Butyl sealing adhesive tape for automobile
Through double-sided auxiliary layer protection and hand pressing roller structure, the problem of uneven stress on the adhesive surface during car body patching is solved, and the uniform stickiness and dust-free adhesive effect of the tape is achieved, avoiding bulging and Glue loss phenomenon.
Patent Information
- Application Number
- CN202420784051.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-16
- Publication Date
- 2025-01-17
- Estimated Expiration
- 2034-04-16
AI Technical Summary
During the car body application process, butyl tape is easily bulged or partially fall off due to uneven adhesion surface due to temperature changes.
The tape structure is protected by a double-sided auxiliary layer, combined with the hand pressing roller structure, to ensure that the glue surface and the attachment surface are evenly sticky, and the adhesive body is protected by a burr layer to avoid touch and dust pollution.
Effectively prevent the tape from being bulged and dissipated, ensure the adhesive effect, and achieve the effect of dust-free adhesive.
Smart Images

Figure CN222362065U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of butyl sealing tapes, and in particular relates to a butyl sealing tape for automobiles. Background Art
[0002] Butyl tape can be widely used in the fields of construction, automobile, shipbuilding, electronics, etc. for sealing and bonding, such as waterproof sealing of roofs, walls, carriages, hulls, etc., as well as bonding of metals, plastics, glass and other materials. In short, butyl tape is a high-performance, environmentally friendly sealing and bonding material with broad application prospects and market demand.
[0003] At present, most of the processes of applying butyl tape to automobile bodies are done by manual pressing. During the pressing process, there will be uneven force on the adhesive surface, and the part of the tape that is partially adhered will bulge or part of the tape will fall off due to temperature changes.
[0004] Therefore, the present application adopts a tape structure that can be protected by a double-sided auxiliary layer, which can effectively remove impurities and dust on the outside of the colloid, and at the same time cooperate with the hand to press the roller structure to evenly press the glue application process. This can improve the adhesion between the glue surface and the attachment surface, and it is not easy to bulge or fall off. At the same time, the adhesive layer structure at the tail of the colloid can facilitate the subsequent glue force without touching the colloid itself, ensuring that the glue body achieves the effect of dust-free glue. Summary of the invention
[0005] In order to achieve the above object, the technical solution of the utility model is as follows:
[0006] A butyl sealing tape for automobiles, comprising a colloid; an upper covering layer and a lower covering layer are attached to the upper and lower end surfaces of the colloid;
[0007] The upper covering layer is a double-layer structure, and the upper covering layer is composed of a main covering film and a secondary covering film. The main covering film has a main adhesive layer extending along the rear of the colloid, and the main adhesive layer is folded to be in a tightly attached state;
[0008] The main adhesive layer is provided with a secondary adhesive layer extending along the rear of the colloid, and the secondary adhesive layer is folded over to be in a tightly attached state;
[0009] A peeling film is provided on the back of the lower covering layer and extends behind the colloid, and the peeling film and the lower covering layer are in an integrated connection structure.
[0010] Furthermore, an extrusion roller is laterally attached to the main adhesive layer along the intersection of the rear end of the colloid.
[0011] Furthermore, two groups of guide strips are integrally connected to both sides of the main adhesive layer, and the inner end surfaces of the two groups of guide strips are in guiding contact with the squeezing roller.
[0012] Furthermore, the ends of the main covering film and the peeling film are integrally connected with pull rings.
[0013] Furthermore, the ends of the main adhesive layer and the secondary adhesive layer are integrally attached with a burr layer, and the main adhesive layer and the secondary adhesive layer are in a closed state of adhesion by the burr layer when not in use.
[0014] The beneficial effects of the utility model are:
[0015] Compared with the prior art, the present application adopts a tape structure that can be protected by a double-sided auxiliary layer, which can effectively remove impurities and dust on the outside of the colloid, and at the same time cooperate with the hand-pressing roller structure to evenly press the glue-sticking process. This can improve the adhesion between the glue surface and the attachment surface, and it is not easy to bulge or fall off. At the same time, the adhesive layer structure at the tail of the colloid can facilitate the subsequent application of glue without touching the colloid itself, ensuring that the glue body achieves the effect of dust-free glue. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 The utility model is a schematic diagram of the top view of the structure of a butyl sealing tape for automobiles.
[0017] Figure 2 The utility model is a schematic diagram of the structure of a butyl sealing tape for automobiles when viewed from above.
[0018] List of Figure Symbols:
[0019] 1 is an upper covering layer, 2 is a colloid, 3 is a lower covering layer, 4 is a guide strip, 5 is a primary adhesive layer, 6 is a primary coating, 7 is a secondary coating, 8 is a secondary adhesive layer, 9 is an extrusion roller, 10 is a pull ring, and 12 is a peeling film. DETAILED DESCRIPTION
[0020] The present invention will be further described below in conjunction with the accompanying drawings and specific implementations. It should be understood that the following specific implementations are only used to illustrate the present invention and are not used to limit the scope of the present invention.
[0021] like Figure 1 and Figure 2 As shown, a butyl sealing tape for automobiles includes a colloid; the upper and lower end surfaces of the colloid 2 are pasted with an upper covering layer 1 and a lower covering layer 3; wherein the upper and lower end surfaces of the colloid 2 are installed with two sets of covering layers, and the covering layers are used to protect the colloid 2 from dust and impurities when it is not in use. Moreover, the shape of the colloid 2 can be changed at any time when it is in use.
[0022] The upper covering layer 1 is a double-layer structure, and is composed of a main covering film 6 and a secondary covering film 7. The main covering film 6 has a main adhesive layer 5 extending behind the colloid 2, and the main adhesive layer 5 is folded to be in a close contact state; wherein, the main covering film 6 and the secondary covering film 7 are used as tearing film structures for subsequent operations, which are convenient for manual operation and complete the colloid covering without touching the colloid 2 itself. When in a state to be used, the upper covering layer 1 is in a folded state to avoid exposure and damage.
[0023] The main adhesive layer 5 is extended with a secondary adhesive layer 8 along the rear of the colloid 2, and the secondary adhesive layer 8 is folded and in a close contact state; wherein, similarly, the secondary adhesive layer 8 is the lower layer in the double-layer structure, and cooperates to complete the uniform rolling of the rubber surface without affecting the protective layer of the surface structure of the colloid 2. When in the state of being used, it is in a folded state to avoid being exposed and damaged.
[0024] A peeling film 12 is provided on the back of the lower cover layer 3 along the back of the colloid 2, and the peeling film 12 is integrally connected with the lower cover layer 3. The peeling film 12 is an anti-adhesive film on the back of the colloid 2. After being torn off, it can be used with the colloid 2 to complete the adhesive process.
[0025] like Figure 1 and Figure 2 As shown, the main adhesive layer 5 is laterally attached with an extrusion roller 9 along the intersection of the rear end of the colloid 2. The extrusion roller 9 can cooperate with manual rolling to complete the colloid 2 punching and adhesion process.
[0026] like Figure 1 and Figure 2 As shown, two sets of guide strips 4 are integrally connected to both sides of the main adhesive layer 5, and the inner end surfaces of the two sets of guide strips 4 are in guiding contact with the squeezing roller 9. The guide strips 4 serve as guides to prevent the squeezing roller 9 from shifting during the rolling process.
[0027] like Figure 1 and Figure 2 As shown, the ends of the main covering film 6 and the peeling film 12 are integrally connected with a pull ring 10. The main covering film 6 and the peeling film 12 can cooperate with the pull ring 10 to improve the operation experience.
[0028] like Figure 1 and Figure 2 As shown, the ends of the main adhesive layer 5 and the secondary adhesive layer 8 are integrally attached with a burr layer, and the main adhesive layer 5 and the secondary adhesive layer 8 are in a closed state of adhesion through the burr layer when not in use. The main adhesive layer 5 and the secondary adhesive layer 8 are attached to each other through the burr layer, which can play a protective role when not in use.
[0029] It should be noted that the above content only illustrates the technical idea of the utility model and cannot be used to limit the protection scope of the utility model. For ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the utility model. These improvements and modifications all fall within the protection scope of the claims of the utility model.
Claims
1. A butyl sealing tape for automobiles, comprising a colloid; wherein: The upper and lower end surfaces of the colloid (2) are adhered with an upper covering layer (1) and a lower covering layer (3); The upper covering layer (1) is of a double-layer structure, and the upper covering layer (1) is composed of a main covering film (6) and a secondary covering film (7), the main covering film (6) has a main adhesive layer (5) extending behind the colloid (2), and the main adhesive layer (5) is folded to be in a tightly attached state; The main adhesive layer (5) is provided with a secondary adhesive layer (8) extending along the rear of the colloid (2), and the secondary adhesive layer (8) is folded over to be in a tightly attached state; A layer of peeling film (12) is provided on the back side of the lower covering layer (3) and extends behind the colloid (2); the peeling film (12) and the lower covering layer (3) are in an integrated connection structure.
2. The butyl sealing tape for automobiles according to claim 1, characterized in that: The main adhesive layer (5) is laterally adhered with an extrusion roller (9) along the intersection of the rear end of the colloid (2).
3. The butyl sealing tape for automobiles according to claim 2, characterized in that: Two sets of guide strips (4) are integrally connected to both sides of the main adhesive layer (5), and the inner end surfaces of the two sets of guide strips (4) are in guiding contact with the squeezing roller (9).
4. The butyl sealing tape for automobiles according to claim 1, characterized in that: The ends of the main covering film (6) and the peeling film (12) are integrally connected with a pull ring (10).
5. The butyl sealing tape for automobiles according to claim 1, characterized in that: The ends of the main adhesive layer (5) and the secondary adhesive layer (8) are integrally attached with a burr layer, and the main adhesive layer (5) and the secondary adhesive layer (8) are in an attached closed state by the burr layer when not in use.