Corrosion-resistant piston assembly for a compressor
Through multi-layer coating and structural optimization design, the problems of insufficient coating adhesion and corrosion of sealing grooves on compressor piston rods have been solved, resulting in piston assemblies with high wear resistance, corrosion resistance and long service life.
Patent Information
- Application Number
- CN202621207891.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-06
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2036-08-06
AI Technical Summary
The existing compressor piston rod coating has insufficient adhesion and is prone to peeling. Crevice corrosion is likely to occur in the sealing groove area, and the surface properties are limited and difficult to adapt to complex working conditions.
The design incorporates a multi-layer coating structure, including a metal base layer, a gradient transition intermediate layer, and a functional top layer. It also incorporates rare earth element doping and laser texturing to optimize the piston connection section structure and cooling hole design.
It significantly improves the wear resistance, corrosion resistance and service life of the piston rod, reduces the coefficient of friction and structural stress concentration, and broadens the range of applicable working conditions.
Smart Images

Figure CN224955897U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of compressor component technology, specifically a corrosion-resistant piston assembly for a compressor. Background Technology
[0002] A compressor is a driven fluid machine that raises low-pressure gas to high-pressure gas, and it is widely used in refrigeration, chemical, petroleum, and natural gas transportation. The piston assembly is the core component of a reciprocating compressor, transmitting power and driving the piston to reciprocate linearly within the cylinder; its working environment is extremely harsh. During compressor operation, the piston rod working surface needs to undergo continuous high-speed reciprocating friction with the packing seals, guide sleeves, etc., bearing alternating loads, while being directly exposed to the compressed gas medium. When the compressor is used to compress gases containing… , , When exposed to corrosive process gases, the piston rod surface is highly susceptible to corrosion, wear, pitting, and even stress corrosion cracking, leading to seal failure and gas leakage, which seriously threatens equipment operation safety and production efficiency.
[0003] Currently, conventional methods to improve the wear and corrosion resistance of piston rods mainly include: using corrosion-resistant materials such as stainless steel or precipitation-hardening alloys for integral manufacturing, or performing surface treatment on the working surfaces of ordinary carbon steel or alloy steel piston rods. Existing surface treatment technologies mostly use single coatings, such as electroplating hard chrome or thermal spraying tungsten carbide. However, electroplated hard chrome layers have microcracks, and corrosive media can easily penetrate along these cracks to the substrate, causing under-film corrosion. Moreover, the chrome plating process causes severe environmental pollution. Although thermally sprayed tungsten carbide coatings have high hardness, their porosity is relatively large, requiring sealing treatment. Furthermore, the bonding between the coating and the substrate is mainly mechanical, which poses a risk of peeling under alternating loads and thermal shock. In addition, the existing piston rod structural design does not adequately consider the sealing groove structure of the piston connection section, allowing corrosive media to easily accumulate at the bottom of the sealing groove, accelerating localized corrosion in this area.
[0004] Therefore, how to design a corrosion-resistant piston assembly for compressors that combines excellent film-substrate adhesion, high density, high hardness, and low coefficient of friction, and whose structure can effectively channel corrosive media, has become a technical problem that urgently needs to be solved in this field. Utility Model Content
[0005] The purpose of this invention is to provide a corrosion-resistant piston assembly for compressors, which has the advantages of high coating bonding strength, excellent wear and corrosion resistance, reasonable structure and long service life, thus solving the problems in the prior art.
[0006] To achieve the above objectives, this utility model provides the following technical solution:
[0007] A corrosion-resistant piston assembly for a compressor includes a piston rod body and a piston connecting section disposed in the middle of the piston rod body. The rod body portions on both axial sides of the piston connecting section are piston rod working surfaces. The piston rod working surfaces of the piston rod body are fully covered with a wear-resistant and corrosion-resistant composite coating.
[0008] The wear-resistant and corrosion-resistant composite coating has a multi-element, multi-layer structure. From the substrate surface of the piston rod working surface outward, it includes: a metal underlayer for improving the adhesion between the film and the substrate, which is a single Cr layer or a single Ti layer; a gradient transition intermediate layer, which is a CrN / TiN alternating nano-multilayer film structure; and a functional top layer, which is a CrWN or TiWN nitride composite layer doped with W.
[0009] At least two annular mounting grooves for installing piston seals are provided on the outer circumferential surface of the piston connecting section. The cross-section of the annular mounting groove is an inverted trapezoid, and several circumferentially evenly distributed guide microholes are provided at the bottom of the annular mounting groove.
[0010] The piston rod body has a first connecting end and a second connecting end at its two ends, and the piston connecting section is located axially between the first connecting end and the second connecting end.
[0011] Preferably, the content of W element in the functional top layer accounts for 5% to 15% of the total atomic percentage of the functional top layer.
[0012] Doping CrN or TiN nitride coatings with an appropriate amount of W can significantly refine the coating grains, improve the coating density and hardness. At the same time, W can form a tungsten oxide transfer film with self-lubricating properties during friction, further reducing the coefficient of friction of the coating. Controlling the W content within the range of 5% to 15% can ensure that the coating obtains good comprehensive mechanical properties, while avoiding the increase in internal stress and decrease in toughness of the coating due to excessive W content.
[0013] Preferably, the number of alternating layers in the gradient transition intermediate layer is 10 to 30.
[0014] The gradient transition intermediate layer adopts an alternating CrN / TiN nano-multilayer film structure, forming a large number of coherent interfaces between adjacent layers. This effectively hinders dislocation movement and crack propagation, significantly improving the toughness and impact resistance of the coating. By controlling the number of alternating layers to 10-30, the gradient transition effect is ensured while avoiding process complexity and reduced production efficiency caused by too many layers.
[0015] Preferably, the thickness of the metal underlayer is 0.1μm to 0.5μm, the total thickness of the gradient transition intermediate layer is 2μm to 5μm, and the thickness of the functional top layer is 3μm to 8μm.
[0016] The main function of the metal underlayer is to enhance the adhesion between the coating and the substrate. If the thickness is too thin, the adhesion enhancement effect will be insufficient, and if it is too thick, it will easily become a soft and weak layer. The gradient transition intermediate layer plays the role of buffering stress and improving the load-bearing capacity of the coating. The functional top layer directly faces the friction and corrosion environment and needs sufficient thickness to ensure service life. The matching design of the thickness of the above layers enables the entire coating system to achieve the optimal balance between adhesion, toughness and wear resistance.
[0017] Preferably, the functional top layer is doped with rare earth elements Ce or Y, and the doping amount of rare earth elements is 0.5% to 2% of the total atomic percentage of the functional top layer, so as to refine the grains and improve the compactness and high-temperature oxidation resistance of the functional top layer.
[0018] The addition of trace amounts of rare earth elements Ce or Y can play a role in "purifying grain boundaries" and "pinning dislocations", effectively inhibiting grain growth and oxidation diffusion of the coating under high-temperature service conditions, and significantly improving the stability of the coating in high-temperature corrosive environments.
[0019] Preferably, the surface of the functional top layer is also implanted with fluorine through an ion implantation process, with an implantation dose of [missing value]. The surface free energy of the functional top layer is reduced by ions / cm² to improve the hydrophobic and anti-adhesion properties.
[0020] Fluorine ion implantation can form a fluoride-modified layer on the coating surface, significantly reducing the surface free energy and making it difficult for corrosive droplets to spread and adhere to the surface. This effectively slows down pitting and crevice corrosion and extends the service life of the piston rod in harsh media containing chloride ions.
[0021] Preferably, the surface of the functional top layer is distributed with an array of micro-pits that have undergone laser surface texturing. The diameter of the micro-pits is 30μm~100μm, the depth is 5μm~15μm, and the area occupancy is 5%~15%, which are used to store lubricating oil and capture wear particles.
[0022] Laser surface texturing technology creates regular micro-pits on the coating surface, which can serve as oil reservoirs to continuously provide lubrication medium under lean oil conditions and reduce the coefficient of friction. On the other hand, it can capture tiny wear debris generated during the wear process, preventing the debris from participating in three-body wear, thereby reducing the wear rate of the coating.
[0023] Preferably, the end face of the first connecting end has a sensor mounting blind hole for connecting the displacement sensor, and the end face of the second connecting end has a ejector center hole for connecting the ejector pin; the piston connecting section and the piston rod working surface are connected by an arc transition section, the radius of the arc transition section is 2mm~5mm, which is used to reduce stress concentration.
[0024] The diameter of the piston connecting section is larger than the diameter of the piston rod working surface. Stress concentration is likely to occur at the point of abrupt change in cross-section. By setting a circular arc transition section with a reasonable radius, the stress flow line can be smoothly transitioned, effectively reducing the peak stress in this area and preventing the initiation of fatigue cracks.
[0025] Preferably, the piston rod body has a central weight-reducing cooling hole that runs through its entire length along the axial direction, and the inner wall of the central weight-reducing cooling hole is also covered with a wear-resistant and corrosion-resistant composite coating; the external thread surfaces of the first connecting end and the second connecting end are fully covered with a chemically plated nickel-phosphorus alloy anti-corrosion layer, and the thickness of the chemically plated nickel-phosphorus alloy anti-corrosion layer is 0.02mm~0.05mm.
[0026] The central weight-reducing cooling hole not only reduces the reciprocating inertial force of the piston assembly, but also allows the cooling medium to be introduced to lower the working temperature of the piston rod. The inner wall of the central hole is covered with a wear-resistant and corrosion-resistant composite coating to prevent the cooling medium from corroding the hole wall. The external thread surface is coated with a chemically plated nickel-phosphorus alloy anti-corrosion layer, which utilizes its excellent corrosion resistance and uniform plating ability to achieve comprehensive protection for irregular parts such as thread grooves.
[0027] Preferably, the hardness of the functional top layer is not less than HV2500.
[0028] Tests have shown that the microhardness of the functional top layer, which employs the aforementioned multi-layered structural design, can reach over HV2500, providing excellent wear-resistant protection for the piston rod working surface.
[0029] Compared with the prior art, the beneficial effects of this utility model are as follows:
[0030] 1. This utility model solves the problems of insufficient adhesion and easy peeling of existing single coatings by designing a multi-layer composite coating structure of "metal base layer + gradient transition intermediate layer + functional top layer". The metal base layer ensures a firm bond between the coating and the substrate, the gradient transition intermediate layer effectively relieves interlayer stress, and the functional top layer provides high hardness, wear resistance and corrosion resistance. The synergistic effect of the three layers significantly improves the service life of the piston rod under the coupling effect of alternating load and corrosive media.
[0031] 2. This utility model improves the density, high-temperature oxidation resistance and self-lubricating properties of the coating by doping W element in the functional top layer and controlling its content, and optionally doping rare earth elements Ce or Y, so that the piston rod can maintain stable performance under harsh working conditions of high temperature, high pressure and corrosive gas.
[0032] 3. This utility model solves the problems of easy liquid accumulation and crevice corrosion in traditional rectangular grooves by designing the cross section of the annular mounting groove of the piston connection section as an inverted trapezoid and opening flow guiding microholes at the bottom of the groove. The inverted trapezoidal structure facilitates the installation of sealing components and forms a wedge-shaped sealing effect. The flow guiding microholes can promptly discharge corrosive media that may seep into the bottom of the groove, effectively reducing the risk of local corrosion in the sealing groove area.
[0033] 4. This utility model selectively performs fluorine ion implantation and laser texturing on the functional top surface to form a hydrophobic anti-adhesion surface and an array of oil-retaining micro-pits, which significantly reduces the adhesion tendency of corrosive media, improves the tribological properties under boundary lubrication conditions, and further broadens the applicable operating conditions of the piston assembly.
[0034] 5. By setting a central weight-reducing cooling hole and an arc transition section, this utility model reduces the mass of reciprocating motion and the inertial force, while effectively reducing structural stress concentration and improving the overall fatigue life of the piston rod; the external thread surface is coated with a chemical nickel-phosphorus alloy anti-corrosion layer, achieving full coverage anti-corrosion protection for the threaded parts. Attached Figure Description
[0035] Figure 1 The diagram shown is a three-dimensional structural schematic of this utility model;
[0036] Figure 2 The diagram shown is a three-dimensional axial half-section view of the piston rod body of this utility model.
[0037] Figure 3 The diagram shown is a three-dimensional structural schematic of the first connecting end of this utility model.
[0038] Figure 4 The diagram shown is a three-dimensional cross-sectional view of the central weight-reducing cooling hole of this utility model.
[0039] Figure 5 This utility model is shown. Figure 4 A magnified three-dimensional structural diagram of a portion of point A in the middle;
[0040] Figure 6 This utility model is shown. Figure 4 A magnified three-dimensional structural diagram of a portion of point B in the middle;
[0041] Figure 7 The diagram shown is a three-dimensional structural schematic of the annular mounting groove of this utility model.
[0042] Figure 8 The diagram shown is a three-dimensional structural schematic of the flow-guiding micropores of this utility model.
[0043] Figure 9 The diagram shown is a three-dimensional structural schematic of the micro-dimple array of this utility model.
[0044] Reference numerals: 1. Piston rod body; 11. Piston rod working surface; 12. First connecting end; 121. Sensor mounting blind hole; 13. Second connecting end; 131. Center hole of ejector pin; 14. Arc transition section; 15. Center weight reduction cooling hole; 2. Piston connecting section; 21. Annular mounting groove; 211. Guide micropores; 3. Wear-resistant and corrosion-resistant composite coating; 31. Metal underlayer; 32. Gradient transition intermediate layer; 33. Functional top layer; 331. Micro-dimple array. Detailed Implementation
[0045] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the protection scope of the present utility model.
[0046] To address the problems of insufficient adhesion of piston rod coatings, easy peeling, susceptibility to crevice corrosion in the sealing groove area, and limited surface properties that make them unsuitable for complex working conditions in existing technologies, the following technical solution is proposed. Please refer to [link / reference needed]. Figures 1-9 .
[0047] A corrosion-resistant piston assembly for a compressor includes a piston rod body 1 and a piston connecting section 2 located in the middle of the piston rod body 1. The rod sections on both axial sides of the piston connecting section 2 form piston rod working surfaces 11. The piston rod working surfaces 11 of the piston rod body 1 are fully covered with a wear-resistant and corrosion-resistant composite coating 3. The wear-resistant and corrosion-resistant composite coating 3 has a multi-element, multi-layer structure, and from the substrate surface of the piston rod working surface 11 outwards includes: a metal underlayer 31 for improving film-substrate adhesion, wherein the metal underlayer 31 is a single-element Cr layer or a single-element Ti layer; a gradient transition intermediate layer 32; and the gradient transition intermediate layer 33... 2 is a CrN / TiN alternating nano-multilayer film structure; the functional top layer 33 is a CrWN or TiWN nitride composite layer doped with W element; at least two annular mounting grooves 21 for installing piston seals are opened on the outer circumferential surface of the piston connecting section 2, the cross section of the annular mounting groove 21 is an inverted trapezoid, and several circumferentially uniformly distributed guiding micropores 211 are opened at the bottom of the annular mounting groove 21; the piston rod body 1 has a first connecting end 12 and a second connecting end 13 at both ends, and the piston connecting section 2 is located axially between the first connecting end 12 and the second connecting end 13.
[0048] In this embodiment, specifically, the content of W element in the functional top layer 33 accounts for 5% to 15% of the total atomic percentage of the functional top layer 33. The number of alternating layers in the gradient transition intermediate layer 32 is 10 to 30. The thickness of the metal base layer 31 is 0.1 μm to 0.5 μm, the total thickness of the gradient transition intermediate layer 32 is 2 μm to 5 μm, and the thickness of the functional top layer 33 is 3 μm to 8 μm.
[0049] In this embodiment, specifically, the end face of the first connecting end 12 is provided with a sensor mounting blind hole 121 for connecting a displacement sensor, and the end face of the second connecting end 13 is provided with a ejector center hole 131 for connecting an ejector pin; the piston connecting section 2 and the piston rod working surface 11 are connected by an arc transition section 14, the radius of the arc transition section 14 is 2mm~5mm, which is used to reduce stress concentration.
[0050] In this embodiment, specifically, a central weight-reducing cooling hole 15 is provided axially inside the piston rod body 1, and the inner wall of the central weight-reducing cooling hole 15 is also covered with a wear-resistant and corrosion-resistant composite coating 3; the external thread surfaces of the first connecting end 12 and the second connecting end 13 are fully covered with a chemically plated nickel-phosphorus alloy anti-corrosion layer, and the thickness of the chemically plated nickel-phosphorus alloy anti-corrosion layer is 0.02mm~0.05mm.
[0051] In this embodiment, specifically, the hardness of the functional top layer 33 is not lower than HV2500.
[0052] Example 1: In this example, specifically, the functional top layer 33 is doped with rare earth elements Ce or Y, and the doping amount of rare earth elements is 0.5% to 2% of the total atomic percentage of the functional top layer 33, so as to refine the grains and improve the compactness and high-temperature oxidation resistance of the functional top layer 33.
[0053] Example 2: As another alternative implementation, the surface of the functional top layer 33 is also implanted with fluorine via ion implantation, with an implantation dose of [missing information]. ions / cm², to reduce the surface free energy of the functional top layer 33 and improve hydrophobic anti-adhesion properties.
[0054] Example 3: As another alternative implementation, the surface of the functional top layer 33 is distributed with a micro-pit array 331 that has undergone laser surface texturing treatment. The diameter of the micro-pits is 30μm~100μm, the depth is 5μm~15μm, and the area occupancy is 5%~15%, which is used to store lubricating oil and capture wear particles.
[0055] It should be noted that the flow guiding micro-hole 211 is a through hole, which is connected to the central weight reduction cooling hole 15, and the opening position of the flow guiding micro-hole 211 avoids the contact area between the piston seal and the bottom of the groove.
[0056] Working principle: During assembly, the piston assembly is fixedly connected to the compressor crosshead or connector through the first connecting end 12, and the second connecting end 13 is fixedly connected to the piston body. The piston connecting section 2 is located in the central shaft hole of the piston body. The piston seal is installed in the annular mounting groove 21. The piston rod working surface 11 slides with the compressor's packing seal assembly and guide sleeve.
[0057] During compressor operation, the piston assembly reciprocates linearly at high speed along the cylinder axis. During this process, the wear-resistant and corrosion-resistant composite coating 3 directly bears the frictional load from the packing seal and the chemical erosion from the compressed corrosive gas. The metal underlayer 31 serves as a transition bridge between the coating and the substrate. Its elemental Cr or Ti component has good metallurgical compatibility with the Fe element in the substrate, ensuring that the coating does not peel off under alternating loads. The CrN / TiN alternating nano-multilayer structure of the gradient transition intermediate layer 32 effectively hinders crack propagation through the multilayer interface, improving the toughness and impact resistance of the entire coating system. The W element in the functional top layer 33 refines the CrN or TiN grains, giving the coating extremely high hardness (above HV2500) and excellent wear resistance. At the same time, the W element can generate tungsten oxide with a self-lubricating effect under frictional heat, further reducing the coefficient of friction.
[0058] In terms of corrosion protection, the dense nitride composite layer effectively blocks corrosion. , , The penetration of corrosive media; when a small amount of corrosive media seeps into the area of the annular mounting groove 21 along the connection gap between the piston rod and the piston, the annular mounting groove 21 with its inverted trapezoidal cross section can use its wedge structure to enhance the clamping force of the seal. At the same time, the guide microholes 211 at the bottom of the groove guide the accumulated media to the internal channel of the piston rod in time to discharge, thus avoiding the crevice corrosion caused by the long-term retention of the media at the bottom of the sealing groove.
[0059] When the compressor is used with a large amount In high-acid gas conditions, the preferred approach is the scheme of Example 2, which involves fluorine ion implantation treatment on the surface of the functional top layer 33. The implanted fluorine element can significantly reduce the surface free energy of the coating, making the coating more resistant to acidic gases. Corrosive droplets are spherical and do not spread easily, thus inhibiting pitting corrosion. When the compressor operates under lean lubrication or frequent start-stop conditions, the solution of Example 3 is preferred, that is, a regular micro-pit array 331 is formed on the surface of the functional top layer 33 by laser surface texturing. The lubricating oil stored in the micro-pits can be continuously supplied under boundary lubrication conditions, while capturing tiny wear debris and significantly reducing the wear rate. When the compressor operates at a high temperature (e.g., exceeding 300°C), the solution of Example 1 is preferred, that is, rare earth elements Ce or Y are doped into the functional top layer 33. The grain boundary pinning effect of rare earth elements is used to inhibit high-temperature grain coarsening and oxidation of the coating, and maintain the high-temperature hardness and corrosion resistance of the coating.
[0060] If maintenance is required after long-term use, the connecting parts at both ends can be removed to check the wear condition of the wear-resistant and corrosion-resistant composite coating 3. Since the thickness of each coating is set within the optimal range, when the functional top layer 33 shows slight wear, the gradient transition intermediate layer 32 can still provide sufficient load-bearing capacity and protection, extending the overall service life of the piston rod.
[0061] It should be noted that, in this document, relational terms such as "first" and "second" are used only to distinguish one entity or operation from another, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such process, method, article, or apparatus.
[0062] Although embodiments of the present invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the present invention.
Claims
1. A corrosion-resistant piston assembly for a compressor, comprising a piston rod body (1) and a piston connecting section (2) arranged at a middle position of the piston rod body (1), the rod body portions on both axial sides of the piston connecting section (2) being piston rod working surfaces (11); characterized in that The piston rod working surface (11) of the piston rod body (1) is fully covered with a wear-resistant and corrosion-resistant composite coating (3). The wear-resistant and corrosion-resistant composite coating (3) is a multi-element multilayer structure, which includes, from the substrate surface of the piston rod working surface (11) outward: a metal base layer (31) for improving the film-substrate adhesion, a gradient transition intermediate layer (32) and a functional top layer (33). The metal base layer (31) is a single Cr layer or a single Ti layer; the gradient transition intermediate layer (32) is a CrN / TiN alternating nano-multilayer film structure; and the functional top layer (33) is a CrWN or TiWN nitride composite layer doped with W. At least two annular mounting grooves (21) for installing piston seals are provided on the outer circumferential surface of the piston connecting section (2). The cross section of the annular mounting groove (21) is an inverted trapezoid, and several circumferentially evenly distributed guide microholes (211) are provided at the bottom of the annular mounting groove (21). The piston rod body (1) has a first connecting end (12) and a second connecting end (13) at both ends, and the piston connecting section (2) is located axially between the first connecting end (12) and the second connecting end (13).
2. The corrosion resistant piston assembly of claim 1, wherein, The number of alternating layers in the gradient transition intermediate layer (32) is 10 to 30.
3. The corrosion resistant piston assembly of claim 1, wherein, The thickness of the metal underlayer (31) is 0.1μm~0.5μm, the total thickness of the gradient transition intermediate layer (32) is 2μm~5μm, and the thickness of the functional top layer (33) is 3μm~8μm.
4. The corrosion resistant piston assembly of claim 1, wherein, The first connecting end (12) has a sensor mounting blind hole (121) for connecting a displacement sensor at the center of its end face, and the second connecting end (13) has a pin center hole (131) for connecting a pin at the center of its end face; the piston connecting section (2) and the piston rod working surface (11) are connected by an arc transition section (14), the radius of the arc transition section (14) is 2mm~5mm, which is used to reduce stress concentration.
5. The corrosion resistant piston assembly of claim 1, wherein, The piston rod body (1) has a central weight-reducing cooling hole (15) that runs through its entire length along the axial direction. The inner wall of the central weight-reducing cooling hole (15) is also covered with a wear-resistant and corrosion-resistant composite coating (3). The external thread surfaces of the first connecting end (12) and the second connecting end (13) are fully covered with a chemically plated nickel-phosphorus alloy anti-corrosion layer with a thickness of 0.02mm to 0.05mm.