Mirror surface composite film

Through the multi-layered mirror composite film, the problems of scratching, low reflectivity and unweather resistance of traditional mirror decorative films are solved, and higher scratch resistance, reflective effect and weather resistance are achieved, extending service life and improving Light utilization rate.

CN222024292UActive Publication Date: 2024-11-19FOSHAN NANHAI HUIYOU DECORATION MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323589064.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-27
Publication Date
2024-11-19
Estimated Expiration
2033-12-27

AI Technical Summary

Technical Problem

Traditional mirror decorative films are easy to scratch, have limited reflectivity, and are not weather-resistant, resulting in short service life and easy to discolor and oxidize.

Method used

A mirror composite film with a multi-layer structure includes an outer protective layer, a specular reflective layer, a bottom reinforced mirror reflective layer, a transparent protective layer, a support layer and an adhesive layer. The outer protective layer is made of polyester resin and the specular reflective layer is metal. The film, the underlying reinforcement mirror reflecting layer is a multi-layer metal or oxide film, the transparent protective layer is a polymer resin, the supporting layer is a polyester film, and the adhesive layer is a hydrophilic polymer material.

Benefits of technology

It improves the scratch resistance, reflection effect and weather resistance of the mirror composite film, extends the service life, enhances the light utilization rate and reduces discoloration and oxidation problems.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222024292U_ABST
    Figure CN222024292U_ABST
Patent Text Reader

Abstract

The utility model discloses a mirror surface composite film which comprises an outer protection layer, a mirror surface reflection layer is fixedly arranged on the inner side face of the outer protection layer, a bottom layer enhanced mirror surface reflection layer is fixedly arranged on the inner side face of the mirror surface reflection layer, a transparent protection layer is fixedly arranged on the inner side face of the bottom layer enhanced mirror surface reflection layer, and a supporting layer is fixedly arranged on the inner side of the transparent protection layer. Compared with the prior art, the novel mirror surface composite film has the advantages that the mirror surface reflecting layer, the bottom enhanced mirror reflecting layer and other multi-layer structures are fixedly arranged on the inner side of the outer protective layer, so that the novel mirror surface composite film has better scratch resistance and damage resistance, and the service life of the novel mirror surface composite film is prolonged; the novel mirror surface composite film can improve the reflection effect and the light utilization rate by adopting the mirror surface reflection layer made of a metal film or a metal coating material and adopting a multi-layer metal or oxide film structure for enhancing the mirror surface reflection layer at the bottom layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of decorative films, in particular to a mirror composite film. Background Art

[0002] Mirror decorative film is a common surface material used to increase the beauty of products and reflect light. Traditional mirror decorative films are usually made of a single layer of material, with a reflective layer or metal film coated on the surface. However, these traditional mirror decorative films have some defects, as shown below.

[0003] 1. Easy to be scratched and damaged: Due to the structure of single-layer material, traditional mirror decorative film is often easy to be scratched and damaged, affecting the service life and appearance.

[0004] 2. Limited refractive index and reflectivity: The selection of reflective layer materials for traditional mirror decorative films is relatively limited, resulting in limitations in reflection effect and light utilization.

[0005] 3. Lack of weather resistance: Traditional mirror decorative films are more sensitive to climate change and external environmental factors, and are prone to discoloration, oxidation and other problems. Utility Model Content

[0006] The utility model provides a mirror composite film to solve the above-mentioned problems.

[0007] In order to solve the above technical problems, the technical solution of the utility model is: a mirror composite film, including an outer protective layer, a mirror reflection layer is fixedly provided on the inner side of the outer protective layer, a bottom-layer enhanced mirror reflection layer is fixedly provided on the inner side of the mirror reflection layer, a transparent protective layer is fixedly provided on the inner side of the bottom-layer enhanced mirror reflection layer, a supporting layer is fixedly provided on the inner side of the transparent protective layer, and an adhesive layer is fixedly provided on the inner side of the supporting layer.

[0008] Furthermore, the outer protective layer is made of polyester resin material.

[0009] Furthermore, the mirror reflection layer is made of a metal film or a metal coating material.

[0010] Furthermore, the metal is silver or aluminum.

[0011] Furthermore, the bottom enhanced mirror reflection layer includes multiple layers of metal or oxide films.

[0012] Furthermore, the metal is silver or aluminum, and the oxide is titanium dioxide.

[0013] Furthermore, the transparent protective layer is a polymer resin.

[0014] Furthermore, the supporting layer is a polyester film.

[0015] Furthermore, the adhesive layer is made of a hydrophilic polymer material.

[0016] Compared with the prior art, the utility model has the following advantages:

[0017] 1. Improve scratch resistance and damage resistance: By fixing a multi-layer structure such as a mirror reflection layer and a bottom enhanced mirror reflection layer on the inner side of the outer protective layer, the new mirror composite film has better scratch resistance and damage resistance, and extends its service life.

[0018] 2. Improve reflection effect and light utilization: By using a mirror reflection layer made of metal film or metal coating material, and a multi-layer metal or oxide film structure of the bottom enhanced mirror reflection layer, the new mirror composite film can improve the reflection effect and light utilization.

[0019] 3. Enhanced weather resistance: By introducing a hierarchical structure including a transparent protective layer, a supporting layer and an adhesive layer, the new mirror composite film has better weather resistance, can resist the influence of climate change and external environmental factors, and reduce problems such as discoloration and oxidation. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 It is a schematic diagram of the layered structure of a mirror composite film of the utility model.

[0021] Figure 2 This is a schematic diagram of the cross-sectional structure of a mirror composite film of the utility model.

[0022] As shown in the figure: 1. Outer protective layer; 2. Mirror reflection layer; 3. Bottom enhanced mirror reflection layer; 4. Transparent protective layer; 5. Support layer; 6. Adhesive layer. DETAILED DESCRIPTION

[0023] In the description of the present invention, it should be understood that the terms "upper", "lower", "front", "back", "left", "right", "inside", "outside", "center", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction structure and operation. Therefore, they should not be understood as limitations on the present invention.

[0024] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "provided with", "installed", "connected", "connected" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection, it can be a mechanical connection, it can be an electrical connection, it can be a direct connection, it can be indirectly connected through an intermediate medium, and it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0025] The utility model is further described in detail below in conjunction with the accompanying drawings.

[0026] Combined with Figure 1 To Attachment Figure 2 A mirror composite film comprises an outer protective layer 1, the outer protective layer 1 is made of polyester resin material, a mirror reflection layer 2 is fixedly arranged on the inner side of the outer protective layer 1, the mirror reflection layer 2 is made of metal film or metal plating material, the metal is silver or aluminum, a bottom layer enhanced mirror reflection layer 3 is fixedly arranged on the inner side of the mirror reflection layer 2, the bottom layer enhanced mirror reflection layer 3 comprises multiple layers of metal or oxide film, the metal is silver or aluminum, the oxide is titanium dioxide, a transparent protective layer 4 is fixedly arranged on the inner side of the bottom layer enhanced mirror reflection layer 3, the transparent protective layer 4 is polymer resin, a supporting layer 5 is fixedly arranged on the inner side of the transparent protective layer 4, the supporting layer 5 is polyester film, an adhesive layer 6 is fixedly arranged on the inner side of the supporting layer 5, and the adhesive layer 6 is made of hydrophilic polymer material.

[0027] The functions of each layer of a mirror composite film are as follows:

[0028] 1. Outer protective layer: The outer protective layer made of polyester resin material is located at the outermost layer of the mirror composite film. Its main function is to protect the internal layer structure from scratches and damage and improve the durability of the mirror composite film.

[0029] 2. Mirror reflection layer: The mirror reflection layer is fixed on the inner side of the outer protective layer. The mirror reflection layer is made of metal film or metal coating material, such as silver or aluminum. The mirror reflection layer has a high reflectivity and can effectively reflect the incident light and provide a good reflection effect.

[0030] 3. Bottom-layer enhanced mirror reflection layer: The bottom-layer enhanced mirror reflection layer is fixed on the inner side of the mirror reflection layer. The bottom-layer enhanced mirror reflection layer is composed of multiple layers of metal or oxide films, such as silver or aluminum and titanium dioxide. The multi-layer structure of the bottom-layer enhanced mirror reflection layer further improves the reflection effect and light utilization.

[0031] 4. Transparent protective layer: The transparent protective layer is located on the inner side of the bottom enhanced mirror reflective layer. The transparent protective layer is made of polymer resin and has good transparency and weather resistance. Its function is to protect the bottom enhanced mirror reflective layer from climate change and external environmental factors, and reduce problems such as discoloration and oxidation.

[0032] 5. Support layer: The support layer is located on the inner side of the transparent protective layer and is made of polyester film. The support layer has good strength and stability, which enhances the structural stability and durability of the mirror composite film.

[0033] 6. Adhesive layer: The adhesive layer is located on the inner side of the support layer and is made of hydrophilic polymer material. The adhesive layer can effectively bond the various layers together and enhance the overall structural stability of the composite membrane.

[0034] The above description of the utility model and its implementation methods is not restrictive. The drawings show only one implementation method of the utility model, and the actual structure is not limited thereto. In short, if ordinary technicians in this field are inspired by it and design structural methods and embodiments similar to the technical solution without creativity without departing from the purpose of the invention of the utility model, they should all fall within the protection scope of the utility model.

Claims

1. A mirror composite film, comprising an outer protective layer (1), characterized in that: A mirror reflection layer (2) is fixedly provided on the inner side of the outer protective layer (1), a bottom-layer enhanced mirror reflection layer (3) is fixedly provided on the inner side of the mirror reflection layer (2), a transparent protective layer (4) is fixedly provided on the inner side of the bottom-layer enhanced mirror reflection layer (3), a support layer (5) is fixedly provided on the inner side of the transparent protective layer (4), and an adhesive layer (6) is fixedly provided on the inner side of the support layer (5); The outer protective layer (1) is made of polyester resin material; The mirror reflection layer (2) is made of a metal film or a metal coating material; The bottom enhanced mirror reflection layer (3) comprises a plurality of thin films made of metal or a plurality of thin films made of oxide; The transparent protective layer (4) is a polymer resin; The support layer (5) is a polyester film; The adhesive layer (6) is made of a hydrophilic polymer material.

2. A mirror composite film according to claim 1, characterized in that: The metal in the mirror reflection layer (2) is silver or aluminum.

3. The mirror composite film according to claim 1, characterized in that: The metal in the bottom enhanced mirror reflection layer (3) is silver or aluminum, and the oxide is titanium dioxide.