Polyester material melt extrusion continuous tackifying system

By introducing a filter box and a treatment device into the continuous tackifying system for melt extrusion of polyester material, the filtration and tackifying treatment of the melt are realized, and the problem of reducing purity caused by the unfiltered melt in the prior art is solved, and the improvement of the purity reduction caused by the melt is improved. The recycling efficiency of polyester materials.

CN222061160UActive Publication Date: 2024-11-26国望高科纤维(宿迁)有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420594844.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-26
Publication Date
2024-11-26
Estimated Expiration
2034-03-26

AI Technical Summary

Technical Problem

The existing polyester material melt extrusion continuous tackification system cannot achieve impurity screening without melt filtration, resulting in a decrease in melt purity during subsequent continuous tackification.

Method used

A polyester material melt extrusion continuous tackification system including a feed pipe, a first filter box, a second filter box and a treatment device is designed, and the melt filtration process is performed through the first filter plate and the second filter plate. A three-screw extruder and a static mixer are also installed in the processing device to realize the filtration and tackification of the melt.

Benefits of technology

Through melt filtration, the purity of the melt during subsequent tackification and discharge is significantly improved, ensuring efficient recycling of polyester materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222061160U_ABST
    Figure CN222061160U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of polyester material processing, in particular to a continuous tackifying system for polyester material melt extrusion. Comprising a feeding pipe and an auxiliary mechanism, the auxiliary mechanism comprises a first filtering box, a first filtering plate, a second filtering box, a second filtering plate, a discharging pipe and a processing device, the first filtering box is detachably connected with the feeding pipe, the first filtering plate is fixedly connected with the first filtering box, and the second filtering box is located on the side, away from the feeding pipe, of the first filtering box; the second filter plate is fixedly connected with the second filter box, the discharge pipe is detachably connected with the second filter box, the treatment device is arranged between the first filter box and the second filter box, an external double-screw extruder is used for melting, plasticizing and extruding raw materials, the raw materials are filtered by the first filter box and the first filter plate, and the raw materials are tackified by the treatment device. And finally, the melt is discharged from a discharging pipe after being filtered by a second filtering box and a second filtering plate, so that the melt can be filtered during use, and the purity of the melt during subsequent tackifying and discharging is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of polyester material processing, in particular to a polyester material melt extrusion continuous viscosity increasing system. Background Art

[0002] At present, when polyester waste is recycled, since it has undergone a high-temperature melt processing process, the polyester macromolecules will undergo a certain degree of hydrolysis or degradation, and its molecular weight and intrinsic viscosity will decrease to varying degrees. In order to make it reach the performance of the original new material, the polyester is often treated to increase its viscosity and molecular weight. Solid-phase viscosity enhancement and chain extension viscosity enhancement are commonly used methods.

[0003] Prior art CN215151684U discloses a polyester material melt extrusion continuous viscosity increasing system, including a twin-screw extruder, a static mixer, and a three-screw extruder connected in sequence. The twin-screw extruder and the three-screw extruder are both exhaust-type extruders, and the exhaust-type extruders are exhausted by vacuuming. The twin-screw extruder and the three-screw extruder are both provided with vacuum exhaust ports; the twin-screw extruder and the three-screw extruder are connected by an insulation pipe, and the static mixer is located on the insulation pipe; the insulation pipe is provided with a catalyst feeding point connected to the inside of the insulation pipe. In this utility model, a twin-screw extruder is used for melt plasticization extrusion, a static mixer is used to mix the melt with the added catalyst, and a three-screw extruder is used for vacuum devolatilization and melt viscosity increasing. The three-screw extruder is fully utilized to use the devolatilization characteristics of high vacuum exhaust and good exhaust effect, so that the small molecules such as the generated moisture can be quickly removed, and the polycondensation reaction is prompted to continue to proceed to the positive reaction. As the reaction proceeds, the molecular weight and intrinsic viscosity of the polyester will continue to increase.

[0004] However, in actual use of the above polyester material melt extrusion continuous viscosity increasing system, the melt is not filtered when it is fed, and impurities cannot be screened, which reduces the purity of the melt after subsequent continuous viscosity increasing. Utility Model Content

[0005] The purpose of the utility model is to provide a polyester material melt extrusion continuous viscosity increasing system, which can be used for melt filtering during use, so as to improve the purity of the melt during subsequent viscosity increasing and discharge.

[0006] To achieve the above-mentioned purpose, the technical solution adopted by the utility model is as follows: The utility model provides a polyester material melt extrusion continuous viscosity enhancement system, including a feed pipe and an auxiliary mechanism;

[0007] The auxiliary mechanism includes a first filter box, a first filter plate, a second filter box, a second filter plate, a discharge pipe and a processing device. The first filter box is detachably connected to the feed pipe and is located at the outlet side of the feed pipe. The first filter plate is fixedly connected to the first filter box and is located in the first filter box. The second filter box is located on the side of the first filter box away from the feed pipe. The second filter plate is fixedly connected to the second filter box and is located in the second filter box. The discharge pipe is detachably connected to the second filter box and is located at the outlet side of the second filter box. The processing device is arranged between the first filter box and the second filter box.

[0008] Wherein, the processing device includes a storage box, a three-screw extruder, a static mixer, a connecting component and an adding component, the storage box is located on the side of the first filter box close to the second filter box; the three-screw extruder is located on the side of the second filter box close to the storage box; the static mixer is located between the storage box and the three-screw extruder; the connecting component is respectively arranged on one side of the storage box, the three-screw extruder and the static mixer; the adding component is arranged on the side of the storage box close to the static mixer.

[0009] Wherein, the connecting assembly includes a first connecting pipe, a second connecting pipe, a third connecting pipe and a fourth connecting pipe, the first connecting pipe is detachably connected to the first filter box and the storage box respectively, and is located on the side of the first filter box close to the storage box; the second connecting pipe is detachably connected to the storage box and the static mixer respectively, and is located below the adding assembly; the third connecting pipe is detachably connected to the static mixer and the three-screw extruder respectively, and is located on the side of the static mixer close to the three-screw extruder; the fourth connecting pipe is detachably connected to the three-screw extruder and the second filter box respectively, and is located on the side of the three-screw extruder close to the second filter box.

[0010] Wherein, the adding component includes an adding connecting pipe and a hopper, the adding connecting pipe is fixedly connected to the second connecting pipe, communicated with the second connecting pipe, and located above the second connecting pipe; the hopper is fixedly connected to the adding connecting pipe and located on the top of the adding connecting pipe.

[0011] Wherein, the auxiliary mechanism further includes a top cover and an auxiliary block, wherein the top cover is detachably connected to the hopper and is located on the top of the hopper; the auxiliary block is fixedly connected to the top cover and is located on the top cover.

[0012] The utility model discloses a polyester material melt extrusion continuous viscosity increasing system, wherein a feed pipe inlet is connected with a twin-screw extruder discharge port, a first filter box is installed at the feed pipe outlet side, a first filter plate is installed in the first filter box, a second filter box is arranged at a side of the first filter box away from the feed pipe, the second filter plate is installed in the second filter box, a processing device is arranged between the first filter box and the second filter box, during processing, an external twin-screw extruder melts and plasticizes and extrude the raw material, after filtering treatment by the first filter box and the first filter plate, it is viscosity increasing treatment by the processing device, and finally after filtering treatment by the second filter box and the second filter plate, it is discharged through the discharge pipe, thereby realizing that melt filtering treatment can be carried out during use, which is beneficial to improving the purity of the melt during subsequent viscosity increasing and discharge. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] The present invention can be further described by the non-limiting embodiments given in the accompanying drawings.

[0014] Figure 1 This is a schematic diagram of the overall structure of the polyester material melt extrusion continuous viscosity increasing system according to the first embodiment of the utility model.

[0015] Figure 2 It is a cross-sectional view of the first filter box of the first embodiment of the utility model.

[0016] Figure 3 This is a schematic diagram of the overall structure of a polyester material melt extrusion continuous viscosity increasing system according to the second embodiment of the utility model.

[0017] In the figure: 101-feed pipe, 102-first filter box, 103-first filter plate, 104-second filter box, 105-second filter plate, 106-discharge pipe, 107-storage box, 108-three-screw extruder, 109-static mixer, 110-first connecting pipe, 111-second connecting pipe, 112-third connecting pipe, 113-fourth connecting pipe, 114-addition connecting pipe, 115-hopper, 201-top cover, 202-auxiliary block. DETAILED DESCRIPTION

[0018] In order to enable those skilled in the art to better understand the present invention, the technical solution of the present invention is further described below in conjunction with the accompanying drawings and embodiments.

[0019] Embodiment 1:

[0020] like Figure 1 and Figure 2 As shown, Figure 1 It is the overall structural diagram of the polyester material melt extrusion continuous viscosity increasing system. Figure 2It is a cross-sectional view of the first filter box 102. The utility model provides a polyester material melt extrusion continuous viscosity increasing system: including a feed pipe 101 and an auxiliary mechanism, the auxiliary mechanism includes a first filter box 102, a first filter plate 103, a second filter box 104, a second filter plate 105, a discharge pipe 106 and a processing device, the processing device includes a storage box 107, a three-screw extruder 108, a static mixer 109, a connection component and an addition component, the connection component includes a first connection pipe 110, a second connection pipe 111, a third connection pipe 112 and a fourth connection pipe 113, and the addition component includes an addition connection pipe 114 and a hopper 115. Through the above scheme, it can be achieved that melt filtering treatment can be carried out during use, which is conducive to improving the purity of the melt during subsequent viscosity increasing and discharge. It can be understood that the above scheme can carry out melt filtering treatment, which is conducive to improving the purity of the melt during subsequent viscosity increasing and discharge.

[0021] In this embodiment, the inlet side of the feed pipe 101 is communicated with the outlet of an external twin-screw extruder, and the outlet side is communicated with the inlet side of the first filter box 102 .

[0022] Among them, the first filter box 102 is detachably connected to the feed pipe 101 and is located at the outlet side of the feed pipe 101, the first filter plate 103 is fixedly connected to the first filter box 102 and is located in the first filter box 102, the second filter box 104 is located on the side of the first filter box 102 away from the feed pipe 101, the second filter plate 105 is fixedly connected to the second filter box 104 and is located in the second filter box 104, the discharge pipe 106 is detachably connected to the second filter box 104 and is located at the outlet side of the second filter box 104, and the processing device is arranged between the first filter box 102 and the second filter box 104. The inlet of the first filter box 102 is connected to the outlet flange of the feed pipe 101 by bolts, the first filter plate 103 is a metal mesh plate, which is installed in the first filter box 102 by bolts, the structure of the second filter box 104 is consistent with the first filter box 102, the second filter plate 105 is installed in the second filter box 104 by bolts, the second filter plate 105 is a metal mesh plate, and the filter hole diameter is smaller than the first filter plate 103, the discharge pipe 106 mounting flange is installed at the discharge port of the second filter box 104 by bolts, and the processing device is arranged between the first filter box 102 and the second filter box 104 for viscosity enhancement treatment.

[0023] Secondly, the storage box 107 is located on the side of the first filter box 102 close to the second filter box 104; the three-screw extruder 108 is located on the side of the second filter box 104 close to the storage box 107; the static mixer 109 is located between the storage box 107 and the three-screw extruder 108; the connecting components are respectively arranged on one side of the storage box 107, the three-screw extruder 108 and the static mixer 109; the adding component is arranged on the side of the storage box 107 close to the static mixer 109. The storage box 107 is used for melt storage, the three-screw extruder 108 adopts a multi-stage vacuum exhaust structure, a vacuum exhaust port is set on the top, and the internal screw adopts a shallow screw groove and a large pitch screw structure, which is conducive to forming a larger melt film surface during the extrusion process of the three-screw extruder 108, and is convenient for the melt devolatilization and viscosity-increasing reaction. Since the melt is pushed forward by the three-screw extruder 108, the polycondensation reaction continues to proceed in the positive reaction direction, thereby increasing the molecular weight of the polyester, the viscosity of the polyester melt is also increased, and the resistance of the screw extrusion becomes larger. Further, the high shear effect of the three-screw extruder 108 can also effectively reduce and alleviate the viscosity increase problem caused by the increase in molecular weight during the extrusion of the polyester melt. The static mixer 109 is used for mixing the melt and the catalyst. The connecting components are respectively arranged on one side of the storage box 107, the three-screw extruder 108 and the static mixer 109, and are used to cooperate to form a feeding system. The adding component is arranged on the side of the storage box 107 close to the static mixer 109, and is used for catalyst addition.

[0024] Then, the first connecting pipe 110 is detachably connected to the first filter box 102 and the storage box 107 respectively, and is located on the side of the first filter box 102 close to the storage box 107; the second connecting pipe 111 is detachably connected to the storage box 107 and the static mixer 109 respectively, and is located below the adding component; the third connecting pipe 112 is detachably connected to the static mixer 109 and the three-screw extruder 108 respectively, and is located on the side of the static mixer 109 close to the three-screw extruder 108; the fourth connecting pipe 113 is detachably connected to the three-screw extruder 108 and the second filter box 104 respectively, and is located on the side of the three-screw extruder 108 close to the second filter box 104. One end of the first connecting pipe 110 is connected to the outlet side of the first filter box 102 by bolts, and the other end is connected to the inlet side of the storage box 107 by bolts. One end of the second connecting pipe 111 is connected to the outlet side of the storage box 107 by bolts, and the other end is connected to the inlet side of the static mixer 109 by bolts. One end of the third connecting pipe 112 is connected to the outlet side of the static mixer 109 by bolts, and the other end is connected to the inlet side of the three-screw extruder 108 by bolts. One end of the fourth connecting pipe 113 is connected to the outlet side of the three-screw extruder 108 by bolts, and the other end is installed on the inlet side of the second filter box 104 by bolts.

[0025] Finally, the addition connecting pipe 114 is fixedly connected to the second connecting pipe 111, communicates with the second connecting pipe 111, and is located above the second connecting pipe 111; the hopper 115 is fixedly connected to the addition connecting pipe 114 and is located on the top of the addition connecting pipe 114. The addition connecting pipe 114 is welded to the second connecting pipe 111 and has a control valve. The bottom of the hopper 115 is a tapered structure, in which the catalyst is stored, and is connected to the mounting plate on the top of the addition connecting pipe 114 by bolts.

[0026] When the utility model is used for melt filtration treatment, it is beneficial to improve the purity of the melt during subsequent viscosity increase and discharge. During processing, first, the external twin-screw extruder melts and plasticizes the raw material and extrude it. Then, the melt enters the first filter box 102 through the feed pipe 101, and is filtered and treated by the first filter plate 103. After removing impurities, the melt enters the storage box 107 through the first connecting pipe 110, and is stored in the storage box 107. Then, it can enter the static mixer 109 through the second connecting pipe 111. At this time, the catalyst can be added by opening the valve on the adding connecting pipe 114. The melt and the catalyst are mixed in the static mixer 109, and then enter the three-screw extruder 1 through the third connecting pipe 112. 08. The three-screw extruder 108 adopts a multi-stage vacuum exhaust structure, a vacuum exhaust port is arranged on the top, and the internal screw adopts a shallow screw groove and a large pitch thread structure, which is conducive to forming a larger melt film surface during the extrusion process of the three-screw extruder 108, and is convenient for the melt devolatilization and viscosity-increasing reaction. Since the melt is pushed forward by the three-screw extruder 108, the polycondensation reaction continues to proceed in the positive reaction direction, thereby increasing the molecular weight of the polyester and the viscosity of the polyester melt. Then, the melt enters the second filter box 104 through the fourth connecting pipe 113, and after being filtered by the second filter plate 105, it is discharged through the discharge pipe 106, so that the melt can be filtered during use, which is conducive to improving the purity of the melt during subsequent viscosity increase and discharge.

[0027] Embodiment 2:

[0028] like Figure 3 As shown, Figure 3 It is a schematic diagram of the overall structure of a polyester material melt extrusion continuous viscosity increasing system. On the basis of the first embodiment, the utility model provides a polyester material melt extrusion continuous viscosity increasing system, and the auxiliary mechanism further includes a top cover 201 and an auxiliary block 202.

[0029] The top cover 201 is detachably connected to the hopper 115 and is located on the top of the hopper 115; the auxiliary block 202 is fixedly connected to the top cover 201 and is located on the top cover 201. The top cover 201 can be directly buckled on the top of the hopper 115, and the auxiliary block 202 has a T-shaped cross section and is mounted on the top cover 201 by bolts.

[0030] In this embodiment, the top cover 201 can be provided to protect the top of the hopper 115 to prevent impurities from falling into the catalyst, and the auxiliary block 202 can be provided to facilitate installation and removal of the top cover 201.

[0031] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the technology may modify or change the above embodiments without violating the spirit and scope of the present invention. Therefore, all equivalent modifications or changes made by those with ordinary knowledge in the relevant technical field without departing from the spirit and technical ideas disclosed in the present invention shall still be covered by the claims of the present invention.

Claims

1. A polyester material melt extrusion continuous viscosity increasing system, comprising a feed pipe, It is characterized in that It also includes auxiliary institutions; The auxiliary mechanism includes a first filter box, a first filter plate, a second filter box, a second filter plate, a discharge pipe and a processing device. The first filter box is detachably connected to the feed pipe and is located at the outlet side of the feed pipe. The first filter plate is fixedly connected to the first filter box and is located in the first filter box. The second filter box is located on the side of the first filter box away from the feed pipe. The second filter plate is fixedly connected to the second filter box and is located in the second filter box. The discharge pipe is detachably connected to the second filter box and is located at the outlet side of the second filter box. The processing device is arranged between the first filter box and the second filter box.

2. The polyester material melt extrusion continuous viscosity increasing system according to claim 1, It is characterized in that The processing device includes a storage box, a three-screw extruder, a static mixer, a connecting component and an adding component. The storage box is located on the side of the first filter box close to the second filter box; the three-screw extruder is located on the side of the second filter box close to the storage box; the static mixer is located between the storage box and the three-screw extruder; the connecting component is respectively arranged on one side of the storage box, the three-screw extruder and the static mixer; the adding component is arranged on the side of the storage box close to the static mixer.

3. The polyester material melt extrusion continuous viscosity increasing system as claimed in claim 2, It is characterized in that The connecting assembly includes a first connecting pipe, a second connecting pipe, a third connecting pipe and a fourth connecting pipe, the first connecting pipe being detachably connected to the first filter box and the storage box respectively, and being located on a side of the first filter box close to the storage box; the second connecting pipe being detachably connected to the storage box and the static mixer respectively, and being located below the adding assembly; the third connecting pipe being detachably connected to the static mixer and the three-screw extruder respectively, and being located on a side of the static mixer close to the three-screw extruder; the fourth connecting pipe being detachably connected to the three-screw extruder and the second filter box respectively, and being located on a side of the three-screw extruder close to the second filter box.

4. The polyester material melt extrusion continuous viscosity increasing system as claimed in claim 3, It is characterized in that The adding component includes an adding connecting pipe and a hopper. The adding connecting pipe is fixedly connected to the second connecting pipe, communicates with the second connecting pipe, and is located above the second connecting pipe. The hopper is fixedly connected to the adding connecting pipe and is located on the top of the adding connecting pipe.

5. The polyester material melt extrusion continuous viscosity increasing system as claimed in claim 4, It is characterized in that The auxiliary mechanism also includes a top cover and an auxiliary block. The top cover is detachably connected to the hopper and is located on the top of the hopper; the auxiliary block is fixedly connected to the top cover and is located on the top cover.