Hot pressing sintering mold
By designing a hot press sintering mold, the pressure head assembly and core in the mold cavity are used to form an adaptive product cavity, the problem of microcracks introduced in the hot press sintered cylindrical blank is solved, and the ceramic pump impeller is realized Efficient direct molding and complex shape processing improve dynamic service performance and reduce costs.
Patent Information
- Application Number
- CN202420502474.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-14
- Publication Date
- 2024-12-06
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
When using hot-pressed sintered cylindrical blank to prepare pump impellers in combination with large amounts of machine processing, due to the complex shape and the high hardness and low toughness of ceramic materials, a large number of microcracks are easily introduced, reducing the dynamic service performance of ceramic pump impellers.
A hot press sintering mold is designed, by providing a first indentation head assembly and a second indentation head assembly at both ends of the mold cavity, and a core part is provided inside the mold cavity, so that the side wall of the core part and the indentation head assembly are formed. The product cavity that is suitable for the shape of the product can be directly formed by hot pressing and sintering to avoid microcracks caused by subsequent machining.
By directly forming products with the desired shape, the surface microcracks caused by machining are reduced, the dynamic service performance and shape complexity of the ceramic pump impeller are improved, and the subsequent processing costs are reduced.
Smart Images

Figure CN222115451U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of powder sintering, in particular to a hot pressing sintering die. Background Art
[0002] Nuclear energy is an important energy source to promote social development. After continuous research and development, the fourth-generation nuclear reactor has higher safety and energy conversion efficiency than the third-generation nuclear reactor, but at the same time, it also has higher requirements for the internal structural materials of the fourth-generation reactor. The internal structural materials of the fourth-generation reactor need to withstand higher temperatures and neutron irradiation, as well as strong corrosion caused by coolants. Ceramic materials have become an important candidate structural material for the fourth-generation reactor due to their excellent high-temperature mechanical properties, radiation resistance, corrosion resistance and chemical stability. As one of the structural components of the fourth-generation reactor, the surface of the pump impeller needs to be intact to withstand the erosion of high-velocity corrosive media. However, when the pump impeller is prepared by hot-pressing sintering cylindrical blanks combined with a large amount of machining, due to the complex impeller shape and the high hardness and low toughness characteristics of ceramic materials, a large number of microcracks are easily introduced during the large-scale machining process, making the blades prone to breakage, thereby reducing the dynamic service performance of the ceramic pump impeller. Utility Model Content
[0003] In view of this, the utility model provides a hot pressing and sintering die to solve the problem that a large number of micro cracks are easily introduced when a large number of machining operations are performed on a hot pressing and sintering cylindrical blank.
[0004] The utility model provides a hot pressing sintering mold, comprising:
[0005] The mold body has a mold cavity, and the mold cavity is cylindrical;
[0006] The first pressing head assembly and the second pressing head assembly are respectively arranged at two ends of the mold cavity along the axial direction, and a cavity is formed between the first pressing head assembly and the second pressing head assembly;
[0007] The core is arranged in the mold cavity and abuts against the first press head assembly and the second press head assembly. At least a part of the core passes through the cavity and has a reserved cavity that overlaps with the cavity part, so that a product cavity is formed between the side wall of the core and the first press head assembly and the second press head assembly.
[0008] Beneficial effect: By respectively arranging the first press head assembly and the second press head assembly at both ends of the mold cavity and arranging the core part inside the mold cavity, a product cavity adapted to the shape of the product is formed between the side wall of the core part and the first press head assembly and the second press head assembly, so that the product with the desired shape is directly formed by hot pressing and sintering, avoiding the subsequent large-scale machining of the product to cause micro cracks on the product surface.
[0009] In an optional embodiment, the product cavity is a multi-tooth cavity, and further includes: a center rod, which is arranged in the mold cavity and abuts against the first press head assembly and the second press head assembly, and at least a part of the center rod passes through the reserved cavity.
[0010] In an optional embodiment, the first ram assembly includes a first ram extending parallel to the axial direction of the mold cavity, and the second ram assembly includes a second ram extending parallel to the axial direction of the mold cavity; the first ram and the second ram are correspondingly provided with a plurality of spaced grooves extending parallel to the axial direction of the mold cavity, the extension direction of the core is parallel to the extension direction of the grooves, and is located in the grooves, and along a direction perpendicular to the axial direction of the mold cavity, the cross-sectional shape of the plurality of grooves is adapted to the cross-sectional shape of the core; the end faces of the first ram and the second ram close to each other respectively have a first groove and a second groove formed by local depressions, and the first groove, the second groove, the side wall of the center rod and the inner side wall of the core form a product cavity.
[0011] Beneficial effect: By opening grooves on the first pressure head and the second pressure head, and by respectively arranging the first groove and the second pressure head, so as to form a product cavity with a complex shape with the side wall of the center rod and the inner wall of the core, a product with a complex shape can be directly formed, which is beneficial to reduce surface microcracks caused by machining the product.
[0012] In an optional embodiment, a plurality of grooves are radially distributed around the axis of the mold cavity, and the width of the grooves gradually increases along the radial direction of the mold cavity, so that the product cavity has a plurality of wing-shaped cavities.
[0013] In an optional embodiment, mounting holes are correspondingly provided in the middle regions of the first pressing head and the second pressing head, the axis of the mounting hole coincides with the axis of the mold cavity, and the diameter of the mounting hole matches the diameter of the center rod.
[0014] In an optional embodiment, a local area of the outer peripheral wall of the center rod protrudes to form a limit block, and the extension direction of the limit block is parallel to the axial direction of the mold cavity; the side wall of the mounting hole is recessed to form a limit groove corresponding to the position of the limit block.
[0015] Beneficial effect: A limiting block is protruded on the center rod, and a limiting groove is set at a corresponding position on the side wall of the mounting hole. The limiting groove abuts against the limiting block to facilitate limiting the relative angle between the center rod and the first pressing head and the second pressing head, so that the grooves on the first pressing head and the second pressing head correspond to each other, which is beneficial to the assembly of the hot pressing sintering mold.
[0016] In an optional embodiment, the first ram assembly also includes a first end cover fixedly connected to a side of the first ram away from the second ram; the second ram assembly also includes a second end cover fixedly connected to a side of the second ram away from the first ram, and the first end cover and the second end cover are respectively abutted against the two ends of the mold body to be suitable for sealing the two end openings of the mold cavity.
[0017] Beneficial effect: The two ends of the mold cavity are blocked by the first end cover and the second end cover to prevent the core or the center rod from leaving the mold cavity along the axial direction of the mold cavity, and the first pressure head and the second pressure head can be pressurized through the first end cover and the second end cover.
[0018] In an optional embodiment, the first ram includes a first ram body and a first gasket that are abutted against each other, the first gasket is located on a side of the first ram body facing the second ram assembly, and a local area of the end surface of the first gasket facing away from the first ram body is recessed to form a first groove.
[0019] Beneficial effect: By setting the first gasket and setting the first groove on the first gasket, when the dimensional accuracy of the first groove is greatly lost, only the first gasket needs to be replaced, and there is no need to replace the entire first pressure head, thereby reducing waste and reducing costs.
[0020] In an optional embodiment, there are multiple first grooves, and the multiple first grooves are radially distributed around the axis of the mold cavity.
[0021] In an optional embodiment, the second ram includes a second ram body and a second gasket that are abutted against each other, the second gasket is located on a side of the second ram body facing the first ram assembly, and the middle area of the end surface of the second gasket facing away from the second ram body is recessed to form a second groove.
[0022] Beneficial effect: By setting the second gasket and setting the second groove on the second gasket, when the dimensional accuracy of the second groove is greatly lost, only the second gasket needs to be replaced without replacing the entire second pressure head, thereby reducing waste and reducing costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] In order to more clearly illustrate the specific implementation methods of the utility model or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0024] Figure 1 It is a three-dimensional schematic diagram of the hot pressing sintering mold of the utility model;
[0025] Figure 2 It is an exploded schematic diagram of the hot pressing sintering mold of the utility model;
[0026] Figure 3 It is a schematic diagram of the assembly of the first end cover and the first pressing head body of the utility model;
[0027] Figure 4 The three-dimensional schematic diagram of the first gasket of the utility model Figure 1 ;
[0028] Figure 5 The three-dimensional schematic diagram of the first gasket of the utility model Figure 2 ;
[0029] Figure 6 It is a three-dimensional schematic diagram of the core of the utility model;
[0030] Figure 7 It is a three-dimensional schematic diagram of the central rod of the utility model;
[0031] Figure 8 It is a three-dimensional schematic diagram of the mold body of the utility model;
[0032] Fig. 9 A three-dimensional schematic diagram of the utility model product Figure 1 ;
[0033] Fig.10 A three-dimensional schematic diagram of the utility model product Figure 2 ;
[0034] Fig.11 The three-dimensional schematic diagram of the second gasket of the utility model Figure 1 ;
[0035] Fig.12 The three-dimensional schematic diagram of the second gasket of the utility model Figure 2 ;
[0036] Fig.13 It is a three-dimensional schematic diagram of the second end cover and the second pressure head body of the utility model.
[0037] Description of reference numerals:
[0038] 1. First ram assembly; 11. First ram; 111. First ram body; 112. First gasket; 1121. First groove; 12. First end cover; 2. Second ram assembly; 21. Second ram; 211. Second ram body; 212. Second gasket; 2121. Second groove; 22. Second end cover; 3. Mold body; 31. Mold cavity; 4. Core; 5. Center rod; 6. Product; 61. First protrusion; 62. Second protrusion; 7. Channel; 8. Mounting hole; 9. Limit block; 10. Limit groove. DETAILED DESCRIPTION
[0039] In order to make the purpose, technical solution and advantages of the embodiment of the utility model clearer, the technical solution in the embodiment of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiment of the utility model. Obviously, the described embodiment is a part of the embodiment of the utility model, not all the embodiments. Based on the embodiment of the utility model, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the utility model.
[0040] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0041] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installation", "connection" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0042] In addition, the technical features involved in the different embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0043] Nuclear energy plays a vital role in alleviating the world's growing energy demand. The fourth-generation nuclear reactor has higher safety and energy conversion efficiency than the third-generation nuclear reactor, but at the same time, it also has higher requirements for the long-term stable service performance of the internal structural materials such as fuel cladding tubes and pump impellers in extreme environments. The internal structural materials of the fourth-generation reactor need to be able to withstand higher temperatures and neutron irradiation, as well as the strong corrosion caused by the coolant. Ceramic materials have become an important candidate structural material for the internal structure of the fourth-generation reactor due to their excellent high-temperature mechanical properties, radiation resistance, corrosion resistance and chemical stability. As one of the structural components of the fourth-generation reactor, the pump impeller achieves efficient transmission of fluids through large size and high-precision design of complex-shaped blades. The impeller surface needs to be intact to withstand the erosion of high-velocity corrosive media. In the related technology, gel injection molding combined with pressureless sintering is used to prepare ceramic pump impellers. This preparation method has strict requirements on slurry ratio, casting molding and sintering conditions, and the preparation process is complicated. When hot pressing and sintering cylindrical blanks are combined with a large amount of machining, the complex impeller shape and the high hardness and low toughness characteristics of ceramic materials lead to the introduction of a large number of microcracks during the machining process, which makes the blades easy to break and reduces the dynamic service performance of the ceramic pump impeller.
[0044] Combine the following Figures 1 to 13 , describing an embodiment of the utility model.
[0045] According to an embodiment of the present utility model, a hot pressing sintering mold is provided, taking the powder material filled into the mold as ceramic powder as an example, comprising:
[0046] The mold body 3 has a mold cavity 31, and the mold cavity 31 is cylindrical;
[0047] The first pressing head assembly 1 and the second pressing head assembly 2 are respectively arranged at two ends of the mold cavity 31 along the axial direction, and a cavity is formed between the first pressing head assembly 1 and the second pressing head assembly 2;
[0048] The core 4 is arranged in the mold cavity 31 and abuts against the first punch assembly 1 and the second punch assembly 2. At least a part of the core 4 passes through the cavity and has a reserved cavity that overlaps with the cavity part, so that a product cavity is formed between the side wall of the core 4 and the first punch assembly 1 and the second punch assembly 2.
[0049] The hot pressing and sintering mold provided in this embodiment is configured by respectively arranging a first punch assembly 1 and a second punch assembly 2 at both ends of the mold cavity 31, and arranging a core 4 inside the mold cavity 31, so that a product cavity adapted to the shape of the product 6 is formed between the side wall of the core 4 and the first punch assembly 1 and the second punch assembly 2, thereby directly forming a product 6 with a desired shape through hot pressing and sintering, avoiding the subsequent large-scale machining of the product that may cause micro cracks on the surface of the product 6.
[0050] Specifically, the mold body 3 has a cylindrical mold cavity 31 inside, and the mold cavity 31 passes through the mold body 3 and forms an opening on the mold body 3. Partial areas of the first ram assembly 1 and the second ram assembly 2 extend into the mold cavity 31 along the axial direction of the mold cavity 31 through the two end openings of the mold cavity 31, and there is a distance between the first ram assembly 1 and the second ram assembly 2, so that a cavity is formed between the end faces of the first ram assembly 1 and the second ram assembly 2 that are close to each other and the inner wall of the mold cavity 31. The core 4 is located inside the mold cavity 31, and its reserved cavity overlaps with the cavity part, so that a product cavity is formed between the inner side wall of the core 4, the end faces of the first ram assembly 1 and the second ram assembly 2 that are close to each other, and the inner wall of the mold cavity 31.
[0051] In some embodiments, in combination Figures 1 to 13 As shown, the product cavity is a multi-tooth cavity, and also includes: a center rod 5, which is arranged in the mold cavity 31 and abuts against the first press head assembly 1 and the second press head assembly 2, and at least a part of the center rod 5 passes through the reserved cavity.
[0052] Specifically, the reserved cavity of the core 4 and the part where the cavity overlaps are multi-tooth cavities, the center line of the multi-tooth cavity overlaps with the axis of the mold cavity 31, and the axis of the center rod 5 overlaps with the axis of the mold cavity 31, and at least part of the center rod 5 passes through the reserved cavity, so as to further limit the product cavity, so that a hole is formed in the middle of the product 6. Of course, the reserved cavity of the core 4 can also be set to other shapes according to actual needs, such as pentagons, hexagons, etc.
[0053] In some embodiments, in combination Figures 1 to 13 As shown, the first ram assembly 1 includes a first ram 11 extending in parallel with the axial direction of the cavity 31, and the second ram assembly 2 includes a second ram 21 extending in parallel with the axial direction of the cavity 31; the first ram 11 and the second ram 21 are correspondingly provided with a plurality of spaced grooves 7 extending in parallel with the axial direction of the cavity 31, the extension direction of the core 4 is parallel to the extension direction of the groove 7, and is located in the groove 7, and along the direction perpendicular to the axial direction of the cavity 31, the cross-sectional shape of the plurality of grooves 7 is adapted to the cross-sectional shape of the core 4; the end faces of the first ram 11 and the second ram 21 close to each other respectively have a first groove 1121 and a second groove 2121 formed by local depressions, and the first groove 1121, the second groove 2121, the side wall of the center rod 5 and the inner wall of the core 4 form a product cavity. Of course, another product cavity can be formed in the first groove 1121, the second groove 2121, the side wall of the center rod 5 and the outer wall of the core 4, or a third product cavity can be formed in the first groove 1121, the second groove 2121, the side wall of the center rod 5 and the outer and inner walls of the core 4.
[0054] The hot pressing sintering mold provided in this embodiment forms a product cavity with a complex shape with the side wall of the center rod 5 and the inner wall of the core 4 by opening a groove 7 on the first press head 11 and the second press head 21, and respectively arranging a first groove 1121 and a second groove 2121 on the first press head 11 and the second press head 21, so as to directly form a product with a complex shape, which is beneficial to reduce surface microcracks caused by machining the product.
[0055] In some embodiments, in combination Figures 1 to 13 As shown, a plurality of grooves 7 are radially distributed around the axis of the mold cavity 31 , and along the radial direction of the mold cavity 31 , the width of the grooves 7 gradually increases, so that the product cavity has a plurality of wing-shaped cavities.
[0056] Specifically, taking the preparation of a pump impeller as an example, along the radial direction of the mold cavity 31, the width of the groove 7 gradually increases to form a fan shape, and the groove 7 forms openings on the outer peripheral walls of the first ram 11 and the second ram 21, respectively, and the outer side walls of the first ram 11 and the second ram 21 parallel to the axial centerline of the mold cavity 31 abut against the inner peripheral wall of the mold cavity 31, so that the first ram 11 and the second ram 21 have multiple fins. The core 4 includes a plurality of spaced-apart fan-shaped portions, which can be produced separately, thereby reducing the production difficulty of the core 4. A reserved cavity is formed between the inner side walls of the plurality of fan-shaped portions, and the number of fan-shaped portions is adapted to the number of the grooves 7, so that each groove 7 is provided with a fan-shaped portion, and these fan-shaped portions can be installed or removed separately, thereby facilitating the assembly or disassembly of the mold. Along the radial direction of the mold cavity 31, the size of the groove 7 is adapted to the size of the fan-shaped portion, so that the first ram 11 and the second ram 21 can limit the core 4 in a direction perpendicular to the axial centerline of the mold cavity 31, and form a product cavity with multiple wing-shaped cavities between the inner side wall of the core 4 and the first ram assembly 1 and the second ram assembly 2, wherein the wing-shaped cavities are suitable for forming wing-shaped blades of a pump impeller.
[0057] In some embodiments, in combination Figures 1 to 13 As shown, the middle regions of the first pressing head 11 and the second pressing head 21 are correspondingly provided with mounting holes 8 , the axis of the mounting hole 8 coincides with the axis of the mold cavity 31 , and the diameter of the mounting hole 8 matches the diameter of the center rod 5 .
[0058] Specifically, the inner peripheral wall of the mounting hole 8 abuts against the outer peripheral wall of the center rod 5 to fix the center rod 5. The center rod 5 further restricts the product cavity to form a hole in the middle of the product 6. By changing the diameter of the mounting hole 8 and the center rod 5 matched therewith, the diameter of the hole in the middle of the product 6 can be adjusted. Therefore, by replacing the first pressing head 11 and the second pressing head 21 with different mounting hole 8 diameters and the center rod 5 matched with the mounting hole 8 diameter, products 6 of different specifications can be prepared, which is conducive to increasing the applicability of the hot pressing sintering mold.
[0059] In some embodiments, in combination Figures 1 to 13 As shown, a local area of the outer peripheral wall of the center rod 5 protrudes to form a limit block 9, and the extension direction of the limit block 9 is parallel to the axial direction of the mold cavity 31; the side wall of the mounting hole 8 is recessed corresponding to the position of the limit block 9 to form a limit groove 10.
[0060] The hot pressing and sintering mold provided in this embodiment has a limiting block 9 protruding from the center rod 5, and a limiting groove 10 is provided at a corresponding position on the side wall of the mounting hole 8. The limiting groove 10 abuts against the limiting block 9 to facilitate limiting the relative angle between the center rod 5 and the first pressing head 11 and the second pressing head 21, so that the grooves 7 on the first pressing head 11 and the second pressing head 21 correspond to each other, which is beneficial to the assembly of the hot pressing and sintering mold.
[0061] Specifically, the limit block 9 is located in the limit groove 10, and the side wall of the limit block 9 abuts against the inner wall of the limit groove 10 to limit the relative angle between the center rod 5 and the first press head 11 and the second press head 21. When the first press head 11 and the second press head 21 are installed on the mold body 3, it is beneficial to ensure that the grooves 7 on the first press head 11 and the second press head 21 correspond to each other, thereby improving the assembly efficiency.
[0062] In some embodiments, in combination Figures 1 to 13 As shown, the first ram assembly 1 also includes a first end cover 12 fixedly connected to a side of the first ram 11 away from the second ram 21; the second ram assembly 2 also includes a second end cover 22 fixedly connected to a side of the second ram 21 away from the first ram 11, and the first end cover 12 and the second end cover 22 are respectively abutted against the two ends of the mold body 3 to be suitable for sealing the two end openings of the mold cavity 31.
[0063] The hot pressing sintering mold provided in this embodiment blocks the two ends of the mold cavity 31 through the first end cover 12 and the second end cover 22 to prevent the core 4 or the center rod 5 from escaping from the mold cavity 31 along the axial direction of the mold cavity 31, and can facilitate pressurization of the first pressure head 11 and the second pressure head 21 through the first end cover 12 and the second end cover 22.
[0064] Specifically, the groove 7 and the mounting hole 8 pass through the first ram 11 and the second ram 21 respectively, and the planes where the first end cover 12 and the second end cover 22 are located are perpendicular to the axial centerline of the mold cavity 31. Along the axial centerline direction of the mold cavity 31, the projections of the first end cover 12 and the second end cover 22 respectively cover the openings at both ends of the mold cavity 31 on the mold body 3, and the first end cover 12 and the second end cover 22 respectively abut against the two end surfaces of the mold body 3, so as to block the through openings formed by the groove 7 and the mounting hole 8 at the end surfaces of the first ram 11 and the second ram 21 that are away from each other, thereby preventing the core 4 and the center rod 5 from detaching from the mold body 3 at the openings at both ends of the mold body 3, and when the hot pressing and sintering mold is pressurized, it is convenient to pressurize the hot pressing and sintering mold along the axial direction of the mold cavity 31 through the first end cover 12 and / or the second end cover 22.
[0065] In some embodiments, in combination Figures 1 to 13 As shown, the first ram 11 includes a first ram body 111 and a first gasket 112 that are abutted against each other. The first gasket 112 is located on the side of the first ram body 111 facing the second ram assembly 2. The end surface of the first gasket 112 facing away from the first ram body 111 is partially recessed to form a first groove 1121.
[0066] The hot pressing sintering mold provided in this embodiment sets a first gasket 112 and sets a first groove 1121 on the first gasket 112, so that when the dimensional accuracy of the first groove 1121 is greatly lost, only the first gasket 112 needs to be replaced, and there is no need to replace the entire first pressing head 11, thereby reducing waste and reducing costs.
[0067] Specifically, along the axial direction perpendicular to the mold cavity 31, the cross-sectional shapes of the first ram body 111 and the first gasket 112 are the same. The first groove 1121 is suitable for forming the first bump 61 of the product 6 after hot pressing and sintering. Due to the complex shape of the finished ceramic product, some precision will be lost at the contact between the mold and the finished ceramic product after demolding. Only the first gasket 112 needs to be replaced, and there is no need to replace the first ram 11 as a whole, which is conducive to reducing waste and reducing costs.
[0068] In some embodiments, in combination Figures 1 to 13 As shown, there are multiple first grooves 1121 , and the multiple first grooves 1121 are radially distributed around the axis of the mold cavity 31 .
[0069] Specifically, the first grooves 1121 are wing-shaped and radially distributed around the axis of the mold cavity 31, and a first groove 1121 is provided between each two adjacent grooves 7 on the first gasket 112. Preferably, when assembling the hot pressing and sintering mold, the first pressing head assembly 1 is arranged below the second pressing head assembly 2 in the direction of gravity, so that the opening of the first groove 1121 faces upward, so as to achieve dense filling when filling the powder material. By replacing the first gasket 112 with first grooves 1121 of different specifications, it is convenient to produce products 6 of different specifications, which is conducive to improving the applicability of the hot pressing and sintering mold and reducing costs.
[0070] In some embodiments, in combination Figures 1 to 13 As shown, the second ram 21 includes a second ram body 211 and a second gasket 212 that are in contact with each other. The second gasket 212 is located on the side of the second ram body 211 facing the first ram assembly 1. The middle area of the end surface of the second gasket 212 facing away from the second ram body 211 is recessed to form a second groove 2121.
[0071] The hot pressing sintering mold provided in this embodiment sets a second gasket 212, and sets the second groove 2121 on the second gasket 212, so that when the dimensional accuracy of the second groove 2121 is greatly lost, only the second gasket 212 needs to be replaced, and there is no need to replace the entire second pressure head 21, thereby reducing waste and reducing costs.
[0072] Specifically, along the axis direction perpendicular to the cavity 31, the cross-sectional shape of the second ram body 211 and the second gasket 212 is the same. The second groove 2121 is a cylindrical groove, the axis of the second groove 2121 coincides with the axis of the mounting hole 8, and the diameter of the second groove 2121 is greater than the diameter of the mounting hole 8, the depth of the second groove 2121 is less than the thickness of the second gasket 212, and the second groove 2121 and the outer peripheral wall of the center rod 5 are suitable for forming the second protrusion 62 of the product 6 after hot pressing and sintering. By replacing the second gasket 212 with the second groove 2121 of different specifications, it is convenient to produce the product 6 with the second protrusion 62 of different specifications, which is conducive to improving the applicability of the hot pressing and sintering mold, and because the shape of the product 6 is complex, the contact between the mold and the product 6 will lose some precision after demolding, only the second gasket 212 is replaced, and there is no need to replace the second ram 21 as a whole, which is conducive to reducing waste and reducing costs.
[0073] As a feasible implementation form, firstly, the first ram body 111 fixedly connected to the first end cover 12 is inserted into the mold cavity 31 of the mold body 3 along the axial direction, and then the multiple fan-shaped parts of the core 4 are respectively inserted into the groove 7, and then the center rod 5 is inserted into the mounting hole 8 of the first ram body 111, and at the same time, the limit block 9 is located in the limit groove 10; the limit groove 10 of the first gasket 112 corresponds to the limit block 9 of the center rod 5 and is placed in the mold cavity 31, and the end surface of the first gasket 112 away from the first groove 1121 is aligned with the first ram body 31. The first and second ram bodies 211 and 212 are in contact with each other; the ceramic powder is filled; the limiting groove 10 of the second gasket 212 corresponds to the limiting block 9 of the center rod 5 and is placed in the mold cavity 31, and the end face of the second gasket 212 with the second groove 2121 faces the first gasket 112; the second pressure head body 211 fixedly connected to the second end cover 22 is inserted into the mold cavity 31 of the mold body 3 along the axial direction; the hot pressing and sintering mold is uniaxially pressurized along the axial centerline direction of the mold cavity 31, so that a large-sized and complex-shaped impeller that meets the use requirements can be directly formed during hot pressing and sintering.
[0074] Obviously, the above embodiments are only examples for clear explanation, and are not intended to limit the implementation methods. Although the embodiments of the present utility model are described in conjunction with the accompanying drawings, those skilled in the art may make various modifications and variations without departing from the spirit and scope of the present utility model, and such modifications and variations are all within the scope defined by the present utility model.
Claims
1. A hot pressing sintering mold, characterized in that: include: The mold body (3) has a mold cavity (31), and the mold cavity (31) is cylindrical; A first pressing head assembly (1) and a second pressing head assembly (2) are respectively arranged at two ends of the mold cavity (31) along the axial direction, and a cavity is formed between the first pressing head assembly (1) and the second pressing head assembly (2); A core (4) is arranged in the mold cavity (31) and abuts against the first press head assembly (1) and the second press head assembly (2). At least a part of the core (4) passes through the cavity and has a reserved cavity that overlaps with the cavity part, so that a product cavity is formed between the side wall of the core (4) and the first press head assembly (1) and the second press head assembly (2).
2. The hot pressing sintering mold according to claim 1, characterized in that: The product cavity is a multi-tooth cavity and further comprises: a center rod (5) which is arranged in the mold cavity (31) and abuts against the first press head assembly (1) and the second press head assembly (2), and at least a part of the center rod (5) passes through the reserved cavity.
3. The hot pressing sintering mold according to claim 2, characterized in that: The first pressing head assembly (1) comprises a first pressing head (11) extending in parallel with the axial centerline direction of the mold cavity (31), and the second pressing head assembly (2) comprises a second pressing head (21) extending in parallel with the axial centerline direction of the mold cavity (31); the first pressing head (11) and the second pressing head (21) are respectively provided with a plurality of slots (7) extending in parallel with the axial centerline direction of the mold cavity (31), and the core (4) extends in parallel with the extension direction of the slots (7) and is located in the slots. The grooves (7) are arranged in a direction perpendicular to the axial centerline of the mold cavity (31), and the cross-sectional shape of the plurality of grooves (7) is adapted to the cross-sectional shape of the core (4); the end surfaces of the first pressing head (11) and the second pressing head (21) close to each other respectively have a first groove (1121) and a second groove (2121) formed by local depressions; the first groove (1121), the second groove (2121), the side wall of the center rod (5) and the inner side wall of the core (4) form the product mold cavity.
4. The hot pressing sintering mold according to claim 3, characterized in that: The plurality of grooves (7) are radially distributed around the axis of the mold cavity (31), and along the radial direction of the mold cavity (31), the width of the grooves (7) gradually increases, so that the product mold cavity has a plurality of wing-shaped mold cavities.
5. The hot pressing sintering mold according to claim 3, characterized in that: Mounting holes (8) are correspondingly arranged in the middle regions of the first pressing head (11) and the second pressing head (21); the axis of the mounting hole (8) coincides with the axis of the mold cavity (31); and the diameter of the mounting hole (8) matches the diameter of the center rod (5).
6. The hot pressing sintering mold according to claim 5, characterized in that: A local area of the outer peripheral wall of the center rod (5) protrudes to form a limit block (9), and the extension direction of the limit block (9) is parallel to the axial centerline direction of the mold cavity (31); the side wall of the mounting hole (8) is recessed corresponding to the position of the limit block (9) to form a limit groove (10).
7. The hot pressing sintering mold according to claim 3, characterized in that: The first pressing head assembly (1) further comprises a first end cover (12) fixedly connected to a side of the first pressing head (11) away from the second pressing head (21); the second pressing head assembly (2) further comprises a second end cover (22) fixedly connected to a side of the second pressing head (21) away from the first pressing head (11), the first end cover (12) and the second end cover (22) respectively abut against two ends of the mold body (3) so as to be suitable for sealing the two end openings of the mold cavity (31).
8. The hot pressing sintering mold according to any one of claims 3 to 7, characterized in that: The first pressing head (11) comprises a first pressing head body (111) and a first gasket (112) which are in contact with each other, wherein the first gasket (112) is located on a side of the first pressing head body (111) facing the second pressing head assembly (2), and a local area of the end surface of the first gasket (112) facing away from the first pressing head body (111) is recessed to form the first groove (1121).
9. The hot pressing sintering mold according to claim 8, characterized in that: There are a plurality of the first grooves (1121), and the plurality of the first grooves (1121) are radially distributed around the axis of the mold cavity (31).
10. The hot pressing sintering mold according to claim 8, characterized in that: The second pressing head (21) comprises a second pressing head body (211) and a second gasket (212) which are in contact with each other, wherein the second gasket (212) is located on a side of the second pressing head body (211) facing the first pressing head assembly (1), and the middle area of the end surface of the second gasket (212) facing away from the second pressing head body (211) is recessed to form the second groove (2121).