Method for producing a rubber composition, method for producing a vulcanizable rubber composition, and method for producing a vulcanized rubber composition
Patent Information
- Application Number
- DE102012010317
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2012-05-24
- Publication Date
- 2024-10-17
- Estimated Expiration
- 2032-05-24
Abstract
Description
[Technical Field]The present invention relates to a method for producing a rubber composition, a method for producing a vulcanizable rubber composition, and a method for producing a vulcanized rubber composition.[Background of Technique]In recent years, because of the increasing interest in environmental problems, demand for automobiles for fuel saving has increased, and rubber compositions to be used for tires are also required to be superior in fuel saving efficiency. As rubber compositions for treads of tires, rubber compositions have been used in which reinforcing agents such as silica are blended into diene-based rubbers such as polybutadiene and styrene-butadiene copolymers.Further, when silica as a reinforcing agent is mixed into a diene-based rubber, a silane coupling agent is mixed to improve affinity of the diene-based rubber and the silica, thereby improving dispersibility of the silica. As a method for producing a rubber composition comprising a diene-based rubber, a silica reinforcing agent and a silane coupling agent, there has been proposed a method for producing a rubber composition as disclosed in Patent Document 1, in which a diene-based rubber and a silica reinforcing agent are kneaded to produce a pre-kneaded composition, and then the pre-kneaded composition and a silane coupling agent are kneaded.Patent Document 2 relates to a method for producing a radial conjugated diene polymer, comprising polymerizing a monomer mixture containing at least one conjugated diene compound using an alkali metal-reacted aromatic compound having three or more carbon atoms directly bonded to alkali metal atoms and aromatic rings in one molecule as a polymerization initiator.Patent Document 3 relates to a specific method for producing a rubber composition containing 20 to 100 parts by weight of an inorganic filler such as silica per 100 parts by weight of a diene rubber, comprising a first step in which the diene rubber, a part of the inorganic filler and a silane coupling agent expressed by a specific formula are mixed, a second step in which the remainder of the inorganic filler is added to and mixed with the mixture obtained above, and a third step in which a vulcanization additive is added to and mixed with the mixture.Patent Document 4 relates to a rubber composition prepared by mixing 100 parts by weight of a diene rubber component mainly comprising a natural or polyisoprene rubber and a polybutadiene rubber with 30-100 parts by weight of silica, provided that at least 50 wt % of the silica and 1-10 parts by weight of a specific silane coupling agent are mixed into the natural or polyisoprene rubber in advance.[Prior Art Documents][Patent Documents][Patent Document 1] JP 2002-201 309 A[Patent Document 2] EP 2 431 395 A1 or US 2012 / 0 071 603 A1 or WO 2010 / 131646 A1[Patent Document 3] JP 2005-263 999 A[Patent Document 4] JP H06-248 117 A[Summary of the Invention][Objects to be Achieved by the Invention]A vulcanized rubber composition obtained by vulcanizing the rubber composition produced by the above-mentioned method is used as a tread of a tire. However, the vulcanized rubber composition was not satisfactory enough in the fuel saving efficiency or grip property when used as a tread of a tire.Under such circumstances, the object to be achieved by the present invention is to provide a method for producing a rubber composition suitable as a raw material for a vulcanized rubber composition, from which a tire superior in fuel saving efficiency and grip property is obtained when the vulcanized rubber composition is used for the tread of the tire, and a method for producing a vulcanized rubber composition using the rubber composition.[Means for Achieving Objects]The present invention relates to a method for producing a rubber composition, the method comprising a step of producing a pre-kneaded rubber composition by kneading, at a temperature of 50° C. or higher and 130° C. or less, butadiene-based rubber, 1 to 20 parts by weight of a silane coupling agent per 100 parts by weight of the butadiene-based rubber and 5 parts by weight or less of silicon oxide per 100 parts by weight of the butadiene-based rubber, and a step of kneading the pre-kneaded rubber composition and 30 to 200 parts by weight of a silicon oxide per 100 parts by weight of the butadiene-based rubber used for producing the pre-kneaded rubber composition.Further, the present invention relates to a method for producing a vulcanizable rubber composition, the method comprising a step of kneading a vulcanizing agent and a rubber composition produced by the above-described method.Further, the present invention relates to a method for producing a vulcanized rubber composition, the method comprising a step of heating a vulcanizable rubber composition produced by the above-described method.[Advantageous Effects of the Invention]According to the present invention, a rubber composition suitable as a vulcanized rubber composition from which a tire superior in fuel saving efficiency and grip property can be obtained when used for the tread of the tire, and a vulcanized rubber composition from which a tire superior in fuel saving efficiency and grip property can be obtained.[Mode for Carrying Out the Invention]< Based on butadiene>The butadiene-based rubber in the present invention is a rubber composed of a polymer containing butadiene as monomer units. Examples of such a butadiene-based rubber include a styrene-butadiene copolymer rubber (SBR), a polybutadiene rubber (BR), a butadiene-isoprene copolymer rubber, an acrylonitrile-butadiene rubber (NBR), and a styrene-isoprene-butadiene terpolymer rubber. The butadiene-based rubber to be used in the present invention is preferably a styrene-butadiene copolymer rubber or a polybutadiene rubber. Two or more butadiene-based rubbers may be used.The butadiene-based rubber may have been modified with a modifier such as a ketone or an amide at its polymer chain ends.The Mooney viscosity (ML 1+4) of the butadiene-based rubber measured at 100° C. is preferably 10 or more, more preferably 20 or more. In order to improve the processability, it is preferably 200 or less, more preferably 150 or less. Mooney viscosity (ML 1+4) is measured according to JIS K6300 (1994).<Silane Coupling Agent>Examples of the silane coupling agent in the present invention include alkoxysilane compounds having a sulfur-containing group, alkoxysilane compounds having an amino group, alkoxysilane compounds having an epoxy group, alkoxysilane compounds having a vinyl group, alkoxysilane compounds having an acrylic group, alkoxysilane compounds having a methacrylic group, alkoxysilane compounds having a styryl group, alkoxysilane compounds having a ureido group, alkoxysilane compounds having an isocyanate group, and alkoxysilane compounds having a halogen atom; alkoxysilane compounds having a sulfur-containing group are preferred.Examples of the sulfur-containing group include a mercapto group, a thioester group, a thiocyanate group, and a polysulfide group; a polysulfide group is preferred.Examples of alkoxysilane compounds having a mercapto group include 3-mercaptopropyltrimethoxysilane, 3-mercaptopropyltriethoxysilane, and 3-mercaptopropylmethyldimethoxysilane. Examples of alkoxysilane compounds having a thioester group include 3-octanoylthio-1-propyltriethoxysilane. Examples of alkoxysilane compounds having a thiocyanate group include 3-thiocyanateopropyltriethoxysilane.Examples of alkoxysilane compounds having a polysulfide group include compounds represented by formula (2): wherein R 21, R 22 and R 23 each represent an alkyl group or an alkoxy group, at least one group selected from R 21, R 22 and R 23, is an alkoxy group, A represents a group selected from the group consisting of dialkyl thiocarbamyl groups, a thiazolyl group, a benzothiazolyl group, and alkoxysilylalkyl groups, i represents an integer of 1 to 5, and j represents an integer of 2 to 8.In formula (2), R 21, R 22 and R 23 each represent an alkyl group or an alkoxy group, and is at least one group selected from R 21, R 22 and R 23, an alkoxy group. Preferably, at least two groups selected from R 21, R 22 and R 23, are alkoxy groups. More preferably, R 21, R 22 and R 23 are alkoxy groups.R 21, R 22 and R 23 are each an alkyl group or alkoxy group preferably having 1 to 8, more preferably 1 to 6, even more preferably 1 to 4, and particularly preferably 1 to 2 carbon atoms.Examples of the alkyl group of R 21, R 22 and R 23 include a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, an isobutyl group, a sec-butyl group, a tert-butyl group, an n-pentyl group, an n-hexyl group and an n-octyl group. A methyl group and an ethyl group are preferred.Examples of the alkoxy group of R 21, R 22 and R 23 include a methoxy group, an ethoxy group, an n-propoxy group and an n-butoxy group. A methoxy group and an ethoxy group are preferred.Preferably, R 21, R 22 and R 23 are groups each selected from the group consisting of a methoxy group, an ethoxy group, a methyl group and an ethyl group, and are at least two groups selected from R 21, R 22 and R 23, each a methoxy group or an ethoxy group. More preferably, R 21, R 22 and R 23 are each a methoxy group or an ethoxy group.In formula (2), i represents an integer of 1 to 5, preferably 2 or 3.In formula (2), j represents an integer of 2 to 8, preferably an integer of 2 to 5.In formula (2), A represents a group selected from the group consisting of dialkyl thiocarbamyl groups, a thiazolyl group, a benzothiazolyl group, and alkoxysilylalkyl groups.Examples of the dialkyl thiocarbamyl groups include a dimethyl thiocarbamyl group and a diethyl thiocarbamyl group.Examples of the alkoxysilylalkyl groups include groups represented by formula (2-S): wherein R 24, R 25 and R 26 each represent an alkyl group or an alkoxy group, at least one group selected from R 24, R 25 and R 26, is an alkoxy group, and k represents an integer of 1 to 5.In formula (2-S), R 24, R 25 and R 26 each represent an alkyl group or an alkoxy group, and is at least one group selected from R 24, R 25 and R 26, an alkoxy group. Preferably, at least two groups selected from R 24, R 25 and R 26, are alkoxy groups. More preferably, R 24, R 25 and R 26 are alkoxy groups.R 24, R 25 and R 21 are each an alkyl group or alkoxy group preferably having 1 to 8, more preferably 1 to 6, even more preferably 1 to 4, and particularly preferably 1 to 2 carbon atoms.Examples of the alkyl group of R 24, R 25 and R 26 include a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, an isobutyl group, a sec-butyl group, a tert-butyl group, an n-pentyl group, an n-hexyl group and an n-octyl group. A methyl group and an ethyl group are preferred.Examples of the alkoxy group of R 24, R 25 and R 26 include a methoxy group, an ethoxy group, an n-propoxy group and an n-butoxy group. A methoxy group and an ethoxy group are preferred.Preferably, R 24, R 25 and R 26 are groups each selected from the group consisting of a methoxy group, an ethoxy group, a methyl group and an ethyl group, and are at least two groups selected from R 24, R 25 and R 26, each a methoxy group or an ethoxy group. More preferably, R 24, R 25 and R 26 are each a methoxy group or an ethoxy group.In formula (2-S), k represents an integer of 1 to 5, preferably 2 or 3.Examples of groups represented by formula (2-S) include a 2-trimethoxysilylethyl group, a 3-trimethoxysilylpropyl group, a 3-triethoxysilylpropyl group, and a 3-dimethoxymethylsilylpropyl group.Among the compounds represented by formula (2), examples of compounds in which A is a dialkylthiocarbamyl residue include γ-trimethoxysilylpropyldimethylthiocarbamyl tetrasulfide. Examples of compounds in which A is a thiazolyl group include γ-trimethoxysilylpropylthiazolyl tetrasulfide. Examples of compounds in which A is benzothiazolyl include γ-trimethoxysilylpropyl benzothiazolyl tetrasulfide.Among the compounds represented by formula (2), examples of compounds in which A is a group represented by formula (2-S) include compounds represented by formula (2-1): wherein R 21, R 22 and R 23 each represent an alkyl group or an alkoxy group, at least one group selected from R 21, R 22 and R 23, is an alkoxy group, R 24, R 25 and R 26 each represent an alkyl group or an alkoxy group, at least one group, selected from R 24, R 25 and R 26, is an alkoxy radical, i is an integer from 1 to 5, j is an integer from 2 to 8 and k is an integer from 1 to 5.Examples of the compounds represented by formula (2-1) include bis(3-triethoxysilylpropyl) disulfide, bis(3-triethoxysilylpropyl) tetrasulfide, and bis(3-dimethoxymethylpropyl) tetrasulfide.Commercial products of the compounds represented by formula (2-1) include those having trade names of Si69 and Si75 produced by Degussa Co., Ltd.Alkoxysilane compounds containing a polysulfide group are preferably compounds represented by formula (2-1), and more preferably compounds wherein R 21, R 22, R 23, R 24, R 25 and R 26 are groups each selected from the group consisting of a methoxy group, an ethoxy group, a methyl group and an ethyl group, at least two groups selected from R 21, R 22 and R 23, are each a methoxy group or an ethoxy group, at least two groups selected from R 24, R 25 and R 26, are each a methoxy group or an ethoxy group, i is an integer of 1 to 5, j is an integer of 2 to 8, and k is an integer of 1 to 5. More preferred are compounds represented by formula (2-1), wherein R is 21, R is 22, R is 23, R is 24, R is 25 and R is 26 each is a methoxy group or an ethoxy group, i is 2 or 3, j is an integer of 2 to 5, and k is 2 or 3.Bis(3-triethoxysilylpropyl) disulfide and bis(3-triethoxysilylpropyl) tetrasulfide are particularly preferred as alkoxysilane compounds containing a polysulfide group.In the present invention, one or more kinds of silane coupling agents are used.<>Examples of the silica in the present invention include dry process silica (silicic anhydride), wet process silica (hydrous silicic acid), colloidal silica, precipitated silica, calcium silicate and aluminum silicate. One or more kinds of silica are used. The BET specific surface area of the silica is preferably 50 to 250 m 2 / g. The BET specific surface area is measured according to ASTM D1993-03. As a commercially available product, for example, a product available under the trade name of ULTRASIL® VN3-G manufactured by Degussa Co., Ltd., products available under the trade names of VN3, AQ, ER, and RS-150 manufactured by Tosoh Silica Corporation, and products available under the trade names of Zeosil® 1115 MP, and Zeosil® 1165 MP manufactured by Rhodia are used.< For Producing Pre-Kneaded Rubber Composition>The pre-kneaded rubber composition in the present invention is a rubber composition prepared by kneading, at a temperature of 50° C. or higher and 130° C. or less, a butadiene-based rubber, 1 part by weight to 20 parts by weight of a silane coupling agent per 100 parts by weight of the butadiene-based rubber, and 5 parts by weight or less of silicon oxide per 100 parts by weight of the butadiene-based rubber. The amount of the silane coupling agent to be kneaded into the butadiene-based rubber is 1 part by weight to 20 parts by weight, preferably 3 parts by weight to 10 parts by weight, per 100 parts by weight of the butadiene-based rubber.The butadiene-based rubber and the silane coupling agent are preferably kneaded by a kneader. Examples of the kneading machine include a Banbury mixer, a Labo Plastomill, a kneader, a roll kneader, and a twin-screw extruder. The temperature at which the butadiene-based rubber and the silane coupling agent are kneaded is 130° C. or less. The temperature at which the butadiene-based rubber and the silane coupling agent are kneaded is 50° C. or higher, and preferably 90° C. or higher. Preferably, the time for which the butadiene-based rubber and the silane coupling agent are kneaded is 1 minute or more and 20 minutes or less.Polymers other than the butadiene-based rubber may be kneaded with the butadiene-based rubber and the silane coupling agent. Examples of such polymers include isoprene rubbers such as natural rubber, polyisoprene rubber (IR), and styrene-isoprene copolymer rubber; chloroprene rubber (CR); ethylene-propylene-diene rubber (EPDM); and ethylene-α-olefin copolymers such as ethylene-propylene copolymers and ethylene-octene copolymers. When such a polymer is kneaded, the amount of the polymer to be kneaded per 100 parts by weight of the butadiene-based rubber is preferably 20 parts by weight or less, more preferably 10 parts by weight or less, even more preferably 5 parts by weight or less, and particularly preferably 2 parts by weight or less.In the step of preparing the pre-kneaded rubber composition, additives such as carbon black, a filler other than silica, an anti-aging agent, zinc oxide, stearic acid, an extender oil, a processing aid, and a lubricant may be kneaded with the butadiene-based rubber and the silane coupling agent. In the step of preparing the pre-kneaded rubber composition, not more than 5 parts by weight of silicon oxide per 100 parts by weight of the butadiene-based rubber is used.Examples of such carbon black include channel carbon black such as EPC, MPC and CC; furnace carbon black such as SAF, ISAF, HAF, MAF, FEF, SRF, GPF, APF, FF, CF, SCF and ECF; thermal carbon black such as FT and MT; acetylene carbon black; and graphite. Two or more kinds of carbon black may be used.The nitrogen adsorption specific surface area (N 2 SA) of carbon black is preferably 5 to 200 m 2 / g, and the dibutyl phthalate (DBP) absorption of carbon black is preferably 5 to 300 ml / 100 g. The nitrogen adsorption specific surface area is measured according to ASTM D4820-93. DBP absorption is measured according to ASTM D2414-93. As a commercially available product, for example, a product available under the trade name of DIABLACK N339 manufactured by Mitsubishi Chemical Corporation, products available under the trade names of SEAST 6, SEAST 7HM, and SEAST KH manufactured by Tokai Carbon Co., Ltd., and products available under the trade names of CK3 and Special Black 4A manufactured by Degussa Co., Ltd. can be used.Examples of such a filler include calcium carbonate, talc, alumina, clay, aluminum hydroxide and mica.Examples of such extender oil include aromatic mineral oils (viscosity-severity constant (V.G.C.): 0.900 to 1.049), naphthene-based mineral oils (V.G.C.: 0.850 to 0.899), and paraffin-based mineral oils (V.G.C.: 0.790 to 0.849). The content of a polycyclic aromatic compound in the extender oil is preferably less than 3 wt %, more preferably less than 1 wt %. The content of the polycyclic aromatic compound is measured according to the method IP 346 / 92 of The Institute of Petroleum. The content of aromatic compounds (CA) of the extender oil is preferably 20 wt % or more. Two or more kinds of extender oils can be used.In the step of preparing the pre-kneaded rubber composition, although it is preferable not to knead silica together with the butadiene-based rubber and the silane coupling agent, silica may be kneaded if the amount thereof is small, i.e., 5 parts by weight or less per 100 parts by weight of the butadiene-based rubber. In order to produce a vulcanized rubber composition superior in fuel saving efficiency and grip property, the amount of silica that can be kneaded in this step is 5 parts by weight or less, and preferably 2 parts by weight or less, per 100 parts by weight of the butadiene-based rubber.When silica is kneaded in the step of preparing the pre-kneaded rubber composition, the pre-kneaded rubber composition may be prepared by simultaneously kneading silica, the silane coupling agent, and the butadiene-based rubber together, or alternatively, the pre-kneaded rubber composition may be prepared by first kneading silica and the butadiene-based rubber to prepare a kneaded material, and then kneading the silane coupling agent into the resultant kneaded material.<Step of Kneading Silicon Oxide and Pre-Kneaded Rubber Composition>The method for producing the rubber composition of the present invention includes a step of kneading pre-kneaded rubber composition produced in the above-described step and 30 parts by weight to 200 parts by weight of a silicon oxide per 100 parts by weight of the butadiene-based rubber used for producing the pre-kneaded rubber composition.The silica and the pre-kneaded rubber composition are preferably kneaded with a kneader. Examples of the kneading machine include a Banbury mixer, a Labo Plastomill, a kneader, a roll kneader, and a twin-screw extruder. The temperature at which the silica and the pre-kneaded rubber composition are kneaded is preferably 160° C. or less, more preferably 130° C. or less, and preferably 30° C. or higher, more preferably 50° C. or higher, and even more preferably 90° C. or higher. The time for kneading the silica and the pre-kneaded rubber composition is preferably 30 seconds to 20 minutes, more preferably one minute or longer.The amount of the silica to be kneaded in the step of kneading the silica and the pre-kneaded rubber composition is 30 parts by weight to 200 parts by weight, preferably 50 parts by weight to 150 parts by weight, more preferably 70 parts by weight to 120 parts by weight, per 100 parts by weight of the butadiene-based rubber used for producing the pre-kneaded rubber composition to be used in this step.In the step of kneading the silica and the pre-kneaded rubber composition, it is also allowed to knead a butadiene-based rubber, a polymer other than the butadiene-based rubber, and the above-mentioned additive with the silica and the pre-kneaded rubber composition. Moreover, it is also permissible to provide, after the step of kneading the silica and the pre-kneaded rubber composition, a step of kneading the rubber composition prepared by the foregoing step, a butadiene-based rubber, a polymer other than the butadiene-based rubber, and the above-mentioned additive.The total amount of the butadiene-based rubber and the polymer(s) other than the butadiene-based rubber to be kneaded in the silica-based kneading step and the pre-kneaded rubber composition and the step after this step is preferably 20 parts by weight or less, more preferably 10 parts by weight or less, and even more preferably 5 parts by weight or less, per 100 parts by weight of the butadiene-based rubber used for preparing the pre-kneaded rubber composition.<Step of Production of Vulcanizable Rubber Composition>The rubber composition prepared by the above-described method and a vulcanizing agent are kneaded, thereby preparing a vulcanizable rubber composition.Examples of such a vulcanizing agent include sulfur, powdery sulfur, precipitated sulfur, colloidal sulfur, insoluble sulfur and highly dispersible sulfur. The amount of the vulcanizing agent to be kneaded is preferably 0.1 part by weight to 15 parts by weight, more preferably 0.3 part by weight to 10 parts by weight, and even more preferably 0.5 part by weight to 5 parts by weight, per 100 parts by weight of the polymer components used for preparing the rubber composition to be used for kneading. The polymer component as used herein means a butadiene-based rubber or collectively means a butadiene-based rubber and a polymer other than the butadiene-based rubber when the polymer is used.In the step of preparing the vulcanizable rubber composition, a vulcanization accelerator may be kneaded with the rubber composition and the vulcanizing agent.Examples of such a vulcanization accelerator include thiazole-based vulcanization accelerators such as 2-mercaptobenzothiazole, dibenzothiazyl disulfide and N-cyclohexyl-2-benzothiazyl sulfenamide; thiuram-based vulcanization accelerators such as tetramethylthiuram monosulfide and tetramethylthiuram disulfide; sulfenamide-based vulcanization accelerators such as N-cyclohexyl-2-benzothiazole sulfenamide, N-tert-butyl-2-benzothiazole sulfenamide, N-oxyethylene-2-benzothiazole sulfenamide, N-oxyethylene-2-benzothiazole sulfenamide and N,N'-diisopropyl-2-benzothiazole sulfenamide; guanidine-based vulcanization accelerators such as diphenylguanidine, diorthotolyl guanidine and orthotolyl biguanidine.The method of kneading the rubber composition and the vulcanizing agent may be a method of kneading the rubber composition and the vulcanizing agent using a kneading machine such as a Banbury mixer, a Labo Plastomill, and a roll kneader. The kneading temperature is preferably 10° C. to 100° C., more preferably 20° C. to 80° C. The kneading time is preferably 30 seconds to 30 minutes, more preferably 1 minute to 20 minutes.<Step of Production of Vulcanized Rubber Composition>A vulcanized rubber composition is prepared by heating the vulcanizable rubber composition prepared by the above-described method.The method of heating the vulcanizable rubber composition may preferably be press vulcanization. In general press vulcanization, a pair of dies are used and the dies are heated to X ° C ± 0.5 ° C, where X ° C is a vulcanization temperature, usually for 20 minutes or longer. The vulcanizable rubber composition is placed between the heated dies, and then the dies are closed, thereby pressing the vulcanizable rubber. At the beginning of vulcanization, a process of applying and removing pressure by closing and opening the dies is repeated twice or three times to remove bubbles in the vulcanizable rubber. The vulcanization time is a time from the moment when the pressure applied to the vulcanizable rubber has reached a specified pressure to the moment when the pressure is removed after the end of vulcanization. After the completion of vulcanization, the dies are opened and then a sheet made of the vulcanized rubber composition is immediately removed. The removed plate is cooled or cooled in water by being left to rest on a metal plate for 10 to 15 minutes. The temperature to which the vulcanizable rubber is heated is preferably 120 to 200° C., more preferably 140 to 180° C. The pressure under which the vulcanizable rubber is compressed is usually 3.5 MPa or higher, preferably 4 MPa or higher. The vulcanization time of the vulcanizable rubber is preferably from 10 minutes to 2 hours, more preferably from 30 minutes to 1 hour.When a polymer other than the butadiene-based rubber is used in the method for producing the vulcanized rubber composition of the present invention, the amount of the polymer other than the butadiene-based rubber to be used in all the steps is preferably 500 parts by weight or less, more preferably 300 parts by weight or less, per 100 parts by weight of the butadiene-based rubber to be used in all the steps.The vulcanized rubber composition produced by the process of the present invention is superior in fuel saving efficiency. It is also superior in hand property.Vulcanized rubber compositions produced by the process of the present invention are used for tires, shoe soles, floor covering materials, vibration insulating materials and so on, and in particular, they are suitably used for tires.[Examples]Evaluation of physical properties was carried out by the following methods.1. Mooney viscosity (ML1+)According to JIS K6300 (1994), the Mooney viscosity of a polymer was measured at 100° C.2. Content of repeating units derived from styrene (unit: % by weight)According to JIS K6383 (1995), the content of repeating units derived from styrene in a polymer was calculated from a refractive index thereof.3. Efficiency in saving fuelA strip-like sample body 4 mm wide, 40 mm long, 1.2 mm thick was punched out from a plate made of a vulcanized rubber composition, and then it was subjected to a test. The loss factor (tan δ (70° C.)) of the sample body at a temperature of 70° C. was measured under the condition represented by an elongation of 1% and a frequency of 10 Hz using a viscoelasticity analyzer (manufactured by Ueshima Seisakusho Co., Ltd.). The smaller this value, the better the fuel saving efficiency.4. GriffigkeitseigenschaftA strip-like sample body 4 mm wide, 40 mm long, 1.2 mm thick was punched out from a plate made of a vulcanized rubber composition, and then it was subjected to a test. The loss factor (tan δ (0° C.)) of the sample body at a temperature of 0° C. was measured under the condition represented by an elongation of 2.5% and a frequency of 10 Hz using a viscoelasticity analyzer (manufactured by Ueshima Seisakusho Co., Ltd.). The larger this value, the better the grip property.The butadiene-based, silicon oxide-based, silane coupling agents and other additives used in the Examples and Comparative Examples are as follows.(a) Butadiene-based rubberSBR-A: styrene-butadiene copolymer manufactured by Sumitomo Chemical Co., Ltd., Mooney viscosity: (ML 1+4(100 ° C.)) 75, styrene-derived repeating unit content: 25 wt %.SBR-B: Styrene-butadiene copolymer with its polymer chain ends modified with an amide compound manufactured by Sumitomo Chemical Co., Ltd., Mooney viscosity: (ML 1+4(100 ° C.)) 70, content of repeating units derived from styrene: 22% by weight.(b) Silicon oxideTrade name: ULTRASIL® VN3-G, manufactured by Degussa Co., Ltd.(c) Silane coupling agentBis(3-triethoxysilylpropyl)tetrasulfide (trade name: Si69® manufactured by Degussa Co., Ltd.).(d) Carbon BlackTrade name: DIABLACK N339 manufactured by Mitsubishi Chemical Corporation(e) Extender OilTrade name: JOMO PROCESS NC-140 manufactured by Japan Energy Corporation(f) AntioxidantTrade name: ANTIGENS 3C manufactured by Sumitomo Chemical Co., Ltd.(g) stearic acidTrade name: STEARIC ACID 50S, manufactured by New Japan Chemical Co., Ltd.(h) Zinc oxideTrade name: ZINC OXIDE manufactured by Seido Chemical Industry Co., Ltd(i) WaxTrade name: SUNNOC N, manufactured by Ouchi Shinko Chemical Industrial Co., Ltd.(j) Vulcanization AcceleratorTrade name: SOXINOL® CZ manufactured by Sumitomo Chemical Co., Ltd., trade name: SOXINOL® D manufactured by Sumitomo Chemical Co., Ltd.(k) sulfurTrade name: SULFUR POWDER manufactured by Tsurumi Chemical Industry Co., Ltd.Example 1One hundred parts by weight of SBR-A and 6.4 parts by weight of a silane coupling agent were kneaded for five minutes with a 10-inch roll set at 105°C to obtain a kneaded material. Then, the kneaded material was charged into a Labo Plastomill set at 70° C., and kneading was started. The temperature of the kneaded material reached 90° C. in 50 seconds from the start of kneading, kneading was thereafter continued, and when the temperature of the kneaded material reached 120° C. at the time of 2 minutes and 30 seconds from the start of kneading, kneading was stopped, and then the kneaded material was cooled to room temperature, so that a pre-kneaded rubber composition was produced.The pre-kneaded rubber composition was filled in a Labo Plastomill set at 70° C., and kneading was started. Where the amount of the SBR-A used for preparing the pre-kneaded rubber composition is 100 parts by weight, 78.4 parts by weight of a silica, 6.4 parts by weight of carbon black, 47.6 parts by weight of an extender oil, 1.5 parts by weight of an antioxidant and 2 parts by weight of stearic acid were charged into the Labo Plastomill in two batches at 30 seconds and at 1 minute and 30 seconds from the start of kneading, and then they were kneaded with the pre-kneaded rubber composition. The temperature of the kneaded material reached 90° C. in 2 minutes and 10 seconds from the start of kneading. kneading was continued thereafter, and when the temperature of the kneaded material reached 120° C. at the time of 4 minutes and 10 seconds from the start of kneading, kneading was finished, so that a rubber composition was produced. Then, where the amount of the SBR-A used for preparing the pre-kneaded rubber composition used for preparing the rubber composition is 100 parts by weight, 2 parts by weight of zinc oxide and 1.5 parts by weight of wax were added to the rubber composition, and kneaded for 10 minutes with a 10-inch roll set at 70° C., so that a rubber composition was prepared.Where the amount of SBR-A used for preparing the pre-kneaded rubber composition used for preparing the rubber composition is 100 parts by weight, 1.4 parts by weight of sulfur and 2 parts by weight of vulcanization accelerators (1 part by weight of SOXINOL® CZ and 1 part by weight of SOXINOL® D) were added to the rubber composition, and they were kneaded for 10 minutes with a 10-inch roll set at 50° C., to obtain a vulcanizable rubber composition.The vulcanizable rubber composition was molded with a 10-inch roll to obtain a sheet made of the composition. Then, the plate was pressed at 160° C., 4 MPa for 45 minutes, so that a 150 mm wide, 150 mm long, and 1.2 mm thick plate made of a vulcanized rubber composition was produced.Comparative Example 1SBR-A was charged into a Labo Plastomill set at 70° C., and kneading was started. 78.4 parts by weight of a silica, 6.4 parts by weight of a silane coupling agent, 6.4 parts by weight of carbon black, 47.6 parts by weight of an extender oil, 1.5 parts by weight of an antioxidant and 2 parts by weight of stearic acid per 100 parts by weight of the above-mentioned SBR-A were charged into the Labo Plastomill in two batches at 30 seconds and at 1 minute and 30 seconds from the start of kneading, and they were kneaded with the SBR-A. The temperature of the kneaded material reached 90° C. in 2 minutes and 30 seconds from the start of kneading. kneading was continued thereafter, and when the temperature of the kneaded material reached 120° C. at the time of 4 minutes and 20 seconds from the start of kneading, kneading was finished, so that a rubber composition was obtained. Then, where the amount of the SBR-A used for preparing the rubber composition is 100 parts by weight, 2 parts by weight of zinc oxide and 1.5 parts by weight of wax were added to the rubber composition, and then they were kneaded for 10 minutes with a 10-inch roll set at 70° C., so that a rubber composition was obtained.Where the amount of SBR-A used for preparing the rubber composition is 100 parts by weight, 1.4 parts by weight of sulfur and 2 parts by weight of vulcanization accelerators (1 part by weight of SOXINOL® CZ and 1 part by weight of SOXINOL® D) were added to the rubber composition, and they were kneaded for 10 minutes with a 10-inch roll set at 50° C., to obtain a vulcanizable rubber composition.The vulcanizable rubber composition was molded with a 10-inch roll to obtain a sheet made of the composition. Then, the plate was pressed at 160° C., 4 MPa for 45 minutes, so that a 150 mm wide, 150 mm long, and 1.2 mm thick plate made of a vulcanized rubber composition was produced.Comparative Example 2SBR-A was charged into a Labo Plastomill set at 70° C., and kneading was started. 78.4 parts by weight of a silica, 6.4 parts by weight of carbon black, 47.6 parts by weight of a extender oil, 1.5 parts by weight of an antioxidant and 2 parts by weight of stearic acid per 100 parts by weight of the SBR-A were charged into the Labo Plastomill in two batches at 30 seconds and at 1 minute and 30 seconds from the start of kneading, and they were kneaded with the SBR-A. The temperature of the kneaded material reached 90° C. in 2 minutes and 30 seconds from the start of kneading. kneading was continued thereafter, and when the temperature of the kneaded material reached 120° C. at the time of 4 minutes and 30 seconds from the start of kneading, kneading was stopped, followed by cooling to room temperature, so that a rubber composition was obtained.The rubber composition and a silane coupling agent in an amount of 6.4 parts by weight per 100 parts by weight of the SBR-A used for preparing the rubber composition were charged into a Labo Plastomill set at 70° C., and kneading was started. The temperature of the kneaded material reached 90° C. in 40 seconds from the start of kneading. kneading was continued thereafter, and when the temperature of the kneaded material reached 120° C. at the time of 1 minute and 50 seconds from the start of kneading, kneading was finished, so that a rubber composition was obtained. Then, where the amount of the SBR-A used for preparing the rubber composition is 100 parts by weight, 2 parts by weight of zinc oxide and 1.5 parts by weight of wax were added to the rubber composition, and they were kneaded for 10 minutes with a 10-inch roll set at 70° C., so that a rubber composition was obtained.Where the amount of SBR-A used for preparing the rubber composition is 100 parts by weight, 1.4 parts by weight of sulfur and 2 parts by weight of vulcanization accelerators (1 part by weight of SOXINOL® CZ and 1 part by weight of SOXINOL® D) were added to the rubber composition, and then they were kneaded for 10 minutes with a 10-inch roll set at 50° C., so that a vulcanizable rubber composition was obtained.The vulcanizable rubber composition was molded with a 10-inch roll to obtain a sheet made of the composition. Then, the plate was pressed at 160° C., 4 MPa for 45 minutes, so that a 150 min wide, 150 mm long, and 1.2 mm thick plate made of a vulcanized rubber composition was produced.The results of evaluation of the properties of the sheets made of the vulcanized rubber compositions obtained in Example 1, Comparative Example 1 and Comparative Example 2, respectively, are shown in Table 1. [Table 1] Table 1] [Table 1] Table 1]Efficiency in saving fuel (tan δ at 70° C.)0,1480,1680,153Grip property (tan δ at 0° C.)0,4530,4190,435Example 2One hundred parts by weight of SBR-B and 6.4 parts by weight of a silane coupling agent were kneaded for five minutes with a 10-inch roll set at 105°C to obtain a kneaded material. Then, the kneaded material was charged into a Labo Plastomill set at 70° C., and kneading was started. The temperature of the kneaded material reached 90° C. in 1 minute and 10 seconds from the start of kneading, kneading was thereafter continued, and when the temperature of the kneaded material reached 120° C. at the time of 2 minutes and 50 seconds from the start of kneading, kneading was stopped, and then the kneaded material was cooled to room temperature, so that a pre-kneaded rubber composition was produced.The pre-kneaded rubber composition was filled in a Labo Plastomill set at 70° C., and kneading was started. Where the amount of the SBR-B used for preparing the pre-kneaded rubber composition is 100 parts by weight, 78.4 parts by weight of a silica, 6.4 parts by weight of carbon black, 47.6 parts by weight of an extender oil, 1.5 parts by weight of an antioxidant and 2 parts by weight of stearic acid were charged into the Labo Plastomill in two batches at 30 seconds and at 1 minute and 30 seconds from the start of kneading, and then they were kneaded with the pre-kneaded rubber composition. The temperature of the kneaded material reached 90° C. in 2 minutes and 20 seconds from the start of kneading, and thereafter, when the temperature of the kneaded material reached 120° C. at the time of 4 minutes and 10 seconds from the start of kneading, kneading was stopped, so that a rubber composition was obtained. Then, where the amount of the SBR-B used for preparing the rubber composition is 100 parts by weight, 2 parts by weight of zinc oxide and 1.5 parts by weight of wax were added to the rubber composition, and then they were kneaded for 10 minutes with a 10-inch roll set at 70° C., so that a rubber composition was obtained.To the rubber composition were added 1.4 parts by weight of sulfur and 2 parts by weight of vulcanization accelerators (1 part by weight of SOXINOL® CZ and 1 part by weight of SOXINOL® D) per 100 parts by weight of the SBR-B contained in the rubber composition, followed by kneading for 10 minutes with a 10-inch roll set at 50° C., to obtain a vulcanizable rubber composition.The vulcanizable rubber composition was molded with a 10-inch roll to obtain a sheet made of the composition. Then, the plate was heated at 160° C., 4 MPa for 45 minutes, so that a 150 mm wide, 150 mm long, and 1.2 mm thick plate made of a vulcanized rubber composition was produced.The results of evaluation of the properties of the sheet made of the vulcanized rubber composition obtained in Example 2 are shown in Table 2. [Table 2] [Table 2]Efficiency in saving fuel (tan δ at 70° C.)0,148Grip property (tan δ at 0° C.)0,660
Claims
A method for producing a rubber composition, the method comprising a step of producing a pre-kneaded rubber composition by kneading, at a temperature of 50°C or higher and 130°C or less, butadiene-based rubber, 1 to 20 parts by weight of a silane coupling agent per 100 parts by weight of the butadiene-based rubber and 5 parts by weight or less of silicon oxide per 100 parts by weight of the butadiene-based rubber, and a step of kneading the pre-kneaded rubber composition and 30 to 200 parts by weight of a silicon oxide per 100 parts by weight of the butadiene-based rubber used for producing the pre-kneaded rubber composition.The method of claim 1, wherein the silane coupling agent is an alkoxysilane compound having a sulfur-containing group.The method according to claim 1 or 2, wherein in the step of kneading the pre-kneaded rubber composition, the temperature at which the silica and the pre-kneaded rubber composition are kneaded is 160°C or less.A method for producing a vulcanizable rubber composition, the method comprising a step of kneading a vulcanizing agent and a rubber composition produced by the method according to any one of claims 1 to 3.A method for producing a vulcanized rubber composition, the method comprising a step of heating a vulcanizable rubber composition produced by the method according to claim 4.
Citation Information
Patent Citations
Method for producing radial conjugated diene polymer
EP2431395A1
Rubber composition for tread
JP1994248117A
Rubber composition and method for producing the same
JP2002201309A
Manufacturing process of rubber composition
JP2005263999A
Method of production of radial conjugated diene polymer
US20120071603A1