Fully corrosion-resistant spiral steel pipe with outer corrugated peak and inner flat wall
By using a fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall, the problems of low structural strength in the void area of the inner plastic coating layer and the spacing at the edge of the traditional spiral steel pipe are solved. This improves the flatness of the metal layer and its compressive bearing capacity, thereby enhancing the overall quality and corrosion resistance of the pipeline.
Patent Information
- Application Number
- CN202522786720.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-29
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-12-29
AI Technical Summary
The inner plastic coating of traditional spiral steel pipes has voids, resulting in low structural strength. The inner plastic coating is not smooth enough, and there are gaps at the edges of the spiral steel pipe, which affects the pipe's compressive strength.
The design adopts a fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall. By setting two overlaps on the steel strip, and making the second overlap overlap with the corrugation during spiral welding, a flat inner circumference is formed. The inner and outer plastic coating layers are bonded to the metal layer through an adhesive resin layer, which enhances the structural strength and sealing performance.
It improves the structural strength of the metal layer and the smoothness of the inner plastic coating, enhances the pipe's compressive strength, ensures smooth fluid transport, and significantly improves the quality and corrosion resistance of the pipe.
Smart Images

Figure CN224983636U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of spiral steel pipe technology, and in particular to a fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall. Background Technology
[0002] Traditional steel-coated spiral wound drainage pipes use an integrated molding process of spiral steel pipes coated with plastic. Their structural design ensures that the pipes can stably bear loads under rated pressure conditions, and with their excellent corrosion resistance, they have been widely used in related engineering fields.
[0003] During production, traditional spiral steel pipes are formed by corrugating steel strips and bending them into a spiral shape. Simultaneously, hot pressing and a plastic coating are applied to both the inner and outer sides of the spiral pipe. To ensure smooth fluid flow inside the pipe, the inner plastic coating is cylindrical. This results in voids between the inner plastic coating and the raised crests, leading to low structural strength. Furthermore, during the forming and cooling of the inner plastic coating, the shrinkage of the coating and the cooling and contraction of the air in the voids cause a slight bulge in the inner plastic coating outwards. Consequently, the flatness of the inner plastic coating is limited, which can affect the flow of water.
[0004] In addition, the spiral steel pipes of this type currently have gaps at their edges, which are sealed using a heat-sealing process with an outer plastic coating. Due to the gaps in the spiral steel pipe itself, the overall compressive strength of the pipe is affected, resulting in a definite upper limit to its actual compressive strength, which is constrained by the structural characteristics. Utility Model Content
[0005] The purpose of this utility model is to solve the above-mentioned problems by providing a fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall.
[0006] To achieve the above objectives, the technical solution of this utility model is as follows: a fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall, comprising a metal layer, an inner plastic coating layer and an outer plastic coating layer disposed on both sides of the metal layer, wherein the metal layer is formed by spiral welding of steel strip pressure. Along the width direction of the steel strip, the steel strip is provided with a first overlap, a second overlap, and a crest located between the first overlap and the second overlap. The first surface of the second overlap near the crest is flush with the second surface of the first overlap, and the dimension a of the second overlap is greater than or equal to the sum of the dimensions b of the first overlap and the crest. The first surface is the same side as the crest of the second edge, and the second surface is the opposite side of the crest of the first edge.
[0007] Furthermore, the peak includes a first peak.
[0008] Furthermore, the wave crest includes a first wave crest and a second wave crest, the second wave crest being located on the side of the first wave crest near the second edge, and the height of the second wave crest being lower than the height of the first wave crest.
[0009] Furthermore, the steel strip may be a perforated steel strip or a non-perforated steel strip.
[0010] Furthermore, the steel strip is a hot-dip galvanized steel strip.
[0011] Furthermore, the surfaces of the metal layer that come into contact with the inner and outer plastic coatings are all thermally coated with polyolefin plastic.
[0012] Furthermore, between adjacent steel strip spiral segments, the second overlap of one steel strip spiral segment overlaps with the first overlap of another steel strip spiral segment and the inner side of the crest, and the end of the second overlap is welded to the bottom of the crest, and the first surface of the second overlap is welded to the end of the first overlap of another steel strip spiral segment.
[0013] Furthermore, both the inner and outer plastic coatings are bonded to the metal layer.
[0014] Furthermore, both the inner and outer plastic coatings are bonded to the metal layer using an adhesive resin layer.
[0015] Compared with existing technologies, the fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall disclosed in this utility model has the following advantages: When the steel strip is corrugated, it will form two overlapping edges of different lengths on both sides of the corrugation peak. The two overlapping edges are staggered in the thickness direction of the plate and are matched with the dimensions a of the overlapping edge 2 and b of the sum of the dimensions of the overlapping edge 1 and the corrugation peak in the width direction of the steel strip. When the metal layer is formed by spiral bending and welding, the bolt segment on the rear side can be wrapped around the outer side of the overlapping edge 2 of the front spiral segment along the spiral winding direction. By overlapping the corrugation peak and overlapping edge 1 of the rear spiral segment with the overlapping edge 2 on the front side, the void area on the inner side of the corrugation peak can be blocked. The formed metal layer has a flat inner circumferential surface. The overlapping and matching method can effectively improve the structural strength of the metal layer and ensure the flatness of the subsequent inner plastic coating layer, which can significantly improve the quality of the pipe. Attached Figure Description
[0016] Figure 1 This is a three-dimensional structural diagram of the fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall, according to this utility model.
[0017] Figure 2 This is a side view of the first embodiment of the fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall.
[0018] Figure 3 This is a side view of the second embodiment of the fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall.
[0019] Figure 4 This is a cross-sectional view of the fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall at point AA.
[0020] Figure 5 This is a partially enlarged structural diagram of point B in the first embodiment of this utility model.
[0021] Figure 6 This is a schematic diagram of the cross-sectional structure of the steel strip after it has been corrugated in the first embodiment of this utility model.
[0022] Figure 7 This is a partially enlarged structural diagram of point B in the second embodiment of this utility model.
[0023] Figure 8 This is a schematic diagram of the cross-sectional structure of the steel strip after it has been corrugated in the second embodiment of this utility model.
[0024] Figure 9 This is a schematic diagram of the steel strip structure in this utility model.
[0025] In the diagram: 1. Pipe body; 10. First crest; 101. Overlap 1; 102. First welding area; 11. Second crest; 110. Second welding area; 12. Inner plastic coating layer; 120. Second overlap area; 13. Outer plastic coating layer; 130. First overlap area; 14. Overlap 2; 15. Outer adhesive layer; 16. Inner adhesive layer; 17. Metal layer; 1a. Steel strip; 1b. Through hole. Detailed Implementation
[0026] The present invention will now be described in further detail with reference to the accompanying drawings. The drawings are simplified schematic diagrams, illustrating only the basic structure of the present invention, and therefore only show the components relevant to the present invention.
[0027] Example 1 Please refer to Figure 1 , Figure 2 , Figure 4 - Figure 6 This utility model provides a fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall, including a metal layer 17, an inner plastic coating layer 12 and an outer plastic coating layer 13 disposed on the inner and outer sides of the metal layer 17, wherein the metal layer 17 is formed by welding the steel strip 1a into a corrugated spiral. Along the width direction of the steel strip 1a, the steel strip 1a is provided with a first lap 101, a second lap 14 and a crest located between the first lap 101 and the second lap 14, wherein the first surface of the second lap 14 near the crest is flush with the second surface of the first lap 101, and the dimension a of the second lap 14 is greater than or equal to the sum of the dimensions b of the first lap 101 and the crest. The first surface is the same side as the crest of the wave, which is edge 2 14, and the second surface is the opposite side of the crest of the wave, which is edge 1 101.
[0028] Specifically, it should be noted that the tube body 1 includes a metal layer 17. During the forming process, the metal layer 17 is formed by corrugating a steel strip 1a using a corrugating machine to create wave crests, then bending and spirally winding it. During spiral winding, adjacent spiral segments can overlap end-to-end or be spaced apart. As a preferred embodiment, in this application, reference is made to... Figure 5 , Figure 6 When the steel strip 1a is corrugated, it forms two overlapping edges 101 and 14 of different lengths on both sides of the crest. The overlapping edges 101 and 14 are staggered in the thickness direction of the plate and are matched with the size a of the overlapping edge 14 and the sum b of the size of the overlapping edge 101 and the crest along the width direction of the steel strip 1a. When the metal layer 17 is formed by spiral bending, the rear spiral segment can be wound around the outside of the overlapping edge 14 of the front spiral segment along the spiral winding direction. By overlapping the crest of the rear spiral segment and the overlapping edge 101 with the front overlapping edge 14, the void area inside the crest can be blocked. The formed metal layer 17 has a flat inner circumferential surface. The overlapping and matching method can effectively improve the structural strength of the metal layer 17 and ensure the flatness of the subsequent inner plastic coating layer 12, which can significantly improve the quality of the pipe.
[0029] It should be noted that both the inner plastic coating layer 12 and the outer plastic coating layer are made of polyethylene, a material commonly used in pipelines in this field. The polyethylene strip is spirally applied to the circumference of the metal layer 17 by a plastic coating equipment. The first overlap area 130 of the outer plastic coating layer 13 is flattened by the pressure roller of the hot press equipment during hot plastic coating. The second overlap area 120 of the inner plastic coating layer 12 is also flattened by the pressure roller during hot plastic coating, so as to ensure the sealing and connection strength of the overlap area of the inner and outer plastic coating layers.
[0030] Furthermore, as a specific implementation method, refer to Figure 5 , Figure 6 The wave crests include a first wave crest 10 and a second wave crest 11. The second wave crest 11 is located on the side of the first wave crest 10 near the edge 14, and the height of the second wave crest 11 is lower than the height of the first wave crest 10.
[0031] Specifically, when processing a wider steel strip 1a, by setting a first peak 10 and a second peak 11, sufficient structural strength is ensured for the metal layer 17 of the subsequently formed pipe, and the wider steel strip 1a improves the efficiency of spiral forming of the metal layer 17. Furthermore, by setting the height of the second peak 11 lower than the height of the first peak 10, structural strength is provided by the second peak 11, and during spiral forming, it is prevented from being too high and affecting the overlap between the subsequent spiral segment and the second overlap 14, thus ensuring forming efficiency.
[0032] Furthermore, as a preferred embodiment, refer to Figure 9The steel strip 1a can be implemented using either perforated or non-perforated steel strip. Specifically, when the steel strip is perforated, through holes 1b are evenly distributed on the steel strip. During the coating process, the molten coating material can permeate each other through the through holes 1b, allowing the inner and outer coating layers to bond together to form an "anchoring" structure. Furthermore, in the wave crest area and on the overlapping edge 14 corresponding to the wave crest, the coating layer can also enter the through holes 1b, allowing for better bonding with the metal layer 17 after cooling. This greatly enhances the connection strength between the coating layer and the metal layer 17, preventing the coating layer from peeling off during long-term use.
[0033] Furthermore, as a preferred embodiment, the steel strip 1a is a hot-dip galvanized steel strip 1a. Hot-dip galvanized steel strip 1a itself has excellent corrosion resistance; its galvanized layer forms the first line of defense against corrosion, effectively resisting the corrosion of the metal layer 17 by the external environment. Simultaneously, the galvanized layer has good compatibility with subsequent plastic coating and adhesive layers, improving the bonding tightness between layers. Compared to ordinary steel strip 1a, hot-dip galvanized steel strip 1a offers stronger corrosion resistance and durability. Combined with a fully plastic-coated structure, this allows the pipeline to better adapt to highly corrosive engineering scenarios such as dampness and acid / alkali environments, significantly extending the pipeline's service life.
[0034] Furthermore, the inner plastic coating 12 and the outer plastic coating 13 are made of PE100 grade polyethylene or polyethylene exceeding the molecular weight limit.
[0035] Furthermore, as a preferred embodiment, refer to Figure 6 Between adjacent spiral segments of steel strip 1a, the second overlap 14 of one spiral segment overlaps with the first overlap 101 and the inner side of the crest of another spiral segment of steel strip. The end of the second overlap 14 is welded to the bottom of the crest through a second welding area 110, and the first surface of the second overlap 14 is welded to the end of the first overlap 101 of the other spiral segment through a first welding area 102. Specifically, through the above arrangement, the double-welded overlap structure completely solves the problem of insufficient compressive strength caused by the gap at the edge of traditional spiral steel pipes: the welding of the second overlap 14 to the bottom of the crest ensures the stability of radial load-bearing capacity, while the welding of the second overlap 14 to the end of the first overlap 101 enhances the axial connection's strength, making the entire metal layer 17 form a continuous and complete load-bearing structure, greatly improving the overall compressive load-bearing capacity of the pipe and breaking through the load-bearing limit of traditional structures. Simultaneously, a flat inner circumferential surface of the metal layer 17 can be obtained.
[0036] Furthermore, both the inner plastic coating layer 12 and the outer plastic coating layer 13 are bonded to the metal layer 17. Specifically, the bonding method ensures a tight fit between the plastic coating layer and the metal layer 17 without gaps, which not only improves the overall integrity and stability of the structure but also effectively blocks the penetration path of corrosive media. Compared with simple mechanical bonding, the bonding connection allows the plastic coating layer to better follow the deformation of the metal layer 17, reducing the risk of interlayer delamination. At the same time, it further improves the flatness of the inner plastic coating layer 12, ensuring smooth fluid transport and avoiding structural strength reduction caused by interlayer gaps.
[0037] Furthermore, both the inner and outer plastic coating layers 12 and 13 are bonded to the metal layer 17 using adhesive resin layers. Specifically, the metal layer 17 has an inner adhesive layer 16 and an outer adhesive layer 15 on its inner and outer sides, respectively. The adhesive resin layer has excellent bonding strength and compatibility, enabling a high-strength and durable connection between the metal layer 17 (such as hot-dip galvanized steel strip 1a) and the plastic coating layer (such as polyolefin) based on their material characteristics. Simultaneously, the adhesive resin, through coating, forms a continuous and complete protective layer on the inner and outer surfaces of the metal layer 17. It possesses certain anti-corrosion properties and can fill minor imperfections and gaps on the surfaces of the metal layer 17 and the plastic coating layer, forming a continuous anti-corrosion barrier and further enhancing the overall anti-corrosion effect of the pipeline. In addition, the adhesive resin layer has good flexibility, which can alleviate the thermal stress difference between the metal layer 17 and the plastic coating layer, reduce the risk of interlayer cracking, and ensure the structural stability of the pipeline under different temperature conditions.
[0038] Example 2 Furthermore, this utility model provides a fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall, for reference. Figure 7 , Figure 8 As a specific implementation method, this embodiment differs from Embodiment 1 in that the wave crest includes a first wave crest 10. Specifically, this simplified wave crest structure reduces the process complexity of steel strip 1a pressure wave forming while ensuring the pipe ring stiffness, and at the same time reduces the contact gap between the inner plastic coating layer 12 and the metal layer 17, further optimizing the bonding effect of the inner plastic coating layer 12.
[0039] A single crest can be adapted to steel strips with a narrower width 1a.
[0040] In some application areas where the stress in the pipe cross section is relatively small, it can also be applied to steel strips with a large width 1a. Compared with the setting of two crests on the same steel strip 1a, the single crest design makes the steel strip 1a easier to form, and the stress it experiences during subsequent spiral bending is also smaller. The roundness of the formed pipe is higher. Combined with the full-coverage overlap of the second 14, it can reduce production difficulty, improve production efficiency, and reduce manufacturing costs.
[0041] Obviously, the above embodiments are merely illustrative examples for clear explanation and are not intended to limit the implementation. Those skilled in the art will recognize that other variations or modifications can be made based on the above description. It is neither necessary nor possible to exhaustively list all possible implementations here. However, obvious variations or modifications derived therefrom are still within the protection scope of this invention.
Claims
1. A fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall, comprising a metal layer (17), an inner plastic coating layer (12) and an outer plastic coating layer (13) disposed on both the inner and outer sides of the metal layer (17), wherein the metal layer (17) is formed by welding a steel strip (1a) into a corrugated spiral, characterized in that, Along the width direction of the steel strip (1a), the steel strip (1a) is provided with a first lap (101), a second lap (14) and a crest located between the first lap (101) and the second lap (14), wherein the first surface of the second lap (14) near the crest is flush with the second surface of the first lap (101), and the dimension a of the second lap (14) is greater than or equal to the sum of the dimensions b of the first lap (101) and the crest; Among them, the first surface is the surface of the second edge (14) on the same side as the crest, and the second surface is the surface of the first edge (101) opposite to the crest.
2. The fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall according to claim 1, characterized in that, The peaks include a first peak (10).
3. The fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall according to claim 1, characterized in that, The crests include a first crest (10) and a second crest (11), the second crest (11) being located on the side of the first crest (10) near the second edge (14), and the height of the second crest (11) being lower than the height of the first crest (10).
4. The fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall according to claim 2 or 3, characterized in that, The steel strip (1a) may be a perforated steel strip or a non-perforated steel strip.
5. The fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall according to claim 4, characterized in that, The steel strip (1a) is hot-dip galvanized steel strip (1a).
6. The fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall according to claim 4, characterized in that, Both the inner plastic coating (12) and the outer plastic coating (13) are made of polyolefin material.
7. The fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall according to claim 4, characterized in that, Between adjacent steel strip spiral segments, the second overlap (14) of one steel strip spiral segment overlaps with the first overlap (101) of another steel strip spiral segment and the inner side of the crest, and the end of the second overlap (14) is welded to the bottom of the crest, and the first surface of the second overlap (14) is welded to the end of the first overlap (101) of another steel strip spiral segment.
8. The fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall according to claim 7, characterized in that, Both the inner plastic coating (12) and the outer plastic coating are bonded to the metal layer (17).
9. The fully corrosion-resistant spiral steel pipe with an outer corrugated peak and an inner flat wall according to claim 8, characterized in that, The inner plastic coating (12) and the outer plastic coating are bonded to the metal layer (17) using an adhesive resin layer.