Metalgate stacks with TiAICN as working functional layer and / or barrier / wetting layer and process
Patent Information
- Application Number
- DE102014119644
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2014-07-10
- Filing Date
- 2014-12-27
- Publication Date
- 2024-10-02
- Estimated Expiration
- 2034-12-27
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
GENERAL STATE OF THE ARTThe integrated circuit (IC) industry has grown rapidly. Technical advances in IC materials and design have produced generations of ICs, each generation having smaller and more complex circuits than the previous generation. These advances have increased the complexity of processing and manufacturing ICs, and in order for these advances to be realized, similar developments in IC processing and manufacturing are needed. In the course of IC development, the functional density (i.e., the number of interconnected devices per chip area) has generally increased, while the geometric size (i.e., the smallest component (or lead) that can be achieved with a fabrication process) has decreased. This downscaling process generally offers advantages by increasing production efficiency and decreasing associated costs. Such downscaling has also increased the complexity of processing and manufacturing ICs, and in order for these advances to be realized, similar developments in IC processing and manufacturing are needed. An integrated circuit is known from DE 11 2009 002 118 T5. Similar circuits are also known from US 2014 / 0 154 877 A1 or US 2013 / 0 075 833 A1.BRIEF DESCRIPTION OF THE DRAWINGSThe present disclosure will be best understood from the following detailed description when read with the accompanying drawings. It is emphasized that, in accordance with common practice in the industry, various features are not drawn to scale and are used for illustrative purposes only. Indeed, the dimensions of the various features may be arbitrarily increased or reduced for clarity of discussion. FIG. 1 is a flow diagram of a method of manufacturing an integrated circuit according to various aspects of the present disclosure.FIGS. 2-7 are diagrammatic cross-sectional views of an integrated circuit during various stages of the method of FIG. 1, in accordance with various aspects of the present disclosure.DETAILED DESCRIPTIONFIG. 1 is a flow diagram of a method 100 for manufacturing an integrated circuit in portions or in whole, in accordance with various aspects of the present disclosure. The method 100 begins at block 110 where a gate structure is formed over a substrate. The gate structure includes a gate stack including a high-k dielectric layer disposed over the substrate and a dummy gate disposed over the high-k dielectric layer. At block 120, the dummy gate is removed from the gate structure to form an opening therein. At block 130, a multifunction barrier / wetting layer, a work function layer, and a conductive layer are formed to fill the opening. The multifunction barrier layer / wetting layer is formed over the high-k dielectric layer, the work function layer is formed over the multifunction barrier layer / wetting layer, and the conductive layer is formed over the work function layer. The multifunction barrier layer / wetting layer comprises a material that sufficiently prevents (or reduces) metal contaminants from entering the high-k dielectric layer (e.g., from the conductive layer) during processing, while providing sufficient wettability (in other words, desired barrier layer quality) with the work function layer. The method 100 may proceed to block 140 to complete the manufacture of the integrated circuit. Additional steps may be provided before, during, and after the method 100, and some of the described steps may be replaced or eliminated for additional embodiments of the method 100.FIGS. 2-7 are diagrammatic cross-sectional views of an integrated circuit 200, in a portion or in whole, at various stages of manufacture according to the method 100 of FIG. 1, FIGS. 2-7 having been simplified for clarity in order to better understand the inventive concepts of the present disclosure. In the illustrated embodiment, the integrated circuit 200 includes a field effect transistor device such as an n-channel field effect transistor (NFET) or a p-channel field effect transistor (PFET). The integrated circuit 200 may be included in memory cells and / or logic circuits including passive devices such as resistors, capacitors, inductors, and / or fuses; active devices such as metal oxide semiconductor field effect transistors (MOSFETs), complementary metal oxide semiconductor transistors (CMOSs), high voltage transistors, and / or high frequency transistors; other suitable components; or combinations thereof. Additional functions may be added in integrated circuit 200 and some of the features described below may be replaced or eliminated in other embodiments of integrated circuit 200.In FIG. 2, integrated circuit 200 includes a substrate 210. In the illustrated embodiment, the substrate 210 is a semiconductor substrate including silicon. Alternatively or additionally, the substrate 210 comprises a further elementary semiconductor such as germanium; a compound semiconductor including silicon carbide, gallium arsenic, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide; an alloy semiconductor including SiGe, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP, and / or GaInAsP; or combinations thereof. In yet another alternative, the substrate 210 is a semiconductor on insulator (SOI). In other alternatives, the semiconductor substrate 210 may include a doped epi layer, a gradient semiconductor layer, and / or a semiconductor layer overlying another semiconductor layer of a different type, such as a silicon layer on a silicon germanium layer. The substrate 210 includes various doping configurations depending on design requirements of the integrated circuit 200. For example, the substrate 210 may include various doped zones doped with p-type dopants such as boron or BF 2; n-type dopants such as phosphorus or arsenic; or combinations thereof. The doped regions may be formed on the semiconductor substrate in a P-well structure, in an N-well structure in a double-well structure, or using a raised structure.An isolation element 212 is disposed in the substrate 210 to isolate various regions and / or devices of the substrate 210. Isolation element 212 uses isolation technology such as local oxidation of silicon (LOCOS) and / or shallow trench isolation (STI) to define and galvanically separate the various regions. The isolation element 212 includes silicon oxide, silicon nitride, silicon oxynitride, and other suitable materials or combinations thereof. The isolation element 212 is formed by any suitable process. For example, forming an STI includes using a lithography process to expose a portion of the substrate, etching a trench in the exposed portion of the substrate (e.g., using a dry etch and / or wet etch), and filling the trench (e.g., using a chemical vapor deposition process) with one or more dielectrics. For example, the filled trench may have a multilayer structure such as a thermal oxide cladding layer filled with silicon nitride or silicon oxide.A gate structure 220 is disposed over the substrate 210. In the illustrated embodiment, the gate structure 220 includes a gate stack having an interlayer dielectric layer 222, a high-k dielectric layer 224, and a dummy gate layer 226. The interlayer dielectric layer 222 and the high-k dielectric layer 224 may collectively be referred to as a gate dielectric layer of the gate structure 220. The gate stack may include additional layers, such as a hard mask layer, a capping layer, a diffusion / barrier layer, a dielectric layer, a metal layer, other suitable layers, or combinations thereof. The gate structure 220 is formed by a process including deposition processes, lithography patterning processes, etching processes, other suitable processes, or combinations thereof. The deposition processes include physical vapor deposition (PVD), chemical vapor deposition (CVD), atomic layer deposition (ALD), plasma enhanced CVD (PECVD), remote plasma CVD (RPCVD), molecular organic CVD (MOCVD), sputtering, plating, other suitable methods, or combinations thereof. The lithography patterning processes include resist coating (e.g., spin-on coating), pre-curing, mask alignment, exposure, post-exposure firing, photoresist developing, rinsing, drying (e.g., post-curing), other suitable processes, or combinations thereof. The lithography exposure process may be implemented or replaced by other suitable methods such as maskless lithography, electron beam writing, ion beam writing, and molecular embossing. The etching processes include dry etching, wet etching, or combinations thereof.The interlayer dielectric layer 222 is disposed over the substrate 210. In an example, the interlayer dielectric layer 222 has a thickness of about 0.5 nm to about 2 nm. In the illustrated embodiment, the interlayer dielectric layer 222 is an oxide-containing layer, such as a silicon oxide (SiO 2) - layer or a silicon oxynitride (SiON) layer. The intermediate layer 222 may comprise other suitable materials. The interlayer dielectric layer 222 is formed by a chemical oxide technique, thermal oxide technique, atomic layer deposition (ALD), chemical vapor deposition (CVD), or other suitable technique. A cleaning process, such as an RF load pre-gate cleaning process (e.g., using a hydrofluoro (RF) acid solution) may be performed before the interlayer dielectric layer 222 is formed over the substrate 210.The high-k dielectric layer 224 is disposed over the interlayer dielectric layer 222, and the dummy gate layer 226 is disposed over the high-k dielectric layer 224. A thickness of the high-k dielectric layer 224 and the dummy gate layer 226 depends on design requirements of the integrated circuit 200. In an example, the high-k dielectric layer 224 has a thickness of about 0.5 nm to about 3 nm and the dummy gate layer has a thickness of about 35 nm to about 70 nm. The high-k dielectric layer 224 includes a high-k dielectric material such as HfO 2, HfSiO, HfSiON, HfTaO, HfTiO, HfNbO, zirconium oxide, aluminum oxide, hafnium dioxide-aluminum oxide (HfO 2- Al 2 O 3) - alloy, other suitable high-k dielectrics, or combinations thereof. The dummy gate layer 226 includes a material suitable for a gate replacement process. For example, in the illustrated embodiment, dummy gate layer 226 includes polysilicon.The gate structure 220 further includes spacer elements 228 formed by a suitable process. For example, a dielectric layer, such as a silicon nitride layer, is deposited over the entire area of the integrated circuit 200; and then the silicon nitride layer is anisotropically etched to remove the silicon nitride layer and form the spacers 228 as illustrated in FIG. 2. The spacers 228 are disposed adjacent the sidewalls of the gate stack (interlayer dielectric layer 222, high-k dielectric layer 224, and dummy gate layer 226) of the gate structure 220. Alternatively or additionally, the spacers 228 include another dielectric material such as silicon oxide, silicon carbonitride, or combinations thereof.Various source / drain elements 230 may be disposed in the substrate 210. The source / drain elements 230 are on both sides of the gate structure 220. The source / drain elements 230 may include lightly doped source and drain (LDD) regions and / or highly doped (HDD) source and drain regions. The LDD and / or HDD regions may be formed by ion implantation or diffusion of n-type dopants such as phosphorus or arsenic or p-type dopants such as boron or BF 2. An annealing process, such as rapid thermal annealing and / or laser thermal annealing, may be performed to activate dopants of the LDD and / or HDD zones. The LDD and / or HDD zones may be formed at any time in the illustrated embodiment. The source / drain elements 230 may include raised source / drain elements such as epitaxial elements (e.g., epitaxial silicon germanium elements or epitaxial silicon elements). Silicide elements may be disposed over the source / drain elements 230 to reduce contact resistance, for example. The silicide elements may be formed over the source and drain elements by a self-aligned salicide process that may include depositing a metal layer, annealing the metal layer such that the metal layer may react with silicon to form silicide, and then removing the unreacted metal layer.A dielectric layer 232 is disposed over the substrate 210, such as an interlayer (or interposer) dielectric (ILD) layer. The dielectric layer 232 includes a dielectric material such as silicon oxide, silicon nitride, silicon oxynitride, tetraethylorthosilicate (TEOS) oxide formed, phosphosilicate glass (PSG), borophosphosilicate glass (BPSG), low-k dielectric material, other suitable dielectric material, or combinations thereof. Exemplary low-k dielectrics include fluorinated silica glass (FSG), carbon doped silicon oxide, black Diamond® (Applied Materials from Santa Clara, California), xerogel, aerogel, amorphous fluorinated carbon, parylene, BCB (bisbenzocyclobutene), SiLK (Dow Chemical, Midland, Michigan), polyimide, other suitable materials, and / or combinations thereof. The dielectric layer 232 may include a multi-layer structure including multiple dielectrics. The dielectric layer 232 is formed to a suitable thickness by any suitable process including CVD, high density plasma CVD, spin-on, and / or other suitable methods. After the deposition of the dielectric layer 232, a chemical mechanical polishing (CMP) process is performed until an upper portion of the gate structure 220 is reached / exposed. In particular, an upper portion of the gate stack of the gate structure 220 (here the dummy gate layer 226) is exposed as illustrated in FIG. 2. Additional layers may be formed overlying and / or underlying the dielectric layer 232.Referring to FIGS. 3 to 7, a gate replacement process is performed in which the dummy gate layer 226 is replaced with a metal gate. In FIG. 3, the dummy gate layer 226 is removed from the gate stack of the gate structure 220, thereby forming an opening 240. The opening 240 exposes the high-k gate dielectric layer 224. The dummy gate layer 226 may be removed by an etching process, other suitable process, or combinations thereof. In an example, an etching process selectively etches dummy gate layer 226.In FIG. 4, a multifunction barrier / wetting layer 242 is formed over the substrate 210 such that the multifunction barrier / wetting layer 242 layer partially fills the opening 240. The multi-function barrier / wetting layer 242 is disposed along the sidewalls of the gate structure 220 that define the opening 240. In the illustrated embodiment, the multi-function barrier / wetting layer 242 is disposed over the high-k dielectric layer 224. In one example, the multifunction barrier / wetting layer 242 has a thickness of about 3 nm to about 10 nm. The multi-function barrier layer / wetting layer 242 functions as both a blocking (or barrier) layer and a wetting layer during processing. For example, the multifunction barrier / wetting layer 242 prevents or reduces metal contaminants from entering any dielectric layers disposed below the multifunction barrier / wetting layer 242 (such as the gate dielectric of the gate stack of the gate structure 220), while improving adhesion between the layer below and the layer above. It also provides a desirable interface quality between the multifunction barrier / wetting layer 242 and each layer of material formed over the multifunction barrier / wetting layer 242. Accordingly, in the illustrated embodiment, the multifunction barrier / wetting layer 242 prevents or reduces metal contaminants from entering the high-k dielectric layer 224 and the interlayer dielectric layer 222, while improving adhesion between layers below and above, such as the high-k dielectric layer 224 and a layer of the gate stack of the gate structure 220 formed over the multifunction barrier / wetting layer 242 (such as the work function layer 244). This functionality is described in further detail below.In the illustrated embodiment, the multi-function barrier / wetting layer 242 comprises titanium aluminum nitride (TiAlN) and in exemplary embodiments, the TiAlN is present as titanium aluminum carbonitride (TiAlCN). An atomic concentration of nitrogen and carbon of the TiAlCN layer is optimized such that the multifunction barrier / wetting layer 242 sufficiently prevents or reduces metal contaminants from entering underlying dielectric layers (e.g., high-k dielectric layer 224 and barrier layer 222) while minimally affecting an operating function of the integrated circuit 200. Therefore, the nitrogen atom concentration and the carbon atom concentration are selected to balance the blocking ability and the desired work function. In the illustrated embodiment, the TiAlCN layer comprises a nitrogen atom concentration of about 5% to about 15% and a carbon atom concentration of about 5% to about 20%. At lower nitrogen and carbon atom concentrations (e.g., less than about 5%), the blocking ability may move in an undesirable direction as it shifts closer to the desired work function. On the other hand, at higher nitrogen and carbon atom concentrations (e.g., nitrogen atom concentrations greater than 15% and carbon atom concentrations greater than 20%), the equilibrium shifts away from the desired work function and moves to the desired blocking capability. In the illustrated embodiment, the TiAlCN ratio includes a Ti:Al ratio that improves the interface quality (which may be referred to as wettability) between the multifunction barrier / wetting layer 242 and a overlying layer comprising aluminum. For example, the TiAlCN layer 242 includes a Ti:Al ratio of about 1:1 to about 1:3.The process used to form the multifunction barrier / wetting layer 242, here the TiAlCN layer, is adjusted to achieve optimal blocking and wettability functionality of the multifunction barrier / wetting layer 242. In the illustrated embodiment, physical vapor deposition (PVD) is used to form the multifunction barrier / wetting layer 242. Various process parameters of the PVD process, such as substrate temperature, gas type, gas flow, chamber pressure, DC current, matching current, processing time, other suitable parameters, or combinations thereof, are adjusted to achieve the desired blocking and wettability functionality. Alternatively, the multifunction barrier / wetting layer 242 is formed by other processes such as chemical vapor deposition (CVD), atomic layer deposition (ALD), plasma enhanced CVD (PECVD), remote plasma CVD (RPCVD), molecular organic CVD (MOCVD), sputtering, plating, other suitable method, or combinations thereof. Various process parameters of such alternative processes may be adjusted to achieve the desired blocking and wettability functionality of the multifunction barrier / wetting layer 242.In the illustrated embodiment, a high pressure PVD process that maintains the chamber pressure of about 13.3322 Pascals to about 666.612 Pascals deposits the multifunction barrier / wetting layer 242 at a temperature of about 250° C. to about 450° C. The high pressure PVD process may ensure that the multifunction barrier / wetting layer 242 fills the opening 240 sufficiently partially. The high pressure PVD process provides suitable coverage, for example, for high aspect ratio openings, such as opening 240. In the illustrated embodiment, high aspect ratio openings refer to openings having a height to width ratio greater than or equal to 2.2 (height / width>2.2). Alternatively, high aspect ratio openings may be defined by other height-to-width ratios.In another embodiment, the multifunction barrier / wetting layer 242 includes multiple TiAlCN layers of different N%. For example, a lower TiAlCN layer has a higher N%, such as from about 5% to about 15%, and an upper TiAlCN layer has a lower N%, such as from about 2% to about 5%. In this case, the lower TiAlCN layer serves mainly as a barrier layer, while the upper TiAlCN layer serves mainly as a work function layer. By selecting an appropriate C % and N %, an optimized blocking capability is achieved. In one example, C% is in a range from about 5% to about 20%, while N% is in a range from about 5% to 15%.In FIG. 5, a work function layer 244 is formed over the substrate 210 such that the work function layer 244 partially fills the opening 240. In the illustrated embodiment, the work function layer 244 is disposed over the multifunction barrier / wetting layer 242. In one example, the work function layer 244 has a thickness of about 3 nm to about 10 nm. In another example, the work function layer 244 disposed on the multifunction barrier / wetting layer 242 may have a thickness of about 3 nm to about 10 nm, and the work function layer 244 disposed along the sidewalls of the opening 240 may have a thickness less than 3 nm or a thickness of about 3 nm to about 10 nm. The work function layer 244 includes a material that can be adjusted to have a suitable work function for enhanced performance of the associated device. For example, in a p-type field effect transistor (PFET) device, work function layer 244 includes a p-type work function material that can be configured to have a desired work function value for the gate electrode of the PFET. In an n-type field effect transistor (NFET) device, on the other hand, work function layer 244 includes an n-type work function material (such as TiAlCN) that may be configured to have a desired work function value of the gate electrode of the NFET. The work function layer 244 is formed by physical vapor deposition (PVD), chemical vapor deposition (CVD), atomic layer deposition (ALD), plasma enhanced CVD (PECVD), remote plasma CVD (RPCVD), molecular organic CVD (MOCVD), sputtering, plating, other suitable methods, or combinations thereof.In example embodiments, work function layer 244 is an n-work function layer comprising TiAlCN. In the illustrated embodiment, the work function layer 244 comprises TiAlCN having a different composition than the TiAlCN in the multi-function barrier / wetting layer 242. For example, the nitrogen atom concentration in the work function layer 244 is lower than the nitrogen atom concentration in the multifunction barrier layer / wetting layer 242. The nitrogen atom concentration is selected to balance the blocking ability and the desired work function. In one embodiment, the nitrogen atom concentration in the work function layer 244 is about 2% up to about 5%. The aluminum in the work function layer 244 has high mobility and can easily penetrate into a lower layer when the nitrogen atom concentration is lower (e.g., less than about 2%). At higher nitrogen atom concentrations (e.g., greater than about 2%), the nitrogen in the work function layer 244 may bind to the aluminum, form a stable phase, and reduce penetration of aluminum into a bottom layer. However, even higher nitrogen atom concentrations (e.g., greater than about 5%) may cause a movement away from a desired or desired work function.In FIG. 6, a conductive layer 246 is formed over the substrate 210 such that the conductive layer 246 partially fills the opening 240. The conductive layer 246 is disposed over the work function layer 244. In an example, the conductive layer 246 has a thickness of about 30 nm to about 150 nm. In the illustrated embodiment, the conductive layer 246 comprises aluminum. Alternatively or additionally, the conductive layer 246 includes copper, tungsten, a metal alloy, a metallic silicide, another conductive material, or combinations thereof. The conductive layer 246 is formed by physical vapor deposition (PVD), chemical vapor deposition (CVD), atomic layer deposition (ALD), plasma enhanced CVD (PECVD), remote plasma CVD (RPCVD), molecular organic CVD (MOCVD), sputtering, plating, other suitable methods, or combinations thereof.In FIG. 7, a chemical mechanical polishing (CMP) process is performed until the dielectric layer 232 is reached or exposed. The CMP process therefore removes portions of the multifunction barrier / wetting layer 242, work function layer 244, and conductive layer 246 that are disposed over the dielectric layer 232. The remaining portions of the multifunction barrier / wetting layer 242, the work function layer 244, and the conductive layer 246 combine to fill the opening 240 such that the gate stack of the gate structure 220 includes the interlayer dielectric layer 222, the high-k dielectric layer 224, the multifunction barrier / wetting layer 242, the work function layer 244, and the conductive layer 246. The multifunction barrier / wetting layer 242, the work function layer 244, and the conductive layer 246 may collectively be referred to as a gate electrode of the gate structure 220.The integrated circuit 200 may include other features. For example, a multi-layer interconnect (MLI) including metal layers and inter-metal dielectric (IMD) layers may be formed over the substrate 210, such as over the dielectric layer 232, to electrically connect various elements or structures of the integrated circuit 200. The multi-layer interconnect includes vertical interconnects such as vias or contacts and horizontal interconnects such as metal traces. In an example, the MLI interconnects to the source / drain elements 230 and / or the gate stack of the gate structure 220. The various interconnect elements include various conductive materials including aluminum, copper, titanium, tungsten, alloys thereof, silicide materials, other suitable materials, or combinations thereof. In one example, a damascene process or dual damascene process is used to form a multi-layer copper or aluminum interconnect structure.The integrated circuit 200 has a reduced leakage current, which leads to an improved operating behavior of the component. Such reduced leakage current and improved device performance may be achieved by the multifunction barrier / wetting layer 242 in the gate stack of the gate structure 220. The multi-function barrier / wetting layer 242 can sufficiently block metal contaminants from entering underlying dielectric layers while providing sufficient wettability (barrier quality) to overlying layers.A conventional gate stack includes a gate dielectric layer, a work function layer disposed over the gate dielectric layer; a barrier layer such as a tantalum nitride (TaN) barrier layer disposed over the work function layer; a wetting layer such as a titanium (Ti) wetting layer disposed over the barrier layer; and a conductive layer such as an aluminum (Al) conductive layer disposed over the wetting layer. The TaN barrier layer provides a barrier capability that is less than desirable, and it has been observed that aluminum contaminants from the conductive aluminum layer may penetrate into the gate dielectric layer during processing. Further, although the Ti wetting layer provides sufficient wettability to the Al conductive layer, it has been observed that phase transformations occur between the Ti wetting layer and the Al conductive layer during processing, resulting in portions of the TaN barrier layer interacting with Ti during processing, and ultimately resulting in missing portions of the TaN barrier layer (in other words, portions of the TaN barrier layer are consumed during processing). The missing portions of the TaN barrier layer further minimize the ability of the TaN barrier layer to prevent aluminum contaminants from entering the gate dielectric layer. Such phase transformations and missing portions of the TaN barrier layer were also observed when the gate stack comprises a titanium aluminum (TiAl) wetting layer.To address these problems, the present disclosure replaces the separate TaN barrier layer and the Ti wetting layer of conventional gate stacks with the TiAlCN multifunction barrier / wetting layer 242. The blocking ability of TiAlCN exceeds the blocking ability of TiN and TaN (specifically, the blocking ability of TiAlCN>TiAlC>TiN>>TaN). Further, TiAlCN provides sufficient wettability to an Al conductive layer. Accordingly, the TiAlCN multifunction barrier / wetting layer provides improved barrierability and wettability, resulting in reduced leakage current and improved device performance compared to gate stacks comprising a conventional TaN barrier / Ti wetting layer. Different embodiments may have different advantages and no particular advantage is necessarily required of any embodiment.The present invention relates to an integrated circuit comprising a semiconductor substrate and a gate stack arranged over the semiconductor substrate. The gate stack includes a gate dielectric layer disposed over the semiconductor substrate, a multifunction barrier / wetting layer disposed over the gate dielectric layer, a work function layer disposed over the multifunction barrier / wetting layer, the work function layer including TiAlCN having a nitrogen atom concentration of about 2% up to about 5%, and a conductive layer disposed over the work function layer. The multifunction barrier layer / wetting layer comprises titanium aluminum carbonitride (TiAlCN), wherein the multifunction barrier layer / wetting layer comprises multiple TiAlCN layers with different nitrogen atom concentrations, wherein the multifunction barrier layer / wetting layer comprises a lower TiAlCN layer and an upper TiAlCN layer, wherein the lower TiAlCN layer has a higher nitrogen atom concentration than the upper TiAlCN layer. The integrated circuit further includes spacer elements adjacent sidewalls of the gate stack, wherein the multi-function barrier / wetting layer directly adjoins the spacer elements and the gate dielectric layer.The invention further relates to an integrated circuit comprising a gate stack arranged over a semiconductor substrate. The gate stack includes a high-k dielectric layer disposed over the semiconductor substrate, a first titanium aluminum carbonitride (TiAlCN) layer disposed directly on the high-k dielectric layer, wherein the nitrogen atom concentration of the first TiAlCN layer decreases from bottom to top, a second TiAlCN layer disposed directly on the first TiAlCN layer, wherein the second TiAlCN layer has a nitrogen atom concentration of about 2% to about 5%, and an aluminum layer disposed directly on the second TiAlCN layer. The integrated circuit further includes spacers adjacent sidewalls of the gate stack, wherein the first TiAlCN layer directly abuts the spacers.The invention further relates to a method comprising forming a gate structure over a semiconductor substrate, removing the dummy gate from the gate structure and thereby forming an opening, and forming a multifunction barrier / wetting layer over the high-k dielectric layer and along the sidewalls of the gate structure (220) defining the opening 240, a work function layer over the multifunction barrier / wetting layer, and a conductive layer over the work layer. The multifunction barrier / wetting layer, the work function layer and the conductive layer fill the opening. The multifunction barrier / wetting layer comprises titanium aluminum carbonitride (TiAlCN) and multiple TiAlCN layers with different nitrogen concentrations, wherein the multifunction barrier / wetting layer (242) comprises a lower TiAlCN layer and an upper TiAlCN layer, wherein the lower TiAlCN layer has a higher nitrogen concentration than the upper TiAlCN layer. The work function layer comprises TiAlCN having a nitrogen atom concentration of from about 2% up to about 5%.
Claims
An integrated circuit (200) comprising: a semiconductor substrate (210); and a gate stack disposed over the semiconductor substrate (210), the gate stack comprising: a gate dielectric layer (224) disposed over the semiconductor substrate (210); a multifunction barrier / wetting layer (242) disposed over the gate dielectric layer (224), the multifunction barrier / wetting layer (242) comprising TiAlCN, the multifunction barrier / wetting layer (242) comprising a plurality of TiAlCN layers having different nitrogen concentrations, the multifunction barrier / wetting layer (242) comprising a lower TiAlCN layer and an upper TiAlCN layer, the lower TiAlCN layer having a higher nitrogen concentration than the upper TiAlCN layer; a work function layer (244) disposed over the multifunction barrier / wetting layer (242), the work function layer (244) comprising TiAlCN having a nitrogen atom concentration of 2% up to 5%; and a conductive layer (246) disposed over the work function layer (244); and spacer elements (228) adjacent sidewalls of the gate stack, the multifunction barrier / wetting layer (242) directly adjacent the spacer elements (228) and the gate dielectric layer (224).The integrated circuit (200) of claim 1, wherein the gate dielectric layer (224) comprises a high-k dielectric layer (224).The integrated circuit (200) of claim 2, wherein the gate dielectric layer (224) comprises an interlayer dielectric layer (222) disposed between the high-k dielectric layer (224) and the semiconductor substrate (210).The integrated circuit (200) of claim 1, wherein the multifunction barrier / wetting layer (242) has a nitrogen atom concentration and carbon atom concentration that prevent metal contaminants from entering the gate dielectric layer (224).The integrated circuit (200) of claim 4, wherein the nitrogen atom concentration is 5% up to 15% and the carbon atom concentration is 5% up to 20%.The integrated circuit (200) of claim 1, wherein the multifunction barrier / wetting layer (242) has a Ti:Al ratio of 1:1 to 1:3.An integrated circuit (200) comprising a gate stack disposed over a semiconductor substrate (210), the gate stack comprising: a high-k dielectric layer (224) disposed over the semiconductor substrate (210); a first TiAlCN layer (242) disposed directly on the high-k dielectric layer (224), wherein the nitrogen atom concentration of the first TiAlCN layer decreases from bottom to top; a second TiAlCN layer (244) disposed directly on the first TiAlCN layer (242), wherein the second TiAlCN layer (244) has a nitrogen atom concentration of 2% to 5%; and an aluminum layer (246) disposed directly on the second TiAlCN layer (244), the integrated circuit (200) further comprising spacers (228) adjacent sidewalls of the gate stack, the first TiAlCN layer (242) directly adjacent the spacers (228).The integrated circuit of claim 7, wherein the first TiAlCN layer has a nitrogen atom concentration of 5% to 15% and a carbon atom concentration of 5% to 20% and a Ti:Al ratio of 1:1 to 1:3.The integrated circuit (200) of claim 7, wherein the gate stack is between a source element and a drain element disposed in the semiconductor substrate (210).The integrated circuit (200) of claim 7, wherein the gate stack further comprises an interlayer dielectric layer (222) disposed between the high-k dielectric layer (224) and the (210) semiconductor substrate.The integrated circuit of any of claims 7 to 10, wherein the first TiAlCN layer (242), the second TiAlCN layer (244), and the aluminum layer (246) extend to a top surface of the gate stack.The integrated circuit of any of claims 7 to 11, wherein the first TiAlCN layer (242) has an opening formed therein, in which the second TiAlCN layer (244) and the aluminum layer (246) are disposed.The integrated circuit of any of claims 7 to 12, wherein the high-k dielectric layer (224) and the first TiAlCN layer (242) have a planar interface extending from a first sidewall of the opposing spacers to a second sidewall of the opposing spacers.The integrated circuit of any of claims 7 to 13, wherein the second TiAlCN layer (244) has a thickness of 3 nm to 10 nm.A method comprising: forming a gate structure (220) over a semiconductor substrate (210), the gate structure (220) having a gate stack comprising a high-k dielectric layer (224) disposed over the semiconductor substrate (210) and a dummy gate (226) disposed over the high-k dielectric layer (224); removing the dummy gate (226) from the gate structure (220) thereby forming an opening (240); and forming a multifunction barrier / wetting layer (242) directly over the high-k dielectric layer (224) and along the sidewalls of the gate structure (220) defining the opening 240, a work function layer (244) over the multifunction barrier / wetting layer (242), and a conductive layer (246) over the work function layer (244), wherein the multifunction barrier / wetting layer (242), the work function layer (244), and the conductive layer (246) fill the opening (240), and further wherein the multifunction barrier / wetting layer (242) comprises TiAlCN, wherein the multifunction barrier / wetting layer (242) comprises a plurality of TiAlCN layers having different nitrogen concentrations, wherein the multifunction barrier / wetting layer (242) comprises a lower TiAlCN layer and an upper TiAlCN layer, wherein the lower TiAlCN layer has a higher nitrogen concentration than the upper TiAlCN layer, wherein the work function layer (244) comprises TiAlCN and the TiAlCN in the work function layer (244) has a nitrogen atom concentration of 2% up to 5%.The method of claim 15, wherein forming the multi-function barrier / wetting layer (242) comprises performing a PVD process.The method of claim 16, wherein performing the PVD process comprises adjusting the PVD process such that the multifunction barrier / wetting layer (242) has a nitrogen atom concentration of 5% to 15% and a carbon atom concentration of 5% to 20%.The method of claim 16, wherein performing the PVD process comprises adjusting the PVD process such that the multi-function barrier layer / wetting layer (242) has a Ti:Al ratio of 1:1 to 1:3.The method of any of claims 16 to 18, wherein the PVD process is a high pressure PVD process in which the chamber pressure is between 13.3322 Pascal and 666.612 Pascal.The method of any of claims 16 to 19, wherein the multifunctional barrier / wetting layer (242) is deposited at a temperature between 250°C and 450°C.
Citation Information
Patent Citations
Method for forming aluminum-doped metal carbonitride gate electrodes
DE112009002118T5
Multi-layer scavenging metal gate stack for ultra-thin interfacial dielctric layer
US20130075833A1
Methods for fabricating integrated circuits having low resistance metal gate structures
US20140154877A1