Resistance spot weldability of an aluminum sheet part
Patent Information
- Application Number
- DE102023001702
- Authority / Receiving Office
- DE · DE
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-27
- Publication Date
- 2024-10-31
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
The invention relates to a method for improving the suitability of a thin-walled sheet metal part made of aluminum or steel for resistance spot welding. Aluminum sheets are used in large quantities, sometimes as large-area components, in modern vehicle bodies. Resistance spot welding of aluminum has established itself as an effective and economical bodyshell manufacturing process. Aluminum sheet metal parts with sheet thicknesses ≤ 1.25 mm arranged on the outside of a sheet stack cannot be spot welded, or can only be spot welded with very limited process reliability. The reason for this lies in the low inherent resistance of the thin-walled component (geometric factor of electrical resistance), particularly when it is a deep-drawing-optimized material for outer skin parts, such as the aluminum alloy Al6-OUT. Such alloys have comparatively high ductility and low strength. This, in turn, is associated with low material electrical resistance. Aluminum sheets are typically subjected to a surface treatment process before further processing in the body shop. This process cleans the components, removes the oxide layer, or adjusts it to a defined level, and thus alters the specific properties of the component surface. These include chemical surface or cleaning processes such as chemical wet cleaning ("Alodine"). Alternatively, laser treatment processes such as the so-called "Laserclean" process are also used. All of these methods aim to clean the surfaces of the aluminum sheets or to remove the oxide layer to a defined residual height and to prepare the component surfaces for subsequent processes such as structural bonding. In this context, DE 10 2004 027 229 B4 relates to a method for welding workpieces made of aluminum or an aluminum alloy, in which a) the welding point is exposed to a first laser beam with a power that is essentially constant over time, at least in some sections, and b) the welding point is simultaneously exposed to a second, pulsed laser beam, the points of action of both laser beams overlapping, c) the workpieces are electrolytically oxidized, and d) the respective anodized layer is at least partially evaporated by the pulsed laser beam. EP 3 393 706 B1 further relates to a method for producing a pre-coated sheet in preparation for welding it to another pre-coated sheet, comprising the successive steps of providing a pre-coated sheet comprising a metallic substrate provided with a pre-coating layer on at least one of its surfaces, then removing at least part of the pre-coating layer on at least one surface of the pre-coated sheet to form a removal region, wherein the removal is carried out by impinging a laser beam on the pre-coating layer, wherein the removal step comprises, to the extent of the removal, the relative displacement of the laser beam with respect to the sheet along an advancing direction, wherein during the removal, the laser beam is inclined with respect to the surface of the sheet in such a way thatthat the perpendicular projection of the laser beam onto the surface of the sheet is located in the area of the sheet in which the removal has already been carried out, forming an angle of inclination with the normal direction to the surface of the workpiece which lies between 12° and 50°. The object of the invention is to improve the resistance spot welding of an aluminum sheet. The invention is based on the features of the independent claims. Advantageous developments and refinements are the subject of the dependent claims. A first aspect of the invention relates to a method for improving the suitability of a thin-walled sheet metal part made of aluminum or steel for resistance spot welding, wherein a machining process is carried out by means of a laser beam on an area of the sheet metal part around the position of a weld nugget to be generated in the future on the sheet metal part, characterized by the successive steps: - machining the area with a first, lower area-related energy density of the laser beam for cleaning and optionally activating the surface of the sheet metal part to ensure the adhesive adhesion of a bodyshell adhesive to the sheet metal part, and subsequently: - machining the area again with a second area-related energy density of the laser beam that is higher than the first, for removing a surface layer,Remelting of a base material of the sheet metal part and increasing the surface roughness of the sheet metal part by texturing as well as oxidizing the surface of the sheet metal part, each to increase an electrical resistance when current flows in the area. In other words, when re-machining the area with a second, higher than the first, area-related energy density of the laser beam for removing a surface layer, the energy density must be selected to be high enough to cause remelting of a base material of the sheet metal part and an increase in the surface roughness of the surface of the sheet metal part by texturing as well as oxidation of the surface of the sheet metal part, each with the purpose of increasing an electrical resistance when current flows in the said area. The temperature at the joint is crucial for the formation of a weld nugget and the resulting size of the weld nugget. When the melting temperature is exceeded, a material bond between the joining partners occurs. The resulting temperature depends on the voltage drop, which in turn depends on the electrical resistance. Studies have shown that a higher electrical resistance results from a Laserclean surface pretreatment according to the first aspect of the invention than from an untreated surface. Preferably, the (initial) processing of the area and the subsequent reprocessing of the area are carried out using a laser cleaning process. Depending on the applied energy density, Laserclean can clean, activate, and / or ablate / passivate the surface. Cleaning refers to the removal of dirt and dust, or release agents and lubricants (particularly when the laser beam energy density is < 10 J / cm2). Activation influences oxide or passivation layers. At an energy density of 20 J / cm2 or higher, oxide / passivation layers are partially ablated or completely removed, or the base material is already remelted. Remelting increases the surface roughness of the metal surface (texturing). The surface also oxidizes. As a result of the texturing process using Laserclean, the electrical resistance of the metal surface increases. Following these steps, an elevated peak in the electrical resistance curve is generated during resistance spot welding at the time of transition from a pre-current phase to the main current phase (upslope, current ramp). The weld nugget forms from this point of transition to the higher current phase and is completed during the main current phase (upper current plateau). In contrast, the electrical resistance at this important transition point at the start of the welding process is lower in the case of an untreated component. The higher electrical resistance at the surface after application of the method according to the invention can be due to increased surface roughness due to the remelting process or to the formation of oxide or silicate layers. Accordingly, the invention describes a method in which the laser cleaning process is used to locally increase the electrical resistance on the surface of thin-walled aluminum components, in particular aluminum sheets, in order to improve spot weldability. The underlying principle is, on the one hand, the change in surface quality / roughness through remelting or texturing with the laser beam, and, on the other hand, the change in electrical resistance through a chemical reaction (oxidation) of the sheet surface generated by the laser. The resulting chemical products, such as oxides, silicates, etc., increase the overall electrical resistance when an electrical current flows. The increased electrical resistance facilitates resistance spot welding. The laser beam preferably has a cross-section such that when it strikes the sheet metal part it does not protrude beyond the edges of an imaginary square on the surface of the sheet metal part with an edge length of 1 mm, more preferably 0.5 mm, especially preferably 0.36 mm. Furthermore, the laser beam preferably strikes the surface of the sheet metal part perpendicularly with a range of area-related energy density in the range of 11-23 joules / square centimeter (abbreviated to [J / cm2]). Furthermore, the working height is preferably plus / minus 1.5 mm at a distance of a laser device from the surface of the sheet metal part of nominally 120 mm. Furthermore, the laser beam is preferably guided over the component surface with a 25 percent overlap in two perpendicular coordinate axes, each in the surface of the sheet metal part. Advantageous effects of the invention are weight / raw material and energy savings by avoiding an increase in the sheet thickness of a sheet metal part such as a thin-walled outer sheet for use in vehicle construction, process-reliable joining, increased production stability, increased straight-line running, reduced need for personnel deployment by eliminating complex welding parameter optimizations, higher transferable weld point strengths, less necessary rework, and traceability. If a so-called laser cleaning system is used to generate the laser beam and to carry out the processing process using the laser beam, this can achieve improved utilization by using the different energy densities of the laser beam emitted by it, and thus a higher efficiency can be achieved, since the laser cleaning system, which may previously only have been used to clean the surface of the sheet metal part, can be used to carry out additional production steps, in particular through the additional use of the higher area-related energy density in a second processing step. According to an advantageous embodiment, the machining process is carried out by means of the laser beam on only one side of the sheet metal part. According to a further advantageous embodiment, the machining process is carried out by means of the laser beam on both sides of the sheet metal part at congruent locations on a front and back side of the sheet metal part. According to a further advantageous embodiment, the first, lower area-related energy density of the laser beam has an energy density of less than 10 J / cm2. According to a further advantageous embodiment, the first, lower area-related energy density of the laser beam has an energy density of less than 15 J / cm2. According to a further advantageous embodiment, the second, higher area-related energy density of the laser beam has an energy density of more than 20 J / cm2. According to a further advantageous embodiment, a sheet metal part made of aluminum or an aluminum alloy is used. According to a further advantageous embodiment, a surface of a joining partner component to be welded to the sheet metal part by resistance spot welding is treated in a zone around the position of a weld nugget to be generated in the future on the joining partner component with a machining process using a laser beam, wherein the laser beam has such a high area-related energy density that a removal of a surface layer of the joining partner component, a remelting of a base material of the joining partner component and an increase in the surface roughness of the surface of the joining partner component by texturing the surface as well as an oxidation of the surface of the joining partner component take place, in each case to increase an electrical resistance when current flows in the zone. Alternatively, the laser processing process can also be applied only to the joining component that is to be welded to the thin-walled aluminum sheet metal part. The zones to be processed face the thin-walled aluminum sheet metal part. Even the surface texturing of the joining component alone locally increases the electrical resistance in the joining plane and improves weldability. According to a further advantageous embodiment, a joining partner component made of aluminum or an aluminum alloy is used. Further advantages, features, and details will become apparent from the following description, which – where appropriate with reference to the drawings – describes at least one embodiment in detail. Identical, similar, and / or functionally equivalent parts are provided with the same reference numerals. They show: Fig. 1: A sheet metal part to which a laser processing process is applied to improve its suitability for resistance spot welding, according to an embodiment of the invention. Fig. 2: A sheet metal part and a joining component, which are welded together according to an embodiment of the invention and are pretreated by means of a laser processing process. The representations in the figures are schematic and not to scale. Fig. 1 shows a thin-walled sheet metal part 1 made of aluminum alloy for use in vehicle construction, to which a method is applied to improve its suitability for connection to another component by resistance spot welding. First, the respective position of a weld nugget 5 to be produced in the future is defined on the sheet metal part 1. In a predetermined area 3 around the future weld nugget 5, a machining process is carried out using a laser beam, ie a laser radiation device, the emitted laser beam of which is directed onto the surface of the sheet metal part 1, is moved in a raster manner parallel to the surface such that the laser beam successively sweeps over the area 3 with at least partial overlaps until the entire area 3 has been swept over by the laser beam at least once.The laser beam processing process is initially carried out by processing as explained above on area 3 with a first, lower area-related energy density of the laser beam of less than ten joules / cm2 for cleaning and up to fifteen joules / cm2 if activation of the surface of the sheet metal part 1 is also desired, in each case to ensure the adhesive adhesion of a body-in-white adhesive to the sheet metal part 1.Once this processing step has been completed, further processing of area 3 is carried out by successively sweeping the laser beam over at least partially overlapping sections of the respective area 3 with a second, higher than the first, area-related energy density of the laser beam in the respective area 3 of at least twenty joules / cm2 to remove dirt, release agent, abrasion, paint, oil, and other substances, which are removed from the surface by suction after separation, as well as to remelt a base material of the sheet metal part 1 and to increase the surface roughness of the surface of the sheet metal part 1 by texturing and to oxidize the surface of the sheet metal part 1, in each case to increase an electrical resistance when current flows in area 3. Fig. 2 shows a machining process carried out analogously to Fig. 1 by means of a laser beam, wherein in this case, in addition to the sheet metal part 1 (as explained in relation to Fig. 1), a surface of a joining partner component 7 to be welded to the sheet metal part 1 by resistance spot welding is treated with a machining process by means of a laser beam in a zone around the position of the welding nugget 5 to be produced in the future, which is intended to connect the joining partner component 7 and the sheet metal part 1.At least in a second processing step, the laser beam has such a high area-related energy density that a surface layer of the joining partner component 7 is removed, a base material of the joining partner component 7 is remelted, the surface roughness of the joining partner component 7 is increased by texturing the surface, and the surface of the joining partner component 7 is oxidized, each of which increases the electrical resistance when current flows in the zone. Subsequently, the sheet metal part 1 and the joining partner component 7 are joined together by resistance spot welding. Alternatively, the laser processing process, which comprises the two processing steps according to Fig. 1, can be carried out only on the joining partner component 7, and the sheet metal part 1 can be left unprocessed, for example if it already has a sufficient material thickness and a clean surface. Although the invention has been illustrated and explained in detail by preferred embodiments, the invention is not limited by the disclosed examples, and other variations may be derived therefrom by those skilled in the art without departing from the scope of the invention. It is therefore clear that a multitude of variations exist. It is also clear that exemplary embodiments are truly only examples and should not be construed as limiting the scope, possible applications, or configuration of the invention in any way.Rather, the preceding description and the description of the figures enable the person skilled in the art to implement the exemplary embodiments in concrete terms, whereby the person skilled in the art, with knowledge of the disclosed inventive concept, can make various changes, for example with regard to the function or the arrangement of individual elements mentioned in an exemplary embodiment, without departing from the scope of protection defined by the claims and their legal equivalents, such as further explanations in the description. List of reference symbols 1 Sheet metal part 3 Area 5 Weld nugget 7 Joining partner component QUOTES CONTAINED IN THE DESCRIPTION This list of documents submitted by the applicant was generated automatically and is included solely for the convenience of the reader. This list is not part of the German patent or utility model application. The DPMA assumes no liability for any errors or omissions. Cited patent literature DE 102004027229 B4
[0004] EP 3393706 B1
[0005]
Claims
A method for improving the suitability of a thin-walled sheet metal part (1) made of aluminum or steel for resistance spot welding, wherein a machining process is carried out by means of a laser beam on an area (3) of the sheet metal part (1) around the position of a weld nugget (5) to be produced in the future on the sheet metal part (1), characterized by the successive steps: - machining the area (3) with a first, lower area-related energy density of the laser beam for cleaning and optionally activating the surface of the sheet metal part (1) to ensure the adhesive adhesion of a bodyshell adhesive to the sheet metal part (1), and subsequently: - re-machining the area (3) with a second area-related energy density of the laser beam that is higher than the first, for removing a surface layer,Remelting a base material of the sheet metal part (1) and increasing the surface roughness of the surface of the sheet metal part (1) by texturing and oxidizing the surface of the sheet metal part (1), each to increase an electrical resistance when current flows in the area (3). Method according to claim 1, wherein the machining process by means of the laser beam is carried out on only one side of the sheet metal part (1). Method according to claim 1, wherein the machining process is carried out by means of the laser beam on both sides of the sheet metal part (1) at congruent locations on a front and back side of the sheet metal part (1). Method according to one of claims 1 to 3, wherein the first, lower areal energy density of the laser beam has an energy density of less than 10 J / cm2. Method according to one of claims 1 to 3, wherein the first, lower areal energy density of the laser beam has an energy density of less than 15 J / cm2. Method according to one of the preceding claims, wherein the second, higher areal energy density of the laser beam has an energy density of more than 20 J / cm2. Method according to one of the preceding claims, wherein a sheet metal part (1) made of aluminum or an aluminum alloy is used. Method according to one of the preceding claims, wherein a surface of a joining partner component (7) to be welded to the sheet metal part (1) by resistance spot welding is treated in a zone around the position of a weld nugget (5) to be produced in the future on the joining partner component (7) with a machining process using a laser beam, wherein the laser beam has such a high area-related energy density that a removal of a surface layer of the joining partner component (7), remelting of a base material of the joining partner component (7), an increase in the surface roughness of the surface of the joining partner component (7) by texturing the surface, and an oxidation of the surface of the joining partner component (7) take place, in each case to increase an electrical resistance when current flows in the zone. Method according to claim 8, wherein a joining partner component (7) made of aluminum or an aluminum alloy is used.
Citation Information
Patent Citations
method of welding aluminum or aluminum alloy workpieces
DE102004027229B4
Method for producing a pre-coated metal sheet, with removal of the coating by means of an inclined laser beam, and corresponding metal sheet
EP3393706B1
Method of preparing and welding zinc coated steel
GB2274257A
Welding equipment
JP1998225770A
JP000H10225770A