A vertical enhancement power device

By designing a multilayer epitaxial drift layer and a second fin structure, the electric field and thermal management of the vertical enhancement-mode power device were optimized, solving the problems of process difficulty and conduction performance, and achieving high breakdown voltage and low conduction loss.

CN224987889UActive Publication Date: 2026-11-17JIANGSU SOLID POWER SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522519263.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-27
Publication Date
2026-11-17
Estimated Expiration
2035-11-27

AI Technical Summary

Technical Problem

Existing vertical power devices face challenges in balancing fabrication difficulty and conduction performance. In particular, the width and doping concentration requirements of finned vertical channels are difficult to balance, leading to excessive breakdown and conduction losses under high electric fields.

Method used

A multilayer epitaxial drift layer structure is adopted, with the doping concentration gradually decreasing from bottom to top. A second fin structure is set at the bottom of the substrate to increase the contact area. Combined with the design of oxide layer and metal layer, the electric field distribution and heat release of the device are optimized.

Benefits of technology

It achieves effective turn-off and high breakdown voltage of vertical enhancement-mode power devices, reduces process complexity and on-state voltage drop, and improves heat dissipation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224987889U_ABST
    Figure CN224987889U_ABST
Patent Text Reader

Abstract

This utility model relates to a vertical enhancement-mode power device, which includes a substrate, a drift region, and a first fin structure stacked sequentially from bottom to top. The substrate, drift region, and first fin structure are all of the same conductivity type. Several first fin structures protrude from the upper end of the drift region. Each first fin structure includes a channel region disposed above the drift region and a source region disposed above the channel region. The doping concentration of the drift region is higher than that of the channel region. By epitaxially layering an ultra-lightly doped n-channel region on the n-type drift region, the gate depletion width is increased, ensuring effective turn-off of the power device. Furthermore, the width of the fin-type vertical channel can be increased, reducing process difficulty and precision requirements.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of semiconductor device technology, and in particular to a vertical enhancement power device. Background Technology

[0002] In recent years, ultrawide bandgap semiconductor materials such as β-Ga2O3, diamond, and AlN have been considered candidate materials for next-generation high-voltage, high-temperature, and radiation-resistant power devices due to their superior physical properties, including high Baliga figures and high breakdown field strength. Among them, β-Ga2O3 is the only ultrawide bandgap material that can be grown into single crystals relatively well through melt growth methods, and it has great application potential.

[0003] like Figure 1 As shown, the cross-section of a FinFET vertical structure typically includes, from bottom to top, a substrate 1, a lightly doped n-type drift region 2, a lightly doped n-type fin vertical channel region 3, and a heavily doped n+ source region 4. By controlling the width of the fin channel, and considering the depletion effect of the gate electrodes on both sides of the channel, an enhancement-mode device can be achieved: when no voltage is applied to the gate, the gate electrodes on both sides deplete the channel, and current cannot flow between the drain and source, resulting in a turn-off state. When an appropriate voltage is applied to the gate, electrons accumulate on the channel surface, thus turning the device on.

[0004] However, finned vertical channels have strict requirements on width and doping concentration. If the width is too large, effective device turn-off may be impossible; if the width is too narrow, the fabrication process will be difficult to achieve. If the doping concentration is too high, the gate cannot completely deplete the channel, making effective turn-off and enhancement-mode operation (threshold voltage < 0) impossible. To achieve enhancement-mode operation, drift region 2 typically uses a lower doping concentration, resulting in excessive resistance in drift region 2, which affects turn-on losses.

[0005] In addition, due to the electric field concentration effect, the maximum electric field usually appears at the bottom of the trench, causing power devices to break down at a relatively low voltage. The higher the doping concentration, the stronger the electric field and the lower the breakdown voltage.

[0006] It should be noted that the information disclosed in the background section above is only used to enhance the understanding of the background of this disclosure, and therefore may include information that does not constitute prior art known to those skilled in the art. Utility Model Content

[0007] To address the shortcomings of existing technologies, this utility model discloses a vertical enhancement power device to solve the problem of not being able to simultaneously achieve both the manufacturing difficulty and conduction performance of vertical power devices.

[0008] The technical solution adopted in this utility model is as follows: A vertical enhancement-mode power device includes a substrate, a drift region, and a first fin structure stacked sequentially from bottom to top. The substrate, drift region, and first fin structure are all of the same conductivity type. The first fin structure has a plurality of fins protruding from the upper end of the drift region. The first fin structure includes a channel region disposed at the upper end of the drift region and a source region disposed at the upper end of the channel region. The doping concentration of the drift region is higher than that of the channel region.

[0009] A further technical solution is that the drift region includes several epitaxial drift layers stacked sequentially from bottom to top, the doping concentration of the several epitaxial drift layers decreases sequentially from bottom to top, and the doping concentration of the uppermost epitaxial drift layer is higher than the doping concentration of the channel region.

[0010] A further technical solution is that the doping concentration of the source region is higher than the doping concentration of the bottommost epitaxial drift layer.

[0011] A further technical solution is that the epitaxial drift layer comprises a first epitaxial drift layer, a second epitaxial drift layer, and a third epitaxial drift layer stacked sequentially from bottom to top; the lower end of the first epitaxial drift layer is connected to the substrate, the thickness of the first epitaxial drift layer is 3~4μm, and the doping concentration of the first epitaxial drift layer is 5e16~8e16cm. -3 The thickness of the second epitaxial drift layer is 2~3 μm, and the doping concentration of the second epitaxial drift layer is 2e16~3e16 cm. -3 The upper end of the third epitaxial drift layer is connected to the channel region. The thickness of the third epitaxial drift layer is 1~2μm, and the doping concentration of the third epitaxial drift layer is 6e15~8e15cm. -3 .

[0012] A further technical solution is that the upper end of the drift region forms a first trench between adjacent first fin structures, an oxide layer is deposited on the inner surface of the first trench, and a gate metal layer is deposited on the inner surface of the oxide layer.

[0013] A further technical solution is that the substrate, drift region, channel region and source region are of n-type conductivity.

[0014] A further technical solution is that the thickness of the channel region is 1.5~2μm, and the doping concentration of the channel region is 2.0e15~4.0e15cm. -3 The doping concentration of the source region is 3.0e19~6.0e19cm. -3 .

[0015] A further technical solution is that a back metal layer is provided at the lower end of the substrate.

[0016] A further technical solution is that a downwardly protruding second fin structure is provided at the lower end of the substrate, the upper end of the back metal layer has a shape that matches the lower end of the substrate, and the lower end of the back metal layer is lower than the lower end of the substrate.

[0017] A further technical solution is that the oxide layer is made of aluminum oxide, and the gate metal layer and the back metal layer are made of Ti / Au metal layers.

[0018] The beneficial effects of this utility model embodiment are as follows: (i) The vertical enhancement power device of this utility model increases the gate depletion width by epitaxially layering an ultralightly doped n-channel region on the n-type drift region, ensuring that the power device can be effectively turned off. On this basis, the width of the fin vertical channel can be increased, reducing the process difficulty and precision.

[0019] (ii) Furthermore, the drift region adopts a multilayer epitaxial drift layer, with the doping concentration decreasing from bottom to top. The doping concentration is low near the n-channel region, which reduces the electric field strength at the bottom of the first trench and increases the breakdown voltage. The doping concentration is increased near the substrate, which reduces the resistance of the drift region and reduces the on-state voltage drop.

[0020] (iii) Furthermore, by opening a second trench at a distance at the lower end of the substrate, a downwardly protruding second fin structure is formed. The second fin structure is distributed in a strip, grid, or honeycomb pattern, etc., which increases the contact area between the substrate and the back metal layer, releases the heat inside the device, and improves the heat dissipation capacity of the power device. Attached Figure Description

[0021] Figure 1 It is a vertical enhancement power device in the prior art.

[0022] Figure 2 This is a schematic diagram of the vertical enhancement power device of this utility model.

[0023] Figure 3 This is a schematic diagram of the strip-etched fit between the substrate 1 and the back metal layer 8 in the vertical enhancement power device of this utility model.

[0024] Figure 4 This is a schematic diagram of the mesh etching connection between the substrate 1 and the back metal layer 8 in the vertical enhancement power device of this utility model.

[0025] Figure 5 This is a schematic diagram of the honeycomb etched fit between the substrate 1 and the back metal layer 8 in the vertical enhancement power device of this utility model.

[0026] In the picture: 1. Substrate; 11. Second trench; 2. Drift region; 21. First epitaxial drift layer; 22. Second epitaxial drift layer; 23. Third epitaxial drift layer; 3. Channel region; 4. Source region; 5. First trench; 6. Oxide layer; 7. Gate metal layer; 8. Back metal layer. Detailed Implementation

[0027] To further illustrate the technical means and effects adopted by this utility model in order to achieve the intended utility model purpose, the following detailed description of the specific implementation methods, structure, features and effects of this utility model is provided in conjunction with the accompanying drawings and preferred embodiments.

[0028] Example: This embodiment discloses a vertical enhancement power device.

[0029] like Figure 2 As shown, the vertical enhancement-mode power device includes a substrate 1, a drift region 2, and a first fin structure stacked sequentially from bottom to top. The substrate 1, drift region 2, and first fin structure are all of the same conductivity type. Several first fin structures protrude from the upper end of the drift region 2. Each first fin structure includes a channel region 3 disposed at the upper end of the drift region 2 and a source region 4 disposed at the upper end of the channel region 3. The doping concentration of the drift region 2 is higher than that of the channel region 3.

[0030] For example, substrate 1, drift region 2, channel region 3, and source region 4 are of n-type conductivity. Specifically, substrate 1 is made of β-Ga2O3 material. The thickness of channel region 3 is 1.5~2μm, and the doping concentration of channel region 3 is 2.0e15~4.0e15cm. -3 The doping concentration in source region 4 is 3.0e19~6.0e19cm. -3 .

[0031] like Figure 2 As shown, further, the drift region 2 includes several epitaxial drift layers stacked sequentially from bottom to top. The doping concentration of the epitaxial drift layers decreases sequentially from bottom to top, and the doping concentration of the uppermost epitaxial drift layer is higher than that of the channel region 3. The doping concentration of the source region 4 is higher than that of the lowermost epitaxial drift layer. For example, the epitaxial drift layers include a first epitaxial drift layer 21, a second epitaxial drift layer 22, and a third epitaxial drift layer 23 stacked sequentially from bottom to top. The lower end of the first epitaxial drift layer 21 is connected to the substrate 1. The thickness of the first epitaxial drift layer 21 is 3~4 μm, and the doping concentration of the first epitaxial drift layer 21 is 5e16~8e16 cm⁻¹. -3 The second epitaxial drift layer 22 has a thickness of 2~3 μm and a doping concentration of 2e16~3e16 cm⁻¹. -3The upper end of the third epitaxial drift layer 23 is connected to the channel region 3. The thickness of the third epitaxial drift layer 23 is 1~2μm, and the doping concentration of the third epitaxial drift layer 23 is 6e15~8e15cm. -3 .

[0032] like Figure 2 As shown, further, a first trench 5 is formed at the upper end of the drift region 2 between adjacent first fin structures. An oxide layer 6 is deposited on the inner surface of the first trench 5, and a gate metal layer 7 is deposited on the inner surface of the oxide layer 6. A back metal layer 8 is disposed at the lower end of the substrate 1. Specifically, the oxide layer 6 is made of aluminum oxide, and the gate metal layer 7 and the back metal layer 8 are made of Ti / Au metal layers.

[0033] Gallium oxide has a low thermal conductivity of only 0.11 W / cm·K. This very low thermal conductivity causes heat to accumulate inside the device, making it difficult to conduct heat to the surface of the power device, leading to thermal failure. For example... Figures 3-5 As shown, preferably, second trenches 11 are spaced apart at the lower end of the substrate 1 to form a downwardly protruding second fin structure. The second fin structure is distributed in a strip, grid, or honeycomb pattern, etc., to increase the contact area between the substrate 1 and the back metal layer 8, release heat inside the device, and improve the heat dissipation capacity of the power device. The upper end of the back metal layer 8 is shaped to match the lower end of the substrate 1, and the lower end of the back metal layer 8 is lower than the lower end of the substrate 1.

[0034] In this embodiment, by epitaxially layering an ultralightly doped n-channel region 3 on the n-type drift region 2, the gate depletion width is increased, ensuring that the power device can be effectively turned off. On this basis, the width of the fin vertical channel can be increased, reducing the process difficulty and precision.

[0035] In addition, the drift region 2 adopts a multilayer epitaxial drift layer with the doping concentration decreasing from bottom to top. The doping concentration is low near the n-channel region 3, which reduces the electric field strength at the bottom of the first trench 5 and increases the breakdown voltage. The doping concentration is increased near the substrate 1, which reduces the resistance of the drift region 2 and reduces the on-state voltage drop.

[0036] The above description is merely a preferred embodiment of the present utility model and is not intended to limit the present utility model in any way. Although the present utility model has been disclosed above with reference to a preferred embodiment, it is not intended to limit the present utility model. Any person skilled in the art can make some modifications or alterations to the above-disclosed technical content to create equivalent embodiments without departing from the scope of the present utility model. Any simple modifications, equivalent changes and alterations made to the above embodiments based on the technical essence of the present utility model without departing from the scope of the present utility model shall still fall within the scope of the present utility model.

Claims

1. A vertical enhancement mode power device, characterized by, The vertical enhancement-mode power device includes a substrate, a drift region, and a first fin structure stacked sequentially from bottom to top. The substrate, drift region, and first fin structure are all of the same conductivity type. There are several first fin structures that protrude from the upper end of the drift region. The first fin structure includes a channel region disposed at the upper end of the drift region and a source region disposed at the upper end of the channel region. The doping concentration of the drift region is higher than that of the channel region.

2. The vertical enhancement mode power device of claim 1, wherein: The drift region includes several epitaxial drift layers stacked sequentially from bottom to top. The doping concentration of the several epitaxial drift layers decreases sequentially from bottom to top, and the doping concentration of the uppermost epitaxial drift layer is higher than that of the channel region.

3. The vertical enhancement mode power device of claim 2, wherein: The doping concentration of the source region is higher than that of the bottommost epitaxial drift layer.

4. The vertical enhancement power device according to claim 1, characterized in that: The upper end of the drift region forms a first trench between adjacent first fin structures, an oxide layer is deposited on the inner surface of the first trench, and a gate metal layer is deposited on the inner surface of the oxide layer.

5. The vertical enhancement power device according to claim 1, characterized in that: The substrate, drift region, channel region, and source region are of n-type conductivity.

6. The vertical enhancement power device according to claim 4, characterized in that: A back metal layer is provided at the lower end of the substrate.

7. The vertical enhancement power device according to claim 6, characterized in that: The substrate has a downwardly protruding second fin structure at its lower end, the upper end of the back metal layer has a shape that matches the lower end of the substrate, and the lower end of the back metal layer is lower than the lower end of the substrate.