Method for reinforcing a building structure and device for such a method

The polymerization acceleration device and method using electrical heating and insulation for carbon fiber strips address the challenge of achieving rapid and reliable adhesion to construction supports, ensuring efficient reinforcement within limited time frames.

FR3139149B1Active Publication Date: 2024-10-25SOLETANCHE FREYSSINET SAS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2022008578
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-08-26
Publication Date
2024-10-25
Estimated Expiration
2042-08-26

Smart Images

  • Figure 00000011_0000
    Figure 00000011_0000
  • Figure 00000011_0001
    Figure 00000011_0001
  • Figure 00000011_0002
    Figure 00000011_0002
Patent Text Reader

Abstract

A polymerization acceleration device (20) designed to heat at least one strip (30) of dry carbon fiber fabric, the device being fixed to an area to be reinforced (10) of a construction structure and comprising: - a pair of connector supports (21), each comprising a fastening element (25) for attaching the connector support to the area to be reinforced; - a pair of electrical contact elements (27) for transmitting an electric current between a first end (31) and a second end (32) of the strip (30); - one or more electrical connectors (23) held by the connector support (21) and in contact with the electrical contact element (27); the device further comprising at least one pair of first insulating elements (26, 40), each arranged in contact with the connector support (21) to electrically insulate the area to be reinforced (10) from the connector support (21). Abstract figure: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Method for reinforcing a construction work and device for such a method Technical field

[0001] The present disclosure relates to the field of strengthening a construction work, such as for example a civil engineering structure, and in particular a method for strengthening a construction work as well as a device for implementing the method. Prior art

[0002] Certain methods of this type are known, such as for example that described by document FR 2 747 146 Bl, using carbon fiber reinforcement strips mixed with an epoxy resin matrix which is applied to the structure to be reinforced. The resin then undergoes polymerization, which forms a composite material and makes the carbon fibers adhere to the support. The polymerization, although highly dependent on thermal conditions, is sometimes time-constrained, which is particularly the case during work to reinforce beams or slabs of reinforced or prestressed concrete bridges, such as viaducts, so as to maintain road traffic on the structure during certain time slots, without however blocking traffic the rest of the time. For practical reasons, the time between the end of the application of the reinforcement strip and the reopening of traffic is for example approximately 3 to 4 hours.Reinforcing strips bonded externally to the concrete must have a minimum adhesion to the substrate and a minimum shear strength before being subjected to loads, otherwise they will slip on the substrate and not sufficiently relieve the metal reinforcements in place in the concrete. A minimum value criterion for adhesion of the composite to the substrate, measured by direct tensile test, has been set at 1.0 MPa, before authorizing the resumption of traffic on the structure.

[0003] On a dry concrete support, the inventors were able to observe that the value of the direct tensile adhesion of epoxy resins, used to produce composite reinforcements bonded to concrete and of millimeter thickness, generally only reaches 1.0 MPa after approximately 7 hours at an ambient temperature of 20°C and approximately 24 hours at an ambient temperature of 10°C. However, during night work, and particularly in western regions, ambient temperatures can quickly drop below 10°C. Furthermore, the concrete support, on which the reinforcing composite is bonded, has a high thermal inertia and is more or less humid, which makes it difficult to heat and unsuitable for epoxy resin because it absorbs and diffuses the surface heat produced by the exothermicity of the resin during its polymerization.

[0004] A common solution consists of confining the entire area to be treated and heating it before, during and after application so as to maintain a constant temperature of at least 20°C. This solution is easy for areas inside structures but more complex and expensive for external surfaces, without real control of the temperature at the composite-support interface.

[0005] A less common solution is to add an accelerator to the formulation of epoxy resins. But to achieve a direct tensile adhesion of at least 1.0 MPa at 4 hours, the quantity of accelerator to be added is such that it modifies the mechanical performance downwards and therefore that of the reinforcement composite in unacceptable proportions.

[0006] Another solution, known from document US 6,605,168 B1, consists, after having formed a composite lamella including carbon fibers, in adhering this composite lamella by means of a bonding resin. To accelerate the polymerization of the bonding resin, the method of this document passes an electric current into the composite lamella where the carbon fibers provide electrical conduction. At each end, the matrix of the composite lamella is removed to expose the carbon fibers and allow the passage of the electric current which is brought by metal plates connected to a current source. The composite lamella thus diffuses towards the bonding resin heat generated by the Joule effect, thus accelerating its polymerization.It is relatively difficult to control the heating of the bonding resin with this type of solution which requires special preparation at the ends of the lamella and can present a risk of short circuit through the substrate to be reinforced.

[0007] The challenge therefore lies in implementing a reinforcement process that is both reliable and possible over a limited time. Summary

[0008] A polymerization acceleration device is provided, intended to heat at least one strip of carbon fiber fabric applied in an area to be reinforced of a construction work extending between a first end and a second end. The device comprises, at each of the first and second ends: - a connector support comprising an element for fixing the connector support to the area to be reinforced; - an electrical contact element for transmitting an electric current through the strip; - one or more connectors held by the connector support and in contact with the electrical contact element; and at least one insulating element in contact with the support. The at least one insulating element electrically insulates the area to be reinforced from the connector support.

[0009] This device allows the matrix of the composite reinforcement formed to be heated directly in the area to be reinforced. It also prevents short circuits from disrupting the operation.

[0010] According to one example, the fixing element may comprise a drilling in the connector support for the passage of a screw, and the at least one insulating element comprises a spacer capable of cooperating with the drilling and the screw, the spacer being made of electrically insulating material.

[0011] Alternatively, or additionally, the at least one insulating element comprises an electrical insulation element arranged in contact with the strip to electrically insulate the area to be reinforced from the electrical contact element. The material of this electrical insulation element may furthermore be polymerizable.

[0012] According to another aspect, there is provided a method for reinforcing a construction work. The method uses a strip of dry carbon fiber fabric in an area to be reinforced extending between a first end and a second end. This method comprises: - arrange at least one insulating element at each of the first and second ends; - coat the area to be reinforced with a layer of thermosetting polymer; - apply a strip of dry carbon fiber fabric to the coated area; - at each of the first and second ends, arrange an electrical contact element over the strip of dry fabric; and - flowing an electric current between the electrical contact elements through the carbon fibers of the strip to accelerate the polymerization of the polymer with the strip.

[0013] The dry carbon fiber fabric strip may further be applied to the coated area by causing it to cover the insulating elements at the first and second ends.

[0014] It is possible to apply a plurality of strips simultaneously to the coated surface for simultaneous polymerization of the plurality of strips with the polymer. According to one example, two strips can be applied simultaneously and by superposition on the previously coated area to be reinforced.

[0015] The strip and the polymer form a composite reinforcement which can be heated for a period of between 50 minutes and 3 hours, at a temperature of between 60°C and 90°C by the circulation of electric current. Brief description of the drawings

[0016] Other characteristics, details and advantages will appear on reading the detailed description below, and on analyzing the attached drawings, in which: Fig.l

[0017] [Fig.l] shows a schematic diagram of the implementation of the method and an associated device. Fig. 2

[0018] [Fig.2] shows an example of embodiment of the device arranged on a concrete support, in a sectional view along a longitudinal direction of the device. Fig. 3

[0019] [Fig.3] shows another example of embodiment of the device arranged on a metal support, in the same view as that of [Fig.2]. Description of the embodiments

[0020] [Fig.l] is a schematic diagram illustrating the method for reinforcing a construction work, comprising an area to be reinforced of a construction work (support 10) and the device 20 used to implement this method. The support 10 may for example be made of reinforced or prestressed concrete, i.e. with metal reinforcements, or a metal structure of the frame type.

[0021] A strip 30 of dry carbon fiber fabric is arranged on the support 10, on which a layer of a thermosetting polymer, such as for example an epoxy resin, is previously coated. The resin is capable of adhering to the support and impregnating the carbon fibers, and is also capable of filling irregularities or cracks that may appear on the surface of the support to be reinforced. For polymerization, the resin impregnates the strip of fabric and contributes to forming a composite adhering to the support 10. The (thermosetting) polymer has a dual function, on the one hand that of a matrix to form with the carbon fibers a composite for reinforcing the structure and on the other hand that of an adhesive to make the composite adhere to the surface of the structure.The reinforcement composite is thus manufactured directly on the surface of the structure to be reinforced, which eliminates a preliminary step of preparing the composite before making it adhere to the surface of the structure to be reinforced.

[0022] The device 20 used during the process makes it possible to accelerate the polymerization of the polymer so as to obtain a composite which meets, in a defined time, a limit criterion of adhesion to the support greater than a given value. As can be seen by way of example in [Fig.l], the device 20 is divided into two identical parts, each being arranged on either side of the strip 30 and is connected to a source of electric current so as to form a closed electric circuit with the strip 30. The strip 30 of carbon fibers, thus crossed by an electric current, diffuses heat to the polymer by the Joule effect, which accelerates its polymerization and the formation of the composite.

[0023] Figures 2 and 3 illustrate by way of example one half of the device 20 used at one end of the strip 30, each of these figures representing an example of embodiment of the device on a different support. The support illustrated in [Fig.2] is made of concrete (reinforced or prestressed), while the support illustrated in [Fig.3] is metallic. In these examples, each half of the device 20 comprises connectors 23 associated with an electrical contact element 27, such as for example a copper plate, electrically conductive. In a manner common to Figures 2 and 3, the connectors 23 can be clamping screws, made of brass, screwed into a connector support 21 and bearing against the electrical contact element 27, to press said element 27 against the strip 30. The figures illustrate four connectors, however the device 20 is not limited to this example.Two connectors per support 21 may, in certain cases, be sufficient to produce the device. At least one of the connectors 23 is electrically connected to a terminal of a variable intensity electric current generator, making it possible to regulate the power, temperature and heating time of the reinforcement. At the opposite end of the strip, the connector(s) 23 are thus connected to the opposite terminal of the generator. The other connectors 23 not connected to the generator can serve only as a support for pressing the electrical contact element against the strip 30. Consequently, the connectors 23, which are for example brass screws, transmit an electric current from a generator to the electrical contact element 27, itself in contact with the carbon fiber strip, thus heated. Advantageously, heating the strip makes it possible to accelerate the polymerization of the thermosetting polymer, and therefore the formation of the reinforcement composite.

[0024] The connector support 21 is made of metallic material, for example steel, chosen in particular for its rigidity. The connector support 21 is arranged over the electrical contact element 27. The connector support 21 comprises an intermediate portion 21A and two end portions 21B. The intermediate portion 21A receives the connectors 23 and is arranged over the electrical contact element 27 (with reference to FIGS. 2 and 3), but without contact with the electrical contact element 27, so as to avoid any short circuit between the support 21 and the electrical contact element 27. The two end portions 21B are arranged opposite the support 10, either directly in support, or indirectly, via an insulating element as described later. Each end portion 21B comprises a fixing element 25 provided for fixing the connector support 21 to the surface of the structure.The fixing element 25 is for example a drilling provided to cooperate with a screw 24, the screw 24 penetrating into the material of the support 10.

[0025] For a reinforced or prestressed concrete support, a fortiori for a metal support (of a metal structure to be reinforced), a risk of short circuit exists, linked to the possible contact of the screws 24 fixing the end portions 21B with the reinforcements concrete or the metal structure of the support. To overcome this drawback, the end portions 21B are equipped so as to be electrically insulated from the power supply connection. For example, a first insulating element 26 may be arranged around the screw 24 so as to insulate it from the connector support 21 in electrical contact with the connectors 23. The insulating element 26, as illustrated in FIGS. 2 and 3, may for example be a spacer arranged in the fixing element 25 of the end portion 21B. The spacer is drilled to allow the screw 24 to be inserted therein. It may be tapped to correspond to the screw 24, or not. The electrically insulating element 26 is made of an electrically non-conductive material, such as for example Teflon. Figures 2 and 3 illustrate an exemplary embodiment of the electrically insulating element 26. However, the electrically insulating element is not limited to this example.Indeed, according to another example, not illustrated, it is possible to provide an electrically insulating element arranged around each connector 23, and in contact with the connector support 21, so as not to transmit an electric current to the connector support 21.

[0026] With reference to the metal support 10 of [Fig. 3], a second risk of short circuit exists, linked to the contact of the carbon fiber fabric with the metal support 10. To remedy this, the device 20, which already comprises a first insulating element 26, may provide a second insulating element 40, arranged between the support 10 and the strip 30. The second insulating element 40 is an interposed element, made of electrically insulating material, and is for example a strip of glass fiber fabric. In [Fig. 3], the strip of glass fiber fabric extends between the resin and the strip 30, of width and length at least equal to the width and length of the strip 30, to electrically insulate the entire strip 30 from the support 10. The strip of glass fiber fabric is associated with the reinforcing composite with the resin and the strip 30.

[0027] Alternatively, as illustrated by way of example in [Fig. 2], the second insulating element 40 may take the form of two insulating parts, each being arranged under an end portion 21B, and of dimensions at least equal to the dimensions of the surface of the end portion 21B in contact with the zone to be reinforced, so as to limit any electrical transmission between the connector support 21 and the zone to be reinforced.

[0028] To reinforce the structure, the strip 30 used may have a length of between 2 m and 6 m, a width of between 75 mm and 300 mm and a thickness of the order of a millimeter. The strip 30 may further have an electrical resistance of between 0.2 and 1.0 Ohm. The strip 30 may be composed of carbon fibers, the weight of which is between 200 g / m2 and 1200 g / m2. However, any other reinforcing fabric having electrical conduction characteristics similar to carbon fibers may be used instead of carbon fibers. Two devices 20 may be arranged on the strip 30, each at one end 31, 32 of the strip. For example, the two devices 20 are separated by a length L of 2 meters.

[0029] The method for reinforcing the construction work is described below. The method consists of preparing the surface of the area to be reinforced of the construction work by coating it with the layer of thermosetting polymer, applying one (or more) strips 30 of dry carbon fiber fabric to the coated surface, then heating the strip 30 to accelerate the polymerization of the polymer and thus accelerate the formation of the reinforcing composite. During the preparation of the support, it may be provided first to apply the resin to the support 10, then to fix the device 20 with its first insulating elements 26 to the support 10, or vice versa.It should also be noted that the resin layer is not visible in Figures 2 and 3 because it is not applied to the ends 31, 32 of the strip, in order to avoid adhesion to the support 10 by polymerization of the strip 30 and thus allow the removal of the device 20 once the reinforcement of the support has been carried out. For example, a gap of 5 cm is provided between the resin and the device 20. The electrical connection of the strip 30 is therefore made at its two ends 31, 32 on an excess length of fabric left dry, without resin.

[0030] The strip 30 is then placed over the resin. In order to make the resin penetrate into the carbon fibers, and obtain a homogeneous composite without discontinuities or occlusions on the surface, it is possible to provide for a marouflage of the strip 30. Alternatively, several strips can be placed simultaneously on the resin, for example two or three strips. An intermediate layer of resin can be provided between each strip to promote their adhesion. This alternative has the advantage of implementing a reinforcement composed of multi-layers (superimposed) in a single matrix impregnation and heating operation, instead of providing for the formation of several composite reinforcement strips and gluing them each one after the other on the support, which represents a considerable time saving.

[0031] At its ends 31, 32, the strip 30 is pressed against the support 10 using the electrical contact element 27 and the connectors 23 installed on the connector support 21. The strip 30 is then heated to obtain the composite reinforcing the structure. Advantageously, the method does not require prior preparation of the reinforcing composite before its bonding to the support 10, by an adhesive to be provided in addition. The composite is in fact formed directly on the support at the same time as it adheres to the support, the resin fulfilling a dual function of matrix of the composite and adhesive for the support. In the case of a composite reinforcement with several strips 30, that is to say multi-layer, the method allows the implementation of the reinforcement in a single operation of impregnation of the matrix and heating. We therefore observe, thanks to the method, a considerable saving of time to make a composite of reinforcement on a support (for example respecting a limit criterion of adhesion to the support greater than 1 MPa). The process is also very simple to implement, thanks in particular to the lightness and maneuverability of the strips of dry fabric to be placed on the support and to the single bonding action required to make the composite stick to the support.

[0032] Alternatively, the second insulating element(s) 40 can be applied to the resin, before the strip 30.

[0033] To accelerate the polymerization of the resin, the generator supplies an electric current to the strip 30, which heats by the Joule effect. The power of the generator is adjustable in order to reach the desired temperature in the strip 30. It is thus possible to provide thermal probes and / or infrared cameras to measure the temperatures of the support 10, of the support-composite interface, of the composite and / or of the surface of the composite.

[0034] The generator may be provided with a regulation system so as to impose a predefined heating cycle, independently of the ambient conditions and the thermal characteristics of the support 10. The heating temperature and its duration are also capped so that the emission of steam at the surface is not detrimental to the bonding interface during polymerization. The heating cycle makes it possible to uniformly heat the composite at the surface and at the core, as well as at the composite-support interface.

[0035] By way of example, the temperature rise rate may be 5 to 10°C / min depending on the number of layers and their dimensions, and the heating time may be 1 hour at 80°C and 2 hours at 60°C, which may be sufficient to achieve a target value of IMPa of adhesion to the support, corresponding to a hardness of 55 to 60 shore D.

[0036] It is therefore possible to provide for heating the strip 30 to a temperature between 60°C and 90°C, for example 70°C, to obtain a direct tensile adhesion value of at least 1.0 MPa after 4 hours of heating. After stopping the heating of the strip, that is to say without additional heating, the polymerization of the composite can continue if it is not completely complete. It is thus possible to obtain a composite adhering to the support having a direct tensile adhesion value greater than the desired target value, for example twice as high.

[0037] It is therefore understood that the method and the device described above make it possible to produce reinforcement for a construction work meeting determined constraints of implementation time and resistance, while presenting a device of reliable, simple and easy-to-use design.

Claims

Claims

1. Device (20) for accelerating polymerization, intended to heat a composite reinforcement including at least one strip (30) of carbon fiber fabric applied in an area to be reinforced (10) of a construction work extending between a first end (31) and a second end (32), the device comprising, at each of the first and second ends: - a connector support (21) comprising a fixing element (25) of the connector support to the area to be reinforced; - an electrical contact element (27) for transmitting an electric current through the strip (30); - one or more connectors (23) held by the connector support (21) and in contact with the electrical contact element (27);and - at least one insulating element (26, 40) in contact with the connector support (21), in which the at least one insulating element (26, 40) electrically insulates the area to be reinforced (10) from the connector support (21), and in which the fixing element (25) comprises a bore in the connector support (21) for the passage of a screw (24), and the at least one insulating element comprises a spacer (26) capable of cooperating with the bore (25) and the screw (24), the spacer (26) being made of electrically insulating material.;

2. Device according to claim 1, in which the at least one insulating element comprises an electrical insulating element (40) arranged in contact with the strip (30) to electrically insulate the area to be reinforced (10) from the electrical contact element (27).

3. A device according to claim 2, wherein the material of the electrically insulating element (40) is polymerizable.

4. A method for reinforcing a construction work using the device according to any one of claims 1 to 3, the method using a strip (30) of dry carbon fiber fabric in an area to be reinforced (10) extending between a first end (31) and a second end (32), and comprising: - arranging at least one insulating element (26, 40) at each of the first and second ends; - coating the area to be reinforced (10) with a layer of thermosetting polymer-

5.

6.

7.

8. cis sand; - impregnate and apply a strip (30) of dry carbon fiber fabric to the coated area; - at each of the first and second ends, arranging an electrical contact element (27) over the strip (30) of dry fabric; and - circulating an electric current between the electrical contact elements (27) through the carbon fibers of the strip (30) to accelerate the polymerization of the polymer with the strip (30). The method of claim 4, wherein the strip (30) of dry carbon fiber fabric is applied to the coated area so that it covers the insulating element (26, 40) disposed at each of the first and second ends. Method according to claim 4 or 5, in which a plurality of strips (30) are applied simultaneously to the coated surface for simultaneous polymerization of the plurality of strips with the polymer. Method according to claim 6, in which two strips (30) are applied simultaneously and by superposition to the previously coated area to be reinforced. A method according to any one of claims 4 to 7, wherein the strip (30) and the polymer form a composite reinforcement which is heated for a period of between 50 minutes and 3 hours, at a temperature of between 60°C and 90°C by the circulation of electric current.