Nanoscale wrapped aluminum hypophosphite production system
In the nano-scale encapsulated aluminum hypophosphate production system, the problem of agglomeration and explosion risk of nano-scale aluminum hypophosphate is solved by using reactors and nanopumps to ensure uniform mixing and wrapping of aluminum hypophosphate and organic calcium, and the problem of nano-scale aluminum hypophosphate agglomeration and explosion is achieved. Stable distribution and close mixing in rubber and plastic.
Patent Information
- Application Number
- CN202420670244.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-02
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2034-04-02
AI Technical Summary
Nano-scale aluminum subphosphate is prone to agglomeration during the production process, resulting in unstable material, and there is a risk of explosion during the crushing process after drying, making it difficult to achieve uniform distribution in rubber or plastic.
A nano-scale encapsulated aluminum hypophosphate production system was designed to ensure uniform mixing and wrapping effect through the reaction of aluminum sulfate, water, sodium hypophosphate and organic calcium in the reactor, and realize the uniform mixing and wrapping effect by boiling dryer. The nano-state does not need to be crushed again to avoid the risk of explosion.
The uniform distribution and stability of nano-scale aluminum hypophosphate in organic calcium is achieved, which avoids the risk of explosion, and ensures its close mixing with rubber and plastic, improving the stability and safety of the material.
Smart Images

Figure CN222034699U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of aluminum hypophosphite production, in particular to a nanometer-level encapsulated aluminum hypophosphite production system. Background Art
[0002] Aluminum hypophosphite is a flame retardant material. In order to achieve the best effect, it needs to be evenly distributed in rubber, plastic and other materials. The finer the aluminum hypophosphite, the more evenly distributed it will be. Therefore, the aluminum hypophosphite needs to reach the nanometer level. The current aluminum hypophosphite can easily reach the nanometer level during the production process, but nanomaterials have a large specific surface area, high activity, and are extremely unstable. They are extremely easy to agglomerate and lose their original properties, reducing the value of the material.
[0003] In order to solve the agglomeration problem of nanopowders, it is necessary to adopt certain means to evenly disperse the nanopowders. At present, the most widely used method is chemical dispersion, that is, surface modification. Surface modification refers to the use of surface additives to cause chemical reactions and physical effects on the surface of particles, thereby changing the surface state of particles. Surface additives are currently mostly inorganic calcium salts, mainly calcium hypophosphite and calcium chloride. Aluminum hypophosphite is also an inorganic salt. Due to the polarity of particles, they can generally only be simply mixed evenly. Inorganic calcium salts are used to isolate the gaps between aluminum hypophosphite particles, and no coating effect can be formed; and after drying, they are only at the micron level. After drying, they need to be crushed and ground. A large amount of heat energy will accumulate during grinding, and explosions will occur under the conditions of oxygen and electric sparks. Nitrogen protection is generally required. Nitrogen protection is required during the crushing process, and improper nitrogen protection will also cause explosions. Utility Model Content
[0004] The utility model aims to provide a nano-scale encapsulated aluminum hypophosphite production system.
[0005] The utility model is implemented by the following technical scheme: a nano-scale encapsulated aluminum hypophosphite production system, which includes an aluminum sulfate storage tank, a water tank, a stirring tank, a high-level tank, a reaction kettle, a sodium hypophosphite storage tank, a filter press, a sodium sulfate storage tank, a boiling dryer, and an organic calcium storage tank;
[0006] The outlet of the aluminum sulfate storage tank and the first outlet of the water tank are respectively connected to the inlet pipeline of the stirring tank, the outlet of the stirring tank is connected to the inlet pipeline of the header tank, and the outlet of the header tank is connected to the inlet pipeline of the reactor;
[0007] The outlet of the sodium hypophosphite storage tank and the second outlet of the water tank are respectively connected to the inlet pipeline of the reactor;
[0008] The outlet of the organic calcium storage tank is connected to the inlet pipeline of the reactor;
[0009] The outlet of the reactor is connected to the inlet pipeline of the filter press, the liquid phase outlet of the filter press is connected to the inlet pipeline of the sodium sulfate storage tank, and the solid phase outlet of the filter press is connected to the inlet pipeline of the boiling dryer.
[0010] Furthermore, a water jacket is fixed on the outer wall of the reactor, and a water inlet and a water outlet are provided on the water jacket.
[0011] Furthermore, a circulation pipe is connected between the bottom and top of the reactor, and a nano pump is installed on the circulation pipe.
[0012] Furthermore, the reactor is provided with a thermometer.
[0013] Furthermore, the outlet of the high-level tank is connected to the inlet pipeline of the reactor through a metering pump.
[0014] The utility model has the following advantages: through the system, nanometer-scale aluminum hypophosphite is evenly distributed in nanometer-scale organic calcium, and it remains in the nanometer state after drying, and does not need to be crushed again, and there is no risk of explosion; the organic calcium is wrapped on the aluminum hypophosphite and is evenly distributed with each other, and the organic calcium is a stabilizer and catalyst for rubber and plastic, and can be fully mixed with rubber and plastic. The organic calcium can be fully mixed with the aluminum hypophosphite and can also be fully mixed with the rubber and plastic, thus ensuring the close mixing of the aluminum hypophosphite and the rubber and plastic. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0016] Figure 1 This is a schematic diagram of the structure of the utility model;
[0017] In the figure: aluminum sulfate storage tank 1, water tank 2, mixing tank 3, high-level tank 4, reactor 5, sodium hypophosphite storage tank 6, organic calcium storage tank 7, circulation pipe 8, nano pump 9, filter press 10, sodium sulfate storage tank 11, boiling dryer 12, water jacket 13, water inlet 14, water outlet 15, thermometer 16, metering pump 17. DETAILED DESCRIPTION
[0018] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0019] like Figure 1 As shown, the nano-scale encapsulated aluminum hypophosphite production system includes an aluminum sulfate storage tank 1, a water tank 2, a stirring tank 3, a high-level tank 4, a reaction kettle 5, a sodium hypophosphite storage tank 6, a filter press 10, a sodium sulfate storage tank 11, a boiling dryer 12, and an organic calcium storage tank 7;
[0020] The outlet of the aluminum sulfate storage tank 1 and the first outlet of the water tank 2 are respectively connected to the inlet pipeline of the stirring tank 3. The stirring tank 3 is provided with an agitator. The aluminum sulfate in the aluminum sulfate storage tank 1 adopts ordinary industrial grade. The outlet of the stirring tank 3 is connected to the inlet pipeline of the high-level tank 4. The outlet of the high-level tank 4 is connected to the inlet pipeline of the reactor 5. In the stirring tank 3, the aluminum sulfate is dissolved in water.
[0021] The outlet of the sodium hypophosphite storage tank 6 and the second outlet of the water tank 2 are respectively connected to the inlet pipeline of the reactor 5, and the outlet of the organic calcium storage tank 7 is connected to the inlet pipeline of the reactor 5. The organic calcium in the organic calcium storage tank 7 is nanometer-grade, specifically calcium terephthalate. Aluminum sulfate solution reacts with sodium hypophosphite to generate aluminum hypophosphite and sodium sulfate. A circulation pipe 8 is connected between the bottom and the top of the reactor 5. A nanopump 9 is installed on the circulation pipe 8. The function of the nanopump 9 is to ensure the full mixing of the sodium hypophosphite and the organic calcium and the full reaction and mixing between the later materials to maintain the formation of the nanometer state.
[0022] The outlet of the reactor 5 is connected to the inlet pipeline of the filter press 10 , the liquid phase outlet of the filter press 10 is connected to the inlet pipeline of the sodium sulfate storage tank 11 , and the solid phase outlet of the filter press 10 is connected to the inlet pipeline of the boiling dryer 12 .
[0023] Furthermore, a water jacket 13 is fixed on the outer wall of the reactor 5, and a water inlet 14 and a water outlet 15 are provided on the water jacket 13. Heat exchange media (such as water) of different temperatures are introduced into the water jacket 13 to heat up or cool down the materials in the reactor 5.
[0024] Furthermore, the reactor 5 is provided with a thermometer 16 , and the thermometer 16 is used to ensure that the reaction temperature in the reactor 5 meets the required value.
[0025] Furthermore, the outlet of the high-level tank 4 is connected to the inlet pipeline of the reactor 5 through a metering pump 17, and the metering pump 17 is used to control the addition amount of the aluminum sulfate aqueous solution.
[0026] Through this system, nano-scale aluminum hypophosphite is evenly distributed in nano-scale organic calcium, and it remains in a nano state after drying, without the need for re-crushing, and there is no risk of explosion; the organic calcium is wrapped on the aluminum hypophosphite and is evenly distributed with each other. In addition, organic calcium is a stabilizer and catalyst for rubber and plastic, and can be fully mixed with rubber and plastic. The organic calcium can be fully mixed with aluminum hypophosphite, and can also be fully mixed with rubber and plastic, thus ensuring the close mixing of aluminum hypophosphite and rubber and plastic.
[0027] The specific operation process of this embodiment is as follows:
[0028] After sodium hypophosphite and water are added into the reactor 5, the temperature is raised to 90°C with stirring, the conversion rate is improved, and the sodium hypophosphite is dissolved in water. Then, organic calcium is added into the reactor 5. Under the action of the nano pump 9, the organic calcium is fully mixed with the sodium hypophosphite, the reaction is uniform, and the nano state is maintained. When the nano pump 9 is running, an aqueous solution of aluminum sulfate is slowly added dropwise, and the aluminum sulfate solution reacts with the sodium hypophosphite to generate aluminum hypophosphite and sodium sulfate. After the addition is completed, the temperature is lowered to room temperature, and the nano pump 9 is maintained to continue circulating for 2 hours to ensure that the reaction is fully carried out, and finally the products of sodium sulfate and encapsulated aluminum hypophosphite are produced;
[0029] The product after the reaction is sent to the filter press 10, and the product is separated into solid and liquid by the filter press 10. The liquid sodium sulfate aqueous solution is sent to the sodium sulfate storage tank 11, and the solid encapsulated aluminum hypophosphite is sent to the boiling dryer 12 for drying.
[0030] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. Nano-scale encapsulated aluminum hypophosphite production system, It is characterized in that It includes aluminum sulfate storage tank, water tank, mixing tank, high-level tank, reactor, sodium hypophosphite storage tank, filter press, sodium sulfate storage tank, boiling dryer, and organic calcium storage tank; The outlet of the aluminum sulfate storage tank and the first outlet of the water tank are respectively connected to the inlet pipeline of the stirring tank, the outlet of the stirring tank is connected to the inlet pipeline of the header tank, and the outlet of the header tank is connected to the inlet pipeline of the reactor; The outlet of the sodium hypophosphite storage tank and the second outlet of the water tank are respectively connected to the inlet pipeline of the reactor; The outlet of the organic calcium storage tank is connected to the inlet pipeline of the reactor; The outlet of the reactor is connected to the inlet pipeline of the filter press, the liquid phase outlet of the filter press is connected to the inlet pipeline of the sodium sulfate storage tank, and the solid phase outlet of the filter press is connected to the inlet pipeline of the boiling dryer.
2. The nano-scale encapsulated aluminum hypophosphite production system according to claim 1, It is characterized in that A water jacket is fixed on the outer wall of the reactor, and a water inlet and a water outlet are arranged on the water jacket.
3. The nano-scale encapsulated aluminum hypophosphite production system according to claim 2, It is characterized in that A circulation pipe is connected between the bottom and the top of the reactor, and a nano pump is installed on the circulation pipe.
4. The nano-scale encapsulated aluminum hypophosphite production system according to claim 3, It is characterized in that The reactor is provided with a thermometer.
5. The nano-scale encapsulated aluminum hypophosphite production system according to claim 4, It is characterized in that The outlet of the high-level tank is connected to the inlet pipeline of the reactor through a metering pump.