A ceramic artificial crystal optical surface processing structure for optical isolators
By combining a non-magnetic composite material base and a magnetically repulsive sliding fixing strip with a chemical mechanical polishing composite grinding head, the problems of crystal breakage and surface roughness in the optical surface processing of ceramic artificial crystals are solved, achieving efficient and precise nanoscale ultra-smooth surface processing, and improving the optical performance and reliability of optical isolators.
Patent Information
- Application Number
- CN202522303707.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-10-30
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2035-10-30
AI Technical Summary
In the current process of processing the optical surface of ceramic artificial crystals, design defects in the fixed structure and processing structure lead to high crystal breakage rate, uneven surface roughness, and low processing efficiency, making it difficult to meet the high precision requirements of optical isolators.
A non-magnetic composite material base is used in conjunction with a sliding fixing bar driven by magnetic repulsion. Combined with a buffer protrusion, it achieves elastic fixation of the crystal without rigid contact and chemical contamination. A chemical mechanical polishing composite grinding head is used, and through the combination of a porous graphite matrix, an elastic buffer layer and a central spray hole, the synergistic effect of chemical corrosion softening and mechanical fine grinding is achieved.
Significantly reduces crystal breakage rate to below 1%, stabilizes surface roughness at Ra≤0.03nm, improves processing efficiency by 20%-30%, adapts to magneto-optical and non-magneto-optical ceramic artificial crystals, and significantly improves the optical performance and reliability of optical isolators.
Smart Images

Figure CN224951637U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of artificial crystal processing technology, specifically to a processing structure for the optical surface of a ceramic artificial crystal for optical isolators. Background Technology
[0002] Ceramic artificial crystals for optical isolators are widely used in optical communication, laser equipment and other fields due to their high light transmittance, excellent magneto-optical properties and mechanical strength. The processing accuracy of their optical surfaces directly affects the insertion loss and isolation of the optical isolator. At present, the core challenges in processing the optical surfaces of ceramic artificial crystals are twofold: first, the crystal fixation must balance stability and non-damage; second, the optical surface processing must achieve a nanoscale ultra-smooth surface while ensuring processing uniformity.
[0003] However, in the current process of processing optical surfaces of ceramic artificial crystals, design flaws in the fixing and processing structures have become a key bottleneck restricting their performance improvement.
[0004] In the crystal fixing process, the existing structure has multiple drawbacks: First, traditional mechanical clamps, such as bolt tightening and chuck clamping, use rigid contact to fix the crystal. However, ceramic artificial crystals have the characteristics of high hardness and high brittleness. Rigid clamping is prone to local stress concentration, which can cause crystal edge cracking. Especially for thin crystals with a thickness of 1-3mm, the cracking rate can reach 10%-15%. At the same time, the contact point between the clamp and the crystal is prone to indentation, which can damage the optical surface processing benchmark. Secondly, some solutions use glue to fix the crystal. Although this can avoid rigid damage, glue residue will contaminate the crystal surface. The subsequent cleaning process may corrode the crystal or introduce scratches. In addition, the glue is easy to soften at the high temperature of processing, which will cause the crystal positioning to shift and affect the processing accuracy. Third, a few magnetic adsorption fixation structures rely on magnetic bases, while the magnetic domain structure of magneto-optical ceramics is easily affected by external magnetic fields, resulting in an increase in the Faraday rotation angle error after processing, which cannot meet the magneto-optical performance requirements of optical isolators.
[0005] In the optical surface processing stage, the limitations of existing processing structures are also significant: traditional single mechanical polishing can remove material quickly, but it relies on pure mechanical force and is prone to forming subsurface damage on the crystal surface, resulting in increased light scattering loss; although simple chemical etching can obtain a smooth surface, the etching rate is difficult to control precisely, and local over-etching or uneven etching is prone to occur, with flatness errors often exceeding 1μm / 25mm; some composite processing structures lack fitting compensation design, and the small gap between the grinding head and the crystal surface will lead to local missed polishing, and the polishing fluid cannot uniformly cover the processing area, resulting in large fluctuations in surface roughness and failure to consistently achieve ultra-smoothness requirements. In addition, existing fixing structures and processing structures are mostly designed independently, and the compatibility between the fixing method and the processing technology is poor, resulting in processing interruptions, low efficiency, and a yield rate that can only be maintained at 70%-80%.
[0006] To address the aforementioned issues, this application proposes a processing structure for the optical surface of ceramic artificial crystals used in optical isolators. By coordinating the design of the fixing and processing mechanisms, the shortcomings of existing technologies are fundamentally resolved. The structural design of this application not only reduces the crystal breakage rate to below 1% and stably controls the surface roughness to Ra≤0.03nm, but also improves processing efficiency through the synergy of fixing and processing. Furthermore, it is adaptable to the processing requirements of both magneto-optical and non-magneto-optical ceramic artificial crystals, significantly improving the optical performance and reliability of optical isolators, making them more practical. Utility Model Content
[0007] To address the shortcomings of existing technologies, this invention provides a processing structure for the optical surface of a ceramic artificial crystal for optical isolators. The fixing mechanism employs a non-magnetic composite material base combined with a sliding fixing strip driven by magnetic repulsion. This, along with a buffer protrusion, achieves elastic fixing of the crystal without rigid contact or chemical contamination, preventing crystal breakage and surface damage while also preventing interference from magnetic fields on magneto-optical properties. The processing mechanism utilizes a chemical mechanical polishing composite grinding head. Through the combination of a porous graphite matrix, an elastic buffer layer, and a central spray hole, it achieves a synergistic effect of "chemical corrosion softening" and "mechanical fine grinding," while ensuring high adhesion between the grinding head and the crystal surface, stably obtaining a nanoscale ultra-smooth surface, thus solving the aforementioned problems.
[0008] To achieve the above-mentioned objectives, this utility model provides the following technical solution: a processing structure for the optical surface of a ceramic artificial crystal for an optical isolator, comprising a base, a fixing component, and a processing component. The top of the base has a recessed processing groove, and the bottom of the inner wall of the processing groove has a slot. The fixing component is installed inside the processing groove by insertion through the slot. The fixing component includes a fixing seat, a groove, and a sliding clamping component. The fixing seat is entirely made of composite material, and the top of the fixing seat has a groove adapted to the ceramic artificial crystal. The groove has a sliding clamping component for fixing the crystal inside. The processing component includes a rotatable main grinding shaft, the end of the main grinding shaft has a composite grinding head assembly for polishing, and a spraying component for conveying polishing fluid is provided at the center of the main grinding shaft and the composite grinding head assembly.
[0009] Preferably, the sliding clamping assembly includes a side buffer strip, a guide groove, and a main slide bar. A side buffer strip is fixedly installed on one side of the inner wall of the groove, and guide grooves are provided on both sides of the inner wall of the groove. A main slide bar is slidably installed between the two sets of guide grooves.
[0010] Preferably, another set of side buffer bars is also fixedly installed on the side corresponding to the main slide bar and the side buffer bar, and the side buffer bars are all stepped.
[0011] Preferably, two sets of back magnets are fixedly installed on the back side of the main slide bar, and a permanent magnet is fixedly installed on the inner wall of the groove on the side corresponding to the back magnet. The back magnet and the permanent magnet are magnetically repelled. Both the back magnet and the permanent magnet are NdFeB permanent magnets with a magnetic field strength of 0.2-0.4T.
[0012] Preferably, the composite grinding head assembly includes a graphite disc, an elastic buffer layer, and diamond grinding blocks. The graphite disc is fixedly installed at the end of the main grinding shaft and is a porous graphite disc with a diameter of 60 mm and an air permeability of 15 μm / s. Several mounting grooves are evenly spaced on the graphite disc and uniformly opened on the side surface of the graphite disc facing the crystal. An elastic buffer layer is fixedly installed inside each mounting groove. A diamond grinding block is fixedly installed at the other end of the elastic buffer layer. The diamond grinding blocks are all fan-shaped and their surfaces are electroplated with diamond micro powder with a particle size of 0.1-0.3 μm.
[0013] Preferably, the spray assembly includes spray holes and a delivery pipe. The spray holes are opened along the central axis of the main grinding shaft and the graphite disk, and have a diameter of 4mm. The delivery pipe is a chemically resistant plastic hose, with one end connected to the spray holes and the other end connected to the outside. The polishing liquid delivered is CMP polishing liquid.
[0014] Compared with the prior art, this utility model provides a ceramic artificial crystal optical surface processing structure for optical isolators, which has the following beneficial effects: 1. The optical isolator uses a ceramic artificial crystal optical surface processing structure. The sliding clamping assembly includes a side buffer bar, a guide groove, a main slide bar, a back magnet, and a permanent magnet. The main slide bar slides through the guide groove. The magnetic repulsion between the back magnet and the permanent magnet pushes the main slide bar. Together with the stepped side buffer bars on both sides, the crystal is clamped. This can prevent the hard and brittle crystal from breaking through elastic contact, and can also provide a stable clamping force through magnetic repulsion to prevent the crystal from shifting during processing.
[0015] 2. The optical isolator uses a ceramic artificial crystal optical surface processing structure. The composite grinding head assembly includes a graphite disk, an elastic buffer layer, and diamond grinding blocks. The porous graphite disk provides efficient heat dissipation, and the elastic buffer layer ensures that the grinding blocks adhere to the crystal surface at a rate of ≥95%. The fine-grained diamond grinding blocks 13, combined with the chemical action of CMP polishing fluid, achieve nanoscale ultra-smooth surface processing while avoiding subsurface damage.
[0016] 3. The optical isolator uses a ceramic artificial crystal optical surface processing structure. The fixed component and the processing component are precisely aligned through the processing groove of the base. The non-magnetic composite material and magnetic repulsion design of the fixed component avoid interference with the performance of the magneto-optical crystal. The central spray and rotating grinding head of the processing component work together to improve the processing efficiency by 20%-30%, and it is compatible with different specifications of ceramic crystals, making it highly versatile. Attached Figure Description
[0017] Figure 1 This is a schematic diagram of the overall structure of this utility model; Figure 2 This is a schematic diagram of the fixing component structure of this utility model; Figure 3 This is a schematic diagram of the internal structure of the fixing component of this utility model; Figure 4 This is a schematic diagram of the composite grinding head assembly of this utility model.
[0018] In the diagram: 1. Base; 2. Machining groove; 3. Fixing seat; 4. Groove; 5. Main grinding shaft; 6. Side buffer strip; 7. Guide groove; 8. Main slide bar; 9. Back magnet; 10. Permanent magnet; 11. Graphite disk; 12. Elastic buffer layer; 13. Diamond grinding block; 14. Spray hole; 15. Conveying pipe. Detailed Implementation
[0019] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the protection scope of the present utility model.
[0020] Please see Figure 1-4 A processing structure for the optical surface of a ceramic artificial crystal used in optical isolators includes a base 1, a fixing component, and a processing component. The base 1 has a recessed processing groove 2 on its top, and a slot is formed at the bottom of the inner wall of the processing groove 2. The fixing component is installed inside the processing groove 2 via the slot. The fixing component includes a fixing seat 3, a groove 4, and a sliding clamping component. The fixing seat 3 is entirely made of composite material, and the top of the fixing seat 3 has a groove 4 adapted to the ceramic artificial crystal. The groove 4 contains a sliding clamping component for fixing the crystal. The processing component includes a rotatable main grinding shaft 5, with a composite grinding head assembly for polishing at its end. A spray component for conveying polishing fluid is located at the center of the main grinding shaft 5 and the composite grinding head assembly. Beneficial effects: The insertion and cooperation between the base 1 and the processing groove 2 achieves precise alignment of the fixing component and the processing component, ensuring the stability of the relative position of the crystal and the grinding head during processing, laying the foundation for high-precision processing.
[0021] Furthermore, the sliding clamping assembly includes a side buffer strip 6, a guide groove 7, and a main slide bar 8. The side buffer strip 6 is fixedly installed on one side of the inner wall of the groove 4, and guide grooves 7 are provided on both sides of the inner wall of the groove 4. The main slide bar 8 is slidably installed between the two sets of guide grooves 7. The guide groove 7 restricts the sliding direction of the main slide bar 8 to prevent the crystal from shifting during clamping. The side buffer strip 6 can buffer the clamping force to prevent the hard and brittle crystal from being damaged due to rigid contact.
[0022] Furthermore, another set of side buffer bars 6 is also fixedly installed on the side corresponding to the main slide bar 8 and the side buffer bar 6. The side buffer bars 6 are all stepped. The stepped side buffer bars 6 increase the contact area with the crystal, making the clamping force more uniform. At the same time, they can adapt to crystals of different thicknesses and improve the versatility of the structure.
[0023] Furthermore, two sets of back magnets 9 are fixedly installed on the back side of the main slide bar 8, and a permanent magnet 10 is fixedly installed on the inner wall of the groove 4 corresponding to the back magnet 9. The back magnet 9 and the permanent magnet 10 are magnetically repelled. Both the back magnet 9 and the permanent magnet 10 are NdFeB permanent magnets with a magnetic field strength of 0.2-0.4T. The magnetic repulsion provides a continuous and adjustable clamping force, avoiding stress concentration from mechanical clamping. At the same time, the non-contact force transmission can prevent crystal surface contamination and protect the cleanliness of the optical surface.
[0024] Furthermore, the composite grinding head assembly includes a graphite disk 11, an elastic buffer layer 12, and diamond grinding blocks 13. The graphite disk 11 is fixedly installed at the end of the main grinding shaft 5. It is a porous graphite disk with a diameter of 60 mm and an air permeability of 15 μm / s. Several mounting grooves are evenly spaced on the graphite disk 11, which are uniformly opened on the side surface of the graphite disk 11 facing the crystal. The elastic buffer layer 12 is fixedly installed inside each mounting groove. The diamond grinding blocks 13 are fixedly installed at the other end of the elastic buffer layer 12. The diamond grinding blocks 13 are all fan-shaped, and their surfaces are electroplated with diamond micro powder with a particle size of 0.1-0.3 μm. The porous graphite disk 11 has excellent heat dissipation, avoiding damage to the crystal caused by frictional heat during processing. The elastic buffer layer 12 ensures that the diamond grinding blocks 13 are in close contact with the crystal surface. With the help of fine-grained diamond micro powder, nanoscale smooth surface processing can be achieved.
[0025] Furthermore, the spray assembly includes spray holes 14 and a delivery pipe 15. The spray holes 14 are opened along the central axis of the main grinding shaft 5 and the graphite disk 11, with a diameter of 4mm. The delivery pipe 15 is a chemically resistant plastic hose, with one end connected to the spray holes 14 and the other end connected to the outside. The polishing fluid delivered is CMP polishing fluid. The central spray holes 14 make the polishing fluid evenly cover the processing area. The chemical action of the CMP polishing fluid and the mechanical grinding of the diamond grinding block 13 work together to soften the crystal surface and accurately remove the material, thereby improving processing efficiency and surface quality. Example
[0026] Example 1: The base 1 provides the installation foundation for the overall structure. The top processing groove 2 is fixedly installed with the mounting seat 3 through the slot. In the groove 4 of the mounting seat 3, the main slide bar 8 slides along the guide groove 7. The repulsive force between the back magnet 9 and the permanent magnet 10 pushes the main slide bar 8, so that the stepped side buffer bars 6 on both sides elastically clamp the ceramic crystal, ensuring that the crystal is free from indentation and cracking. During processing, the main grinding shaft 5 rotates at a speed of 200 rpm, driving the end graphite disk 11 to rotate synchronously. The 6 sets of fan-shaped diamond grinding blocks 13 on the graphite disk 11 are attached to the crystal surface through the elastic buffer layer 12. The central spray hole 14 delivers CMP polishing fluid through the delivery pipe 15 to achieve chemical softening and mechanical grinding synergy. Through the combination of magnetic repulsion clamping and elastic buffering, the crystal damage problem is completely solved. The high fit of the composite grinding head and the chemical mechanical action stably obtain an ultra-smooth surface with Ra≤0.03nm, which is suitable for high-precision optical isolator crystal processing.
[0027] Example 2: The processing groove 2 of the base 1 can be quickly replaced with a fixed seat 3 of different specifications through a slot, which can be adapted to ceramic crystals with a diameter of 5-20mm. In the fixing component, the back magnet 9 and the permanent magnet 10 can be adjusted to different sizes. By changing the repulsive force, they can be adapted to crystals of different thicknesses. The stepped structure of the side buffer strip 6 further improves the adaptability. In the processing component, the mounting groove of the graphite disk 11 can be replaced with diamond grinding blocks 13 of different grit sizes. The polishing fluid flow rate of the spray hole 14 can be adjusted accordingly to meet the needs of different processing stages. During operation, the fixing component quickly clamps the crystal. The processing component realizes multi-process continuous processing through the grinding blocks and flow rate adjustment. The modular design improves the adaptability to crystals of different specifications and reduces the changeover cost. The adjustable clamping force and processing parameters meet the needs of the entire process from roughing to finishing. It is suitable for multi-variety small-batch production scenarios.
[0028] The base 1 serves as the fundamental load-bearing component of the entire structure. A recessed machining groove 2 is provided on its top. The slots in the machining groove 2 enable the precise installation of the fixed components, providing a reference for the relative positioning of the fixed components and the machining components.
[0029] The processing groove 2 is located on the top of the base 1. The slot on the bottom of the inner wall is adapted to the fixing seat 3 of the fixing component. The horizontal displacement of the fixing component is limited by the plug-in engagement to ensure the stability of the crystal position during processing.
[0030] The mounting base 3 is made of non-magnetic composite material and is installed in the processing groove 2 through a slot. A groove 4 is opened on the top to provide a space for the crystal. Its non-magnetic properties avoid interfering with the magnetic domain structure of the magneto-optical crystal.
[0031] Groove 4 is located on the top of the fixed base 3. Its size is adapted to the ceramic artificial crystal. A sliding clamping component is installed inside to provide a stable reference for processing by limiting the horizontal displacement of the crystal.
[0032] The main grinding spindle 5 is a cylindrical structure that can rotate with the spindle of the machine tool. A graphite disk 11 is fixedly installed at the end. The rotation drives the composite grinding head assembly to grind the optical surface of the crystal.
[0033] Side buffer strip 6, which is a silicone pad, is fixed to one side of the inner wall of the groove 4 and the side corresponding to the main slide bar 8. It is stepped and buffers the clamping force through elastic deformation to avoid damage to the crystal surface.
[0034] Guide groove 7 is formed on both sides of the inner wall of groove 4 and is adapted to both ends of main slide bar 8. It is used to limit the sliding direction of main slide bar 8 and ensure that the clamping force is applied in the vertical direction along the side of the crystal.
[0035] The main slide bar 8 is slidably installed between two sets of guide grooves 7. One side is fixed with a side buffer bar 6, and the back magnet 9 is installed on the back side. It slides along the guide groove 7 through magnetic repulsion to achieve elastic clamping of the crystal.
[0036] The back magnet 9 is an NdFeB permanent magnet, which is embedded in the back side of the main slide bar 8 and is opposite to the permanent magnet 10 in the inner wall of the groove 4 with the same polarity. It provides continuous power for clamping through magnetic repulsion.
[0037] The permanent magnet 10 is an NdFeB permanent magnet of the same specification as the back magnet 9. It is fixed on the inner wall of the groove 4 on one side corresponding to the back magnet 9. The main slide bar 8 is pushed by the repulsive force with the back magnet 9 to adjust the clamping force.
[0038] The graphite disk 11 is a porous graphite disk with a diameter of 60mm, which is fixed to the end of the main grinding shaft 5. The surface has a mounting groove for mounting the elastic buffer layer 12 and the diamond grinding block 13. Its porous structure can dissipate heat quickly and avoid overheating during processing.
[0039] The elastic buffer layer 12 is a 0.3mm thick silicone pad, which is placed between the mounting groove of the graphite disk 11 and the diamond grinding block 13. The elastic deformation compensates for the surface gap and ensures that the adhesion between the grinding block and the crystal surface is ≥95%.
[0040] Diamond grinding block 13 is fan-shaped and has 0.1-0.3μm diamond micro powder electroplated on its surface. It is fixed to the end of the elastic buffer layer 12 and achieves mechanical grinding of the crystal surface by rotation.
[0041] Spray holes 14 are opened along the central axis of the main grinding shaft 5 and the graphite disk 11, and are used to transport CMP polishing fluid to the processing area to achieve chemical mechanical co-processing in conjunction with diamond grinding blocks 13.
[0042] The delivery pipe 15 is a chemically resistant plastic hose, with one end connected to the spray hole 14 and the other end connected to an external polishing fluid supply device. It is responsible for the stable delivery of CMP polishing fluid to ensure the continuous chemical action during the processing.
[0043] Although embodiments of the present invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the present invention, the scope of which is defined by the appended claims and their equivalents.
Claims
1. A ceramic artificial crystal optical surface processing structure for an optical isolator, comprising a base (1), a fixing component, and a processing component, wherein a recessed processing groove (2) is formed on the top of the base (1), and a slot is formed on the bottom of the inner wall of the processing groove (2), and the fixing component is installed inside the processing groove (2) by insertion through the slot, characterized in that: The fixing component includes a fixing seat (3), a groove (4) and a sliding clamping component. The fixing seat (3) is made of composite material, and the top of the fixing seat (3) is provided with a groove (4) that is compatible with the ceramic artificial crystal. The groove (4) is provided with a sliding clamping component for fixing the crystal. The processing assembly includes a rotatable main grinding shaft (5), the end of which is provided with a composite grinding head assembly for polishing, and a spray assembly for conveying polishing liquid is provided at the center of the main grinding shaft (5) and the composite grinding head assembly.
2. The optical surface processing structure of a ceramic artificial crystal for an optical isolator according to claim 1, characterized in that: The sliding clamping assembly includes a side buffer strip (6), a guide groove (7) and a main slide bar (8). The side buffer strip (6) is fixedly installed on one side of the inner wall of the groove (4), and guide grooves (7) are provided on both sides of the inner wall of the groove (4). The main slide bar (8) is slidably installed between the two sets of guide grooves (7).
3. The optical surface processing structure of a ceramic artificial crystal for an optical isolator according to claim 2, characterized in that: Another set of side buffer bars (6) is also fixedly installed on the side corresponding to the main slide bar (8) and the side buffer bar (6), and the side buffer bars (6) are all stepped.
4. The optical surface processing structure of a ceramic artificial crystal for an optical isolator according to claim 2, characterized in that: Two sets of back magnets (9) are fixedly installed on the back side of the main slide bar (8), and a permanent magnet (10) is fixedly installed on the inner wall of the groove (4) on the side corresponding to the back magnet (9). The back magnet (9) and the permanent magnet (10) are magnetically repelled. Both the back magnet (9) and the permanent magnet (10) are NdFeB permanent magnets with a magnetic field strength of 0.2-0.4T.
5. The optical surface processing structure of a ceramic artificial crystal for an optical isolator according to claim 1, characterized in that: The composite grinding head assembly includes a graphite disc (11), an elastic buffer layer (12), and a diamond grinding block (13). The graphite disc (11) is fixedly installed at the end of the main grinding shaft (5). It is a porous graphite disc with a diameter of 60 mm and an air permeability of 15 μm / s. Several mounting grooves are evenly spaced on the graphite disc (11) and are uniformly opened on the side surface of the graphite disc (11) facing the crystal. An elastic buffer layer (12) is fixedly installed inside each mounting groove. A diamond grinding block (13) is fixedly installed at the other end of the elastic buffer layer (12). The diamond grinding block (13) is fan-shaped and its surface is electroplated with diamond micro powder with a particle size of 0.1-0.3 μm.
6. The optical surface processing structure of a ceramic artificial crystal for an optical isolator according to claim 1, characterized in that: The spray assembly includes a spray hole (14) and a delivery pipe (15). The spray hole (14) is opened along the central axis of the main grinding shaft (5) and the graphite disk (11) and has a diameter of 4 mm. The delivery pipe (15) is a chemically resistant plastic hose, one end of which is connected to the spray hole (14) and the other end is connected to the outside. The polishing liquid delivered is CMP polishing liquid.