Optoelectronic semiconductor chip and methods for its manufacture

DE112015002498B4Active Publication Date: 2024-10-31AMS OSRAM INT GMBH
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
DE112015002498
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2014-05-26
Filing Date
2015-05-20
Publication Date
2024-10-31
Estimated Expiration
2035-05-20

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Optoelectronic semiconductor chip (1), which is a light-emitting diode, with a semiconductor layer sequence (2), wherein the semiconductor layer sequence (2) comprises: - an n-type layer sequence (21), - a p-type layer sequence (23), - an active zone (22) located between the n-type layer sequence (21) and the p-type layer sequence (23), - at least one etch signal layer (24) in the p-type layer sequence (23) and / or in the n-type layer sequence (21), and - an etch structure (3) on a side of the etch signal layer (24) facing away from the active zone (22), wherein - the etch structure (3) extends at least into the etch signal layer (24), - the etch signal layer (24) has a signal component, - the active zone (22) is configured for radiation generation and is based on InAlGaP or on InAlGaAs, - the etch signal layer (24) is located in or located on the p-conducting layer sequence (23) and is based on In1-x-yAlyGaxP or on In1-x-yAlyGaxAs with x + y < 1,- the signal component is Ga and 0.005 ≤ x ≤ 0.2,- in a layer (25) adjacent to the etch signal layer (24) in the direction towards the etch structure (3) the signal component is not present,- the thickness of the etch signal layer (24) is between 50 nm and 800 nm inclusive,- a material of the etch signal layer (24) is partially removed by the etch structure (3),- the semiconductor chip (1) is free of a growth substrate of the semiconductor layer sequence (2), and- radiation coupling takes place at the n-type layer sequence (21) and a carrier (6) is located at the p-type layer sequence (23).
Need to check novelty before this filing date? Find Prior Art

Description

An optoelectronic semiconductor chip is specified. Furthermore, a method for producing such a semiconductor chip is specified.The documents US 2013 / 0 182 735 A1, US 2007 / 0 099 324 A1, US 2009 / 0 206 354 A1 and DE 10 2011 111 919 A1 relate to light-emitting optoelectronic semiconductor components.One object to be achieved is to specify an optoelectronic semiconductor chip which has efficient coupling-out of light.This object is achieved by an optoelectronic semiconductor chip and a method for producing the same having the features of the independent patent claims. Preferred developments are the subject matter of the dependent claims.The optoelectronic semiconductor chip is a light-emitting diode or a laser diode. The semiconductor chip is configured to emit electromagnetic radiation during operation. For example, visible light or near infrared radiation is generated during operation of the semiconductor chip. It is possible in particular for the semiconductor chip to be configured for generating yellow light, orange light and / or red light or for generating near-infrared radiation in the wavelength range between 760 nm and 870 nm inclusive.The optoelectronic semiconductor chip comprises at least one semiconductor layer sequence. In particular, the semiconductor layer sequence is epitaxially grown. The semiconductor layer sequence is preferably based on a III-V compound semiconductor material. The semiconductor material is, for example, a nitride compound semiconductor material such as Al n In 1-n-m Ga m N or a phosphide compound semiconductor material such as Al n In 1-n-m Ga m P or else an arsenide compound semiconductor material such as Al n In 1-n-m Ga m As, where 0≤n≤1, 0≤m≤1 and n+m≤1 in each case. The semiconductor layer sequence can have dopants and additional components. For the sake of simplicity, however, only the essential constituents of the crystal lattice of the semiconductor layer sequence, i.e. Al, As, Ga, In, N or P, are specified, even if these may be partially replaced and / or supplemented by small amounts of further substances.The semiconductor layer sequence comprises an n-conducting layer sequence. The n-conducting layer sequence is n-doped continuously or in regions. The n-conducting layer sequence can have one or more sublayers. The term layer sequence therefore does not necessarily mean that a plurality of layers must be present in the n-conducting layer sequence.The semiconductor chip has a p-conducting layer sequence which comprises one or, preferably, a plurality of p-conducting layers. The p-conducting layer sequence is preferably p-doped.The semiconductor chip has at least one active zone. The one or more active zones are arranged between the n-conducting layer sequence and the p-conducting layer sequence. In particular, the active zone is in direct contact with the n-conducting layer sequence and with the p-conducting layer sequence. The active zone comprises, for example, a pn junction, a single quantum well structure or a multiple quantum well structure. In particular, the active zone includes a plurality of quantum wells separated from one another by barrier layers.The semiconductor layer sequence includes one or more etching signal layers. The at least one etching signal layer is located in or on the p-conducting layer sequence or in the n-conducting layer sequence. If a plurality of etching signal layers are present, then in each case one etching signal layer can be located in the p-conducting layer sequence and one etching signal layer can be located in the n-conducting layer sequence. A plurality of etching signal layers in one of the layer sequences are also possible.The semiconductor chip has one or more etching structures. The at least one etching structure extends at least in larger regions or over the whole area as far as at least into the etching signal layer. This means that the etching signal layer is exposed at least in places by the etching structure and / or a material of the etching signal layer is at least partially removed during the production of the etching structure. It is also possible that the etching signal layer is completely removed over larger regions when producing the etching structure. For example, the etching structure has a prismatic or trapezoidal shape, as seen in cross section, wherein a width of the etching structure in the direction of the active zone is preferably reduced.The etching signal layer includes a signal component. The signal component is preferably a main component of a semiconductor material on which the etching signal layer is based. Alternatively, the signal component can be a doping of the etching signal layer.The etching signal layer adjoins, in the direction towards the etching structure and in the direction away from the active zone, a layer which is free of the signal component or has only a small amount of the signal component. This means in particular that the signal component is at most present in the form of an impurity and / or that a concentration of the signal component in this layer is reduced by at least a factor of two or five or ten or hundred compared to the etching signal layer. In other words, this layer is free of the signal component or has little of the signal component compared to the etching signal layer.The signal component has an atomic fraction of at least 0.5%, or 1%, or 1.75% at the etching signal layer. Alternatively or additionally, this proportion is at most 20% or 10% or 5% or 3.5%. In other words, the signal component then only makes up a comparatively small proportion of the etching signal layer.The semiconductor chip comprises a semiconductor layer sequence. The semiconductor layer sequence has an n-conducting layer sequence and a p-conducting layer sequence and an active zone lying between these layer sequences for generating electromagnetic radiation. Furthermore, at least one etching signal layer is located in or on the p-conducting layer sequence and / or in or on the n-conducting layer sequence in the semiconductor layer sequence. Furthermore, an etching structure is located on the semiconductor layer sequence on a side of the etching signal layer facing away from the active zone. The etching structure extends at least in places at least into the etching signal layer. The etching signal layer has a signal component which is absent or is present only in a reduced concentration in a layer adjoining the etching signal layer in the direction toward the etching structure and / or in the direction away from the active zone.In particular in thin-film light-emitting diodes, that is to say in light-emitting diodes without growth substrate, light generated in an active zone propagates in a comparatively thin layer package in the semiconductor layer sequence until the generated light is either coupled out or absorbed. Since, because of the high refractive index of semiconductor materials, a coupling-out probability per incidence of the light on a coupling-out surface is comparatively small, light travels in the semiconductor for a relatively long time until coupling-out takes place. Accordingly, an efficiency of thin-film light-emitting diodes depends comparatively strongly on absorptions in or at the semiconductor layer sequence.Absorption takes place, for example, by metallic contact surfaces, since such contact surfaces are optimized for an electrical connection and not for optical properties. Such metallic contact areas are located on one or on two sides of the semiconductor layer sequence. In order to keep light away from the electrical contact surfaces or to reduce a probability of incidence, an etching structure with so-called micro-prisms is etched on a side opposite these contact surfaces, especially in the case of thin-film light-emitting diodes based on InGaAlP or on InAlGaAs. A semiconductor material is removed locally by this etching structure.Such an etching structure also leads to a current-widening layer being locally missing or greatly thinned, so that no or only a few charge carriers flow in these regions as far as below the electrical contact surfaces and from there into the active zone and generate light there. In other words, light generation close to the metallic contact surfaces is avoided. In addition, the remaining semiconductor material of the semiconductor layer sequence is tapered, so that a probability of light striking a surface per distance covered by the light is increased. As a result, a coupling-out probability of the light is increased. The etching structure and the associated micro prism-like structure also increase a coupling-out probability, since the light is reflected and / or scattered at the etching structure. Such an etching structure is usually produced by a plasma etching method, in particular by etching with an inductively coupled plasma, or ICP for short.In such an etching method, however, it is comparatively difficult to accurately meet the proper etching depth. If too deep etching is used, the active zone is disturbed, which can cause poorer low current behavior, poorer temperature response and initial positive aging. Too shallow an etching, on the other hand, leads to poorer light decoupling and thus to less efficient components. Therefore, it is important to reproducibly achieve the proper etch depth. If etching is stopped at the time, i.e. after a predetermined duration, varying etching rates or even layer thickness variations in the semiconductor layer sequence as a result of the epitaxial growth make it difficult to precisely meet the suitable etching depth.The semiconductor chip described here has the etching signal layer. If the signal component is released during the etching, this signal component can be detected and the etching of the etching structure is stopped as soon as the signal component is detected or the etching is stopped after a certain time after the signal component appears or disappears, in particular in or from an etching plasma. A comparatively thin region of semiconductor material can thus be achieved in a controllable manner between the etching structure and the active zone, with the result that a low current impression takes place in these regions into the active zone and a high light decoupling efficiency is achieved. In other words, the etching signal layer allows an early and exact stopping of the etching when producing the etching structure.The active zone is based on InAlGaP or on InAlGaAs. The active zone may include one or more layers free from one or more of the main components of the respective semiconductor material. In other words, the active zone then has a varying material composition.The etching signal layer is based on In 1-x-y Al y Ga x P or on In 1-x-y Al y Ga x As. In this case, the following applies: x+y<1. The signal component is Ga, where x is greater than or equal to 0.005 or 0.01 or 0.02. In addition, x is less than or equal to 0.2 or 0.15 or 0.1 or 0.075. It may be true that y is greater than or equal to 0.3 or 0.35 or 0.4 and / or that y is less than or equal to 0.5 or 0.55 or 0.6.The thickness of the etching signal layer is at least 50 nm or 100 nm or 150 nm or 200 nm. In addition, the thickness of the etching signal layer is at most 800 nm or 600 nm or 500 nm or 400 nm.According to at least one embodiment, a concentration of the signal component is constant within the etching signal layer. Constant means in particular that a locally present concentration deviates from an average concentration of the signal component by at most 30% or 20% or 10% or 5%. In other words, no targeted concentration fluctuation of the signal component is then introduced into the etching signal layer.According to at least one embodiment, the etch signal layer is directly at the active zone, towards the etch structure and away from the active zone. In other words, the active zone and the etching signal layer then touch.According to at least one embodiment, the etching signal layer is spaced apart from the active zone. This means that the etching signal layer lies on the one hand between the active zone and the etching structure and on the other hand at least one further layer of the semiconductor layer sequence is located between the etching signal layer and the active zone.According to at least one embodiment, a respective further layer is located on each side of the etching signal layer, wherein these two further layers preferably have the same material composition within the scope of the manufacturing tolerances. In particular, these two further layers are each free of the signal constituent or the signal constituent has in these further layers at most 50% or 20% or 10% or 1% or 1 -4 or 10 or 10 -5 of the concentration in the etching signal layer.According to at least one embodiment, a ramp layer is located between the etching signal layer and the active zone. The ramp layer is preferably accommodated in the p-layer sequence. The ramp layer may directly adjoin the active zone. Alternatively or additionally, the ramp layer is also in direct contact with the etching signal layer. Ramp layer means that a concentration of at least one constituent of the ramp layer changes in a ramp-shaped manner, along a growth direction of the semiconductor layer sequence.According to at least one embodiment, the ramp layer is based on InAlGaP or on InAlGaAs. The ramp layer is based on In 1-a-b Al b Ga a P or on In 1-a-b Al b Ga a As with a+b<1. The In content 1-a-b is preferably constant in the ramp layer, within the scope of the manufacturing tolerances.In this case, the following applies preferably to a side of the ramp layer closest to the active zone: 0.10≤a or 0.15≤a or 0.2≤a and / or a≤0.3 or a≤0.35 or a≤0.4. the same values apply alternatively or additionally to b. The sum of a and b is preferably greater than or equal to 0.3 or 0.4 or 0.5 and / or less than or equal to 0.65 or 0.6 or 0.55.For a side of the ramp layer facing away from the active zone, a≤0.1 or a≤0.05 or a≤0.02 or a≤0.005 preferably applies. Alternatively or additionally, 0.35≤b or 0.4≤b or 0.45≤b and / or b≤0.65 or b≤0.6 or b≤0.55.According to at least one embodiment, the aluminum content b increases monotonically or strictly monotonically in the ramp in the direction away from the active zone. Alternatively or additionally, the aluminum content b in the active zone can change continuously, i.e. without cracks. In particular, the aluminum content b changes linearly or approximately linearly in the ramp.According to at least one embodiment, the ramp layer has a thickness of at least 50 nm or 150 nm or 200 nm. Alternatively or additionally, this thickness is at most 800 nm or 600 nm or 400 nm.According to at least one embodiment, the semiconductor chip has a p-electrode on the p-conducting layer sequence. Furthermore, the semiconductor chip contains an n-electrode on the n-conducting layer sequence. The two electrodes can each directly adjoin the associated layer sequence. The two electrodes are preferably in each case metallic electrodes, that is to say the electrodes are in each case formed by one or more layers each of a metal or a metal alloy. The p-electrode may comprise materials other than the n-electrode.According to at least one embodiment, the electrodes or at least one of the electrodes is structured to form a plurality of strips. Strip means in particular that, viewed in a plan view of the semiconductor layer sequence, a longitudinal extent of the strip exceeds a width of the strip by at least a factor of 10 or 100. The individual strips can be connected to one another and / or to a contact region for external electrical contacting by connecting webs or further elements. Instead of strips, the p-electrode can in particular also be structured to form a multiplicity of smaller island-shaped regions or islands.According to at least one embodiment, the strips and the island-shaped regions are configured to apply current to the semiconductor layer sequence. In other words, there is then no layer provided for current insulation between the strips or island-shaped regions and the semiconductor layer sequence. Such an insulation layer can be attached to the electrical contact regions for external electrical contacting and / or to the connecting webs, which are then accordingly not provided for current injection.According to at least one embodiment, the two electrodes do not overlap each other, viewed in plan view. In other words, the island-shaped regions can lie between the strips or, in the case of two electrodes structured to form strips, the electrodes can engage one in the other in a comb-like manner, wherein the strips then do not cover one another or shadow one another, as seen in plan view of the semiconductor layer sequence.According to at least one embodiment, the etching structure in the p-conducting layer sequence is located only between adjacent strips or island-shaped regions of the p-electrode, as seen in plan view. In other words, no etching structure is then present in the region of the strips or the island-shaped regions of the p-electrode. Therefore, as viewed in plan view, the etching signal layer may be entirely present below the stripes or island-shaped regions and the p-electrode.According to at least one embodiment, a roughening is present between adjacent strips on the n-electrode in the n-conducting layer sequence. It is possible for the etching structure in the p-conducting layer sequence to overlap the roughening in the n-conducting layer sequence in places, as seen in plan view of the semiconductor layer sequence.The semiconductor chip is a thin-film semiconductor chip. That is to say that the semiconductor chip is free of a growth substrate of the semiconductor layer sequence. For a mechanical stabilization and preferably also for an electrical contacting of the semiconductor layer sequence, a carrier is then present which is different from the growth substrate. In particular, the carrier is located on the p-conducting layer sequence and / or on the p-electrode. In this case, the n-conducting layer sequence is preferably provided for radiation decoupling from the semiconductor layer sequence.According to at least one embodiment, the n-conducting layer sequence and the p-conducting layer sequence are doped.A dopant concentration is preferably at least 1×10 16 / cm 3 or 1×10 17 / cm 3 or 1×10 18 / cm 3 and / or at most 3×10 16 / cm 3 or 3×10 17 / cm 3 or 3×1018 / cm3. A p-doping is effected here, for example, with magnesium. A plurality of dopants can also be present in combination.According to at least one embodiment, a distance between the etch signal layer and the active zone is at least 100 nm or 200 nm or 300 nm. Alternatively or additionally, this distance is at most 800 nm or 600 nm or 400 nm.According to at least one embodiment, the etching structure has an average depth of at least 0.25 μm or 0.75 μm and / or of at most 5 μm or 3.5 μm. Alternatively or additionally, an average width of the etching structure is at least 5 μm or 10 μm or 20 μm and / or at most 150 μm or 100 μm or 40 μm. In this case, the etching structure preferably has a planar base surface and oblique side surfaces within the scope of the production tolerances. An angle between the side surfaces and a growth direction of the semiconductor layer sequence is preferably at least 15° or 30° or 45° or 55° and / or at most 85° or 75° or 60° or 45°.According to at least one embodiment, the roughening has an average depth or average structure size or average roughness of at least 200 nm or 250 nm or 350 nm or 500 nm. Alternatively or additionally, this value is at most 5 μm or 2.5 μm or 1 μm or 0.75 μm.According to at least one embodiment, a distance between the etching structure and the active zone is at least 100 nm or 200 nm or 300 nm. Alternatively or additionally, this distance is at most 750 nm or 500 nm or 350 nm. The distance corresponds in particular to a minimum thickness of a material of the semiconductor layer sequence between the etching structure and the active zone.Furthermore, a method for producing an optoelectronic semiconductor chip is specified. The method produces an optoelectronic semiconductor chip as specified in connection with one or more of the abovementioned embodiments. Features of the semiconductor chip are therefore also disclosed for the method and vice versa.According to the method, the etching structure is created in the semiconductor layer sequence by means of dry chemical etching. The etching is preferably an etching with an inductively coupled plasma.During the etching and during the production of the etching structure, the signal component of the etching signal layer is detected and it is measured, in particular continuously, for this signal component. The etching is controlled and / or ended by an evaluation of the measurement of the signal component. For example, the etching is ended when the signal component is measured. Likewise, the etching can be terminated after a certain time after the signal component occurs. It is also possible to end the etching only when a measurement signal of the signal component decreases or disappears, i.e. when the etching signal layer is etched through.An optoelectronic semiconductor chip described here is explained in more detail below with reference to the drawing on the basis of exemplary embodiments. Identical reference numerals indicate identical elements in the individual figures. However, no references to scale are shown; rather, individual elements may be shown with exaggerated size for better understanding.The following are shown: FIGS. 1 to 5 show schematic representations of exemplary embodiments of optoelectronic semiconductor chips described here.FIG. 1 shows a schematic illustration of a structure of a semiconductor layer sequence 2 for an optoelectronic semiconductor chip 1. What is shown here is a portion x of a signal component in the semiconductor layer sequence 2 along a growth direction G of the semiconductor layer sequence 2. the semiconductor chip 1 is a light-emitting diode chip for generating preferably yellow or red light.The semiconductor layer sequence 2 has an n-conducting layer sequence 21. In contrast to the illustration, the n-conducting layer sequence 21 can have a plurality of sublayers. The n-conducting layer sequence 21 is based, for example, on InAlP. A thickness of the n-conducting layer sequence 21 is preferably at least 1 μm or 2 μm or 3 μm and / or at most 10 μm or 7 μm or 5 μm, as is also the case in all other exemplary embodiments.Along the growth direction G, the n-conducting layer sequence 21 is followed by an active zone 22. The active zone 22 is illustrated only in a greatly simplified manner and preferably comprises a plurality of quantum wells and interposed barrier layers and preferably also barrier layers for holes and for electrons. The active zone 22 is based on In 1-x-y Al y Ga x P. Depending on the emission wavelength, the quantum troughs in the active zone 22 are considered to be 0.15≤x or 0.2≤x and / or x≤0.5 or x≤0.4. The barrier layers in the active zone 22 are considered to be, depending on the emission wavelength, preferably 0.15≤x or 0.2≤x and / or x≤0.4 or x≤0.35. an indium content 1-x-y is about 50% and thus 0.5 with a tolerance of preferably at most 0.1 or 0.05. A thickness of the active zone 22 is, for example, at least 300 nm or 100 nm and / or at most 1000 nm or 2000 nm.Along the growth direction G, the active zone 22 is immediately followed by a p-conducting layer sequence 23. A first layer of the p-conducting layer sequence 23 is formed by a p-doped etching signal layer 24. A thickness of the etching signal layer 24 is preferably about 300 nm. The etching signal layer 24 is based on In 1-x-y Al y Ga x P with x≈0.05 and y≈0.45.The Ga content x of the etching signal layer 24, corresponding to the signal component, is selected such that, on the one hand, an effective charge carrier barrier is formed with respect to the active zone 22 and that, on the other hand, during the etching of the semiconductor layer sequence 2, a sufficient measurement signal with respect to the signal component results when the etching signal layer 24 is exposed. Accordingly, the Ga content x is comparatively small to achieve sufficient charge carrier capture in the active region 22.Along the growth direction G, the etching signal layer 24 is followed by a further p-layer 25. The p-layer 25 is based on InAlP. A thickness of the further p-layer 25 is at least in regions preferably at least 500 nm or 1000 nm or 1500 nm and / or at most 3000 nm or 2000 nm.The p-conducting layer sequence 23 can have additional layers, not shown, on a side of the further p-layer 25 facing away from the active zone 22, for example for better electrical contacting of the semiconductor layer sequence 2.An etching structure 3 is produced on the p-conducting layer sequence 23, see also the sectional illustration in FIG. 5A and the schematic plan view in FIG. 5B. The etching structure on the p-conducting layer sequence 23 is produced in regions between a p-electrode 43 structured to form islands 46. Due to the etching structure 3 and thus due to the regional removal of the p-layer 25 following along the growth direction G of the etching signal layer 24, current expansion is locally prevented and radiation decoupling efficiency is increased. Instead of islands 46, the p-electrode 43, unlike that shown, can also be structured to strips, analogously to the n-electrode 41.According to FIG. 5A, a growth substrate is removed from the semiconductor layer sequence 2. Instead, a carrier 6 for electrical contacting and mechanical stabilization is attached to the p-conducting semiconductor layer sequence 23. On the n-conducting layer sequence 21, there is an n-electrode 41 structured to form webs 44 and an electrical contact surface 45, in particular for attaching a bonding wire, not shown. Optionally, a roughening 5 is produced on the n-conducting layer sequence 21. In contrast to the illustration, an etching signal layer can likewise be present for producing the roughening 5.FIG. 2 shows a further exemplary embodiment of the semiconductor chip 1. According to FIG. 2, a p-layer 25 aof the same composition is situated between the active zone 22 and the etching signal layer 24 as on a side of the etching signal layer 24 facing away from the active zone 22. Due to this p-type layer 25 alocated between the active region 22 and the etching signal layer 24, a full barrier height toward the active region 22 can be exhausted, whereby improved charge carrier trapping in the active region 22 can be realized. A thickness of this p-layer 25 ais, for example, at least 50 nm or 100 nm and / or at most 500 nm or 400 nm, preferably approximately 300 nm. The structure of the semiconductor layer sequence 2, as illustrated in FIG. 2, also corresponds to the structure of the semiconductor layer sequence, as drawn in FIG. 5A.In comparison to the semiconductor layer sequence 2 according to FIG. 1, the etching signal layer 24 is therefore located further away from the active zone 22. In order nevertheless to achieve a small remaining thickness of the p-conducting layer sequence 23 in regions with the etching structure 3, it is possible for the etching of the etching structure 3 to take place only with a time delay after the occurrence of the signal constituent, that is to say Ga, or for the etching to be stopped in response to a falling signal of the signal constituent. If overetched over in time, this nevertheless takes place with a comparatively high precision, since a proportion of the overetch time is small compared to a total etching time, so that an influence of a varying etching rate or a thickness variation in the semiconductor layer sequence 2 due to epitaxy tolerances is correspondingly reduced.Thus, in contrast to the illustration in FIG. 5A, the etching structure 3 can also penetrate the etching signal layer 24 in places. Likewise, in the regions between the webs 44 of the p-electrode 43, the etching signal layer 24 can be completely removed.In the embodiment according to FIG. 3, a ramp layer 26 is located between the active zone 22 and the etching signal layer 24. An indium content remains approximately constant in this case, such that an aluminum fraction in the ramp layer 26 increases along the growth direction G. A thickness of the ramp layer 26 is, for example, approximately 300 nm. Thus, in the ramp layer 26, in contrast to the etching signal layer 24, a proportion of aluminum and gallium is varied.In the embodiment according to FIG. 4, the intermediate layer 25a is located between the ramp layer 26 and the etching signal layer 24, in a similar manner to the embodiment according to FIG. 2.

Claims

Optoelectronic semiconductor chip (1) which is a light emitting diode, having a semiconductor layer sequence (2), wherein the semiconductor layer sequence (2) has: - an n-conducting layer sequence (21), - a p-conducting layer sequence (23), - an active zone (22) which lies between the n-conducting layer sequence (21) and the p-conducting layer sequence (23), - at least one etching signal layer (24) in the p-conducting layer sequence (23) and / or in the n-conducting layer sequence (21), and - an etching structure (3) on a side of the etching signal layer (24) remote from the active zone (22), wherein - the etching structure (3) reaches at least as far as into the etching signal layer (24), - the etching signal layer (24) has a signal constituent, the active zone (22) is configured for generating radiation and is based on InAlGaP or on InAlGaAs, the etching signal layer (24) is located in or on the p-conducting layer sequence (23) and is based on In 1-x-y Al y Ga x P or on In 1-x-y Al y Ga x As with x+y<1, the signal component is Ga and 0.005≤x≤0.2, the signal component is not present in a layer (25) adjoining the etching signal layer (24) in the direction of the etching structure (3), a thickness of the etching signal layer (24) is between 50 nm and 800 nm inclusive, a material of the etching signal layer (24) is partially removed by the etching structure (3), the semiconductor chip (1) is free of a growth substrate of the semiconductor layer sequence (2), and radiation decoupling takes place at the n-conducting layer sequence (21) and a carrier (6) is located at the p-conducting layer sequence (23).Optoelectronic semiconductor chip (1) according to the preceding claim, in which the etching structure (3) has a prismatic or trapezoidal shape, as seen in cross section, wherein a width of the etching structure (3) decreases in the direction towards the active zone (22), such that an upstream-widening layer of the semiconductor layer sequence (2) is removed locally by the etching structure (3) and such that a coupling-out probability of light generated in the active zone (22) out of the semiconductor layer sequence (2) is increased by the etching structure (3).Optoelectronic semiconductor chip (1) according to one of the preceding claims, in which a concentration of the signal constituent in the etching signal layer (24) is constant, with a tolerance of at most 20% of an average concentration of the signal constituent in the etching signal layer (24).Optoelectronic semiconductor chip (1) according to one of the preceding claims, in which the etching signal layer (24) directly adjoins the active zone (22), in the direction of the etching structure (3).Optoelectronic semiconductor chip (1) according to one of Claims 1 to 3, in which the etching signal layer (24) is spaced apart from the active zone (22).Optoelectronic semiconductor chip (1) according to the preceding claim, in which a respective further layer (25) is located on each side of the etching signal layer (24), and these further layers (25) have the same material composition, wherein these further layers (25) are free of the signal constituent.Optoelectronic semiconductor chip (1) according to either of Claims 5 and 6, in which a ramp layer (26) is situated between the etching signal layer (24) and the active zone (22) in the p-layer sequence (23), said ramp layer being based on In 1-a-b Al b Ga a P or on In1 -a-b Al b Ga a As, where a + b < 1, wherein - in the direction away from the active zone (22) in the ramp layer (26), the Al content b increases monotonically or strictly monotonically and the ramp layer (26) directly adjoins the active zone (22), - at the active zone (22), 0.15≤a≤0.35 and 0.15≤b≤0.35 and 0.4≤a+b≤0.6, and - at a side of the ramp layer (26) facing away from the active zone (22), a≤0.05 and 0.4≤b≤0.6.Optoelectronic semiconductor chip (1) according to the preceding claim, in which the Al content b changes linearly in the ramp layer (26) and the indium content 1-a-b is constant, wherein a thickness of the ramp layer (26) is between 50 nm and 500 nm inclusive.Optoelectronic semiconductor chip (1) according to one of the preceding claims, which furthermore has a p-electrode (43) on the p-conducting layer sequence (23) and an n-electrode (41) on the n-conducting layer sequence (21), wherein the electrodes (41, 43) are each structured to form a multiplicity of strips (44) or islands (46), and the strips (44) or the islands (46) of both electrodes (41, 42) are arranged without overlapping in a radiation-generating region, viewed in plan view, and wherein the etching structure (3) in the p-conducting layer sequence (23) is present in the radiation-generating region only between adjacent strips (44) or islands (46) of the p-electrode (43).Optoelectronic semiconductor chip (1) according to the preceding claim, in which a roughening (5) is present between adjacent strips (44) of the n-electrode (41) in the n-conducting layer sequence (21).Optoelectronic semiconductor chip (1) according to one of the preceding claims, wherein - the etching signal layer (24) is based on In 1-x-y Al y Ga x P with 0.35 ≤ y ≤ 0.55 and with 0.02 ≤ x ≤ 0.15 and has a thickness between 150 nm and 500 nm inclusive and is doped with Mg with a concentration between 1 × 10 16 cm -3 and 3 × 10 18 cm -3 inclusive, - the p-layer (25) adjoining the etching signal layer (24) is based on In 1-x-y Al y Ga x P with 0.4 ≤ y ≤ 0.6 and with x ≤ 0.001, a distance between the etching signal layer (26) and the active zone (22) is between 200 nm and 600 nm inclusive, the etching structure (5) has an average depth between 250 nm and 5 μm inclusive, and a distance between the etching structure (3) and the active zone (22) is between 100 nm and 500 nm inclusive.Method with which an optoelectronic semiconductor chip (1) according to one of the preceding claims is produced, having the steps: - providing the semiconductor layer sequence (2) with the n-conducting layer sequence (21), the p-conducting layer sequence (23), the active zone (22) and the etching signal layer (24), - producing the etching structure (3) by means of dry-chemical etching of the semiconductor layer sequence (2), and - finishing the semiconductor chip (1), wherein - during the etching the signal component of the etching signal layer (24) is measured, and - the etching is ended by an evaluation of the measurement of the signal component.Method according to the preceding claim, wherein the etching is an etching with inductively coupled plasma, wherein the etching signal layer (24) is completely penetrated locally during the etching.

Citation Information

Patent Citations

  • Optoelectronic semiconductor chip

    DE102011111919A1

  • METHOD AND DEVICE FOR ENDPOINT CONTROL IN PLASMA ETCHING

    DE2736262A1

  • Method of manufacturing an optical semiconductor element

    US20070099324A1

  • Semiconductor light-emitting device

    US20090206354A1

  • Semiconductor laser

    US20130182735A1