soldering lug and module
By setting a stepped three-dimensional structure on the solder pad, the problems of void defects and insufficient filling of solder during chip warping are solved, thereby improving the soldering quality and reliability, and making it suitable for semiconductor power device packaging.
Patent Information
- Application Number
- CN202522021691.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-09-16
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-09-16
AI Technical Summary
Traditional preformed solder pads can cause chip warping during chip packaging due to differences in the coefficient of thermal expansion of materials or limitations in process conditions. This warping results in a sunken central area and upturned ends, which prevents the solder from adhering evenly, leading to voids and insufficient solder filling, thus affecting soldering reliability.
The solder pad adopts a stepped three-dimensional structure, with the boss and base area forming an integrated structure. The boss matches the product warpage. Through capillary action and local pressure gradient design, it ensures smooth flow of molten solder, exhausts gas and fills the tight area, avoiding voids and insufficient filling.
It effectively eliminates the "air trap" effect, improves welding quality, reduces void rate and solder overflow risk, enhances welding reliability and process tolerance, and achieves both process compatibility and structural stability in high-density power module packaging.
Smart Images

Figure CN224988022U_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to the field of semiconductor power device packaging technology, and more specifically, to a solder pad and module. Background Technology
[0002] Preformed solder pads are an advanced soldering material used in the packaging and soldering of semiconductor power devices. Traditional preformed solder pads typically employ a flat structure with uniform thickness and parallel to the soldering interface. However, during chip packaging, due to differences in the coefficients of thermal expansion of materials or limitations in process conditions, packaged chips often exhibit a warped shape, with the central area sinking and the ends tilting upwards. This warping prevents the solder pad from forming a uniform bond with the heat sink during reflow soldering. The molten solder in the central area suffers from impeded heat conduction due to the tight bond, resulting in a slower melting rate compared to the edge areas and the formation of localized "gas traps." Gases generated by flux decomposition and oxide breakage become trapped in the liquid solder in the central area, eventually solidifying into voids.
[0003] Furthermore, excessive gaps at both ends caused by warping can lead to insufficient solder filling, further reducing welding reliability. Utility Model Content
[0004] To address the aforementioned technical problems, this disclosure provides a solder pad and a module to improve the issues of void defects and insufficient solder filling.
[0005] According to one aspect of the embodiments of this disclosure, a solder pad is provided, comprising:
[0006] The base region has a top plane;
[0007] The boss is located at the center of the top plane of the base area.
[0008] The boss and the base area have a stepped difference, forming an integrated stepped structure.
[0009] Optionally, the thickness ratio of the boss to the base region is 1 / 3 to 1.
[0010] Optionally, the thickness of the boss is 0.2~0.3mm.
[0011] Optionally, the thickness of the base region is 0.3~0.6 mm.
[0012] Optionally, the size of the boss is set according to the warp of the product it is welded to, so as to match the warp shape of the weld surface of the product.
[0013] Optionally, the length direction of the boss is consistent with the warping direction of the product, and the length of the boss matches the size of the unwarped portion of the product.
[0014] Optionally, the length of the boss is 30% to 60% of the total length of the solder pad, and the width is 40% to 70% of the total width of the solder pad.
[0015] Optionally, the height of the boss is positively correlated with the warpage of the product.
[0016] Optionally, the solder pad is made of a tin-based alloy material, and the boss is made of the same material as the base region.
[0017] According to another aspect of the embodiments of this disclosure, a module is provided, comprising:
[0018] product;
[0019] Base plate;
[0020] The product and the base plate are welded together using the welding plates described above.
[0021] One of the above technical solutions has the following beneficial effects:
[0022] By setting a stepped three-dimensional structure in the central region of the solder pad, a differentiated melting sequence is created during reflow soldering. The bosses are matched to the product's warp. When the product to be soldered exhibits a warped shape—a center sinking and both ends rising—due to differences in material thermal expansion, the boss area of the solder pad forms a preferential contact point with the product's welding surface. This area melts first due to reduced thermal resistance, and the molten solder flows from the center towards the base region under capillary action. This melting sequence matches the product's warp shape, allowing the decomposition gases generated during solder melting to be smoothly discharged along the progressive gap channel formed by the base region and the heat sink, effectively eliminating the "gas trap" effect formed during traditional flat solder pad welding.
[0023] Furthermore, this stepped integrated solder pad expands the process window through the coordinated design of structural parameters and product warpage. The boss height is positively correlated with the product warpage, and the boss length is 30% to 60% of the total solder pad length, while the width is 40% to 70% of the total solder pad width. This ensures efficient heat conduction in the boss area while reserving sufficient space for solder flow in the base area. During melting, the local pressure gradient formed by the stepped structure encourages the solder to preferentially fill the tightly fitted area in the middle of the product, and then expand towards the warped areas at both ends. This adaptive filling mechanism, combined with the chamfered design of the solder pad platform area, effectively alleviates the problem of insufficient filling caused by uneven solder flow. By matching the solder pad melting characteristics with the product deformation characteristics in three-dimensional space, this solution achieves a dual improvement in welding quality without increasing the total amount of solder, providing a solution for high-density power module packaging that combines process compatibility and structural stability.
[0024] It should be noted that the above general description and the following detailed description are exemplary and explanatory only, and do not limit this disclosure. Attached Figure Description
[0025] To more clearly illustrate the technical solutions of the embodiments of this disclosure, the accompanying drawings of the embodiments will be briefly introduced below. Obviously, the drawings described below only relate to some embodiments of this disclosure, and are not intended to limit this disclosure.
[0026] Figure 1 A three-dimensional structural schematic diagram of the solder pad according to an embodiment of the present disclosure is shown.
[0027] Figure 2 It shows Figure 1 Top view of the middle solder pad.
[0028] Figure 3 It shows Figure 1 Front view of the middle welding piece.
[0029] Figure 4 A schematic diagram of the structure in which the solder pads are placed on the base plate is shown according to an embodiment of the present disclosure.
[0030] Figure 5 A schematic diagram of a structure in which a plastic-encapsulated product is placed on a solder pad is shown according to an embodiment of the present disclosure.
[0031] Figure 6 It shows Figure 5 Side view. Detailed Implementation
[0032] The present invention will now be described based on embodiments, but it is not limited to these embodiments. In the following detailed description of the present invention, certain specific details are described in detail. Those skilled in the art will fully understand the present invention even without these details. To avoid obscuring the essence of the present invention, well-known methods, processes, flows, elements, and circuits are not described in detail.
[0033] Furthermore, those skilled in the art should understand that the accompanying drawings provided herein are for illustrative purposes only and are not necessarily drawn to scale.
[0034] Unless the context explicitly requires it, the words "comprising," "including," and similar terms throughout the specification and claims should be interpreted as encompassing rather than being exclusive or exhaustive; that is, meaning "including but not limited to."
[0035] In this description, it should be understood that the terms "first," "second," etc., are used for descriptive purposes only and should not be construed as indicating or implying relative importance. Furthermore, in this description, unless otherwise stated, "multiple" means two or more.
[0036] The following will combine Figures 1 to 3 The solder pad structure of the present disclosure will be described in detail, wherein the X-axis direction represents the length direction of the solder pad, the Y-axis direction represents the width direction of the solder pad, and the Z-axis direction represents the thickness direction of the solder pad.
[0037] like Figures 1 to 3 As shown, the solder pad 200 includes a base region 210 and a boss 220. The base region 210 has a top plane 210a, and the boss 220 is located at the center of the top plane 210a of the base region 210. The boss 220 and the base region 210 have a stepped difference, thus making the solder pad 200 an integral stepped structure. The base region 210 and the boss 220 can be integrally formed by a stamping process to form an overall structure with a preset stepped difference, thereby ensuring that there is no seam between the boss 220 and the base region 210, avoiding contamination or stress concentration introduced by secondary processing; using a stamping process can also simplify the manufacturing process, reduce tooling costs, and improve batch consistency.
[0038] In some alternative embodiments, the thickness ratio of the boss 220 to the base region 210 can be 1 / 3 to 1. In some specific embodiments, the thickness of the boss 220 is, for example, 0.2 to 0.3 mm, and the thickness of the base region 210 is 0.3 to 0.6 mm.
[0039] In some alternative embodiments, the length of the boss 220 can be 30% to 60% of the total length of the solder pad 200, and the width can be 40% to 70% of the total width of the solder pad 200.
[0040] In some specific embodiments, the length of the boss 220 is, for example, 35~50mm, and the width is, for example, 5.5~8mm.
[0041] In some alternative embodiments, the connection between the base region 210 and the boss 220 adopts a right-angle or rounded transition design. The rounded transition can reduce stress concentration and prevent the solder sheet from cracking during stamping or reflowing, while the right-angle transition is easier to mold processing, taking into account both manufacturing economy and structural integrity.
[0042] In some alternative embodiments, the outer edge of the base region 210 is provided with a chamfer / rounded corner structure, which can be used to guide excess solder to flow outward, forming a smooth rounded corner and avoiding the formation of solder spikes from sharp edges.
[0043] In some alternative embodiments, the solder pad 200 is made of a tin-based material or a tin-based alloy material, such as at least one of the group consisting of AgSn, AuSn, NiSn, CuSn, AgCuSn, and InSn. Tin can have excellent soldering properties. At least one additional metallic component can improve the properties of the solder material.
[0044] In this embodiment, the boss 220 is made of the same material as the base region 210, thereby ensuring that the thermal expansion coefficient and melting point of the boss 220 and the base region 210 are completely consistent, eliminating the risk of thermal fatigue caused by the interface of dissimilar materials. However, the embodiments disclosed herein are not limited thereto, and those skilled in the art can make other settings for the material of the solder sheet 200 and the morphology of the base region 210 and the boss 220 as needed.
[0045] The following will combine Figures 4 to 6 The module structure of the embodiments of this disclosure will be described in detail.
[0046] like Figures 4 to 6 As shown, the module of this embodiment includes: a base plate 100, a welding piece 200, and a product 300. The welding piece 200 is disposed on the upper surface of the base plate 100, the product 300 is located on the welding piece 200, and the product 300 is welded to the base plate 100 through the welding piece 200.
[0047] In some embodiments, the base plate 100 can be a heat dissipation base plate or a heat sink with heat dissipation fins. For example, it can be a copper heat dissipation base plate, or a heat sink with multiple pin-fin structures 101 on its lower surface, or a heat sink with other structures.
[0048] In this embodiment, the module is, for example, a power module.
[0049] In this embodiment, product 300 is one of the components of the module. For example, it can be a plastic-encapsulated component, a plastic-encapsulated module, or other types of components or encapsulation structures formed by plastic encapsulation.
[0050] Product 300 includes a chip, such as a power chip, which may include a diode, IGBT (Insulated Gate Bipolar Transistor), MOSFET (Metal-Oxide-Semiconductor Field-Effect Transistor), JFET (Junction Field-Effect Transistor), HEMT (High Electron Mobility Transistor), or any other suitable controllable or uncontrollable semiconductor element.
[0051] This power chip can be formed using a wide variety of semiconductor materials and a wide variety of device technologies. Examples of such materials include, but are not limited to, elemental semiconductor materials such as silicon (Si) or germanium (Ge), group IV compound semiconductor materials such as silicon carbide (SiC) or silicon germanium (SiGe), and binary, ternary, or quaternary III-V semiconductor materials such as gallium nitride (GaN), gallium arsenide (GaAs), gallium phosphide (GaP), indium phosphide (InP), indium gallium phosphide (InGaP), aluminum gallium nitride (AlGaN), aluminum indium nitride (AlInN), indium gallium nitride (InGaN), aluminum gallium indium nitride (AlGaInN), or indium gallium arsenide (InGaAsP), etc.
[0052] In some specific embodiments, product 300 is, for example, a SiC MOSFET molded module.
[0053] In this embodiment, the boss 220 of the solder pad 200 is rectangular. The size of the boss 220 is set according to the warpage of the product 300 it is soldering, so as to match the warpage shape of the soldering surface of the product 300. This allows the solder pad 200 to make full contact with the central region 301 of the product 300 during reflow soldering, forming a preferential melting zone and significantly reducing the probability of central "gas trap" formation. The step difference provides a lateral escape channel for gas, reducing the overall void ratio. After soldering is completed, the central region 301 and the edge region 302 of the product 300 are in full contact with the base plate 100 through the soldering material. The boss 220 can also avoid the risk of solder overflow caused by the overall thickening of the solder pad 200, balancing low void ratio and process window.
[0054] In this embodiment, the length direction (X-axis direction) of the boss 220 is consistent with the warping direction of the product 300, and the length of the boss 220 matches the size of the non-warped portion of the product 300, thereby providing continuous support along the direction of maximum warping and eliminating insufficient solder filling at both ends due to upward warping; it can also reduce unnecessary solder usage and further reduce the risk of solder overflow and bridging.
[0055] In the thickness direction (Z-axis direction) of the solder pad 200, the height of the boss 220 is positively correlated with the warpage of the product 300. Since the height of the boss 220 is positively correlated with the warpage, "quantitative compensation" can be achieved—the greater the warpage, the higher the boss 220 should be, thus maintaining the optimal initial contact area between the solder pad 200 and the product 300 and avoiding insufficient compensation due to the boss 220 being too low.
[0056] During module packaging, when the product 300 is placed on top of the solder pad 200, the central recessed area of its soldering surface makes preferential contact with the solder pad boss 220, while the two upturned areas maintain a preset gap with the base area 210. During the reflow soldering stage, the boss 220 melts first due to the increased contact area and reduced thermal resistance. The molten solder expands towards the base area 210 along the rounded transition area under capillary action. At this time, the gases generated by flux decomposition and the gases released by oxide rupture are orderly discharged through the progressive gap channel formed by the base area 210 and the heat sink 100, avoiding the "gas trap" effect caused by the disordered melting sequence of traditional flat solder pads. At the same time, the local pressure gradient generated by the stepped structure causes the solder to preferentially fill the central tightly fitted area and then expand towards the two upturned areas. This adaptive filling mechanism works synergistically with the chamfer design of the base area 210 to effectively alleviate the problem of insufficient filling caused by uneven solder flow. Experiments have verified that the solder pads with this structure can reduce the solder void rate from more than 10% in the traditional solution to less than 2%, and reduce the risk of solder overflow by 40%, which significantly improves the soldering reliability and process tolerance of the power module.
Claims
1. A soldering tab, characterized by The soldering sheet comprises: a base area with a top plane; a boss in the center of the top plane of the base area, wherein the boss and the base area have a stepped difference to form an integrated stepped structure, and the size of the boss is set according to the warping degree of the product to be welded so as to match the warping topography of the welding surface of the product.
2. The soldering tab of claim 1, wherein, The thickness ratio of the boss to the base area is 1 / 3-1.
3. The soldering tab of claim 2, wherein, The thickness of the boss is 0.2-0.3 mm.
4. The soldering tab of claim 2, wherein, The thickness of the base area is 0.3-0.6 mm.
5. The soldering tab of claim 1, wherein, The length direction of the boss is consistent with the warping direction of the product, and the length of the boss matches the size of the non-warping part of the product.
6. The soldering tab of claim 5, wherein, The length of the boss is 30%-60% of the total length of the soldering sheet, and the width is 40%-70% of the total width of the soldering sheet.
7. The soldering tab of claim 1, wherein, The height of the boss is positively correlated with the warping amount of the product to be welded.
8. The soldering tab of claim 1, wherein, The soldering sheet is made of tin-based material or tin-based alloy material, and the material of the boss is the same as that of the base area.
9. A module characterized in that, The soldering sheet comprises: a product; a bottom plate; the product and the bottom plate are welded and connected by the soldering sheet according to any one of claims 1-8.