Method for forming a fusion weld joint on components made of steel
Patent Information
- Application Number
- DE102019209650
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2019-07-02
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2039-07-02
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
The invention relates to a method for forming a fusion weld on components made of a steel which has a proportion of non-carbide-bonded free carbon of up to 1.8 mass% and the fusion weld is carried out with an energy beam. To date, there are hardly any options for welding hypereutectoid steels with approximately > 0.8 mass% non-carbide-bonded free carbon using an energy beam with minimal damage. These steels are largely considered unsuitable for welding. The use of beam welding processes generally leads to extremely high hardening and a strong tendency to hardening cracks. Only with welding processes involving very high energy input, e.g., with process-accompanying furnace heating or induction heating, can crack-free welds possibly be formed. However, these steels lose their essential desired properties, particularly their hardness (e.g., the wear properties of cams, ball bearings, and other rolling bearings deteriorate). To overcome the largely limited weldability of these high-carbon steels (e.g., C100, 100CrMnSi6-4, or 100Cr6), relatively complex and / or energy-intensive thermal pre- or post-treatment steps have been required (e.g., preheating, tempering, design compromises, masking, use of wire-shaped or pre-deposited foil-shaped iron- or nickel-containing filler materials). Here, too, the welding possibilities are limited, since weldability can be achieved with increasingly higher energy inputs into the weld melt. On the other hand, however, the strength properties of the steel are adversely altered in a variety of ways. Furthermore, the thermal transient strain differences and the resulting extremely high stresses are a cause of crack formation and thus considerably limit the application possibilities. This problem is generally considered unresolved. Through avoidance strategies, joining tasks involving these steels are usually "solved" with other joining processes (without melting), with their specific disadvantages. In “Microstructure and corrosion behavior of austhenitic stainless steel treated with laser”; Optics & Laser Technology; 43; 2011; pp. 806-813 ; IY Khalfallah et al. describe ways of influencing steels. WO 2018 / 220430 A1 concerns steel plates and their production with a residual austenite content. From DE 10 2015 006 079 A1, steel components and a process for their production are known which are said to have a locally differentiated hardness. JP 2019-99 889 A discloses carburized components with improved abrasion behavior and a method for their production. CN 104 212 965 A concerns possibilities for influencing surfaces, in particular surfaces on rails, by means of laser radiation. It is therefore an object of the invention to provide possibilities for welding steels with an energy beam which have an approx. 0.8 mass% proportion of non-carbide-bonded free carbon, with which an adverse impairment of the original properties of the respective steel material can be avoided and the formation of crack-free welds can be made possible with little effort. According to the invention, this object is achieved by a method having the features of claim 1. Advantageous embodiments and further developments of the invention can be realized with features defined in subordinate claims. In welding processes using energy beams, particularly laser beams or electron beams, a non-contact, concentrated energy is introduced into the steel component, particularly into the surface of a steel component. The energy beam is influenced in such a way that a local temperature increase occurs at the edge layer of the surface of a component exposed to the energy beam, resulting in the melting of the base materials to be welded, forming a common melting zone in which the molten pool material solidifies after the energy input has ceased. These processes are generally referred to as remelting or welding. If the surface of the steel component(s) to be locally melted is coated with an adhesive layer of carbon of a suitable thickness prior to the melting process, this pre-deposited carbon is melted by the energy beam and mixed into the resulting melt. This increases the carbon content of the steel material in the melt zone, resulting in a different chemical composition with a higher carbon content, e.g., in the range of 1.6 mass% to 1.8 mass% carbon, and thus different transformation and material properties than the non-melted base material. If this melt is cooled, the solidified material in the melt zone can achieve lower hardness and higher ductility (local microplastic deformation potential) than was the case with the chemical composition of the base material.This allows for drastically reducing high transient thermal stresses, a key cause of cracking. This utilizes the metal-physical principle that with increasing carbon content, the transformation entropy for martensite formation increases. This means that the supercooling and quenching rate required for martensitic transformation (= hardening) increase beyond what is technically achievable. The additional carbon introduced according to the invention stabilizes the ductile austenitic phase after solidification until cooling to room temperature (residual austenite) and, if sufficiently high, also prevents subsequent transformation upon cooling to lower, technically relevant temperatures. The chemical composition (carbon content) in the molten zone suitable for welding, which is determined by the molten pool, is adjusted by the appropriate ratio of the molten carbon layer thickness to the molten pool size or cross-sectional area of the molten pool (area in cross-section). This ratio ranges from approximately 0.01 to 0.02, depending on the carbon content of the base materials (2, 2n). Thus, with knowledge of the above-mentioned relationship, depending on the selected base material or base material combination, one can determine the appropriate ratio between the desired cross-sectional area of the melt pool (also welding depth or melt pool volume) and the applied carbon layer thickness (cross-sectional area) with a few adjustment tests. The detection of retained austenite is subsequently carried out using suitable X-ray or metallographic methods after appropriate preparation with a light microscope on a cross-section of the melt zone. Since the melt pool volumes and deposited layer thicknesses can be reproduced with extreme precision using modern methods, the corresponding suitable ratio of carbon layer thickness to melt pool area can also be reproduced and verified as often as required. For example, joint welds for a 100Cr6 steel, which is unsuitable for energy beam welding, can be created using a fast-moving, focused energy beam with extremely low energy input. The thickness of the previously applied carbon layer is gradually increased over several trials until residual austenite is visible under the microscope across the entire surface of the molten zone. Depending on experience, the appropriate layer thickness for any desired melt pool volume of any shape and size can be determined after just a few trials. This procedure can be applied to a wide variety of steels to determine the required coating thicknesses. For example, tool steels such as C85W or 90MnCrV8; tempering steels such as 42CrMo4 or C100; martensitic spring steels such as 51CrV4 or Ck67; and rolling bearing steels such as 100Cr6 or 100CrMnSi6-4 can be machined as base materials using this process. In other words: The carbon coating thickness to be applied to two joints of the base materials of steel components to be welded with an energy beam is increased during the calibration process through several tests until a retained austenitic fusion zone can be detected over the entire surface in the cross-section. Once this coating thickness has been determined for a defined welding process, it can be reproducibly applied to any number of parts to be welded and measured and monitored at any time for quality assurance. The layer should preferably be formed from carbon with graphite, which should particularly preferably be in powder form. Powdered graphite can be used inexpensively in dry form or in a suspension. Suspensions can be applied inexpensively by spraying or printing with a suitable viscosity. The respective liquid can be removed later by drying, leaving the layer free of liquid. In addition to water with a suitable emulsifier, alcohols mixed with a suitable wetting agent can also be used as the liquid. The energy beam can be a laser beam or an electron beam. The feed rate of the focal spot of a laser beam should be at least 1 m / min. In joint welding, the process according to the invention can significantly expand the group of fusion-weldable steels to include previously limited or non-weldable steels (e.g., approximately carbon content > 1.0 mass%). Complex upstream or downstream thermal processes can be largely eliminated or minimized. The base materials largely retain their properties. The application of carbon coatings to component surfaces in many conceivable, defined layer thicknesses can be easily adjusted. By applying the coating (e.g., spraying, printing, vapor deposition, or other means) in the form of a pre-deposition on steel component surfaces, this process can be temporally and spatially decoupled from the previously described melting processes. Coating the surfaces with carbon can be carried out at a relatively low temperature level and is therefore significantly less energy-intensive than established furnace or induction processes. Suitable layer thicknesses of carbon layers for the steel 100Cr6 were determined to be 0.015 mm. The pre-deposited carbon (graphite) has the desired metal-physical properties to influence the melt in a suitable manner (weldability) in a comparatively simple way. The following welding tasks can be performed using the method according to the invention: • Joining hardenable cams (lifting and zero cams) on camshafts → e.g. material 100Cr6, 100CrMnSi6-4 • Welding of roller bearings, ball bearings, • Welding of eutectoid unalloyed and low-alloyed and tool steels → e.g. material C85, C100 or 90MnCrV8 and comparable • Welding of martensitic spring steels such as 51CrV4 or Ck67 • Welding of tempering steels such as 42CrMo4 The invention will be explained in more detail below by way of example. Fig. 1a and b show the formation of a layer of graphitic carbon on a surface of a steel component to be welded or of two steel components to be joined together by fusion welding and Fig. 2a and b show the melting of carbon and base material with a laser beam in a melting zone. As can be seen in Fig. 1a and Fig. 1b, a layer 3 of graphitic carbon was applied to the surface of one or two components made of base material 2 or 2n. The base material 2 or 2n 100Cr6 had a carbon content of approximately 1.0 mass%, and the layer thickness of layer 3 was 0.015 mm. The cross-sectional area of layer 3, which was also melted, was 0.015 times the cross-sectional area of the melt pool 4. As can be seen in Fig. 2a and Fig. 2b, the graphitic carbon and the base material 2 and, if present, 2n were melted in the melting zone 4 using a laser beam as energy beam 1 of a wavelength of one wavelength, thus achieving mixing. The carbon content in the melting zone increased to 1.8 mass%. Laser beam 1 was operated at a power of 1400 watts. The feed rate of the focal spot was 4 m / min. The focal spot of the focused energy beam had a diameter of 0.3 mm. Based on a micrograph of the solidified melt pool 4, residual austenite could be detected over the entire surface of the melt zone using a light microscope at a magnification of 500 times.
Claims
Method for forming a fusion weld on components made of a steel having a non-carbide-bonded free carbon content of approximately 0.8 mass%, with a non-carbide-bonded free carbon content of up to 1.8 mass% in a fusion zone of the fusion weld using an energy beam (1), in which a layer (3) of carbon is applied to the respective component surface in the welding area on a joining surface which is up to 0.02 times the size of the cross-sectional area of a molten pool (4) formed in the fusion zone by the energy input of the energy beam (1) with a base material-specific layer thickness, so that in the volume of the molten pool material melted by the energy input after its solidification, a full-surface presence of residual austenite microstructure can be detected on a cross-section of the solidified molten pool material; wherein for this purpose, the chemical composition in the molten zone suitable for welding,which is predetermined by the melt pool, is set by a suitable ratio of the molten carbon layer thickness to the cross-sectional area of the melt pool depending on the selected base material (2) or the base material combination (2, 2n), and the detection of the residual austenite is carried out using suitable X-ray or metallographic methods after appropriate preparation with a light microscope on a cross-section of the melt zone. For this purpose, the thickness of the previously applied layer (3) of carbon is gradually increased in several tests until residual austenite can be detected over the entire area of the melt zone under the microscope. Following the formation of the layer (3) of carbon, the base material (2, 2n) of the respective component(s) is melted within the melt zone with the energy beam (1) to form the melt pool (4), and the fusion weld is formed upon solidification. Method according to claim 1, characterized in that the layer (3) is formed with graphite. Method according to one of the preceding claims, characterized in that powdered graphite is used. Method according to one of the preceding claims, characterized in that a laser beam or an electron beam is used as the energy beam (1). Method according to one of the preceding claims, characterized in that the layer (3) is formed by spraying, printing with a suspension or vapor deposition. Method according to one of the preceding claims, characterized in that the proportion of residual austenite in a section of the melt zone of the solidified melt pool material is detected microscopically or X-ray-graphically. Method according to one of the preceding claims, characterized in that the proportion of carbon in the melting zone is increased to 1.8 mass%.
Citation Information
Patent Citations
Method for online laser broadband quenching on surface of steel rail
CN104212965A
Component, in particular for a vehicle, and method for manufacturing such a component
DE102015006079A1
Carburized parts, and production method thereof
JP2019099889A
Steel sheet for manufacturing press hardened parts, press hardened part having a combination of high strength and crash ductility, and manufacturing methods thereof
WO2018220430A1
CN000104212965A