Process for the production of olefin

DE112013006222B4Active Publication Date: 2024-10-31KAO CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
DE112013006222
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2013-12-19
Publication Date
2024-10-31
Estimated Expiration
2033-12-19
Patent Text Reader

Abstract

A process for the production of olefins, comprising the step of carrying out a dehydration reaction with an alcohol having not less than 8 and not more than 22 carbon atoms in the presence of a solid acidic catalyst, wherein the solid acidic catalyst comprises aluminum oxide and an oxide of an element having a higher electronegativity than that of aluminum, which is carried on the aluminum oxide, wherein the dehydration reaction is a liquid-phase reaction and the average pore size of the catalyst is not less than 5 nm and not more than 50 nm.
Need to check novelty before this filing date? Find Prior Art

Description

Field of the InventionThis invention relates to a process for the production of long chain olefins.BACKGROUND OF THE INVENTIONVarious methods for producing olefin compounds by dehydration reaction of alcohols are known. For example, Patent Literature 1 discloses a method for producing an olefin compound by conducting a dehydration reaction with a tertiary alcohol in a gas phase at a temperature of 200 to 400° C. in the presence of an aluminosilicate as a solid catalyst.In addition, Patent Literature 2 discloses a method for producing ethylene by conducting a dehydration reaction of ethanol in a gas phase in the presence of a catalyst prepared by adding a phosphate to an active alumina.On the other hand, the present inventors have found that olefins can be produced for a short period of time at a high yield by subjecting a long-chain alcohol to a liquid phase dehydration reaction using a catalyst having specific weak-acidic sites such as γ-alumina, and have previously filed a patent application concerning it (see Patent Literature 3).WO97 / 03932 A1 describes the dehydrogenation of primary alcohols to alpha-unsaturated hydrocarbons by bringing them into contact with a catalyst comprising niobic acid and / or tantalic acid. The catalyst may be activated by heating prior to the reaction.US 3 246 045 A describes a process for the preparation of terminal olefins comprising contacting a feedstock having the structural formula wherein R is a lower alkyl group, R' is selected from the group consisting of hydrogen and a lower alkyl group, Y is selected from the group consisting of hydrogen and hydroxy, and when Y is hydrogen, R" is hydroxymethyl, and when Y is hydroxy, R" is methyl, said feedstock containing up to about 12 carbon atoms, with a catalyst consisting essentially of a catalytic amount of alkali metal sulfate having an atomic number of 11 to 55 on alumina under dehydration conditions including a temperature of about 600 to 975° F.List of ReferencesPatent LiteraturePatent Literature 1: JP 2008-56671 APatent Literature 2: JP 59-40057BPatent Literature 3: WO 2011 / 052732ASUMMARY OF THE INVENTIONThis invention relates to a process for producing olefins, comprising the step of conducting a dehydration reaction with an alcohol having not less than 8 and not more than 22 carbon atoms in the presence of a solid acidic catalyst, wherein the solid acidic catalyst comprises alumina and an oxide of an element having a higher electronegativity than that of aluminum supported on the alumina, wherein the dehydration reaction is a liquid phase reaction, and the average pore size of the catalyst is not less than 5 nm and not more than 50 nm.DETAILED DESCRIPTION OF THE INVENTIONHowever, in the gas phase reaction such as typically in the processes described in Patent Literatures 1 and 2, it is necessary to evaporate a total amount of the starting material used therein, so that particularly when the long-chain aliphatic alcohol having a high boiling point is evaporated, high energy consumption is required, which is disadvantageous in view of cost. Further, the silica-alumina catalyst used in Patent Literature 1 tends to branch the olefins due to the alkyl rearrangement together with the production of a multimer of the olefins, so that a problem may arise that the yield of the intended reaction product is lowered. In addition, in Patent Literature 2, only suppressing decomposition of carbonaceous substances is described, but there is no description regarding suppression of branching of olefins due to alkyl rearrangement and production of multimers from the olefins.The olefins produced by the method described in Patent Literature 3 contain only a small amount of by-products produced due to the production of multimers or by branching. However, it is still required to develop a process for producing olefins with an even higher efficiency.This invention relates to a process for producing long-chain olefins for a short period of time with high efficiency by conducting a dehydration reaction with a long-chain aliphatic alcohol.The present inventors have found that by conducting a dehydration reaction with a long-chain aliphatic alcohol in the presence of a specific catalyst, it is possible to produce long-chain olefins for a short period of time in high yield.More specifically, the process for producing olefins according to this invention is such a process wherein an alcohol is subjected to a dehydration reaction in the presence of a solid acidic catalyst to produce olefins. The solid acid catalyst is formed of alumina and an oxide of an element having a higher electronegativity than that of aluminum supported on the alumina.The production process of this invention can provide a process for producing long-chain olefins for a short period of time with a high yield and a high selectivity by subjecting a long-chain aliphatic alcohol to a dehydration reaction.The process for producing olefins according to this invention is a process for producing olefins by conducting a dehydration reaction with an alcohol using a solid acidic catalyst prepared by supporting an oxide of an element having an electronegativity higher than that of aluminum on alumina.[Catalyst]In this invention, the solid acid catalyst prepared by supporting an oxide of an element having a higher electronegativity than that of aluminum on alumina is used. The value of electronegativity as used in the present invention means the value of Pauling electronegativity.The electronegativity of the solid acid catalyst is preferably not less than 1.6, more preferably not less than 1.7, and even more preferably not less than 1.8, and is also preferably not more than 2.6, and more preferably not more than 2.0 from the viewpoint of suppressing the occurrence of side reactions.Examples of the element having a higher electronegativity than aluminum (Al: 1.5) include sulfur (S: 2.8), tungsten (W: 1.7), phosphorus (P: 2.1), silicon (Si: 1.8), molybdenum (Mo: 1.8), iron (Fe: 1.8), cobalt (Co: 1.8), nickel (Ni: 1.8), copper (Cu: 1.9), zinc (Zn: 1.6), boron (B: 2.0), gallium (Ga: 1.6), indium (In: 1.7), germanium (Ge: 1.8), tin (Sn: 1.8), antimony (Sb: 1.9), bismuth (Bi: 1.9), and selenium (Se: 2.4). Of these elements, sulfur (S), tungsten (W), phosphorus (P), and silicon (Si) are preferable from the viewpoint of suppressing the occurrence of side reactions. The numerical value in the above respective parentheses means the value of Pauling electronegativity of the element.As the compound as an oxide source of the element, at least one compound selected from the group consisting of a water-soluble ammonium salt, metal alkoxide, and oxoacid, and a salt thereof is preferred from the viewpoint of good catalytic activity. Specific examples of the compound as an oxide source of the element include water-soluble ammonium salts such as ammonium sulfate and ammonium tungstate, metal alkoxides rendered water-soluble by hydrolysis such as tetramethyl orthosilicate and tetraethyl orthosilicate, and oxoacids such as silicatungstic acid and phosphotungstic acid, and salts thereof. The catalytic activity as used herein means a reaction rate of the above dehydration reaction according to this invention when the above catalyst is used therein.Further specific examples of the compound as an oxide source of the element include at least one compound selected from the group consisting of sulfuric acid, ammonium sulfate, sodium sulfate, potassium sulfate, magnesium sulfate, calcium sulfate, sodium thiosulfate, ammonium thiosulfate, tungstate, ammonium tungstate, sodium tungstate, potassium tungstate, calcium tungstate, ammonium paratungstate, ammonium metatungstate, silicatungstate, phosphotungstate acid, ammonium phosphotungstate, sodium phosphotungstate, potassium phosphotungstate, colloidal silica, silica gel, water glass, tetramethylammonium silicate, tetramethylorthosilicate, tetraethylorthosilicate, phosphoric acid, ammonium phosphate, diammonium hydrogen phosphate, sodium phosphate, potassium phosphate, magnesium phosphate and calcium phosphate.Of these compounds, ammonium sulfate, ammonium tungstate, diammonium hydrogenphosphate and tetraethyl orthosilicate are preferred as the oxide source of the element in view of good catalytic activity. When such a catalyst is used, the dehydration reaction of the long-chain alcohol proceeds rapidly, so that the long-chain olefins as a target product can be produced in high yield.The amount of the oxide of the element supported on alumina is preferably not less than 0.01 mass %, more preferably not less than 0.1 mass %, even more preferably not less than 0.5 mass %, and still more preferably not less than 0.8 mass %, from the viewpoint of good catalytic activity, based on the amount of the alumina. From the same viewpoint, the amount of the oxide of the element supported on alumina is preferably not more than 10 mass %, more preferably not more than 9 mass %, even more preferably not more than 8 mass %, further preferably not more than 7 mass %, and further more preferably not more than 2 mass %, based on the amount of alumina.When the amount of the oxide of the element supported on alumina is within the above-mentioned range, it is possible to complete the reaction in a short period of time.The catalyst used in the present invention can be produced by a method of evaporating to dryness, an absorption method, equilibration-adsorption method, pore-filling method, spraying method, precipitating method or the like.As a specific method for producing the catalyst, in view of a good catalytic activity thereof, there can be mentioned the method comprising the steps of mixing an aqueous suspension or a hydrous solid of the alumina, a compound as an oxide source of the element or the oxide of the element, and ion-exchanged water to produce an impregnated product, and drying and calcining the resulting impregnated product. The alumina acting as a carrier can be produced, for example, by a precipitation method, a sol-gel method or an alkoxide method. From the viewpoint of good catalytic activity of the resulting catalyst, the alumina used above is preferably in the form of a calcined product obtained by calcining it at a temperature of not less than 400° C., more preferably not less than 450° C., and further preferably not less than 500° C. From the same viewpoint, the temperature of calcination is also preferably not more than 900° C., more preferably not more than 850° C., and still more preferably not more than 800° C. According to the present invention, from the viewpoint of good catalytic activity of the resulting catalyst, the alumina is preferably γ-alumina.The temperature at which the alumina is impregnated with the compound as an oxide source of the element or the oxide of the element is preferably not less than 0° C., more preferably not less than 20° C., further preferably not less than 50° C., and still further preferably not less than 60° C., and is also preferably not more than 100° C., more preferably not more than 95° C., still further preferably not more than 90° C., and still further preferably not more than 80° C., from the viewpoint of a high carrying speed and uniformity of the resulting catalyst.The time of impregnation is preferably not less than 0.1 hour, more preferably not less than 0.2 hour, and even more preferably not less than 0.5 hour, and is also preferably not more than 10 hours, more preferably not more than 5 hours, and even more preferably not more than 2 hours from the viewpoint of a high carrying speed and uniformity of the resulting catalyst.The calcination temperature of the impregnated product is preferably not less than 300°C, more preferably not less than 400°C, even more preferably not less than 450°C from the viewpoint of good catalytic activity of the resultant catalyst, and is also preferably not more than 900°C, more preferably not more than 850°C, even more preferably not more than 800°C, further more preferably not more than 700°C, and further still more preferably not more than 600°C from the viewpoint of preventing reduction of the surface of the resultant catalyst and achieving high degree of dispersion of the member to be supported.The calcination time of the impregnated product is preferably not less than 1 hour, and more preferably not less than 2 hours from the viewpoint of good catalytic activity of the resultant catalyst, and is also preferably not more than 10 hours, and more preferably not more than 5 hours from the viewpoint of preventing reduction of the surface of the resultant catalyst and achieving a high degree of dispersion of the element to be supported.The atmosphere used in calcination is not particularly limited, and calcination may be carried out in an inert gas atmosphere, oxidizing atmosphere or reducing atmosphere. Further, the calcination may be carried out in a closed or gas flow state. In the present invention, in view of a good catalytic activity of the resulting catalyst, calcination is preferably carried out in a gas flow of air or oxygen.The catalyst thus obtained is maintained in an aggregated state and therefore can be appropriately pulverized into a powder or granules or formed into needles, pellets, etc. in use.When the catalyst is used in the form of a powder, the average particle size of the powder is preferably not less than 1 μm, more preferably not less than 5 μm, even more preferably not less than 10 μm, even more preferably not less than 20 μm, and even more preferably not less than 30 μm from the viewpoint of facilitating recovery of the catalyst after completion of the reaction, and is also preferably not more than 300 μm, more preferably not more than 250 μm, even more preferably not more than 200 μm, even more preferably not more than 150 μm, still more preferably not more than 100 μm, and even more preferably not more than 50 μm from the viewpoint of good catalytic activity of the resulting catalyst.The BET specific surface area of the catalyst is preferably not less than 100 m 2 / g, more preferably not less than 120 m 2 / g, and further more preferably not less than 140 m 2 / g from the viewpoint of good catalytic activity of the resulting catalyst, and is also preferably not more than 500 m 2 / g, more preferably not more than 400 m 2 / g, further more preferably not more than 300 m 2 / g, and further more preferably not more than 200 m 2 / g from the viewpoint of good durability and high strength of the resulting catalyst.The average pore size of the catalyst is not less than 5 nm, preferably not less than 7 nm, and more preferably not less than 9 nm from the viewpoint of good catalytic activity of the resulting catalyst, and is also not more than 50 nm, preferably not more than 40 nm, more preferably not more than 25 nm, even more preferably not more than 25 nm, and still more preferably not more than 15 nm from the same viewpoint.The pore volume of the catalyst is preferably not less than 0.20 cm 3 / g, more preferably not less than 0.25 cm 3 / g, and further preferably not less than 0.30 cm 3 / g from the viewpoint of good catalytic activity of the resulting catalyst, and is also preferably not more than 2.0 cm 3 / g, not more than 1.5 cm 3 / g, further preferably not more than 1.2 cm 3 / g, still further preferably not more than 1.0 cm 3 / g, and further still further preferably not more than 0.7 cm 3 / g from the same viewpoint.The average particle size is an average particle size of the catalyst determined as follows. That is, 0.05 g of the catalyst is dispersed while stirring in ethanol (available from Kanto Chemical Co., Inc.: First grade Cica reagent) as a measurement solvent for measuring the particle sizes thereof (stirring rate: level 4) using a laser diffraction scattering particle size distribution analyzer "LA-920" (available from HORIBA Ltd.), and an average particle size of the catalyst is calculated from the particle sizes thus measured, on the assumption that a refractive index of the catalyst is 1.10.The BET specific surface area, the average pore size and the pore volume of the catalyst can be measured by the following methods. Using an accelerated surface porosimetry analyzer "ASAP2020" available from Micromeritics Instrument Corp., a sample is heat-treated at 250°C for 5 hours, and then a BET specific surface area of the sample is measured by a multipoint method using liquid nitrogen to obtain the value in such a range that a parameter C is positive.The pore volume of the catalyst can be calculated by a BJH method (Barrett-Joyner-Halenda method), and further a peak-to-peak of a pore distribution curve for the catalyst is defined as an average pore size thereof. The BJH method as used herein is such a method wherein the pore volume of one cylindrical pore is calculated as a model pore not associated with any other pore for determining the pore distribution by capillary condensation and multilayered adsorption of a nitrogen gas. The details of the BJH method are described in "SHIMADZU Review", Vol. 48, No. 1, pp. 35 to 44, 1991.The amount of the catalyst used in a suspended bed reaction is preferably not less than 0.1 mass %, more preferably not less than 0.3 mass %, even more preferably not less than 0.5 mass %, and further preferably not less than 2 mass %, and is also preferably not more than 30 mass %, more preferably not more than 20 mass %, further preferably not more than 15 mass %, and further preferably not more than 12 mass %, based on the alcohol as the starting material. When the amount of the catalyst used is within the above range, it is possible to reduce the reaction temperature and hence to provide an economically advantageous process.The details of the mechanism of the reaction using the above-mentioned catalyst are still unclear, but it is considered that the reaction proceeds as follows. It is considered that the alumina is increased adequately in acid strength by the action of the element supported thereon having higher electronegativity, so that the reaction activity is enhanced.[Alcohol as Starting Material]The number of carbon atoms contained in the alcohol used as the starting material in this invention is preferably not less than 8, more preferably not less than 12, and even more preferably not less than 14, and is also preferably not more than 22, more preferably not more than 20, and even more preferably not more than 18, from the viewpoint of the utility of the resulting olefins. From the same viewpoint, the number of carbon atoms contained in the alcohol is not less than 8 and not more than 22, preferably not less than 12 and not more than 20, and more preferably not less than 14 and not more than 18.Specific examples of the preferred alcohol as the starting material include at least one alcohol selected from the group consisting of 1-dodecanol, 1-tridecanol, 1-tetradecanol, 1-pentadecanol, 1-hexadecanol, 1-heptadecanol, 1-octadecanol, 1-nonadecanol and 1-eicosanol in view of the usefulness of the resulting olefins.[Organic Solvent]In the production process of this invention, an organic solvent may be used as needed. The organic solvent usable in the present invention is not particularly limited as long as the organic solvent is maintained in a liquid state at the reaction temperature and is compatible with the substrate and the reaction product, and as long as the organic solvent has no adverse influence on the reaction. The organic solvent may be in the form of a mixture of organic solvents. In addition, the organic solvent is preferably separable from the reaction product by using a difference between the boiling points thereof after completion of the reaction.Examples of the preferred organic solvent usable in the present invention include hydrocarbon-based organic solvents such as saturated aliphatic hydrocarbons, unsaturated aliphatic hydrocarbons and aromatic hydrocarbons.The saturated aliphatic hydrocarbon may be a straight chain or branched hydrocarbon.Specific examples of the saturated aliphatic hydrocarbon include compounds having not less than 10 and not more than 35 carbon atoms such as tridecane, hexadecane, octadecane, eicosane, docosane, triacontane and squarane.In addition, the saturated aliphatic hydrocarbon may also be in the form of a mixture such as liquid paraffin, naphthene-based hydrocarbons, and isoparaffin-based hydrocarbons. As the saturated aliphatic hydrocarbon, solid paraffin which is maintained in a solid state at normal temperature but changes in a liquid state at room temperature can also be used.As the saturated aliphatic hydrocarbon, oligomers of propylene, isobutene, etc. can also be used.The unsaturated aliphatic hydrocarbon may be a straight chain or branched hydrocarbon.Specific examples of the unsaturated aliphatic hydrocarbon include compounds having preferably not less than 15 carbon atoms, and more preferably not less than 30 carbon atoms, and preferably not more than 35 carbon atoms, and more preferably not more than 30 carbon atoms, such as eicosane, heneicosene, docosene, trocosene, and squalene. The unsaturated aliphatic hydrocarbon may be in the form of a mixture of unsaturated aliphatic hydrocarbons.Specific examples of the aromatic hydrocarbon include alkylbenzenes and alkylnaphthalenes such as n-dodecylbenzene, n-tridecylbenzene, n-tetradecylbenzene, n-pentadecylbenzene, n-hexadecylbenzene, and diisopropylnaphthalene.[Dehydration Reaction (Olefin Formation Reaction)]The reaction used in the process of this invention is a dehydration reaction of the alcohol. When water by-produced in the reaction is present or remains in the reaction system, the reaction rate can be lowered. For this reason, in view of increasing the reaction rate, an inert gas such as nitrogen and argon is preferably introduced into the reaction system while being stirred under reduced pressure of usually not less than 0.03 mPa and not less than 0.09 MPa or under normal pressure to conduct the reaction to remove the water generated in the reaction from the reaction system.The reaction temperature is preferably not higher than a boiling point of the alcohol as a starting material from the viewpoint of achieving a high reaction rate and suppressing occurrence of undesirable side reactions such as alkyl rearrangement and production of multimers of the olefins. More specifically, the reaction temperature is preferably not less than 150° C., more preferably not less than 200° C., even more preferably not less than 220° C., further preferably not more than 230° C., and further more preferably not less than 270° C. from the viewpoint of suppressing the occurrence of undesirable side reactions and achieving a high reaction rate, and is also preferably not more than 350° C., more preferably not more than 310° C., even more preferably not more than 295° C., and even more preferably not more than 290° C. from the viewpoint of high energy efficiency and low load in the facilities.In the present invention, the olefin formation reaction is carried out in a liquid phase reaction. The liquid phase reaction used herein means a reaction carried out at a temperature of not more than a boiling point of the alcohol of raw material, that is, not more than a temperature at which a liquid phase is still present. When the olefin formation reaction is carried out in the liquid phase reaction, it is not necessary to evaporate the total amount of the starting material, and it is therefore possible to suppress an increase in production cost. In addition, it is possible to suppress the occurrence of branching of the olefins due to alkyl rearrangement and production of multimers of the olefins, and thus to produce the target product in high yield.In view of a high yield of the olefins as the target product, the reaction time can be controlled so that the reaction rate of the alcohol is preferably not less than 95%, more preferably not less than 97%, and further preferably not less than 98%. The reaction time may vary depending on the reaction temperature, the kind of the organic solvent used, as well as the kind and amount of the catalyst used, etc. In suspended bed batch reactions, the reaction time is preferably not less than 0.1 hour, more preferably not less than 0.5 hour, and even more preferably not less than 1 hour, and is preferably not more than 20 hours, more preferably not more than 10 hours, and even more preferably not more than 7 hours.In the fixed bed reaction, from the viewpoint of a high yield, LHSV (liquid hourly space velocity) is preferably not less than 0.05 / h, more preferably not less than 0.1 / h, and even more preferably not less than 0.2 / h. For the same reason, LHSV is also preferably not more than 10 / h, more preferably not more than 7 / h, and even more preferably not more than 5 / h.According to the product process of this invention, the reaction rate of the alcohol is usually not less than 80%, preferably not less than 90%, and the yield of the olefins usually reaches not less than 90%. In addition, the production rate of branched olefins and dimers of olefins contained in the resulting olefins are usually not more than 5%. The olefins obtained by the production process of this invention contain a high proportion of internally isomerized olefins, and it is therefore possible to easily obtain the target product with internally isomerized olefins in an amount of 30% or more on the basis of the total olefins.According to the present invention, only the olefins can be separated from the reaction product thus obtained by distillative purification. The high purity olefins thus produced by distillative purification are useful as a starting material or an intermediate for surfactants, organic solvents, plasticizers, sizing agents, etc.[Method for Producing Olefin Sulfonate]The process for producing an olefin sulfonate according to this invention comprises the steps of sulfonating the olefins produced by the above process of this invention to obtain a sulfonated product; and neutralizing the sulfonated product and then subjecting the resulting neutralized product to hydrolysis treatment.The sulfonation reaction in the sulfonated product obtaining step can be carried out by reacting 1 mole of the olefins with preferably not less than 1 mole and not more than 1.2 moles of sulfur trioxide or sulfuric anhydride.The reaction temperature used in the sulfonation reaction is preferably not less than 0° C. and not higher than 40° C. from a high yield point of view.When sulfuric anhydride is used in the sulfonation reaction, the reaction temperature is preferably not less than 0° C. and not higher than 20° C., and more preferably not less than 0° C. and not higher than 10° C. from a high yield point of view.In the step of carrying out a hydrolysis treatment with the neutralized product, neutralization may be carried out by reacting the neutralized product with an alkali aqueous solution so that the alkali aqueous solution is reacted in an amount of not less than 1 mol and not more than 1.5 mol per 1 mol of a stoichiometric amount of a sulfone group in the neutralized product.Examples of the alkali aqueous solution used in neutralization include sodium hydroxide aqueous solution, potassium hydroxide aqueous solution, ammonia aqueous solution, 2-aminoethanol aqueous solution or the like.The hydrolysis reaction can be carried out in the presence of water at a temperature of not less than 90°C and not more than 200°C for not less than 30 minutes and not less than 4 hours.The sulfonation reaction and neutralization reaction can be carried out continuously. After completion of the neutralization reaction, the resulting product can be purified by extraction, washing, etc.In addition to the above-mentioned embodiments, this invention provides the following aspects regarding the process for producing olefins. <1> Process for producing olefins comprising the step of conducting a dehydration reaction of an alcohol in the presence of a solid acidic catalyst, wherein the solid acidic catalyst contains alumina and an oxide of an element having a higher electronegativity than that of aluminum supported on the alumina, wherein the dehydration reaction is a liquid phase reaction and the average pore size of the catalyst is not less than 5 nm and not more than 50 nm. <2> Process for producing the olefins according to the above aspect <1>, wherein an electronegativity of the oxide of the element is preferably not less than 1.6, more preferably not less than 1.7 and more preferably not less than 1.8 and also preferably not more than 2.6 and more preferably not more than 2.0. <3> The process for producing olefins according to the above aspect <1> or <2>, wherein an amount of the oxide of the element supported on the alumina is preferably not less than 0.01 mass %, more preferably not less than 0.1 mass %, even more preferably not less than 0.5 mass % and more preferably not less than 0.8 mass %, and also preferably not more than 10 mass %, more preferably not more than 9 mass %, more preferably not more than 8 mass %, even more preferably not more than 7 mass % and even more preferably not more than 2 mass %, <4> The method for producing olefins according to any one of the above aspects <1> to <3>, wherein the element is at least one element selected from the group consisting of sulfur, tungsten, phosphorus and silicon. <5> The method for producing olefins according to any one of the above aspects <1> to <4>, wherein a method for producing the catalyst by supporting the oxide of the element on the alumina includes the steps of mixing an aqueous suspension or a hydrous solid of the alumina, a compound as an oxide source of the element or the oxide of the element, and ion-exchanged water, for producing an impregnated product and drying and calcining the resulting impregnated product. <6> The process for producing olefins according to the above aspect <5>, wherein the compound as an oxide source of the element is preferably a water-soluble ammonium salt, metal alkoxide or oxo acid or a salt thereof, more preferably at least one compound selected from the group consisting of ammonium sulfate, ammonium tungstate, tetraethyl orthosilicate and diammonium hydrogen phosphate, and even more preferably ammonium sulfate, ammonium tungstate, diammonium hydrogen phosphate or tetraethyl orthosilicate. <7> The process for producing olefins according to the above aspects <5> or <6>, wherein the temperature at which the aluminum oxide is impregnated with the compound as an oxide source of the element or the oxide of the element, A process for producing olefins according to any of the above aspects <5> to <7>, wherein a calcination temperature of the impregnated product is preferably not less than 300° C., more preferably not less than 400° C., more preferably not more than 100° C., more preferably not more than 95° C., more preferably not more than 90° C. and more preferably not more than 80° C., is preferably not less than 300° C., more preferably not less than 400° C., more preferably not less than 450° C. and preferably not more than 900° C., more preferably not more than 850° C., more preferably not more than 800° C., Still more preferably not more than 700°C, and still more preferably not more than 600°C. <9> The process for producing olefins according to any one of the above aspects <5> to <8>, wherein a calcination time of the impregnated product is preferably not less than 1 hour, and more preferably not less than 2 hours, and preferably not more than 10 hours, and more preferably not more than 5 hours. <10> The process for producing olefins according to the above aspects <5> to <9>, wherein the calcination is carried out in an inert gas atmosphere, oxidizing atmosphere, or reducing atmosphere. <11> The process for producing olefins according to any one of the above aspects <5> to <10>, wherein the calcination is preferably carried out in a closed condition or in a gas flow condition, and more preferably in a gas flow of air or oxygen. <12> The process for producing olefins according to any one of the above aspects <1> to <11>, wherein the alumina is γ-alumina. <13> The process for producing olefins according to any one of the above aspects <1> to <12>, wherein the catalyst is produced by at least one process selected from the group consisting of a process evaporated to dryness, an adsorption process, equilibration adsorption process, pore filling process, spraying process and precipitation process. <14> The process for producing olefins according to any one of the above aspects <1> to <13>, wherein an average particle size of the catalyst is preferably not less than 1 μM, more preferably not less than 5 μm, even more preferably not less than 10 μm, even more preferably not less than 20 μm and further preferably not less than 30 μm and is preferably not more than 300 μm, preferably not more than 250 μm, even more preferably not more than 200 μm, further preferably not more than 150 μm, even further preferably not more than 100 μm and further more preferably not more than 50 μm. <15> The process for producing olefins according to any one of the above aspects <1> to <14>, wherein a BET specific surface area of the catalyst is preferably not less than 100 m 2 / g, more preferably not less than 120 m 2 / g and even more preferably not less than 140 m 2 / g and also preferably not more than 500 m 2 / g, more preferably not more than 400 m 2 / g, further preferably not more than 300 m 2 / g and further preferably not more than 200 m 2 / g. <16> Process for producing olefins according to any of the above aspects <1> to <15>, wherein an average pore size of the catalyst is preferably not less than 7 nm, and more preferably not less than 9 nm, and preferably not more than 40 nm, further preferably not more than 25 nm, A process for producing olefins according to any one of the above aspects <1> to <16>, wherein a pore volume of the catalyst is preferably not less than 0.20 cm 3 / g, more preferably not less than 0.25 cm 3 / g, and more preferably not less than 0.30 cm 3 / g, and also preferably not more than 2.0 cm 3 / g, more preferably not more than 1.5 cm 3 / g, even more preferably not more than 1.2 cm 3 / g, even more preferably not more than 20 nm, and even more preferably not more than 15 nm, further preferably not more than 1.0 cm 3 / g and even more preferably not more than 0.7 cm 3 / g. <18> Process for producing olefins according to any of the above aspects <1> to <17>, in which the alcohol is a primary alcohol. <19> Process for producing olefins according to any of the above aspects <1> to <18>, in which the number of carbon atoms contained in the alcohol is preferably not less than 8, more preferably not less than 12 and even more preferably not less than 14 and likewise preferably not more than 22, more preferably not more than 20 and even more preferably not more than 18. <20> Process for producing olefins according to any of the above aspects <1> to <19>, in which the number of carbon atoms contained in the alcohol is preferably not less than 8, more preferably not less than 12 and even more preferably not less than 14, The process for producing olefins according to any one of the above aspects <1> to <20> wherein the dehydration reaction is carried out while removing water produced therein from the reaction system. <22> The process for producing olefins according to any one of the above aspects <1> to <21> The process for producing olefins according to any one of the above aspects <1> to <21> wherein the dehydration reaction is carried out while introducing an inert gas into the reaction system. <23> The process for producing olefins according to any one of the above aspects <1> to <22>, wherein the dehydration reaction is carried out under a reduced pressure of not less than 0.03 MPa and not more than 0.09 MPa or under a normal pressure. <24> The process for producing olefins according to any one of the above aspects <1> to <23>, wherein the dehydration reaction is preferably carried out at a temperature of not more than a boiling point of the alcohol as a starting material, more specifically at a temperature of preferably not less than 150° C., more preferably not less than 200° C., even more preferably not less than 220° C., even more preferably not less than 230° C., and further preferably not less than 270° C., and also preferably at not more than 350° C., more preferably not more than 310° C., even more preferably not more than 295° C., and further preferably not more than 290° C.ExamplesCatalyst Preparation Example 1A 500 ml eggshell flask was charged with 10.0 g of alumina "GP-20" (available from Mizusawa Industrial Chemicals, Ltd.: BET specific surface area: 189 m 2 / g, average particle size: 33 μm, average pore size: 12.1 nm, pore volume: 0.44 cm 3 / g), 0.69 g of ammonium sulfate (available from Wako Pure Chemical Industries, Ltd.: 5 mass % in terms of SO 4 based on alumina) and 100 g of ion-exchanged water, and water was evaporated to dryness using a rotary evaporator (70° C.; 30 mmHg). The resulting powder was dried at 120°C for 12 hours and calcined in air at 500°C for 3 hours to obtain an acidic solid catalyst. The resulting solid acid catalyst had a BET specific surface area of 162 m 2 / g, an average particle size of 36 μm, an average pore size of 11.8 nm, and a pore volume of 0.41 cm 3 / g.Catalyst Preparation Example 2The same procedure as in Catalyst Preparation Example 1 was repeated except for using 0.56 g of ammonium tungstate (available from Wako Pure Chemical Industries, Ltd.: 5 mass % in terms of WO 3 based on alumina) in place of ammonium sulfate to prepare a solid acid catalyst. The resulting solid acid catalyst had a BET specific surface area of 159 m 2 / g, an average particle size of 34 μm, an average pore size of 11.7 nm, and a pore volume of 0.40 cm 3 / g.Catalyst Preparation Example 3The same procedure as in Catalyst Preparation Example 1 was repeated except for using 0.65 g of diammonium hydrogen phosphate (available from Wako Pure Chemical Industries, Ltd.: 5 mass % in terms of PO 4 based on alumina) in place of ammonium sulfate to prepare a solid acid catalyst. The resulting solid acid catalyst had a BET specific surface area of 154 m 2 / g, an average particle size of 33 μm, an average pore size of 11.9 nm, and a pore volume of 0.41 cm 3 / g.Catalyst Preparation Example 4The same procedure as in Catalyst Preparation Example 1 was repeated except for using 1.73 g of tetraethyl orthosilicate (available from Wako Pure Chemical Industries, Ltd.: 5 mass % in terms of SiO 2 based on alumina) and 0.2 g of 0.1 N aqueous nitric acid solution instead of ammonium sulfate to prepare a solid acid catalyst. The resulting solid acid catalyst had a BET specific surface area of 158 m 2 / g, an average particle size of 38 μm, an average pore size of 11.8 nm, and a pore volume of 0.42 cm 3 / g.Catalyst Preparation Example 5The same procedure as in Catalyst Preparation Example 1 was repeated except for using 0.14 g of ammonium sulfate (available from Wako Pure Chemical Industries, Ltd.: 1 mass % in terms of SO 4 based on alumina) to prepare a solid acid catalyst. The resulting solid acidic catalyst had a BET specific surface area of 164 m 2 / g, an average particle size of 35 μm, an average pore size of 11.9 nm, and a pore volume of 0.42 cm 3 / g.Catalyst Preparation Example 6The same procedure as in Catalyst Preparation Example 1 was repeated except for using 0.12 g of ammonium tungstate (available from Wako Pure Chemical Industries, Ltd.: 1 mass % in terms of WO 3 based on alumina) instead of ammonium sulfate to prepare a solid acid catalyst. The resulting solid acidic catalyst had a BET specific surface area of 152 m 2 / g, an average particle size of 36 μm, an average pore size of 12.0 nm, and a pore volume of 0.41 cm 3 / g.Catalyst Preparation Example 7The same procedure as in Catalyst Preparation Example 1 was repeated except for using 0.35 g of tetraethyl orthosilicate (available from Wako Pure Chemical Industries, Ltd.: 1 mass % in terms of SiO 2 based on alumina) and 0.1 g of 1N aqueous nitric acid solution instead of ammonium sulfate to prepare a solid acid catalyst. The resulting solid acid catalyst had a BET specific surface area of 110 m 2 / g, an average particle size of 35 μm, an average pore size of 11.9 nm, and a pore volume of 0.41 cm 3 / g.Comparative Catalyst Preparation Example 1The same procedure as in Catalyst Preparation Example 1 was repeated except for using 1.25 g of cerium nitrate (available from Wako Pure Chemical Industries, Ltd.: 5 mass % in terms of CeO 2 based on alumina) in place of ammonium sulfate to prepare a solid acid catalyst. The resulting solid acid catalyst had a BET specific surface area of 154 m 2 / g, an average particle size of 35 μm, an average pore size of 11.9 nm, and a pore volume of 0.41 cm 3 / g.Comparative Catalyst Preparation Example 2The same procedure as in Catalyst Preparation Example 1 was repeated except for using 1.33 g of lanthanum nitrate (available from Wako Pure Chemical Industries, Ltd.: 2.5 mass % in terms of La 2 O 3 based on alumina) in place of ammonium sulfate to prepare a solid acid catalyst. The resulting solid acid catalyst had a BET specific surface area of 159 m 2 / g, an average particle size of 34 μm, an average pore size of 11.9 nm, and a pore volume of 0.42 cm 3 / g.Example 1[Olefination reaction]100 A four-necked ml flask equipped with a stirrer was charged with 50.0 g (0.19 mol) of 1-octadecanol "KALCOL 8098" (available from Kao Corp.) and 1.5 g (3 mass % based on the alcohol) of the solid acid catalyst prepared in Catalyst Preparation Example 1, and the content of the flask was reacted at 280° C. for one hour with stirring while nitrogen flowed through the reaction system (nitrogen flow rate: 50 ml / min).After completion of the reaction, the resulting reaction solution was diluted with hexane, and the resulting diluted solution was analyzed using a gas chromatographic analyzer "HP6890" (available from HEWLETT PACKARD Co.) equipped with a column "Ultra ALLOY-1" (available from Frontier Laboratories Ltd.; capillary column: 30.0 m × 250 μm) and a flame ionization detector (FID) under the conditions of an injection temperature of 300°C, a detector temperature of 350°C, a flow rate of He of 4.6 ml / min to conduct quantitative determination of the resulting reaction product. The results are shown in Table 1.The yield of the olefins was calculated according to the following formula:Examples 2 to 9 and Comparative Examples 1 to 4[Olefination reaction]The reaction was carried out in the same manner as in Example 1 except that the catalyst and the reaction conditions therein were changed as in Table 1, and the reaction solution obtained after completion of the reaction was subjected to measurement. The reaction conditions and the results are collectively shown in Table 1. In Comparative Example 1, only the alumina used in Catalyst Production Example 1 was used as a catalyst. Table 1 Table 1Catalyst*a*b*c*d*e*f*gSupported ElementS. SW. WPSiIS. SW. WSiIElectronegativity2,51,72, 11, 82,51,71, 8Carried Amount* 1 (mass %)5555111Alcohol as starting material*1*1*1*1*1*1*1Amount of catalyst * 2 (mass %)3333333Reaction temperature (° C.)280280280280280280280Reaction time (h)1553554Yield of olefins (%)89807694949896Production Rate of Dimer (%)6,84,35,06,14,31,53,5Selectivity to Monomeric Olefins (%)93959494969896Note: *a: Catalyst Preparation Example 1; *b: Catalyst Preparation Example 2; *c: Catalyst Preparation Example 3; *d: Catalyst Preparation Example 4; *e: Catalyst Preparation Example 5; *f: Catalyst Preparation Example 6; *g: Catalyst Preparation Example 7; *h: Alumina; *i:Comparative Catalyst Preparation Example 1; *j: Comparative Catalyst Preparation Example 2; *k: Silica-Alumina*3; *1: Octadecanol; *m: Tetradecanol*1: Value as an alumina-based oxide*2: Amount based on alcohol as a starting material*3: available from JGC Catalysts and Chemicals Ltd.; Si / Al = 81 / 19 (molar ratio)Table 1 (continuation)Table 1 (continuation)Catalyst*f*g*h*i*j*kSupported ElementW. WSiI-CeELa-Electronegativity1, 71, 8-1,11,1-Carried Amount* 1 (mass %)11-55-Alcohol as starting material*m*m*1*1*1*1Amount of catalyst * 2 (mass %)10103333Reaction temperature (° C.)240240280280280280Reaction time (h)865552Yield of olefins (%)97945710684Production Rate of Dimer (%)2, 13,93,41,00,016,0Selectivity to Monomeric Olefins (%)9896949110084Note: *a: Catalyst Preparation Example 1; *b: Catalyst Preparation Example 2; *c: Catalyst Preparation Example 3; *d: Catalyst Preparation Example 4; *e: Catalyst Preparation Example 5; *f: Catalyst Preparation Example 6; *g: Catalyst Preparation Example 7; *h: Alumina; *i: Comparative Catalyst Preparation Example 1; *j: Comparative Catalyst Preparation Example 2; *k: Silica-Alumina*3; *1: Octadecanol; *m: Tetradecanol*1: Value as an alumina-based oxide*2: Amount based on alcohol as a starting material*3: available from JGC Catalysts and Chemicals Ltd.; Si / Al = 81 / 19 (molar ratio)From the results of Table 1, it was confirmed that when the catalyst carrying the element having a higher electronegativity than aluminum was used, the olefins were produced in a very high yield.As described above, according to the production method of the present invention, it is possible to produce long-chain olefins in high yield for a short period of time by subjecting a long-chain aliphatic primary alcohol to a dehydration reaction.Example 10 [Sulfonation Reaction]Step for obtaining a sulfonated productA 3000 ml four-necked flask was equipped with a mechanical stirrer and a thermometer and further with two dropping funnels. The inside of the four-necked flask was maintained under reduced pressure and then flooded with nitrogen to bring an internal pressure of the flask to atmospheric pressure. Then, 211 g of 1,4-dioxane (available from Wako Pure Chemical Industries, Ltd.) and 975 g of chloroform (available from Wako Pure Chemical Industries, Ltd.) were added to the flask. The resulting reaction solution in the four-necked flask was cooled to a temperature of 5°C or less in an ice bath. After cooling, 56.8 g of sulfuric anhydride (sulfur trioxide) "NISSO SULFAN" (available from Nisso Metalochemical Co., Ltd.) was added dropwise to the flask through a dropping funnel over one hour. After completion of the dropwise addition, the contents of the flask were stirred for 0.5 hour. Thereafter, 152 g of the olefins produced in Example 5 was added dropwise to the flask through a dropping funnel over an hour.Steps of neutralization and hydrolysis treatmentA 3000 ml SUS beaker was charged with 119 g of a 48 mass % aqueous sodium hydroxide solution and 302 g of ion-exchanged water, and the contents of the beaker were cooled in an ice bath. After sufficiently cooling, while continuously cooling the contents of the beaker in an ice bath, the reaction solution obtained in the above reaction step was gradually added to the beaker while the contents of the beaker were stirred using a homomixer. After adding the whole amount of the reaction solution obtained in the above reaction step to the beaker, the contents of the beaker were stirred at 5000 rpm for 3 hours.The reaction solution obtained in the neutralization step was charged into an egg-shaped flask, and while heating the contents of the flask in a hot water bath at 55°C, chloroform, 1,4-dioxane and water were distilled off therefrom using a rotary evaporator. The resulting concentrated product was mixed with 670 g of ion-exchanged water to prepare an aqueous solution comprising sodium olefin sulfonate at a concentration of 40 mass %. Then, 400 g of the aqueous solution thus prepared was placed in a 1 liter autoclave and reacted at 160°C for 3 hours to obtain 385 g of an aqueous solution of sodium olefinsulfonate.The content of the effective components in the aqueous sodium olefin sulfonate solution thus obtained was 16% by mass. The content of the effective components in the aqueous solution was determined by a potentiometric titration method using a benzethonium chloride solution (JIS K3362 "Testing Method for Synthetic Detergents").

Claims

A process for producing olefins, comprising the step of conducting a dehydration reaction with an alcohol having not less than 8 and not more than 22 carbon atoms in the presence of a solid acidic catalyst, wherein the solid acidic catalyst contains alumina and an oxide of an element having a higher electronegativity than that of aluminum supported on the alumina, wherein the dehydration reaction is a liquid phase reaction, and the average pore size of the catalyst is not less than 5 nm and not more than 50 nm.The process for producing olefins according to claim 1, wherein the element is at least one element selected from the group consisting of sulfur, tungsten, phosphorus and silicon.The process for producing olefins according to claim 1 or 2, wherein an amount of the oxide of the element supported on the alumina is not less than 0.01 mass% and not more than 10 mass% based on the amount of alumina.The process for producing olefins according to any one of claims 1 to 3, wherein the alumina is γ-alumina.The process for producing olefins according to any one of claims 1 to 4, wherein the alcohol is a primary alcohol.The process for producing olefins according to any one of claims 1 to 5, wherein the dehydration reaction is carried out at a temperature of not less than 150°C and not more than 350°C.The process for producing olefins according to any one of claims 1 to 6, wherein a process for producing the catalyst by supporting the oxide of the element on the alumina comprises the step of mixing an aqueous suspension or a hydrous solid of the alumina, a compound as an oxide source of the element or the oxide of the element and ion-exchanged water to produce an impregnated product, and drying and calcining the resulting impregnated product.The process for producing olefins according to claim 7, wherein the compound as an oxide source of the element is a water-soluble ammonium salt, a metal alkoxide or an oxoacid, or a salt thereof.The process for producing olefins according to any one of claims 1 to 8, wherein the dehydration reaction is carried out while removing water produced therein from the reaction system.The process for producing olefins according to any one of claims 1 to 9, wherein the dehydration reaction is carried out while an inert gas is introduced into the reaction system.The process for producing olefins according to any one of claims 1 to 10, wherein the BET specific surface area of the catalyst is not less than 100 m 2 / g and not more than 500 m 2 / g.The process for producing olefins according to any one of claims 1 to 11, wherein the pore volume of the catalyst is not less than 0.20 cm 3 / g and not more than 2.0 cm 3 / g.A process for producing an olefin sulfonate, comprising the steps of: sulfonating the olefins produced by the process according to any one of claims 1 to 12 to obtain a sulfonated product, and neutralizing the sulfonated product, and then performing a hydrolysis treatment on the resulting neutralized product.

Citation Information

Patent Citations

  • Method for preparing isoolefin

    JP2008056671A

  • A highly sensitive quantitative detection method for 8-oxo-2'-deoxyguanosine in an aqueous sample solution

    JP5940057B2

  • Method for manufacturing olefins

    WO2011052732A1

  • Method for producing terminal olefins

    US3246045A

  • Dehydration of primary alcohols

    WO1997003932A1