METHOD FOR PROCESSING A WAFER

DE102017215047B4Inactive Publication Date: 2024-10-31DISCO CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
DE102017215047
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2016-09-09
Filing Date
2017-08-29
Publication Date
2024-10-31
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A method for processing a wafer having on one face side a component area with several components formed therein and an outer circumferential additional area surrounding the component area, comprising: a first grinding step for grinding a rear face of the wafer corresponding to the component area with a grinding wheel whose diameter is smaller than the wafer, forming a first section corresponding to the component area and an annular second section surrounding the first section, the second annular section being thicker than the first section and projecting further towards a rear face therein than the first section; a second grinding step for further grinding using a grinding wheel different from the grinding wheel used in the first grinding step, forming a depression.which has a smoother bottom surface than the rear side of the first section, wherein in the first grinding step the grinding wheel and the wafer are moved relative to each other, such that when the grinding wheel rises after being lowered vertically to grind the wafer, the grinding wheel and the wafer are moved relative to each other along a direction inclined to the horizontal and vertical directions, such that an angle formed between the rear side of the first section and an inner side surface of the second annular section is greater than 45° and less than 75°.
Need to check novelty before this filing date? Find Prior Art

Description

Technical FieldThe present invention relates to a wafer and a method for processing a wafer.Description of the Prior ArtIn the past, it has been necessary to process a wafer made of a material such as silicon, gallium arsenide, or the like into a thin profile in order to realize small and light-weight device chips. Specifically, after devices such as integrated circuits (ICs) or the like are formed in respective regions separated by projected dicing lines or streets on the surface side of a wafer, the back side of the wafer W is ground until the wafer is thinned to a desired thickness. If a wafer is made thin by grinding or the like, the strength of the wafer will decrease massively, making it difficult to handle the wafer in the subsequent steps. With this difficulty in mind, a processing method has been proposed in which only the central portion of a wafer having devices formed thereon is ground to keep the wafer thick in an outer circumferential portion thereof, whereby the ground wafer remains fixed to a certain degree (see, for example, JP 2007-19 461 A According to a proposed method, the back side of the wafer is ground using a grinding wheel smaller in diameter than the wafer, whereby a central portion of the wafer is made thin. The strength of the wafer is secured by the outer peripheral portion thereof, the thickness of which is maintained. The outer peripheral portion is subsequently separated and removed by irradiating the boundary between the outer peripheral portion and the central portion with a laser beam (see, for example, JP 2008-53 341 AIf the rear side of the central portion of the wafer and an inner side surface of the outer peripheral portion, i.e., a side surface near the central portion of the wafer, are perpendicular to each other due to grinding of the rear side of the central portion of the wafer, the edge of the inner side surface of the outer peripheral portion tends to chip off during subsequent handling of the wafer. When the wafer on which the edge of the inner side surface of the outer peripheral portion is peeled off is treated by etching or the like, the outer peripheral portion is progressively peeled off from the peeled edge and becomes brittle and fragile. Moreover, the inner side surface of the outer peripheral portion, which is perpendicular to the rear side of the central portion of the wafer, makes it difficult for chemicals used in various processing steps, for example, a resist solution used to form a distribution layer, to be discharged from the wafer. Due to these problems, a processing method for inclining the inner side surface of the outer peripheral portion of a wafer with respect to the rear side of the central portion of the wafer has recently been proposed (see, for example, JP 2011-54 808 A.SUMMARY OF THE INVENTIONHowever, an inclination of the inner side surface of the outer peripheral portion with respect to the rear side of the central portion may result in the central portion being reduced to such an extent that the wafer does not provide enough space required to form devices thereon. In addition, the edge of the inner side surface of the outer peripheral portion is further likely to chip off by contact with grinding stones or the like used to grind the wafer.It is an object of the present invention to provide a method of processing a wafer in a manner that prevents parts from chipping off the wafer while maintaining a wide range for forming devices in the wafer, and a wafer processed by a method of processing the wafer.An aspect of the present invention is a method of processing a wafer having, on a surface side thereof, a device region having a plurality of devices formed therein and an outer peripheral additional region surrounding the device region, comprising:a first grinding step of grinding a rear side of the wafer corresponding to the device region with a grinding wheel smaller in diameter than the wafer, thereby forming a first portion corresponding to the device region and an annular second portion surrounding the first portion, the second annular portion being thicker than the first portion and protruding further toward a rear side thereof than the first portion,a second grinding step for further grinding using a grinding wheel different from the grinding wheel used in the first grinding step, thereby forming a recess having a smoother bottom surface than the rear side of the first portion,wherein, in the first grinding step, the grinding wheel and the wafer are moved relative to each other such that when the grinding wheel rises after being vertically lowered to grind the wafer, the grinding wheel and the wafer are moved relative to each other along a direction inclined to the horizontal and vertical directions such that an angle formed between the rear side of the first portion and an inner side surface of the second annular portion is greater than 45° and less than 75°.According to another aspect of the present invention, in the grinding step, the grinding wheel and the wafer should preferably be moved relative to each other so that the angle formed between the rear side of the first portion and the inner side surface of the annular second portion is equal to or greater than 55° and equal to or less than 70°.With the method of processing a wafer according to aspects of the present invention, since the angle formed between the rear side of the first portion and the inner side surface of the annular second portion is greater than 45° and less than 75°, the wafer is prevented from chipping off while a wide range of the first portion corresponding to the device region is maintained.The above object and other objects, features and advantages of the present invention and the manner of realizing them will become clearer, and the invention itself will best be understood by studying the following description and appended claims with reference to the appended figures showing a preferred embodiment of the invention.BRIEF DESCRIPTION OF THE FIGURESFIG. 1A is a schematic perspective view of a wafer to be processed by a method of processing a wafer according to an embodiment of the present invention; FIG. 1B is a schematic perspective view showing a protective member applying step; FIG. 2A is a side elevational view, partially in cross section, schematically illustrating a first grinding step; FIG. 2B is a side elevational view, partially in cross section, schematically illustrating the wafer being treated in the first grinding step; FIG. 3A is a side elevational view, partially in cross section, schematically illustrating a second grinding step; FIG. 3B is a side elevational view, partly in cross section, schematically illustrating the wafer after being processed in the second grinding step; and FIG. 4 is a graph schematically illustrating the result of an experiment performed on wafers.DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTA method of processing a wafer according to a preferred embodiment of the present invention will be described in detail below with reference to the figures. The method for processing a wafer according to the present invention includes a protective member applying step (see FIG. 1B ), a first grinding step (see FIGS. 2A and 2B ), and a second grinding step (see FIGS. 3A and 3B ). In the protective member applying step, a protective member is applied to the surface side of a wafer including a device region on which a plurality of devices are formed and an outer peripheral additional region surrounding the device region. In the first grinding step, the back side of the wafer corresponding to the device region is ground using a grinding wheel smaller than the diameter of the wafer, thereby forming a first portion and a thick second portion surrounding the first portion. In the first grinding step, the grinding wheel is moved relative to the wafer so that an angle greater than 45° and less than 75° is formed between the rear side of the first portion and an inner side surface of the second portion. In the second grinding step, the rear side of the first portion is further ground using a grinding wheel different from the grinding wheel used in the first grinding step. The method for processing a wafer according to the present invention will be described in detail below.FIG. 1A schematically illustrates, in perspective, a wafer 11 to be processed by the method for processing a wafer according to the present embodiment. As illustrated in FIG. 1A, the wafer 11 to be processed according to the present embodiment has a disc shape, is formed of a semiconductor material such as silicon (Si), gallium arsenide (GaAs), or the like. The wafer 11 has a face side 11 aseparated into a central device region and an outer peripheral additional region surrounding the device region. The device area is divided into a plurality of areas by a grid-like array of projected division lines or streets 13, where devices 15 such as ICs, large scale integration (LSIs), circuits, etc. are formed in the respective areas. According to the present embodiment, the wafer 11 is disc-shaped and formed of a semiconductor material. However, the wafer 11 is not limited to materials, shapes, and configurations, etc. The wafer 11 may be formed of, for example, ceramics, metal, plastic, or the like. Similarly, the constituent elements 15 are not limited to a type, number, and arrangement.In the method for processing a wafer according to the present embodiment, the protective member applying step is performed to apply a protective member 21 to the surface 11 aof the wafer 11. FIG. 1B schematically illustrates the protective element applying step in perspective. The protection member 21 includes, for example, a circular film or circular tape having the same diameter as the wafer 11 and having an adhesion promoting layer having an adhesion promoting force on its surface side 21 a. When the face side 21 aof the protection member 21 is brought into close contact with the face side 11 aof the wafer 11, the protection member 21 is mounted on the wafer 11. The protection member 21 applied to the wafer 11 is effective to attenuate impacts applied to the wafer 11 in the first grinding step in the second grinding step, thereby protecting the devices 15 on the surface 11 aof the wafer 11, for example.The protective member applying step is followed by the first grinding step in which the back side 11 bof the wafer 11 corresponding to the device region is ground to form a thin first portion and a thick second portion surrounding the first portion. FIG. 2A schematically illustrates the first grinding step in a side plan view, partially in cross section. FIG. 2B schematically illustrates the wafer 11 after being ground in the first grinding step, in a side plan view, partially in cross section. The first grinding step is performed using a grinding apparatus 2 illustrated in FIG. 2A, for example. The grinding apparatus 2 includes a chuck table 4 for holding the wafer 11 under suction. The chuck table 4 is coupled to a rotational drive source, not illustrated, including a motor, etc., and is rotatable about a rotational axis extending substantially parallel to vertical directions. The grinding apparatus 2 also includes a moving mechanism, not illustrated, disposed below the chuck table 4 to move the chuck table 4 in horizontal and vertical directions. The chuck table 4 has a surface serving as a holding surface 4 afor holding the rear side 21 bof the protective member 21 attached to the wafer 11 under suction. The holding surface 4 ais connected to a suction source, which is not illustrated, through a suction channel, which is not illustrated, formed in the chuck table 4. The wafer 11 is held under suction on the chuck table 4 by the protective member 21 when the suction source applies a negative pressure to the holding surface 4 a.The grinding apparatus 2 also includes a first grinding unit 6 disposed above the chuck table 4. The first grinding unit 6 includes a spindle housing, not illustrated, supported by a moving mechanism, not illustrated. The spindle housing is horizontally and vertically movable by a moving mechanism. The spindle housing houses a spindle 8 having a lower end to which a disk-shaped fastener 10 is fixed. The first grinding unit 6 includes a grinding wheel 12 fixed to the lower surface of the mount 10 and having substantially the same diameter as the mount 10. The grinding wheel 12 includes a wheel base 14 formed of a metal material such as stainless steel, aluminum, or the like, and a plurality of grinding stones 16 arranged in an annular pattern on the lower surface of the wheel base 14. The spindle 8 has an upper proximal end coupled to a rotational drive source, which is not illustrated, such as a motor or the like. The grinding wheel 12 is rotatable about a rotation axis extending substantially parallel to vertical directions by a rotational power generated by the rotational drive source. Nozzles, not illustrated, for supplying a grinding liquid such as pure water or the like to the wafer 11 are provided in or near the first grinding unit 6.In the first grinding step, the rear side 21 bof the protective member 21 mounted on the wafer 11 is brought into contact with the holding surface 4 aof the chuck table 4, and thereafter the suction source applies a negative pressure to the holding surface 4 a. The wafer 11 is now held on the chuck table 4 under suction with the back side 11b exposed upward. Thereafter, the chuck table 4 is moved to a position below the first grinding unit 6, and the grinding wheel 12 brings its end, i.e., an outer side surface of the annular array of grinding stones 16, into alignment with the boundary between the component area and the additional outer peripheral area. As shown in FIG. 2A, the chuck table 4 and the grinding wheel 12 are rotated about their axis, and while the grinding liquid is supplied to the rear side 11 bof the wafer 11, the spindle housing and thus the spindle 8 and the grinding wheel 12 are lowered. The rate of lowering of the spindle case, i.e., the distance at which the spindle case is lowered, is adjusted so that the lower surface of the grinding stones 16 is pressed against the back side 11 bof the wafer 11. Simultaneously, the spindle housing and thus the spindle 8 and the grinding wheel 12 are moved horizontally to the center of the wafer 11. In other words, the grinding wheel 12 and the wafer 11 are moved relative to each other along a direction oblique to the horizontal and vertical directions.In this manner, the back side 11 bof the wafer 11 corresponding to the device region is ground to form a first thin portion 11 ccorresponding to the device region and a thick second portion 11 dcorresponding to the outer peripheral additional region, as illustrated in FIG. 2B. The second portion 11 dis annular, surrounds the first portion 11 c, and protrudes further toward the rear side 11 bof the wafer 11 than the first portion 11 c. The first portion 11c has a rear side 11e and the second portion 11d has an inner side surface 11f, i.e., a side surface near the first portion 11c. The rear side 11 eand the inner side surface 11 fform an angle θ therebetween depending on the relative movement of the grinding wheel 12 and the wafer 11. If the angle θ is 75° or greater, the edge of the inner side surface 11 fof the second portion 11 dis more likely to chip off. If the angle θ is 45° or less, the distance that the grinding wheel 12 and the wafer 11 are relatively moved horizontally in grinding the wafer 11 is increased, thereby making it difficult to sufficiently configure the first portion 11 ccorresponding to the device area. According to the present embodiment, the angle θ is set to a value greater than 45° and less than 75°. Preferably, the angle θ should be set to a value equal to or greater than 55° and set to be equal to or less than 70°. Setting the angle makes it possible to sufficiently configure the first portion 11 cand prevent the edge of the inner side surface 11 ffrom chipping off. The first grinding step is followed by the second grinding step in which the rear side 11 eof the first portion 11 cis further ground using a grinding wheel different from the grinding wheel 12 in the first grinding step. FIG. 3A shows the second grinding step in a side view, partly in cross section. FIG. 3B schematically illustrates the wafer 11 after being ground in the second grinding step, in a side plan view, partially in cross section. The second grinding step is further performed using the grinding apparatus 2. As illustrated in FIG. 3A, the grinding apparatus 2 includes a second grinding unit 26 different from the first grinding unit 6 provided above the chuck table 4. The second grinding unit 26 is structurally similar to the first grinding unit 6. the second grinding unit 26 includes a spindle housing, not illustrated, supported by a moving mechanism, not illustrated. The spindle housing is horizontally and vertically movable by the moving mechanism. The spindle housing houses a spindle 28 having a lower end to which a disk-shaped fastener 30 is fixed. The second grinding unit 26 also includes a grinding wheel 32 mounted on the lower surface of the mount 30, and has substantially the same diameter as the mount 30. The grinding wheel 32 includes a wheel base 34 formed of a metal material such as stainless steel, aluminum, or the like, and a plurality of grinding stones 36 arranged in an annular pattern on the lower surface of the wheel base 34. The grinding stones 36 include abrasive grains smaller than those of the grinding stones 16 of the first grinding unit 6. The spindle 28 has an upper proximal end coupled to a rotational drive source, not shown, such as a motor or the like. The grinding wheel 32 can be rotated about a rotation axis extending substantially parallel to vertical directions by a rotational power generated by the rotational drive source. Nozzles, not shown, for supplying a grinding liquid such as pure water or the like to the wafer 11 are provided in or near the second grinding unit 26.In the second grinding step, the chuck table 4 is moved to a position below the second grinding unit 26, and the grinding wheel 32 brings its end, i.e., an outer side surface of the annular array of the grinding stones 36, radially inward from the inner side surface 11 fof the second portion 11 d. Thereafter, as shown in FIG. 3A, the chuck table 4 and the grinding wheel 32 are rotated about their axis, and while the grinding liquid is supplied to the rear side 11 bof the wafer 11, the spindle housing, and thus the spindle 28 and the grinding wheel 32, are lowered. The rate of lowering the spindle housing, i.e., the distance the spindle housing is lowered, is adjusted so that the lower surfaces of the grinding stones 36 are pressed against the rear side 11 bof the first portion 11 c. In this manner, the first portion 11 cof the wafer 11 is further ground to form a recess 11 gthereof having a smoother bottom surface than the back side 11 bas illustrated in FIG. 3B.An experiment performed to confirm the effectiveness of the method for processing a wafer according to the present embodiment will be described below. In this experiment, a plurality of wafers processed in the first grinding step having different angles θ in the range of 30° to 90° are prepared. Grinding conditions except for the angles θ for the first grinding step are given below. In the experiment, the rate of lowering the grinding wheel in actually grinding the wafer in three stages, i.e., a 1-3. The speed is changed. Rotational speed of the spindle: 4500 revolutions / min Rotational speed of the chuck table: 300 revolutions / min Rate of lowering of the grinding wheel (first speed): 6 μm / s Rate of lowering of the grinding wheel (second speed): 3 μm / s Rate of lowering of the grinding wheel (third speed): 1 μm / s Feed rate of a grinding liquid (first nozzle): 4 l / min Feed rate of a grinding liquid (second nozzle) 3 l / minThereafter, the number of chippings on each of the wafers was confirmed. FIG. 4 is a graph illustrating the result of the experiment performed on the wafers. In FIG. 4, the horizontal axis represents the values of the angle θ and the vertical axis represents the number of chippings, so that the graph represents the relationship between the angle θ and the number of chippings whose size is 100 μm or more. As illustrated in FIG. 4, if the angle θ exceeds 70° and reaches 75°, the number of chippings increases significantly. Therefore, the value of the angle θ should be less than 75°, and preferably, it should be equal to or less than 70°. If the value of the angle θ is too small, the first portion corresponding to the device area may not be sufficiently large. Accordingly, the value of the angle θ should be greater than 45°, and preferably 55° or greater.With the method of processing a wafer, since the angle formed between the rear side 11 eof the first portion 11 cand the inner side surface 11 fof the second portion 11 dis greater than 45° and less than 75°, parts of the wafer are prevented from chipping off while a wide range for the first portion 11 ccorresponding to the device area is maintained.According to the present invention, when the grinding wheel 12 rises after being vertically lowered to grind the wafer 11, the grinding wheel 12 and the wafer 11 can be moved relative to each other along a direction inclined to the horizontal and vertical directions, thereby forming the angle θ.In the above embodiment, the protective member applying step and the second grinding step are additionally performed. In other words, the protective member applying step may be omitted if not needed.In the second grinding step according to the above embodiment, the grinding wheel 32 and the wafer 11 are moved relative to each other in a vertical direction. However, in the second grinding step, the grinding wheel 32 and the wafer 11 may be moved relative to each other along a direction inclined to the horizontal and vertical directions.

Claims

A method for processing a wafer having, on a surface side thereof, a device region having a plurality of devices formed therein and an outer peripheral additional region surrounding the device region, comprising: a first grinding step of grinding a rear side of the wafer corresponding to the device region with a grinding wheel smaller in diameter than the wafer, thereby forming a first portion corresponding to the device region and an annular second portion surrounding the first portion, the second annular portion being thicker than the first portion and projecting further toward a rear side thereof than the first portion, a second grinding step of further grinding using a grinding wheel different from the grinding wheel used in the first grinding step, thereby forming a recess, The grinding wheel has a smoother bottom surface than the rear side of the first portion, wherein in the first grinding step, the grinding wheel and the wafer are moved relative to each other, so that when the grinding wheel rises after being vertically lowered to grind the wafer, the grinding wheel and the wafer are moved relative to each other along a direction inclined to the horizontal and vertical directions, so that an angle formed between the rear side of the first portion and an inner side surface of the second annular portion is greater than 45° and less than 75°.The method for processing a wafer according to claim 1, wherein in the first grinding step, the grinding wheel and the wafer are moved relative to each other such that the angle formed between the rear side of the first portion and the inner side surface of the annular second portion is equal to or greater than 55° and equal to or less than 70°.The method for processing a wafer according to claim 1 or 2, wherein in the second grinding step, the grinding wheel and the wafer are moved relative to each other only in the vertical direction.The method for processing a wafer according to claim 1 or 2, wherein in the second grinding step, the grinding wheel and the wafer are moved relative to each other along a direction inclined to the horizontal and vertical directions.

Citation Information

Patent Citations

  • Method for processing wafer and wafer

    JP2007019461A

  • Wafer processing method

    JP2008053341A

  • Method of processing wafer, and wafer processed by the same

    JP2011054808A

  • Single-stage wafer and process for producing a single-stage wafer

    DE112015006676T5

  • Process of forming ultra thin wafers having an edge support ring

    US20090020854A1