Suspended particle dimming device

By adopting a multi-layer frame body structure and supporting particle distribution in the suspended particle dimming device, the problem of changes in thickness and high driving voltage when the device is bent is solved, and the support performance and molding uniformity of the device are improved.

CN222105784UActive Publication Date: 2024-12-03TD ELECTROOPTIC FILMS (TDEF) INC
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420884817.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-26
Publication Date
2024-12-03
Estimated Expiration
2034-04-26

AI Technical Summary

Technical Problem

The existing suspended particle dimming devices have a problem of changing thickness or flowing when bending, high driving voltage, weak adhesion and uneven molding.

Method used

Using multi-layer frame body structure and supporting particle distribution, the dimming material is fixed by supporting particles, the structural support performance is improved, and the adhesion of the conductive base layer is improved. UV curing or thermosetting adhesives and epoxy resins are used. The adhesive forms the frame sealing body to ensure that the dimming material and the uncured adhesive are not soluble.

Benefits of technology

It effectively avoids the thickness changes and flow of the dimming layer when bending, reduces the driving voltage, improves the molding uniformity and adhesion of the device, and solves the problems of high voltage and uneven molding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222105784U_ABST
    Figure CN222105784U_ABST
Patent Text Reader

Abstract

The utility model provides a suspended particle dimming device which comprises a first conductive base layer, a dimming layer and a second conductive base layer which are sequentially stacked, and the dimming layer comprises at least two layers of frame sealing bodies which are sequentially nested. A containing cavity is formed among the first conductive base layer, the second conductive base layer and the sealing frame body located on the inner layer, the containing cavity is filled with dimming materials, and a plurality of evenly-distributed supporting particles are arranged in at least one layer of sealing frame body. According to the utility model, the problems of large voltage, poor supporting performance, low binding power and non-uniform device molding of the existing flexible dimming device are solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of dimming, and relates to a suspended particle dimming device. Background Art

[0002] Since the development of suspended particle dimming technology (SPD), its formula and device preparation process have been very mature. At present, SPD dimming devices are mainly composed of a first transparent conductive layer, an SPD dimming layer and a second transparent conductive layer. The SPD dimming layer mainly adopts a three-phase separation process, that is, through the principle of incompatibility between silicone and dispersion liquid and nanoparticles, emulsification and photopolymerization are used to form a solid composite layer with silicone as a support, dispersion liquid and nanoparticles as the color-changing body. Such as the document J.Mater.Chem.A, 2018, 6, 24157-24165, patents CN219574554U, US6900923B2, etc.

[0003] Since the film-forming process of SPD is a three-phase separation, solving the effective separation of the three phases while ensuring the mechanical properties of the film has become a key problem in the industrial production of SPD dimming film. Although this process has great advantages in continuous roll-to-roll production, storage and transportation, cutting into any shape, and lightweight devices, silicone has defects in water and oxygen barrier. Water vapor and oxygen can easily enter the structure, resulting in hidden dangers in the stability of the device. In addition, since the SPD dimming device is a capacitor structure device in principle, silicone, as a system support, not only has weak adhesion to the substrate, but also easily produces current shunt, causing the driving voltage of the device to be very large (usually 110V to 220V), far exceeding the safe voltage.

[0004] At present, the most convenient way to solve the driving voltage is to avoid current sharing, that is, to make all electric fields effectively act on the polarization and rotation of the nanoparticles in the SPD. Therefore, removing the silicone support in the bulk phase or increasing the effective resistance of the silicone support is an effective means to reduce the SPD dimming driving voltage. It can be found from liquid crystal devices that the voltage required for PDLC (polymer dispersed liquid crystal) devices with polymer support structures is significantly higher than that of liquid crystal devices without polymer support in the bulk phase. Therefore, simplifying the original coating process of SPD to a device structure constructed by frame glue will effectively reduce the driving voltage required for the device.

[0005] However, although SPD dimming films have been developed for decades, they still have many defects. For example, the SPD flexible device using traditional methods with silicone as the support does not have sufficient adhesion support between its dimming layer and the transparent conductive substrate, resulting in the prepared dimming film being damaged due to stress generated by bending, folding, collision, etc. Improved methods such as patents CN111100299A and US7791788, etc., but the effect is not obvious.

[0006] In addition, the presence of silicone supports will spread the current, causing the driving voltage required for the device to be very high, far exceeding the safe operating voltage, which seriously limits the application of the device. Although the use of traditional spacers to make devices can solve the problem of high driving voltage, the existing methods are more suitable for preparing rigid devices. The use of sticky spacers is a common solution for liquid crystal displays (such as patent KR101107696B1), but the use of such spacers is mainly based on the process of melting and bonding of the surface glue at high temperatures, which makes the device prone to defects. In addition, this method is limited by the characteristics of the surface glue of the spacer, has low universality, and is expensive, and cannot be used on a large scale. Utility Model Content

[0007] In view of the shortcomings of the prior art, the purpose of the utility model is to provide a suspended particle dimming device with a better supporting structure to avoid thickness changes or flow of the dimming material when bending, thereby solving the problems of high voltage, low adhesion and uneven device molding of the existing flexible dimming devices.

[0008] To achieve this purpose, the utility model adopts the following technical solutions:

[0009] The utility model provides a suspended particle dimming device, which comprises a first conductive base layer, a dimming layer and a second conductive base layer which are stacked in sequence, the dimming layer comprises at least two layers of sealing frame bodies which are nested in sequence, a receiving cavity is formed between the first conductive base layer, the second conductive base layer and the sealing frame body located in the inner layer, the receiving cavity is filled with a dimming material, and a plurality of supporting particles uniformly distributed are arranged inside at least one layer of the sealing frame body.

[0010] The suspended particle dimming device provided by the utility model has a dimming layer with supporting particles distributed inside, thereby improving the structural support performance of the device. Even when bent, the thickness of the dimming layer will not change and will not flow. At the same time, a multi-layer sealing frame body structure is adopted. On the one hand, it prevents the organic small molecules in the dimming material from contacting with the uncured adhesive and dissolving each other, causing the adhesive to fail. On the other hand, it can also improve the bonding strength with the conductive base layers on both sides, thereby making the device uniformly molded.

[0011] It should be noted that the accommodating cavity described in the present invention refers to the enclosed space formed between the surrounding space of the innermost sealing frame body and the first conductive base layer and the second conductive base layer on its upper and lower sides; the interior of the sealing frame body refers to the internal space of the sealing frame body itself.

[0012] As a preferred technical solution of the utility model, at least two layers of the sealing frame body include a first sealing frame body and at least one layer of a second sealing frame body sleeved on the outside of the first sealing frame body, the accommodating cavity is formed between the first sealing frame body, the first conductive base layer and the second conductive base layer, and the supporting particles are arranged inside at least the first sealing frame body.

[0013] In the utility model, the first sealing frame can block the diffusion of small molecules of the dimming material to prevent them from contacting and dissolving with uncured non-silicone adhesive, and the second sealing frame can adhere firmly to the first conductive base layer and the second conductive base layer on both sides to improve the bonding force of the device.

[0014] The material of the first sealing frame includes UV curing silicone adhesive, thermosetting silicone adhesive, moisture curing silicone adhesive, and UV heating hybrid silicone adhesive. The material of the second sealing frame includes epoxy resin thermosetting adhesive, acrylic light curing adhesive, or UV heating hybrid adhesive. It should be noted that all of the above adhesives are commercially available materials well known to those skilled in the art.

[0015] As a preferred technical solution of the utility model, the supporting particles are evenly distributed in the containing cavity.

[0016] As a preferred technical solution of the utility model, the distribution density of the supporting particles is 1 to 100 particles / mm 2 , for example, 1 particle / mm 2 , 3 pieces / mm 2 , 5 / mm 2 , 8 / mm 2 , 10 / mm 2 , 20 / mm 2 , 30 / mm 2 , 40 / mm 2 , 50 / mm 2 , 60 pieces / mm 2 , 70 pieces / mm 2 , 80 pcs / mm 2 , 90 particles / mm 2 , 95 pieces / mm 2 or 100 pcs / mm 2 , but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0017] It should be noted that in the present invention, the distribution density of the supporting particles is calculated based on the bottom surface of the accommodating cavity.

[0018] The diameter of the supporting particles is 2 to 100 μm, for example, 2 μm, 5 μm, 10 μm, 20 μm, 30 μm, 40 μm, 50 μm, 55 μm, 60 μm, 65 μm, 70 μm, 80 μm, 90 μm or 100 μm, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0019] Preferably, the material of the supporting particles can be selected from polymer resins, glass fibers or inorganic materials well known to those skilled in the art.

[0020] As a preferred technical solution of the utility model, the shape of the supporting particles includes spherical, cylindrical or cubic.

[0021] The color of the supporting particles is colorless, gray, red, green, white or black.

[0022] As a preferred technical solution of the utility model, the dimming layer is a flexible dimming layer, and the dimming material is a liquid material or a gel material.

[0023] The utility model uses supporting particles to evenly fix the liquid or gel dimming material between the first conductive base layer and the second conductive base layer, thereby obtaining a flexible dimming layer. The dimming material can be any one of SDP suspension, SPD suspension gel, liquid crystal composition or electrochromic gel known to those skilled in the art, or a combination of at least two thereof.

[0024] As a preferred technical solution of the utility model, at least one fixed coating layer is further arranged between the first conductive base layer and the dimming layer, and / or between the second conductive base layer and the dimming layer.

[0025] The present invention can fix the supporting particles more evenly by setting a fixed coating, so that the dimming material is evenly distributed between the first conductive base layer and the second conductive base layer. The present invention provides the following three solutions based on different settings of the fixed coating: (1) The suspended particle dimming device is composed of a first conductive base layer, a fixed coating, a dimming layer and a second conductive base layer stacked in sequence; (2) The suspended particle dimming device is composed of a first conductive base layer, a dimming layer, a fixed coating and a second conductive base layer stacked in sequence; (3) The suspended particle dimming device is composed of a first conductive base layer, a fixed coating, a dimming layer, a fixed coating and a second conductive base layer stacked in sequence.

[0026] Preferably, the thickness of the fixed coating is 0.005 to 30 μm, for example, 0.005 μm, 0.01 μm, 0.05 μm, 0.1 μm, 0.2 μm, 0.5 μm, 1 μm, 2 μm, 3 μm, 4 μm, 5 μm, 6 μm, 7 μm, 8 μm, 9 μm, 10 μm, 15 μm, 18 μm, 20 μm, 25 μm or 30 μm, but is not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0027] Preferably, the fixing coating comprises an organic silicone layer, an acrylic resin layer, a polyurethane resin layer or an epoxy resin layer.

[0028] As a preferred technical solution of the utility model, the first conductive base layer includes a first substrate, and a first conductive film is arranged on a surface of the first substrate close to the dimming layer; the second conductive base layer includes a second substrate, and a second conductive film is arranged on a surface of the second substrate close to the dimming layer.

[0029] That is, the suspended particle dimming device of the present invention is composed of a first substrate, a first conductive film, a dimming layer, a second conductive film and a second substrate which are stacked in sequence.

[0030] As a preferred technical solution of the present invention, the thickness of the first conductive film and the second conductive film are independently 50 to 500 μm, for example, 50 μm, 60 μm, 80 μm, 100 μm, 110 μm, 120 μm, 125 μm, 130 μm, 150 μm, 180 μm, 200 μm, 240 μm, 250 μm, 300 μm, 350 μm, 400 μm, 450 μm or 500 μm, but are not limited to the listed values, and other unlisted values ​​within the numerical range are also applicable.

[0031] As a preferred technical solution of the present invention, the first substrate and the second substrate are independently transparent substrates.

[0032] Exemplarily, the utility model provides a method for preparing the suspended particle dimming device, which includes: wet spraying supporting particles on the surface of the first conductive base layer and / or the second conductive base layer, and after making at least two layers of sealing frame bodies, filling dimming materials to form a dimming layer, and after curing the sealing frame body, obtaining the suspended particle dimming device.

[0033] Specifically, the wet spraying includes: after the supporting particles and the solvent are mixed, they are added to the feeding chamber of the powder spraying device, and the surface of the first conductive base layer or the second conductive base layer is sprayed by circulating feeding. The utility model first mixes the supporting particles and the solvent in a certain proportion as required, adds them to the feeding chamber of the powder spraying device, then turns on the heating, stirring and circulation functions of the equipment, sets the powder spraying time and the sedimentation time, and after the temperature in the cavity of the equipment rises to the set value, the first conductive base layer and / or the second conductive base layer is placed in the cavity of the powder spraying device for powder spraying. The feeding chamber needs to adopt the method of continuous stirring and circulating feeding, the purpose of which is to ensure that the supporting particles and the solvent are mixed evenly, which is conducive to achieving uniform distribution of supporting particles in the later stage. The purpose of heating is to partially volatilize the solvent after it is sprayed out. The temperature setting range depends on the volatility characteristics of the wet spraying solvent. The density of the powder spraying can also be controlled by adjusting the setting of the powder spraying time and the sedimentation time.

[0034] Specifically, the method for manufacturing the sealing frame body includes: using an adhesive material to sequentially form at least two layers of the sealing frame body on the surface of the first conductive base layer or the second conductive base layer sprayed with supporting particles, and performing a curing process.

[0035] Specifically, the dimming material is filled by vacuum infusion method or dripping vacuum bonding method. That is, the utility model provides the following two solutions for filling the dimming material, specifically including:

[0036] Option 1: Vacuum infusion method

[0037] S1: wet-spraying supporting particles on the surface of the first conductive base layer to obtain an intermediate;

[0038] S2: making at least two layers of sealing frame bodies on the side of the intermediate body sprayed with supporting particles, the sealing frame body being provided with a material injection port, and then laminating the second conductive base layer and performing a curing treatment to obtain an empty box structure with a receiving cavity;

[0039] S3: placing the dimming material and the empty box structure at different positions in the crystal filling device, and evacuating the device, then bringing the dimming material into contact with the empty box structure, and gradually releasing the pressure so that the dimming material is poured into the containing cavity to obtain a suspended particle dimming device.

[0040] Solution 2: Instillation vacuum lamination

[0041] S01: wet-spraying supporting particles on the surface of the first conductive base layer to obtain an intermediate;

[0042] S02: making at least two layers of sealing frame bodies on one side of the intermediate body sprayed with supporting particles, wherein the sealing frame bodies are fully enclosed, and uniformly dripping dimming materials into the space surrounded by the sealing frame bodies located on the inner side to obtain a filling box structure;

[0043] S03: Move the potting structure and the second conductive base layer into the vacuum chamber, adsorb them in the equipment through vacuum, and evacuate the equipment so that the second conductive base layer fits the potting structure, and then perform a curing process on the sealing frame body to obtain a suspended particle dimming device.

[0044] It should be noted that the present invention does not impose any specific limitation or special requirements on the selection and type of dimming materials, and any suspension that can be used for dimming devices and is well known to those skilled in the art can be used.

[0045] Preferably, the preparation method further comprises: before the wet spraying, coating a primer on the surface of the first conductive base layer and / or the second conductive base layer, and performing a drying treatment to form a fixed coating.

[0046] Taking thermally-inherent organic silicone as an example, the coating method of the bottom glue in the utility model can be a micro-concave roller coating method, a slit extrusion coating method, a spraying method, or a micro-concave roller coating method. According to the target thickness, different micro-concave roller meshes and solid contents are selected to obtain a thinner and more uniform coating thickness. Among them, slit extrusion coating can adjust different solid contents, flow rates, and line speeds to obtain different target thicknesses. The drying treatment temperature can be set according to the actual amount of glue and the actual curing requirements. After the drying treatment is completed, PET (polyethylene glycol terephthalate) or fluorine release film can be selected for lamination protection according to the adhesion of the fixed coating.

[0047] In addition, epoxy resin heat-curing adhesive, polyurethane resin, acrylic and other light-curing adhesives can all be prepared by the above coating method. The difference is that glues of different properties have different curing methods. Light-curing adhesives need to be first heated in an oven to evaporate the solvent and then cured by UV lamp.

[0048] The suspended particle dimming device provided by the utility model is suitable for flat glass or curved glass. By arranging a supporting particle structure inside the dimming layer, the supporting performance of the device is improved. The thickness will not change when bending, and no flow will occur. Therefore, it can be effectively applied to flat glass or curved glass, such as automobile sunroofs, side windows, and various types of architectural glass.

[0049] The numerical range described in the present invention not only includes the point values ​​listed above, but also includes any point values ​​between the above numerical ranges that are not listed. Due to space limitations and for the sake of simplicity, the present invention no longer exhaustively lists the specific point values ​​included in the range.

[0050] Compared with the prior art, the beneficial effects of the utility model are:

[0051] The utility model provides a suspended particle dimming device. The structural support performance of the device is improved by distributing supporting particles inside the dimming layer. Even when bent, the thickness of the dimming layer will not change and will not flow. At the same time, a multi-layer sealing frame body structure is adopted. On the one hand, it avoids the organic small molecules in the dimming material from contacting with the uncured adhesive and dissolving each other, causing the adhesive to fail. On the other hand, it can also improve the bonding force with the conductive base layers on both sides, solving the problems of high voltage, low bonding force, single preparation method and uneven device molding in the existing flexible dimming devices. BRIEF DESCRIPTION OF THE DRAWINGS

[0052] Figure 1 This is a schematic diagram of the structure of the suspended particle dimming device provided in Example 1 of the utility model.

[0053] Figure 2 A top view of a first sealing frame and a second sealing frame provided in Example 1 of the utility model.

[0054] Figure 3 A top view of a first sealing frame and a second sealing frame provided in Example 2 of the utility model.

[0055] Figure 4 This is a top view of the first sealing frame and the second sealing frame provided in Example 3 of the utility model.

[0056] Figure 5 This is a schematic diagram of the structure of the suspended particle dimming device provided in Example 6 of the utility model.

[0057] Figure 6 This is a schematic diagram of the structure of the suspended particle dimming device provided in Example 7 of the utility model.

[0058] Figure 7 This is a schematic diagram of dripping dimming material provided in Example 10 of the utility model.

[0059] Figure 8 This is a schematic diagram of the structure of the suspended particle dimming device provided in Comparative Example 1 of the present invention.

[0060] Fig. 9 This is a top view of the second sealing frame provided in comparative example 1 of the present invention.

[0061] Fig.10 It is a schematic diagram of applying pressure to the suspended particle dimming device of the first embodiment.

[0062] Fig.11 Schematic diagram of applying pressure to the suspended particle dimming device of Example 6.

[0063] Among them, 101 is a first substrate; 102 is a first conductive film; 103 is supporting particles; 104 is a dimming material; 105 is a second substrate; 106 is a second conductive film; 107 is a fixed coating; 201 is a first sealing frame; 202 is a second sealing frame. DETAILED DESCRIPTION

[0064] It should be understood that, in the description of the present utility model, the terms "center", "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, which is only for the convenience of describing the present utility model and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present utility model. In addition, the terms "first", "second", etc. are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first", "second", etc. may explicitly or implicitly include one or more of the features. In the description of the present utility model, unless otherwise specified, "multiple" means two or more.

[0065] It should be noted that in the description of the present invention, unless otherwise clearly specified and limited, the term "disposition" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0066] The technical solution of the utility model is further explained below with reference to the accompanying drawings and through specific implementation methods.

[0067] In a specific embodiment, the utility model provides a suspended particle dimming device, comprising a first conductive base layer, a dimming layer and a second conductive base layer stacked in sequence, the dimming layer comprising at least two layers of sealing frame bodies nested in sequence, a receiving cavity is formed between the first conductive base layer, the second conductive base layer and the sealing frame body located in the inner layer, the receiving cavity is filled with dimming material, and a plurality of supporting particles evenly distributed are arranged inside at least one layer of the sealing frame body.

[0068] In some embodiments, at least two layers of the sealing frame body include a first sealing frame body and at least one second sealing frame body sleeved on the outside of the first sealing frame body, the accommodating cavity is formed between the first sealing frame body, the first conductive base layer and the second conductive base layer, and the supporting particles are arranged inside at least the first sealing frame body.

[0069] In some embodiments, the material of the first sealing frame includes any one of UV-curing silicone adhesive, thermosetting silicone adhesive, moisture-curing silicone adhesive, and UV heating hybrid silicone adhesive, or a combination of at least two. The material of the second sealing frame includes any one of epoxy resin thermosetting glue, acrylic light-curing glue, or UV heating hybrid glue, or a combination of at least two. In the utility model, the first sealing frame can block the diffusion of small molecules of the dimming material to prevent it from contacting with uncured non-silicone adhesives and dissolving each other, and the second sealing frame can adhere to the first conductive base layer and the second conductive base layer on both sides to improve the bonding force of the device. All of the above materials are conventional materials well known to those skilled in the art.

[0070] In some embodiments, the supporting particles are evenly distributed in the containing cavity.

[0071] In some embodiments, the distribution density of the supporting particles is 1 to 100 particles / mm 2 The diameter of the supporting particles is 2 to 100 μm. The supporting particles can be made of polymer resins, glass fibers or inorganic materials commonly used in the art. For example, the supporting particles can be polystyrene, silicon dioxide, SiO2-PS composite materials, and the like.

[0072] In some embodiments, the shape of the support particles includes sphere, cylinder or cube. The color of the support particles includes colorless, gray, red, green, white or black.

[0073] In some embodiments, the dimming layer is a flexible dimming layer, and the dimming material is a liquid material or a gel material. The utility model uniformly fixes the liquid or gel dimming material between the first conductive base layer and the second conductive base layer by supporting particles, thereby obtaining a flexible dimming layer. Specifically, the dimming material can be a SDP suspension, SPD suspension gel, liquid crystal composition or electrochromic gel well known to those skilled in the art. Exemplarily, the dimming material can be a suspended particle dispersion disclosed in CN112731722A, or a suspended particle dispersion disclosed in the document J.Mater.Chem.A, 2018, 6, 24157-24165, or other suspended particle dispersions well known to those skilled in the art, and the utility model does not specifically limit this.

[0074] In some embodiments, at least one fixed coating is further provided between the first conductive base layer and the dimming layer, and / or between the second conductive base layer and the dimming layer. Specifically, the thickness of the fixed coating is 0.005 to 30 μm. The utility model can fix the supporting particles more evenly by providing a fixed coating, so that the dimming material is evenly distributed between the first conductive base layer and the second conductive base layer. The utility model provides the following three solutions based on different settings of the fixed coating: (1) The suspended particle dimming device is composed of a first conductive base layer, a fixed coating, a dimming layer and a second conductive base layer stacked in sequence; (2) The suspended particle dimming device is composed of a first conductive base layer, a dimming layer, a fixed coating and a second conductive base layer stacked in sequence; (3) The suspended particle dimming device is composed of a first conductive base layer, a fixed coating, a dimming layer, a fixed coating and a second conductive base layer stacked in sequence.

[0075] The fixed coating layer includes any one of an organic silicone layer, an acrylic resin layer, a polyurethane resin layer or an epoxy resin layer, or a combination of at least two of them. The present invention does not specifically limit the curing method of the fixed coating layer, and can be any curing technology well known to those skilled in the art, including but not limited to heat curing, UV curing, moisture curing and peroxide curing, etc. Of course, it is understandable that other curing technologies disclosed in the prior art or not disclosed in the new technology can also be used in the present invention.

[0076] In some embodiments, the first conductive base layer includes a first substrate, and a first conductive film is disposed on a surface of the first substrate close to the dimming layer; the second conductive base layer includes a second substrate, and a second conductive film is disposed on a surface of the second substrate close to the dimming layer. That is, the suspended particle dimming device of the utility model is composed of a first substrate, a first conductive film, a dimming layer, a second conductive film and a second substrate which are stacked in sequence.

[0077] In some embodiments, the thickness of the first conductive film and the second conductive film are independently 50 to 500 μm, preferably 125 to 250 μm.

[0078] In some embodiments, the first substrate and the second substrate are independently transparent substrates. Specifically, the first substrate and the second substrate can be plastic substrates, including but not limited to polyethylene terephthalate, polyvinyl alcohol film, polymethyl methacrylate, polyethylene, polypropylene, polyvinyl chloride, polyamide, chlorinated polypropylene, and their corresponding functional coated plastic films. The first conductive film and the second conductive film independently include any one of a carbon conductive film, a metal nanowire conductive film or a metal oxide film or a combination of at least two. The carbon conductive film described in the utility model includes but is not limited to a graphene conductive film, a carbon nanotube conductive film and a graphyne conductive film. The metal nanowire conductive film includes but is not limited to a nano silver wire conductive film and a nano copper wire conductive film. The metal oxide film includes but is not limited to an indium tin oxide, an indium oxide, a tin oxide, a zinc oxide, and a mixed system of other metal oxides. It should be noted that all of the above materials are commercially available materials well known to those skilled in the art.

[0079] In another specific embodiment, the utility model provides a method for preparing a suspended particle dimming device described in a specific embodiment, the preparation method comprising: wet spraying supporting particles on the surface of a first conductive base layer and / or a second conductive base layer, and after making at least two layers of a sealing frame body, filling the dimming material to form a dimming layer, and after curing the sealing frame body, obtaining a suspended particle dimming device.

[0080] In some embodiments, the wet spraying comprises: mixing the supporting particles with a solvent, adding the mixture into a feeding chamber of a powder spraying device, and spraying the mixture onto the surface of the first conductive base layer or the second conductive base layer by circulating the mixture.

[0081] Specifically, the supporting particles include any one of high molecular polymer resin, glass fiber or inorganic material or a combination of at least two thereof; the solvent includes any one of water, ethanol, isopropanol, acetone, N-methylpyrrolidone, ethyl acetate, propylene glycol methyl ether acetate or a combination of at least two thereof. It should be noted that all of the above materials are commercially available materials well known to those skilled in the art.

[0082] The utility model first mixes the supporting particles and the solvent in a certain proportion as required, adds them to the feeding chamber of the powder spraying device, then turns on the heating, stirring and circulation functions of the equipment, sets the powder spraying time and the settling time, and after the temperature in the cavity of the equipment rises to the set value, puts the first conductive base layer and / or the second conductive base layer into the cavity of the powder spraying device to perform the powder spraying operation. The feeding chamber needs to adopt the method of continuous stirring and circulating feeding, the purpose is to ensure that the supporting particles and the solvent are mixed evenly, which is conducive to achieving uniform distribution of supporting particles in the later stage. The purpose of heating is to partially volatilize the solvent after spraying. The temperature setting range depends on the volatility characteristics of the wet spraying solvent, and the density of the powder spraying can also be controlled by adjusting the setting of the powder spraying time and the settling time. Since the surface of the organic silicone fixed coating has a certain adhesion after curing, the spraying operation of the supporting particles can be carried out after curing. However, epoxy resin, polyurethane, acrylic acid, etc. have no sticky glue on the surface after curing. If the supporting particles are sprayed after curing, the supporting particles will not be fixed. Therefore, it is necessary to spray the supporting particles evenly on the surface of the conductive base layer before curing, and then cure the fixed coating.

[0083] In some embodiments, the method for making the sealing frame body includes: using an adhesive material to sequentially form at least two layers of the sealing frame body on the surface of the first conductive base layer or the second conductive base layer sprayed with supporting particles, and performing a curing process. The adhesive material includes any one of UV curable silicone adhesive, epoxy resin thermosetting adhesive, acrylic light curing adhesive, or UV heating mixed adhesive, or a combination of at least two.

[0084] In some embodiments, the dimming material is filled by vacuum infusion or drip vacuum lamination. The vacuum infusion method is suitable for the preparation of small-sized products, and the drip vacuum lamination method is suitable for the preparation of large-sized products. That is, the utility model provides the following two solutions for filling the dimming material, specifically including:

[0085] Option 1: Vacuum infusion method

[0086] S1: wet-spraying supporting particles on the surface of the first conductive base layer to obtain an intermediate;

[0087] S2: making at least two layers of sealing frame bodies on the side of the intermediate body sprayed with supporting particles, the sealing frame body being provided with a material injection port, and then laminating the second conductive base layer and performing a curing treatment to obtain an empty box structure with a receiving cavity;

[0088] S3: placing the dimming material and the empty box structure at different positions in the crystal filling device, and evacuating the device, then bringing the dimming material into contact with the empty box structure, and gradually releasing the pressure so that the dimming material is poured into the containing cavity to obtain a suspended particle dimming device.

[0089] Solution 2: Instillation vacuum lamination

[0090] S01: wet-spraying supporting particles on the surface of the first conductive base layer to obtain an intermediate;

[0091] S02: making at least two layers of sealing frame bodies on one side of the intermediate body sprayed with supporting particles, wherein the sealing frame bodies are fully enclosed, and uniformly dripping dimming materials into the space surrounded by the sealing frame bodies located on the inner side to obtain a filling box structure;

[0092] S03: Move the potting structure and the second conductive base layer into the vacuum chamber, adsorb them in the equipment through vacuum, and evacuate the equipment so that the second conductive base layer fits the potting structure, and then perform a curing process on the sealing frame body to obtain a suspended particle dimming device.

[0093] In some embodiments, the preparation method further comprises: before the wet spraying, coating a primer on the surface of the first conductive base layer and / or the second conductive base layer, and performing a drying treatment to form a fixed coating.

[0094] Taking thermally inherent organic silica gel as an example, the coating method of the bottom glue in the utility model can be a micro-concave roller coating method, a slit extrusion coating method, a spraying method, or a micro-concave roller coating method. According to the target thickness, different micro-concave roller meshes and solid contents are selected to obtain a thinner coating thickness with higher uniformity. Among them, slit extrusion coating can adjust different solid contents, flow rates, and line speeds to obtain different target thicknesses. The drying treatment temperature can be set according to the actual amount of glue and the actual curing requirements. After the drying treatment is completed, PET or fluorine release film can be selected for lamination protection according to the adhesion of the fixed coating. In addition, epoxy resin heat-curing glue, polyurethane resin, acrylic and other light-curing glues can all be prepared by the above coating methods. The difference is that the curing methods of glues of different properties are different. The light-curing glue needs to be first superheated in an oven to volatilize the solvent and then be cured by UV lamp illumination.

[0095] In some embodiments, the preparation method further comprises: performing plasma treatment on the surface of the first conductive base layer and / or the second conductive base layer to remove organic residues on the surface and simultaneously achieve the effect of activating the surface.

[0096] Example 1

[0097] This embodiment provides a suspended particle dimming device, denoted as b1. Figure 1 and Figure 2As shown, it specifically includes a first substrate 101, a first conductive film 102, a flexible dimming layer, a second conductive film 106 and a second substrate 105 which are stacked in sequence. The thickness of the first conductive film 102 and the second conductive film 106 are both 200 μm, and both are indium tin oxide conductive films. The flexible dimming layer includes a first sealing frame 201 and a second sealing frame 202 which are nested in sequence, and a receiving cavity is formed between the first conductive base layer, the second conductive base layer and the first sealing frame 201, and the receiving cavity is filled with a dimming material 104, and the interior of the receiving cavity and the first sealing frame 201 is filled with spherical supporting particles 103. The material of the first sealing frame 201 is a UV-curable silicone adhesive to block the diffusion of small molecules of the dimming material 104, and the material of the second sealing frame 202 is an epoxy resin thermosetting adhesive to firmly bond the first conductive film 102 and the second conductive film 106.

[0098] The method for preparing the suspended particle dimming device in this embodiment includes the following steps:

[0099] (1) providing a first substrate 101 having a first conductive film 102 and a second substrate 105 having a second conductive film 106, and performing plasma treatment on the first conductive film 102 and the second conductive film 106;

[0100] (2) mixing the supporting particles 103 and the solvent in a certain proportion, adding the mixture into the feeding chamber of the powder spraying device, heating and stirring the mixture, and spraying the mixture onto the surface of the first conductive film 102 by circulating the feeding, so that the supporting particles 103 are evenly distributed on the first conductive film 102, thereby obtaining an intermediate;

[0101] (3) On the side of the intermediate body sprayed with the supporting particles 103, two layers of the first sealing frame 201 and the second sealing frame 202 are sequentially manufactured, and the first sealing frame 201 and the second sealing frame 202 are provided with injection ports, and then the second substrate 105 is bonded and cured to obtain an empty box structure with a receiving cavity;

[0102] (4) The dimming material 104 and the empty box structure are placed at different positions in the crystal filling device, and the vacuum is continuously applied for more than 30 minutes. Then, the dimming material 104 is brought into contact with the empty box structure, and the pressure is gradually released so that the dimming material 104 is poured into the containing cavity to obtain a suspended particle dimming device.

[0103] The dimming material 104 used in this embodiment is a suspended particle dispersion disclosed in CN112731722A. The specific raw materials and preparation method thereof are as described in CN112731722A and are not described in detail herein.

[0104] Example 2

[0105] This embodiment provides a suspended particle dimming device, denoted as b2. Figure 3 As shown, the difference from Example 1 is that support particles 103 are also provided inside the second sealing frame 202, that is, support particles 103 are provided inside the accommodating cavity, inside the first sealing frame 201, and inside the second sealing frame 202, and the rest of the structure, parameters, materials and preparation method are the same as those in Example 1.

[0106] Example 3

[0107] This embodiment provides a suspended particle dimming device, denoted as b3. Figure 4 As shown, the difference from Example 1 is that: the interior of the first sealing frame 201 is not provided with supporting particles 103, and the interior of the second sealing frame 202 is provided with supporting particles 103, that is, supporting particles 103 are provided in the accommodating cavity and the interior of the second sealing frame 202, and the rest of the structure, parameters, materials and preparation method are the same as those in Example 1.

[0108] Example 4

[0109] This embodiment provides a suspended particle dimming device, denoted as b4, which differs from Embodiment 1 in that the materials of the first sealing frame 201 and the second sealing frame 202 are both UV-curable silicone adhesives, and the rest of the structure, parameters, materials and preparation methods are the same as those of Embodiment 1.

[0110] Example 5

[0111] This embodiment provides a suspended particle dimming device, denoted as b5, which differs from Embodiment 1 in that the materials of the first sealing frame 201 and the second sealing frame 202 are both epoxy resin thermosetting adhesive, and the rest of the structure, parameters, materials and preparation methods are the same as those of Embodiment 1.

[0112] Example 6

[0113] This embodiment provides a suspended particle dimming device, denoted as b6. Figure 5 As shown, the difference from Example 1 is that a fixed coating 107 is provided between the first conductive film 102 and the flexible dimming layer, and between the second conductive film 106 and the flexible dimming layer. The remaining structures and parameters are the same as those of Example 1.

[0114] The method for preparing the suspended particle dimming device in this embodiment includes the following steps:

[0115] (1) providing a first substrate 101 having a first conductive film 102 and a second substrate 105 having a second conductive film 106, and performing plasma treatment on the first conductive film 102 and the second conductive film 106;

[0116] (2) coating the surface of the first conductive film 102 and the second conductive film 106 with organic silica gel by slit extrusion coating, and drying the coating to form a fixed coating 107;

[0117] (3) Mixing the supporting particles 103 and the solvent in a certain proportion, adding the mixture into the feeding chamber of the powder spraying device, heating and stirring the mixture, and spraying the mixture onto the surface of the first conductive film 102 by circulating the feeding, so that the supporting particles 103 are evenly distributed on the fixed coating 107, thereby obtaining an intermediate;

[0118] (4) On the side of the intermediate body sprayed with the supporting particles 103, two layers of the first sealing frame 201 and the second sealing frame 202 are sequentially manufactured, and the first sealing frame 201 and the second sealing frame 202 are provided with injection ports, and then the second substrate 105 is bonded and cured to obtain an empty box structure with a receiving cavity;

[0119] (5) The dimming material 104 and the empty box structure are placed at different positions in the crystal filling device, and the vacuum is continuously applied for more than 30 minutes. Then, the dimming material 104 is brought into contact with the empty box structure, and the pressure is gradually released so that the dimming material 104 is poured into the containing cavity to obtain a suspended particle dimming device.

[0120] Example 7

[0121] This embodiment provides a suspended particle dimming device, which is different from the embodiment 6 in that: Figure 6 As shown, only the fixed coating layer 107 is provided between the first conductive film 102 and the flexible dimming layer, and the rest of the structure, parameters, materials and preparation method are the same as those in the sixth embodiment.

[0122] Example 8

[0123] This embodiment provides a suspended particle dimming device, which differs from Embodiment 6 in that only a fixed coating 107 is provided between the second conductive film 106 and the flexible dimming layer, and the rest of the structure, parameters, materials and preparation methods are the same as those of Embodiment 6.

[0124] Example 9

[0125] This embodiment provides a suspended particle dimming device, which is different from the sixth embodiment in that the fixed coating 107 is made of epoxy resin, and the rest of the structure and parameters are the same as those of the sixth embodiment.

[0126] The method for preparing the suspended particle dimming device in this embodiment includes the following steps:

[0127] (1) providing a first substrate 101 having a first conductive film 102 and a second substrate 105 having a second conductive film 106, and performing plasma treatment on the first conductive film 102 and the second conductive film 106;

[0128] (2) coating the epoxy resin on the surface of the first conductive film 102 and the second conductive film 106 by slit extrusion coating;

[0129] (3) Mixing the supporting particles 103 and the solvent in a certain proportion, adding the mixture into the feeding chamber of the powder spraying device, heating and stirring the mixture, and spraying the powder onto the surface of the first conductive film 102 by circulating the feeding method, so that the supporting particles 103 are evenly distributed on the epoxy resin, and drying and curing the epoxy resin to form a fixed coating 107, thereby obtaining an intermediate;

[0130] (4) On the side of the intermediate body sprayed with the supporting particles 103, two layers of the first sealing frame 201 and the second sealing frame 202 are sequentially manufactured, and the first sealing frame 201 and the second sealing frame 202 are provided with injection ports, and then the second substrate 105 is bonded and cured to obtain an empty box structure with a receiving cavity;

[0131] (5) The dimming material 104 and the empty box structure are placed at different positions in the crystal filling device, and the vacuum is continuously applied for more than 30 minutes. Then, the dimming material 104 is brought into contact with the empty box structure, and the pressure is gradually released so that the dimming material 104 is poured into the containing cavity to obtain a suspended particle dimming device.

[0132] Example 10

[0133] This embodiment provides a suspended particle dimming device, denoted as b7, whose preparation method is different from that of embodiment 1, and the rest of the structure, parameters and materials are the same as those of embodiment 1.

[0134] The method for preparing the suspended particle dimming device of this embodiment comprises the following steps:

[0135] (1) providing a first substrate 101 having a first conductive film 102 and a second substrate 105 having a second conductive film 106, and performing plasma treatment on the first conductive film 102 and the second conductive film 106;

[0136] (2) coating the surface of the first conductive film 102 and the second conductive film 106 with organic silica gel by slit extrusion coating, and drying the coating to form a fixed coating 107;

[0137] (3) Mixing the supporting particles 103 and the solvent in a certain proportion, adding the mixture into the feeding chamber of the powder spraying device, heating and stirring the mixture, and spraying the mixture onto the surface of the first conductive film 102 by circulating the feeding, so that the supporting particles 103 are evenly distributed on the fixed coating 107, thereby obtaining an intermediate;

[0138] (4) Two layers of a first sealing frame 201 and a second sealing frame 202 are sequentially manufactured on one side of the intermediate body sprayed with the supporting particles 103, and both the first sealing frame 201 and the second sealing frame 202 are fully enclosed, such as Figure 7 As shown, the dimming material 104 is evenly dripped into the space surrounded by the first sealing frame 201 located on the inner side, and the total amount of the liquid dimming material 104 is the same as the required total amount of the first sealing frame 201 size, thereby obtaining a filling box structure;

[0139] (5) The filling box structure and the second conductive base layer are moved into a vacuum chamber, adsorbed in the device by vacuum, and evacuated so that the second substrate 105 with the second conductive film 106 fits the filling box structure, and then the first sealing frame 201 and the second sealing frame 202 are cured to obtain a suspended particle dimming device.

[0140] Embodiment 11

[0141] This embodiment provides a suspended particle dimming device, denoted as b8, which differs from Embodiment 1 in that the material of the second sealing frame 202 is acrylic light-curing adhesive, and the rest of the structure, parameters, materials and preparation method are the same as those of Embodiment 1.

[0142] Example 12

[0143] This embodiment provides a suspended particle dimming device, denoted as b9, which differs from Embodiment 1 in that the material of the second sealing frame 202 is UV heating mixed glue, and the rest of the structure, parameters, materials and preparation method are the same as those of Embodiment 1.

[0144] Comparative Example 1

[0145] This comparative example provides a suspended particle dimming device, denoted as a1, such as Figure 8 and Fig. 9 As shown, the difference from Example 1 is that the first sealing frame 201 is not provided, and the supporting particles 103 are provided in the second sealing frame 202. The rest of the structure, parameters, materials and preparation method are the same as those of Example 1.

[0146] Comparative Example 2

[0147] This comparative example provides a suspended particle dimming device, denoted as a2, which differs from Example 1 in that the second sealing frame 202 is not provided, and the rest of the structure, parameters, materials and preparation method are the same as those of Example 1.

[0148] Comparative Example 3

[0149] This comparative example provides a silicone support SPD device disclosed in the document J.Mater.Chem.A, 2018, 6, 24157-24165, denoted as a3.

[0150] Comparative Example 4

[0151] This comparative example provides a suspended particle dimming device, denoted as a4, which differs from Example 1 in that: no supporting particles 103 are provided in the flexible dimming layer, and the rest of the structure, parameters, materials and preparation method are the same as those in Example 1.

[0152] The utility model adopts b1~b9 and a1~a4 to obtain dimming devices for electrode preparation. In order to prevent short circuit between the upper and lower electrodes, all device edges are passivated. All devices are subjected to high temperature and high humidity and peeling force tests, wherein the high temperature and high humidity conditions are 70°C, 100% humidity, and drying for 6 hours; the peeling force test is measured on an electronic tensile testing machine, and the transmittance dynamic range is measured by a voltage-transmittance test device, and the results are shown in Table 1 (NA in the table means below the detection limit).

[0153] Table 1

[0154]

[0155]

[0156] It can be seen from the contents of Table 1 that, compared with Examples 1 and 2, the device uniformity of Example 3 is reduced. This is mainly because no supporting particles 103 are provided in the first sealing frame 201 of Example 3. Since the first sealing frame 201 is located between the accommodating cavity and the second sealing frame 202, a structure is formed in which the supporting force in the middle is lower than the supporting force on both sides, resulting in poor uniformity of the device in the peeling force test.

[0157] By comparing Example 1, Example 4 and Example 5, it can be seen that when the first sealing frame 201 and the second sealing frame 202 are made of the same material, their colored state and transparent state deteriorate, while in Example 1, the first sealing frame 201 can block the diffusion of small molecules of the dimming material 104, and the second sealing frame 202 firmly bonds the first conductive film 102 and the second conductive film 106, thereby effectively improving the device performance.

[0158] It can be seen from Table 1 that the device performance of Example 1 and Example 6 is better. Fig.10 and Fig.11It is not difficult to see that, when a certain pressure is applied, Example 6 can alleviate the movement of the supporting particles 103 by fixing the coating 107, while in Example 1, the friction between the supporting particles 103 and the conductive film is smaller, making it easier to move under pressure, causing the uniformity of the device to deteriorate after a certain pressure.

[0159] Compared with Example 6 and Example 9, both sides of the supporting particle 103 are fixed by a fixed coating 107, while in Example 7 and Example 8, only one side of the supporting particle 103 is fixed. When pressure is applied in different directions, the device with a single-sided fixed structure is prone to movement of the supporting particle 103.

[0160] It can be seen from Table 1 that the devices of Examples 10 to 12 have good supporting performance, and the bonding force between the first conductive film 102 and the second conductive film 106 is relatively high, and can also block the diffusion of small organic molecules in the dimming material 104, avoiding the failure of the adhesive, thereby maintaining a relatively high uniformity.

[0161] The applicant declares that the above is only a specific implementation method of the present utility model, but the protection scope of the present utility model is not limited thereto. The technicians in the relevant technical field should understand that any changes or substitutions that can be easily thought of by the technicians in the relevant technical field within the technical scope disclosed in the present utility model fall within the protection scope and disclosure scope of the present utility model.

Claims

1. A suspended particle dimming device, characterized in that: The suspended particle dimming device includes a first conductive base layer, a dimming layer and a second conductive base layer stacked in sequence, the dimming layer includes at least two layers of sealing frame bodies nested in sequence, a receiving cavity is formed between the first conductive base layer, the second conductive base layer and the sealing frame body located in the inner layer, the receiving cavity is filled with dimming material, and a plurality of supporting particles evenly distributed are arranged inside at least one layer of the sealing frame body.

2. The suspended particle dimming device according to claim 1, characterized in that: The at least two layers of the sealing frame body include a first sealing frame body and at least one second sealing frame body sleeved on the outside of the first sealing frame body, the accommodating cavity is formed between the first sealing frame body, the first conductive base layer and the second conductive base layer, and the supporting particles are arranged inside at least the first sealing frame body.

3. The suspended particle dimming device according to claim 1 or 2, characterized in that: The supporting particles are evenly distributed in the containing cavity.

4. The suspended particle dimming device according to claim 1, characterized in that: The distribution density of the supporting particles is 1 to 100 particles / mm 2 ; The diameter of the supporting particles is 2 to 100 μm.

5. The suspended particle dimming device according to claim 1, characterized in that: The shapes of the supporting particles include sphere, cylinder or cube.

6. The suspended particle dimming device according to claim 1, characterized in that: The dimming layer is a flexible dimming layer, and the dimming material is a liquid material or a gel material.

7. The suspended particle dimming device according to claim 1, characterized in that: At least one fixed coating layer is disposed between the first conductive base layer and the dimming layer, and / or between the second conductive base layer and the dimming layer.

8. The suspended particle dimming device according to claim 1, characterized in that: The first conductive base layer includes a first substrate, and a first conductive film is disposed on a surface of the first substrate close to the dimming layer; the second conductive base layer includes a second substrate, and a second conductive film is disposed on a surface of the second substrate close to the dimming layer.

9. The suspended particle dimming device according to claim 8, characterized in that: The thickness of the first conductive film and the second conductive film are independently 50 to 500 μm.

10. The suspended particle dimming device according to claim 8, characterized in that: The first substrate and the second substrate are independently transparent substrates.

Citation Information

Cited By

  • Suspended particle dimming device and preparation method and application thereof

    CN118330946A