovskite photovoltaic component. Background Art

[0002] Perovskite photovoltaic modules have great potential in terms of power generation efficiency and cost per kilowatt-hour, and have become a hot spot for research and development. However, the perovskite absorption layer is sensitive to water vapor, and water vapor intrusion can easily cause failure; although various packaging structures are used in the industry to ensure low water vapor transmittance of the module, when the perovskite photovoltaic module needs to be in an outdoor humid environment for a long time, water vapor can still penetrate and erode the perovskite absorption layer at an extremely slow rate, thereby limiting the application of perovskite photovoltaic modules. Therefore, how to improve the water vapor barrier ability of perovskite photovoltaic modules is of great significance to the widespread application of perovskite photovoltaic modules. Utility Model Content

[0003] The purpose of the utility model is to provide a perovskite photovoltaic module, which can improve the water vapor barrier capability to a certain extent, and is conducive to the wide application of the perovskite photovoltaic module.

[0004] In order to solve the above technical problems, the utility model provides a perovskite photovoltaic module, comprising a front plate glass, a battery layer, a packaging film and a back plate stacked in sequence; a frame; an inner edge sealant and an outer edge sealant;

[0005] The inner edge sealant is filled in the gap formed between the lower surface of the edge of the front plate glass, the upper surface of the edge of the back plate, and the side of the battery layer and the packaging film;

[0006] The outer edge sealant extends from the upper surface of the edge of the front plate glass through the side of the front plate glass and the side of the back plate to the lower surface of the edge of the back plate;

[0007] The frame is wrapped with a sealant setting on the outer edge.

[0008] In an optional embodiment of the present application, a high-barrier gap filler is further included to fill and cover the splicing gap area of ​​the frame.

[0009] In an optional embodiment of the present application, the high-barrier gap filler is any one of a two-component curing epoxy resin, a UV curing epoxy resin, or a UV-moisture dual-curing polyurethane modified epoxy resin.

[0010] In an optional embodiment of the present application, the high-barrier gap filler extends to fill the gap between the frame and the front glass;

[0011] And / or, the high-barrier gap filler extends to fill the gap between the frame and the back panel.

[0012] In an optional embodiment of the present application, the cross-section of the frame is a U-shaped cross-section, and the frame is a steel frame with a thickness of 0.3 mm-1 mm.

[0013] In an optional embodiment of the present application, the outer edge sealant is a glue layer with a U-shaped cross section.

[0014] In an optional embodiment of the present application, the inner edge sealant and the outer edge sealant are both butyl rubber.

[0015] In an optional embodiment of the present application, the width of the inner edge sealant is 8mm-15mm.

[0016] In an optional embodiment of the present application, the front panel glass is ultra-white non-tempered glass with a thickness of 2.5mm-3.2mm; the back panel is ordinary white tempered glass with a thickness of 2.5mm-4mm.

[0017] In an optional embodiment of the present application, the packaging film is any one of a POE adhesive layer, a PDMS adhesive layer or a TPU adhesive layer; and the thickness of the packaging film is 0.5 mm-1 mm.

[0018] The utility model provides a perovskite photovoltaic module, comprising a front plate glass, a battery layer, a packaging film and a back plate stacked in sequence; a frame; an inner edge sealant and an outer edge sealant; wherein the inner edge sealant is filled in a gap formed between the lower surface of the edge of the front plate glass, the upper surface of the edge of the back plate, and the side surfaces of the battery layer and the packaging film; the outer edge sealant extends from the upper surface of the edge of the front plate glass through the side surfaces of the front plate glass and the side surfaces of the back plate to the lower surface of the edge of the back plate; and the frame wraps the outer edge sealant.

[0019] In the present application, an inner edge sealant and an outer edge sealant are arranged at the edge of the perovskite photovoltaic module; wherein the inner edge sealant is arranged between the lower surface of the edge of the front plate glass and the upper surface of the edge of the back plate to seal and encapsulate the battery layer from the side of the battery layer; on this basis, the outer edge sealant is arranged as a glue layer structure extending from the upper surface of the front plate glass to the lower surface of the back plate, forming a wrapping and sealing of the edge of the front plate glass, the side of the inner edge sealant and the edge structure of the back plate; thereby, through the joint action of the two-layer sealing structure of the inner edge sealant and the outer edge sealant, the water vapor blocking ability of the perovskite module is guaranteed to a great extent, which is conducive to the widespread application of the perovskite module. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] In order to more clearly illustrate the embodiments of the utility model or the technical solutions of the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0021] Figure 1 A schematic diagram of the cross-sectional structure of the edge structure of the perovskite component provided in an embodiment of the present application. DETAILED DESCRIPTION

[0022] The core of the utility model is to provide a perovskite photovoltaic module, which can achieve good water vapor isolation effect of the perovskite photovoltaic module and is conducive to the wide application of the perovskite photovoltaic module.

[0023] In order to enable those skilled in the art to better understand the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present invention.

[0024] like Figure 1 As shown, Figure 1 A schematic diagram of the cross-sectional structure of the edge structure of the perovskite component provided in an embodiment of the present application.

[0025] In a specific embodiment of the present application, the perovskite photovoltaic module may include:

[0026] A front glass plate 1, a battery layer 2, a packaging film 3 and a back plate 4 are stacked in sequence; a frame 7; an inner edge sealant 5 and an outer edge sealant 6;

[0027] The inner edge sealant 5 is filled in the gap formed between the lower surface of the edge of the front glass 1, the upper surface of the edge of the back plate 4, and the side surfaces of the battery layer 2 and the packaging film 3;

[0028] The outer edge sealant 6 extends from the upper surface of the edge of the front plate glass 1 through the side of the front plate glass 1 and the side of the back plate 4 to the lower surface of the edge of the back plate 4;

[0029] The cross section of the frame 7 is wrapped with a sealant 6 at the outer edge.

[0030] like Figure 1 As shown, the main structure of the perovskite photovoltaic module in this embodiment is composed of a front plate glass 1, a battery layer 2, a packaging film 3 and a back plate 4 which are stacked in sequence.

[0031] In this embodiment, the front glass 1 can be made of ultra-white non-tempered glass with a thickness of 2.5mm-3.2mm, and a layer of ITO or FTO transparent conductive oxide is sputtered on its lower surface; while the back glass can be made of ordinary white tempered glass with a thickness of 2.5mm-4mm.

[0032] The battery layer 2 can be a perovskite battery layer, which includes a hole transport layer, a perovskite absorption layer, an electron transport layer, an electrode layer and a bus bar starting from the front glass 1; of course, in practical applications, the battery layer 2 can also be a battery structure layer formed by stacking perovskite batteries and crystalline silicon batteries.

[0033] The encapsulating film may be any one of a POE adhesive layer, a PDMS adhesive layer or a TPU adhesive layer; and the thickness of the encapsulating film may be 0.5 mm-1 mm.

[0034] exist Figure 1 In the embodiment shown, the size of the front plate glass 1 and the back plate 4 is the same, so the sides of the front plate glass 1 and the back plate 4 are aligned; and the size of the encapsulation film 3 is approximately the same as the size of the battery layer 2, so the side of the battery layer 2 and the side of the encapsulation film 3 are also approximately flush. The size of the front plate glass 1 and the back plate 4 is slightly larger than the size of the battery layer 2. Generally, along the direction perpendicular to the side of the front plate glass 1, the size of the battery layer 2 is approximately 10mm-20mm smaller than the size of the front plate glass 1; thus, the depth of the groove is approximately 5mm-10mm. Therefore, on the basis that the battery layer 2 and the encapsulation film 3 are arranged between the front plate glass 1 and the back plate 4, a gap is formed between the lower surface of the edge of the front plate glass 1, the upper surface of the edge of the back plate 4, and the battery layer 2 and the side of the encapsulation film 3. In this embodiment, the inner edge sealant 5 is filled in the gap; the inner edge sealant 5 surrounds the side of the battery layer 2 to form a circle of glue layer structure, which can also perform the first layer of sealing and encapsulation on the side of the battery layer 2. It is understandable that the inner edge sealant 5 can just completely fill the gap, so that the side of the inner edge sealant 5 facing away from the battery layer 2 and the side of the front plate glass 1 and the side of the back plate 4 are flush with each other. Of course, the inner edge sealant 5 can also extend outside the groove, and a part of the gap can be left on the side facing away from the battery layer 2 without being completely filled, which is not specifically limited in this application. In practical applications, the width of the inner edge sealant 5 along the side direction perpendicular to the front plate glass 1 can be 8mm-15mm.

[0035] On the basis of filling the side of the battery layer 2 with the inner edge sealant 5, an outer edge sealant 6 can be further arranged. The outer edge sealant 6 extends from the upper surface of the edge of the front glass 1 through the side of the front glass 1, the side of the inner edge sealant 5 and the side of the back plate 4 to the lower surface of the edge of the back plate 4, and finally forms a glue layer structure with a cross-section that is roughly a U-shaped cross-section; thereby, the outer edge sealant 6 can fully wrap and seal the edge of the front glass 1, the inner edge sealant 5 and the edge of the back plate 4, that is, to achieve a second layer of sealing of the battery layer 2.

[0036] It should be noted that the upper surface of the front glass 1 in this embodiment is the surface away from the back plate 4, and the lower surface is the surface close to the back plate 4; accordingly, the upper surface of the back plate 4 is the surface close to the front glass 1, and the lower surface is the surface away from the front glass 1.

[0037] In addition, the width of the outer edge sealant 6 on the upper surface of the front glass 1 and extending in a direction perpendicular to the side of the front glass 1 can be 5mm-10mm, so that the edge of the outer edge sealant 6 on the upper surface of the front glass 1 is flush with the side of the inner edge sealant 5 close to the battery layer 2, thereby avoiding the battery layer 2 from absorbing light energy while ensuring a good blocking effect on water vapor.

[0038] In addition, the inner edge sealant 5 and the outer edge sealant 6 can both be made of butyl rubber having a water vapor transmission rate of 0.01 g per square meter per day.

[0039] Based on the above discussion, the inner edge sealant 5 and the outer edge sealant 6 in the present application jointly perform two layers of sealing on the sides of the battery layer 2 from the edge portions of the front glass panel 1 and the back glass panel 4, thereby largely preventing water vapor from penetrating into the interior of the perovskite photovoltaic module, thereby effectively blocking the erosion of the battery layer 2 by water vapor.

[0040] On this basis, a frame 7 is further wrapped on the outer surface of the outer edge sealant 6; the structure of the frame 7 is roughly the same as the shape structure of the outer edge sealant 6, that is, the cross-section of the frame 7 can also be roughly U-shaped, so that the frame 7 can be fully wrapped from the outer surface of the outer edge sealant 6, and then the outer edge sealant 6, the edge structure of the front plate glass 1, the edge structure of the back plate 4 and the inner edge sealant 5 are all wrapped and encapsulated inside the frame 7, thereby further blocking water vapor from penetrating into the interior of the component.

[0041] It can be understood that in addition to blocking the penetration of environmental water vapor into the component, the frame 7 also supports the main structure of the perovskite photovoltaic component; for this reason, in practical applications, the frame 7 can adopt a steel frame 7 with a thickness of 0.3mm-1mm, which has good wind and pressure resistance, thereby improving the overall mechanical strength of the perovskite photovoltaic component.

[0042] In general, the perovskite module mostly adopts a rectangular structure, so the frame 7 can be spliced ​​by two pairs of long frames 7 and short frames 7, and a specific frame assembly machine is also used to bend the four corners of the perovskite module to form a full-circle edge. Regardless of how the frame 7 of the perovskite module is packaged and set at the edge of the module, there will inevitably be a splicing gap; in order to prevent the water vapor in the environment from penetrating into the interior of the module through the splicing gap of the frame 7, in another optional embodiment of the present application, the perovskite photovoltaic module can further include a high-barrier gap filler that fills and covers the splicing gap of the frame 7.

[0043] In this embodiment, a high-barrier gap filler is arranged at the small joints of the frame 7. The high-barrier filler can be made of a two-component curing epoxy resin, a UV-curing epoxy resin, or a UV-moisture dual-curing polyurethane modified epoxy resin, etc. The water vapor permeability of the cured high-barrier gap filler reaches an extremely low 1E-5g per square meter per day; thus, the high-barrier gap filler blocks water vapor from contacting the outer edge sealant 6 from the tiny gaps of the frame 7.

[0044] In an optional embodiment of the present application, the high-barrier gap filler 8 can be further extended to fill the gap between the frame 7 and the front glass 1, thereby achieving a sealed package between the edge of the frame 7 and the front glass 1;

[0045] And / or, the high-barrier gap filler 8 extends to fill the gap between the frame 7 and the back panel 4 .

[0046] like Figure 1 As shown, in Figure 1 In the embodiment shown, the edge of one side of the high-barrier gap filler 8 is flush with the edge of the frame 7. In actual applications, the edge of the high-barrier gap filler 8 close to the frame 7 can be further extended to cover the edge of the frame 7 until it contacts the front glass 1, thereby further improving the sealing effect between the frame 7 and the front glass 1.

[0047] Similarly, the gap between the edge of the frame 7 on the lower surface of the photovoltaic module and the back plate 4 can also be filled and sealed with a high-barrier gap filler 8 .

[0048] In summary, in the present application, an inner edge sealant and an outer edge sealant are arranged at the edge of the perovskite photovoltaic module; wherein the inner edge sealant is arranged between the lower surface of the edge of the front plate glass and the upper surface of the edge of the back plate to seal and encapsulate the battery layer from the side of the battery layer; on this basis, the outer edge sealant is arranged as a glue layer structure extending from the upper surface of the front plate glass to the lower surface of the back plate, forming a U-shaped structure that wraps and seals the edge of the front plate glass, the side of the inner edge sealant and the edge structure of the back plate; thereby, through the joint action of the two-layer sealing structure of the inner edge sealant and the outer edge sealant, the water vapor blocking ability of the perovskite module is largely guaranteed, which is conducive to the widespread application of the perovskite module.

[0049] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply that there is any such actual relationship or order between these entities or operations. Moreover, the term "include", "comprise" or any other variant thereof is intended to cover non-exclusive inclusion, so that the process, method, article or equipment that includes a series of elements are inherent to the elements. In the absence of more restrictions, the elements limited by the sentence "comprise one..." do not exclude the presence of other identical elements in the process, method, article or equipment that includes the elements. In addition, the above-mentioned technical solution provided in the embodiment of the present application is consistent with the corresponding technical solution in the prior art in principle, and the part is not described in detail, so as not to repeat too much.

[0050] This article uses specific examples to illustrate the principles and implementation methods of the utility model. The above examples are only used to help understand the method and core ideas of the utility model. It should be pointed out that for ordinary technicians in this technical field, without departing from the principles of the utility model, the utility model can also be improved and modified, and these improvements and modifications also fall within the scope of protection of the claims of the utility model.

Claims

1. A perovskite photovoltaic module, characterized in that: It includes a front glass, a battery layer, a packaging film and a back plate stacked in sequence; a frame; an inner edge sealant and an outer edge sealant; The inner edge sealant is filled in the gap formed between the lower surface of the edge of the front plate glass, the upper surface of the edge of the back plate, and the side of the battery layer and the packaging film; The outer edge sealant extends from the upper surface of the edge of the front plate glass through the side of the front plate glass and the side of the back plate to the lower surface of the edge of the back plate; The frame is wrapped with a sealant setting on the outer edge.

2. The perovskite photovoltaic module according to claim 1, characterized in that: It also includes a high-barrier gap filler that fills and covers the splicing gap area of ​​the frame.

3. The perovskite photovoltaic module according to claim 2, characterized in that: The high-barrier gap filler is any one of a two-component curing epoxy resin, an ultraviolet curing epoxy resin or an ultraviolet-moisture dual-curing polyurethane modified epoxy resin.

4. The perovskite photovoltaic module according to claim 2, characterized in that: The high-barrier gap filler extends to fill the gap between the frame and the front glass; And / or, the high-barrier gap filler extends to fill the gap between the frame and the back panel.

5. The perovskite photovoltaic module according to claim 2, characterized in that: The cross section of the frame is a U-shaped steel frame with a thickness of 0.3mm-1mm.

6. The perovskite photovoltaic module according to claim 1, characterized in that: The outer edge sealant is a glue layer with a U-shaped cross section.

7. The perovskite photovoltaic module according to claim 1, characterized in that: The inner edge sealant and the outer edge sealant are both butyl rubber.

8. The perovskite photovoltaic module according to claim 1, characterized in that: The width of the inner edge sealant is 8mm-15mm.

9. The perovskite photovoltaic module according to claim 1, characterized in that: The front plate glass is ultra-white non-tempered glass with a thickness of 2.5mm-3.2mm; the back plate is ordinary white tempered glass with a thickness of 2.5mm-4mm.

10. The perovskite photovoltaic module according to claim 1, characterized in that: The packaging film is any one of a POE adhesive layer, a PDMS adhesive layer or a TPU adhesive layer; and the thickness of the packaging film is 0.5 mm-1 mm.