Mattress made from plant fibers derived from cereal crops.
A mattress of plant fibers using heat-binding fibers with a decitex less than 1.9 dtex, made from cereal lignocellulosic plants, addresses the thermal conductivity and biosourced limitations of existing insulation materials, achieving optimal insulation performance and supporting a circular economy.
Patent Information
- Application Number
- FR2022012791
- Authority / Receiving Office
- FR · FR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-12-05
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2042-12-05
AI Technical Summary
Existing insulation materials, such as rice straw fiber mattresses, have suboptimal thermal conductivity and rely on thermobonding fibers with plastic materials, limiting their biosourced nature and availability, which is a challenge for a circular economy approach.
A mattress of plant fibers secured by heat-binding fibers with a decitex less than or equal to 1.9 dtex, using cereal lignocellulosic plants like wheat straw, with a specific core and sheath structure to ensure bonding and mechanical resistance while minimizing thermal bridges.
The solution achieves a thermal conductivity of less than 40 mW/m/K, optimizing insulation performance and promoting a biosourced, locally producible, and eco-friendly insulation material.
Smart Images

Figure 00000016_0000 
Figure 00000016_0001 
Figure 00000017_0000
Abstract
Description
Title of the invention: Mattress made of plant fibers based on cereal plants.
[0001] The present invention relates to the field of construction materials, and more particularly to construction materials intended to provide thermal and / or acoustic insulation.
[0002] Construction materials represent a significant portion of energy consumption and greenhouse gas emissions. Among these construction materials, mineral wools are the most energy-intensive insulation materials. Manufacturers of construction materials for insulation are seeking to reduce the environmental impact of insulation materials, particularly by researching new insulation materials.
[0003] Among the options considered by these manufacturers, insulation materials made from plant fiber mats appear to be particularly relevant. In particular, insulating mats can be made from wood fibers. While these mats are highly effective, whether for interior or exterior building insulation, the availability of raw materials is a problem. Plants for defibrating and manufacturing insulation materials must be located as close as possible to forests to be part of a circular economy, and the forests from which wood can be harvested for the production of insulation panels are scattered. It is also known to use rice straw to make insulating mats from plant fibers. However, the thermal conductivity characteristics of this straw are not optimal.Indeed, existing rice straw fiber mattresses have a thermal conductivity value of at best 0.040 W / m / K at 20°C, which makes rice straw an insulating material whose use for building insulation remains limited, given that in these applications, insulating mattresses with a thermal conductivity value equal to or less than 0.036 W / m / K at 20°C are particularly sought after.
[0004] Furthermore, it is known to bind these plant fibers with thermal bonding fibers, which ensure that the fibers hold together with respect to each other once all of these fibers have been passed through an oven, but the use of these thermal bonding fibers, which contain plastic materials, must be controlled to ensure that the insulating material panels produced are as bio-based as possible.
[0005] The present invention takes into account this threefold context, namely to offer an insulating product that fits within a circular economy context, which presents low thermal conductivity values and as bio-based as possible.
[0006] The present invention relates to a mattress of plant fibers characterized in that it comprises plant fibers based on cereal plants bonded together by means of thermal bonding fibers, the thermal bonding fibers having a decitex less than or equal to 1.9 dtex.
[0007] The plant fibers present in the mattress according to the invention, i.e. a mattress intended for the production of insulating panels, and in particular semi-rigid panels intended for the interior insulation of buildings, are specific fibers from cereal lignocellulosic plants.
[0008] Straw is a lignocellulosic material which presents an eco-responsible image and the inventors were able to observe that its technical characteristics could be favorable to an application to plant fiber mattresses for insulating panels.
[0009] Straw is a very abundant raw material, particularly in France where it is estimated that approximately 30 million tons are produced each year. Straw is thus a widely available and readily mobilized resource due to its production throughout metropolitan France and also across Europe. Consequently, the production of insulating panels using plant fibers derived from cereal crops is fully aligned with a circular economy approach, since it is possible to establish straw processing and insulating panel manufacturing plants in scattered areas of the country and to be as close as possible to potential buyers.
[0010] The plant fibers are bonded together by means of thermally bonding fibers. These thermally bonding fibers have a rigid core and a more flexible sheath. The core and the sheath have distinct melting temperatures. More precisely, the core has a higher melting temperature than the sheath. The mixture of thermally bonding fibers and plant fibers is intended to be heated in an oven to a temperature such that the sheath melts and bonds with the plant fibers adjacent to the sheath, while the structure of the core remains unchanged. It is understood that the thermally bonding fibers ensure, on the one hand, the bonding of the plant fibers to one another by means of the sheath, and on the other hand, a mechanical role by providing mechanical resistance to the mat of plant fibers by means of the rigid core.These thermally bonding fibers are mixed with the plant fibers in a sufficient percentage to obtain adequate adhesion of the plant fibers to each other, but low enough not to limit the insulating properties of the plant fiber mat.
[0011] The decitex of the thermally bonding fibers is a known parameter that defines the fineness of said thermally bonding fibers. It should be noted that this parameter defines the fineness The thermal bonding fibers must be measured before being placed in an oven and partially melted. The decitex of the thermal bonding fibers should therefore be measured prior to mixing the plant fibers and the thermal bonding fibers, or at the very least before placing the mixture in an oven.
[0012] More specifically, the inventors have highlighted that, in a context where it is sought to use a maximum of bio-based elements, thermal bonding fibers with a low decitex make it possible to reduce the mass of thermal bonding fibers relative to the mass of the plant fiber mat, without limiting the holding of the plant fibers to each other thanks to these thermal bonding fibers and thus ensuring that thermal bridges are not created between the plant fibers and do not degrade the thermal insulation properties.
[0013] This reduction is possible through improved homogenization of the mixture of plant fibers and thermal bonding fibers. Indeed, thermal bonding fibers with a low decitex value are finer, for the same fiber length, than thermal bonding fibers with a higher decitex value. As a result, the thermal bonding fibers blended with the plant fibers are better able to interlock with neighboring plant fibers and thus distribute themselves more evenly throughout the volume of the plant fiber mat. For the same thermal performance, it is therefore possible to reduce the percentage of thermal bonding fibers required and to increase the proportion of bio-based components in the finished product.
[0014] The inventors were thus able to determine through appropriate tests that the mixture of plant fibers based on cereal crops and thermally bonding fibers with a lower decitex value than usual, and in particular less than or equal to 1.9, makes it possible to produce a mattress with a high bio-based content, particularly suitable for building insulation, and especially for interior insulation of such buildings. In particular, the plant fiber mattress according to the invention has a thermal conductivity of less than 40 mW / m / K at 20°C.
[0015] According to a feature of the invention, the thermal bonding fibers have a decitex less than or equal to 1.7 dtex.
[0016] According to one feature of the invention, the thermal bonding fibers have a decitex less than or equal to 1.5 dtex. Above this value, the processes to be implemented to obtain such fine thermal bonding fibers are complex, but the inventors have noted that the thermal conductivity of an insulating material using such fine thermal bonding fibers is reduced and can tend towards thermal conductivity values of the order of 36 to 38 mW / m / K at 20°C.
[0017] According to a feature of the invention, the straw fiber mattress comprises at most 15% thermal bonding fibers.
[0018] According to one feature of the invention, the straw fiber mattress comprises between 2% and 8% thermal bonding fibers. It is understood here that the percentage in question is a mass percentage relative to the mass of the straw fiber mattress in question.
[0019] According to one feature of the invention, the plant fibers have a cellulose content of between 30 and 50 kg. 100 kg 1 of dry matter and a lignin content of between 4.5 and 25 kg. 100 kg 1 of dry matter.
[0020] The lignin and cellulose content of these plant fibers is measured on a dry matter basis. The dry matter considered here is obtained by drying the cereal plants from which the plant fibers are obtained in a ventilated oven. In this ventilated oven, the cereal plants are heated to approximately 105°C until a constant mass is reached. This constant mass is commonly referred to as the reference mass, and the cellulose, lignin, and other component levels are expressed on a basis of this reference mass. It should be noted that the oven referred to here is separate from the oven used to heat the mixture of thermally bonding fibers and plant fibers within the mattress.
[0021] The inventors have determined through appropriate tests that plant fibers with the lignin and cellulose contents mentioned are particularly suitable for use in plant fiber mats for insulation products. The plant fiber mat according to the invention can be obtained from various cereal crops such as, for example, oats, wheat, rye, barley, or rice.
[0022] According to one feature of the invention, the plant fibers have a cellulose content of between 30.9 and 42.3 kg / 100 kg dry matter and a lignin content of between 12.2 and 21.6 kg / 100 kg dry matter. The inventors have demonstrated that plant fibers, particularly those derived from wheat, barley, corn, or oat straw, exhibit more suitable structural characteristics for producing a plant fiber mattress according to the invention with low thermal conductivity. More specifically, these plant fibers have lignin contents that offer a good compromise between very woody and very short wood fibers and rice straw fibers, as previously mentioned, which have suboptimal insulation characteristics and are less readily available than wheat, barley, corn, or oats.
[0023] These parameters are obtained, in particular, from plant fibers derived from wheat straw, which is available in large quantities throughout the country, thus ensuring local production with factories located as close as possible to the raw material harvesting areas. It should be noted that the plant fiber mattress can be made from a mixture of plant fibers from two distinct plant species, starting from when the latter have characteristics in terms of lignin content and cellulose content in accordance with the invention.
[0024] According to one feature of the invention, at least 60% of the plant fibers have a diameter less than or equal to 300pm.
[0025] According to one feature of the invention, at least 75% of the plant fibers have a diameter of less than 300pm.
[0026] According to one feature of the invention, at least 55% of the plant fibers have a diameter of less than 200 µm.
[0027] According to one feature of the invention, at least 50% of the plant fibers have a diameter between 100pm and 300pm.
[0028] The inventors have observed that the thermal conductivity value of a cereal-based plant fiber mat, such as the one described in the present invention, is lower, and therefore more advantageous for building insulation applications, when the particle size of the plant fibers in the mat conforms to certain values. In particular, to achieve the desired thermal conductivity values, at least below 0.040 W / m / K, at least 60% of the plant fibers must have a diameter of 300 microns or less. The large quantity of fine plant fibers resulting from this particle size distribution ensures good thermal conductivity of the finished product, notably due to the average fineness of the plant fiber and the homogeneity of fineness between the plant fibers and the thermal bonding fibers.
[0029] Having homogeneity between the fineness of the thermal bonding fibers, i.e. thermal bonding fibers with a low decitex, and the fineness of the plant fibers allows for good mixing of all the fibers, it being understood that a non-homogeneous distribution favors local clusters of thermal bonding fibers which implies an absence of these thermal bonding fibers in other areas of the mattress and therefore of plant fibers likely to be in contact with each other and to create a thermal bridge which is bad for the thermal conductivity value of the finished product.
[0030] It should be noted that the diameter characteristic of plant fibers is particularly considered, but that it is possible that these characteristics may be combined with other characteristics relating to the dimension of plant fibers, such as their length.
[0031] According to one feature of the invention, at least 60% of the plant fibers have a length less than or equal to 5mm.
[0032] According to one feature of the invention, at least 40% of the plant fibers have a length of less than 2mm.
[0033] According to a feature of the invention, the vegetable fiber mattress has a thickness greater than 20 mm.
[0034] According to one feature of the invention, the vegetable fiber mattress has a thickness of at least 40 mm.
[0035] The thickness of the vegetable fibre mattress to be considered here is the nominal thickness of the mattress, that is to say the thickness which can be observed by the user when using the product for the purpose of insulating a building in particular.
[0036] In accordance with practices known in the prior art, the vegetable fiber mat according to the invention is obtained by passing a vegetable fiber mat, previously formed, where appropriate on a conveyor device directing the vegetable fiber mat towards the oven, by a mixture of vegetable fibers entangled with each other, and binding elements intended to bind the vegetable fibers together during the passage through the oven, into an oven configured at a determined cooking temperature.
[0037] The nominal thickness can notably be measured after packaging, for example when purchasing the product. By way of example, the nominal thickness as mentioned above is observed after various successive stages of the industrial manufacturing process during the implementation of the product, these stages may include, after drying the straw fiber mat in an oven, cutting, for example, into panels of appropriate dimensions, subsequent compression of the straw fiber mat obtained after drying during packaging, packaging and storage before marketing.
[0038] According to a feature of the invention, the plant fiber mattress has a volumetric density between 20kg.m3 and 80kg.m3.
[0039] According to a feature of the invention, the thermal bonding fibers have a length of 6 mm.
[0040] According to one feature of the invention, the thermal bonding fibers comprise at least polyethylene.
[0041] According to one feature of the invention, the plant fiber mat has a thermal conductivity of less than or equal to 40 mW / m / K at 20°C. More particularly, the plant fiber mat can have a thermal conductivity of less than or equal to 37 mW / m / K at 20°C. Thus, assembled into panels intended to provide insulation, particularly in construction, straw has a thermal conductivity that makes it a suitable building material for insulation.
[0042] Other features, details and advantages of the invention will become clearer upon reading the following description on the one hand, and the illustrative and non-limiting examples of embodiments given with reference to the accompanying schematic drawings on the other hand, in which:
[0043] [Fig. 1] schematically represents a general view of a fibre mattress plant-based products conforming to the present invention;
[0044] [Fig.2] represents a table illustrating a distribution of plant fibers in the plant fiber mattress according to their lengths for wheat straw;
[0045] [Fig.3] represents a table illustrating the distribution of plant fibers in the plant fiber mattress according to their lengths for rice straw;
[0046] [Fig.4] represents a table illustrating the distribution of plant fibers in the plant fiber mattress according to their diameters for wheat straw;
[0047] [Fig.5] represents a table illustrating the distribution of plant fibers in the plant fiber mattress according to their diameters for rice straw;
[0048] [Fig.6] represents a local view of the plant fibers and thermally bonding fibers present within the plant fiber mat represented by [Fig.1].
[0049] It should first be noted that while the figures illustrate the invention in detail for its implementation, these figures can of course also serve to further define the invention, if necessary. It should also be noted that these figures only show examples of embodiments of the invention.
[0050] The features, variants, and different embodiments of the invention can be combined in various ways, provided they are not incompatible or mutually exclusive. In particular, variants of the invention may be conceived comprising only a selection of features, described hereafter in isolation from the other described features, if this selection of features is sufficient to confer a technical advantage or to differentiate the invention from the prior art.
[0051] In the figures, the elements common to several figures retain the same reference.
[0052] Figure 1 shows a plant fiber mattress 1 according to the present invention. The plant fiber mattress 1 is formed of a plurality of plant fibers 2 intertwined with each other. In the embodiment shown, these plant fibers 2 are straw fibers, and more specifically wheat straw fibers.
[0053] The plant fibers 2 used to manufacture the plant fiber mattress 1 are obtained after processing cereal crop residues in a defibration unit. More specifically, these residues represent the stalks and / or leaves of these cereal crops, also known as cereal grains, after harvest. These cereal grains can be wheat, barley, oats, maize, sorghum, rice, or rye. In the embodiment shown, the plant fibers 2 are derived, as mentioned above, from wheat straw. Wheat straw has the particular advantage of being available in large quantities.
[0054] Furthermore, this wheat straw, like other plants of interest such as barley or maize, has a cellulose content of between 30 and 50 kg per 100 kg of dry matter, commonly written as "kg 100 kg DM", and a lignin content of between 4.5 and 25 kg 100 kg DM. The inventors were able, through appropriate tests, to determine that the plant fibers from these plants of interest have a structure that allows for the production of plant fiber mats with optimal insulating properties.
[0055] More specifically, the inventors were able to determine that cereal plants with structural characteristics similar to wheat straw were ideal for providing plant fibers 2 suitable for forming a plant fiber mat 1 with optimal insulating properties. These cereal plants had a cellulose content of between 30.9 and 42.3 kg / 100 kg 1 of dry matter and a lignin content of between 12.2 and 21.6 kg / 100 kg 1 of dry matter.
[0056] The fiber-making unit is a device for forming plant fibers 2 from wheat straw residues. These wheat straw residues may be in the form of rectangular or round bales or stored in bulk. Furthermore, as illustrated in Figures 2 and 4, the fiber-making unit is advantageously configured to obtain wheat straw fibers with a median diameter of approximately 180 µm and a median length of 3500 µm.
[0057] Figures 2 to 5 highlight structural differences that the inventors have observed in the case of a rice straw fiber mattress (Figures 3 and 5) and a plant fiber mattress 1 according to the invention, here made with wheat straw fibers (Figures 2 and 4).
[0058] Figures 2 and 4 illustrate the distribution of wheat straw fibers within a plant fiber mat 1 according to the invention, for a sample of given dimensions, and for which it has been demonstrated that it provides a thermal conductivity of less than 40 mW / m / K. Figures 3 and 5 illustrate the equivalent distribution of rice straw fibers within a sample of fiber mats of equivalent dimensions, and for which it has been demonstrated that it can only offer, at best, a thermal conductivity of 40 mW / m / K.
[0059] More specifically, [Fig.2] illustrates the cumulative distribution DC of the fibers as a function of their length LF.
[0060] Each cumulative distribution value DC illustrates the percentage of fibers within a given sample that have a length less than a given dimension. For example, [Fig. 2] illustrates, in the first cell C1, that 10% of the fibers present in a given sample of a fiber mattress according to the invention have a length LF less than or equal to 700 µm. And in the second cell C2, it can be seen that 18% of the fibers present in this same given sample of a mattress of fiber according to the invention have a length LF less than or equal to 1000pm. It can be deduced from these two values that 8% of the fibers present in this sample have a length LF between 700pm and 1000pm, the 10% of fibers whose length LF is less than or equal to 700pm being part of the 18% of fibers whose length LF is less than or equal to 1000pm.
[0061] Thus, the tests that the inventors were able to carry out on this sample show, by studying the values of the cumulative distribution DC, that at least 40% of the fibers forming a mat of plant fibers 1 according to the invention have a length of at most 2000 pm. Moreover, it should be noted that, as can be seen in [Fig. 2], 73% of the fibers have a length LF of at most 5000 pm.
[0062] By carrying out tests on other types of straws having lignite and cellulose contents in accordance with what has been mentioned previously, and in particular on barley straws, the inventors were able to find that a straw fiber mattress according to the invention can comprise at least 60% of fibers whose length is less than or equal to 5000pm.
[0063] Figure 2 also allows us to highlight ranges of values of di fiber dimensions, here their length, most represented within the plant fiber mattress 1. More specifically, the increase in the cumulative distribution DC between a first given LF fiber length, for example <2000pm, a second given LF fiber length, for example <5000pm, and a third given LF fiber length, for example <7000pm, highlights the fact that there are more wheat straw fibers with a length between 2000pm and 5000pm, knowing that they represent about 33% of the total mass of plant fibers present in the mattress, than wheat straw fibers with a length between 5000pm and 7000pm, knowing that they represent about 10% of the total mass of plant fibers present in the mattress.
[0064] Figure 3 illustrates a table similar to that shown in Figure 2 and, by comparing the values in these two tables, demonstrates that the rice straw fibers have a greater average length than the wheat straw fibers present in the fiber mat. Indeed, 40% of the rice straw fibers in a given sample have a length (LF) less than or equal to 5000 µm, whereas 60% of the wheat straw fibers in an equivalent sample have the same length. The thermal conductivity of the rice straw fiber mat, the analysis of which yielded the table in Figure 3, is higher than that of the wheat straw fiber mat, the analysis of which yielded the table in Figure 2.
[0065] It follows from the cross-analysis of the two tables just mentioned that the length of the LF fibers has an impact on thermal conductivity, in particular because that fibers that are too long can more easily come into contact with neighboring fibers and create a thermal bridge.
[0066] Figures 4 and 5 show the same tests as those highlighted in Figures 2 and 3, this time taking into account the diameter of the DF fibers.
[0067] Each cumulative distribution value DC illustrates the percentage of fibers, within a given sample, that have a diameter less than a given dimension. The values shown in [Fig. 4] successively illustrate that 5% of the fibers present in a given sample of a fiber mat according to the invention have a diameter DF less than or equal to 70 pm, that 18% of the fibers present in this sample have a diameter DF less than or equal to 100 pm, that 38% of the fibers present in a given sample of a fiber mat according to the invention have a diameter DF less than or equal to 150 pm, that 55% of the fibers present in this sample have a diameter DF less than or equal to 200 pm, and that 75% of the fibers present in this sample have a diameter DF less than or equal to 300 pm.
[0068] Thus, the tests that could be carried out by the inventors on this sample show, by studying the values of the cumulative distribution DC, that at least 75% of the plant fibers 2 from wheat straw have a diameter less than or equal to 300pm and at least 55% of the fibers have a diameter DF less than or equal to 200pm.
[0069] Here again, it should be noted that by carrying out tests on other types of straws with lignite and cellulose contents in accordance with what has been mentioned previously, and in particular on barley straws, the inventors were able to find that a straw fiber mattress according to the invention can comprise at least 60% of fibers whose diameter DF is less than or equal to 300pm and at least 50% of fibers whose diameter DF is between 100pm and 300pm.
[0070] Figure 5, as previously mentioned, shows the particle size distribution of a plant fiber mat containing rice straw fibers, with a thermal conductivity greater than 40 mW / m / K. As can be seen in Figure 5, only 52% of the fibers have a diameter DF less than or equal to 300 µm. In other words, nearly half of the fibers have a diameter DF greater than 300 µm.
[0071] Here again, it follows from the cross-analysis of the two tables just mentioned that the diameter of the DF fibers has an impact on thermal conductivity, in particular because plant fibers that are too thick can prevent the presence of thermally bonding fibers between them and because they can thus more easily come into contact with neighboring plant fibers and create a thermal bridge.
[0072] As mentioned previously, the straw fiber mattress 1 is formed from an intertwining of plant fibers 2. These plant fibers 2 are, as can be seen in [Fig. 2], bonded together by means of dry-bonding binding elements. These binding elements are more particularly formed by thermally bonding fibers 3.
[0073] The straw fiber mattress 1 is obtained by means of a manufacturing installation in which the plant fibers 2 are mixed with the thermal bonding fibers 3 so as to obtain a thermal bonding fiber content which is less than 15%, preferably between 2% and 8%, more preferably between 2% and 5%.
[0074] In one embodiment of the invention, the mixture of plant fibers 2 and thermally bonding fibers 3, obtained according to the proportions just mentioned, is blown into a manufacturing installation and then drawn against a conveyor to form a straw fiber mat. This straw fiber mat is then heated in an oven to form the straw fiber mattress 1. The straw fiber mattress can be cut into insulating panels of various sizes or rolled and compressed for storage.
[0075] The thermally bonding fibers 3 are formed of a core 31 and a sheath 32. The core 31 forms a rigid part of the thermally bonding fibers 3, contributing to the mechanical strength of the straw fiber mat 1, while the sheath 32 ensures the bonding of the plant fibers 2 to one another. To this end, the core 31 and the sheath 32 have different melting points, and more specifically, the sheath 32 has a lower melting point than the core 31.
[0076] Thus, when the straw fiber mat is placed in an oven to obtain a straw fiber mattress according to the invention, the temperature inside the oven is such that the sheath 32 melts, immersing the adjacent plant fibers 2. The entire assembly solidifies upon cooling after exiting the oven, thereby bonding the straw fibers together. It should be noted that the melting temperature of the core 31 is designed so that, despite the passage through the oven of a straw fiber mat made of a mixture of straw fibers and binders, the core 31 retains its rigidity, contributing to the mechanical strength of the straw fiber mattress 1 after oven drying.
[0077] It is understood that within the oven, the plant fibers 2 and the heat-bonding fibers 3 are heated so that the plant fibers 2 bond together. At least the oven treatment, and where applicable subsequent compression and cutting before packaging, transforms the straw fiber mat into a straw fiber mattress according to the invention.
[0078] The straw fiber mattress has a thickness of at least 20 mm and preferably greater than 40 mm. This thickness is considered after the straw fiber mattress 1 has passed through the oven.
[0079] In the embodiment shown, the sheath 32 of the heat-bonding fibers 3 is made of polyethylene and the core 31 is also made of polyethylene. It should be noted that in an alternative embodiment, the core 31 of the heat-bonding fibers can be made of polyester, and more specifically of polyethylene terephthalate. Polyethylene has the advantage of bonding easily to plant fibers, which in makes a good candidate for forming the sheath 32 of the thermal bonding fibers.
[0080] It should be noted that this is only one example of an embodiment, the straw fiber mattress 1 being able to be obtained by a different manufacturing installation, for example a manufacturing installation in which the lignocellulosic fibers 2 and the binding elements 3 are mechanically deposited on a conveyor and then directed to an oven so as to form the straw fiber mattress 1. However, the content of the straw fiber mattress 1 in thermal bonding fibers 3 and the structure of said thermal bonding fibers 3 remain identical.
[0081] Thermal bonding fibers are characterized in particular by their fineness. This fineness is expressed in decitex, commonly defined as the mass in grams of ten thousand meters of this thermal bonding fiber 3. According to the invention, the thermal bonding fibers 3 have a fineness less than or equal to 1.9 dtex, preferably less than or equal to 1.7 dtex, and more preferably less than or equal to 1.5 dtex. Such a fineness of the thermal bonding fibers 3 allows for better distribution of these thermal bonding fibers within the mattress, between the plant fibers, which is more effective for gluing and fixing the position of the plant fibers relative to each other. It is understood that this makes it easier to ensure that the plant fibers do not come into contact and do not form thermal bridges.The improved distribution of thermal bonding fibers, resulting from the fineness of these fibers as highlighted by the invention, makes it possible to limit the mass or volume ratio of thermal bonding elements in the mass or overall volume of the insulating product formed by the mat of plant fibers.
[0082] In addition, the thermal bonding fibers 3 have a length, taking into account manufacturing tolerances, of approximately 6 mm, which can allow, in addition to the previously mentioned fineness, a better distribution of the thermal bonding fibers within the straw fiber mattress 1.
[0083] The fineness of the thermal bonding fibers is particularly interesting here as it is complementary to the fineness of the plant fibers, suggested by the fact that at least 60% of the plant fibers have a diameter of less than 300 microns, which allows a good mix of the two types of fibers present in the mat and a homogeneous distribution of the thermal bonding fibers between the plant fibers, which allows good fixation of the plant fibers and the regular formation of air pockets allowing the thermal conductivity value to be lowered to the values desired for application to building insulation.
[0084] The various elements presented for contributing to the formation of the straw fiber mattress 1 make it possible to obtain such a mattress with a volumetric density between 20 kg.m3 and 80 kg.m3 and, as mentioned previously, a thickness of at least 20 mm. Such a straw fiber mattress exhibits thermal conductivity less than 40 mW / m / K at 20°C, and in particular less than or equal to 37 mW / m / K at 20°C, allowing optimal insulation properties to be provided to a building material.
[0085] The invention as just described achieves the goal it set for itself by proposing a straw fiber mattress whose thermal insulation performance is optimized by means of a composition and a distribution of dimensions of the straw fibers particular within the straw fiber mattress.
Claims
Claims
1. Mattress of plant fibers characterized in that it comprises plant fibers (2) based on cereal plants joined together by means of thermobinding fibers (3), the thermobinding fibers (3) having a decitex less than or equal to 1.9 dtex, the plant fibers (2) having a cellulose content of between 30 and 50 kg. 100 kg 1 of dry matter and a lignin content of between 4.5 and 25 kg. 100 kg 1 of dry matter.
2. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that the thermobonding fibers (3) have a decitex less than or equal to 1.7 dtex.
3. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that the thermobonding fibers (3) have a decitex less than or equal to 1.5 dtex.
4. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that it comprises at most 15% of thermobonding fibers (3).
5. Mattress of plant fibers (1) according to the preceding claim, characterized in that it comprises between 2% and 8% of thermobinding fibers (3).
6. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that the plant fibers (2) have a cellulose content of between 30.9 and 42.3 kg. 100 kg 1 of dry matter and a lignin content of between 12.2 and 21.6 kg. 100 kg 1 of dry matter.
7. Mattress of plant fibers according to any one of the preceding claims, characterized in that at least 60% of the plant fibers have a diameter less than or equal to 300 pm.
8. Mattress of plant fibers (1) according to the preceding claim, characterized in that at least 75% of the plant fibers (2) have a diameter of less than 300 pm.
9. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that at least 55% of the plant fibers (2) have a diameter of less than 200 pm.
10. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that at least 50% of the plant fibers (2) have a diameter of between 100 pm and 300 pm.
11. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that at least 60% of the plant fibers have a length less than or equal to 5mm.
12. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that at least 40% of the plant fibers (2) have a length of less than 2 mm.
13. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that it has a thickness greater than 20 mm.
14. Mattress of plant fibers (1) according to the preceding claim, characterized in that it has a thickness of at least 40 mm.
15. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that it has a volume density of between 20kg.m3 and 80kg.m3.
16. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that the thermobonding fibers (3) have a length of 6 mm.
17. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that the thermobonding fibers (3) comprise at least polyethylene.
18. Mattress of plant fibers (1) according to any one of the preceding claims, characterized in that it has a thermal conductivity less than or equal to 40 mW / m / K at 20°C.