Perforated PFA film for composite material

By installing corrosion-resistant layers and opening holes on the perforated PFA film, the problem of insufficient corrosion resistance to chemicals is solved, significantly extending the service life and reducing the risk of leakage, while improving breathability and permeability.

CN222099840UActive Publication Date: 2024-12-03SUZHOU QIANMI TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420687923.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-07
Publication Date
2024-12-03
Estimated Expiration
2034-04-07

AI Technical Summary

Technical Problem

Existing hole-punched PFA films used in composite materials have poor corrosion resistance to chemical substances, resulting in damage, corrosion, shortened service life and potential risk of chemical substance leakage on the material surface.

Method used

Corrosion-resistant layers are installed on both sides of the perforated PFA film, including nickel metal coating, fluoropolymer protective coating and ceramic laminate coating, and evenly distributed holes are opened on both sides of the film.

Benefits of technology

It effectively enhances the corrosion resistance of perforated PFA films, extends service life, reduces maintenance and repair costs, reduces the risk of chemical leakage, improves breathability and permeability, and ensures material integrity and performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222099840U_ABST
    Figure CN222099840U_ABST
Patent Text Reader

Abstract

The utility model discloses a perforated PFA (Polyfluoroalkoxy) film for a composite material, which relates to the technical field of composite material processing and comprises a perforated PFA film main body, corrosion-resistant layers are fixedly mounted on two sides of the perforated PFA film main body, and each corrosion-resistant layer comprises a metal coating, a protective coating and a laminated coating. The metal coating is arranged on the surface of the perforated PFA film main body. According to the perforated PFA thin film for the composite material, through the arrangement of the corrosion-resistant layer, the corrosion resistance of the perforated PFA thin film to chemical substances can be effectively enhanced, the service life of the composite material is prolonged, the integrity and performance of the perforated PFA thin film can be kept, frequent downtime for maintenance or replacement is not needed, and the service life of the composite material is prolonged. Therefore, the continuity and the working efficiency of the production process are improved, the cost required by maintenance and repair can be effectively reduced, the leakage of chemical substances can be effectively blocked, and the pollution risk to the environment is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of composite material processing, and in particular relates to a perforated PFA film used for composite materials. Background Art

[0002] Perforated PFA film is a film material made of polytetrafluoroethylene and perfluoropropylene copolymer. It has excellent chemical stability, high temperature resistance and electrical insulation properties. It is often used in the field of composite materials for isolation, filtration and protection. By introducing perforated PFA film into composite materials, the air permeability of the material can be controlled, and it can also be used to control the liquid permeability of the composite material.

[0003] The perforated PFA film currently used in composite materials has poor corrosion resistance to chemicals, resulting in the inability of the perforated PFA film to effectively resist the erosion of chemicals, causing damage or corrosion to the surface of the material, thereby causing material failure and affecting its performance and function. At the same time, as a part of the composite material, if the PFA film cannot effectively resist the erosion of chemicals, there may be a risk of chemical leakage, causing environmental pollution and safety hazards, and may also shorten its service life, requiring more frequent replacement or maintenance, increasing costs and workload. Utility Model Content

[0004] The technical problem to be solved by the utility model is that the existing perforated PFA film used for composite materials has poor corrosion resistance to chemical substances.

[0005] The technical solution adopted by the utility model to solve its technical problems is: a perforated PFA film for composite materials, including a perforated PFA film body, both sides of the perforated PFA film body are fixedly installed with corrosion-resistant layers, the corrosion-resistant layers include a metal coating, a protective coating and a laminated coating, the metal coating is arranged on the surface of the perforated PFA film body, the protective coating is arranged on the surface of the metal coating on a side away from the perforated PFA film body, and the laminated coating is arranged on the surface of the protective coating on a side away from the metal coating.

[0006] As a preferred embodiment of the present invention, holes are formed on both sides of the perforated PFA film body.

[0007] As a preferred embodiment of the present invention, the holes are circular and are evenly distributed on both sides of the perforated PFA film body.

[0008] As a preferred embodiment of the present invention, the metal coating is nickel metal plated on the surface of the perforated PFA film body.

[0009] As a preferred embodiment of the present invention, the protective coating is a fluoropolymer coated on the surface of the metal coating.

[0010] As a preferred embodiment of the present invention, the laminated coating is a ceramic coated on the surface of the protective coating.

[0011] The beneficial effects of the utility model are:

[0012] 1. The perforated PFA film for composite materials can effectively enhance the corrosion resistance of the perforated PFA film to chemical substances by setting a corrosion-resistant layer, thereby reducing damage and corrosion on the surface of the material and extending the service life of the composite material. The perforated PFA film can also maintain its integrity and performance without frequent downtime for repair or replacement, thereby improving the continuity and work efficiency of the production process, and effectively reducing the cost required for maintenance and repair. It can also effectively block the leakage of chemical substances, reduce the risk of pollution to the environment, and also reduce the safety hazards caused by leakage.

[0013] 2. The perforated PFA film for composite materials can increase the air permeability and permeability of the perforated PFA film body by opening holes. The evenly distributed holes can provide uniform air permeability, allowing gas or liquid to pass more evenly on the surface of the film, which helps to maintain uniform flow and distribution of gas or liquid and avoid local pressure changes. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a schematic diagram of the overall structure provided by an embodiment of the utility model;

[0015] Figure 2 It is a top view of the overall structure provided by the embodiment of the utility model;

[0016] Figure 3 It is an exploded view of the overall structure provided by the embodiment of the utility model;

[0017] Figure 4 It is an exploded view of the corrosion-resistant layer structure provided by an embodiment of the utility model.

[0018] Markings in the figure: 1. Perforated PFA film body; 2. Corrosion-resistant layer; 201. Metal coating; 202. Protective coating; 203. Laminated coating; 3. Holes. DETAILED DESCRIPTION

[0019] The present invention will now be further described in detail in conjunction with the accompanying drawings and preferred embodiments. These drawings are simplified schematic diagrams that only illustrate the basic structure of the present invention in a schematic manner, and therefore only show the components related to the present invention.

[0020] like Figures 1 to 4As shown, the utility model provides a perforated PFA film for a composite material, including a perforated PFA film body 1, both sides of the perforated PFA film body 1 are fixedly installed with a corrosion-resistant layer 2, the corrosion-resistant layer 2 includes a metal coating 201, a protective coating 202 and a laminated coating 203, the metal coating 201 is arranged on the surface of the perforated PFA film body 1, the protective coating 202 is arranged on the surface of the metal coating 201 away from the perforated PFA film body 1, and the laminated coating 203 is arranged on the surface of the protective coating 202 away from the metal coating 201.

[0021] refer to Figure 3 Holes 3 are provided on both sides of the perforated PFA film body 1 . The holes 3 are circular and evenly distributed on both sides of the perforated PFA film body 1 .

[0022] By adopting the above scheme: the air permeability and permeability of the perforated PFA film body 1 can be increased by opening the holes 3, and the evenly distributed holes 3 can provide uniform air permeability, so that the gas or liquid passes through the surface of the film more evenly, which helps to maintain uniform flow and distribution of the gas or liquid and avoid local pressure changes.

[0023] refer to Figures 1 to 4 The metal coating 201 is nickel metal plated on the surface of the perforated PFA film body 1 , the protective coating 202 is a fluoropolymer coated on the surface of the metal coating 201 , and the laminated coating 203 is a ceramic coated on the surface of the protective coating 202 .

[0024] The above scheme is adopted: by plating nickel metal on the surface of the perforated PFA film body 1, it can provide excellent corrosion resistance, effectively protect the substrate from corrosion and oxidation, and increase the hardness and mechanical strength of the film. By coating the fluoropolymer on the surface of the metal coating 201, it can resist the erosion of various acids, alkalis, solvents and other chemical substances, which enables the metal coating 201 and the perforated PFA film body 1 to obtain better protection in harsh chemical environments and extend the service life. At the same time, the fluoropolymer coating also has excellent high temperature resistance and can maintain stability in high temperature environments. By coating the ceramic on the surface of the protective coating 202, the hardness of the surface of the perforated PFA film body 1 can be increased, and its ability to resist scratches, scratches and punctures can be improved, and its quality and stability can be improved. At the same time, the ceramic coating has good anti-adhesion properties, making it difficult for dirt, grease and other substances to adhere to the surface of the perforated PFA film body 1.

[0025] Working principle:

[0026] When in use, the nickel metal plated on the surface of the perforated PFA film body 1 provides excellent corrosion resistance, protects the substrate from corrosion and oxidation, and can increase the hardness and mechanical strength of the film. The fluoropolymer coated on the surface of the metal coating 201 resists erosion by various acids, alkalis, solvents and other chemical substances, which enables the metal coating 201 and the perforated PFA film body 1 to obtain better protection in harsh chemical environments and extend the service life. At the same time, the fluoropolymer coating also has excellent high temperature resistance and can maintain stability in high temperature environments. The ceramic coated on the surface of the protective coating 202 increases the hardness of the surface of the perforated PFA film body 1, improves its ability to resist scratches, scratches and punctures, and improves its quality and stability. At the same time, the ceramic coating has good anti-adhesion properties, making it difficult for dirt, grease and other substances to adhere to the surface of the perforated PFA film body 1.

[0027] To sum up: this perforated PFA film for composite materials, through the setting of the corrosion-resistant layer 2, can effectively enhance the corrosion resistance of the perforated PFA film to chemical substances, thereby reducing damage and corrosion on the surface of the material, extending the service life of the composite material, and can also enable the perforated PFA film to maintain its integrity and performance, without the need for frequent downtime for repair or replacement, thereby improving the continuity and work efficiency of the production process, and at the same time can effectively reduce the cost required for maintenance and repair, and can also effectively block the leakage of chemical substances, reduce the risk of pollution to the environment, and also reduce the safety hazards caused by leakage.

[0028] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device that includes a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device;

[0029] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and the scope of the present invention is defined by the appended claims and their equivalents;

[0030] The above description only describes the specific implementation methods of the utility model. Various examples do not limit the essential content of the utility model. Ordinary technicians in the relevant technical field can modify or deform the specific implementation methods described above after reading the description without departing from the essence and scope of the utility model.

Claims

1. A perforated PFA film for composite materials, comprising a perforated PFA film body (1), characterized in that: A corrosion-resistant layer (2) is fixedly installed on both sides of the perforated PFA film body (1), and the corrosion-resistant layer (2) includes a metal coating (201), a protective coating (202) and a laminated coating (203). The metal coating (201) is arranged on the surface of the perforated PFA film body (1), the protective coating (202) is arranged on the surface of the metal coating (201) away from the perforated PFA film body (1), and the laminated coating (203) is arranged on the surface of the protective coating (202) away from the metal coating (201).

2. A perforated PFA film for composite materials according to claim 1, characterized in that: Holes (3) are provided on both sides of the perforated PFA film body (1).

3. A perforated PFA film for composite materials according to claim 2, characterized in that: The holes (3) are circular and are evenly distributed on both sides of the perforated PFA film body (1).

4. A perforated PFA film for composite materials according to claim 1, characterized in that: The metal coating (201) is nickel metal plated on the surface of the perforated PFA film body (1).

5. A perforated PFA film for composite materials according to claim 1, characterized in that: The protective coating (202) is a fluoropolymer coated on the surface of the metal coating (201).

6. A perforated PFA film for composite materials according to claim 1, characterized in that: The stacked coating (203) is a ceramic coated on the surface of the protective coating (202).