Self-supporting structures with adsorptive properties

DE102012006272B4Inactive Publication Date: 2024-10-31BLUCHER GMBH
View PDF 13 Cites 0 Cited by

Patent Information

Application Number
DE102012006272
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2011-09-30
Filing Date
2012-03-29
Publication Date
2024-10-31
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A self-supporting three-dimensional adsorptive structure, wherein the adsorptive structure comprises a plurality of individual adsorber particles, wherein the individual adsorber particles are connected to form a self-supporting three-dimensional adsorptive structure by means of at least one hydrocolloid, and / or wherein the individual adsorber particles are connected to each other and / or fixed to each other and / or made to adhere to each other by means of at least one hydrocolloid, wherein the hydrocolloid is selected from the group consisting of gelatin, collagen, xanthan gum, dextran, agar, carrageenan, pectin, gum arabic, galactomannan, and their derivatives and mixtures or combinations, wherein the adsorber particles are granular in shape and have absolute particle diameters in the range of 0.001 to 3 mm.wherein the adsorptive structure comprises the hydrocolloid and the adsorber particles in a mass-related ratio of hydrocolloid to adsorber particles “[hydrocolloid : adsorber particles]” in the range of [1 : 100] to [1 : 1], based on the respective dry weight, and wherein the adsorptive structure is porous and / or foam-like, and wherein the adsorptive structure has a pore system.
Need to check novelty before this filing date? Find Prior Art

Description

The present invention relates to the field of adsorption filter technology.In particular, the present invention relates to self-supporting three-dimensional adsorptive structures, in particular adsorptive shaped bodies which comprise a multiplicity of individual adsorber particles. The present invention furthermore relates to a production process in this respect.The present invention further relates to a use of a hydrocolloid for obtaining the self-supporting three-dimensional adsorptive structure according to the invention. The present invention also relates to a use of the self-supporting three-dimensional adsorptive structure according to the invention. Finally, the present invention relates to filters comprising the self-supporting three-dimensional adsorptive structure according to the invention.For the purification or treatment of fluid media, such as in particular gases or gas mixtures, such as air, or liquids, such as water, for example, particulate systems based on particles with specific action (e.g. adsorbents, ion exchangers, catalysts, etc.) are often used. For example, the use of adsorber particles for removing toxicants or pollutants and odors from gas or air streams or liquids is known in the art.The use of loose fills of such particles, preferably adsorber particles, in particular in the form of so-called fill filters, represents a central application form in this case in order to bring the relevant particles, such as adsorber particles, into contact with the relevant gas or the relevant liquid.However, the disadvantage of using loose beds is that they are usually associated with a high pressure loss and thus a reduced adsorption capacity. In addition, the formation of channels within the bed is promoted, so that medium which has not yet been purified can break through.In particular, loose fills of adsorber particles are also disadvantageous in that they are only accessible to a restricted geometric shape, i.e. an individual and in particular intended adaptation of the geometric shape to the intended use is hardly implementable, especially since no rigid shaped bodies can be obtained on the basis of fills.EP 0 492 081 A1 relates to thin-walled honeycomb structures based on activated carbon, which are used for adsorbing hydrocarbon vapors. The honeycomb structures are produced by extruding a mixture based on cellulose ether or derivatives thereof, such as, for example, methylcellulose, an additional binder, such as, for example, polyvinyl alcohol resins, and activated carbon particles into a honeycomb form and subsequently drying it at temperatures of about 300° C.US 2010 / 0173772 A1 relates to shaped bodies based on adsorbing material, which have particulate activated carbon material, which is bonded or bonded by a suitable binder from the group of sodium alginate, calcium alginate, chitosan, polyacrylamide, polyethylene oxide and mixtures thereof.JP 58099109 A relates to shaped bodies based on powdered activated carbon particles, wherein carboxymethylcellulose is used as binder for producing the shaped bodies.DE 10 2008 058 248 A1 relates to an adsorptive shaped body which is preferably formed monolithically or integrally, wherein the shaped body is constructed from a multiplicity of adsorptive structures based on agglomerates of adsorber particles, and to a method for the production thereof and the use thereof.Park et al., "Activated carbon-containing alginate adsorbent for the simultaneous removal of heavy metals and toxic organics", Process Biochemistry, Vol. 42, pages 1371 to 1377, relates to alginate beads containing activated carbon and also suitable for the removal of heavy metal ions and toxic organics.U.S. Pat. No. 6,989,102 B1 relates to adsorptive beads based on alginate and activated carbon, which are suitable for removing heavy metals.Lin et al., "Removal of organic compounds by alginate gel beads with untrapped activated carbon", Journal of Hazardous Materials, Elsevier 2005, Vol. 12, pages 237 to 241 relate to the preparation and characterization of alginate capsules containing powdered activated carbon. In the capsules described with a diameter of about 2 mm, powdered activated carbon is incorporated into an alginate gel, wherein the cross-linking and curing of the resulting alginate capsules takes place by the addition of metal ions, in particular calcium chloride.DE 38 13 564 A1 and EP 0 338 551 A2 belonging to the same patent family disclose an activated carbon filter layer for ABC protection masks, which comprises a highly air-permeable, substantially dimensionally stable three-dimensional support structure to which a layer of granular, in particular spherical, activated carbon particles with diameters of 0.1 to 1 mm is fixed, wherein the support structure is to be a mesh of wires, monofilaments or webs or a large-pore reticulated polyurethane foam. A disadvantage of the system described therein is the fact that the carrier material used requires a relatively complicated processing process in conjunction with the exposure to the particles in question. Furthermore, the selected carrier materials cannot be used or shaped universally, so that the resulting filters are limited to a few applications.Furthermore, DE 42 39 520 A1 discloses a high-performance filter which consists of a three-dimensional support structure on which adsorber particles are fixed by means of an adhesive compound, wherein the support structure is sheathed by a thermally stable and hydrolysis-resistant plastic. In particular, the support structure is a large-pore reticulated polyurethane foam which is sheathed by a silicone resin, polypropylene, hydrolysis-resistant polyurethane, an acrylate, a synthetic rubber or with fluoropolymers. The production process for these structures, which are sometimes multiply sheathed, in particular the production of the carrier structure, is relatively complicated. Individual or intended shaping is also possible only to a limited extent.Furthermore, DE 43 43 358 A1 discloses porous bodies containing activated carbon, which consist of plates and agglomerates of ground activated carbon incorporated in a porous SiO 2- matrix. In particular, porous plates or bodies with adsorbing properties are described therein, in which activated carbon grains or activated carbon beads or activated carbon-containing grains or beads are adhered to one another with the aid of a silicate solution and the silicate bridges are subsequently converted into silica gel bridges. Here too, the fixed geometry of these porous bodies or their lack of flexibility in connection with the shaping is disadvantageous. Moreover, the bodies as such do not have sufficient mechanical stability. It is likewise disadvantageous that the activated carbon-containing particles are completely wetted with the silicate solution, so that a large part of the capacity of these particles is no longer available for adsorptive processes.Similarly, from DE 43 31 586 C2 agglomerates of activated carbon are known, in which activated carbon particles with a diameter between 0.1 to 5 mm are arranged by light pressure under heating around an approximately equally sized particle of pitch and are caused to adhere and subsequently the pitch particle is made infusible and converted into activated carbon, wherein a defined free space between the particles is to be present in the agglomerate. A disadvantage of the particles or agglomerates described therein is the relatively complicated, energy-intensive production. In addition, the mechanical stability is only inadequate, which can result in high wear in particular. Also, due to the lack of stability, further processing to form molded bodies under compression is only possible to a limited extent.The same applies to the porous bodies having adsorptive properties according to DE 42 38 142 A1, which relates to adsorber particles which are connected to one another via bridges made of an inorganic material, in particular alumina, wherein the cavities between the adsorber particles are intended to be 10 to 100% of the volume of the adsorber particles. The porous bodies described therein also have only a low mechanical stability, since the bridges made of inorganic material can only be able to withstand mechanical action to a slight extent, so that use under mechanical loading and further processing to give moldings under compression is not readily possible. A disadvantage in this connection is also that a suitable shaping is sometimes not possible.Furthermore, DE 202 21 547 U1 relates to porous activated carbon bodies having a first framework structure based on carbonized resin and a further framework structure based on ceramic material and / or fired refractory material and binder, wherein the activated carbon particles are fixed to the framework structure. However, by fixing the activated carbon particles by melting them into the resin, these are covered to a large extent and only accessible to a limited extent for gases or liquids to be purified, resulting in losses in terms of the adsorption capacity.The object of the present invention is therefore to provide three-dimensional adsorptive structures or shaped bodies for the removal of toxicants, harmful substances or fragrances from fluid media, such as, for example, gas streams or water, which at least largely avoid or at least alleviate the disadvantages of the prior art described above.In particular, the object of the present invention is to provide three-dimensional adsorptive structures or shaped bodies which have an excellent adsorption capacity, in particular with respect to toxicants, harmful substances and / or odour substances present in fluid media, such as gas streams and liquids, and which are moreover stable under mechanical stress and in which individual shaping, in particular directed to the purpose, into a wide variety of geometric shapes is possible. In addition, the production method for obtaining the three-dimensional shaped bodies according to the invention in this respect is intended to enable low material and energy consumption.The object described above is achieved according to the proposal - according to an aspect of the present invention - by the subject matter of patent claim 1, which relates to a self-supporting three-dimensional adsorptive structure according to the invention; further advantageous embodiments of this aspect of the invention are the subject matter of the dependent claims in this respect.The present invention further provides, according to a second aspect of the present invention, the process according to the invention as claimed in the respective independent process claims for producing the adsorptive structure according to the invention; further advantageous configurations of this aspect of the invention are the subject of the relevant process sub-claims.Furthermore, the present invention relates - according to a third aspect of the present invention - to the use according to the invention of a hydrocolloid according to the present invention for providing the three-dimensional adsorptive structure according to the invention, wherein the use according to the invention is defined in the independent claim of use.Furthermore, the present invention relates - according to a fourth aspect of the present invention - to the uses according to the invention of the self-supporting three-dimensional adsorptive structure according to the present invention, as defined in the further independent use claims.Finally, the present invention relates - according to a fifth aspect of the present invention - to a filter according to the invention according to the independent claim in this respect, wherein the filter according to the invention has an adsorptive structure according to the present invention; further advantageous configurations of this aspect of the invention are the subject matter of the dependent claims in this respect.It goes without saying that configurations, embodiments, advantages and the like, which are mentioned below for the purpose of avoiding repetitions only for one aspect of the invention, naturally also apply correspondingly with respect to the other aspects of the invention.Furthermore, it goes without saying that in the following values, numbers and ranges data, the ranges specified are not to be understood as limiting; it goes without saying for the person skilled in the art that, depending on the individual case or on the application, the ranges and data specified can be deviated without departing from the scope of the present invention.In addition, it applies that all values or parameter data or the like mentioned below can in principle be determined or determined using standardized or standardized or explicitly specified determination methods or else otherwise using determination or measurement methods familiar per se to the person skilled in the art.It is also true that in all the relative or percentage, in particular weight-related, stated below, it should be noted that these details are to be selected or combined by the skilled person in the context of the present invention in such a way that the sum of these, optionally including further components or ingredients, in particular as defined below, always results in 100% or 100% by weight. However, this is self-evident to the person skilled in the art.In the foregoing, the present invention will be described in detail below.The present invention thus provides, according to a first aspect of the present invention, a self-supporting three-dimensional adsorptive structure, in particular an adsorptive shaped body, wherein the adsorptive structure comprises a multiplicity of individual adsorber particles, wherein the individual adsorber particles are joined by means of at least one hydrocolloid to form a self-supporting three-dimensional adsorptive structure, in particular an adsorptive shaped body, or wherein the individual adsorber particles are joined together by means of at least one hydrocolloid and / or are fixed to one another and / or are brought to adhere to one another, wherein the hydrocolloid is selected from the group of gelatin, collagen, xanthan, dextran, agar, carrageenan, pectin, gum arabic, galactomannan and derivatives and mixtures or combinations thereof, wherein the adsorber particles are configured in the form of grains and have absolute particle diameters in the range from 0.001 to 3 mm, wherein the adsorptive structure comprises the hydrocolloid and the adsorber particles in a mass-related ratio of hydrocolloid to adsorber particles "[hydrocolloid:adsorber particles]" in the range from [1:100] to [1:1], based on the respective dry weight, and wherein the adsorptive structure is porous and / or foam-like and wherein the adsorptive structure comprises a pore system.The basic idea of the present invention is thus to be seen in the fact that particulate or discrete adsorbents or adsorber particles are bonded or fixed to one another by means of a hydrocolloid as binder in order to obtain a three-dimensional structure having adsorptive properties. The three-dimensional structure is obtained, so to speak, by the adsorbents or adsorber particles being bonded or fixed to one another in a web-like or punctiform manner by means of the hydrocolloid and, so to speak, a framework and / or a matrix based on adsorber particles and hydrocolloid being formed. In their entirety, the discrete adsorbents in combination with the hydrocolloid thus form a stable three-dimensional structure-i.e. a rigid (shaped) body which is at least substantially non-reversibly deformable.In the context of the present invention, it was completely surprising that structures which are stable at all can be obtained using a hydrocolloid as bonding agent for fixing and / or adhering the adsorber particles, and which structures can also be shaped extremely individually, in particular in a targeted or customized manner, preferably by pouring into the desired shape, but on the other hand are nevertheless readily accessible to the substances to be adsorbed and thus have an excellent adsorption capacity, in particular with regard to toxicants, harmful substances or odorants, as can occur in fluid media, it also being possible for the porosity of the shaped bodies or of the three-dimensional structures to be adjusted individually.As regards the term "hydrocolloid" as used in the context of the present invention and as is well known per se to the skilled person, this is to be understood very broadly. Hydrocolloids are generally understood to mean at least substantially water-soluble, natural or synthetic polymers which form gels or viscous solutions in aqueous systems. These are usually substances belonging to the substance classes of the proteins or polysaccharides, a large number of hydrocolloids originating from nature, in particular from land plants, algae, animals and bacteria. Hydrocolloids are often used as thickeners in cosmetics and products of the food industry. For more detailed information on the term "hydrocolloid", reference may be made to Rompp Chemielexikon, 10th Edition, Georg Thieme Verlag, Stuttgart / New York, keyword: "hydrocolloids", page 1837, including the literature referenced therein, the content of which in this respect is hereby incorporated by reference in its entirety.The terms "self-supporting three-dimensional adsorptive structure" or "adsorptive shaped body" as used according to the invention refer in particular to a consolidated or combined accumulation of previously loose or separate constituents in the form of individual adsorber particles using at least one hydrocolloid as adhesive or adhesive, it being possible for the individual constituents to be bonded together in particular in the form of a foam or a foam-like structure in the form of a web or point.Furthermore, the terms "self-supporting three-dimensional adsorptive structure" or "adsorptive shaped body", as used according to the invention, are intended to be relevant for the structures according to the invention additionally having adsorptive properties, in particular with respect to preferably gaseous, but sometimes also liquid or solid substances or compounds, the adsorption properties comprising in particular inorganic or organic compounds or substances. In particular, these are harmful or toxicants, but equally also odors or odorants, as may occur in fluid media, for example gas streams and / or liquids.In the context of the present invention, the term "multiplicity of adsorber particles" is to be understood as meaning in each case in particular at least two, preferably more than two, adsorber particles which are joined to form a self-supporting three-dimensional adsorptive structure. Usually, however, the number of adsorber particles in the adsorptive structure according to the invention is at least 10, in particular at least 20, preferably at least 50, preferably at least 100, particularly preferably at least 1,000.Overall, the present invention has a multiplicity of advantages and features which distinguish it from the prior art and are now described in a non-limiting manner in the following:In the context of the present invention, self-supporting three-dimensional adsorptive structures, in particular adsorptive shaped bodies, are provided for the first time, which have a combination of advantageous properties which is complementary in a targeted manner, as it has not been possible to realize hitherto in the prior art. For example, it has been possible within the scope of the present invention to provide self-supporting three-dimensional adsorptive structures with good handling in use and production and, in addition, excellent adsorption performance, good mechanical stability and variable shaping, i.e. production of customized geometric shapes or shaped bodies.In addition, it is even possible, on the basis of the design according to the invention, to provide shaped bodies which, by means of the shaping, are additionally provided with defined perforations or channels (for example honeycomb shaped bodies or the like) without this having a disadvantageous effect on the stability. A further central feature of the present invention is also to be seen in the fact that, in particular by using the hydrocolloid as a binder or adhesion promoter for connecting and / or fixing and / or adhering discrete adsorber particles to one another or to one another, an extremely variable shaping of the resulting self-supporting structures is possible.The process according to the invention for producing the adsorptive structures as such according to the invention makes it possible to produce the shaped bodies in an extremely wide variety of geometric shapes, which in particular also ensures a shaping which is specific for the purpose or is customized for the particular intended use.According to the invention, it is also possible to produce agglomerates ("break agglomerates") which likewise have excellent adsorption properties and high stability, preferably when used in the form of a loose bed of the agglomerates. The production of such fracture agglomerates is generally effected by mechanical comminution, preferably by breaking or mortaring, of larger shaped bodies to give smaller fracture agglomerates. The breaking agglomerates are clearly smaller than the previously described shaped bodies, but the micro- or basic structure-i.e. the manner of connection or adhesion of the adsorber particles by means of the hydrocolloid-is identical to the larger shaped bodies.In a completely surprising manner, the use of the hydrocolloid as a bonding agent or adhesive agent leads to an excellent mechanical stability of the adsorptive structures according to the invention both in the form of shaped bodies and in the form of broken agglomerates. In particular, the binder enables such good adhesion and / or fixation of the adsorber particles that even the use of extremely small amounts leads to excellent stability and, in addition, the surface of the individual adsorber particles remains largely free of binder. As a result, both the diffusion processes in the adsorptive structure and the adsorption performance of the adsorber particles on which the adsorptive structure is based are therefore not adversely affected by the binder; nevertheless, the mechanical stability of the adsorptive structures is excellent despite the small amounts of hydrocolloid used.Surprisingly, the use of a hydrocolloid as a binding agent or adhesion promoter also makes it possible for the resulting adsorptive shaped bodies or adsorptive structures to have good diffusion properties for the fluid media to be purified. Thus, the pore structure of the individual adsorber particles is substantially not blocked by the binder. The binder can, if necessary, penetrate, and this in addition only to an extremely minor extent, into macropores; the micro- or meso pores which are particularly relevant for the purification of fluid media, on the other hand, remain free of hydrocolloid. In addition, on the basis of the hydrocolloid, a well-permeable pore system is provided which penetrates the molded body.The adsorptive structures according to the invention also have an extremely high resistance or resistance to physical and chemical influences; in particular, they remain stable under compressive stress and exhibit an extremely good resistance under conditions of use. In addition, the temperature resistance of the adsorptive structures according to the invention is above 200° C. In addition, the adsorptive structures or the hydrocolloid used for this purpose are at least largely insoluble in organic aprotic solvents, in particular acetone. The properties described above permit the use of the adsorptive structures according to the invention in a broad field of application, for example also the use at locations with high temperatures or in the presence of solvents.It is also particularly advantageous for the adsorptive structures according to the invention that they can be handled extremely well both when used or when used as filter or adsorption material and when produced. The shaped bodies in question are namely usually free from toxic substances, above all they generally have no toxic solvents or the like. The production process also does not require any toxic or volatile toxic substances, in particular solvents. In addition, the further processing of the adsorptive structures is easy to handle; subsequent shaping or alterations, for example by sawing or cutting, are also possible. Moreover, the adsorptive structures of the invention can be easily purified with water. In addition, the adsorptive structures according to the invention are also suitable for foods and for medical applications because of their non-toxicity. Furthermore, the adsorptive structures according to the invention are distinguished in particular by a low density and thus a low weight, which is extremely advantageous for certain applications, for example as filter material for ABC protection masks.The self-supporting three-dimensional adsorptive structures according to the invention can be designed in a variety of ways. Possible embodiments of the invention are illustrated below for better understanding:As regards the hydrocolloid used, it can be provided according to the invention if this is a natural or nature-identical hydrocolloid. In this context, it can be provided in particular that the hydrocolloid is of vegetable or bacterial or animal origin.Furthermore, it can be provided within the scope of the present invention that the hydrocolloid is a macromolecule or comprises a plurality of macromolecules. Usually, such a macromolecule or hydrocolloid has an average molar mass, in particular a weight-average molar mass, in the range from 5,000 to 500,000 g / mol, in particular in the range from 10,000 to 400,000 g / mol, preferably in the range from 12,500 to 300,000 g / mol, preferably in the range from 15,000 to 250,000 g / mol. In particular, the weight-average molecular weight (M W) can be determined by gel permeation chromatography (GPC), in particular according to standardized measurement or determination methods (e.g. DIN 55672, ASTM D 3536-91 or OECD TG 119 (1996)).As far as the substance class of the hydrocolloid used is concerned, the hydrocolloid is preferably selected from the group of gelatin, collagen, xanthan, dextran, agar, carrageenan, carboxymethylcellulose, pectin, gum arabic, galactomannan, guar gum, locust bean gum and derivatives and mixtures or combinations thereof, preferably gelatin, collagen and derivatives and mixtures or combinations thereof. However, the hydrocolloid is particularly preferably gelatin, since this also enables excellent adhesion when small amounts are used. Hydrocolloids have the advantage over conventional binding and adhesion promoters that they are nontoxic and, moreover, even food compatible. In particular, no toxic or harmful vapors are formed during processing, which also has a positive effect on the economics of the production process of the structures according to the invention, since no complicated safety measures are necessary for removing the vapors.According to a particularly preferred embodiment, it can be provided in the context of the present invention that the hydrocolloid is gelatin and / or collagen and / or derivatives thereof. As regards the derivatives in particular, they may be made acidic or basic or chemically modified.The term "gelatin" is understood in the context of the present invention to mean in particular a polypeptide which is obtained predominantly by hydrolysis of the collagen contained in skin and bone of animals under acidic or basic conditions. In this case, the recovery of gelatin under acidic conditions leads to the so-called type A gelatin or the recovery under alkaline conditions leads to the so-called type B gelatin. Gelatin swells strongly in water, in particular under the simultaneous influence of heat, and dissolves therein to form a viscous solution, which finally solidifies in a gelatinous manner below 35° C. As far as possible chemical modifications of gelatin are concerned, these can be effected in particular by reaction in particular of the amino acid residues with mono- or polyfunctional reagents, such as, for example, acylating agents, aldehydes, epoxides, halogen compounds, cyanamide or activated unsaturated compounds. In this way, the properties of the gelatin can be varied widely, for example with regard to the solubility behavior and the formation of gel-like structures of the resulting solution. For further details on the term "gelatin", reference may be made to Rompp Chemielexikon, 10th edition, Georg Thieme Verlag Stuttgart / New York, keyword: "gelatin", page 1484, and the literature referred to herein, the content of which is hereby incorporated by reference in its entirety.As far as the adsorber particles used according to the invention are concerned, these can be designed in various ways within the scope of the present invention. The adsorber particles can be tailored, so to speak, or selected very specifically and in a targeted manner with regard to the respective field of application of the resulting adsorptive structure.It is usually provided within the scope of the present invention that the adsorber particles have an inner porous structure or an inner pore system. In this way, it can be ensured that the individual adsorber particles and thus also the resulting adsorptive structure according to the invention have a high overall adsorption capacity.In this context, it is provided according to the invention that the adsorber particles are configured in grain form, in particular in the form of a sphere. Adsorber particles of this type are distinguished, on the one hand, by their good accessibility for the substances to be adsorbed and their resulting improved adsorption capacity; on the other hand, owing to their geometry or their geometric shape, they are also outstandingly suitable for implementing a specific or individual shaping of the adsorptive structures, since they can be fixed to one another particularly well. The grain or spherical shape enables uniform or homogeneous packing and / or agglomeration of the adsorber particles. In addition, cavities result between the corresponding particles, through which the medium to be purified can flow.As regards the particle size of the adsorber particles to be used, this can vary within wide ranges. In the context of the present invention, it is provided that the adsorber particles have particle diameters (absolute) in the range from 0.001 to 3 mm, in particular 0.005 to 2.5 mm, preferably 0.01 to 2 mm, particularly preferably 0.02 to 1.5 mm, very particularly preferably 0.05 to 1 mm. In particular, it can be provided according to the invention that the adsorber particles have average particle sizes, in particular average particle diameters (D50), in the range from 0.01 to 2 mm, in particular 0.05 to 1.5 mm, preferably 0.1 to 1 mm.The corresponding particle sizes or diameters can be determined, for example, on the basis of the method according to ASTM D 2862-97 / 04. In addition, the above-mentioned variables can be determined using further determination methods based on sieve analysis, X-ray diffraction, laser diffractometry or the like. The respective determination methods are well known as such to the person skilled in the art, so that no further details are required in this respect.The material from which the adsorber particles consist or are formed can also be selected in many ways. In the context of the present invention, however, it is preferred if the material is selected from the group of activated carbon; zeolites; inorganic oxides, in particular silicon dioxides, silica gels and aluminum oxides; molecular sieves; mineral granules; clathrates; metalorganic framework materials (MOFs) and mixtures or combinations thereof. Particularly preferably, however, the adsorber particles consist of activated carbon or are formed from activated carbon.In this context, it is furthermore preferred according to the invention if the adsorber particles are formed from granular or activated carbon granules, in particular spherical activated carbon or activated carbon beads.With regard to the stability of the adsorber particles used, it is advantageous according to the invention if the adsorber particles, in particular the activated carbon particles or the activated carbon, preferably the activated carbon grains or activated carbon beads, have a burst pressure of at least 5 Newton, in particular a burst pressure in the range from 5 Newton to 50 Newton, per particle.The parameter data of the activated carbon now mentioned below are determined using standardized or explicitly specified determination methods or determination methods familiar to the person skilled in the art. Unless otherwise stated below, these parameter data are obtained in particular from the nitrogen sorption isotherms of the activated carbon.According to the invention, it can be provided in particular that the adsorber particles, in particular the activated carbon particles or the activated carbon, have a specific surface area (BET surface area) of at least 500 m 2 / g, in particular at least 750 m 2 / g, preferably at least 1,000 m 2 / g, particularly preferably at least 1,200 m 2 / g. In this context, it is particularly preferred if the adsorber particles, in particular the activated carbon particles, have a specific surface area (BET surface area) in the range from 500 to 4,000 m 2 / g, in particular 750 to 3,000 m 2 / g, preferably 900 to 2,500 m 2 / g, particularly preferably 950 to 2,000 m 2 / g.The determination of the specific surface area according to BET is fundamentally known to the person skilled in the art, so that no further details need be carried out in this regard. All BET surface area data relate to the determination according to ASTM D 6556-04. In the context of the present invention, the BET surface area is determined using, in particular, the so-called Multipoint BET determination method (MP-BET) in a partial pressure range p / p 0 of from 0.05 to 0.1. With regard to further details for determining the BET surface area or the BET method, reference may be made to the abovementioned ASTM D 6556-04 and to Rompp Chemielexikon, 10th edition, Georg Thieme Verlag, Stuttgart / New York, keyword: "BET method", including the literature referred to therein and to Winnacker-Kuchler (3rd edition), volume 7, pages 93 ff. and to Z. Anal. Chem. 238, pages 187 to 193 (1968).In addition, it can be provided in the context of the present invention that the adsorber particles, in particular the activated carbon particles or the activated carbon, have an adsorption volume V ads of at least 250 cm 3 / g, in particular at least 300 cm 3 / g, preferably at least 350 cm 3 / g, particularly preferably at least 400 cm 3 / g. In particular, it can also be provided that the adsorber particles, in particular the activated carbon particles, have an adsorption volume V ads in the range from 250 to 3,000 cm 3 / g, in particular 300 to 2,000 cm 3 / g, preferably 350 to 2,500 cm 3 / g.The adsorption volume V ads is a variable well known to the skilled person for characterizing the particulate adsorption materials used. The determination methods in this respect are also well known per se to the person skilled in the art. More specifically, the adsorption volume V ads is the weight-related adsorbed N 2- volume, which is generally determined at a partial pressure p / p 0 of 0.995.As regards the total pore volume according to Gurvich of the adsorber particles used, in particular the activated carbon particles or the activated carbon, this can be at least 0.30 cm 3 / g, in particular at least 0.50 cm 3 / g, preferably at least 0.55 cm 3 / g, preferably at least 0.60 cm 3 / g, particularly preferably at least 0.65 cm 3 / g, very particularly preferably at least 0.70 cm 3 / g. In particular, the adsorber particles, in particular the activated carbon particles, have a total pore volume according to Gurvich in the range from 0.30 to 2.0 cm 3 / g, in particular in the range from 0.50 to 2.0 cm 3 / g, preferably in the range from 0.55 to 1.5 cm 3 / g, preferably in the range from 0.60 to 1.2 cm 3 / g, particularly preferably in the range from 0.65 to 1.0 cm 3 / g.As regards the determination of the total pore volume according to Gurvich, this is a measurement or determination method known per se to the person skilled in the art. For further details regarding the determination of the total pore volume according to Gurvich, reference may be made, for example, to L. Gurvich (1915), J. Phys. Chem. Soc. Soot. 47, 805, and also to S. Lowell et al., Characterization of Porous Solids and Powders: Surface Area Pore Size and Density, Kluwer Academic Publishers, Article Technologies Series, pages 111 ff.In order to enable particularly good adsorption efficiency of the adsorptive structures according to the invention, it is furthermore preferred in the context of the present invention if the adsorber particles, in particular the activated carbon particles or the activated carbon, have a total porosity in the range from 10% to 80%, in particular 20% to 75%, preferably 25% to 70%.It can also be provided that the adsorber particles, in particular the activated carbon particles or the activated carbon, have a specific total pore volume in the range from 0.01 to 4.0 cm 3 / g, in particular 0.1 to 3.0 cm 3 / g, preferably 0.2 to 2.0 cm 3 / g. In this context, it is particularly preferred if the proportion of pores having pore diameters ≤75 Å, in particular ≤50 Å, is at least 65%, in particular at least 70%, preferably at least 75%. Likewise, it can be provided according to the invention that the proportion of micro- and meso-pores is at least 65%, in particular at least 70%, preferably at least 75%.In the context of the present invention, the term micropore denotes such pores having pore diameters of less than 2 nm, whereas the term mesopore denotes such pores having pore diameters in the range of 2 nm (i.e. 2 nm inclusive) to 50 nm inclusive and the term macropore denotes such pores having pore diameters of more than 50 nm (i.e. >50 nm).According to the invention, it is provided that the adsorptive structure comprises the hydrocolloid and the adsorber particles, in particular the activated carbon particles or the activated carbon, in a mass-related ratio of hydrocolloid to adsorber particles "[hydrocolloid:adsorber particles]" in the range from [1:100] to [1:1], in particular in the range from [1:80] to [1:2], preferably in the range from [1:50] to [1:5], preferably in the range from [1:30] to [1:10], particularly preferably in the range from [1:25] to [1:15], very particularly preferably in the range from [1:22] to [1:18], based on the respective dry weight.The defined and targeted selection of the hydrocolloid / adsorber particle ratio ensures-without wishing to be tied or limited to this theory-that the adsorber particles adhere well to one another on the one hand and thus result in a stable shaped body, but on the other hand that the adsorber particles are nevertheless readily accessible for the substances to be adsorbed and the adsorption performance is at least substantially not adversely affected. In particular, it is ensured that the binder does not penetrate, or at most only penetrates, into the macro pores of the adsorber particles used. By contrast, micro- and meso pores, which are of particular relevance for increased adsorption efficiency, in particular of harmful, toxic or odour substances, remain at least substantially free of binder. Moreover, the targeted selection of this very specific weight ratio contributes to producing a uniform and homogeneous pore system in the resulting adsorptive structure according to the invention, in particular in the adsorptive shaped body.As far as the amount of adsorber particles used is concerned, it can likewise vary within wide ranges. In the context of the present invention, it is preferred if the adsorptive structure comprises the adsorber particles, in particular the activated carbon particles or the activated carbon, in an amount of at least 70% by weight, in particular of at least 80% by weight, preferably of at least 75% by weight, preferably of at least 90% by weight, particularly preferably of at least 95% by weight, based on the total weight of the adsorptive structure. In particular, it can be provided that the adsorptive structure according to the invention comprises the adsorber particles, in particular the activated carbon particles, in an amount in the range from 70 to 99% by weight, in particular in the range from 80 to 98% by weight, preferably in the range from 85 to 97% by weight, preferably in the range from 90 to 96% by weight, particularly preferably in the range from 92.5 to 95% by weight, based on the total weight of the self-supporting structure.As for the hydrocolloid, moreover, it can be used in a variable amount. In the context of the present invention, it is generally provided that the adsorptive structure comprises the hydrocolloid in an amount of at most 30% by weight, in particular at most 20% by weight, preferably at most 15% by weight, particularly preferably at most 10% by weight, very particularly preferably however at most 5% by weight, based on the total weight of the adsorptive structure. In this context, it may be provided in particular that the adsorptive structure comprises the hydrocolloid in an amount in the range from 0.1 to 30% by weight, in particular in the range from 1 to 20% by weight, preferably in the range from 2 to 15% by weight, particularly preferably in the range from 3 to 10% by weight, very particularly preferably in the range from 4 to 7% by weight, based on the total weight of the adsorptive structure.With regard to the further configuration of the adsorptive structure according to the invention, it is preferred according to the invention if the adsorber particles, in particular the activated carbon particles or the activated carbon, are permanently or irreversibly joined to form the adsorptive structure by means of the hydrocolloid. The terms "permanent" or "irreversible" are to be understood within the scope of the present invention to mean that the connection or fixation or adhesion of the adsorber particles to the adsorptive structure, after shaping has been completed, in the structure according to the invention under normal conditions (1.013 bar and 22° C.) generally no longer changes and is thus, so to speak, a "rigid body" having a stable or mechanically loadable structure.With regard to the configuration of the adsorptive structure according to the invention, it is preferred according to the invention if the adsorber particles, in particular the activated carbon particles or the activated carbon, are brought into contact with the hydrocolloid by wetting. In the context of the present invention, this is to be understood in particular as meaning that the hydrocolloid is first brought into solution and subsequently the activated carbon particles are brought into contact with the hydrocolloid solution, for example by mixing in or introducing into the solution. By the subsequent removal of the solvent, the adsorber particles are connected to one another or fixed to one another with curing by means of the hydrocolloid, so that adsorber particles and hydrocolloid in their entirety form, so to speak, a matrix or a three-dimensional framework.In order to make good accessibility of the adsorber particles for substances to be adsorbed possible, it is additionally preferred if the surface of the individual adsorber particles, in particular of the activated carbon particles or of the activated carbon, in the adsorptive structure is covered and / or coated with hydrocolloid to the extent of in each case at most 50%, in particular at most 40%, preferably at most 30%, particularly preferably at most 20%, based on the surface of the respective adsorber particle. In particular, in this context, it may be provided that the surface of the individual adsorber particles, in particular of the activated carbon particles, of the adsorptive structure is covered and / or covered with hydrocolloid in each case in the range from 1 to 50%, in particular in the range from 5 to 40%, preferably in the range from 10 to 30%, based on the surface of the respective adsorber particle, in order to enable the adsorption of toxicants, harmful substances or odorants in an efficient manner.In the context of the present invention, it is also provided that the adsorptive structure is porous or foam-like or in the form of a foam. According to the invention, it is provided that the adsorptive structure has a pore system.As far as the adsorptive structure according to the invention is further concerned, it can be provided in particular that it has an open-pore or open-cell pore system or a closed or closed-cell pore system, preferably an open-pore or open-cell pore system.In this context, a porous or foam-like structure is understood according to the invention to mean a solid foam or a solid porous body-i.e. in particular based on a dispersion with a solid as dispersion medium and a gas as dispersed phase. Solid foams generally defined are structures of gas-, in particular air-filled, spherical or polyhedron-shaped pores or cells which are bounded by solid cell webs and / or lamellae. The cell webs and / or lamellae based on a material on which the foam is based, which are connected, so to speak, via nodes, form a coherent framework. In other words, the gas- or air-filled cells form a porous structure overall within the cell webs and / or lamellae. If the cell webs or lamellae are only incompletely formed or partially destroyed, an open-cell and / or open-cell foam is produced. An advantage of open-cell or open-cell pore systems is, in particular, that they are particularly readily accessible to the fluid media to be purified and, in general, hardly any pressure losses occur. For further details on the term "foam", reference may be made to Rompp, Chemielexikon, 10th edition, Georg Thieme Verlag, Stuttgart / New York, keyword: "Foam", pages 3950 and 3951 and the literature referred to therein, the entire content of which in this respect is hereby incorporated by reference in its entirety.As regards the pore system of the adsorptive structure according to the invention in particular, this is formed by the at least one hydrocolloid and the adsorber particles. In particular, it can be provided according to the invention that the adsorber particles are connected or fixed to one another in a web-like or punctiform manner by means of the hydrocolloid, wherein the surface of the adsorber particles is generally only covered to a slight extent with hydrocolloid. The hydrocolloid can thus form a "connecting web" between individual adsorber particles, wherein it is also possible for the "connecting web" as such to be connected or equipped with further adsorber particles. According to the invention, the pore system formed by the adsorber particles and the hydrocolloid has air-filled cavities or pores. In order to make good flow-throughability with the fluid media to be purified possible, it is preferred according to the invention if the air-filled cavities or pores are connected to one another or are in contact with one another, i.e. if, as mentioned above, they form an open-pored or open-celled pore system.As for the average pore sizes of the pore system, they are variable and can be tailored according to the purpose of use of the adsorptive structure of the invention. In this context, it may be provided according to the invention that the ratio of the average pore size of the pore system of the adsorptive structure to the average particle size of the adsorber particles [average pore size of the pore system:average particle size of the adsorber particles] is in the range from 0.01:1 to 10 000:1, in particular from 0.2:1 to 1 000:1, preferably from 0.5:1 to 500:1, preferably from 1:1 to 250:1, more preferably from 1.2:1 to 200:1, most preferably from 1.5:1 to 100:1. Likewise, it can be provided that the ratio of the average pore size of the pore system of the adsorptive structure to the average particle size of the adsorber particles [average pore size of the pore system:average particle size of the adsorber particles] is at least 0.1:1, in particular at least 0.5:1, preferably at least 1:1, preferably at least 1.2:1, particularly preferably at least 1.5:1, very particularly preferably at least 2:1, even more preferably at least 3:1.According to the invention, the adsorptive structure according to the invention can additionally have a porosity (porosity) in the range from 2 to 100 ppi (=pores per inch), in particular 5 to 90 ppi, preferably 10 to 80 ppi, preferably 15 to 75 ppi. In this way, a gas permeability or permeability for liquids is ensured with simultaneously good adsorption performance.It is furthermore advantageous if the adsorptive structure according to the present invention has pores having an average pore diameter in the range from 0.001 to 10 mm, in particular 0.01 to 8 mm, preferably 0.05 to 5 mm, preferably 0.1 to 3 mm. In other words, the adsorptive structure has the form of a foam or porous framework which has, in particular, open cells or pores with a web-like boundary, this boundary being formed, in particular, by the composite or the composite material of adsorber particles and hydrocolloid.The adsorptive structure according to the invention is extremely diverse in its moldability and can be brought, in particular by pouring, into virtually any conceivable geometric shape and size or can be present in virtually any geometric shape and size.In this context, it can be provided within the scope of the present invention that the adsorptive structure is formed monolithically or integrally.For example, it is possible for the adsorptive structure to be cylindrical, rod-shaped, plate-shaped, cuboidal, polyhedronic, honeycomb-shaped or the like. In particular, it is also possible according to the invention for the adsorptive structure to be additionally provided with defined perforations or channels within the scope of shaping. In this case, owing to the excellent properties of the adsorptive structures according to the invention, there are no sustained losses in stability in the shaped body.According to an alternative embodiment of the present invention, however, it can also be provided that the adsorptive structure is present as an agglomerate (fracture agglomerate). In this context, it is particularly preferred if a single agglomerate comprises in each case at least 5 adsorber particles, in particular at least 10 adsorber particles, preferably at least 15 adsorber particles, preferably at least 20 adsorber particles or more. Likewise, it can be provided that a single agglomerate comprises in each case up to 50 adsorber particles, in particular up to 75 adsorber particles, preferably up to 100 adsorber particles.The fracture agglomerates according to the invention generally have significantly fewer adsorber particles than the previously described embodiments based on the monolithic shaped bodies and, in addition, generally have a significantly smaller size in comparison therewith. However, as regards the microstructure or the basic structure, both embodiments do not differ from one another since such agglomerates are obtained in particular by breaking or mortars of larger monolithic or one-piece adsorptive structures or adsorptive shaped bodies. In this context, it was completely surprising that, owing to the sole use of the hydrocolloid as binder for fixing or bonding the adsorber particles, the resulting agglomerates still have sufficient stability with simultaneously good adsorption performance even after breaking or mortaring. According to the invention, a large number of such agglomerates are particularly suitable for use as filter material in the form of a loose bed.In particular, the adsorptive structures of the invention have excellent adsorption properties which are described below:The adsorptive structure, in particular a multiplicity of adsorptive structures in loose packing or as monolithic shaped bodies, have in particular a longitudinal pressure loss at a flow rate of 0.2 m / sec of not more than 150 Pa / cm, preferably not more than 100 Pa / cm, preferably not more than 90 Pa / cm, particularly preferably not more than 70 Pa / cm, very particularly preferably not more than 50 Pa / cm. In particular, it can be provided that the adsorptive structure, in particular a multiplicity of adsorptive structures in loose packing or as monolithic shaped body, has a longitudinal pressure loss at a flow rate in the range from 10 to 1,000 Pa / cm, in particular in the range from 25 to 500 Pa / cm, preferably in the range from 30 to 250 Pa / cm, particularly preferably in the range from 40 to 200 Pa / cm.As for butane adsorption of the adsorptive structure of the present invention, it should be at least 20%, especially at least 25%, preferably at least 30%. In particular, the butane adsorption of the adsorptive structure can be in the range from 20 to 80%, in particular in the range from 25 to 70%, preferably in the range from 30 to 65%.Also as for resistance to physical and chemical influences, the adsorptive structure of the present invention has excellent properties. The adsorptive structure according to the invention usually has a temperature resistance of at least 100° C., in particular at least 130° C., preferably at least 180° C., particularly preferably at least 200° C. The adsorptive structure according to the invention is also at least substantially insoluble in organic, in particular aprotic solvents, in particular acetone.Further advantageous properties, aspects and features of the present invention are evident from the following description of the exemplary embodiment shown in the single figure. It shows:FIG. shows a schematic illustration of an adsorbent structure according to the invention based on adsorber particles in cross section and two enlargements of the sections of the pore system of the adsorbent structure.The single FIGURE shows a schematic illustration of the cross section of a monolithic cylindrical adsorptive structure 1 according to the invention on the basis of adsorber particles 2 which are made to adhere to one another by means of a hydrocolloid 3, in accordance with a special embodiment of the present invention. The single figure shows the foam-like or porous structure of the adsorptive structure 1, wherein the latter has a preferably open pore system having numerous pores 4, wherein the pores 4 are generally significantly larger than the adsorber particles 2 adapted thereto. The pore 4 is bounded by a plurality of individual adsorber particles 2. The adsorber particles 2 are fixed to one another or connected to one another by the hydrocolloid 3, wherein adsorber particles 2 and hydrocolloid 3 form, so to speak, a matrix or a framework which has a further pore system which is likewise in particular open-pored and generally has smaller pores 4' which are formed overall by the adsorber particles 2 directly arranged to one another by means of the hydrocolloid 3. The second enlargement of the detail shows the structure of the more narrow-pore pore system based on the pore 4'. The individual adsorber particles 2 are permanently or irreversibly connected to the adsorptive structure 1 in particular in punctiform fashion via hydrocolloid webs 3, the surface of the adsorber particles 2 preferably being covered with hydrocolloid to the extent of at most 20%.The above statements show that it has been possible for the first time within the scope of the present invention to provide self-supporting three-dimensional adsorptive structures based on a multiplicity of adsorber particles which, by virtue of the intended use according to the invention of a hydrocolloid as binder, have good mechanical stability and excellent adsorption properties and also variable or intended formability into virtually any conceivable geometric shape and size.The present invention further provides, according to a second aspect of the present invention, a method for producing a self-supporting three-dimensional adsorptive structure, in particular an adsorptive shaped body, in particular as defined above, wherein the method comprises the following steps in the sequence (a) to (c) specified below: (a) production of a solution and / or dispersion of at least one hydrocolloid selected from the group of gelatin, collagen, xanthan, dextran, agar, carrageenan, pectin, gum arabic, galactomannan and derivatives and mixtures or combinations thereof; (b) contacting the solution and / or dispersion prepared in step (a) with a plurality of individual granular adsorber particles having absolute particle diameters in the range from 0.001 to 3 mm to obtain a suspension of the adsorber particles in the solution and / or dispersion of the hydrocolloid, wherein the adsorber particles are used in a mass-related ratio of hydrocolloid to adsorber particles "[hydrocolloid:adsorber particles]" in the range from [1:100] to [1:1], based on the respective dry weight, and wherein by releasing gases from the adsorber particles and / or by introducing gases a volume expansion and / or formation of a foam and / or a porous structure in the suspension takes place, wherein the volume expansion and / or formation of a foam and / or a porous structure is controlled by applying shear forces and adjusting the suspension to temperatures in the range from 50 to 150° C.; (c) removing the solution and / or dispersion medium from the suspension and curing to obtain the self-supporting three-dimensional adsorptive structure.In other words, the invention thus relates to a method for producing a self-supporting three-dimensional adsorptive structure, in particular an adsorptive shaped body, in particular as defined above, wherein a multiplicity of individual adsorber particles are brought into suspension in a solution and / or dispersion of at least one hydrocolloid and subsequently the solution and / or dispersion medium is removed from the suspension in order to obtain the self-supporting three-dimensional adsorptive structure.In the context of the present invention, it has been shown in a completely surprising manner that self-supporting three-dimensional structures having adsorptive properties, which have the positive properties described above, can be obtained by means of the method according to the invention.The details and specific features of the process according to the invention are described in detail below:With regard to the performance of method step (a) or the provision of the solution and / or dispersion of the hydrocolloid, it has proven to be particularly advantageous if the solvent for obtaining the solution or dispersion of the at least one hydrocolloid is selected from the group of aqueous and organic solvents and mixtures or combinations thereof, in particular from the group of water, ethylene glycol, glycerol, formamide and acetic acid and mixtures or combinations thereof. However, water is preferably used as solvent.With regard to the amount of hydrocolloid used to provide the solution and / or dispersion of the hydrocolloid used and / or of the hydrocolloid used in method step (a), this can be selected according to the invention in such a way that, on the one hand, good stability of the resulting shaped body is ensured, on the other hand, the adsorption properties are nevertheless not impaired and as small as possible proportions of the surface of the adsorber particles are covered with hydrocolloid. In this context, it has proven to be particularly advantageous if, in order to provide the solution and / or dispersion of the hydrocolloid and / or in method step (a), the at least one hydrocolloid is used in an amount in the range from 0.1 to 30 wt %, in particular in the range from 0.5 to 15 wt %, preferably in the range from 1 to 10 wt %, preferably in the range from 2 to 8 wt %, based on the solvent and / or the dispersion.The solution and / or dispersion of the hydrocolloid and / or process step (a) can be provided with heating to temperatures in the range from 40 to 120° C., in particular in the range from 50 to 110° C., preferably in the range from 60 to 100° C., preferably in the range from 70 to 90° C. In addition, it has proven advantageous if, when the solution and / or dispersion of the hydrocolloid is provided and / or in method step (a), the process is carried out with application of shear forces, in particular with stirring. In this way, a uniform solution or dispersion of the hydrocolloid in the respective solvent is achieved, which is deposited in the resulting products in the formation of a particularly homogeneous pore system in the foam according to the invention.The solution or dispersion produced in the context of the provision of the solution and / or dispersion of a hydrocolloid and / or of process step (a) can be used-in particular as explained below-to provide a suspension of adsorber particles in order on this basis to subsequently obtain the adsorptive shaped body according to the invention.As regards the amount of adsorber particles used according to the invention, it is provided in the context of the present invention that, when the suspension of a plurality of individual adsorber particles is provided in the solution and / or dispersion of the hydrocolloid and / or when, in process step (b), the adsorber particles are used in a mass-related ratio of hydrocolloid to adsorber particles "[hydrocolloid:adsorber particles]" in the range from [1:100] to [1:1], in particular in the range from [1:80] to [1:2], preferably in the range from [1:50] to [1:5], preferably in the range from [1:30] to [1:10], particularly preferably in the range from [1:25] to [1:15], very particularly preferably in the range from [1:22] to [1:18], based on the respective dry weight. Surprisingly, it has been found in this context that the specific setting of a defined ratio of hydrocolloid to adsorber particles can impart particularly good stability and a homogeneous pore system to the adsorptive structures according to the invention.With regard to the provision of the suspension of a plurality of individual adsorber particles in a solution and / or dispersion of the hydrocolloid and / or process step (b), it can be provided according to the invention that, by contacting the provided solution and / or dispersion of the at least one hydrocolloid produced in step (a) with the plurality of individual adsorber particles to obtain the suspension of the adsorber particles, the proportion of the solvent in the suspension is adjusted to a range from 20 to 90 wt %, in particular to a range from 25 to 80 wt %, preferably to a range from 30 to 70 wt %, preferably to a range from 35 to 60 wt %, based on the suspension. By the defined proportion of the solvent in relation to adsorber particles and hydrocolloid, according to the invention, a particularly homogeneous pore system can be produced in the adsorptive structure, which in turn improves the flow behavior of the fluid media to be purified within the shaped body.Furthermore, it is provided in the context of the present invention that, when a suspension of a plurality of individual adsorber particles is provided in a solution and / or dispersion of the hydrocolloid or in method step (b), volume expansion and / or formation of a foam and / or a porous structure in the suspension takes place by releasing gases from the adsorber particles and / or by introducing gases.In this context, without wishing to be limited to this theory, foam formation takes place, as it were, by forming gas- or air-filled cavities in the suspension of adsorber particles in a solution and / or dispersion of the hydrocolloid, by means of which cavities, as it were, a pore system is formed in the suspension.In this context, the formation of a foam and / or a porous structure is also to be understood as meaning that gas-filled cells are formed as a result of the gases, in particular air, emerging or being introduced into the suspension, said cells being bounded by liquid cell webs based on hydrocolloid and the solvent and also the adsorber particles. This is thus initially in particular a liquid or viscous foam, i.e. a dispersion of a liquid as the dispersed phase in which both the solid adsorber particles and the gas, in particular the air, are preferably dispersed. A system is formed, as it were, which comprises adsorber particles, hydrocolloid and air-filled cavities, wherein the air-filled cavities are bounded by adsorber particles and hydrocolloid and, after curing, form the pore system in the adsorptive structure according to the invention in the form of a solid foam, as it were. For further details on the term "foam" and "foam formation", reference may be made to Rompp, Chemielexikon, 10th edition, Georg Thieme Verlag, Stuttgart / New York, keyword: "foam", pages 3950 and 3951, and the literature referred to therein, the content of which in this respect is hereby incorporated by reference in its entirety.In the context of the present invention, it is provided that the provision of the suspension of a multiplicity of individual adsorber particles in a solution and / or dispersion of the hydrocolloid and / or that in process step (b) the volume expansion and / or the formation of a porous and / or foam-like structure is carried out with application of shear forces, in particular with stirring. In this way, a uniform or homogeneous distribution of the adsorber particles in the suspension is made possible.According to the invention, it is provided that, when the suspension of a plurality of individual adsorber particles is provided in a solution and / or dispersion of the hydrocolloid and / or that, in process step (b), the suspension is adjusted to temperatures in the range from 50 to 150° C., in particular in the range from 60 to 140° C., preferably in the range from 70 to 130° C., preferably in the range from 80 to 120° C., particularly preferably in the range from 90 to 110° C. This allows the formation of uniform and homogeneous porous structures or foams to be improved.In addition, it is possible to further adjust the porosity of the resultant adsorptive structures by the duration of the introduction of shear forces, in particular of stirring, of the suspension. In this context, it has proven to be particularly advantageous if, when the suspension of a plurality of individual adsorber particles is provided in a solution and / or dispersion of the hydrocolloid and / or in process step (b), the introduction of shear forces, in particular the stirring, of the suspension takes place over a period in the range from 5 to 180 s, in particular in the range from 10 to 150 s, preferably in the range from 15 to 120 s, preferably in the range from 20 to 100 s. The studies carried out by the applicant have shown that with an increase in the stirring durations in the stated range, the pore system in the resulting adsorptive structure becomes both more narrow-pored and homogeneous. Short stirring durations, on the other hand, generally result in adsorptive structures having a large-pore pore system.Depending on the field of application, the pore system produced can be tailored, so to speak, by means of the method according to the invention, in particular on the basis of the measures described above.After the completion of the provision of the suspension of a multiplicity of individual adsorber particles in a solution and / or dispersion of the hydrocolloid and / or of process step (b), the removal of the solution and / or dispersion medium generally takes place in order to obtain the self-supporting three-dimensional adsorptive structure according to the invention.According to the invention, it can be provided in particular in this regard that the removal of the solution and / or dispersion medium and / or that process step (c) takes place with formation of a porous and / or foam-like structure. In this context, a porous or foam-like structure is to be understood as meaning, in particular, a dispersion based on a solid as the dispersion medium and a gas as the disperse phase. In this case, without wishing to be limited to this theory, gaseous bubbles or pores-resulting from the gas retained or introduced in the suspension of adsorber particles-are enclosed by solid cell lamellae or webs-namely the adsorber particles and the hydrocolloid.With regard to the removal of the solution and / or dispersion medium and / or with regard to process step (c), it is particularly preferred if the process is carried out with heating and / or adjustment of the suspension to temperatures in the range from 70 to 200° C., in particular in the range from 90 to 180° C., preferably in the range from 100 to 160° C., particularly preferably in the range from 110 to 150° C. The removal of the solution and / or dispersion medium and / or process step (c) can generally be carried out with heating and / or adjustment of the suspension to temperatures of at least 70° C., in particular at least 90° C., preferably at least 110° C., particularly preferably at least 130° C. In the context of the method according to the invention, it is also possible in this context to further control, in particular, the homogeneity of the pore distribution and the pore volumes by adjusting the temperature during the removal of the solution and / or dispersion medium. In the context of the studies carried out, it has namely been found that relatively large pores or pore volumes can generally also be produced by relatively high temperatures, while relatively low temperatures generally lead to relatively low pore sizes.In addition, it is possible within the scope of the present invention for the removal of the solution and / or dispersion medium and / or for process step (c) to be carried out with optionally further volume expansion and / or with optionally further formation of a foam and / or a porous structure, in particular by introducing gases, in the suspension.It has additionally proven to be particularly advantageous in the context of the present invention if the removal of the solution and / or dispersion medium and / or if process step (c) is carried out with shaping and / or formation of the self-supporting three-dimensional adsorptive structure. As regards the shaping or formation of the structure according to the invention, this can be effected in particular by pouring it out into a corresponding (casting or casting) mold. By means of the process according to the invention it is surprisingly possible to bring the adsorptive structures according to the invention, in particular the adsorptive shaped bodies, into virtually any conceivable geometric shape and size without this suffering adsorption performance or stability. In addition, it is also possible to equip the molded bodies with perforations which completely pass through the molded body without loss of stability, in particular on the basis of the selection of special shapes.With regard to the method according to the invention, it can be provided in particular that the removal of the solution and / or dispersion medium and / or that process step (c), in particular for curing the suspension, is carried out over a period of time in the range from 2 to 22 hours, in particular in the range from 4 to 20 hours, preferably in the range from 8 to 18 hours, preferably in the range from 10 to 14 hours.As described above, the process according to the invention results in self-supporting three-dimensional adsorptive structures according to the invention, in particular adsorptive shaped bodies, which have significantly improved properties compared with the corresponding materials of the prior art. In particular, the process according to the invention as such is extremely easy to handle.Moreover, the present invention also relates to a self-supporting structure having adsorptive properties, which is obtainable by the process described above.The present invention also provides, according to a third aspect of the present invention, the use of at least one hydrocolloid for connecting or fixing or adhering individual adsorber particles to one another to obtain a self-supporting three-dimensional adsorptive structure, in particular an adsorptive shaped body, as defined above, or the use of a hydrocolloid to connect individual adsorber particles to one another and / or fix them to one another and / or adhere them to one another, in particular obtaining a self-supporting three-dimensional adsorptive structure as already defined above.In addition, the self-supporting three-dimensional adsorptive structures according to the invention allow a broad range of applications.The present invention therefore further provides, according to a fourth aspect of the present invention, the use of a self-supporting three-dimensional adsorptive structure as defined above for the adsorption of toxicants, pollutants and odors, in particular from gas or air streams or else from liquids, in particular water, or for the purification or treatment of gases, gas streams or gas mixtures, in particular air, or of liquids, in particular water.Furthermore, it can be provided within the scope of the present invention to use a self-supporting three-dimensional adsorptive structure as described above in adsorption filters or for producing filters, in particular adsorption filters, and / or as substrate or support (material), in particular for catalysts and / or catalytic systems and / or reactive compounds.The present invention also relates, according to one aspect of the present invention, to a filter comprising a self-supporting three-dimensional adsorptive structure as defined above.With regard to the filter according to the invention, it can be provided in particular that it has a longitudinal pressure loss at a flow speed of 0.2 m / s of at most 150 Pa / cm, preferably at most 100 Pa / cm, preferably at most 90 Pa / cm, particularly preferably at most 70 Pa / cm, very particularly preferably at most 50 Pa / cm.In addition, it has proven advantageous if the filter according to the invention has a longitudinal pressure loss at a flow speed of 0.2 m / s in the range from 5 to 150 Pa / cm, preferably in the range from 5 to 100 Pa / cm, preferably in the range from 7.5 to 90 Pa / cm, particularly preferably in the range from 10 to 80 Pa / cm.In the context of the present invention, it has thus been possible for the first time to provide self-supporting three-dimensional adsorptive structures, in particular adsorptive shaped bodies, which, with individual and in particular targeted moldability, simultaneously have a high stability and excellent adsorption properties. Such materials which combine all the aforementioned properties have not yet been produced or provided in the prior art.Further embodiments, modifications and variations of the present invention can be easily recognized and realized by the person skilled in the art upon reading the description without thereby departing from the scope of the present invention.The present invention is illustrated by the following working examples, which, however, are not intended to limit the present invention in any way.EMBODIMENTS:The production of self-supporting three-dimensional adsorptive structures according to the invention as monolithic shaped bodies on the one hand and as fracture agglomerate on the other hand is described below.To produce the structures according to the invention, spherical adsorber particles based on activated carbon are used as adsorber particles (obtainable, for example, from Blucher GmbH, Erkrath, Germany, or from Adsor-Tech GmbH, Premnitz, Germany).1. Production of Inventive Shaped Bodies and Fracture AgglomeratesProduction of Inventive Shaped BodiesThe inventive moldings were produced by first dissolving 1 g of gelatin granules as hydrocolloid in 25 ml of distilled water while heating to 80° C. and stirring. 20 g of the adsorber particles in the form of spherical activated carbon were added to the gel formed in the process. The solvent content was about 54% by weight, based on the total weight of the suspension produced. The ratio [hydrocolloid:adsorber particles] was 1:20. When the adsorber particles were added to the gel, some of the air present in the pores of the activated carbon emerged, in particular by temperature-induced volume expansion and displacement of water, which led to a doubling of the volume of the suspension. Subsequently, by further heating to a temperature of 100° C. and stirring over a period of 40 seconds, the volume of the gel adsorber particle mass was adjusted to about 40% of the maximum volume in order to produce an average pore size distribution of the remaining shaped body. Subsequently, the molding composition was charged into a mold. Curing was then carried out in a drying cabinet at a temperature of 130° C. over a period of 12 hours. The result was shaped bodies having a uniformly distributed pore system with average pore sizes.In connection with the production of adsorptive shaped bodies, test series were also carried out in which the following parameters were varied:• Ratio [hydrocolloid:adsorber particles]• Amount of solvent• Stirring Time• Cure temperatureRatio [hydrocolloid:adsorber particles]In addition to the ratio [hydrocolloid:adsorber particles] of 1:20 described above, [hydrocolloid:adsorber particles] ratios of 1:5, 1:10, 1:25 and 1:30 were also tested. The remaining parameters (amount of solvent, stirring time, curing temperature) were kept constant as described above.In this connection, it has been found that shaped bodies which have [hydrocolloid:adsorber particles] ratios of 1:5 and 1:10 are slightly impaired in their adsorption properties by the high gel content, since the adsorber particles are slightly less accessible, since there is a slightly increased coverage with the hydrocolloid. Overall, the adsorption performances when using the aforementioned ratios are nevertheless to be evaluated as satisfactory. Shaped bodies with [hydrocolloid:adsorber particles] ratios of 1:25 or 1:30, on the other hand, are slightly more unstable due to the very small amount of hydrocolloid as "adhesive". However, for the typical fields of application of such shaped bodies for purifying fluid media such as gaseous media, the stability is still satisfactory. The mechanically most stable shaped body, in which the surface of the adsorber particles is nevertheless only minimally covered with hydrocolloid, could be produced using a [hydrocolloid:adsorber particle] ratio of 1:20.Amount of SolventTo investigate the influence of the amount of solvent used on the properties of the shaped bodies according to the invention, solvent fractions of 25% by weight, 35% by weight, 50% by weight, 60% by weight and 75% by weight, based on the suspension of hydrocolloid, adsorber particles and solvent, were used. The remaining parameters (ratio [hydrocolloid:adsorber particles], stirring time, curing temperature) were kept constant as described above.It was found that the use of solvent contents of less than 25 wt % leads to a slightly impaired distribution of the hydrocolloid. Solvent fractions of more than 60% by weight, on the other hand, lead to less well distributed and inhomogeneous pore systems. In particular, somewhat larger pores are formed in the interior of the shaped body, whereas the pores have smaller diameters in the outer regions. The best results are thus achieved when solvent fractions of from 35% by weight to 60% by weight are used. Nevertheless, even when using smaller or larger amounts or proportions of the solvent, moldings which overall have satisfactory properties can be provided.Stirring TimeTo investigate the influence of the stirring time on the pore system of the shaped bodies, stirring times in the range from 10 to 150 s were used. The remaining parameters (ratio [hydrocolloid:adsorber particles], amount of solvent, curing temperature) were kept constant as described above.It has been found here that with increasing stirring time, more narrow-pore to closed pore systems can be produced. For formulations with a total weight of the suspension of hydrocolloid, solvent and adsorber particles of 46 g, an open-cell pore system with an average pore size distribution could be produced at a stirring time of 37 to 40 seconds. Short stirring durations, on the other hand, lead to larger pores in the adsorptive structure. It is thus possible to control the pore size distribution or the porosity of the adsorptive structure in a targeted manner by correspondingly adapting the stirring durations.Cure TemperatureTo investigate the influence of the curing temperature on the pore system of the moldings, temperatures of 60° C., 70° C., 85° C., 100° C., 110° C., 130° C. and 150° C. were used for curing times of 2 hours. The remaining parameters (i.e. ratio [hydrocolloid:adsorber particles], amount of solvent, stirring duration) were kept constant as described above.In this context, it has been found that temperatures below 110° C. lead to larger hollow spaces at the outer layer than at the base of the shaped bodies and thus a partly inhomogeneous pore system is produced. A curing temperature of 130° C. leads to a particularly homogeneous and uniform pore system in the resulting molded bodies. In addition, it is possible to produce larger pore volumes by using temperatures of more than 130° C. with simultaneously shorter curing times.Preparation of Fracture Agglomerates According to the InventionFor the production of broken agglomerates, 4 g of gelatine granules as hydrocolloid were dissolved in 100 ml of distilled water at a temperature of 80° C. with continuous stirring. To the resulting gel was added 80 g of adsorbent so that the [hydrocolloid:adsorbent particle] ratio was 1:20. As a result of the evolution of gas which occurred, the volume of the suspension based on hydrocolloid, adsorber particles and solvent was doubled. By further heating the suspension to 100° C. and continuous stirring, the volume was concentrated until a viscous mass was formed, which was then transferred to a dish for curing. Curing took place at 130° C. in a drying cabinet. After cooling, first a coarse comminution was effected with the mortar, then a fine comminution in the screen. The obtained break agglomerates were fractionated or classified by sieving. For analyses to be described below, the fractional agglomerate fractions I, II and III were retained, the agglomerates of fraction I having a size of 0.6 to 1.0 mm, those of fraction II having a size of 0.8 to 1.25 mm and those of fraction III having a size of 1.25 to 2.5 mm.Production of Comparative Shaped Bodies and Comparative Fracture AgglomeratesFor comparison purposes, moldings and comparative breaking agglomerates based on activated carbon, not according to the invention, on the one hand, and a thermoplastic hotmelt adhesive as adhesion promoter or binder, on the other hand, were also produced.For this purpose, a thermoplastic hot melt adhesive was sprayed onto granular activated carbon particles at temperatures in the range from 150 to 180° C. The activated carbon particles sprayed with adhesion promoter were converted into a corresponding shape to obtain a cylindrical shaped body for curing. Here too, a [hotmelt adhesive:adsorber particles] ratio of 1:20 was initially used. However, the molded articles produced in this manner were extremely unstable even without external application of pressure. Furthermore, moldings having a [hotmelt adhesive:adsorber particles] ratio of 3:7 and 4:6 were produced. Even at a ratio of 3:7, the molded articles were extremely unstable and deformable at room temperature. Only from a [hot melt adhesive:adsorber particles] ratio of 4:6 could a stability be achieved which would make it possible at all to use the shaped body for purifying fluid media such as gaseous media. Nevertheless, the mechanical stability of such comparative shaped bodies was significantly lower than that of the shaped bodies according to the invention. In addition, analogously to the fracture agglomerates according to the invention, starting from the comparative shaped body having a [hotmelt adhesive:adsorber particle] ratio of 4:6, comparative fracture agglomerates were produced by mortaring and subsequent finer comminution with the aid of a sieve. These too were significantly more unstable compared to the fracture agglomerates according to the invention.In addition, the comparative shaped bodies and fracture agglomerates were analyzed industrially for subsequent comparison with the shaped bodies and fracture agglomerates according to the invention. In this connection, their resistance to (air) moisture and organic solvents was investigated. In addition, their temperature resistance was determined.As for the temperature resistance of the comparative molded articles and fracture agglomerates, it was insufficient. At temperatures of 170° C., a strong decomposition was already observed. Resistance to organic solvents, in particular to acetone, was also unsatisfactory since the hot-melt adhesive used was attacked by the solvents. Resistance to atmospheric humidity, on the other hand, was largely satisfactory.2. Industrial Analysis of the Inventive Shaped Bodies and Fracture AgglomeratesBoth the structures according to the invention in the form of shaped bodies and in the form of broken agglomerates were investigated with regard to their adsorption performance. Furthermore, analyses were carried out in order to test the resistance of the adsorptive structures to chemico-physical influences.Resistance to (air) moistureTo characterize the resistance to (air) moisture, both the fracture agglomerates and the shaped bodies were stored in a climate cabinet at an air humidity of 80% and a temperature of 65° C. for a period of 94 hours. The molded bodies were stable in shape and the pore system remained intact despite the high atmospheric humidity at at the same time relatively high temperatures, which accelerate the solubility of gelatin on contact with water. After storage in a climate control cabinet, the molded bodies exhibited only a slight deformation under the influence of pressure. No decomposition or decomposition could be observed in the fracture agglomerates either.Resistance to acetoneFurthermore, the shaped bodies and fracture agglomerates were examined for their solubility in acetone. For this purpose, both shaped bodies and also broken agglomerates were immersed in acetone over a period of 2 hours and then dried in air. In this connection, neither decomposition nor deformation under pressure could be observed in the molded bodies or agglomerates.Heat resistanceThe structures according to the invention exhibited excellent properties also with respect to resistance to high temperatures. Both shaped bodies and also fracture agglomerates were stable at temperatures of 200° C. and only started to decompose from temperatures of at least 250 to 300° C.3. Analysis of the Adsorption Performance of Inventive and Comparative Manufactured Molded Articles and Fracture AgglomeratesTo determine the adsorption performance, the butane adsorption of the inventive moldings and of the comparative moldings was determined. All the molded bodies tested were cylindrical and had a cylinder height of 20 mm and a cylinder diameter of 50 mm. The shaped body according to the invention had a [hydrocolloid:adsorber particles] ratio of 1:20. The comparative shaped body had a [hotmelt adhesive:adsorber particle] ratio of 4:6. The height of the bulk material was 20 mm and the diameter of the bulk material was 50 mm.The basic adsorbents on which the shaped bodies or fracture agglomerates are based, i.e. the granular activated carbon particles used, had a butane adsorption or adsorption performance of 32.7% by weight. The fracture agglomerates according to the invention could achieve an adsorption performance of 31.6% by weight. The adsorption performance of the moldings of the invention was 30.4% by weight. These results confirm that, when a hydrocolloid is used as adhesive or binder, the adsorption performance of the base adsorbents is at least substantially not impaired. In contrast, in the case of the comparative shaped bodies, the adsorption performance was only 11.0% by weight, which is to be regarded as a clear indicator of impairment of the adsorption performance by the adhesion promoter used. A similar drop in the adsorption performance compared with the fracture agglomerates according to the invention was observed in the case of the comparative fracture agglomerates as well; it was only 12.3% by weight here.Moreover, the cylindrical shaped bodies of the present invention and the agglomerates of fractions I, II and III which differ from each other in size were examined for pressure losses and initial breakthroughs with respect to cyclohexane as the substance to be adsorbed. The results thereof are shown in Table 1. Table 1: Determination of Pressure Losses and Initial Breakthroughs of the Inventive Shaped Bodies and Fracture Agglomerates Table 1: Determination of Pressure Losses and Initial Breakthroughs of the Inventive Shaped Bodies and Fracture AgglomeratesAgglomerate Size [mm]0,6 - 1,00,8 - 1,251,25 - 2,5-Bulk height [mm]20,020,020,020,0 (Cylinder Height)Volm. Bulk [mm]50,050,050,050,0 (Cylinder Diameter)Weight of bulk material [g]17,916,112,9-Bulk density [g / cm 3]0,50,40,3-Toluene concentration [ppm]79,479,879,379,5Temperature [° C.]23,023,223,223,0rel. Moisture [%]49,949,949,949,9Inflow Wind. (Target value) [m / s]0,10,10,10,1Pressure loss [Pa]21,819,315,123,2Volume [%] / time [min]10,00,00,00,050,00,00,00,0100,00,00,00,0300,10,10,10,0600,10,10,10,01200,10,10,10,01800,10,10,10,12400,10,10,10,13600,10,10,10,16000,10,10,20,19000,30,41,00,21.2000,91,23,80,3Time [min] to Breakthrough [%]51.649,31.344,01.100,51.948,2101.715,71.385,11.172,32.053,4301.799,31.460,71.286,32.258,1The results shown in Table 1 show that pressure losses of at most 23.2 Pa occur in the structures according to the invention. The pressure losses in agglomerates in loose packing are even somewhat lower than in the case of the shaped bodies, since the shaped body has a higher density. The break-through properties of the shaped bodies and agglomerates according to the invention are also excellent. As regards the initial break-through, the shaped body has slightly improved properties compared with the agglomerates. Nevertheless, the times until the initial break-through are also excellent in the agglomerates in a loose bed and are only slightly shorter than in the case of the molded bodies.The above statements show that the structures according to the invention-both the shaped bodies and the fracture agglomerates-are distinguished in particular by an excellent adsorption performance, low pressure losses and initial breakthroughs. Without wishing to be limited to this theory, the excellent properties of the adsorptive structures according to the invention are due to the fact that even very small amounts of the hydrocolloid are sufficient for producing shaped bodies based on particulate adsorbents, so that, on the one hand, there is a high adsorption performance and, on the other hand, very good accessibility of the adsorption particles. In addition, the structures according to the invention are distinguished by their excellent mechanical stability under mechanical action. In particular, the good stability also makes it possible to achieve variable shaping, such as, for example, the production of honeycomb bodies having pore ducts of up to 10 mm or more. In addition, the structures according to the invention have excellent resistance to chemico-physical influences and good resistance under normal conditions. Due to the resistance to liquids, it is even possible to clean the structures according to the invention in a simple manner with water. Overall, the structures according to the invention have excellent properties, as could not yet be realized.

Claims

Self-supporting three-dimensional adsorptive structure, wherein the adsorptive structure comprises a multiplicity of individual adsorber particles, wherein the individual adsorber particles are joined by means of at least one hydrocolloid to form a self-supporting three-dimensional adsorptive structure and / or wherein the individual adsorber particles are joined by means of at least one hydrocolloid and / or are fixed to one another and / or are brought to adhere to one another, wherein the hydrocolloid is selected from the group of gelatin, collagen, xanthan, dextran, agar, carrageenan, pectin, gum arabic, galactomannan and derivatives and mixtures or combinations thereof, wherein the adsorber particles are configured in the form of grains and have absolute particle diameters in the range from 0.001 to 3 mm, wherein the adsorptive structure comprises the hydrocolloid and the adsorber particles in a mass-related ratio of hydrocolloid to adsorber particles "[hydrocolloid:adsorber particles]" in the range from [1:100] to [1:1], based on the respective dry weight, and wherein the adsorptive structure is porous and / or foam-like and wherein the adsorptive structure comprises a pore system.The adsorptive structure according to claim 1, wherein the hydrocolloid is a macromolecule and / or has a plurality of macromolecules, in particular wherein the macromolecule and / or the hydrocolloid has an average molar mass, in particular a weight-average molar mass, in the range from 5,000 to 500,000 g / mol, in particular in the range from 10,000 to 400,000 g / mol, preferably in the range from 12,500 to 300,000 g / mol, preferably in the range from 15,000 to 250,000 g / mol; and / or wherein the hydrocolloid is gelatin and / or collagen and / or derivatives thereof, in particular gelatin and / or derivatives thereof, in particular wherein the derivatives are made acidic or basic and / or chemically modified.The adsorptive structure according to any of the preceding claims, wherein the adsorber particles have an inner porous structure and / or an inner pore system, and / or wherein the adsorber particles consist of activated carbon and / or wherein the adsorber particles are formed from activated carbon; and / or wherein the adsorber particles are spherical in shape; and / or wherein the adsorber particles have particle sizes (absolute), in particular particle diameters (absolute), in the range from 0.005 to 2.5 mm, preferably in the range from 0.01 to 2 mm, particularly preferably in the range from 0.02 to 1.5 mm, very particularly preferably in the range from 0.05 to 1 mm, and / or wherein the adsorber particles have average particle sizes, in particular average particle diameters (D50), in the range from 0.01 to 2 mm, in particular in the range from 0.05 to 1.5 mm, preferably in the range from 0.1 to 1 mm.The adsorptive structure according to any of the preceding claims, wherein the adsorber particles consist of a material selected from the group of activated carbon; zeolites; inorganic oxides, in particular silicon dioxides, silica gels and aluminum oxides; molecular sieves; mineral granules; clathrates; metal-organic framework materials (MOFs) and mixtures or combinations thereof, particularly preferably activated carbon, and / or wherein the adsorber particles consist of activated carbon and / or wherein the adsorber particles are formed from activated carbon; and / or wherein the adsorber particles are formed from granular, in particular spherical, activated carbon.The adsorptive structure according to any of the preceding claims, wherein the adsorptive structure comprises the hydrocolloid and the adsorber particles, in particular the activated carbon particles, in a mass-related ratio of hydrocolloid to adsorber particles "[hydrocolloid:adsorber particles]" in the range from [1:80] to [1:2], preferably in the range from [1:50] to [1:5], preferably in the range from [1:30] to [1:10], particularly preferably in the range from [1:25] to [1:15], very particularly preferably in the range from [1:22] to [1:18], based on the respective dry weight; and / or wherein the adsorptive structure comprises the adsorber particles, in particular the activated carbon particles, in an amount of at least 70% by weight, in particular of at least 80% by weight, preferably of at least 75% by weight, preferably of at least 90% by weight, particularly preferably of at least 95% by weight, based on the total weight of the self-supporting structure, and / or wherein the adsorptive structure comprises the adsorber particles, in particular the activated carbon particles, in an amount in the range from 70 to 99% by weight, in particular in the range from 80 to 98% by weight, preferably in the range from 85 to 97% by weight, preferably in the range from 90 to 96% by weight, particularly preferably in the range from 92.5 to 95% by weight, based on the total weight of the self-supporting structure.The adsorptive structure according to any of the preceding claims, wherein the adsorptive structure comprises the hydrocolloid in an amount of at most 30% by weight, in particular of at most 20% by weight, preferably of at most 15% by weight, particularly preferably of at most 10% by weight, very particularly preferably of at most 5% by weight, based on the total weight of the adsorptive structure, and / or wherein the adsorptive structure comprises the hydrocolloid in an amount in the range from 0.1 to 30% by weight, in particular in the range from 1 to 20% by weight, preferably in the range from 2 to 15% by weight, particularly preferably in the range from 3 to 10% by weight, very particularly preferably in the range from 4 to 7% by weight, based on the total weight of the adsorptive structure.The adsorptive structure according to any of the preceding claims, wherein the adsorber particles, in particular the activated carbon particles, are permanently and / or irreversibly joined to form the adsorptive structure by means of the hydrocolloid; and / or wherein the adsorber particles, in particular the activated carbon particles, are brought into contact with the hydrocolloid by wetting and / or wherein the adsorber particles and the hydrocolloid form a framework and / or a matrix of the hydrocolloid in their entirety; and / or wherein the surface of the individual adsorber particles, in particular of the activated carbon particles, in the adsorptive structure is covered and / or covered with hydrocolloid to an extent of in each case at most 50%, in particular at most 40%, preferably at most 30%, particularly preferably at most 20%, based on the surface, and / or wherein the surface of the individual adsorber particles, in particular of the activated carbon particles, of the adsorptive structure is covered and / or covered with hydrocolloid in each case in the range from 1 to 50%, in particular in the range from 5 to 40%, preferably in the range from 10 to 30%, based on the surface.The adsorptive structure according to any of the preceding claims, wherein the adsorptive structure has an open-pore and / or open-cell pore system and / or framework or a closed and / or closed-cell pore system and / or framework, preferably an open-pore and / or open-cell pore system and / or framework; in particular wherein the pore system is formed by the at least one hydrocolloid and the adsorber particles, in particular wherein the adsorber particles are preferably connected to one another and / or fixed to one another in a punctiform manner by means of the hydrocolloid and / or wherein the pore system has air-filled cavities and / or pores bounded by the adsorber particles and the hydrocolloid; and / or in particular wherein the ratio of the average pore size of the pore system of the adsorptive structure to the average particle size of the adsorber particles [average pore size of the pore system: average particle size of the adsorber particles] is in the range from 0.01:1 to 10,000:1, in particular 0.2:1 to 1,000:1, preferably 0.5:1 to 500:1, preferably 1:1 to 250:1, particularly preferably 1.2:1 to 200:1, very particularly preferably 1.5:1 to 100:1, and / or wherein the ratio of the average pore size of the pore system of the adsorptive structure to the average particle size of the adsorber particles [average pore size of the pore system: average particle size of the adsorber particles] is at least 0.1:1, in particular at least 0.5:1, preferably at least 1:1, preferably at least 1.2:1, particularly preferably at least 1.5:1, very particularly preferably at least 2:1, even more preferably at least 3:1.The adsorptive structure according to any of the preceding claims, wherein the adsorptive structure has a porosity (porosity) of 2 to 100 ppi, in particular 5 to 90 ppi, preferably 10 to 80 ppi, preferably 15 to 75 ppi, and / or wherein the adsorptive structure has pores having an average pore diameter in the range of 0.001 to 10 mm, in particular 0.01 to 8 mm, preferably 0.05 to 5 mm, preferably 0.1 to 3 mm.The adsorptive structure according to any of the preceding claims, wherein the adsorptive structure is formed monolithically and / or integrally; and / or wherein the adsorptive structure is formed cylindrically, rod-shaped, plate-shaped, cuboidal, polyhedral, honeycomb-shaped or the like.The adsorptive structure according to any of claims 1 to 9, wherein the adsorptive structure is present as an agglomerate, in particular wherein a single agglomerate comprises in each case at least 5 adsorber particles, in particular at least 10 adsorber particles, preferably at least 15 adsorber particles, preferably at least 20 adsorber particles, and / or wherein a single agglomerate comprises in each case up to 50 adsorber particles, in particular up to 75 adsorber particles, preferably up to 100 adsorber particles or more.The adsorptive structure according to any of the preceding claims, wherein the adsorptive structure has a temperature resistance of at least 100°C, in particular at least 130°C, preferably at least 180°C, particularly preferably at least 200°C, and / or wherein the adsorptive structure is at least substantially insoluble in organic, in particular aprotic solvents, in particular acetone.A method for producing a self-supporting three-dimensional adsorptive structure, in particular as defined in any of the preceding claims, wherein the method comprises the following steps in the sequence (a) to (c) specified below: (a) production of a solution and / or dispersion of at least one hydrocolloid selected from the group of gelatin, collagen, xanthan, dextran, agar, carrageenan, pectin, gum arabic, galactomannan and derivatives and mixtures or combinations thereof; (b) contacting the solution and / or dispersion produced in step (a) with a plurality of individual granular adsorber particles having absolute particle diameters in the range from 0.001 to 3 mm to obtain a suspension of the adsorber particles in the solution and / or dispersion of the hydrocolloid, wherein the adsorber particles are used in a mass-related ratio of hydrocolloid to adsorber particles "[hydrocolloid:adsorber particles]" in the range from [1:100] to [1:1], based on the respective dry weight, and wherein a volume expansion and / or formation of a foam and / or a porous structure in the suspension takes place by releasing gases from the adsorber particles and / or by introducing gases, wherein the volume expansion and / or formation of a foam and / or a porous structure is controlled by introduction of shear forces and setting the suspension to temperatures in the range from 50 to 150° C.; (c) removal of the solution and / or dispersion medium from the suspension and curing to obtain the self-supporting three-dimensional adsorptive structure.The method according to claim 13, wherein, in order to provide the solution and / or dispersion of a hydrocolloid and / or in method step (a), the solvent for obtaining the solution and / or dispersion of the at least one hydrocolloid is selected from the group of aqueous and organic solvents and mixtures or combinations thereof, in particular from the group of water, ethylene glycol, glycerol, formamide and acetic acid and mixtures or combinations thereof, preferably water; and / or wherein, in order to provide the solution and / or dispersion of a hydrocolloid and / or in process step (a), the at least one hydrocolloid is used in an amount in the range from 0.1 to 30% by weight, in particular in the range from 0.5 to 15% by weight, preferably in the range from 1 to 10% by weight, preferably in the range from 2 to 8% by weight, based on the solvent and / or the dispersion.The method according to claim 13 or 14, wherein the provision of the solution and / or dispersion of a hydrocolloid and / or method step (a) is carried out with heating to temperatures in the range from 40 to 120°C, in particular in the range from 50 to 110°C, preferably in the range from 60 to 100°C, preferably in the range from 70 to 90°C, and / or wherein the method is carried out with application of shear forces, in particular with stirring, in order to provide the solution and / or dispersion of a hydrocolloid and / or in method step (a); and / or wherein, in the provision of the suspension of a multiplicity of individual adsorber particles in the solution and / or dispersion of the hydrocolloid and / or in process step (b), the adsorber particles are used in a mass-related ratio of hydrocolloid to adsorber particles "[hydrocolloid:adsorber particles]" in the range from [1:80] to [1:2], preferably in the range from [1:50] to [1:5], preferably in the range from [1:30] to [1:10], particularly preferably in the range from [1:25] to [1:15], very particularly preferably in the range from [1:22] to [1:18], based on the respective dry weight.The method according to any of claims 13 to 15, wherein, in the provision of the suspension of a plurality of individual adsorber particles in the solution and / or dispersion of the hydrocolloid and / or in method step (b), the proportion of the solvent in the suspension is adjusted to a range from 20 to 90% by weight, in particular to a range from 25 to 80% by weight, preferably to a range from 30 to 70% by weight, preferably to a range from 35 to 60% by weight, based on the suspension, by contacting the provided solution and / or dispersion of the at least one hydrocolloid and / or the solution and / or dispersion prepared in step (a) with the plurality of individual adsorber particles to obtain the suspension of adsorber particles.The method according to any of claims 13 to 16, wherein, when providing the suspension of a plurality of individual adsorber particles in the solution and / or dispersion of the hydrocolloid and / or in method step (b), the volume expansion and / or the formation of a porous structure is controlled by introduction of shear forces, in particular with stirring, and / or setting the suspension to temperatures in the range from 60 to 140°C, preferably in the range from 70 to 130°C, preferably in the range from 80 to 120°C, particularly preferably in the range from 90 to 110°C, in particular wherein, when providing the suspension of a plurality of individual adsorber particles in the solution and / or dispersion of the hydrocolloid and / or in method step (b), introduction of shear forces, in particular stirring, is controlled, the suspension is carried out over a period in the range from 5 to 180 s, in particular in the range from 10 to 150 s, preferably in the range from 15 to 120 s, preferably in the range from 20 to 100 s.The method according to any of claims 13 to 17, wherein, during the removal of the solution and / or dispersion medium and / or in process step (c), the removal of the solution and / or dispersion medium from the suspension and curing takes place with formation of a porous and / or foam-like structure; and / or wherein the removal of the solution and / or dispersion medium and / or process step (c) is carried out with heating and / or adjustment of the suspension to temperatures in the range from 70 to 200°C, in particular in the range from 90 to 180°C, preferably in the range from 100 to 160°C, particularly preferably in the range from 110 to 150°C; and / or wherein the removal of the solution and / or dispersion medium and / or process step (c) is carried out with heating and / or adjustment of the suspension to temperatures of at least 70° C., in particular at least 90° C., preferably at least 110° C., particularly preferably at least 130° C.; and / or wherein the removal of the solution and / or dispersion medium and / or process step (c) is carried out with optionally further volume expansion and / or with optionally further formation of a foam and / or a porous structure, in particular by introduction of gases, in the suspension; and / or wherein the removal of the solution and / or dispersion medium and / or process step (c) is carried out with shaping and / or formation of the self-supporting three-dimensional adsorptive structure; and / or wherein the removal of the solution and / or dispersion medium and / or process step (c) is carried out, in particular for curing the suspension, over a period in the range from 2 to 22 hours, in particular in the range from 4 to 20 hours, preferably in the range from 8 to 18 hours, preferably in the range from 10 to 14 hours.A self-supporting structure having adsorptive properties obtainable by a process according to claims 13 to 18.Use of at least one hydrocolloid for connecting and / or fixing and / or adhering individual adsorber particles to one another to obtain a self-supporting three-dimensional adsorptive structure as defined in any of claims 1 to 12, and / or use of at least one hydrocolloid for connecting and / or fixing individual adsorber particles to one another and / or adhering to one another to obtain a self-supporting three-dimensional adsorptive structure as defined in any of claims 1 to 12.Use of a self-supporting three-dimensional adsorptive structure as defined in any of claims 1 to 12 for the adsorption of toxicants, pollutants and odors, in particular from gas or air streams or else from liquids, in particular water, and / or for the purification or treatment of gases, gas streams or gas mixtures, in particular air, or of liquids, in particular water.Use of a self-supporting three-dimensional adsorptive structure as defined in any of Claims 1 to 12 in adsorption filters and / or for the production of filters, in particular adsorption filters, and / or as substrate and / or support (material), in particular for catalysts and / or catalytic systems and / or reactive compounds.A filter comprising a self-supporting three-dimensional adsorptive structure as defined in any one of claims 1 to 12.

Citation Information

Patent Citations

  • Adsorptive molded bodies, methods for their manufacture and their use

    DE102008058248A1

  • Mechanically stable, porous shaped activated carbon article comprises first three-dimensional framework structure based on carbonized resin, and second three-dimensional inorganic framework structure

    DE20221547U1

  • activated carbon filter layer for gas masks

    DE3813564A1

  • Self-supporting porous bodies with adsorbent properties - contain spherical adsorber particles, e.g. active carbon, linked with bridges, e.g. of clay, carbon etc, with voids between particles

    DE4238142A1

  • High-performance filter with high thermal and chemical stability - has adsorber particles bonded to a three-dimensional porous support coated with a thermally stable, hydrolysis-resistant plastic

    DE4239520A1