A thermal management system for a power battery pack

By combining a PI heating film and a silicone heating film into a three-dimensional heating structure, along with limiting adhesive strips and thermal conductive gel, the problems of easy tearing and uneven temperature of the power battery heating film are solved, thereby improving battery performance and safety.

CN224986405UActive Publication Date: 2026-11-17JIANGXI JINGWEI HENGRUN TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522470252.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-20
Publication Date
2026-11-17
Estimated Expiration
2035-11-20

AI Technical Summary

Technical Problem

Existing power battery heating methods are prone to causing the heating film to tear and resulting in uneven temperature, which affects battery performance and safety.

Method used

A three-dimensional heating structure combining PI heating film and silicone heating film, along with limiting strips and thermally conductive gel, forms an all-round heating and stable support, and is combined with a liquid cooling plate for thermal management.

Benefits of technology

It achieves uniform heating of the battery temperature, prevents damage to the heating film, improves battery performance and lifespan, and enhances structural reliability and thermal management efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224986405U_ABST
    Figure CN224986405U_ABST
Patent Text Reader

Abstract

This specification discloses a thermal management system for a power battery pack. The power battery pack includes multiple cell groups, each cell group consisting of multiple individual cells arranged in a predetermined direction. The thermal management system includes: first and second PI heating films disposed on the outer surfaces of the two outermost cell groups; a silicone heating film attached to the mating surfaces of adjacent cell groups; two first limiting adhesive strips; several second limiting adhesive strips; thermally conductive gel; and a liquid cooling plate. The liquid cooling plate is located at the bottom of the cell group. The first limiting adhesive strips are attached to the top two ends of the liquid cooling plate, supporting the bottom outer edges of the outermost cell groups. The second limiting adhesive strips are spaced apart between the bottom edges of adjacent cell groups. All limiting adhesive strips are single-sided adhesive. The silicone heating films are double-sided adhesive, and the thermally conductive gel is applied between the liquid cooling plate and the cell groups.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of electric vehicle technology, and more specifically, to a thermal management system for a power battery pack. Background Technology

[0002] With increasing global environmental awareness and the rapid development of automotive technology, electric vehicles are becoming increasingly widely used in daily life due to their significant advantages such as zero emissions and low noise. As the core energy source of electric vehicles, the performance and safety of the battery pack directly determine the overall performance of the vehicle. Lithium-ion batteries, with their high energy density and long cycle life, have become the preferred choice for power batteries. However, lithium-ion batteries are extremely sensitive to temperature changes, with a narrow optimal operating temperature range that must be maintained within a suitable range, such as 20-40℃. When the operating temperature is below this range, the rate of chemical reactions inside the battery decreases, leading to an irreversible reduction in battery capacity and severely affecting the driving range of electric vehicles. On the other hand, excessively high temperatures not only shorten the cycle life of the battery but may also trigger thermal runaway, potentially leading to vehicle fires and posing a serious threat to the lives of passengers. Furthermore, uneven temperature distribution between batteries can cause differences in the rate of chemical reactions within the batteries, exacerbating battery inconsistency and negatively impacting the overall charge and discharge behavior of the battery pack, thus reducing overall battery performance. Therefore, the temperature difference between individual battery cells should be controlled below a certain temperature range.

[0003] Currently, in the field of power battery cooling, indirect liquid cooling technology has become the most widely used cooling method due to its advantages such as high cooling efficiency and low short-circuit risk. This method indirectly cools the battery by circulating coolant within structures such as cold plates and pipes. However, existing technologies have many problems in power battery heating. The common heating method currently is to directly attach a heating film made of resistance wire to the outer surface of the battery, and heat it by power from an internal or external charger. However, this method has obvious drawbacks: the battery cell expands during charging and discharging, which can easily cause the heating film to tear, leading to the breakage of the heating wire. Summary of the Invention

[0004] This specification provides a thermal management system for a power battery pack to overcome at least one technical problem existing in the related art.

[0005] According to embodiments of this specification, a thermal management system for a power battery pack is provided. The power battery pack includes multiple cell groups, each cell group consisting of multiple individual cells arranged sequentially according to a predetermined rule. The thermal management system includes: a first PI heating film disposed on the outer surface of a first cell group of the power battery pack; a second PI heating film disposed on the outer surface of a second cell group of the power battery pack; silicone heating films disposed on the side mating surfaces of every two adjacent cell groups in the plurality of cell groups; two first limiting adhesive strips; several second limiting adhesive strips; thermally conductive gel; and a liquid cooling plate. The first cell group and the second cell group are the two outermost cell assemblies of the power battery pack, each cell assembly consisting of several individual cells. The silicone heating films are adhered to the side mating surfaces of adjacent cell groups using double-sided adhesive. The liquid cooling plate is disposed at the bottom of the plurality of battery cell groups. The two first limiting adhesive strips are respectively located at both ends of the top of the liquid cooling plate, and are used to support the bottom positions of the first battery cell group and the second battery cell group near the outer side. The plurality of second limiting adhesive strips are spaced apart along the arrangement direction of the plurality of battery cell groups, and each second limiting adhesive strip is correspondingly disposed between the bottoms of two adjacent battery cell groups. The first limiting adhesive strips and the second limiting adhesive strips are attached to the corresponding positions on the top of the liquid cooling plate with single-sided adhesive. The thermally conductive gel is applied between the liquid cooling plate and the battery cells.

[0006] In some optional embodiments, the first PI heating film, the second PI heating film, and the silicone heating film all include: The heating film body is bonded to the surface of the corresponding battery cell assembly via adhesive backing; wherein, the first PI heating film and the second PI heating film are bonded to the outer surface of the corresponding battery cell assembly via single-sided adhesive backing, and the silicone heating film is bonded to the side mating surfaces of two adjacent battery cell assemblies via double-sided adhesive backing; the heating film bodies of the first PI heating film and the second PI heating film are made of PI material, and the heating film body of the silicone heating film is made of silicone material. The wire outlet is located at one end of the heating film body. The wire outlet is made of silicone material and has an anti-wear layer on the outside. The first connecting wire harness and the second connecting wire harness are respectively led out from the outlet end; An input connector and an output connector; wherein the input connector is connected to the first connection harness, and the output connector is connected to the second connection harness; The input connector of the first PI heating film is plugged into the input terminal of the heating power supply at the battery pack end. The output connector of the first PI heating film is plugged into the input connector of the adjacent silicone heating film. The output connector of the adjacent silicone heating film is plugged into the input connector of its next silicone heating film. The output connector of the second PI heating film is plugged into the output terminal of the heating power supply at the battery pack end. The input connector of the second PI heating film is plugged into the output connector of the previous silicone heating film. The output terminal of the internal silicone heating film forms a series path with its adjacent silicone heating film through the input connector and the output connector.

[0007] In some optional embodiments, the surfaces of the heating film bodies of the first PI heating film and the second PI heating film are provided with a plurality of openings, the distribution of which is aligned with the gaps between adjacent cells in the plurality of cells of the cell group to which the PI heating film is attached; the surface of the silicone heating film is free of openings.

[0008] In some alternative embodiments, the edge of the opening is provided with annular reinforcing ribs protruding toward the surface of the heating film body on which it is located.

[0009] In some alternative embodiments, the width of the second limiting strip is greater than the width of the first limiting strip.

[0010] In some alternative embodiments, the liquid cooling plate includes: The first base plate and the second base plate are connected by friction stir welding, forming four independent flow channels inside; The first sealing component, the second sealing component, the third sealing component, and the fourth sealing component are respectively sealed to the ends of the first base plate and the second base plate by friction stir welding and argon arc welding; The inlet and outlet are fixed to the top of the liquid cooling plate by argon arc welding. in, The four independent flow channels are arranged in parallel to form a four-in-four-out structure. The cross-section of each flow channel is a closed U-shape, and it is integrally formed inside the first and second base plates by aluminum extrusion. The inner wall of the flow channel is machined to form a smooth flow surface. The first base plate, the first sealing component, the second sealing component, the third sealing component, the fourth sealing component, the inlet and the outlet are all made of aluminum alloy.

[0011] In some alternative embodiments, the inner wall of the flow channel of the liquid cooling plate is provided with a corrosion-resistant surface treatment coating. In some optional embodiments, the thickness of the first limiting adhesive strip and the second limiting adhesive strip is matched with the coating thickness of the thermally conductive gel to control the amount of adhesive overflow of the thermally conductive gel.

[0012] In some alternative embodiments, the bottom outer surface of the liquid cooling plate is provided with an array of heat dissipation fins.

[0013] In some alternative embodiments, the first and second limiting strips are made of thermally conductive silicone or thermally conductive foam.

[0014] The technical solution of this application has several significant technical advantages, as detailed below: 1. By setting symmetrical PI heating films on both sides of the outer surface of the battery cell, and cooperating with the silicone heating film on the mating surface of adjacent battery cells, a comprehensive three-dimensional heating structure is formed. This layout can quickly and uniformly heat the battery cell in low-temperature environments, avoiding temperature gradient problems caused by unilateral or localized heating, significantly reducing the temperature difference on the battery cell surface, effectively ensuring that the battery cell is in the suitable operating temperature range under low-temperature conditions, and improving the battery's charging and discharging performance and service life.

[0015] 2. The first and second limiting adhesive strips are designed in conjunction to limit and fix the two ends of the cell array and the bottom of adjacent cell groups, respectively. This effectively prevents the cells from shifting within the battery pack and avoids the risk of insulation failure caused by damage to the blue film at the bottom of the cells. Simultaneously, the limiting adhesive strips restrict the thickness and amount of thermally conductive adhesive at the bottom of the cells, ensuring uniform distribution of the adhesive, maintaining stable thermal conductivity, and enhancing the structural reliability of the battery pack under complex operating conditions such as vibration and impact.

[0016] 3. The thermally conductive gel is applied between the liquid cooling plate and the battery cell, effectively filling the tiny gaps between them, significantly reducing thermal resistance and enhancing heat transfer efficiency. During heating and cooling, the thermally conductive gel works in conjunction with components such as the liquid cooling plate and heating film to ensure rapid and stable heat transfer, accelerate the cell temperature regulation process, improve the overall efficiency of the thermal management system, and ensure efficient operation of the battery pack. Attached Figure Description

[0017] To more clearly illustrate the technical solutions in the embodiments or related technologies of this specification, the drawings used in the description of the embodiments or related technologies will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this utility model. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0018] Figure 1 Exploded view of the structure of a thermal management system for a power battery pack provided by this utility model; Figure 2 A structural diagram of the thermal management assembly in the thermal management system of the power battery pack provided by this utility model; Figure 3A cross-sectional view of the thermal management assembly in the thermal management system of the power battery pack provided by this utility model; Figure 4 A partial enlarged view of the vicinity of the second limiting rubber strip in the thermal management system of the power battery pack provided by this utility model; Figure 5 Structural diagram of the heating film assembly in the thermal management system of the power battery pack provided by this utility model; Figure 6 A comparative schematic diagram of the heating film with and without openings in the thermal management system of the power battery pack provided by this utility model; Figure 7 A front view of the thermal management assembly structure in the thermal management system of the power battery pack provided by this utility model; Figure 8 Structural diagram of the liquid cooling plate assembly in the thermal management system of the power battery pack provided by this utility model; Figure 9 A cross-sectional view of the liquid cooling plate flow channel in the thermal management system of the power battery pack provided by this utility model; Figure 10 Design drawing of the liquid cooling plate flow channel in the thermal management system of the power battery pack provided by this utility model; Figure 11 This is a design drawing of the liquid cooling plate flow channel in the existing technology.

[0019] Wherein, 1 represents a battery cell, 11 represents the first battery cell group, 12 represents the third battery cell group, and 13 represents the second battery cell group; 2 represents a PI heating film, 21 represents the first PI heating film, 22 represents the second PI heating film, 211 represents the body of the first PI heating film, 212 represents the lead-out end of the first PI heating film, 213 represents the first wire harness, 214 represents the second wire harness, 215 represents the first connector, 216 represents the second connector, and 217 represents an opening; 3 represents a silicone heating film, 31 represents the first silicone heating film, 32 represents the second silicone heating film, 321 represents the body of the second silicone heating film, and 322 represents the second silicone heating film... At the outlet of the thermal film, 323 represents the third wiring harness, 324 represents the fourth wiring harness, 325 represents the third connector, and 326 represents the fourth connector; 4 represents the first limiting adhesive strip, 41 represents the first first limiting adhesive strip, and 42 represents the second first limiting adhesive strip; 5 represents the second limiting adhesive strip, 51 represents the first second limiting adhesive strip, and 52 represents the second second limiting adhesive strip; 6 represents thermally conductive gel; 7 represents the liquid cooling plate, 711 represents the water outlet, 712 represents the water inlet, 72 represents the first base plate, 73 represents the first sealing component, 74 represents the second sealing component, 75 represents the third sealing component, 76 represents the second base plate, and 77 represents the fourth sealing component. Detailed Implementation

[0020] The present invention will now be described in further detail with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the present invention and not intended to limit it. Furthermore, it should be noted that, for ease of description, the accompanying drawings show only the parts relevant to the present invention, not the entire structure.

[0021] In the description of this utility model, unless otherwise explicitly specified and limited, the terms "connected," "linked," and "fixed" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this utility model based on the specific circumstances.

[0022] In this invention, unless otherwise explicitly specified and limited, "above" or "below" the second feature can include direct contact between the first and second features, or contact between the first and second features through another feature between them. Furthermore, "above," "over," and "on top" of the second feature includes the first feature directly above or diagonally above the second feature, or simply indicates that the first feature is at a higher horizontal level than the second feature. "Below," "below," and "under" the second feature includes the first feature directly below or diagonally below the second feature, or simply indicates that the first feature is at a lower horizontal level than the second feature.

[0023] In the description of this embodiment, the terms "upper," "lower," "right," etc., refer to the orientation or positional relationship shown in the accompanying drawings. They are used only for ease of description and simplification of operation, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this utility model. In addition, the terms "first" and "second" are only used for distinction in description and have no special meaning.

[0024] Before introducing the technical solution of this application, the basic structure of a power battery will be explained. The main components of a power battery include cells, modules, and battery packs. A cell is the basic unit of a battery, a module is multiple cells assembled together in a specific way, and a battery pack is a complete battery system that further integrates multiple modules and a management system. A cell is the smallest energy storage unit of a battery system, typically composed of positive and negative electrode materials, an electrolyte, and a separator, and it stores and releases electrical energy through electrochemical reactions.

[0025] The structure of the thermal management system for the power battery pack provided in the embodiments of this specification will be described in detail below with reference to the accompanying drawings. Figure 1 As shown, Figure 1 An exploded view of the structure of a thermal management system for a power battery pack provided by this utility model. Figure 2 This is a structural diagram of the thermal management assembly in the thermal management system of the power battery pack. Figure 3 A cross-sectional view of the thermal management assembly in the thermal management system of the power battery pack provided by this utility model.

[0026] In this application's technical solution, the power battery pack may include multiple cell groups, each cell group consisting of multiple individual cells 1 arranged sequentially according to a predetermined rule. To clearly illustrate this application's technical solution, the structure of the power battery pack's thermal management system provided by this application's technical solution is described below using a power battery pack comprising three cell groups as an example. Figure 1 As shown, the thermal management system may include: A first PI heating film 21 is disposed on the outer surface of the first cell group 11 of the power battery pack, and a second PI heating film 22 is disposed on the outer surface of the second cell group 13 of the power battery pack. Figure 1 In the exploded structural diagram, for clarity, the first PI heating film 21 and the second PI heating film 22 are not labeled separately, but are uniformly represented by the number 2; the silicone heating film 3 is respectively disposed on the side mating surfaces of every two adjacent battery cell groups in multiple battery cell groups; and the two first limiting adhesive strips 4 (for example, in...) Figure 3 In the diagram, 41 represents the first first limiting adhesive strip, 42 represents the second first limiting adhesive strip), several second limiting adhesive strips 5, thermal conductive gel 6, and liquid cooling plate 7; wherein, the first cell group 11 and the second cell group 13 are the two outermost cell assemblies of the power battery pack, and the cell assembly is composed of several individual cells 1.

[0027] A liquid cooling plate 7 is disposed at the bottom of multiple battery cell groups. Two first limiting adhesive strips 4 are respectively located at the two ends of the top of the liquid cooling plate 7, and are used to support the bottom positions of the first battery cell group 11 and the second battery cell group 13 near the outer side. Several second limiting adhesive strips 5 are arranged at intervals along the arrangement direction of the multiple battery cell groups, and each second limiting adhesive strip 5 is correspondingly disposed between the bottoms of two adjacent battery cell groups. The first limiting adhesive strips 4 and the second limiting adhesive strips 5 are pasted to the corresponding positions on the top of the liquid cooling plate 7 with single-sided adhesive. Thermal conductive gel 6 is applied between the liquid cooling plate 7 and the battery cell 1.

[0028] In the above technical solution, the battery cells in the power battery pack are usually arranged in a dense row and column pattern, with regular gaps between the bottoms of adjacent battery cells. The second limiting strip 5 is spaced along the arrangement direction of the battery cells, with each strip corresponding to the bottom gap of a group of adjacent battery cells (e.g., ...). Figure 3In the middle, the bottom gaps between the first cell group 11 and the third cell group 12, and between the third cell group 12 and the second cell group 13, are arranged in a "one-to-one correspondence" manner to achieve full coverage support for all gaps between adjacent cell groups. This multi-strip arrangement strictly matches the arrangement period of the cell groups, ensuring that each gap area has a corresponding limiting strip to prevent displacement of the bottom of the cell due to lack of support. Figure 3 As shown, Figure 3 There are 3 battery cell groups, therefore, two second limiting adhesive strips, the first second limiting adhesive strip 51 and the second second limiting adhesive strip 52, and two silicone heating films are required. Figure 3 The first silicone heating film 31 and the second silicone heating film 32 are illustrated in the diagram. Figure 4 As shown, Figure 4 A partial enlarged view of the vicinity of the first second limiting rubber strip 51 in the thermal management system of the power battery pack provided by this utility model, from... Figure 4 It can be clearly seen that each second limiting strip corresponds to the bottom gap of a group of adjacent battery cells.

[0029] Meanwhile, considering that the core function of the first limiting adhesive strip 4 and the second limiting adhesive strip 5 is to support the bottom of the battery cell and prevent the battery cell from directly contacting the liquid cooling plate 7 and causing damage to the blue film, and to control the amount of adhesive overflow of the thermal conductive gel 6 by matching the thickness, in the above technical solution, the first limiting adhesive strip 4 and the second limiting adhesive strip 5 are pasted to the corresponding positions on the top of the liquid cooling plate 7 with single-sided adhesive. The single-sided adhesive is only set on the contact surface of the "adhesive strip-liquid cooling plate", while the contact surface of the "adhesive strip-battery cell" remains unadhesive. In this way, after the single-sided adhesive is fixed, the unadhesive side can be freely compressed as the battery cell expands.

[0030] In this application's technical solution, symmetrical PI heating films are set on the outer surfaces of both sides of the battery cell, combined with silicone heating films on the mating surfaces of adjacent battery cells, forming a comprehensive three-dimensional heating structure. This layout can rapidly and uniformly heat the battery cell in low-temperature environments, avoiding temperature gradient problems caused by unilateral or localized heating, significantly reducing the temperature difference on the battery cell surface, and effectively ensuring that the battery cell remains within its suitable operating temperature range under low-temperature conditions, thus improving battery charging and discharging performance and lifespan. Simultaneously, the first limiting adhesive strip 4 and the second limiting adhesive strip 5 are collaboratively set to limit and fix the ends of the battery cell array and the bottom of adjacent battery cell groups, effectively preventing displacement of the battery cells within the battery pack and avoiding the risk of insulation failure due to damage to the blue film at the bottom of the battery cell. Furthermore, the limiting adhesive strips limit the thickness and overflow of the thermally conductive adhesive at the bottom of the battery cell, ensuring uniform distribution of the thermally conductive adhesive, maintaining stable thermal conductivity, and enhancing the structural reliability of the battery pack under complex conditions such as vibration and impact. The thermally conductive gel 6 is applied between the liquid cooling plate 7 and the bottom of the battery cell, effectively filling the tiny gaps between them, significantly reducing thermal resistance, and enhancing thermal conductivity efficiency. During the heating and cooling process, the thermally conductive gel 6 works in conjunction with components such as the liquid cooling plate 7 and the heating film to transfer heat quickly and stably, accelerate the cell temperature regulation process, improve the overall efficiency of the thermal management system, and ensure the efficient operation of the power battery pack.

[0031] Based on the technical solutions described above, some more specific technical solutions are provided below, which will be elaborated on separately.

[0032] Taking a power battery pack consisting of three cell groups as an example, such as Figure 5 As shown, Figure 5 This is a structural diagram of the heating film assembly in the thermal management system of the power battery pack provided by this utility model. In an optional embodiment, the first PI heating film 21, the second PI heating film 22, and the silicone heating film 3 may all include: The heating film body is bonded to the surface of the corresponding battery cell assembly using an adhesive backing method; wherein, the first PI heating film 21 and the second PI heating film 22 are bonded to the outer surface of the corresponding battery cell assembly using a single-sided adhesive backing method, and the silicone heating film 3 is bonded to the side mating surfaces of two adjacent battery cell assemblies using a double-sided adhesive backing method; the heating film bodies of the first PI heating film 21 and the second PI heating film 22 are made of PI material, and the heating film body of the silicone heating film 3 is made of silicone material. The wire outlet is located at one end of the heating film body. The wire outlet is made of silicone material and has an anti-wear layer on the outside. The first connecting wire harness and the second connecting wire harness are respectively led out from the outlet end; An input connector and an output connector; wherein the input connector is connected to the first connection harness, and the output connector is connected to the second connection harness; The input connector of the first PI heating film 21 is plugged into the input terminal of the heating power supply at the battery pack end. The output connector of the first PI heating film 21 is plugged into the input connector of the adjacent silicone heating film. The output connector of the adjacent silicone heating film is plugged into the input connector of its next silicone heating film. The output connector of the second PI heating film 22 is plugged into the output terminal of the heating power supply at the battery pack end. The input connector of the second PI heating film 22 is plugged into the output connector of the previous silicone heating film. The output terminal of the internal silicone heating film forms a series path with its adjacent silicone heating film through the input connector and the output connector.

[0033] Figure 5 In this embodiment, 211 represents the body of the first PI heating film, 212 represents the output terminal of the first PI heating film, 213 represents the first wire harness, 214 represents the second wire harness, 215 represents the first connector, 216 represents the second connector, and 217 represents the opening; 3 represents the silicone heating film, 31 represents the first silicone heating film, 32 represents the second silicone heating film, 321 represents the body of the second silicone heating film, 322 represents the output terminal of the second silicone heating film, 323 represents the third wire harness, 324 represents the fourth wire harness, 325 represents the third connector, and 326 represents the fourth connector. In this embodiment, both output terminals 212 and 322 are made of silicone, with an external anti-wear layer added to prevent insulation failure due to friction with other metal parts. Each heating film has two wire harnesses and two connectors, and the internal and external wire harnesses of the heating film are connected in series, using a one-in-one-out configuration. Connector 216 of the PI heating film 21 is plugged into the input terminal of the heating connector on the battery pack side. Its internal wiring is also in series. Lead-out wire harness 213 connects to connector 215. Connector 325 on the silicone heating film 32 is plugged into connector 215 on the PI heating film 21, serving as the input terminal of the silicone heating film 32. Through wire harness 323 and the series wiring inside the heating film, lead-out wire harness 326 connects to connector 326. Similarly, the four heating films are connected in series via wire harnesses and connectors. Finally, connector 225 serves as the output terminal and plugs into the output terminal of the heating connector on the battery pack side, forming a heating circuit. The assembled schematic diagram is shown below. Figure 7 As shown, this method of connecting the wiring harness is simple, easy for workers to operate, and can save space at the front end of the battery pack.

[0034] In an optional embodiment, the surface of the heating film body of the first PI heating film 21 and the second PI heating film 22 may be provided with a plurality of openings, the distribution of which is aligned with the gap between adjacent cells in the plurality of cells of the cell group to which the PI heating film 2 is attached; the surface of the silicone heating film 3 has no openings.

[0035] In this embodiment, considering that the volume of a power battery cell (such as a ternary lithium battery) undergoes periodic expansion and contraction during charging and discharging due to lithium ion insertion / extraction, if the heating film has no openings, the cell expansion force will directly act on the film, causing the heating wire inside the heating film to break due to tearing. In this embodiment, multiple openings 217 are provided on the surface of the heating film body of the first cell group 11 and the second PI heating film 22, such as... Figure 6 As shown, Figure 6 This is a comparative schematic diagram showing the heating film with and without openings in the thermal management system of the power battery pack provided by this utility model. Figure 6 The upper center shows a design with a 217 aperture, while the lower center shows a comparison design without an aperture. Figure 6 As shown, the opening 217 is a longitudinally elongated strip, the length of which is adapted to the extension direction of the gap between the battery cells (assuming the battery cells are arranged laterally, and the gaps between adjacent battery cells are distributed longitudinally). The design of the opening allows the expansion stress to be released through the gap between the battery cells, effectively reducing the tensile stress borne by the heating film. This design utilizes the large tensile deformation of the PI material itself, and further enhances the elastic deformation capability of the film through the opening. Combined with the single-sided adhesive bonding method, the heating film can elastically deform with the opening during the expansion of the battery cells, maintaining close contact with the surface of the battery cells and avoiding structural damage caused by hard compression.

[0036] Meanwhile, considering the natural gaps between battery cells, if the heating wires are evenly distributed on the film surface, the heating wires in the gaps are prone to heat accumulation due to lack of contact with the battery cells for heat dissipation, leading to localized dry burning. The opening position of the PI heating film is located precisely above the gap between the battery cells. The air channel formed by the opening 217 promotes natural convection, while also creating a "avoidance area" for the heating wires in the gaps, reducing the distribution of heating wires in this area, and preventing the heating film from wrinkling due to the expansion and compression of the battery cells in the gaps.

[0037] In an optional embodiment, the width of the second limiting strip 5 is greater than the width of the first limiting strip 4.

[0038] In this embodiment, each second limiting adhesive strip 5 is correspondingly disposed between the bottoms of two adjacent battery cell groups in the plurality of battery cell groups.

[0039] The width of the second limiting strip 5 is greater than that of the first limiting strip 4. This design is based on the different installation positions and stress requirements of the limiting strips between the liquid cooling plate and the battery cell, aiming to achieve more precise support and constraint through differentiated width design. The second limiting strip 5 is usually placed in the middle of the battery cell assembly or in areas with greater stress. It needs to withstand greater forces when facing battery cell expansion or external pressure. Therefore, a wider width can provide stronger support rigidity, ensuring that the thermal conductive gel thickness in this area is uniform and does not overflow excessively. At the same time, it effectively prevents the bottom of the battery cell from contacting the upper surface of the liquid cooling plate to protect the blue film insulation. On the other hand, the first limiting strip 4 is mostly placed at the edge of the battery cell assembly, where the stress is relatively small. A narrower width is sufficient to meet the constraint requirements of the edge area. This width difference design not only ensures the support strength of the critical area but also avoids material waste. Through the reasonable width ratio, it achieves precise control of the amount of thermal conductive gel overflow and effective support for the bottom of the battery cell, improving the reliability of the thermal management system while optimizing the overall structural design.

[0040] In an optional embodiment, the liquid cooling plate 7 may include: The first base plate 72 and the second base plate 76 are connected by friction stir welding, forming four independent flow channels inside; The first sealing element 73, the second sealing element 74, the third sealing element 75 and the fourth sealing element 77 are respectively sealed to the ends of the first base plate 72 and the second base plate 76 by friction stir welding and argon arc welding; The inlet 712 and outlet 711 are fixed to the top of the liquid cooling plate 7 by argon arc welding; in, The four independent flow channels are arranged in parallel to form a four-in-four-out structure. The cross-section of each flow channel is a closed U-shape, and it is integrally formed inside the first base plate 72 and the second base plate 76 by aluminum extrusion. The inner wall of the flow channel is machined to form a smooth flow surface. The first base plate 72, the first sealing component 73, the second sealing component 74, the third sealing component 75 and the fourth sealing component 77, the water inlet 712 and the water outlet 711 can all be made of aluminum alloy 6061.

[0041] like Figure 8 and 9As shown in the technical solution of this embodiment, the first base plate 72 and the second base plate 76 are spliced ​​together by friction stir welding, and four independent flow channels (U-shaped cross-section) are integrally formed inside, constituting the main body of the liquid cooling plate 7 and the flow channel cavity. Four sealing components—first sealing component 73, second sealing component 74, third sealing component 75, and fourth sealing component 77—are distributed at the ends of the base plates and on both sides of the splicing seam, and are sealed together by friction stir welding and argon arc welding. Their function is to separate the parallel flow channels (dividing the single cavity into four independent flow channels, forming a "four-in, four-out" layout) and to seal the ends of the flow channels to prevent coolant leakage. The outlet 711 and the inlet 712 are fixed to the top of the liquid cooling plate 7 by argon arc welding, serving as the inlet and outlet interfaces for coolant, enabling connection to the external cooling system. Both the outlet 711 and the inlet 712 can be machined parts or standard parts.

[0042] The first base plate 72 and the second base plate 76 are connected by friction stir welding. Both have flow channels arranged inside, and the cross-section of the flow channels is formed by aluminum extrusion. The cross-section of the flow channels is as follows: Figure 9 As shown, the flow channel cross-section is U-shaped, which is simple and easy to process. From a manufacturing cost perspective, aluminum extrusion dies are less expensive than those for stamping and die-casting liquid cooling plates, allowing for better cost control. From a design perspective, the internal structure of the aluminum extrusion flow channel is simple and easy to process, and the flatness of the extruded aluminum is better controlled than that of stamping and die-casting liquid cooling plates, reducing the amount of thermally conductive adhesive used. To facilitate coolant flow, a disc milling cutter can be used to cut the bottom plate flow channel after aluminum extrusion; this processing method is more efficient than side milling cutters. Traditional single-inlet / single-outlet or single-inlet / double-outlet liquid cooling plates require coolant diversion and convergence within the liquid cooling plate, leading to a complex flow channel design and significant pressure drop. The flow channel arrangement in this embodiment uses a four-channel parallel configuration, which, compared to a traditional two-inlet / two-outlet die-casting liquid cooling plate, is significantly improved. Figure 10 and 11 As shown in the figure, the four-in-four-out structure design is simple, while the two-in-two-out design is complex. The four-in-four-out structure can significantly reduce the flow path of a single channel of the cooling medium, reduce flow resistance, reduce internal pressure drop loss, and improve the temperature uniformity of the battery pack. Through steady-state flow simulation analysis, compared with the traditional two-in-two-out die-cast liquid cooling plate, it can reduce flow resistance, and under the same inlet flow rate, the inlet and outlet pressure drop can be significantly reduced. In the optional embodiment, the thickness of the first limiting adhesive strip 4 and the second limiting adhesive strip 5 matches the coating thickness of the thermally conductive gel 6 to control the amount of overflow of the thermally conductive gel 6.

[0043] In this embodiment, the thicknesses of the first limiting adhesive strip 4 and the second limiting adhesive strip 5 match the coating thickness of the thermally conductive gel 6. This thickness matching creates a physical constraint on the thermally conductive gel 6, thereby controlling the amount of adhesive overflow. The limiting adhesive strips are attached to the top of the liquid cooling plate 7 using a single-sided adhesive method, located between the liquid cooling plate 7 and the battery cell. Their thickness is designed based on the target coating thickness of the thermally conductive gel 6. Utilizing the elastic compression properties of the adhesive strips themselves, they are compressed during assembly and then match the target thickness of the thermally conductive gel 6. This forms an annular constraint boundary between the liquid cooling plate and the bottom of the battery cell, confining the thermally conductive gel 6 within a specified area and preventing it from overflowing into non-thermally conductive areas. This design precisely matches the thickness of the thermal conductive gel 6 by using the thickness of the limiting adhesive strip. By utilizing the physical blocking and elastic deformation characteristics of the adhesive strip, it effectively controls the amount of thermal conductive gel 6 overflowing, while ensuring the uniform thickness of the thermal conductive gel 6. This ensures good thermal conductivity and avoids problems such as increased thermal resistance and battery pack component contamination caused by overflowing adhesive. It also prevents the bottom of the battery cell from directly contacting the upper surface of the liquid cooling plate, protecting the blue film on the bottom of the battery cell and providing insulation. This design improves the reliability and stability of the assembly process while ensuring thermal conductivity.

[0044] In an optional embodiment, the edge of the opening is provided with annular reinforcing ribs protruding toward the surface of the heating film body.

[0045] In this embodiment, an annular reinforcing rib protruding towards the surface of the heating film body is provided at the edge of the opening. This annular reinforcing rib can be integrally formed using the same polyimide material as the PI heating film substrate through molding or photolithography, forming a continuous protruding structure surrounding the edge of the opening. Therefore, when the battery cell expands during charge-discharge cycles, the annular reinforcing rib increases the sectional modulus of the opening edge, thereby improving the bending stiffness of that area. This allows the expansion stress to be more evenly distributed to the surrounding film area, thus inhibiting the initiation and propagation of microcracks at the opening edge where stress concentration is greatest.

[0046] In an optional embodiment, the inner wall of the flow channel of the liquid cooling plate 7 is provided with a corrosion-resistant surface treatment coating.

[0047] In this embodiment, the inner wall of the flow channel of the liquid cooling plate 7 is provided with a corrosion-resistant surface treatment coating. This coating can form a dense inorganic protective layer on the inner surface of the aluminum alloy flow channel through micro-arc oxidation or chemical nickel plating process, thereby effectively isolating the coolant from direct contact with the aluminum alloy substrate and preventing corrosion and oxidation inside the flow channel caused by free ions that may be contained in the coolant or by electrochemical action during use, thereby improving the structural integrity and reliability of the liquid cooling plate during long-term use.

[0048] In an optional embodiment, the width of the second limiting adhesive strip 5 is greater than the width of the first limiting adhesive strip 4.

[0049] In this embodiment, the design that the width of the second limiting adhesive strip 5 is greater than the width of the first limiting adhesive strip 4 is mainly based on the following considerations: from Figure 1 and Figure 3 From the layout, in the technical solution of this application, the two first limiting adhesive strips 4 are respectively located at the bottom edges of the first battery cell 11 and the second battery cell 13, that is, as shown in the figure. Figure 3 As shown, the first limiting strip 41 is located between the liquid cooling plate 7 and the bottom edge of the first cell assembly 11 near the outer side, and the second limiting strip 42 is located between the liquid cooling plate 7 and the bottom edge of the second cell assembly 13 near the outer side. The space in this location is relatively limited, and the narrower width design avoids interference with other edge components of the battery pack (such as side panels and wiring harnesses), ensuring a compact installation. The second limiting strip 5 is located in the middle interval area at the bottom of the cell assembly, requiring support for a larger area of ​​the cell bottom to prevent contact between the cells in the middle area and the liquid cooling plate 7. The wider width enhances the support force on the middle area. Therefore, when the battery pack expands during charging and discharging or is subjected to external vibrations, this design can improve the support strength and stability of the middle area of ​​the cell, maintaining the overall mechanical balance of the cell. Meanwhile, since the thermally conductive adhesive is a paste-like fluid, if the amount applied exceeds the gap volume between the liquid cooling plate and the bottom of the battery cell, or if the application is uneven, the adhesive is prone to overflowing out of the gap when the battery cell is squeezed after installation. The first limiting adhesive strip 4 and the second limiting adhesive strip 5 have the same thickness and are attached to the top of the liquid cooling plate 7 with single-sided adhesive. Their thickness is consistent with the designed thickness of the thermally conductive adhesive (e.g., 0.5~1mm), forming a "height-fixed limiting space" between the liquid cooling plate 7 and the bottom of the battery cell. At the same time, the adhesive strips are distributed along the battery cell arrangement direction at both ends of the bottom and between adjacent battery cells, forming a grid-like limiting structure that confines the thermally conductive adhesive within the contact area between the liquid cooling plate and the bottom of the battery cell assembly, preventing the adhesive from spreading to non-thermally conductive areas such as the liquid cooling plate flow channels and electrical connection parts.

[0050] In an optional embodiment, a heat dissipation fin array is provided on the bottom outer surface of the liquid cooling plate 7.

[0051] In this embodiment, a heat dissipation fin array is provided on the bottom outer surface of the liquid cooling plate 7. This heat dissipation fin array can be integrally formed with the bottom plate of the liquid cooling plate 7 through aluminum extrusion or fixedly connected to the bottom outer surface of the liquid cooling plate 7 by welding. The heat dissipation fin array consists of multiple parallel fins, and the extension direction of the fins is parallel or perpendicular to the direction of the internal flow channel of the liquid cooling plate 7, thereby enhancing the passive heat dissipation capability by increasing the contact area between the liquid cooling plate 7 and the outside air. When the battery pack is in a high-temperature environment and the liquid cooling system malfunctions or has insufficient power, the heat dissipation fin array can remove the residual heat transferred from the battery cells to the liquid cooling plate 7 via the thermally conductive gel 6 through natural convection and radiation, preventing heat accumulation in the battery pack.

[0052] In an optional embodiment, the first limiting strip 4 and the second limiting strip 5 are made of thermally conductive silicone or thermally conductive foam.

[0053] In this embodiment, the first limiting strip 4 and the second limiting strip 5 are made of thermally conductive silicone or thermally conductive foam. When thermally conductive silicone is selected, it has good elastic deformation capability and insulation properties. It can effectively absorb the expansion stress during the charging and discharging process of the battery cell through compression deformation, maintain a stable support spacing to control the thickness of the thermally conductive gel 6, and due to its large thermal conductivity, it can transform from a heat insulation component into an auxiliary heat conduction path. When heat from the bottom of the battery cell is conducted to the limiting strip, it can diffuse laterally to adjacent areas or be transferred downward to the liquid cooling plate 7 through its thermally conductive network, which helps to reduce the temperature gradient in different areas of the bottom of the battery cell assembly. If thermally conductive foam is selected, while maintaining compression resilience and installation gap filling capability, the thermally conductive filler filled in its porous structure can form a continuous heat conduction path, which can further improve the uniformity of heat distribution between the bottom of the battery cell and the liquid cooling plate.

[0054] Obviously, the above embodiments of this utility model are merely examples for clearly illustrating the present utility model, and are not intended to limit the implementation of the present utility model. Those skilled in the art can make various obvious changes, readjustments, and substitutions without departing from the protection scope of this utility model. It is neither necessary nor possible to exhaustively describe all embodiments here. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of this utility model should be included within the protection scope of the claims of this utility model.

Claims

1. A thermal management system of a power battery pack, the power battery pack comprising a plurality of cell groups, each cell group being sequentially arranged by a plurality of single cells (1) along a predetermined arrangement rule, characterized in that, The thermal management system includes: A first PI heating film (21) is disposed on the outer surface of the first cell group (11) of the power battery pack, a second PI heating film (22) is disposed on the outer surface of the second cell group (13) of the power battery pack, a silicone heating film (3) is disposed on the side mating surface of each of the multiple cell groups, two first limiting strips (4), several second limiting strips (5), thermal conductive gel (6) and liquid cooling plate (7); wherein, the first cell group (11) and the second cell group (13) are the two outermost cell assemblies of the power battery pack, and the cell assembly is composed of several individual cells (1); The liquid cooling plate (7) is disposed at the bottom of the plurality of battery cell groups. The two first limiting adhesive strips (4) are respectively located at the two ends of the top of the liquid cooling plate (7) and are used to support the bottom positions of the first battery cell group (11) and the second battery cell group (13) near the outer side. The plurality of second limiting adhesive strips (5) are arranged at intervals along the arrangement direction of the plurality of battery cell groups, and each second limiting adhesive strip (5) is correspondingly disposed between the bottoms of two adjacent battery cell groups in the plurality of battery cell groups. The first limiting adhesive strips (4) and the second limiting adhesive strips (5) are pasted to the corresponding positions on the top of the liquid cooling plate (7) by means of single-sided adhesive. The thermally conductive gel (6) is applied between the liquid cooling plate (7) and the battery cell (1).

2. The thermal management system of a power battery pack according to claim 1, wherein, The first PI heating film (21), the second PI heating film (22), and the silicone heating film (3) all include: The heating film body is attached to the surface of the corresponding battery cell group by means of adhesive backing; wherein, the first PI heating film (21) and the second PI heating film (22) are attached to the outer surface of the corresponding battery cell group by means of single-sided adhesive backing, and the silicone heating film (3) is attached to the side mating surface of two adjacent battery cell groups by means of double-sided adhesive backing; the heating film body of the first PI heating film (21) and the second PI heating film (22) is made of PI material, and the heating film body of the silicone heating film (3) is made of silicone material; The wire outlet is located at one end of the heating film body. The wire outlet is made of silicone material and has an anti-wear layer on the outside. The first connecting wire harness and the second connecting wire harness are respectively led out from the outlet end; An input connector and an output connector; wherein the input connector is connected to the first connection harness, and the output connector is connected to the second connection harness; The input connector of the first PI heating film (21) is plugged into the input terminal of the battery pack heating power supply. The output connector of the first PI heating film (21) is plugged into the input connector of the adjacent silicone heating film. The output connector of the adjacent silicone heating film is plugged into the input connector of its next silicone heating film. The output connector of the second PI heating film (22) is plugged into the output terminal of the battery pack heating power supply. The input connector of the second PI heating film (22) is plugged into the output connector of the previous silicone heating film. The output terminal of the internal silicone heating film forms a series path with its adjacent silicone heating film through the input connector and the output connector.

3. The thermal management system of a power battery pack according to claim 1, wherein, The surface of the heating film body of the first PI heating film (21) and the second PI heating film (22) is provided with a plurality of openings, and the distribution position of the openings is aligned with the gap between adjacent cells in the multiple cells of the cell group to which the PI heating film (2) is attached; the surface of the silicone heating film (3) has no openings.

4. The thermal management system of a power battery pack according to claim 3, wherein, The edge of the opening is provided with annular reinforcing ribs protruding toward the surface of the heating film body on which it is located.

5. The thermal management system for the power battery pack according to claim 1, characterized in that, The width of the second limiting strip (5) is greater than the width of the first limiting strip (4).

6. The thermal management system for the power battery pack according to claim 1, characterized in that, The liquid cooling plate (7) includes: The first base plate (72) and the second base plate (76) are connected by friction stir welding, forming four independent flow channels inside; The first sealing component (73), the second sealing component (74), the third sealing component (75) and the fourth sealing component (77) are respectively sealed to the ends of the first base plate (72) and the second base plate (76) by friction stir welding and argon arc welding; The inlet (712) and outlet (711) are fixed to the top of the liquid cooling plate (7) by argon arc welding; in, The four independent flow channels are arranged in parallel to form a four-in-four-out structure. The cross-section of each flow channel is a closed U-shape. It is integrally formed inside the first base plate (72) and the second base plate (76) by aluminum extrusion. The inner wall of the flow channel is cut to form a smooth flow surface. The first base plate (72), the first sealing component (73), the second sealing component (74), the third sealing component (75) and the fourth sealing component (77), the inlet (712) and the outlet (711) are all made of aluminum alloy.

7. The thermal management system for the power battery pack according to claim 6, characterized in that, The inner wall of the flow channel of the liquid cooling plate (7) is provided with a corrosion-resistant surface treatment coating.

8. The thermal management system for the power battery pack according to claim 1, characterized in that, The thickness of the first limiting adhesive strip (4) and the second limiting adhesive strip (5) is matched with the coating thickness of the thermal conductive gel (6) to control the amount of adhesive overflow of the thermal conductive gel (6).

9. The thermal management system for the power battery pack according to claim 1, characterized in that, The bottom outer surface of the liquid cooling plate (7) is provided with a heat dissipation fin array.

10. The thermal management system for the power battery pack according to claim 1, characterized in that, The first limiting strip (4) and the second limiting strip (5) are made of thermally conductive silicone or thermally conductive foam.