Copper-aluminum composite welding device
By using high-frequency heating devices and cooling water to adjust the temperature in copper-aluminum composite welding devices, the problems of slow heating speed and unstable temperature regulation of existing equipment are solved, and rapid welding and high consistency are achieved, suitable for large batches welding.
Patent Information
- Application Number
- CN202420606824.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-27
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2034-03-27
AI Technical Summary
The existing copper-aluminum composite welding equipment has slow heating speed, resulting in long welding time, unstable temperature regulation, affecting product reliability, and making it difficult to be suitable for large-scale composite welding.
A copper-aluminum composite welding device was designed, using a high-frequency heating device, including a total magnet-conducting magnet, a pressure-bearing block and a heating copper tube. The temperature was adjusted through magnetic field directional heating and cooling water, and the bolted connection between the cast iron formwork and the base plate was ensured. Rapid temperature increase and flexible temperature control.
It achieves rapid and flexible adjustment of welding temperature, shortens welding cycle, improves welding consistency and reliability, and is suitable for large-scale composite welding.
Smart Images

Figure CN222020843U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a copper-aluminum composite welding device. Background Art
[0002] Copper-aluminum composite materials are widely used in the field of electrical hardware. Copper-aluminum composite welding forms a copper-aluminum eutectic at the welding center by heating and pressurizing. The existing copper-aluminum composite welding equipment has a slow heating speed, which leads to a long welding time and a long welding cycle for the product. It is not convenient for large-scale composite welding and has poor temperature control. It cannot stably and reliably maintain the temperature as required, affecting the reliability of the finished product of the entire copper-aluminum composite welding. Therefore, the heating system needs to be further improved and optimized. Utility Model Content
[0003] In order to solve the above problems, the technical problem to be solved by the utility model is to provide a copper-aluminum composite welding device.
[0004] The technical solution adopted by the copper-aluminum composite welding device of the utility model includes: comprising a welding press, an upper template device and a lower template device arranged on the welding press, characterized in that the upper template device and the lower template device both include templates, high-frequency heating devices and a bottom plate in contact with copper and aluminum which are arranged in sequence, the template and the bottom plate are connected by bolts, the high-frequency heating device includes a heating receiving plate arranged on the template, a total combination of magnets arranged between the bottom plate and the heating receiving plate, a pressure block and a heating copper tube, the total combination of magnets includes magnet groups arranged at equal intervals in the horizontal direction, the pressure block is arranged longitudinally between two magnet groups, the magnet groups include magnets arranged at equal intervals in the longitudinal direction, the magnets are concave structures, a magnet insertion opening is provided at the bottom, the heating copper tube is inserted in the magnet insertion opening and is in a hairpin shape, and cooling water is connected in the heating copper tube.
[0005] The height of the pressure block is greater than the height of the magnetic conductor.
[0006] It also includes a buffer pad placed between the magnetic conductor and the bottom plate, and a buffer pad positioning groove is provided at the bottom of the buffer pad for limiting the upper end of the magnetic conductor.
[0007] The heating receiving plate is provided with a first receiving plate limiting groove for limiting the pressure block and a second receiving plate limiting groove for limiting the magnetic conductor.
[0008] It also includes a quartz plate, which is placed between the template and the heating receiving plate.
[0009] The template and the base plate are made of cast iron.
[0010] The advantages of the copper-aluminum composite welding device of the utility model are: the high-frequency heating device directionally heats the welding area by generating a magnetic field, which effectively enables the temperature at the bottom plate to quickly reach the specified welding requirements, and the welding cycle is shorter. At the same time, the welding temperature can be adjusted at any time by connecting cooling water to the copper tube. It is more flexible and controllable to use, has high welding consistency, and is suitable for large-scale composite welding. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] The utility model is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0012] Figure 1 It is a structural schematic diagram of the copper-aluminum composite welding device of the utility model;
[0013] Figure 2 It is an exploded view of the upper template device of the utility model;
[0014] Figure 3 This is a schematic diagram of the installation of the high-frequency heating device of the utility model;
[0015] Figure 4 It is a structural schematic diagram of the magnetic conductor of the utility model;
[0016] Figure 5 It is a structural schematic diagram of the buffer pad of the utility model;
[0017] Figure 6 It is a structural schematic diagram of a heating receiving plate of the utility model. DETAILED DESCRIPTION
[0018] like Figure 1-6As shown, the copper-aluminum composite welding device involved in the utility model comprises a welding press 1, an upper template device 2 and a lower template device 3 arranged on the welding press 1, the upper template device 2 and the lower template device 3 each comprise a template 5, a high-frequency heating device and a bottom plate 11 in contact with the copper and aluminum arranged in sequence, the template 5 and the bottom plate 11 are connected by bolts, the high-frequency heating device comprises a heating receiving plate 7 arranged on the template 5, a magnetic conductor assembly 8 arranged between the bottom plate 11 and the heating receiving plate 7, a pressure block 9 and a heating copper tube 10, the magnetic conductor assembly 8 comprises a magnetic conductor group arranged at equal intervals in the horizontal direction, the bearing The pressing block 9 is longitudinally arranged between the two magnet groups, and the magnet groups include magnets 13 arranged at equal intervals in the longitudinal direction. The magnet 13 is a concave structure, and a magnet insertion opening 14 is provided at the bottom. The heating copper tube 10 is inserted into the magnet insertion opening 14 and is in a hairpin shape. Cooling water is connected to the heating copper tube 10. The high-frequency heating device directionally heats the welding area by generating a magnetic field, which effectively enables the temperature at the bottom plate to quickly reach the specified welding requirements. The welding cycle is shorter and the welding temperature can be adjusted at any time by connecting cooling water to the copper tube. It is more flexible and controllable to use, with high welding consistency, and is suitable for large-scale composite welding.
[0019] The height of the pressure block 9 is greater than the height of the magnetizer 13 to prevent the magnetizer 13 from being damaged due to pressure, thereby increasing the service life of the product.
[0020] It also includes a buffer pad 16 placed between the magnet 13 and the base plate 11. The bottom of the buffer pad 16 is provided with a buffer pad positioning groove 17 for limiting the upper end of the magnet 13, which plays a role in buffering and limiting the upper end of the magnet 13, so that the magnet 13 can be installed more firmly.
[0021] The heating receiving plate 7 is provided with a first receiving plate limiting groove 19 for limiting the pressure block 9 and a second receiving plate limiting groove 20 for limiting the magnetic conductor 13, which can accurately position and is not easy to loosen during pressurization and welding.
[0022] It also includes a quartz plate 6, which is placed between the template 5 and the heating receiving plate 7 to play a heat insulation role to prevent excessive temperature from affecting personnel operations.
[0023] The template 5 and the base plate 11 are made of cast iron, which has higher strength and rigidity and is more heat-resistant.
[0024] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention are included in the protection scope of the present invention.
Claims
1. A copper-aluminum composite welding device, comprising a welding press (1), an upper template device (2) and a lower template device (3) arranged on the welding press (1), characterized in that: The upper template device (2) and the lower template device (3) both comprise a template (5), a high-frequency heating device and a bottom plate (11) in contact with the copper and aluminum, which are arranged in sequence. The template (5) and the bottom plate (11) are connected by bolts. The high-frequency heating device comprises a heating receiving plate (7) arranged on the template (5), a total magnet assembly (8) arranged between the bottom plate (11) and the heating receiving plate (7), a pressure block (9) and a heating copper tube (10). The total magnet assembly (8) comprises magnet groups arranged at equal intervals in the horizontal direction. The pressure block (9) is arranged longitudinally between two magnet groups. The magnet groups comprise magnets (13) arranged at equal intervals in the longitudinal direction. The magnets (13) are concave structures, and a magnet insertion opening (14) is provided at the bottom. The heating copper tube (10) is inserted into the magnet insertion opening (14) and is in a hairpin shape. Cooling water is connected to the heating copper tube (10).
2. The copper-aluminum composite welding device according to claim 1 is characterized in that: The height of the pressure bearing block (9) is greater than the height of the magnetic conductor (13).
3. The copper-aluminum composite welding device according to claim 2 is characterized in that: It also includes a buffer pad (16) disposed between the magnetic conductor (13) and the bottom plate (11), wherein a buffer pad positioning groove (17) for limiting the upper end of the magnetic conductor (13) is provided at the bottom of the buffer pad (16).
4. The copper-aluminum composite welding device according to claim 1, characterized in that: The heating receiving plate (7) is provided with a first receiving plate limiting groove (19) for limiting the pressure block (9) and a second receiving plate limiting groove (20) for limiting the magnetic conductor (13).
5. The copper-aluminum composite welding device according to claim 1, characterized in that: It also includes a quartz plate (6), wherein the quartz plate (6) is placed between the template (5) and the heating receiving plate (7).
6. The copper-aluminum composite welding device according to claim 1, characterized in that: The template (5) and the base plate (11) are made of cast iron.