Crystallizer with rapid cooling function and vertical continuous casting system
By using a cooling method combined with water-cooled sleeve and rapid spraying and a double-layer water-cooled sleeve structure in the vertical continuous casting process, the problems of slow cooling speed and easy oxidation of the casting blank are solved, and uniform cooling of the ingot is achieved and Efficient production.
Patent Information
- Application Number
- CN202421371303.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-17
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2034-06-17
AI Technical Summary
The cooling speed is slow during the traditional vertical continuous casting process, resulting in uneven structure of the casting blank, poor performance, and the casting blank is prone to oxidation during the crystallization process.
A crystallizer with rapid cooling function is designed, using a cooling method combining water-cooling sleeve and rapid spraying. A double-layer water-cooling sleeve structure is formed through a partition plate. The cooling water is first filled with the outer cooling chamber and then enters the inner cooling chamber, and then passes through the The spray port is re-cooled to ensure that the ingot is cooled evenly throughout the cooling process and isolate the air through water to avoid oxidation.
It significantly improves the cooling speed, improves the structural uniformity and performance of the ingot, avoids oxidation during the solidification process, and ensures efficient production and quality of the casting billet.
Smart Images

Figure CN222113482U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of casting technology, and in particular to a crystallizer with rapid cooling function and a vertical continuous casting system. Background Art
[0002] Vertical continuous casting, also known as vertical continuous casting, refers to a continuous steel casting method in which the entire process of casting and solidification of the ingot is carried out in a vertical state. However, there are many defects in the traditional vertical continuous casting process. For example, only a water cooling jacket is used to cool the ingot in the crystallizer, and the cooling rate is slow, which leads to a slow continuous casting rate and ultimately low production efficiency. It is also easy to cause uneven ingot temperature, uneven structure, and poor performance. In addition, the ingot is easily exposed to air during the crystallization process, which leads to oxidation. Utility Model Content
[0003] The purpose of the present application is to provide a crystallizer and a vertical continuous casting system with a rapid cooling function, which to a certain extent solves the technical problem that the traditional vertical continuous casting in the prior art only uses a water cooling jacket for cooling, and the cooling speed is slow, which not only reduces the continuous casting speed, but also easily causes uneven structure of the ingot and poor performance. In addition, the ingot is easily exposed to air during the crystallization process, which leads to oxidation.
[0004] The present application provides a crystallizer with a rapid cooling function, comprising a main body, wherein the main body is formed with a continuous casting cavity, a cooling cavity and a water inlet; the continuous casting cavity runs through the top and bottom of the main body along its height direction, the cooling cavity surrounds the outer circumference of the continuous casting cavity and is spaced apart from the continuous casting cavity, and a spray port connecting the cooling cavity and the continuous casting cavity is formed at the lower part of the side wall between the cooling cavity and the continuous casting cavity; the water inlet is communicated with the cooling cavity.
[0005] In the above technical solution, further, the crystallizer with rapid cooling function also includes a partition plate, which is arranged in the cooling cavity and along the direction of the cooling cavity toward the continuous casting cavity, the partition plate divides the cooling cavity into an outer cooling cavity and an inner cooling cavity;
[0006] The partition plate is formed with a first port, and along the height direction of the cooling cavity, one of the first port and the water inlet is close to the top end of the cooling cavity, and the other is arranged close to the bottom end of the cooling cavity.
[0007] In any of the above technical solutions, further, the water inlet is arranged on the outer side of the main body near its bottom end; and the first outlet is arranged at a position of the partition plate near its top end.
[0008] In any of the above technical solutions, further, the number of the spray ports is multiple, and they are arranged in an array along the height direction of the main body and the periphery of the main body.
[0009] In any of the above technical solutions, further, along the height direction of the main body, two adjacent rows of the spray ports are staggered.
[0010] In any of the above technical solutions, further, the plurality of spray ports are distributed from the lower part of the body to the bottom of the body to form a spray area.
[0011] In any of the above technical solutions, further, the cross-section of the continuous casting cavity along its height direction is circular, and the inner diameter of the spraying zone of the continuous casting cavity is larger than the inner diameter of other positions of the continuous casting cavity.
[0012] In any of the above technical solutions, further, the body includes an inner ring portion and an outer ring portion, the outer ring portion is sleeved outside the inner ring portion and connected, and the cooling cavity is formed between the inner ring portion and the outer ring portion;
[0013] The crystallizer with rapid cooling function also includes a dynamic seal and a dummy rod; wherein the dynamic seal is movably arranged in the continuous casting cavity, and the outer side wall of the dynamic seal is against the inner wall of the continuous casting cavity; the dummy rod is arranged below the dynamic seal, and the dummy rod is connected to the bottom of the dynamic seal.
[0014] The present application also provides a vertical continuous casting system, comprising a heat preservation bag and a crystallizer with a rapid cooling function as described in any of the above technical solutions, wherein the heat preservation bag is arranged on the top of the body of the crystallizer with a rapid cooling function, and a second port connected to the interior of the heat preservation bag is formed at the bottom of the heat preservation bag, and the second port is connected to the opening at the top of the continuous casting cavity. Therefore, all the beneficial technical effects of the crystallizer with a rapid cooling function are not repeated here.
[0015] In the above technical solution, further, the insulation bag includes a crucible, insulation cotton and a heating device; wherein the insulation cotton is wrapped around the outer wall of the crucible, and the heating device is arranged on a side of the insulation cotton away from the crucible, and is used to heat the crucible.
[0016] Compared with the prior art, the beneficial effects of this application are:
[0017] When the improved crystallizer with rapid cooling function provided by the present application is in operation, cooling water first enters the cooling chamber from the water inlet, and then cools the inner wall of the continuous casting chamber, that is, gradually cools the molten steel that continuously moves downward in the continuous casting chamber. Under the cooling action, the molten steel gradually becomes an ingot. When the ingot passes through the spray port at the bottom, it can be cooled for the second time, that is, a cooling method combining a water cooling jacket and rapid spraying is adopted, thereby accelerating the cooling speed, improving the efficiency of vertical continuous casting, and making the structure of the ingot more uniform and the performance better.
[0018] In addition, a water seal can be formed between the ingot and the inner wall of the body of the crystallizer to completely isolate the solidification process of the molten steel in the upper part of the crystallizer from the outside air, thereby avoiding oxidation during the solidification process. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0020] Figure 1 A schematic diagram of the structure of a crystallizer with a rapid cooling function provided in an embodiment of the present application;
[0021] Figure 2 A schematic diagram of the expansion of the partition plate provided in an embodiment of the present application.
[0022] Reference numerals:
[0023] 1-main body, 11-inner ring, 12-outer ring, 13-continuous casting chamber, 14-cooling chamber, 141-outer cooling chamber, 142-inner cooling chamber, 15-first port, 16-water inlet, 17-spray port, 2-partition plate, 3-dynamic seal, 4-ingot rod, 5-ingot head, 6-insulation bag, 61-crucible, 62-insulation cotton, 63-heating device, 7-molten steel. DETAILED DESCRIPTION
[0024] The technical solution of the present application will be clearly and completely described below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments.
[0025] The components of the embodiments of the present application generally described and shown in the drawings herein can be arranged and designed in various different configurations. Therefore, the following detailed description of the embodiments of the present application provided in the drawings is not intended to limit the scope of the application claimed, but merely represents the selected embodiments of the present application.
[0026] Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making any creative work shall fall within the scope of protection of this application.
[0027] In the description of the present application, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present application. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0028] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0029] Refer to the following Figure 1 and Figure 2 A crystallizer and a vertical continuous casting system with rapid cooling function according to some embodiments of the present application are described.
[0030] See also Figure 1 and Figure 2 As shown, an embodiment of the present application provides a crystallizer with a rapid cooling function, including a main body 1, and the main body 1 is formed with a continuous casting cavity 13, a cooling cavity 14 and a water inlet 16; the continuous casting cavity 13 runs through the top and bottom of the main body 1 along its height direction, the cooling cavity 14 surrounds the outer circumference of the continuous casting cavity 13 and is spaced apart from the continuous casting cavity 13, and a spray port 17 connecting the cooling cavity 14 and the continuous casting cavity 13 is formed at the lower part of the side wall between the cooling cavity 14 and the continuous casting cavity 13; the water inlet 16 is communicated with the cooling cavity 14.
[0031] In this embodiment, when the improved crystallizer is working, cooling water first enters the cooling chamber 14 from the water inlet 16, and then cools the inner wall of the continuous casting chamber 13, that is, gradually cools the molten steel 7 that continuously moves downward in the continuous casting chamber 13. Under the cooling effect, the molten steel 7 gradually becomes an ingot. When the ingot passes through the lower spray port 17, it can be cooled for the second time, that is, a cooling method combining a water cooling jacket and rapid spraying is adopted, thereby accelerating the cooling speed, improving the efficiency of vertical continuous casting, and making the structure of the ingot more uniform and the performance better.
[0032] In addition, a water seal can be formed between the ingot and the inner wall of the body 1 of the crystallizer to completely isolate the solidification process of the molten steel 7 in the upper part of the crystallizer from the outside air, thereby avoiding oxidation during the solidification process.
[0033] In one embodiment of the present application, preferably, Figure 1 As shown, the crystallizer with rapid cooling function further includes a partition plate 2, which is disposed in the cooling chamber 14 and along the direction of the cooling chamber 14 toward the continuous casting chamber 13, the partition plate 2 divides the cooling chamber 14 into an outer cooling chamber 141 and an inner cooling chamber 142;
[0034] The partition plate 2 is formed with a first port 15 , and along the height direction of the cooling cavity 14 , one of the first port 15 and the water inlet 16 is close to the top of the cooling cavity 14 , and the other is close to the bottom of the cooling cavity 14 .
[0035] In this embodiment, the cooling chamber 14 is divided into an outer cooling chamber 141 and an inner cooling chamber 142 by a partition plate 2, that is, a double-layer water-cooling jacket structure is formed. Compared with the single-layer water-cooling jacket in the prior art, the cooling water first enters the outer cooling chamber 141 through the water inlet 16. When the outer cooling chamber 141 is filled, it flows into the inner cooling chamber 142 through the first port 15, which increases the travel distance of the coolant, greatly improves the cooling effect, and can effectively avoid the eddy current phenomenon caused by the single-layer water-cooling structure, thereby making the heat exchange more uniform and effective.
[0036] In addition, only when the outer cooling cavity 141 is filled with water can the water flow into the inner cooling cavity 142. The outer layer of cooling water also cools the water in the inner cooling cavity 142, thereby achieving a good cooling effect.
[0037] Further, preferably, the partition plate 2 and the cooling chamber 14 can be connected by snapping, gluing, bolts or other interference fit methods.
[0038] In one embodiment of the present application, preferably, Figure 1 As shown, the water inlet 16 is arranged on the outer side of the body 1 near the bottom end thereof; the first outlet 15 is arranged at a position of the partition plate 2 near the top end thereof.
[0039] In this embodiment, the cooling water first enters the outer cooling chamber 141 through the water inlet 16 near the bottom. When the outer cooling chamber 141 is filled, it flows into the inner cooling chamber 142 through the first outlet 15 near the top, thereby increasing the travel distance of the coolant and greatly improving the cooling effect. Finally, the cooling water is sprayed out through the spray port 17 at the bottom.
[0040] Further, preferably, there are multiple first ports 15, which are evenly arranged along the outer circumference of the inner cooling cavity 142. Of course, this is not limited to this. The number of the first ports 15 can also be one, which is arranged in a ring shape, and the specific design is based on actual needs.
[0041] In one embodiment of the present application, preferably, Figure 1 and Figure 2 As shown, there are multiple spray ports 17 , which are arranged in an array along the height direction of the body 1 and the periphery of the body 1 .
[0042] In this embodiment, a plurality of spray ports 17 are designed to be arranged in a display, which can ensure the uniformity of the coolant sprayed at various locations, thereby ensuring the consistency of the cooling effect on various positions of the ingot, thereby ensuring the uniformity of the structure, and helping to improve the performance of the ingot.
[0043] In one embodiment of the present application, preferably, Figure 2 As shown, along the height direction of the body 1, two adjacent rows of spray ports 17 are staggered to further ensure the uniformity of the distribution of the multiple spray ports 17. Of course, it is not limited to this, and it can be set according to actual needs. For example, along the height direction of the body 1, two adjacent rows of spray ports 17 can be set directly opposite each other.
[0044] In one embodiment of the present application, preferably, Figure 1 As shown, the plurality of spray ports 17 are distributed from the lower portion of the main body 1 to the bottom of the main body 1 to form a spray zone, thereby increasing the spray area, improving the cooling effect on the ingot, and ensuring sufficient water sealing thickness to improve the anti-oxidation effect.
[0045] In one embodiment of the present application, preferably, Figure 1 As shown, the cross section of the continuous casting cavity 13 along its height direction is circular, and the inner diameter of the spraying zone of the continuous casting cavity 13 is larger than the inner diameter of other positions of the continuous casting cavity 13, which helps to increase the flow space of water and speed up the spraying speed.
[0046] In one embodiment of the present application, preferably, Figure 1 As shown, the body 1 includes an inner ring portion 11 and an outer ring portion 12 . The outer ring portion 12 is sleeved outside the inner ring portion 11 and connected to each other. A cooling cavity 14 is formed between the inner ring portion 11 and the outer ring portion 12 .
[0047] In this embodiment, the main body 1 is designed to be an inner ring portion 11 and an outer ring portion 12, so that it is easy to install the partition plate 2 and other structures therein, and the operation is simple and convenient.
[0048] Further, preferably, the inner ring portion 11 includes a main body and a first flange and a second flange connected to the main body, the first flange is arranged at the top of the main body, the second flange is arranged at the bottom of the main body, the main body, the first flange and the second flange form a groove opening toward the outside, the outer ring portion 12 is snapped into the groove, and the top end of the outer ring portion 12 abuts against the bottom of the first flange, and the bottom end of the outer ring portion 12 abuts against the top of the second flange. It can be seen that the outer wall of the main body, the first flange, the second flange and the inner wall of the outer ring portion 12 are surrounded to form the aforementioned cooling cavity 14. Of course, the structure and assembly method of the outer ring portion 12 and the inner ring portion 11 are not limited to this, and can also be designed according to actual needs. For example, the inner ring portion 11 and the outer ring portion 12 can be connected by gluing, bolts or snap-on.
[0049] In one embodiment of the present application, preferably, Figure 1 As shown, the crystallizer with rapid cooling function further includes a dynamic seal 3 , which is movably disposed in the continuous casting cavity 13 , and an outer side wall of the dynamic seal 3 abuts against an inner wall of the continuous casting cavity 13 .
[0050] Further, preferably, the crystallizer with rapid cooling function further comprises a dummy rod 4 and a dummy head 5 , the dummy rod 4 is arranged below the dynamic seal 3 , and the dummy head 5 arranged at the head of the dummy rod 4 is embedded in the dynamic seal 3 .
[0051] In this embodiment, the dummy rod 4 plays the role of pulling the molten steel 7 downward; the dynamic seal 3 ensures the sealing performance during the movement to prevent the molten steel 7 from leaking.
[0052] An embodiment of the present application also provides a vertical continuous casting system, comprising a crystallizer with a rapid cooling function as described in any of the above embodiments. Therefore, all the beneficial technical effects of the crystallizer with a rapid cooling function are not repeated here.
[0053] In one embodiment of the present application, preferably, Figure 1 As shown, the vertical continuous casting system also includes an insulation bag 6, which is arranged on the top of the main body 1 of the crystallizer with a rapid cooling function. A second port connected to the interior of the insulation bag 6 is formed at the bottom of the insulation bag 6, and the second port is connected to the opening at the top of the continuous casting cavity 13.
[0054] Further, preferably, the heat preservation bag 6 includes a crucible 61, heat preservation cotton 62 and a heating device 63; wherein the heat preservation cotton 62 is wrapped around the outer wall of the crucible 61, and the heating device 63 is arranged on the side of the heat preservation cotton 62 away from the crucible 61, and is used to heat the crucible 61, and the heat preservation cotton 62 plays a role of heat preservation. Of course, the structure of the heat preservation bag 6 is not limited to the above, as long as it can play a role of heat preservation and does not react with the molten steel 7.
[0055] In summary, the detailed working process of the vertical continuous casting system provided by this application is as follows:
[0056] First, connect the ingot guide rod 4 and the dynamic seal 3 together and move them to the upper initial position. During the melting process of the molten steel 7, there is no need to pass cooling water into the cooling chamber 14 in the crystallizer. When the smelting is completed and it is ready to be poured, start to pass water into the cooling chamber 14 of the crystallizer. At this time, some water will flow out of the spray port 17. When the cooling water flows out of the spray port 17 in a large amount and the flow rate does not increase, the molten steel 7 is cast into the insulation bag 6, that is, the molten steel 7 is transferred to the crucible 61. At this time, the ingot supporting mechanism begins to move down slowly, driving the ingot guide rod 4 and the dynamic seal 3 to move down, while continuing to cast, and keeping the liquid level of the molten steel 7 in a basically stable state. It can solidify when passing through the inner wall of the crystallizer, and can be quickly cooled again when passing through the spray port 17. When it reaches the position of the spray port 17, the cooling speed is very fast, so the speed of the ingot support can be appropriately accelerated. At the same time, the pouring speed should also be increased to keep the molten steel 7 balanced. After the casting is completed, the temperature of the ingot will not be very high due to the spraying.
[0057] It can be seen that the double-layer water cooling jacket is designed in the crystallizer of the present application, which has a fast cooling speed and good cooling effect, and has a very good effect on metal solidification and metal crystallization. The water seal formed by the spray water below isolates the ingot from the air during the solidification process, thereby reducing the pores on the surface of the ingot and also reducing the oxidation of the metal during the solidification process.
[0058] In the past, some heavy skin or scarring would occur during the top supporting process. The main reason was that molten steel penetrated into the gap between the crystallizer and the ingot. The problem occurred because the continuous casting speed was too slow, resulting in the solidified ingot not being dragged out in time. If the ingot dragging speed was increased, steel leakage might occur. The present application utilizes a rapid cooling method that combines two cooling methods, and the ingot will be cooled and solidified at the spray port 17, avoiding the phenomenon of steel leakage during rapid continuous casting.
[0059] In the past, continuous casting was not only slow, but also the temperature of the ingot was still very high after the continuous casting was completed, even up to more than 700 degrees. It was also a troublesome thing to move the ingot. In the past, the ingot was moved after it cooled down. However, in the present application, the temperature of the ingot dropped quickly during the continuous casting process, and it only took a short wait to move it away after the continuous casting was completed.
[0060] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit it. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present application.
Claims
1. A crystallizer with rapid cooling function, characterized in that: It includes a main body, and the main body is formed with a continuous casting cavity, a cooling cavity and a water inlet; the continuous casting cavity runs through the top and bottom of the main body along its height direction, the cooling cavity surrounds the outer circumference of the continuous casting cavity and is spaced apart from the continuous casting cavity, and a spray port connecting the cooling cavity and the continuous casting cavity is formed at the lower part of the side wall between the two; the water inlet is connected to the cooling cavity.
2. The crystallizer with rapid cooling function according to claim 1, characterized in that: The crystallizer with rapid cooling function further comprises a partition plate, which is arranged in the cooling cavity and along the direction from the cooling cavity to the continuous casting cavity, and the partition plate divides the cooling cavity into an outer cooling cavity and an inner cooling cavity; The partition plate is formed with a first port, and along the height direction of the cooling cavity, one of the first port and the water inlet is close to the top end of the cooling cavity, and the other is arranged close to the bottom end of the cooling cavity.
3. The crystallizer with rapid cooling function according to claim 2, characterized in that: The water inlet is arranged on the outer side of the main body close to the bottom end thereof; the first outlet is arranged at a position of the partition plate close to the top end thereof.
4. The crystallizer with rapid cooling function according to claim 1, characterized in that: The number of the spray ports is multiple and they are arranged in an array along the height direction of the body and the periphery of the body.
5. The crystallizer with rapid cooling function according to claim 4, characterized in that: Along the height direction of the main body, two adjacent rows of spray ports are staggered.
6. The crystallizer with rapid cooling function according to claim 4, characterized in that: The plurality of spray ports are distributed from the lower portion of the body to the bottom of the body to form a spray area.
7. The crystallizer with rapid cooling function according to claim 6, characterized in that: The cross section of the continuous casting cavity along its height direction is circular, and the inner diameter of the spraying zone of the continuous casting cavity is larger than the inner diameter of other positions of the continuous casting cavity.
8. The crystallizer with rapid cooling function according to claim 1, characterized in that: The body comprises an inner ring portion and an outer ring portion, wherein the outer ring portion is sleeved outside the inner ring portion and connected to the inner ring portion, and the cooling cavity is formed between the inner ring portion and the outer ring portion; The crystallizer with rapid cooling function also includes a dynamic seal and a dummy rod; wherein the dynamic seal is movably arranged in the continuous casting cavity, and the outer side wall of the dynamic seal is against the inner wall of the continuous casting cavity; the dummy rod is arranged below the dynamic seal, and the dummy rod is connected to the bottom of the dynamic seal.
9. A vertical continuous casting system, characterized in that: It comprises an insulation bag and a crystallizer with rapid cooling function as described in any one of claims 1 to 8; wherein the insulation bag is arranged on the top of the body of the crystallizer with rapid cooling function, and a second port connected to the interior thereof is formed at the bottom of the insulation bag, and the second port is connected to the opening at the top of the continuous casting cavity.
10. The vertical continuous casting system according to claim 9, characterized in that: The insulation bag comprises a crucible, insulation cotton and a heating device; wherein the insulation cotton is wrapped around the outer wall of the crucible, and the heating device is arranged on a side of the insulation cotton away from the crucible and is used to heat the crucible.
Citation Information
Cited By
Safe deep well casting device for aluminum alloy pipe
CN120095112A
A deep well casting device for safe aluminum alloy pipes
CN120095112B