PROCESSING METHOD FOR A WAFER
The use of a carbon black-containing sealing member for WL-CSP wafers allows accurate alignment and cutting by infrared imaging, addressing alignment inaccuracies and protecting semiconductor components in WL-CSP manufacturing.
Patent Information
- Application Number
- DE102018215820
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2017-09-19
- Filing Date
- 2018-09-18
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2038-09-18
AI Technical Summary
Existing wafer-level Chip Size Package (WL-CSP) manufacturing methods face inaccuracies in aligning cutting blades due to low accuracy of electrode bumps or printed targets on the wafer's plastic surface, leading to potential offset cutting and damage to semiconductor components.
A processing method using a sealing member containing carbon black, allowing alignment through infrared imaging to detect alignment marks beneath the sealing member, followed by laser processing along the detected lines to divide the wafer accurately.
Enables precise alignment and cutting of WL-CSP wafers without exposing the device pattern, reducing the risk of offset cuts and protecting semiconductor components.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Technical field
[0001] The present invention relates to a processing method for a WL-CSP wafer. Description of the state of the art
[0002] A WL-CSP (wafer-level chip size package) wafer is a technology for sealing the wafer after a wiring layer and electrodes (metal pins) have been formed. While the WL-CSP wafer is in a wafer state, its front surface is covered with plastic, and portions of the wafer are cut into components using a cutting blade or similar device. Because the size of the packages obtained by cutting the wafer is equivalent to the size of the semiconductor device chips, the technology is widely adapted for reducing size and weight.
[0003] In the manufacturing process of the WL-CSP wafer, a wiring layer is formed on a component face of a component wafer on which several components are formed, and metal pins connected to electrodes in components are formed through the wiring layer, and then the metal pins and the components are sealed with plastic.
[0004] A sealing element is then made thin so that the metal pins are exposed on the front surface of the sealing element, and external connections, called electrode protrusions, are formed on one end face of the metal pins. The WL-CSP wafer is then cut by a cutting device or similar instrument to divide it into individual CSPs.
[0005] To protect semiconductor devices from impact, moisture, or similar hazards, it is important to seal them with a sealing element. Typically, a sealing material is created by mixing a SiC filler into an epoxy resin, ensuring that the coefficient of thermal expansion of the sealing element is close to that of the semiconductor chips. This prevents damage to the packings during heating, which would otherwise be caused by a difference in their coefficients of thermal expansion.
[0006] A WL-CSP wafer is generally divided into individual CSPs using a cutting device. In this case, because a component used to detect a planned division line within the WL-CSP wafer is covered with plastic, a target pattern of the component cannot be detected from the front surface.
[0007] Therefore, alignment of the planned parting line and the cutting blade must be carried out by indexing the planned parting line, setting the electrode protrusions formed on the plastic of the WL-CSP wafer as a target, or by printing a target for alignment on the top surface of the plastic.
[0008] However, the electrode protrusions or the target printed on the plastic are not formed with the same high accuracy as the components, resulting in a problem where the target has low accuracy for alignment. In cases where a planned parting line is indicated based on electrode protrusions or a printed target, there is a possibility that a cutting point will be offset from the planned parting line, resulting in a component section being cut. Therefore, for example, Japanese patent application JP 2013-74 021 A proposes a method whereby alignment is performed based on a pattern of the component wafer exposed in an external environment of the wafer.
[0009] JP 2017-64746A relates to a laser processing device and a laser processing method. JP 2016-15438A relates to an alignment method. US 2014 / 0295643A1 relates to a wafer processing method. JP 2015-28980A relates to a wafer processing method. PRESENTATION OF THE INVENTION
[0010] However, in general, component accuracy on the outer environment of the wafer is somewhat inaccurate, and if alignment is performed based on a pattern exposed on the outer environment of the wafer, there is a possibility that the wafer will be split at a position offset from a planned split line, and furthermore, depending on the wafer, a pattern of the component may not be exposed on the outer environment.
[0011] Therefore, an objective of the present invention is to provide a processing method for a wafer by which an alignment step can be carried out by means of a sealing element that covers the front surface of the wafer and contains carbon black.
[0012] In accordance with one aspect of the present invention, a processing method for a wafer is provided, wherein a front surface of the wafer, on which a component is formed in each chip area divided by several planned division lines formed in an intersecting relationship on the front surface of the wafer, is sealed with a sealing element, and wherein several raised areas are individually formed in the chip areas of the sealing element, the processing method comprising an alignment step for acquiring an image of a front surface of the wafer through the sealing material with an infrared imaging means from the front surface of the wafer to detect alignment marks, and detecting a planned division line to be laser-processed based on the alignment marks.A training step for a modified layer for positioning, after the alignment step has been performed; a focal point of a laser beam of a wavelength that can pass through the wafer and the sealing element, in an interior of the wafer or the sealing element; and irradiation of the laser beam along the planned division line from the front surface of the wafer to form a modified layer in the interior of the wafer and the sealing element; and a division step for applying, after the training step for a modified layer has been performed, an external force on the wafer and the sealing element to divide the wafer from a division start point given by the modified layer into individual device chips, each sealed with the sealing element. The sealing element contains carbon black of 0.1 to 0.2% by mass and exhibits such transparency that infrared rays intended to be received by the infrared imaging device pass through the sealing element.
[0013] Preferably, the infrared imaging means used in the alignment step is an InGaAs image acquisition element.
[0014] According to the processing method for the wafer of the present embodiment, the front surface of the wafer is sealed with the sealing element, through which infrared rays, to be received by the infrared imaging device, pass, and the alignment marks formed on the wafer are detected by the sealing element with an infrared imaging device, so that alignment can be carried out based on the alignment marks. Therefore, the alignment step can be carried out easily without removing the sealing element from the outer circumferential section of the front surface of the wafer, as in the prior art.
[0015] Therefore, it is possible to place a focal point of the laser beam of a wavelength that can pass through the wafer and the sealing element inside the wafer or the sealing element, to irradiate the laser beam from the front surface of the wafer in this state to form the modified layer inside the wafer and the sealing element, and to divide the wafer into the individual component chips whose surface is sealed with the sealing element, from a division start point given by the modified layer.
[0016] The above and other aims, features and advantages of the present invention and the way in which they are realized will be made clearer and the invention itself best understood by studying the following description and the attached claims with reference to the attached figures which show a preferred embodiment of the invention. BRIEF DESCRIPTION OF THE FIGURES Fig. 1A is a perspective exploded view of a WL-CSP wafer; Fig. Figure 1B is a perspective view of the WL-CSP wafer; Fig. Figure 2 is an enlarged cross-sectional view of the WL-CSP wafer; Fig. Figure 3 is a perspective view showing a way in which the WL-CSP wafer is glued onto a slitting tape, the outer circumferential section of which is attached to an annular frame; Fig. Figure 4 is a section view showing an alignment step; Fig. 5A is a sectional view showing a training step for a modified layer; Fig. 5B is a partially enlarged sectional view showing the WL-CSP wafer in a state where a focal point is positioned inside the device wafer; Fig. 5C is a partially enlarged sectional view of the WL-CSP wafer in a state where the focal point is positioned inside the sealing element; Fig. Figure 6 is a perspective view of a dividing device; Fig. Figure 7 is a sectional view showing a division step; and Fig. Figure 8 is a partially enlarged sectional view of the WL-CSP wafer after the splitting step has been performed. DETAILED DESCRIPTION OF THE PREFERRED VERSION
[0017] In the following, an embodiment of the present invention is described in detail with reference to the figures. Fig. Figure 1A shows a perspective exploded view of a WL-CSP wafer 27. Fig. Figure 1B is a perspective view of the WL-CSP wafer 27. As shown in Fig. As shown in Figure 1A, components 15, such as LSIs (large scale integrations), are formed in areas divided by several planned division lines (roads) 13, which are formed in a grid pattern on a front surface side 11A of the component wafer 11.
[0018] The component wafer (hereinafter sometimes simply referred to as wafer) 11 is pre-ground on a rear surface 11b so that it is thin to a predetermined thickness (approximately 100 to 200 µm). Then, as in Fig. As shown in Figure 2, several metal pins 21, which are electrically coupled to electrodes 17 in the components 15, are formed and then the front surface side 11a of the wafer 11 is sealed with a sealing element 23 so that the metal pins 21 are embedded in it.
[0019] The sealing element 23 has a composition that includes epoxy resin or epoxy resin with phenolic resin at 10.3%, silica filler at 8.53%, carbon black at 0.1 to 0.2%, and some other components at 4.2 to 4.3% by mass. Other components include, for example, metal hydroxide, antimony trioxide, silicon dioxide, or the like.
[0020] If the front surface 11a of the wafer 11 is covered and sealed with the sealing element 23, which has a composition as described above, then the sealing element 23 has a black color resulting from the carbon black contained in a very small amount in the sealing material 23, and it is normally difficult to see the front surface 11a of the wafer 11 through the sealing element 23. The reason for the carbon black being mixed into the sealing element 23 is primarily to prevent electrostatic damage to a component 15, and a sealing material that does not contain carbon black is not currently available on the market.
[0021] As another embodiment, after a wiring layer is formed on the front surface 11a of the component wafer 11, metal pins 21, which are electrically coupled to the electrodes 17 in the components 15, can be formed on the wiring layer.
[0022] The sealing element 23 is then thinned using a surface cutting device (a surface planer) having a cutting tool made of a single-crystal diamond, or a grinding device called a grinder. After the sealing element 23 has been thinned, an end face of the metal pin 21 is exposed, for example by plasma etching.
[0023] Then, metal protrusions 25 made of solder or the like are formed on the exposed end faces of the metal pins 21 by a well-known method to complete the WL-CSP wafer 27. In this WL-CSP wafer 27 of the present embodiment, the thickness of the sealing element 23 is approximately 100 µm.
[0024] When the WL-CSP wafer 27 is laser-processed by a laser processing device, the WL-CSP wafer 27 is preferably adhered to a parting strip T as an adhesion-promoting strip, the outer circumferential section of which is attached to an annular frame F, as shown in Fig. Figure 3 shows that the WL-CSP wafer 27 is attached. Consequently, the WL-CSP wafer 27 is positioned in a state where it is supported on the annular frame F by the dividing strip T. However, if the WL-CSP wafer 27 is to be laser-processed by the laser processing device, an embodiment can be used in which an adhesive strip is applied to the rear surface of the WL-CSP wafer 27 without using the annular frame F.
[0025] In the processing method for a wafer of the present invention, an alignment step is performed to capture an image of the front surface 11a of the component wafer 11 by the sealing element 23 from a front surface side of the WL-CSP wafer 27 by an infrared imaging means, detecting at least two alignment marks such as target patterns formed on a front surface of the component wafer 11, and then detecting a planned parting line 13 to be cut based on the alignment marks.
[0026] This alignment step will be described in detail with reference to Fig. 4 described. In the alignment step, the WL-CSP wafer 27 is inserted by a clamping table 10 of the laser processing device with the dividing belt T in between, suctioned and held, so that the sealing element 23, which seals the front surface 11a of the component wafer 11, is exposed upwards, as in Fig. 4 shown. Then the ring-shaped frame 11 is clamped and fixed by a clamp 12.
[0027] Then, an image of the front surface 11a of the component wafer 11 is acquired through the sealing element 23 of the WL-CSP wafer 27 by an infrared image acquisition element of an image acquisition unit 14 of the laser processing device (not shown). Since the sealing element 23 is made of a sealing material through which infrared rays, which are to be acquired by the infrared acquisition element of the image acquisition unit 14, can pass, at least two alignment marks, such as target patterns, which are formed on the front surface as 1a of the component wafer 11, can be detected by the infrared image acquisition element. Preferably, an InGaAs image acquisition element with high sensitivity is adapted as the infrared image acquisition element. Preferably, the image acquisition unit 14 includes an exposure unit that can adjust the exposure time or the like.
[0028] Then the clamping table 10 is rotated by θ degrees so that a straight line connecting the alignment marks is positioned parallel to a processing feed direction and a laser head of the laser processing devices is further moved in a direction orthogonal to the processing feed direction by a distance equal to a distance between the alignment marks and the center of the planned division lines 13 in order to detect the planned division line 13 to be laser processed.
[0029] After the alignment step was carried out, as described in Fig. As shown in Figure 5A, a laser beam LB of a wavelength (for example, 1064 nm) that can pass through the component wafer 11 and the sealing element 23 is emitted from the laser head (condenser) 16 of the laser processing device with a focal point positioned in the interior of the component wafer 11 or the interior of the sealing element 23, and in this state the clamping table 10 is moved for processing in one direction of an arrow marking X1 or in one direction of another arrow marking X2 to form a training step for a modified layer to form modified layers 29 (29a, 29b) in the interior of a modified wafer and the interior of the sealing element 23.
[0030] In the training step for a modified layer, the focal point of the laser beam LB is located in the interior of the component wafer 11, as shown in Fig. 5B is shown, positioned and in this state the clamping table 10 is fed for processing in the direction of arrow X1 in order to form a focus point 29a in the interior of the component wafer 11.
[0031] Then, as in Fig. As shown in Figure 5C, the focal point of the laser beam LB is positioned inside the sealing element 23 and the clamping table 10 is fed in the direction of the arrow marking X2 for processing in order to form a modified layer 29b inside the sealing element 23. After this training step for a modified layer has been successively carried out in forward and backward movements along a planned division line 13 extending in a first direction, the clamping table 10 is rotated by 90° and then the training step for a modified layer is successively carried out in forward and backward movements along a planned division line 13 extending in a second direction orthogonal to the first direction.
[0032] After the training step for a modified shift has been carried out, a division device 50, which is in Fig. Figure 6 is shown, used to apply an external force to the WL-CSP wafer 27 in order to perform a division step to divide the WL-CSP wafer into individual component chips 31. The division device 50, which is shown in Fig. Figure 6 shows a frame holding element 52 for holding an annular frame F and a band expansion means 54 for expanding a dividing band T which is attached to the annular frame F which is held on the frame holding element 52.
[0033] The frame holding device 52 is formed from an annular frame holding element 56 and several clamps 58 as fixing means, which are arranged on an outer surface of the frame holding element 56. The frame holding element 56 has an upper surface that forms a receiving surface 56a for receiving the annular frame F placed thereon, and the annular frame F is placed on the receiving surface 56a.
[0034] The ring-shaped frame F, which is positioned on the receiving surface 56a, is fixed to the frame holding element 56 by the clamps 58. The frame holding element 52, which is designed in this way, is movably supported in an upward and a downward direction by the band expansion element 54.
[0035] The tape expansion device 54 includes an expansion drum 60, which is arranged on an inner side of the annular frame retaining element 56. One upper end of the expansion drum 60 is closed with a cover 62. The expansion drum 60 has an inner diameter that is smaller than the inner diameter of the annular frame F but larger than the outer diameter of the WL-CSP wafer 27, which is to be bonded to the dividing tape T, which is attached to the annular frame F.
[0036] The expansion drum 60 has a support flange 64 that is integrally formed at one of its lower ends. The belt expansion element 54 further comprises a drive element 66 for moving the annular frame retaining element 56 in an upward and downward direction. The drive element 66 is formed from several air cylinders 68 arranged on the support flange 64, and a piston rod 70 from each of the air cylinders 68 is connected to a lower surface of the frame retaining element 56.
[0037] The drive means 66, which is formed from the several air cylinders 68, moves the annular frame retaining element 56 in an upward and downward direction, so that the receiving surface 56a is positioned between a reference position at a height substantially equal to the height of the surface of the cover 62, which is an upper end of the expansion drum 60, and an expansion position by a predetermined amount lower from the upper end of the expansion drum 60.
[0038] A division step of the WL-CSP wafer 27, which is carried out using the division device 50, which is configured in such a way as above, is described with reference to Fig. 7A and Fig. 7B described. As in Fig. As shown in Figure 7A, the annular frame F, which carries the WL-CSP wafer 27 with the dividing strip inserted between it, is placed on the receiving surface 56a of the frame holding element 56 and fixed to the frame holding element 56 by the clamps 58. The frame holding element 56 is then positioned at the reference position, where the receiving surface 56a is positioned at a height substantially equal to that of the upper end of the expansion drum 60.
[0039] Then the air cylinders 68 are driven to move the receiving surface 56a to the expansion position which is in Fig. 7B is shown. Consequently, as the annular frame F, which is fixed to the receiving surface 56a of the frame retaining element 56, is lowered, the dividing band T, which is attached to the annular frame F, is brought into contact with the upper end edge of the expansion drum 60 and is generally expanded in radial directions.
[0040] As a result, a tensile force acts radially on the WL-CSP wafer 37, which is attached to the splitting strip T. When the tensile force acts radially on the WL-CSP wafer in this manner, the WL-CSP wafer 27, as shown in the extended sectional view of Fig. 8 specified, cut along a planned division line 13 from a division start point given by the modified layer 29a formed in the component wafer 11 and the modified layer 29b formed in the sealing element 23, whereupon the WL-CSP wafer 27 is divided into individual component chips 31, each having a surface sealed with the sealing element 23.
Claims
[1] A processing method for a wafer (11), in which a front surface (11a) of the wafer (11) on which a component (15) is formed in each of the chip regions divided by a plurality of intersecting dividing lines (13) formed in an intersecting relationship on the front surface (11a) of the wafer (11) is sealed with a sealing member (23), and a plurality of protrusions (25) are individually formed in the chip regions of the sealing member (23), the processing method comprising: an alignment step of capturing an image of a front surface side (11a) of the wafer (11) through the sealing member (23) by an infrared image pickup means from the front surface side (11a) of the wafer (11) to detect alignment marks, and detecting a planned dividing line (13) to be laser-machined based on the alignment marks; and a modified layer forming step (29) for positioning, after the alignment step has been performed, a focal point of a laser beam (LB) of a wavelength that can pass through the wafer (11) and the sealing member (23) in an interior of the wafer (11) or the sealing member (23) and irradiating the laser beam (LB) along the planned dividing line (13) from the front surface side (11a) of the wafer (11) to form a modified layer (29a, 29b) in the interior of the wafer (11) and the sealing member (23); and a dividing step for applying, after the modified layer (29a, 29a) forming step has been carried out, an external force to the wafer (11) and the sealing member (23) to divide the wafer (11) from a division starting point defined by the modified layer (29b) into individual component chips (31), each of which is sealed with the sealing member (23); wherein the sealing element (23) contains carbon black of 0.1 to 0.2% by mass and has a transparency such that infrared rays to be received by the infrared image recording element pass through the sealing element (23). [2] A wafer processing method (11) according to claim 1, wherein the infrared image pickup means used in the alignment step includes an InGaAs image pickup element (14).
Citation Information
Patent Citations
Alignment method
JP2013074021A
Wafer processing method
JP2015028980A
Alignment method
JP2016015438A
Laser processing device and laser processing method
JP2017064746A
Wafer processing method
US20140295643A1