A composite metallic effect coating
By designing a composite metallic effect coating, the problems of dust pollution and insufficient weather resistance in liquid metallic coatings during construction are solved, achieving a safe and uniform paint surface and good adhesion, thus improving the safety of the construction environment and the durability of the coating.
Patent Information
- Application Number
- CN202522707374.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-22
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-12-22
AI Technical Summary
Existing liquid metal coatings generate dust during spraying and polishing, which endangers the health of construction workers. The construction process is complex and lacks weather resistance and wear resistance, resulting in high maintenance costs.
The composite metal effect coating is used, and the wall body, substrate layer, interface reinforcement layer and composite metal coating are set from the inside to the outside. It includes a base layer, a top layer and an effect layer. The top layer has grooves for applying magnetic paint. Combined with fine aggregate materials and sponge wiping process, the sanding step is eliminated, forming a magnetic effect and a uniform paint surface.
It improves construction safety and health friendliness, with uniform paint thickness, strong adhesion, excellent wear resistance and weather resistance, and reduces dust pollution and construction difficulty.
Smart Images

Figure CN224982489U_ABST
Abstract
Description
Technical Field
[0001] This application relates to the technical field of coatings, and in particular to a composite metallic effect coating. Background Technology
[0002] Liquid metal is commonly used in the interior decoration of various buildings. It is made by mixing metal powder with paint and then applying it to the wall or using it as a decorative material on the surface. Its advantage is that it can create an extremely realistic metallic texture. However, in existing technologies, the spraying and polishing processes during the use of liquid metal easily generate dust that permeates the working environment. This dust is metallic dust, and if construction workers inhale it for a long time, it can damage the respiratory system, causing lung diseases. In addition, some metallic components, such as lead and cadmium, can enter the human body through the respiratory tract or skin and accumulate in the body, damaging the nervous and hematopoietic systems and seriously affecting health. Furthermore, the construction process in existing technologies is complex and has stringent requirements for the construction environment. Moreover, the weather resistance and wear resistance of the metal coating are insufficient, and long-term outdoor use is prone to fading and peeling, resulting in high maintenance costs. Utility Model Content
[0003] This utility model provides a composite metallic effect coating that improves the safety of the construction process and ensures uniform coating thickness and strong adhesion after film formation.
[0004] To achieve the aforementioned objectives, this application adopts the following technical solution: A composite metallic effect coating is configured from the inside to the outside as a wall body, a substrate layer, an interface reinforcement layer, and a composite metallic coating. The composite metallic coating includes a base layer, a top layer, and an effect layer. The base layer is located on the inside, the effect layer is on the outside, and the top layer is located between the base layer and the effect layer. The top layer has several grooves to form a serrated structure on the surface of the top layer. The inside of the grooves is coated with magnetic paint to form a magnetic paint layer.
[0005] In some alternative embodiments, the outer surface of the magnetic paint layer and the outer surface of the surface layer are on the same horizontal plane.
[0006] In some alternative implementations, the depth of the groove is 0.5 mm.
[0007] In some alternative embodiments, the outer surface of the magnetic paint layer is higher than the outer surface of the surface layer.
[0008] In some alternative embodiments, the thickness of the magnetic paint layer is 0.5~1.0 mm.
[0009] In some alternative implementations, the thickness of a single layer of the interface reinforcement layer is 0.95~0.1mm.
[0010] In some alternative implementations, the thickness of the bottom layer is 0.95~0.1mm.
[0011] In some alternative implementations, the undercoat is applied using a roller coating method.
[0012] In some alternative implementations, the groove is square, rectangular, or triangular in shape.
[0013] The composite metallic effect coating provided in this application has the following beneficial effects: The technical solution adopted in this application uses a composite metallic effect coating. It employs a combination of processes, including using a fine aggregate material as a base layer and applying the effect layer with a sponge or a similar material. This process allows for flexible adjustment of the metallic texture and color depth, avoiding the need for polishing required in traditional liquid metallic paints. This solves the problem of metal dust posing a health hazard and ensures the safety and health-friendliness of the application. Meanwhile, by setting grooves on the surface layer and coating the inside of the grooves with magnetic paint to form a magnetic paint layer, and combining it with the substrate layer, interface reinforcement layer, composite metal coating, bottom layer, top layer, and effect layer, the composite metal coating as a whole has both a metallic effect and a magnetic effect, effectively improving the aesthetics and interactivity of the wall. The coating undergoes a multi-layered process, including applying a base coat, top coat, and effect coat, followed by meticulous sanding (using 240-grit sandpaper for the base coat and 180-grit sandpaper for the top coat and magnetic paint layer). Combined with controlled drying time of over 24 hours for each layer, the resulting paint film exhibits uniform thickness, excellent smoothness, outstanding adhesion, and good surface hardness. This effectively overcomes the limitations of traditional liquid metallic paints, such as insufficient wear resistance and weather resistance, and stringent application requirements. Attached Figure Description
[0014] Other features, objects, and advantages of this application will become more apparent from the following detailed description of non-limiting embodiments with reference to the accompanying drawings: Figure 1 This is a structural diagram of a composite metallic effect coating according to this application; Figure 2 yes Figure 1 An enlarged view of circle A shown.
[0015] Figure label: 10. Wall body; 11. Substrate layer; 12. Interface reinforcement layer; 13. Composite metal coating; 14. Base layer; 15. Top layer; 16. Effect layer; 17. Groove; 18. Magnetic paint layer. Detailed Implementation
[0016] The specific embodiments of this application are described below with reference to the accompanying drawings and examples. Through the content described in this specification, those skilled in the art can clearly and completely understand the technical solution, the technical problem solved, and the resulting technical effects of this application. It is understood that the specific embodiments described herein are only for explaining this application and not for limiting it. Furthermore, for ease of description, only the parts related to this application are shown in the accompanying drawings.
[0017] It should be noted that the structures, proportions, sizes, etc., shown in the accompanying drawings are only for the purpose of assisting those skilled in the art in understanding and reading the contents described in the specification, and are not intended to limit the conditions under which this application can be implemented. Therefore, they have no substantial technical significance. Any modifications to the structure, changes in the proportional relationships, or adjustments to the size should fall within the scope of the technical content disclosed in this application, provided that they do not affect the effects and purposes that this application can produce.
[0018] The use of terms such as "first," "second," and "the" does not imply quantity limitation and may indicate singular or plural. The terms "comprising," "including," "having," and any variations thereof used in this application are intended to cover non-exclusive inclusion; for example, processes, methods, systems that include a series of steps or modules. The product or equipment is not limited to the listed steps or units, but may also include steps or units not listed, or other steps or units inherent to these processes, methods, products, or equipment. Terms such as “connection,” “linking,” and “coupled” used in this application are not limited to physical or mechanical connections, but may also include direct or indirect electrical connections.
[0019] It should also be noted that the longitudinal section corresponding to the embodiment of this application can be the section corresponding to the front view direction, the transverse section can be the section corresponding to the right view direction, and the horizontal section can be the section corresponding to the top view direction.
[0020] Furthermore, where there is no conflict, the embodiments and features described in this application can be combined with each other. This application will now be described in detail with reference to the accompanying drawings and embodiments.
[0021] A composite metallic effect coating is configured from the inside to the outside as a wall body 10, a substrate layer 11, an interface reinforcement layer 12, and a composite metallic coating 13. The composite metallic coating 13 includes a base layer 14, a top layer 15, and an effect layer 16. The base layer 14 is located on the inside, the effect layer 16 is located on the outside, and the top layer 15 is located between the base layer 14 and the effect layer 16. Further, the top layer 15 is provided with a plurality of grooves 17 to form a serrated structure on the surface of the top layer 15. The inside of the grooves 17 is coated with magnetic paint to form a magnetic paint layer 18 to achieve an overall metallic effect of the composite metallic coating 13, as well as a certain magnetic effect. It should be noted that the depth of the grooves 17 is 0.5mm, and the shape of the grooves 17 includes, but is not limited to, squares, rectangles, triangles, etc. The outer surface of the magnetic paint layer 18 is at the same level as the outer surface of the top layer 15, or the outer surface of the magnetic paint layer 18 is higher than the outer surface of the top layer 15.
[0022] Preferably, the thickness of the magnetic paint layer 18 is 0.5~1.0 mm.
[0023] Preferably, the substrate layer 11 is a putty layer, and the construction material used is epoxy putty.
[0024] Preferably, the interface reinforcement layer 12 is a two-component sand-containing acrylate primer layer with a single layer thickness of 0.95~0.1mm.
[0025] Preferably, the bottom layer 14 is a colored intermediate coating layer with a single layer thickness of 0.95~0.1mm, and is applied by roller in 1~2 coats.
[0026] Preferably, the surface layer 15 is a fine-grained polyurethane coating layer or a fine-grained micro-cement.
[0027] Preferably, effect layer 16 is a metallic effect layer.
[0028] The application method for the composite metallic effect coating in this application is as follows: Example 1: The base material is a damaged putty wall surface (old wall); Step 1: Fill and repair the cracks in the wall with environmentally friendly putty, and after drying for more than 24 hours, sand it until smooth. The error range of its smoothness is ≤0.5mm. Step 2: After applying one coat of interface reinforcement layer 12 by roller, allow it to dry for more than 24 hours to ensure it is completely dry; Step 3: Apply two coats of intermediate color coating by roller and allow it to dry for more than 24 hours to ensure it is completely dry. Then, lightly sand it by hand with 240-grit sandpaper. Step 4: Apply two coats of fine-grained polyurethane topcoat. Simultaneously, use a mold with the same shape as groove 17 to carve groove 17 onto the paint surface to create groove 17. Allow it to dry for at least 24 hours to ensure it is completely dry. Then, finely sand it with 180-grit sandpaper. Allow at least 24 hours between each coat. The ambient temperature should be 20~25℃ and the humidity ≤75%. Step 5: Apply magnetic paint to the inside of groove 17 until it is completely filled, and allow it to dry for more than 72 hours to ensure it is completely dry. Then, use 180-grit sandpaper to finely polish it. Step 6: Apply one to three coats of metallic effect paint using a sponge. Each coat should be allowed to dry for at least 24 hours. Each coat must be completely dry before applying the next. Finally, allow the finished metallic effect paint to cure for at least 72 hours to prevent damage to the paint surface.
[0029] Example 2: Using ceramic tiles as the base material; Step 1: After applying one coat of interface reinforcement layer 12 by roller, allow it to dry for more than 24 hours to ensure it is completely dry; Step 2: Apply two coats of intermediate color using a roller and allow them to dry for at least 24 hours. Once completely dry, lightly sand them by hand using 240-grit sandpaper. Step 3: Apply two coats of fine aggregate micro cement. At the same time, use a mold with the same shape as groove 17 to carve groove 17 on the paint surface to make groove 17. After drying for more than 24 hours, allow it to dry completely. Then, use 180-grit sandpaper for fine sanding. Each layer should be spaced at least 24 hours apart. The ambient temperature should be 20~25℃ and the humidity ≤75%. Step 4: Apply magnetic paint to the inside of groove 17 until it is completely filled, and allow it to dry for more than 72 hours to ensure it is completely dry. Then, use 180-grit sandpaper to finely polish it. Step 5: Apply one to three coats of metallic effect paint using a sponge. Each coat should be allowed to dry for at least 24 hours. Each coat must be completely dry before applying the next. Finally, allow the finished metallic effect paint to cure for at least 72 hours to prevent damage to the paint surface.
[0030] In some alternative embodiments, an interface reinforcement layer 12 to enhance adhesion is directly rolled onto the substrate layer 11, and after drying, the metallic effect paint is directly wiped off, thereby simplifying the process, reducing the use of construction materials, and improving environmental performance.
[0031] Here, the composite metallic effect coating uses a fine aggregate material as the top layer 15 and is leveled. Then, a sponge or similar material is used to apply the effect layer in a circular motion, creating a natural and delicate metallic effect on the paint surface. This eliminates the dust-generating sanding step, avoiding dust pollution in the construction environment and protecting the health of the construction workers. Instead, the texture and color depth of the metallic effect are achieved through repeated rubbing. The application process is flexible, and after film formation, the rubbing process results in a uniform and smooth paint surface. It exhibits excellent adhesion and good surface hardness, making it suitable for various wall construction environments, such as irregular facades and decorative surfaces. Furthermore, by setting grooves 17 on the surface layer and coating the interior of the grooves 17 with magnetic paint to form a magnetic paint layer 18, and combining it with the substrate layer 11, interface reinforcement layer 12, composite metal coating 13, base layer 14, top layer 15, and effect layer 16, a composite metal coating is formed that has both a full, polished metallic effect and a magnetic effect, effectively enhancing the aesthetics and interactivity of the wall surface.
[0032] Although this application has been described and illustrated with reference to specific embodiments thereof, such description and illustration are not limiting of this application. It will be readily understood by those skilled in the art that various changes can be made and equivalent elements can be substituted within embodiments without departing from the true spirit and scope of this application as defined by the appended claims. Illustrations may not be drawn to scale. Differences may exist between the technical representation in this application and actual implementation due to variables in the manufacturing process, etc. Other embodiments of this application may exist that are not specifically described. The description and illustrations should be considered illustrative rather than restrictive. Modifications can be made to adapt particular circumstances, materials, composition, methods, or processes to the objectives, spirit, and scope of this application. All such modifications fall within the scope of the appended claims. While the methods disclosed herein have been described with reference to specific operations performed in a particular order, it should be understood that these operations can be combined, subdivided, or reordered to form equivalent methods without departing from the teachings of this application. Therefore, unless specifically indicated herein, the order and grouping of operations do not limit this application.
Claims
1. A composite metallic effect coating, characterized in that: The wall body (10), substrate layer (11), interface reinforcement layer (12) and composite metal coating (13) are arranged sequentially from the inside to the outside. The composite metal coating (13) includes a base layer (14), a top layer (15) and an effect layer (16). The base layer (14) is located on the inside, the effect layer (16) is located on the outside, and the top layer (15) is located between the base layer (14) and the effect layer (16). The top layer (15) is provided with a plurality of grooves (17) to form a sawtooth structure on the surface of the top layer (15). The inside of the grooves (17) is coated with magnetic paint to form a magnetic paint layer (18).
2. The composite metallic effect coating according to claim 1, characterized in that, The outer surface of the magnetic paint layer (18) is on the same horizontal plane as the outer surface of the surface layer (15).
3. The composite metallic effect coating according to claim 2, characterized in that, The depth of the groove (17) is 0.5 mm.
4. The composite metallic effect coating according to claim 3, characterized in that, The outer surface of the magnetic paint layer (18) is higher than the outer surface of the surface layer (15).
5. The composite metallic effect coating according to claim 4, characterized in that, The thickness of the magnetic paint layer (18) is 0.5~1.0 mm.
6. The composite metallic effect coating according to claim 5, characterized in that, The thickness of a single layer of the interface enhancement layer (12) is 0.95~0.1mm.
7. The composite metallic effect coating according to claim 6, characterized in that, The thickness of a single layer of the bottom layer (14) is 0.95~0.1mm.
8. The composite metallic effect coating according to claim 7, characterized in that, The base layer (14) is applied by roller coating.
9. The composite metallic effect coating according to claim 8, characterized in that, The groove (17) is square, rectangular or triangular in shape.