Silicon carbide semiconductor device and method for its manufacture
Patent Information
- Application Number
- DE112014001539
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2013-03-19
- Filing Date
- 2014-02-04
- Publication Date
- 2024-11-28
- Estimated Expiration
- Not applicable · inactive patent
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Technical area
[0001] The present invention relates to a silicon carbide semiconductor device and a method for manufacturing the silicon carbide semiconductor device, particularly to a silicon carbide semiconductor device having a trench and a method for manufacturing the silicon carbide semiconductor device. State of the art
[0002] Published Japanese Patent Application JP H7-326755 A (Patent Document 1) discloses a trench MOSFET (metal oxide semiconductor field-effect transistor) using a silicon carbide substrate. According to this publication, the thickness of a gate thermal oxidation film on the bottom surface of the trench is greater than the thickness of the gate thermal oxidation film on the side surface of the trench. Citation listPatent document
[0003] PTD1: Published Japanese patent application JP H7- 326 755 A Summary of the inventionTechnical problem
[0004] The goal is to achieve a lower gate electrode capacitance in a semiconductor device with a gate electrode. For example, in a MISFET (metal insulator semiconductor field-effect transistor), a lower capacitance between the gate electrode and the drain electrode is desired as a feedback capacitance. According to the method described in the above publication, the gate electrode capacitance can be reduced to some extent by forming a thick gate insulating film (gate thermal oxidation film) on the bottom surface, but it is desirable to achieve an even lower gate electrode capacitance.
[0005] Document WO 2012 / 098861 A relates to a semiconductor device comprising a silicon carbide layer on a main surface of a substrate, a trench having a bottom surface and side surfaces disposed in the silicon carbide layer, an insulating film on the bottom surface and side surfaces of the trench, and a conductor layer insulated from the silicon carbide layer by the insulating film. The conductor layer is made of silicon. The insulating film has a first insulating layer on the bottom surface and side surfaces of the trench and a second insulating layer made of silicon disposed between the part of the first insulating layer lying on the bottom surface of the trench and the conductor layer. The second insulating layer is in contact with the conductor layer, and the thickness of the insulating film on the bottom surface of the trench is three times or more of the thickness on the side surfaces of the trench.
[0006] Document JP2009-224365 A relates to a semiconductor device having a trench structure. The semiconductor device includes: a first n-type semiconductor layer; a second 2n-type semiconductor layer; a p-type semiconductor layer; a trench penetrating the p-type semiconductor layer and reaching the second 2n-type semiconductor layer; an insulating layer formed on the bottom and side of the trench along the surface of the trench; a gate electrode insulated from the second 2n-type semiconductor layer and the p-type semiconductor layer by the insulating layer and formed at least partially in the trench; and an n-type semiconductor region formed around the trench on the p-type semiconductor layer.
[0007] The present invention has been conceived to solve the above-described problem, and it is an object of the present invention to provide a silicon carbide semiconductor device having a small gate electrode capacitance and a method for manufacturing the silicon carbide semiconductor device.
[0008] A silicon carbide semiconductor device of the present invention includes a silicon carbide substrate, a gate insulating film, and a gate electrode. The silicon carbide substrate includes a first semiconductor layer, a second semiconductor layer, and a third semiconductor layer, wherein the first semiconductor layer has a first conductivity type, the second semiconductor layer is provided on the first semiconductor layer, the second semiconductor layer has a second conductivity type, the third semiconductor layer is provided on the second semiconductor layer, the third semiconductor layer is separated from the first semiconductor layer by the second semiconductor layer, and the third semiconductor layer has the first conductivity type. The silicon carbide substrate is formed with a trench.The trench includes a bottom surface and a sidewall surface, the bottom surface being formed from the first semiconductor layer, and the sidewall surface having first to third sidewall surfaces formed from the first to third semiconductor layers, respectively. The gate insulating film is provided on the trench. The gate insulating film includes a first insulating film and a second insulating film, the first insulating film directly covering both the sidewall surface and bottom surface, and the second insulating film being provided on the first insulating film. The first insulating film includes a first bottom portion and a first sidewall portion, the first bottom portion being arranged on the bottom surface and the first sidewall portion being arranged on the sidewall surface. The first sidewall portion includes first to third regions arranged on the first to third sidewall surfaces, respectively.The second insulating film has a second bottom portion and a second sidewall portion, the second bottom portion being disposed on the first bottom portion and the second sidewall portion being disposed on the first sidewall portion. The second sidewall portion is formed with one end and the other end, one end being connected to the second bottom portion, the other end being disposed on one of the first and second regions, and the other end being separated from the third region. The gate electrode is formed on the trench with the gate insulating film interposed therebetween. The second insulating film includes a thermal oxidation film made of a film including silicon and no carbon. A method for manufacturing a silicon carbide semiconductor device of the present invention includes the following steps: First, a silicon carbide substrate is prepared which has a first semiconductor layer, a second semiconductor layer and a third semiconductor layer, wherein the first semiconductor layer has a first conductivity type, the second semiconductor layer is provided on the first semiconductor layer, the second semiconductor layer has a second conductivity type, the third semiconductor layer is provided on the second semiconductor layer, the third semiconductor layer is separated from the first semiconductor layer by the second semiconductor layer and the third semiconductor layer has the first conductivity type.
[0009] A trench is formed in the silicon carbide substrate. The trench includes a bottom surface and a sidewall surface, wherein the bottom surface is formed from the first semiconductor layer, and the sidewall surface has first to third side surfaces, each formed from the first to third semiconductor layers.
[0010] A first insulating film is formed directly on the sidewall surface and the bottom surface. The first insulating film includes a first bottom portion and a first sidewall portion, the first bottom portion being disposed on the bottom surface and the first sidewall portion being disposed on the sidewall surface. The first sidewall portion includes first to third regions disposed on the first to third side surfaces, respectively.
[0011] A silicon film is formed on the first insulating film. The silicon film includes a second bottom portion and a second sidewall portion, the second bottom portion being disposed on the first bottom portion, and the second sidewall portion being disposed on the first sidewall portion. The second sidewall portion is formed with one end and another end, the other end being connected to the second bottom portion, the other end being disposed on the first or second region, and the other end being separated from the third region.
[0012] A second insulating film is formed by oxidizing the silicon film. The first and second insulating films form a gate insulating film.
[0013] A gate electrode is formed on the trench with the gate insulating film interposed therebetween. Advantageous effects of the invention
[0014] According to the present invention, the gate electrode capacitance can be reduced. Short description of the drawings Fig. 1 is a partial cross-sectional view schematically showing a structure of the silicon carbide semiconductor device of a first embodiment of the present invention. Fig. Fig. 2 is a perspective view schematically showing a shape of a silicon carbide substrate used in the Fig. 1 shown silicon carbide semiconductor device. Fig. 3 shows a more detailed structure of the Fig. 2, wherein for the purpose of illustration in the figure an area with the second conductivity type is shown hatched. Fig. 4 shows an enlarged view of the Fig. 1, in particular to represent a component of a first insulating film. Fig. 5 shows an enlarged view of the Fig. 1, specifically to show the dimension of a gate insulating film. Fig. Fig. 6 is a partial cross-sectional view schematically showing a first step of a method for manufacturing the silicon carbide semiconductor device of the Fig. 1 represents. Fig. Fig. 7 is a partial cross-sectional view schematically showing a second step of the method for manufacturing the silicon carbide semiconductor device of Fig. 1 represents. Fig. Fig. 8 is a partial cross-sectional view schematically showing a third step of the method for manufacturing the silicon carbide semiconductor device of Fig. 1 represents. Fig. Fig. 9 is a partial cross-sectional view schematically showing a fourth step of the method for manufacturing the silicon carbide semiconductor device of the Fig. 1 represents. Fig. Fig. 10 is a partial cross-sectional view schematically showing a fifth step of the method for manufacturing the silicon carbide semiconductor device of the Fig. 1 represents. Fig. Fig. 11 is a partial cross-sectional view schematically showing a sixth step of the method for manufacturing the silicon carbide semiconductor device of the Fig. 1 represents. Fig. Fig. 12 is a partial cross-sectional view schematically showing a seventh step of the method for manufacturing the silicon carbide semiconductor device of the Fig. 1 represents. Fig. Fig. 13 is a partial cross-sectional view schematically showing an eighth step of the method for manufacturing the silicon carbide semiconductor device of the Fig. 1 represents. Fig. Fig. 14 is a partial cross-sectional view schematically showing a ninth step of the method for manufacturing the silicon carbide semiconductor device of the Fig. 1 represents. Fig. Fig. 15 is a partial cross-sectional view schematically showing a tenth step of the method for manufacturing the silicon carbide semiconductor device of the Fig. 1 represents. Fig. Fig. 16 is a partial cross-sectional view schematically showing an eleventh step of the method for manufacturing the silicon carbide semiconductor device of the Fig. 1 represents. Fig. Fig. 17 is a partial cross-sectional view schematically showing a twelfth step of the method for manufacturing the silicon carbide semiconductor device of the Fig. 1 represents. Fig. Fig. 18 is a partial cross-sectional view schematically showing a thirteenth step of the method for manufacturing the silicon carbide semiconductor device of the Fig. 1 represents. Fig. 19 is a partial cross-sectional view schematically showing a structure of a silicon carbide semiconductor device according to a second embodiment of the present invention. Fig. 20 is a partial cross-sectional view schematically showing a structure of a silicon carbide semiconductor device according to a third embodiment of the present invention. Fig. 21 is a partial cross-sectional view schematically showing a fine structure of a surface of a silicon carbide substrate provided in the silicon carbide semiconductor device. Fig. Figure 22 shows a crystal structure of a ((000-1) plane in a hexagonal 4H polytype crystal. Fig. Figure 23 shows a crystal structure of a (11-20) plane along a line XXIII-XXIII of the Fig. 22. Fig. Figure 24 shows a crystal structure near a surface with a combined plane of Fig. 21 within a (11-20) plane. Fig. 25 shows the combined level of Fig. 21 from the perspective of a (01-10) level. Fig. 26 is a diagram showing an exemplary relationship between the channel mobility and an angle between a channel surface and the (000-1) plane from a macroscopic point of view, for both a case where a thermal etching step is performed and a case where a thermal etching step is not performed. Fig. 27 is a diagram illustrating an exemplary relationship between channel mobility and an angle between a channel direction and a <0-11-2> direction. Fig. 28 shows a modification of the Fig. 21. Fig. 29 shows a relationship between a capacity C gd between a gate electrode and a drain electrode and a voltage V DSbetween the drain electrode and a source electrode. Description of the embodiments
[0015] In the following, an overview of the embodiments with regard to points (i) to (xiii) is first described.
[0016] (i) Each of the silicon carbide semiconductor devices 501 to 503 includes a silicon carbide substrate 100, a gate insulating film 200, and a gate electrode 230. The silicon carbide substrate 100 includes a first semiconductor layer 121, a second semiconductor layer 122, and a third semiconductor layer 123, wherein the first semiconductor layer 121 has a first conductivity type, the second semiconductor layer 122 is provided on the first semiconductor layer 121, the second semiconductor layer 122 has a second conductivity type, the third semiconductor layer 123 is provided on the second semiconductor layer 122, the third semiconductor layer 123 is separated from the first semiconductor layer 121 by the second semiconductor layer 122, and the third semiconductor layer 123 has the first conductivity type. The silicon carbide substrate 100 is formed with a trench TR.The trench TR includes a bottom surface BT and a sidewall surface SW, wherein the bottom surface BT is formed from the first semiconductor layer 121, and the sidewall surface SW has first to third sidewall surfaces SW1 to SW3, each formed from the first to third semiconductor layers 121 to 123. The gate insulating film 200 is provided on the trench TR. The gate insulating film 200 includes a first insulating film 201 and a second insulating film 202, wherein the first insulating film 201 directly covers both the sidewall surface SW and the bottom surface BT, and wherein the second insulating film 202 is provided on the first insulating film 201. The first insulating film 201 includes a first bottom portion 201B and a first sidewall portion 201S, wherein the first bottom portion 201B is disposed on the bottom surface BT, and the first sidewall portion 201S is disposed on the sidewall surface SW.The first sidewall portion 201S includes first to third regions 201a to 201c, which are respectively disposed on the first to third sidewall surfaces SW1 to SW3. The second insulating film 202 includes a second bottom portion 202B and a second sidewall portion 202S, wherein the second bottom portion 202B is disposed on the first bottom portion 201B, and the second sidewall portion 202S is disposed on the first sidewall portion 201S. The second sidewall portion 202S is formed of one end E1 and another end E2, wherein one end E1 is connected to the second bottom portion 202B, the other end E2 is disposed on the first or second region 202a, 202b, and the other end E2 is separated from the third region 201c. The gate electrode 230 is provided on the trench TR with the gate insulating film 200 interposed therebetween.The second insulating film 202 comprises a thermal oxidation film made of a film containing silicon and no carbon.
[0017] According to each of the silicon carbide semiconductor devices 501 to 503, the second insulating film 202, which together with the first insulating film 201 forms the gate insulating film 200, is formed not only on the first bottom portion 201B of the first insulating film 201 but also on the first sidewall portion 201S of the first insulating film 201. Accordingly, the gate insulating film 200 has a greater thickness not only on the bottom surface BT of the trench TR but also on the sidewall surface SW, which, together with the bottom surface BT, forms the corner portion CR near the bottom surface BT. Thus, the gate electrode capacitance can be reduced compared to the case where the gate insulating film 200 is formed thick only on the bottom surface BT of the trench. Since the thermal oxidation film comprises a film including silicon and no carbon, the breakdown voltage of each of the silicon carbide semiconductor devices 501 to 503 can be further increased.
[0018] (ii) According to item (i), the other end E2 of the second sidewall portion 202S may be arranged on an interface between the first region 201a and the second region 201b.
[0019] Accordingly, the second sidewall portion 202S extends at most to such an extent that it does not overlap the second region 201b forming the channel surface. Thus, the gate electrode capacitance can be effectively reduced to such an extent that the channel characteristics are hardly affected.
[0020] (iii) According to item (i), the other end E2 of the second sidewall portion 202S may be formed away from the second region 201b and disposed on the first region 201a.
[0021] Accordingly, the second sidewall portion 202S extends to such an extent that it is not located near the second region 201b forming the channel surface. Thus, the gate electrode capacitance can be reduced to such an extent that the channel characteristics are not affected.
[0022] (iv) According to item (i), the other end E2 of the second sidewall portion 202S may be formed away from the third region 201c and disposed on the second region 201b.
[0023] Accordingly, the second sidewall portion 202S extends further than in the case where the second sidewall portion 202S is provided only on the first region 201a. Furthermore, the second sidewall portion 202S is provided away from the interface between the second region 201b and the third region 201c, which has a great influence on the channel properties. Thus, the gate electrode capacitance can be more effectively reduced while suppressing the deterioration of the channel properties.
[0024] (v) According to item (iv), the second semiconductor layer 122 may have a depth position DP at which an impurity concentration has a maximum value, and the other end E2 of the second sidewall portion 202S may be arranged deeper than the depth position DP.
[0025] Accordingly, the second sidewall portion 202S extends further than in the case where the second sidewall portion 202S is provided only on the first region 201a. Furthermore, the second sidewall portion 202S is formed away from the depth position DP, which has a great influence on the channel characteristics. Thus, the gate electrode capacitance can be more effectively reduced while suppressing the deterioration of the channel characteristics.
[0026] (vi) According to items (i) to (v), the other end E2 of the second side wall portion 202S may have an inclination angle AG of less than 70° with respect to the first side wall portion 201S.
[0027] Accordingly, variations in the thickness of the gate insulating film 200 at the other end E2 are reduced.
[0028] (vii) According to items (i) to (vi), the first and second insulating films 201, 202 may each have a first and a second carbon atom concentration, wherein the second carbon atom concentration is lower than the first carbon atom concentration.
[0029] Accordingly, the second insulating film 202 has a high dielectric breakdown strength due to the low carbon atom concentration. Thus, each of the silicon carbide semiconductor devices 501 to 503 has a high breakdown voltage.
[0030] (viii) According to point (vii), the first carbon atom concentration is more than 1 × 10 15 cm -3 and the second carbon atom concentration is less than 1 × 10 15 cm -3Accordingly, the carbon atom concentration of the second insulating film 202 can be made sufficiently low. Thus, the breakdown voltage of each of the silicon carbide semiconductor devices 501 to 503 can be further increased.
[0031] (ix) According to items (i) to (viii), the second insulating film 202 may be formed of silicon oxide and / or silicon nitride and / or phosphosilicate glass.
[0032] Accordingly, the breakdown voltage of each of the silicon carbide semiconductor devices 501 to 503 can be further increased.
[0033] (xi) A method for manufacturing each of the silicon carbide semiconductor devices 501 to 503 includes the following steps.
[0034] First, a silicon carbide substrate 100 is formed with a first semiconductor layer 121, a second semiconductor layer 122, and a third semiconductor layer 123, wherein the first semiconductor layer 121 has a first conductivity type, the second semiconductor layer 122 is formed on the first semiconductor layer 121, the second semiconductor layer 122 has a second conductivity type, the third semiconductor layer 123 is provided on the second semiconductor layer 122, the third semiconductor layer 123 is separated from the first semiconductor layer 121 by the second semiconductor layer 122, and the third semiconductor layer 123 has the first conductivity type.
[0035] A trench TR is formed in the silicon carbide substrate 100. The trench TR includes a bottom surface BT and a sidewall surface SW, wherein the bottom surface BT is formed from the first semiconductor layer 121, and the sidewall surface SW has first to third side surfaces SW1 to SW3, each formed from the first to third semiconductor layers 121 to 123.
[0036] A first insulating film 201 is formed to directly cover both the sidewall surface SW and the bottom surface BT. The first insulating film 201 includes a first bottom portion 201B and a first sidewall portion 201S, with the first bottom portion 201B being disposed on the bottom surface BT, and the first sidewall portion 201S being disposed on the sidewall surface SW. The first sidewall portion 201S includes first to third regions 201a to 201c, which are disposed on the first to third side surfaces SW1 to SW3, respectively.
[0037] A silicon film 302 is formed on the first insulating film 201. The silicon film 302 includes a second bottom portion 202B and a second sidewall portion 202S, wherein the second bottom portion 202B is disposed on the first bottom portion 201B, and the second sidewall portion 202S is disposed on the first sidewall portion 201S. The second sidewall portion 202S is formed of one end E1 and another end E2, wherein one end E1 is connected to the second bottom portion 202B, the other end E2 is disposed on the first region or the second region 201a, 201b, and the other end E2 is separated from the third region 201c.
[0038] A second insulating film 202 is formed by oxidizing the silicon film 302. The first and second insulating films 201, 202 form a gate insulating film 200.
[0039] A gate electrode 230 is formed on the trench TR with the gate insulating film 200 interposed therebetween.
[0040] According to the manufacturing method, the second insulating film 202, which together with the first insulating film 201 forms the gate insulating film 200, is formed not only on the first bottom portion 201B of the first insulating film 201, but also on the first sidewall portion 201S of the first insulating film 201. Accordingly, the gate insulating film 200 has a greater thickness not only on the bottom surface BT of the trench, but also on the sidewall surface SW, which, together with the bottom surface BT, forms the corner portion CR near the bottom surface BT. Thus, the gate electrode capacitance can be reduced more than in the case where the gate insulating film 200 is formed thick only on the bottom surface BT of the trench.
[0041] (xii) According to item (xi), the step of forming the second insulating film 202 may be performed by oxidizing the silicon film 302 at not less than 800°C and not more than 1150°C.
[0042] By oxidizing the silicon film 302 at no less than 800°C, the surface roughness of the silicon film 302 can be suppressed. Furthermore, by oxidizing the silicon film at no more than 1150°C, it is possible to suppress an increase in the vapor pressure of the second insulating film 202, which is formed from silicon dioxide and is formed by oxidizing the silicon film 302. Consequently, the shape of the second insulating film 202 can be maintained.
[0043] (xiii) According to item (xi), the step of forming the second insulating film 202 may include a step of heating the second sidewall portion 202S to reduce an angle AG of the other end E2 of the second sidewall portion 202S with respect to the first sidewall portion 201S.
[0044] Accordingly, a change in the thickness of the gate insulating film 200 at the other end E2 can be reduced.
[0045] (xiv) According to item (xiii), the step of heating the second sidewall portion 202S may be performed at not less than 1300°C and not more than 1400°C.
[0046] Accordingly, the angle AG of the other end E2 can be made sufficiently small without using too high a temperature.
[0047] For a more detailed description of the embodiments of the present invention, the first to third embodiments and additional aspects are described below. Regarding the crystallographic notations in this specification, a single orientation is represented by [], a group orientation by <>, a single plane by (), and a group plane by {}. Furthermore, a negative crystallographic index is usually represented by placing a "-" (bar) above a number; in this specification, this is expressed by placing a negative sign in front of the number. (First embodiment)
[0048] As in Fig. 1, a vertical MOSFET 501 (silicon carbide semiconductor device) of the present embodiment includes an epitaxial substrate 100 (silicon carbide substrate), gate insulating films 200, gate electrodes 230, interlayer insulating films 203, source electrodes 221, a drain electrode 211, a source interconnection 222, and a guard electrode 212.
[0049] The epitaxial substrate 100 is made of silicon carbide and has a single-crystal substrate 110 and an epitaxial layer thereon. The single-crystal substrate 110 has the n-type conductivity (the first conductivity type). The plane orientation (hklm) of a main surface (top surface in Fig. 1) of the single-crystal substrate 110 preferably has a negative m-value, and more preferably is approximately a (000-1) plane. The epitaxial layer comprises an n -Layer 121 (first semiconductor layer), p-body layers 122 (second semiconductor layer), n-regions 123 (third semiconductor layer), and contact regions 124. The silicon carbide of the epitaxial substrate 100 preferably has a hexagonal crystal structure and more preferably a 4H polytype. The n - Layer 121 has an added donor and thus the n-type conductivity. The donor is preferably formed by adding an impurity during the epitaxial growth of the n - Layer 121 and not by ion implantation of the n - Layer 121 added. The n - Layer 121 preferably has a donor concentration that is lower than that of the single crystal substrate 110. The n - Layer 121 preferably has a donor concentration of not less than 1 × 10 15 cm -3 and not more than 5 × 10 16 cm -3 , for example 8 × 10 15 cm -3Each of the n - The p-body layer 122 provided in layer 121 has an added acceptor and thus the p-conductivity type (second conductivity type). For example, the p-body layer 122 has an acceptor concentration of 1 × 10 18 cm -3 The n-type region 123 has the n-type conductivity type. The n-type region 123 is provided on the p-type body layer 122 and is separated from the n-type by the p-type body layer 122. - Layer 121 is separated. Contact region 124 has a p-type conductivity. Contact region 124 is formed on a portion of p-body layer 122 to be connected to p-body layer 122.
[0050] Referring to Fig. 2 and Fig. 3, the epitaxial substrate 100 is formed with a trench TR. The trench TR has sidewall surfaces SW and a bottom surface BT. Each of the sidewall surfaces SW extends through the n-type region 123 and the p-type body layer 122 and reaches to the n-type - Layer 121. The floor area BT is from the n - Layer 121 is formed. Each of the side wall surfaces SW has a channel surface CH ( Fig. 3) on the p-body layer 122. The bottom surface BT is a flat surface substantially parallel to the main surface of the epitaxial substrate 100. The reason that the epitaxial substrate 100 has the trench TR is that the epitaxial layer has been partially removed from the upper surface of the single-crystal substrate 110. In the present embodiment, a plurality of mesa structures are formed on the upper surface of the single-crystal substrate 110. Specifically, each of the mesa structures has a top surface and a bottom surface, each having a hexagonal shape, and sidewall surfaces inclined with respect to the upper surface of the single-crystal substrate 110. Accordingly, the trench TR extends toward the opening side. Preferably, the sidewall surface SW has a predetermined crystal plane (also referred to as a "special plane") particularly on the p-body layer 122.Details of the special level are described below.
[0051] Furthermore, with reference to Fig. 4 the side wall surface SW has a first to third side surface SW1 to SW3, each consisting of the n - Layer 121, the p-body layer 122 and the n-region 123.
[0052] The gate insulating film 200 is formed on the trench TR. The gate insulating film 200 separates the epitaxial substrate 100 and the gate electrode 230 in the trench TR. The gate insulating film 200 includes: a first insulating film 201 directly covering both the sidewall surface SW and the bottom surface BT; and a second insulating film 202 provided on the first insulating film 201. The first and second insulating films 201, 202 each have a first and a second carbon atom concentration. The second carbon atom concentration may be smaller than the first carbon atom concentration. The first carbon atom concentration may be more than 1 × 10 15 cm -3 The second carbon atom concentration can be less than 1 × 10 15 cm -3 , whereby the concentration can essentially be zero.
[0053] The first insulating film 201 includes a first bottom portion 201B disposed on the bottom surface BT; and a first sidewall portion 201S disposed on the sidewall surface SW. The first sidewall portion 201S includes first to third regions 201a to 201c disposed on the first to third sidewall surfaces SW1 to SW3, respectively. The first insulating film 201 preferably includes an oxidation film, and is more preferably obtained by thermally oxidizing the surface of the trench TR of the epitaxial substrate 100.
[0054] Furthermore, with reference to Fig. 5 the second insulating film 202 has a portion formed at a corner portion CR ( Fig. 1), which is formed by the bottom surface BT and the side wall surface SW with the first insulating film 201 therebetween. In particular, the second insulating film 202 comprises: a second bottom portion 202B disposed on the first bottom portion 201B; and a second side wall portion 202S disposed on the first side wall portion 201S. The second side wall portion 202S comprises: one end E1 connected to the second bottom portion 202B; and another end E2 disposed on the first or second region 201a, 201b ( Fig. 4) and is separated from the third region. In the present embodiment, the other end E2 is separated from the third region 201c and is arranged on the second region 201b. The other end E2 has an inclination angle AG ( Fig. 5) relative to the first sidewall portion 201S. The inclination angle AG forms an angle formed by an end portion of the surface of the other end E2 and a portion of the surface of the first sidewall portion 201S that is in contact with the other end E2. The inclination angle AG is preferably less than 70°. The second semiconductor layer 122 may have a depth position DP ( Fig. 5) where the impurity concentration is at its maximum, in which case the other end E2 is preferably located deeper than the depth position DP. The second insulating film 202 may be formed of silicon oxide and / or silicon nitride and / or phosphosilicate glass. The second insulating film 202 comprises a thermal oxidation film made of a film containing silicon and no carbon, and is formed, for example, of SiO2.
[0055] The gate insulating film 200 includes a portion with the first and second insulating films 201, 202 on the bottom surface BT of the trench TR, and this portion has a thickness d0. Furthermore, the gate insulating film 200 includes a portion with the first insulating film 201 and without the second insulating film 202 on the sidewall surface SW of the trench TR, that is, it includes a portion formed only of the first insulating film 201, this portion having a thickness d1. Furthermore, the gate insulating film 200 includes a portion with the first and second insulating films 201, 202 on the first side surface SW1 of the sidewall surface SW of the trench TR, and this portion has a thickness d2. Preferably, the relationship d2 > d1 × 1.5 is satisfied. Preferably, the relationship d2 < d1 × 5 is satisfied. Preferably, the relationship d0 > d1 is satisfied. Preferably, the relationship d0 ≥ d2 is satisfied.
[0056] The gate electrode 230 is formed in the trench TR. Specifically, the gate electrode 230 is formed on the trench TR with the gate insulating film 200 therebetween. The gate electrode 230 is in contact with the second region 201b of the first insulating film 201. The gate electrode 230 has a top surface substantially equal to the top surface of a portion of the gate insulating film 200 on the top surface of the n-type region 123. The interlayer insulating film 203 is formed to cover the gate electrode 230 and to cover the gate insulating film 200 in the portion extending on the top surface of the n-type region 123.
[0057] The source electrode 221 extends through the interlayer insulating film 203 and is in contact with both the n-type region 123 and the contact region 124. The source interconnect 222 is formed on the source electrode 221, and the interlayer insulating film 203 is in contact with the source electrode 221. The drain electrode 211 is formed on the surface of the epitaxial substrate 100 opposite the surface provided with the trench TR. The guard electrode 212 covers the drain electrode 211.
[0058] The following describes a method for manufacturing the MOSFET 501 ( Fig. 1) described.
[0059] As in Fig. 6, the n -Layer 121 is formed. This epitaxial growth can be carried out using a CVD (chemical vapor deposition) process that uses a mixed gas of silane (Si4H) and propane (C3H8) as the starting material gas and hydrogen gas (H2) as the carrier gas. Preferably, nitrogen (N) or phosphorus (P) is introduced as the donor. Subsequently, the p-body layer 122 is deposited on the n- - Layer 121 is formed, and the n-region 123 is formed on the p-body layer 122. In particular, ions are injected into the upper surface of the n - Layer 121 is implanted. During the ion implantation to form the p-body layer 122, ions of an acceptor, such as aluminum (Al), are implanted. Meanwhile, during the ion implantation to form the n-region 123, ions of a donor, such as phosphorus (P), are implanted. In this way, the epitaxial substrate 100 is formed, which contains the n- -Layer 121, the p-body layer 122, and the n-type region 123. It should be noted that instead of ion implantation, epitaxial growth may be performed by adding an impurity. Subsequently, the contact region 124 is formed by ion implantation. Next, an activation heat treatment is performed to activate the impurities added by the ion implantation. This heat treatment is preferably performed at a temperature of not less than 1500°C and not more than 1900°C, for example, at a temperature of approximately 1700°C. The heat treatment is performed for, for example, about 30 minutes. The heat treatment atmosphere preferably includes an inert gas atmosphere, such as an Ar atmosphere. In this way, the silicon carbide substrate 100 is manufactured.
[0060] As in Fig. 7, a mask 401 having an opening for partially exposing the n-type region 123 is formed on the epitaxial substrate 100. The opening is formed in accordance with the position of the trench TR ( Fig. 1). For example, a silicon oxide film formed by thermal oxidation can be used as the mask 401.
[0061] As in Fig. 8, in the opening of the mask 401, the n-region 123, the p-body layer 122 and a portion of the n - Layer 121 is removed by etching. An exemplary usable etching method includes reactive ion etching (RIE), and in particular inductively coupled plasma (ICP) RIE. In particular, ICP RIE can be used, which uses, for example, SF6 or a mixed gas of SF6 and O2 as the reactive gas. The etching process creates a layer of fluorine in the region where the trench TR ( Fig. 1), a recess TQ is formed which has a side wall with an inner surface SV which is substantially perpendicular to the main surface of the single-crystal substrate 110.
[0062] Subsequently, the epitaxial substrate 100 is etched using the mask 401. Specifically, the inner surface SV of the recess TQ of the epitaxial substrate 100 is thermally etched. The thermal etching can be performed, for example, by heating the epitaxial substrate 100 in an atmosphere containing a reactive gas having at least one or more types of halogen atoms. The at least one or more types of halogen atoms include chlorine (Cl) atoms and / or fluorine (F) atoms. The atmosphere includes, for example, Cl2, BCl3, SF6, or CF4. For example, the thermal etching is performed using a mixed gas of chlorine gas and oxygen gas as the reactive gas at a heat treatment temperature of, for example, not lower than 700°C and not higher than 1000°C. It should be noted that the reactive gas may include a carrier gas in addition to the chlorine gas and the oxygen gas.For example, a usable carrier gas includes nitrogen (N2) gas, argon gas, helium gas, or the like. When the heat treatment temperature is set to not less than 700°C and not more than 1000°C as described above, the etching rate of SiC is approximately 70 μm / hour. Moreover, in this case, the mask 401, which is formed of silicon oxide and thus has a very high etching selectivity with respect to SiC, is substantially not etched during SiC etching.
[0063] As in Fig. As shown in Figure 9, the trench TR is formed in the silicon carbide substrate 100 by the previously described thermal etching process. During the formation of the trench TR, the epitaxial substrate 100 is etched laterally from the opening of the mask 401, as indicated by arrow SE. Furthermore, during the thermal etching, a special plane spontaneously forms on the sidewall surface SW of the trench TR, particularly on the portion formed by the p-type body layer 122.
[0064] As in Fig. As shown in Figure 10, the first insulating film 201 is formed to directly cover both the sidewall surface SW and the bottom surface BT. In other words, the first insulating film 201 includes both a portion directly disposed on the bottom surface BT and a portion directly disposed on the sidewall surface SW. The first insulating film 201 can be formed by thermally oxidizing the bottom surface BT and the sidewall surface SW of the trench TR.
[0065] As in Fig. As shown in Figure 11, the silicon film 302 is formed on the first insulating film 201. The silicon film 302 can be formed, for example, by chemical vapor deposition (CVD) methods.
[0066] As in Fig. As shown in Figure 12, a resist layer 402 is formed on the silicon film 302 to fill the trench TR with the first insulating film 201 and the silicon film 302 therebetween. The resist layer 402 can be formed by applying a resist liquid. Subsequently, the resist layer 402 and a portion of the silicon film 302 are etched. This etching process can be performed without using an etching mask. That is, the etching process can be performed by etching back.
[0067] As in Fig. As shown in Figure 13, based on the previously described etching process, the resist layer 402 and the silicon film 302 remain on the bottom surface BT to partially fill the trench TR. The silicon film 302 includes: a second bottom portion 302B disposed on the first bottom portion 201B; and a second sidewall portion 302S disposed on the first sidewall portion 201S. The second sidewall portion 302S includes: one end E1 connected to the second bottom portion 302B; and the other end E2 disposed on the second region 201B and separated from the third region 201C. Subsequently, the resist layer 402 is removed ( Fig. 14). Next, an etching process is performed to remove the first insulating film 201 at the exposed portion not covered with the silicon film 302 ( Fig. 15), to be removed.
[0068] Subsequently, the trench TR with the first insulating film 201 formed thereon and the silicon film 302 are thermally oxidized. This leads to the thermal oxidation of the silicon film 302 and the exposed portion of the sidewall surface SW of the trench TR. The silicon film 302 is thermally etched, for example, at not less than 800°C and not more than 1150°C. Through this thermal etching process, the second insulating film 202 is formed from the silicon film 302 ( Fig. 16). The first and second insulating films 201, 202 form the gate insulating film 200.
[0069] Preferably, the silicon film 302 is thermally oxidized, for example, at not less than 950°C and not more than 1100°C. When the silicon film 302 is oxidized at a temperature of less than 950°C, stress relaxation is expected to occur due to the viscous flow of a silicon film formed by oxidizing the silicon film 302, thereby moving silicon near the grain boundaries to the surface side, resulting in a crystal grain growing on the surface of the silicon film 302 and forming a protrusion. The formation of the protrusion can be suppressed by oxidizing the silicon film 302 at not less than 950°C, thereby effectively reducing the surface roughness of the second insulating film 202.On the other hand, when the silicon film 302 is oxidized at a temperature higher than 1100°C, the first insulating film 201 made of silicon oxide and the silicon film 302 chemically react to form silicon oxide, making it difficult to maintain the shape of the second insulating film 202. Thus, by oxidizing the silicon film 302 at not more than 1100°C, an increase in the vapor pressure of silicon oxide can be suppressed, thereby effectively maintaining the shape of the second insulating film 202.
[0070] As in Fig. 17, during the formation of the second insulating film 202 of the angle AG ( Fig. 5) by heating the second sidewall portion 202S at a sufficient temperature. The heating temperature is preferably not less than 1300°C and not more than 1400°C. By performing this heat treatment in an oxidizing atmosphere, the film thickness of the first insulating film 201 can be made thicker.
[0071] As in Fig. As shown in Figure 18, the gate electrode 230 is formed on the trench TR with the gate insulating film 200 therebetween. The gate electrode 230 is formed, for example, by forming a film of a conductor or doped polysilicon and performing a CMP (Chemical Mechanical Polishing) process.
[0072] With reference again to Fig. 1, the interlayer insulating film 203 is formed on the gate electrode 230 and the gate insulating film 200 to cover the exposed area of the gate electrode 230. An etching process is performed to form an opening in the interlayer insulating film 203 and the gate insulating film 200. Through the opening, both the n-type region 123 and the contact region 124 on the upper surface of the mesa structure are exposed. Next, the source electrode 221 is formed on the upper surface of the mesa structure in contact with both the n-type region 123 and the contact region 124. Next, the source interconnection 222, the drain electrode 211, and the guard electrode 212 are formed. In this way, the MOSFET 501 is obtained.
[0073] According to the present embodiment, the Fig. 5, which together with the first insulating film 201 forms the gate insulating film 200, is formed not only on the first bottom portion 201B of the first insulating film 201 but also on the first sidewall portion 201S of the first insulating film 201. Accordingly, the gate insulating film 200 has a greater thickness not only on the bottom surface BT of the trench TR but also on the sidewall surface SW, which, together with the bottom surface BT, forms the corner portion CR near the bottom surface BT. Thus, the gate electrode capacitance can be reduced more than in the case where the gate insulating film 200 is formed thick only on the bottom surface BT of the trench TR.
[0074] Furthermore, if a load connected to the MOSFET 501 is short-circuited, a large amount of current flows into a channel surface CH, thereby increasing the temperature of the gate insulating film 200. Consequently, the insulating property of the gate insulating film 200 decreases, causing a leakage current to flow. This leakage current causes problems, particularly near an interface between the first and second regions 201a, 201b, where the channel current is concentrated and a relatively high voltage is applied to the gate insulating film 200 ( Fig. 4). According to the present embodiment, the second sidewall portion 202S of the second insulating film 202 is formed in the portion where the leakage current is most likely to flow. In this way, the leakage current can be suppressed. If the channel surface CH ( Fig. 3) formed from a special plane, the previously described temperature rise becomes noticeable due to the high carrier mobility in the channel surface CH, so it is particularly important to suppress the leakage current.
[0075] In addition, the impurity concentration of the p-body layer 122 near the interface is often lower than in the depth position DP ( Fig. 5). If the drain voltage is high in such cases, a short-channel effect is likely to occur. According to the present embodiment, the influence of such a short-channel effect can be reduced. Furthermore, the short-circuit performance can be improved accordingly.
[0076] If d2 is large enough to satisfy the relationship d2 > d1 × 1.5, the previously described advantages can be achieved even more effectively. Furthermore, if d2 is too large, the current is blocked and cannot be directed near the corner section CR ( Fig. 1) and thus the on-resistance becomes correspondingly large, so that the relationship d2 < d1 × 5 is preferably fulfilled.
[0077] In addition, the other end E2 of the second side wall portion 202S, as shown in Fig. 4, separated from the third region 201c and disposed on the second region 201b. Accordingly, the second sidewall portion 202S extends further than in the case where the second sidewall portion 202S is formed only on the first region 201a. Moreover, the second sidewall portion 202S is formed away from the interface, which has a great influence on the channel characteristics, between the second region 201b and the third region 201c. Thus, while suppressing deterioration of the channel characteristics, the gate electrode capacitance can be more effectively reduced.
[0078] In addition, the second semiconductor layer 122 preferably has the depth position DP ( Fig. 5) where the impurity concentration is at its highest, the other end E2 of the second sidewall portion 202S is preferably located deeper than the depth position DP. Thus, the second sidewall portion 202S extends further than in the case where the second sidewall portion 202S is formed only on the first region 201a. Moreover, the second sidewall portion 202S is formed away from the depth position DP, which has a great influence on the channel characteristics. Thus, while suppressing deterioration of the channel characteristics, the gate electrode capacitance can be reduced more effectively.
[0079] The other end E2 of the second sidewall portion 202S preferably has an inclination angle AG of less than 70° relative to the first sidewall portion 201S. Accordingly, a change in the thickness of the gate insulating film 200 at the other end E2 is reduced.
[0080] The first and second insulating films 201, 202 each have the first and second carbon atom concentrations, with the second carbon atom concentration preferably being lower than the first carbon atom concentration. Accordingly, the second insulating film 202 has a high dielectric breakdown strength due to the low carbon atom concentration. Thus, the silicon carbide semiconductor device 501 has a high breakdown voltage. It should be noted that the first insulating film 201 is formed by thermally oxidizing the bottom surface BT and the sidewall surface SW of the trench TR, which are formed of silicon carbide, and thus includes many carbon atoms originating from the silicon carbide. The second insulating film 202, on the other hand, is formed by oxidizing the silicon film 302.Thus, the carbon atom concentration of the second insulating film 202 becomes lower than the carbon atom concentration of the first insulating film 201.
[0081] The first carbon atom concentration is preferably more than 1 × 10 15 cm -3 and the second carbon atom concentration is less than 1 × 10 15 cm -3 Accordingly, the carbon atom concentration of the second insulating film 202 is made sufficiently low. Thus, the breakdown voltage of the silicon carbide semiconductor device 501 can be further increased.
[0082] The second insulating film 202 is preferably formed of silicon oxide and / or silicon nitride and / or phosphosilicate glass. Accordingly, the breakdown voltage of the silicon carbide semiconductor device 501 can be further increased.
[0083] The second insulating film 202 comprises a thermal oxidation film of a film containing silicon and no carbon. Accordingly, the breakdown voltage of the silicon carbide semiconductor device 501 can be further increased.
[0084] The step of forming the second insulating film 202 by oxidizing the silicon film 302 is preferably performed at not less than 800°C and not more than 1150°C. By oxidizing the silicon film 302 at not less than 800°C, the surface roughness of the silicon film 302 can be suppressed. Furthermore, by oxidizing the silicon film at not more than 1150°C, it is possible to suppress an increase in the vapor pressure of the second insulating film 202, which is formed of silicon oxide and produced by oxidizing the silicon film 302. Consequently, the shape of the second insulating film 202 can be maintained.
[0085] The step of forming the second insulating film 202 preferably includes the step of heating the second sidewall portion 202S to reduce the angle AG of the other end E2 of the second sidewall portion 202S relative to the first sidewall portion 201S. Accordingly, a change in the thickness of the gate insulating film 200 at the other end E2 is reduced. This step is preferably performed at not less than 1300°C and not more than 1400°C. Accordingly, the angle AG of the other end E2 can be made sufficiently small using a high temperature.
[0086] It should be noted that the method using thermal oxidation of the silicon film was described as a method for forming the second insulating film 202 in the present embodiment; however, the second insulating film 202 may also be formed by a deposition method or directly by a CVD method. Furthermore, the "first conductivity type" was assumed to include the n-type and the "second conductivity type" the p-type, but these conductivity types may be interchanged. In this case, the donors and acceptors in the above description are also interchanged. It should be noted that in order to achieve high channel mobility, the "first conductivity type" preferably includes the n-type.Furthermore, the silicon carbide semiconductor device is not limited to the MOSFET and may include, for example, an IGBT (Insulated Gate Bipolar Transistor) with a trench. (Second embodiment)
[0087] As in Fig. As shown in Figure 19, in a MOSFET 502 (silicon carbide semiconductor device) of the present embodiment, the other end E2 of the second sidewall portion 202S of the second insulating film 202 is disposed at an interface between the first region 201a and the second region 201b. The term "disposed at the interface" used here is intended to allow an error to such an extent that both the gate electrode capacitance and the channel characteristics are maintained at substantially the same level. Specifically, an error of about ±0.1 µm is allowed. Such a second sidewall portion 202S can be formed, for example, by continuing the etch-back process ( Fig. 13) in the first embodiment, so that the other end E2 of the second sidewall portion 202S of the silicon film 302 coincides with the vicinity of the aforementioned interface. It should be noted that configurations other than the above are substantially the same as those of the first embodiment. Thus, the same or corresponding elements are denoted by the same reference numerals and will not be described repeatedly.
[0088] According to the present embodiment, the second sidewall portion 202S extends at most to such an extent that it does not overlap the second region 201b forming the channel surface. Thus, the gate electrode capacitance can be effectively reduced with little impact on the channel characteristics. (Third embodiment)
[0089] As in Fig. As shown in Figure 20, in a MOSFET 503 (silicon carbide semiconductor device) of the present embodiment, the other end E2 of the second sidewall portion 202S of the second insulating film 202 is separated from the second region 201b and disposed on the first region 201a. Preferably, the other end E2 is separated from the second region 201b by more than ±0.1 µm. Such a second sidewall portion 202S can be formed, for example, by continuing the etch-back process ( Fig. 13) of the first embodiment, such that the other end E2 of the second sidewall portion 202S of the silicon film 302 is separated from the second region 201b and disposed on the first region 201a. It should be noted that configurations other than the above are substantially the same as those of the first embodiment. Thus, the same or corresponding elements are denoted by the same reference numerals and will not be described repeatedly.
[0090] According to the present embodiment, the second sidewall portion 202S extends such that it is not located near the second region 201b forming the channel surface. Thus, the gate electrode capacitance can be reduced without affecting the channel characteristics. (Surface with the “special layer”)
[0091] As previously described, the side wall surface SW ( Fig. 1) of the trench TR preferably has a predetermined crystal plane (also referred to as a “special plane”), in particular on the p-body layer 122. Such a sidewall surface SW comprises a Fig. 21, plane S1 (first plane) with a {0-33-8} plane orientation. Plane S1 preferably has a (0-33-8) plane orientation.
[0092] More preferably, the sidewall surface SW microscopically includes the plane S1, and the sidewall surface SW further microscopically includes a plane S2 (second plane) with a {0-11-1} plane orientation. Herein, the term "microscopic" means "so small that at least about twice the size of an interatomic distance is considered." As a method for observing such a microscopic structure, a method such as a TEM (transmission electron microscope) method is used, for example. The plane S2 preferably has a (0-11-1) plane orientation.
[0093] Preferably, the plane S1 and the plane S2 of the sidewall surface SW form a combined plane SR with a {0-1 1-2} plane orientation. In particular, the combined plane SR is formed from the periodically repeating planes S1 and S2. Such a periodic structure can be observed, for example, by TEM or AFM (atomic force microscope). In this case, the combined plane macroscopically has a deviation angle of 62° with respect to the {000-1} plane. Herein, the term "macroscopic" means "neglecting a fine structure with a size of approximately one interatomic distance." For measuring such a macroscopic deviation angle, a method using general X-ray diffraction, for example, is used. Preferably, the combined plane SR has a (0-1 1-2) plane orientation. In this case, the combined plane SR has a macroscopic deviation angle of 62° with respect to the (000-1) plane.
[0094] Preferably, the charge carriers flow in the channel surface in a channel direction CD in which the previously described periodic repetition takes place.
[0095] A detailed structure of the combined SR level is described below.
[0096] Regarding Si atoms (or C atoms), when a silicon carbide 4H polytype single crystal is observed from the (000-1) plane, atoms in a layer A (the solid line in the figure), atoms in a layer B located therebelow (the dashed line in the figure), and atoms in a layer C located therebelow (the chain line in the figure), as well as atoms in a layer B located therebelow (not shown in the figure) are repeatedly formed as shown in Fig. 22. In other words, if the four layers ABCB are considered as a periodic stack, a periodic stack structure such as ABCBABCBABCB ... is formed.
[0097] As in Fig. 23 are in the (11-20) plane (cross-section along a line XXIII-XXIII of the Fig. 22) the atoms in each of the four layers ABCB that form the period stack described above are not completely aligned along the (0-11-2) plane. Fig. In Figure 23, the (0-11-2) plane is shown as passing through the positions of the atoms in layer B. In this case, it can be seen that each of the atoms in layers A and C deviates from the (0-11-2) plane. Thus, even if the macroscopic plane orientation of the surface of the silicon carbide single crystal—that is, its plane orientation neglecting the atomic level structure—is limited to the (0-11-2) plane, this surface can assume macroscopically different structures.
[0098] As in Fig. As shown in Figure 24, the combined plane SR is formed by alternately forming the planes S1 having a (0-33-8) plane orientation and the planes S2 connected to the planes S1 and having a plane orientation different from that of the respective planes S1. Each of the planes S1 and S2 has a length twice the interatomic distance of the Si atoms (or C atoms). It should be noted that a plane with an average of the plane S1 and the plane S2 corresponds to the (0-11-2) plane ( Fig. 23).
[0099] Will, as in Fig. 25, the combined plane SR viewed from the (01-10) plane, the single crystal structure has a portion periodically comprising a structure (S1 plane portion) corresponding to a cubic structure. Specifically, the combined plane SR is formed by alternately forming the S1 planes having a (001) plane orientation in the above-described structure, which corresponds to the cubic structure, and the S2 planes connected to the S1 planes and having a plane orientation different from that of the S1 planes. Even in a polytype other than 4H, the surface can thus be composed of the planes (S1 planes in Fig. 25) with a (001) plane orientation in the structure corresponding to the cubic structure and the planes (planes S2 in Fig. 25) that are connected to the protruding planes and have a plane orientation different from the protruding planes. The polytype can be, for example, a 6H or 15R type.
[0100] Next, with reference to Fig. 26 describes a relationship between the crystal plane of the sidewall surface SW and the mobility MB of the channel surface. In the diagram of the Fig. In Figure 26, the horizontal axis represents an angle D1 formed by the (000-1) plane and the macroscopic plane orientation of the sidewall surface SW, which includes the channel surface, while the vertical axis represents the mobility MB. A group of measurement points CM corresponds to the case where the sidewall surface SW was thermally etched to conform to a special plane, while a group of measurement points MC corresponds to a case where the sidewall surface SW was not thermally etched.
[0101] In the group of measurement points MC, the mobility MB reaches a maximum value when the channel surface exhibits a macroscopic (0-33-8) plane alignment. The reason for this is presumably as follows: in the case where no thermal etching step is performed, that is, in the case where the microscopic structure of the channel surface is not specifically controlled, its macroscopic plane alignment corresponds to the (0-33-8) orientation, resulting in a ratio of the microscopic (0-33-8) plane alignment, that is, the (0-33-8) plane alignment at the atomic level, statistically high.
[0102] On the other hand, the mobility MB in the group of measurement points CM reaches a maximum value when the microscopic plane orientation of the channel surface is the (0-11-2) orientation (arrow EX). The reason for this is presumably as follows: as in Fig. 24 and Fig. 25, the plurality of planes S1 each having a (0-33-8) plane orientation are densely and uniformly aligned with the planes S2 arranged therebetween, thereby increasing a ratio of the microscopic (0-33-8) plane orientation in the channel surface.
[0103] It should be noted that the mobility MB has an orientation dependence on the combined plane SR. In the diagram of the Fig. 27, the horizontal axis shows an angle D2 between the channel direction and the <0-11-2> direction, while the vertical axis represents the mobility MB (in any unit) in the channel surface. A dashed line is shown in addition to the curve representation. From the diagram, it can be seen that to increase the channel mobility MB, the channel direction CD ( Fig. 21) preferably has an angle D2 of not less than 0° and not more than 60°, more preferably substantially 0°.
[0104] As in Fig. As shown in Figure 28, the sidewall surface SW may further include a plane S3 (third plane) in addition to the combined plane SR. More specifically, the sidewall surface SW may include a combined plane SQ formed by periodically arranging the plane S3 and the combined plane SR. In this case, the deviation angle of the sidewall surface SW with respect to the (000-1) plane deviates from the ideal deviation angle of the combined plane SR, i.e., 62°. Preferably, the deviation angle is small and in the range of ±10°. Examples of a surface falling within such an angular range include a surface having a macroscopic plane orientation of the {0-33-8} plane. Even more preferably, the deviation angle of the sidewall surface SW with respect to the (000-1) plane deviates from the ideal deviation angle of the combined plane SR, i.e., 62°. Preferably, this deviation is small and in the range of ±10°.Examples of a surface lying in such an angular range include a surface with a macroscopic plane orientation of the (0-33-8) plane.
[0105] Such a periodic structure can be observed, for example, using TEM or AFM. [Example]
[0106] First, MOSFETs were fabricated according to an example and a comparative example. The MOSFET according to the example was a MOSFET with the Fig. 20 was fabricated. Specifically, a gate insulating film 200 of the MOSFET according to the example included the first insulating film 201 and the second insulating film 202 partially formed on the first insulating film 201. In other words, the MOSFET according to the example had a structure such that the gate insulating film 200 facing the sidewall surface SW of the trench TR was formed thick. The other end E2 of the second sidewall portion 202S of the second insulating film 202 was formed separately from the second region 201b and disposed on the first region 201a. A distance from the bottom portion of the first insulating film 201 to the other end E2 of the second sidewall portion 202S of the second insulating film 202 in the normal direction of the bottom surface BT of the trench TR was 0.67 μm. The thickness of the second insulating film 202 was 200 nm. The angle AG (see Fig. 5) The angle of the other end E2 of the second insulating film 202 was 67° in the channel portion and about 62° on average on the inclined surface. In the MOSFET according to the example, the gate insulating film 200 including the first insulating film 201 and the second insulating film 202 was formed by oxidizing the first insulating film 301 and the silicon film 302 at 1100°C for 95 minutes and then oxidizing the films at 1350°C for 3 minutes. Subsequently, the silicon carbide substrate 100 including the gate insulating film 200 including the first insulating film 201 and the second insulating film 202 was thermally treated for 28 minutes at a measured temperature of 1350°C in a NO atmosphere. Subsequently, the silicon carbide substrate 100 with the gate insulating film 200 comprising the first insulating film 201 and the second insulating film 202 was thermally treated for 40 minutes at a temperature of 1350°C in an Ar atmosphere.
[0107] The gate insulating film 200 of the MOSFET according to the comparative example was formed with only the first insulating film 201 and did not include the second insulating film 202. In other words, the MOSFET according to the comparative example had a structure such that the gate insulating film 200 facing the sidewall surface SW of the trench TR was not formed thickly. In the MOSFET according to the comparative example, the gate insulating film 200 was formed by oxidizing the silicon carbide substrate 100 at 1100°C for 95 minutes and then oxidizing it at 1350°C for 6 minutes. Subsequently, the silicon carbide substrate 100 with the gate insulating film 200 was thermally treated at a temperature of 1350°C for 10 minutes in a NO atmosphere. Subsequently, the silicon carbide substrate 100 with the gate insulating film 200 was thermally treated at a temperature of 1350°C for 10 minutes in an Ar atmosphere.
[0108] With reference to Fig. 29, a relationship is shown below between a capacity C gd between the gate electrode 230 and the drain electrode 211 and a voltage V DS between the drain electrode 211 and the source electrode 221. In Fig. 29, the capacitance of the MOSFET according to the example is represented by a solid line 101 and the capacitance of the MOSFET according to the comparative example is represented by a dashed line 102.
[0109] With reference to Fig. 29 was the capacity C gd of the MOSFET according to the example is smaller than the capacitance C gd of the MOSFET according to the comparative example when the voltage V DS between the drain electrode 211 and the source electrode 221 was not less than 0 V and not more than 600 V over the entire area. If the voltage V DS between the drain electrode 211 and the source electrode 221 600 volts, the capacitance C gdof the MOSFET according to the example 32 pF and the capacitance C gd of the MOSFET according to Comparative Example 27 pF. As described above, by forming a thick gate insulating film 200 facing the sidewall surface SW of the trench TR (in other words, by forming the second insulating film 202 on the first insulating film 201), it was confirmed that the capacitance C gd between the gate electrode 230 and the drain electrode 211 can be effectively reduced. List of reference symbols 100 epitaxial substrate (silicon carbide substrate); 110 single crystal substrate; 121 n - layer (first semiconductor layer); 122 p-body layer (second semiconductor layer) 123 n-region (third semiconductor layer); 124 contact area; 200 gate insulation film; 201 first insulating film; 202 second insulating film; 201B first floor section; 201S first side wall section; 201a to 201c first to third areas; 202B, 302B second floor section; 202S, 302S second side wall section; 203 Interlayer insulating film; 211 drain electrode; 212 protective electrode; 221 source electrode; 222 source interconnect; 230 gate electrode; 302 silicon layer; 401 mask; 402 resist layer; 501-503 MOSFET (silicon carbide semiconductor device); AG inclination angle; BT floor area; CH canal area; CR corner section; DP depth position; E1 an end; E2 the other end; SW side wall surface; SW1 to SW3 first to third side surface; TR Graben
Claims
[1] A silicon carbide semiconductor device (501 - 503) comprising: a silicon carbide substrate (100) having a first semiconductor layer (121), a second semiconductor layer (122), and a third semiconductor layer (123), wherein the first semiconductor layer (121) has a first conductivity type, the second semiconductor layer (122) is provided on the first semiconductor layer (121), the second semiconductor layer (122) has a second conductivity type, the third semiconductor layer (123) is provided on the second semiconductor layer (122), the third semiconductor layer (123) is separated from the first semiconductor layer (123) by the second semiconductor layer (122), the third semiconductor layer (123) has the first conductivity type, wherein the silicon carbide substrate (100) is provided with a trench (TR), the trench (TR) having a bottom surface (BT) and a sidewall surface (SW), the bottom surface (BT) being formed from the first semiconductor layer (121), and first to third side surfaces (SW1-SW3) of the sidewall surface (SW) being formed from the first to third semiconductor layers (121-123), respectively; a gate insulating film (200) provided on the trench (TR), the gate insulating film (200) comprising a first insulating film (201) and a second insulating film (202), the first insulating film (201) directly covering both the sidewall surface (SW) and the bottom surface (BT), the second insulating film (202) being formed on the first insulating film (201), the first insulating film (201) comprising a first bottom portion (201B) and a first sidewall portion (201S), the first bottom portion (201B) being arranged on the bottom surface (BT), the first sidewall portion (201S) being arranged on the sidewall surface (SW), first to third regions (201a-201c) of the first sidewall portion (201S) being arranged on the first to third side surfaces (Sw1-SW3), respectively, the second insulating film (202) comprising a second bottom portion (202B) and a second side wall portion (202S),the second bottom portion (202B) is arranged on the first bottom portion (201B), the second sidewall portion (202S) is arranged on the first sidewall portion (201S), the second sidewall portion (202S) being formed with one end (E1) and another end (E2), the one end (E1) being connected to the second bottom portion (202B), the other end (E2) being arranged on the first or second region (201a, 201b), and the other end (E2) being separated from the third region (201c); a gate electrode (230) provided on the trench (TR) with the gate insulating film (200) therebetween, and the second insulating film (202) comprises a thermal oxidation film made of a film comprising silicon and no carbon. [2] The silicon carbide semiconductor device (501-503) according to claim 1, wherein the other end (E2) of the second sidewall portion (202S) is located at an interface between the first region (201a) and the second region (201b). [3] The silicon carbide semiconductor device (501-503) according to claim 1, wherein the other end (E2) of the second sidewall portion (202S) is separated from the second region (201b) and disposed on the first region (201a). [4] The silicon carbide semiconductor device (501-503) according to claim 1, wherein the other end (E2) of the second sidewall portion (202S) is separated from the third region (201c) and disposed on the second region (201b). [5] The silicon carbide semiconductor device (501-503) according to claim 4, wherein the second semiconductor layer (122) has a depth position (DP) at which an impurity concentration has a maximum value, and the other end (E2) of the second sidewall portion (202S) is located deeper than the depth position (DP). [6] The silicon carbide semiconductor device (501-503) according to any one of claims 1 to 5, wherein the other end (E2) of the second sidewall portion (202S) has an inclination angle (AG) of less than 70° with respect to the first sidewall portion (201S). [7] The silicon carbide semiconductor device (501-503) according to any one of claims 1 to 6, wherein the first and second insulating films (201, 202) each have a first and second carbon atom concentration, and the second carbon atom concentration is lower than the first carbon atom concentration. [8] The silicon carbide semiconductor device (501 - 503) according to claim 7, wherein the first carbon atom concentration is more than 1 × 10 15 cm -3 and the second carbon atom concentration is less than 1 × 10 15 cm -3 be. [9] The silicon carbide semiconductor device (501-503) according to any one of claims 1 to 8, wherein the second insulating film (202) is formed of silicon oxide, silicon nitride, and / or phosphosilicate glass. [10] A method for manufacturing a silicon carbide semiconductor device (501-503) comprising the steps of: Producing a silicon carbide substrate (100) having a first semiconductor layer (121), a second semiconductor layer (122), and a third semiconductor layer (123), wherein the first semiconductor layer (121) has a first conductivity type, the second semiconductor layer (122) is provided on the first semiconductor layer (121), the second semiconductor layer (122) has a second conductivity type, the third semiconductor layer (123) is provided on the second semiconductor layer (122), the third semiconductor layer (123) is separated from the first semiconductor layer (121) by the second semiconductor layer (122), and the third semiconductor layer (123) has the first conductivity type, Forming a trench (TR) in the silicon carbide substrate (100), wherein the trench (TR) has a bottom surface (BT) and a sidewall surface (SW), the bottom surface (BT) is formed from the first semiconductor layer (121), and first to third side surfaces (SW1-SW3) of the sidewall surface (SW) are each formed from the first to third semiconductor layers (121-123); Forming a first insulating film (201) to cover both the side wall surface (SW) and the bottom surface (BT), wherein the first insulating film (201) is provided with a first bottom portion (201B) and a first side wall portion (201S), wherein the first bottom portion (201B) is arranged on the bottom surface (BT), the first side wall portion (201S) is arranged on the side wall surface (SW), wherein first to third regions (201a-201c) of the first side wall portion (201S) are arranged on the first to third side surfaces (SW1-SW3), respectively, Forming a silicon film (302) on the first insulating film (201), wherein the silicon film (302) has a second bottom portion (202B) and a second sidewall portion (202S), the second bottom portion (202B) is arranged on the first bottom portion (201B), the second sidewall portion (202S) is arranged on the first sidewall portion (201S), the second sidewall portion (202S) is formed with one end (E1) and another end (E2), the one end (E1) being connected to the second bottom portion (202B), the other end (E2) being arranged on the first or second region (201a, 201b), and the other end (E2) being separated from the third region (201c); Forming a second insulating film (202) by oxidizing the silicon film (302), wherein the first and second insulating films (201, 202) form a gate insulating film (200); and Forming a gate electrode (230) on the trench (TR) with the gate insulating film (200) disposed therebetween. [11] A method of manufacturing the silicon carbide semiconductor device according to claim 10, wherein the step of forming the second insulating film (202) is performed by oxidizing the silicon film (302) at not less than 800°C not more than 1150°C. [12] A method of manufacturing the silicon carbide semiconductor device according to claim 10, wherein the step of forming the second insulating film (202) includes a step of heating the second sidewall portion (202S) to reduce an angle of the other end (E2) of the second sidewall portion (202S) with respect to the first sidewall portion (201S). [13] A method of manufacturing the silicon carbide semiconductor device according to claim 12, wherein the step of heating the second sidewall portion (202S) is performed at not less than 1300°C not more than 1400°C.
Citation Information
Patent Citations
Semiconductor device and manufacture thereof
JP1995326755A
Semiconductor device and method for fabricating the same
JP2009224365A
Semiconductor device and method for manufacturing same
WO2012098861A1
JP002009224365A