Rubber compound and its use in vehicle tires
Patent Information
- Application Number
- DE102013105193
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2013-05-22
- Publication Date
- 2024-10-17
- Estimated Expiration
- 2033-05-22
Abstract
Description
The invention relates to a rubber mixture and a use thereof in vehicle tires, which rubber mixture preferably contains at least in the tread.The rubber composition of the tread highly determines the running properties of a vehicle tire, in particular a pneumatic vehicle tire. Likewise, the rubber mixtures which find use in belts, hoses and belts, especially in the mechanically heavily stressed sites, are essentially responsible for the stability and durability of these rubber articles. Therefore, very high requirements are imposed on these rubber mixtures for vehicle tires, belts, belts and hoses.By partially or completely replacing the filler carbon black with silica in rubber mixtures, for example, the driving properties of a tire have been brought overall to a higher level in recent years. The known conflicts with the aim of tire properties which behave in opposite directions continue to exist, however, even in the case of silicic acid-containing tread mixtures. Thus, an improvement in wet grip and dry braking generally further results in a deterioration in rolling resistance, winter properties and abrasion performance. These properties are also an important quality criterion in technical rubber articles, such as belts, belts and hoses.In particular in vehicle tires, various attempts have been made to positively influence the properties of the tire by varying the polymer components, the fillers and the other additives, especially in the tread mixture. In the focus here, the properties rolling resistance and abrasion are above all. It is necessary to take account of the fact that an improvement in one tire property often results in a deterioration of another property. In a given mixing system, there are, for example, various known possibilities for optimizing the rolling resistance. Mention should be made here of lowering the glass transition temperature of the rubber mixture, reducing the degree of filling and changing the polymer system. All of the measures mentioned inevitably lead to a deterioration of at least one further of the other tire properties, such as the abrasion behaviour and / or the wet grip and / or the tear properties and / or the handling behaviour, of the given mixture. The term "vehicle tires" is understood in the present specification to mean pneumatic vehicle tires, solid rubber tires and two-wheeler tires.For optimizing the rolling resistance behavior or optimizing various other properties of rubber mixtures relevant for use in the tire without degrading the rolling resistance behavior, it is known to functionalize the diene rubber used in such a way that bonding to the filler(s) takes place.For example, EP 2357211 A1 discloses a rubber mixture which comprises at least one aliphatic and / or aromatic hydrocarbon resin, at least one filler and at least one functionalized diene rubber, the functionalization of which is present along the polymer chain and / or at the end and makes possible a bonding to fillers. Hydroxyl groups are disclosed as functionalizations in Table 1 for a linkage of the polymers to silica. As is apparent from the examples, for the desired improvement of the abrasion performance and the wet grip properties, 20 phr of a hydrocarbon resin as a plasticizer is necessary, and the rolling resistance performance deteriorates.EP 0806452 A1 also describes a rubber mixture comprising a functionalized diene rubber which carries hydroxyl groups, inter alia, as functional groups for the attachment to silica.EP 1457501 A1 discloses a functionalized styrene-butadiene copolymer which bears a primary amino group and an alkoxysilyl group as functional groups per styrene-butadiene copolymer chain. Furthermore, EP 1457501 A1 discloses rubber mixtures comprising this styrene-butadiene copolymer and tires whose tread strips consist of this rubber mixture. The tires are said to be distinguished by a good balance between abrasion resistance, durability, hysteresis loss and wet grip behavior. EP 1837370 A1 also discloses a rubber mixture in which a functionalized styrene-butadiene copolymer of this type is contained which carries a primary amino group and an alkoxysilyl group as functional groups per styrene-butadiene copolymer chain. Here, the rubber mixture in combination with a certain type of carbon black exhibits improved tire properties, such as wet braking, abrasion and rolling resistance behavior.EP 1 457 501 B1 discloses a composition comprising a copolymer having a side chain bearing a primary amino group and an alkoxysilyl group.EP 1 837 370 A1 discloses a sulfur-crosslinkable rubber mixture comprising 30 to 90 phr of at least one solution-polymerized styrene-butadiene copolymer having a vinyl fraction of more than 35% by weight and modified with primary amino groups and with alkoxysilyl groups.DE 697 04 724 T2 discloses a rubber mixture based on a diene polymer having a silanol group, which contains an organosilane derivative.DE 10 2004 059 379 A1 discloses prepolymers obtainable using aminomethyl-functional alkoxysilanes.US 2011 / 0178233 A1 discloses modified diene elastomers predominantly coupled by means of alkoxysilane groups which carry tertiary or secondary amines.WO 2009 / 133068 A1 discloses an elastomer mixture resulting from the modification of a diene elastomer by a coupling agent which introduces an alkoxysilane group having a tertiary or secondary amine function into the elastomer chain.JP H11-189616 A discloses a method for polymerizing or co-polymerizing conjugated diene monomers using an organolithium compound as an initiator with a cyclic aminoalkoxysilane.DE 600 18 649 T2 discloses a rubber composition comprising a diene-based rubber, silicon dioxide and a compatibilizer.Proceeding from the state of the art mentioned, the object of the present invention is now to provide a rubber mixture, in particular for vehicle tires, belts, belts and hoses, which is distinguished by a further improvement in the rolling resistance behavior, wherein the further physical properties remain at the same level or, in particular, the abrasion behavior and / or the wet grip properties are likewise intended to be further optimized.This object is achieved by providing a rubber mixture which comprises at least the following constituents:5 to 95 phr of at least one functionalized styrene-butadiene copolymer, the functionalized styrene-butadiene copolymer being functionalized per polymer chain at at least one chain end with an amino group-containing alkoxysilyl group and at least one further amino group-containing alkoxysilyl group(s), the amino groups being bonded to the chain end of the polymer chain with or without spacers, the functionalized styrene-butadiene copolymer having been obtained by the following process:anionic polymerization of styrene and butadiene monomers to form a styrene-butadiene copolymer chain by means of an alkali metal or alkaline earth metal; andreacting the living end of the polymer chain activated via alkali metal or alkaline earth metal with an alkoxysilane, at least one alkoxysilyl group of the alkoxysilane being protected with a protective group containing amino groups, andreaction of the alkoxysilyl-functionalized polymer chain with a further alkoxysilane to form a polymer chain functionalized with an alkoxysilyl group containing amino groups and at least one further alkoxysilyl group,and wherein the further alkoxysilyl group is likewise provided with a protective group comprising amino groups;and20 to 300 phr of silica and / or carbon black.Surprisingly, it has been found that the combination of at least one functionalized styrene-butadiene copolymer having the abovementioned features with 20 to 300 phr of silica and / or carbon black in the rubber mixture according to the invention is distinguished by optimizing the rolling resistance behavior. At the same time, the remaining tire properties remain at an approximately equally high level or are even improved, wherein in particular the abrasion behavior and / or the wet grip behavior of the rubber mixture remain at an approximately equally high level or are even improved.The stated phr (parts per hundred parts of rubber by weight) used in this specification is the stated amount of mixture formulations customary in the rubber industry. The dosage of the parts by weight of the individual substances is referred to in this specification to 100 parts by weight of the total mass of all high molecular weight and thereby solid rubbers present in the mixture.The term "functionalized styrene-butadiene copolymer" is understood in the context of the present invention to mean that the degree of functionalization of the total amount of styrene-butadiene copolymer is 30 to 100 mol %, i.e. that 30 to 100 mol %, preferably 70 to 100 mol %, of the polymer chains are functionalized.Essential to the invention, the functionalized styrene-butadiene copolymer per polymer chain is functionalized at at least one chain end with an amino group-containing alkoxysilyl group and at least one further amino group-containing alkoxysilyl group(s), the amino groups being bonded to the chain end of the polymer chain with or without spacers. To the amino group-containing alkoxysilyl group which is present by constraint, at least one further functional group is thus linked to the chain end of the functionalized styrene-butadiene copolymer.The functional groups of the functionalized styrene-butadiene copolymer are thus alkoxysilyl groups containing amino groups. All amino groups of the functionalized styrene-butadiene copolymer can be bonded to the chain end of the polymer chain with or without spacers. The bonding with spacer means that there is no direct linkage between the carbon atom of the chain end of the polymer chain and the nitrogen atom of the amino group, but a group of one or more atoms is interposed therebetween.The amino groups are preferably represented by one of the following formulae: H 2 N-R 1-; R 2 HN-R 1- and / or R 22 N-R 1-, where R 1 is a spacer, preferably an alkyl chain, branched or unbranched with C 0 to C 12, and R 2 is an alkyl selected from the group consisting of methyl, ethyl, propyl, butyl, branched or unbranched.The amino groups are particularly preferably represented by one of the following formulae: H 2 N-R 1-; R 2 HN-R 1- and / or R 22 N-R 1-, where R 1 is a spacer, preferably an alkyl chain, branched or unbranched with C 1 to C 12, and R 2 is an alkyl selected from the group consisting of methyl, ethyl, propyl, butyl, branched or unbranched.The amino group-containing alkoxysilyl group(s) and the amino group(s) and / or the alkoxysilyl group(s) may additionally carry protective groups.Functionalized styrene-butadiene copolymers of this type are obtained according to the invention by the following process:anionic polymerization of styrene and butadiene monomers to form a styrene-butadiene copolymer chain by means of an alkali metal or alkaline earth metal; andreacting the living end of the polymer chain activated via alkali metal or alkaline earth metal with an alkoxysilane, at least one alkoxysilyl group of the alkoxysilane being protected with a protective group containing amino groups, andreaction of the alkoxysilyl-functionalized polymer chain with a further alkoxysilane to form a polymer chain functionalized with an alkoxysilyl group containing amino groups and at least one further alkoxysilyl group.In this preparation process of the functionalized styrene-butadiene copolymer, the further alkoxysilyl group likewise bears an amino-group-containing protective group, so that the polymer is functionalized in this case with two amino-group-containing alkoxysilyl groups. The amino groups may also carry protecting groups.The functionalized styrene-butadiene copolymer may be solution polymerized or emulsion polymerized. It is preferably solution-polymerized styrene-butadiene copolymer (SSBR).The functionalized styrene-butadiene copolymer is also referred to in the context of the present invention as "functionalized styrene-butadiene rubber". The copolymer or rubber mentioned is a diene rubber.The functionalized styrene-butadiene copolymer preferably has a styrene content of 5 to 45 wt %, particularly preferably a styrene content of 14 to 30 wt %, and a vinyl content of 5 to 80 wt %, particularly preferably a vinyl content of 10 to 70 wt %. The glass transition temperature of the functionalized styrene-butadiene copolymer is preferably -10° C. to -80° C., particularly preferably -15 to -70° C. With such a preferred and particularly preferred microstructure of the functionalized styrene-butadiene copolymer, advantages with respect to the rolling resistance behavior can be achieved in the rubber mixtures according to the invention compared to the prior art, wherein the remaining tire properties, such as abrasion, wet grip and tear properties, remain at a good level or even are improved compared to the prior art. The determination of the styrene content and the vinyl fraction of the polymers discussed in the context of the present invention is carried out by means of 13 C-NMR (solvent deuterochloroform CDCl 3; NMR: nuclear magnetic resonance) and alignment with data from infrared spectrometry (IR; FT-IR spectrometer from Nicote, KBr window 25 mm diameter x 5 mm, 80 mg sample in 5 ml of 1,2-dichlorobenzene). The glass transition temperature (T g) is determined by means of dynamic difference calorimetry (engl. Dynamic scanning calorimetry, DSC according to DIN 53765: 1994-03 or ISO 11357-2: 1999-03, calibrated DSC with low-temperature device, calibration according to the type of instrument and manufacturer specifications, sample in the aluminium crucible with aluminium lid, cooling to temperatures lower than -120° C. at 10° C. / min).The functionalized styrene-butadiene copolymer is used in the rubber mixture according to the invention in amounts of 5 to 95 phr, preferably 20 to 95 phr, particularly preferably 50 to 95 phr, very particularly preferably in amounts of 60 to 95 phr. In a yet very particularly preferred embodiment of the invention, the amount of functionalized styrene-butadiene copolymer used is 75 to 95 phr, in particular 85 to 95 phr.Comparatively large amounts, i.e. 20 phr to 95 phr, of the functionalized styrene-butadiene copolymer have the effect of a comparatively great improvement in the rolling resistance behavior of the rubber mixture according to the invention.However, the rubber mixture according to the invention has optimum processability only at amounts up to 95 phr of the functionalized styrene-butadiene copolymer. The rubber mixture according to the invention therefore comprises from 5 to 95 phr of at least one further diene rubber.The rubber mixture preferably comprises, as a further diene rubber, at least one natural polyisoprene and / or at least one synthetic polyisoprene.The natural polyisoprene and the synthetic polyisoprene can be all types known to the skilled person. According to a further preferred development of the invention, the rubber mixture therefore contains 5 to 95 phr of at least one natural polyisoprene and / or 5 to 95 phr of at least one synthetic polyisoprene.According to a preferred embodiment of the invention, the rubber mixture contains 5 to 15 phr of at least one natural and / or synthetic polyisoprene.With the exception of the above-mentioned embodiment, the rubber mixture can also comprise at least one further polar or nonpolar rubber in other embodiments. The polar or nonpolar rubber is selected from the group consisting of and / or butadiene rubber and / or a further styrene-butadiene rubber and / or liquid rubbers and / or halobutyl rubber and / or polynorbornene and / or isoprene-isobutylene copolymer and / or ethylene-propylene-diene rubber and / or nitrile rubber and / or chloroprene rubber and / or acrylate rubber and / or fluororubber and / or silicone rubber and / or polysulfide rubber and / or epichlorohydrin rubber and / or styrene-isoprene-butadiene terpolymer and / or hydrogenated acrylonitrile-butadiene rubber and / or isoprene-butadiene copolymer and / or hydrogenated styrene-butadiene rubber.If a further styrene-butadiene rubber is used, this is different from the functionalized styrene-butadiene rubber as described above. Nitrile rubber, hydrogenated acrylonitrile butadiene rubber, chloroprene rubber, butyl rubber, halobutyl rubber or ethylene-propylene-diene rubber are used in particular in the production of industrial rubber articles, such as belts, belts and hoses.The rubber mixture according to the invention contains 20 to 300 phr of silica and / or carbon black. The rubber mixture preferably comprises at least one silica.The rubber mixture may comprise 0 to 270 phr, preferably 0 to 200 phr, particularly preferably 0 to 150 phr, of silica. According to a preferred embodiment of the invention, the rubber mixture contains at least, but preferably at least 0.1 phr, particularly preferably at least 0.5 phr, of silica. The rubber mixture in this embodiment particularly preferably comprises 20 to 150 phr, very particularly preferably 60 to 150 phr, of silica. This results in particularly good rolling resistance properties with simultaneously good and / or improved abrasion properties. In this preferred embodiment, preferably 0 to 15 phr, particularly preferably 0 to 7 phr, but at least 0.1 phr, of carbon black are contained in the rubber mixture.If only silica is used as the sole filler, the amount of silica is preferably 70 to 270 phr, particularly preferably 20 to 150 phr.The silica can be the silicas known to the skilled worker which are suitable as filler for tire rubber mixtures. It is, however, particularly preferred if a finely divided, precipitated silica is used which has a nitrogen surface area (BET surface area) (according to DIN ISO 9277 and DIN 66132) of 35 to 350 m 2 / g, preferably of 35 to 260 m 2 / g, particularly preferably of 100 to 260 m 2 / g and very particularly preferably of 130 to 235 m 2 / g and a CTAB surface area (according to ASTM D 3765) of 30 to 400 m 2 / g, preferably of 30 to 250 m 2 / g, particularly preferably of 100 to 250 m 2 / g and very particularly preferably of 125 to 230 m 2 / g. Such silicas lead, for example in rubber mixtures for tire treads, to particularly good physical properties of the vulcanizates. In addition, advantages in mixing processing can result from a reduction in mixing time with constant product properties, which leads to improved productivity. Thus, for example, both those of the type Ultrasil® VN3 (trade name) from Evonik and highly dispersible silicas, so-called HD silicas (for example Zeosil® 1165 MP from Rhodia), can be used as silicas. It is preferred that the silica be a highly dispersible silica type having a CTAB surface area according to ASTM D 3765 of between 125 and 230 m 2 / g. Such a silica has particular advantages in rolling resistance behavior.To improve the processability and to attach the silica and other polar fillers, if present, to the diene rubber, silane coupling agents can be used in rubber mixtures. The silane coupling agents react with the surface silanol groups of the silica or other polar groups during the mixing of the rubber or of the rubber mixture (in situ) or already before the addition of the filler to the rubber in the sense of a pretreatment (pre-modification). The silane coupling agents used can be all silane coupling agents known to the skilled person for use in rubber mixtures. Such coupling agents known from the prior art are bifunctional organosilanes which have at least one alkoxy, cycloalkoxy or phenoxy group as leaving group on the silicon atom and which have as other functionality a group which, if appropriate after cleavage, can enter into a chemical reaction with the double bonds of the polymer. The latter group may be, for example, the following chemical groups:-SCN, -SH, -NH 2 or -S x- ( where x=2 to 8).Thus, for example, 3-mercaptopropyltriethoxysilane, 3-thiothionopropyltrimethoxysilane or 3,3'-bis(triethoxysilylpropyl)polysulfides having 2 to 8 sulfur atoms, such as, for example, 3,3'-bis(triethoxysilylpropyl)tetrasulfide (TESPT), the corresponding disulfide (TESPD) or else mixtures of the sulfides having 1 to 8 sulfur atoms with different contents of the various sulfides, can be used as silane coupling agents. TESPT can also be added, for example, as a mixture with carbon black (trade name X50S® from Evonik). Preference is given to using a silane mixture which comprises from 40 to 100% by weight of disulfides, more preferably from 55 to 85% by weight of disulfides and most preferably from 60 to 80% by weight of disulfides. Such a mixture is available, for example, under the trade name Si 261® from Evonik, which is described, for example, in DE 102006004062 A1. Blocked mercaptosilanes, as are known, for example, from WO 99 / 09036, can also be used as silane coupling agent. It is also possible to use silanes as described in WO 2008 / 083241 A1, WO 2008 / 083242 A1, WO 2008 / 083243 A1 and WO 2008 / 083244 A1. Usable are, for example, silanes sold under the name NXT in various variants by Momentive, USA, or those sold under the name VP Si 363® by Evonik Industries.The silane coupling agents are used in amounts of 0.2 to 30 phf, preferably 1 to 15 phf, since an optimum bonding of the filler to the rubber or rubbers can then take place. The unit phf (parts per hundred parts of filler by weight) refers in the context of the present application to 100 parts by weight of silica in each case.Furthermore, the rubber mixture according to the invention may preferably comprise 0 to 100 phr, preferably 0 to 80 phr, of carbon black.According to a preferred embodiment of the invention, the rubber mixture comprises at least 0.1 phr, more preferably at least 0.5 phr, of at least one carbon black.Particularly preferably, the amount of carbon black in this embodiment of the invention is 5 to 70 phr.If only carbon black is used as the sole filler, the amount of carbon black is preferably at least 30 phr.All carbon blacks known to the person skilled in the art are possible here. In a particularly preferred embodiment, the carbon black has an iodine value, according to ASTM D 1510, which is also referred to as iodine adsorption value, of between 80 g / kg and 250 g / kg, and a DBP number greater than or equal to 90 cm 3 / 100 g, preferably between 100 cm 3 / 100 g and 200 cm 3 / 100 g, particularly preferably between 115 cm 3 / 100 g and 200 cm 3 / 100 g. The DBP number according to ASTM D 2414 determines the specific absorption volume of a carbon black or a light filler by means of dibutyl phthalate. The use of such a type of carbon black in the rubber mixture, in particular for vehicle tires, ensures the best possible compromise between abrasion resistance and heat build-up, which in turn influences the ecologically relevant rolling resistance. It is preferred here if only one type of carbon black is used in the respective rubber mixture, but it is also possible to mix different types of carbon black into the rubber mixture.The rubber mixture may also contain other polar fillers, such as, for example, aluminosilicates, chalk, starch, magnesium oxide, titanium dioxide or rubber gels.The rubber mixture may also contain 0 to 60 phr, preferably 0.1 to 50 phr, preferably 0.1 to 40 phr, of at least one plasticizer. These include all plasticizers known to the skilled worker, such as aromatic, naphthenic or paraffinic mineral oil plasticizers, such as, for example, MES (mild extraction solvate) or TDAE (treated distillate aromatic extract), or rubber-to-liquid oils (RTL) or biomass-to-liquid oils (BTL) or factices or plasticizer resins or liquid polymers (such as liquid BR), the average molecular weight of which (determined by GPC=gel permeation chromatography, based on BS ISO 11344:2004) is between 500 and 25000 g / mol. If liquid polymers are used as plasticizers in the rubber mixture according to the invention, these do not enter into the calculation of the composition of the polymer matrix as rubber. When mineral oil is used, it is preferably selected from the group consisting of DAE (distilled aromatic extracts) and / or RAE (residual aromatic extract) and / or TDAE (treated distilled aromatic extracts) and / or MES (mild extracted solvents) and / or naphthenic oils.Furthermore, the rubber mixture according to the invention may comprise customary additives in customary parts by weight. These additives include a) anti-aging agents such as N-phenyl-N'-(1,3-dimethylbutyl)-p-phenylenediamine (6PP), N,N'-diphenyl-p-phenylenediamine (DPPD), N,N'-ditolyl-p-phenylenediamine (DTPD), N-isopropyl-N'-phenyl-p-phenylenediamine (IPPD), 2,2,4-trimethyl-1,2-dihydroquinoline (TMQ), b) activators such as zinc oxide and fatty acids (e.g. stearic acid), c) waxes, d) resins and e) masticating aids such as 2,2'-dibenzamidodiphenyl disulfide (DBD).In the total amount fraction of the further additives, there is also 0.1 to 10 phr, preferably 0.2 to 8 phr, particularly preferably 0.2 to 4 phr, of zinc oxide (ZnO). These can be all types of zinc oxide known to the skilled worker, such as, for example, ZnO granules or powders. Furthermore, the ZnO can be nanoscale zinc oxide.Vulcanization is carried out in the presence of sulfur or sulfur donors with the aid of vulcanization accelerators, it being possible for some vulcanization accelerators to act simultaneously as sulfur donors. Sulfur or sulfur donors and one or more accelerators are added in the amounts mentioned to the rubber mixture in the last mixing step. The accelerator is selected from the group consisting of thiazole accelerators and / or mercapto accelerators and / or sulfenamide accelerators and / or thiocarbamate accelerators and / or thiuram accelerators and / or thiophosphate accelerators and / or thiourea accelerators and / or xanthate accelerators and / or guanidine accelerators. Preference is given to the use of a sulfenamide accelerator selected from the group consisting of N-cyclohexyl-2-benzothiazolesulfenamide (CBS) and / or N,N-dicyclohexylbenzothiazole-2-sulfenamide (DCBS) and / or benzothiazyl-2-sulfenomorpholide (MBS) and / or N-tert-butyl-2-benzothiazylsulfenamide (TBBS).In a preferred embodiment of the invention, the rubber mixture comprises TBBS as accelerator. This achieves particularly good tear properties of the rubber mixture.According to an advantageous development of the invention, a plurality of accelerators are used. Preference is given to using a sulfenamide accelerator, more preferably CBS, in combination with the guanidine accelerator DPG (diphenylguanidine). The amount of DPG is 0 to 5 phr, preferably 0.1 to 3 phr, particularly preferably 0.5 to 2.5 phr, very particularly preferably 1 to 2.5 phr.The rubber mixture according to the invention is produced by the process customary in the rubber industry, in which a masterbatch is first prepared in one or more mixing stages with all constituents other than the vulcanization system (sulfur and vulcanization-influencing substances). By adding the vulcanization system in a final mixing stage, the final mixture is produced. The finished mixture is further processed, for example, by an extrusion process and is brought into the corresponding shape.The invention is further based on the object, on the basis of the prior art mentioned at the beginning, of further improving the rolling resistance behavior of vehicle tires without significantly adversely affecting other relevant properties, in particular the abrasion behavior.This object is achieved by providing a vehicle tire which preferably uses the rubber mixture according to the invention in running stiffness.Surprisingly, a vehicle tire which uses the rubber mixture according to the invention, preferably in the tread, exhibits improved rolling resistance behavior in comparison with the prior art, wherein the remaining tire properties are not significantly adversely affected and the abrasion behavior is even partially improved.For the description of the functionalized styrene-butadiene copolymer and all constituents of the rubber mixture, all embodiments mentioned above in the description of the rubber mixture according to the invention apply.The vehicle tire is preferably a pneumatic vehicle tire.Furthermore, the rubber mixture according to the invention described above is for the body mixture of a tire and for the production of industrial rubber articles, such as, for example. These may be used in any suitable manner, such as belts, belts and hoses. The term body mixture here refers to the rubber mixtures for the inner components of a tire. Inner tire components are essentially called a squeezee, sidewall, innerliner (inner layer), core profile, belt, shoulder, belt profile, carcass, bead enhancer, bead profile, horn profile and bandage.For use in vehicle tyres, the mixture is preferably shaped into a tread and applied as known in the manufacture of the green vehicle tyre. The tread can, however, also be wound onto a tyre blank in the form of a narrow rubber compound strip. In the case of two-part tread (upper part: cap and lower part: base), the rubber mixture according to the invention can be used both for cap and for base, use in cap being preferred.The rubber mixture according to the invention for use as a body mixture in vehicle tires is produced as already described for the tread. The difference lies in the shaping after the extrusion process. The forms of the rubber mixture according to the invention thus obtained for one or more different body mixtures then serve to construct a tire blank.The invention will now be explained in more detail with reference to comparative and exemplary embodiments, which are summarized in Tables 1 and 2. The mixtures marked "E" are mixtures according to the invention, while the mixtures marked "V" are comparative mixtures. In all the mixing examples contained in the table, the stated amounts are parts by weight, based on 100 parts by weight of total rubber (phr) or based on 100 parts by weight of silica (phf).The functionalized styrene-butadiene copolymers described above are obtained by the following process:anionic polymerization of styrene and butadiene monomers to form a styrene-butadiene copolymer chain by means of an alkali metal or alkaline earth metal; andreacting the living end of the polymer chain activated via alkali metal or alkaline earth metal with an alkoxysilane, at least one alkoxysilyl group of the alkoxysilane being protected with a protective group containing amino groups, andreaction of the alkoxysilyl-functionalized polymer chain with a further alkoxysilane to form a polymer chain functionalized with an alkoxysilyl group containing amino groups and at least one further alkoxysilyl group.Here, the further alkoxysilyl group likewise bears a protective group comprising amino groups, and so the polymer is functionalized in this case with two alkoxysilyl groups comprising amino groups. The amino groups may also carry protecting groups.The mixture was prepared under customary conditions in three stages in a laboratory tangential mixer. Test specimens were produced from all the mixtures by vulcanization and typical material properties for the rubber industry were determined with these test specimens. The test methods described above for test specimens were as follows:• Shore A hardness (unit Shore A, abbreviated ShA) at room temperature (RT) according to DIN 53 505• Rebound resilience (abbreviated rebound) at room temperature (RT) and 70° C. according to DIN 53 512• Tensile strength and elongation at break at room temperature according to DIN 53 504• Abrasion at room temperature according to DIN53 516 or DIN / ISO 4649• Maximum (max) loss factor tan δ (tan delta) from dynamic-mechanical measurement at 55° C. in accordance with DIN 53 513, strain sweep (strain sweep)Table 1 Table 1SSBR a)phr phr phr phr phr phr phr phr phr phr90--SSBR A b)phr phr phr phr phr phr phr phr phr phr-90-SSBR A' c)phr phr phr phr phr phr phr phr phr phr--90NR: TSRphr phr phr phr phr phr phr phr phr phr101010Silica d)phr phr phr phr phr phr phr phr phr phr959595Silane,TESPDphf7,27,27,2TDAEphr phr phr phr phr phr phr phr phr phr353535ZnOphr phr phr phr phr phr phr phr phr phr2,52,52,5Antiaging agent / antiozonant / stearic acidphr phr phr phr phr phr phr phr phr phr6,56,56,5DPGphr phr phr phr phr phr phr phr phr phr222CBSphr phr phr phr phr phr phr phr phr phr222Sulfurphr phr phr phr phr phr phr phr phr phr222Shore A hardness at RTShA707070Rebound at RT%374140Rebound b. 70° C%485250Tan δ (max)0,1930,1630,163Substances used from Table 1:SSBR: Solution polymerized styrene-butadiene copolymer from the prior art functionalized with hydroxy groups, Nipol® NS 612, Fa. Zeon Corporationb) SSBR A: functionalized styrene-butadiene copolymer functionalized per polymer chain at at least one chain end with an amino group-containing alkoxysilyl group and a further amino group-containing alkoxysilyl group, wherein the amino groups are bonded to the chain end of the polymer chain with or without spacers; styrene content: 14.7% by weight, vinyl content about 34%, T g = - 59,3 ° Cc) SSBR A': functionalized styrene-butadiene copolymer functionalized according to SSBR A; styrene content: 10% by weight, vinyl content about 40%, T g = - 61 ° Cd) Silica: VN3, Fa. EvonikTable 2Table 2SSBR e)phr phr phr phr phr phr phr phr phr phr90---SSBR f)-90--SSBR B g)phr phr phr phr phr phr phr phr phr phr--90-SSBR B' h)phr phr phr phr phr phr phr phr phr phr---90NR: TSRphr phr phr phr phr phr phr phr phr phr10101010Silica d)phr phr phr phr phr phr phr phr phr phr95959595Silane,TESPDphf7,27,27,27,2TDAEphr phr phr phr phr phr phr phr phr phr35353535ZnOphr phr phr phr phr phr phr phr phr phr2,52,52,52,5Antiaging agent / antiozonant / stearic acidphr phr phr phr phr phr phr phr phr phr6,56,56,56,5DPGphr phr phr phr phr phr phr phr phr phr2222CBSphr phr phr phr phr phr phr phr phr phr2222Sulfurphr phr phr phr phr phr phr phr phr phr2222Shore A hardness at RTShA72706567Rebound at RT%18182319Rebound b. 70° C%47505654Diff. Rebound29323335Tensile StrengthMPa8151115Elongation at break%252419322386Tan δ (max)0,1940,1900,1500,163DIN Abrasion3 mm 3 mm165164154158Substances used from Table 2:d) Silica: VN3, Fa. EvonikSSBR: Solution polymerized styrene-butadiene copolymer from the prior art functionalized with hydroxy groups, Nipol® NS 616, Fa. Zeon CorporationSSBR: Solution polymerized styrene-butadiene copolymer from the prior art functionalized with an amino group and an alkoxysilyl group, HPR 355 H, JSR Corporation, Japan, styrene content: 28% by weight, vinyl content: 56%,g) SSBR B: functionalized styrene-butadiene copolymer functionalized per polymer chain at at least one chain end with a first and a further amino group-containing alkoxysilyl group and at least one further functional group selected from the group consisting of amino groups and alkoxysilyl groups, wherein the amino groups are bonded to the chain end of the polymer chain with or without spacers; styrene content: 20.2% by weight, vinyl content about 63.3%, T g = - 25,4 ° Ch) SSBR B': functionalized styrene-butadiene copolymer functionalized according to SSBR B; styrene content: 25% by weight, vinyl content about 56%, T g = - 31 ° CIt can be seen from the tables that the rubber mixtures E1, E2 and E3 and E4 according to the invention have significantly improved rolling resistance indicators compared with their respective comparative mixtures V1 or V2 and V3. This is evident from the lower tan δ (tan delta) values and the increased rebound resilience values at 70°C. In addition, the rubber mixtures E3 and E4 show improved abrasion resistance compared with their comparative mixtures with styrene-butadiene copolymers from the prior art V2 and V3, and also have greater values for the difference in rebound elasticities at 70° C. and room temperature (RT). The greater this difference, the more strongly the conflict of goals is decoupled from rolling resistance behavior and wet grip properties.
Claims
Rubber mixture, characterized in that it comprises at least the following constituents: - 5 to 95 phr of at least one functionalized styrene-butadiene copolymer, the functionalized styrene-butadiene copolymer being functionalized per polymer chain at at least one chain end with an alkoxysilyl group containing amino groups and at least one further alkoxysilyl group(s) containing amino groups, the amino groups being bonded to the chain end of the polymer chain with or without spacers, the functionalized styrene-butadiene copolymer having been obtained by the following process: - anionic polymerization of styrene and butadiene monomers to form a styrene-butadiene copolymer chain by means of an alkali metal or alkaline earth metal and - reaction of the living, alkaline earth metal, End of the polymer chain activated via alkali metal or alkaline earth metal with an alkoxysilane, at least one alkoxysilyl group of the alkoxysilane being protected with a protective group containing amino groups, and - reacting the alkoxysilyl-functionalized polymer chain with a further alkoxysilane to give a polymer chain functionalized with an alkoxysilyl group containing amino groups and at least one further alkoxysilyl group, - and the further alkoxysilyl group likewise being provided with a protective group containing amino groups; - and - 20 to 300 phr of silica and / or carbon black.Rubber mixture according to Claim 1, characterized in that the amino group(s) are represented by one of the following formulae: H 2 N-R 1-, R 2 HN-R 1- and / or R 22 N-R 1-, where R 1 is a spacer, preferably an alkyl chain, branched or unbranched with C 0 to C 12, and R 2 is an alkyl selected from the group consisting of methyl, ethyl, propyl, butyl, branched or unbranched.Rubber mixture according to any of the preceding claims, characterized in that the functionalized styrene-butadiene copolymer has a styrene content of 5 to 45% by weight.Rubber mixture according to any of the preceding claims, characterized in that the functionalized styrene-butadiene copolymer has a vinyl fraction of 5 to 80% by weight.Rubber mixture according to any of the preceding claims, characterized in that the functionalized styrene-butadiene copolymer has a glass transition temperature of -10°C to -80°C.Use of the rubber mixture according to any of Claims 1 to 5 in vehicle tyres.
Citation Information
Patent Citations
alkoxysilane terminated prepolymers
DE102004059379A1
rubber compounds
DE102006004062A1
rubber composition and tires made from it
DE60018649T2
Rubber compound based on a diene polymer with a silanol group containing an organosilane derivative
DE69704724T2
Rubber composition and process for preparing the same
EP0806452A1