METHOD FOR MANUFACTURED A PART AND THE PART THUS MANUFACTURED

The method addresses the challenge of adapting aeronautical parts to varying constraints by treating adjacent zones with distinct composite structures and assembling a metal part, ensuring efficient and cost-effective production with high-quality surfaces.

FR3147726A1Pending Publication Date: 2024-10-18SAFRAN AIRCRAFT ENGINES SAS
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
FR2023003835
Authority / Receiving Office
FR · FR
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-17
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

Aeronautical parts, particularly rotor blades, face challenges in adapting to varying spatial and temporal constraints and temperatures due to the complexity and high cost of assembling multiple parts with different composite materials, and the use of metal for blade roots can result in rough surfaces.

Method used

A method for manufacturing a part with a preform comprising reinforcing fibers, where adjacent zones are treated separately with distinct composite structures using a metallic composite matrix and a metal part is assembled, ensuring continuity and quality surface finish.

Benefits of technology

The method allows for efficient production of composite parts with distinct zones meeting varying constraints, providing a high-quality surface finish and reducing manufacturing costs by using conventional processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The invention relates to a method for manufacturing a part (26) from a preform comprising reinforcing fibers and two adjacent zones connected by reinforcing fibers, comprising the realization of a distinct composite structure for each zone, by making a first metallic structure (10a') of a first zone, then a second structure (10b') of a second zone, each distinct composite structure being made by introducing a composite matrix into a zone of the preform and applying to this zone operating conditions, in particular of temperature, specific to the realization of the structure from the fibers of the zone and the matrix introduced, the different zones of the preform being treated in an order corresponding to the decreasing order of temperatures used in the operating conditions applied to the realization of the distinct composite structures.The process includes assembling a metal part (24) with the first zone. Figure for the abstract: Fig. 3.
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: METHOD FOR MANUFACTURING A PART AND PART THUS MANUFACTURED Technical field

[0001] The present disclosure relates to a method of manufacturing a part and a part thus manufactured.

[0002] The invention applies in particular to aeronautical and space parts, in particular in turbomachines, in particular aeronautical. Prior art

[0003] In aeronautics, the parts which are used, for example in turbojets and, in particular, rotor blades, are subject to severe operational constraints.

[0004] More and more aeronautical parts are made from composite materials due to the very good weight / stiffness compromise that these materials can achieve.

[0005] The choice of a composite material is generally made according to the expected operating temperatures. For an aeronautical part, the choice may, for example, relate to the use of an Organic Matrix Composite (OMC), a Metal Matrix Composite (MMC) or a Ceramic Matrix Composite (CMC).

[0006] However, a problem may arise when the part must be adapted to a stress or temperature field which is likely to vary spatially and / or temporally, significantly, during use of the part.

[0007] To take into account such an adaptation, the part can be made in several parts which are each adapted to a specific stress / temperature field and which are then assembled to obtain the final part. However, the operation of assembling the different parts can prove to be critical, or even very complex to implement and of a relatively high economic cost.

[0008] Furthermore, when the parts to be manufactured are rotor blades, metal is generally used to make the blade root taking into account the stresses to which the root is subjected when the blade is used.

[0009] The use of a Metal Matrix Composite (MMC) which is obtained by molding, can generate at the level of the blade root a rough surface state and therefore of insufficient quality if one wishes in particular to arrange around the root bearings used for adjusting the pitch of the blade.

[0010] In view of the above, it would therefore be useful to be able to produce a part in a simple manner which makes it possible to take into account the requirements formulated above. Statement of the invention

[0011] The invention thus relates to a method for manufacturing a part from a preform comprising reinforcing fibers and which comprises several zones, the preform comprising at least two adjacent zones which are such that at least certain reinforcing fibers of the preform have a length which extends in said at least two adjacent zones so as to ensure continuity of the reinforcing fibers from one zone to the other, the method comprising the production of a separate composite structure for each of said at least two adjacent zones of the preform, by firstly producing a first metallic composite structure of a first of these zones, then a second composite structure of a second zone adjacent to this first zone, and so on for each possible additional adjacent zone, the first composite structure being produced, on the one hand, by introducing a metallic composite matrix into the first zone and, on the other hand,by applying to this zone operating conditions, in particular temperature, suitable for producing the composite structure from the reinforcing fibers of the zone and the composite matrix introduced, the different zones of said at least two adjacent zones of the preform being treated in an order which corresponds to the decreasing order of temperatures used in the operating conditions applied to the production of the separate composite structures, characterized in that the method also comprises the assembly of a metal part with the first zone of the preform.

[0012] This method makes it possible to manufacture parts in a particularly simple and efficient manner. The method described above makes it possible to treat separately (spatially and temporally) adjacent or contiguous zones (two by two) of the same preform insofar as these adjacent zones have in common reinforcing fibers of the preform which physically extend in each of these zones and connect one zone to the other. These reinforcing fibers thus ensure spatial / geometric continuity between the treated zones within which they extend, in such a way that the preform is formed in a single piece and not in several parts. Each of these zones can thus undergo its own (specific) treatment in order to produce a specific composite material structure, distinct from one zone to another.Specific treatment is a treatment or treatment method (type of composite matrix used, operating conditions, in particular temperature, pressure, specific to the production of a given composite) which aims to produce a composite structure in an area called the application area, while the area adjacent to this application area, in the sense defined previously (i.e. the area which is spatially linked to the application area by means of reinforcing fibres) is not treated during this time (it may have already been treated or will be treated afterwards). The area. adjacent is for example protected or isolated from the application zone (zone being treated). This process thus makes it possible to produce a part in composite material which has distinct composite structures corresponding to distinct zones or geometric portions of the part meeting constraints of use, environment or interface varying from one zone to another (these different constraints prevent the part from being produced in a single composite material which could not in fact simultaneously meet such specifications).

[0013] More particularly, the first zone of the preform is made with a metallic composite structure and a metallic part is assembled with this first zone, either after the production of the composite structure in this first zone or during this. The added metallic part has the advantage of offering a surface finish which does not depend on the production of the composite part and the manufacturing particularities linked thereto. Thus, the metallic part can have a high-quality surface finish (with minimal and controlled roughness), making it possible, for example, to accommodate external bearings, as is required for variable-pitch blade roots. The metal itself can also be of better quality than a metal which is, for example, obtained by casting.The manufacturing processes used to produce such an added metal part can be conventional and therefore of a relatively reasonable economic cost in view of the production of a composite part.

[0014] According to other possible characteristics: -the metal part is a part of revolution; - the assembly is carried out as desired: by insertion of the metal part during low pressure or gravity casting of the metal composite structure; by welding; by mechanical assembly, preferably using at least one added assembly member;

[0015] -the metal part is inserted at the bottom of a mold, the preform is introduced into the mold above the metal part and a metal composite matrix is ​​introduced into the mold in order to carry out the low pressure or gravity molding of the metal composite structure and the joining of the latter with the metal part;

[0016] -the preform comprises two distinct adjacent zones, the matrix introduced into the second zone being different from that of the first zone and chosen from an organic matrix and a ceramic matrix; -reinforcing fibers include carbon fibers, silicon carbide fibers, glass fibers, boron fibers, alumina fibers; -the preform is formed from a single piece.

[0017] The invention also relates to a part made of composite material which comprises several distinct composite structures produced by the method briefly described above and which are intimately linked to each other by the common reinforcing fibers.

[0018] According to other possible characteristics:

[0019] -the separate composite structures are each intended to be subjected to a field of mechanical and / or temperature stresses which is distinct from one zone to another;

[0020] -the composite material part is a turbomachine rotor blade (fan blade);

[0021] -the rotor blade comprises, on the one hand, a blade root comprising a first part formed from a composite structure made from a metal matrix (CMM) and a second part formed from the metal part assembled with the first zone of the preform and, on the other hand, a blade forming a composite structure made from an organic matrix (CMO);

[0022] -the part is a turboprop propeller.

[0023] The invention also relates to a turbomachine rotor (fan) comprising a plurality of parts (rotor blades) as briefly set out above.

[0024] The invention also relates to a turbomachine comprising a turbomachine rotor as briefly described above. Brief description of the drawings

[0025] Other characteristics and advantages of the subject of the present disclosure will emerge from the following description of embodiments, given as non-limiting examples, with reference to the appended figures.

[0026] [Fig.lA] [Fig.lA] is a schematic representation of a first step of producing a fan blade preform according to an embodiment of a method according to the invention;

[0027] [Fig. 1B] [Fig. 1B] illustrates a subsequent step of placing the preform of [Fig. 1A] in a mold according to the embodiment of the method;

[0028] [Fig.lC] [Fig.lC] illustrates a next step of the embodiment of the method during which a metallic composite matrix is ​​introduced into the mold of [Fig.lB];

[0029] [Fig.lD] [Fig.lD] illustrates a step of producing a first metallic composite structure according to the embodiment of the method;

[0030] [Fig.lE] [Fig.lE] illustrates a subsequent step of the embodiment of the method during which the composite structure undergoes a mechanical finishing treatment after demolding;

[0031] [Fig.lF] [Fig.lF] illustrates a subsequent step of placing the partially processed preform of [Fig.lE] into a mold according to the embodiment of the method;

[0032] [Fig.lG] [Fig.lG] is a schematic view illustrating the introduction of an organic composite matrix into the mold of [Fig.lF];

[0033] [Fig. 1H] [Fig. 1H] illustrates the production of the second composite structure organic according to the method of carrying out the process in order to obtain a composite part;

[0034] [Fig.2A] [Fig.2A] illustrates a step of assembling a metal part to the composite part of [Fig.1H];

[0035] [Fig.2B] [Fig.2B] illustrates an example of a possible embodiment for the assembly step of [Fig.2A];

[0036] [Fig.3] [Fig.3] is a schematic representation of a fan blade obtained after assembly of the metal part of [Fig.2A];

[0037] [Fig.4A] [Fig.4A] illustrates a following step of inserting a metal part into the bottom of a mold according to an alternative embodiment of the method;

[0038] [Fig.4B] [Fig.4B] illustrates a subsequent step of placing the preform of [Fig.1A] in the mold of [Fig.4A];

[0039] [Fig.4C] [Fig.4C] illustrates a next step in which a metal composite matrix is ​​introduced into the mold of [Fig.4B];

[0040] [Fig.4D] [Fig.4D] illustrates a step in producing a first metallic composite structure secured to the metallic part inserted in [Fig.4A];

[0041] [Fig.4E] [Fig.4E] illustrates a subsequent step during which the entire composite structure and the metal part undergo a mechanical finishing treatment after demolding;

[0042] [Fig.5] [Fig.5] is a schematic representation of a turbomachine incorporating a blower whose blades have been manufactured according to the embodiment of the process whose steps are illustrated in the preceding figures;

[0043] [Fig.6] [Fig.6] illustrates one of the blades of [Fig.5]. Detailed description

[0044] The following detailed description relates to an embodiment of a method for manufacturing a fan blade, partly made of composite material, of a turbomachine for an aircraft.

[0045] However, the manufacturing method according to the invention applies to the manufacturing of other parts for aeronautics and space for which distinct zones of the same part must meet functional specifications that differ from one zone to another when the part is put into operation.

[0046] Figures 1A-H illustrate different possible steps of the manufacturing process. of a blade partially made of the above-mentioned composite material. It will be noted that the following description also applies to the manufacture of any other part having at least two parts or areas to be transformed into composite areas independently of each other, using either the same composite dies or one or more other composite dies.

[0047] [Fig. 1A] illustrates very schematically the manufacture of a preform 10 of a fan blade (it could generally be a rotor blade). This preform is composed of long reinforcing fibers, for example carbon fibers, which form a mesh or structure of intertwined fibers in two dimensions or three dimensions. The production of such a preform or blank in reinforcing fibers is widely known to those skilled in the art. For example, the preform can be produced in a known manner by 3D weaving.

[0048] In [Fig.lA], the reinforcing fibers are represented in the form of an interweaving of first fibers which extend in a first direction f1 (long fibers) and second fibers which extend in a second direction f2, here perpendicular to the first direction.

[0049] In the present embodiment, the first fibers are called longitudinal fibers and are intended to extend along the longitudinal dimension or height of the blank (corresponding to the height of the blade), while the second fibers are called transverse fibers and are intended to extend along the transverse dimension or width of the blank (this dimension extends along the chord of the blade, i.e. between the leading edge and the trailing edge thereof).

[0050] The preform 10 comprises two adjacent or contiguous (spatially) parts or zones, namely a part or zone 10a, called lower, which forms a part of the root of the future blade and a part or zone 10b, called upper, which forms the upper part or blade of the future blade. Each of these parts is subjected to very different stresses when the blade is used on a fan rotor. In particular, the blade root may be subjected to higher thermal stresses than the upper part further from the rotor, to more restrictive assembly stresses than the upper part (for example due to machining, drilling, etc.) or to specific mechanical stresses (for example due to the existence of matting pressures). Furthermore, it is more particularly sought to achieve a weight saving on the upper part of the blade due to the high rotation speeds.The two parts 10a and 10b described above are geometrically arranged adjacent or contiguous to each other. In this regard, it will be noted that the same reinforcing fibers fl extend here continuously in the two distinct parts or zones 10a and 10b of the preform so that it is not possible to physically separate the two parts from each other without damaging one and / or the other of them. The presence . reinforcing fibers common to both zones give the preform thus formed sufficient mechanical strength so that the subsequent stages of manufacturing the composite structures on each of these zones can be carried out without affecting the preform, and in particular without damaging it.

[0051] Due to the environmental constraints specific to each of the parts or areas described above, each of them will be subjected to a different treatment method from one area to another in order to obtain a composite material structure that is different from one area to another. Each distinct composite structure will thus make it possible to meet locally different functional requirements.

[0052] The following steps illustrate very schematically, successively, the production of a first composite structure, on a first zone of the preform, here the lower zone 10a, using a first treatment method (here introduction of a first metal matrix in order to form a metal matrix composite structure) and the production of a second composite structure, on the second adjacent zone of the preform, here the upper zone 10b, using a second treatment method (here introduction of a second non-metal matrix, for example organic, in order to form here an organic matrix composite structure).

[0053] [Fig. 1B] illustrates the vertical positioning of the preform 10 in a mold 12 with the first zone 10a of the preform arranged in the lower part of the mold, that is to say close to the bottom thereof.

[0054] [Fig. 1C] illustrates a step of introducing a liquid metal (introduction of a metal matrix M) inside the mold 12 so that the metal is in contact with the first zone 10a of the preform located at the bottom of the mold and can impregnate all of the reinforcing fibers constituting this first zone. The internal part of the mold with which the first zone 10a of the preform is in contact is shaped so as to give the desired shape to this zone (here intended to form the root of the blade).

[0055] The metal can for example be poured by gravity inside the mold (for example from a container 14) or injected at low pressure (for example of the order of a few MPa) into the latter by a known means.

[0056] In the embodiment described, the metal is for example aluminum and the temperature applied is substantially equal to the melting temperature of the metal matrix, i.e. here approximately 660°C for aluminum. Other metals are of course conceivable depending on the functional constraints to which the first zone of the part must respond. For example, titanium can be used to form the metal matrix and the temperature applied is substantially equal to the melting temperature of the metal matrix, i.e. here approximately 1660°C for titanium.

[0057] During this step, the second zone 10b of the preform is preserved from any treatment and, in particular, is not treated by the method which is used only for the treatment of the first zone 10a.

[0058] [Fig.lD] schematically illustrates and groups together the steps of cooling, then hardening of the assembly formed by the reinforcing fibers and the metal matrix introduced into the first zone 10a of the preform in order to obtain a metal-based composite structure for this zone. The first zone thus treated is represented by the reference 10a'. The second zone 10b which is located in the upper part of the mold 12 is still not treated and only comprises, for the moment, the reinforcing fibers of the preform illustrated in [Fig.lA].The longitudinal reinforcing fibers fl of the preform which extend along their length straddling the two zones of the preform thus have, on the one hand, a first portion of their length located in the first zone 10a' which is now part of the first structure made of metallic composite material and, on the other hand, a second portion of their length located in the second zone 10b not yet treated. These second portions of longitudinal fibers are thus physically integral with the first zone via the first portions to which they are still linked.It will be noted that only a portion of the total reinforcing fibers fl of the preform may extend from one zone to the other, while the remaining portion of the reinforcing fibers of the preform may extend only in one or the other of these zones, to the extent that a significant fraction of the reinforcing fibers extends both in one zone and in the other zone and therefore makes it possible to ensure physical continuity between these zones.

[0059] [Fig. 1E] illustrates in a schematic and grouped manner the steps of demolding, then deburring or machining, for example on a support 16 of the first metallic composite structure 10a', for example in anticipation of the mechanical assembly of a part of revolution such as the part 24 shown in [Fig. 2B] which will be described later.

[0060] [Fig. 1F] schematically illustrates the positioning of the second zone 10b of the preform not yet treated inside a second mold or container 18, leaving the first metal composite structure 10a' outside this mold. A peripheral seal system 20 may be provided at the junction between the two zones 10a' and 10b in order to hermetically close the mold 18 on the second zone 10b, thus forming an autoclave inside which a desired temperature (non-ambient temperature) can be applied in a controlled manner for the production of the composite structure.

[0061] The internal part of the mold 18 with which the second zone 10b of the preform is in contact is shaped so as to give the desired shape to this zone.

[0062] A system 22 for injecting under pressure a second matrix, here a resin epoxy, is implemented in order to inject under pressure into the mold 18 a controlled quantity (volume) of resin via an orifice 18a from a reservoir and, for example, a pumping device. As an example, the known technique of resin transfer molding or RTM (known in English terminology as "Resin Transfer Molding") can be used. The temperature of the epoxy resin is of the order of 150°C and the pressure in the mold is substantially equal to 10 bars.

[0063] It will be noted that the temperature used during this step is lower than that used for the production of the first metallic composite structure. Indeed, the production of the composite structures in the reverse order to that described would not be possible because it would lead to degradation of the second non-metallic composite structure obtained.

[0064] The introduction of the resin inside the mold 18 makes it possible to impregnate or coat all of the reinforcing fibers not yet treated in the second zone 10b with this matrix.

[0065] Once the resin has been completely injected into the mold, the assembly formed by the reinforcing fibers and the resin introduced into the second zone 10b (organic matrix) is allowed to cool and then harden in order to obtain an organic-based composite structure for this zone. The second zone thus treated is represented by the reference 10b' in [Fig. 1H].

[0066] Steps of demolding, then deburring or machining of this second zone are then carried out in order to obtain the composite material part illustrated very schematically in [Fig. 1H] and which comprises the two adjacent composite structures thus manufactured 10a' and 10b'.

[0067] [Fig.2A] illustrates the composite part thus manufactured with zone 10b' represented with a blade blade shape and zone 10a' represented with a shape of the upper part of the blade root which is connected to the blade by the common long fibers (fibers fl in [Fig.1A]), where the same zones have been deliberately represented very schematically in the previous figures for the sake of simplification.

[0068] As illustrated in [Fig.2A], a metal part, here a part 24 having a shape of revolution, for example cylindrical, is approached to the first metal composite zone 10a' with a view to its assembly with the latter.

[0069] The part 24 is made of the same metal as that of the metal composite structure 10a' when the assembly of the structure 10a' and the part 24 is carried out by insertion, during low-pressure molding, or by welding. It may be, for example, a forged and machined billet, in particular the forged billet may undergo turning and grinding. The part 24 thus has a very good external surface condition. Typically, the part 24 may undergo turning and grinding operations allowing to obtain a roughness between 0.8 pm and 0.02 pm, where a roughness of a part obtained by molding is of the order of 3 to 6 pm. The manufacturing process of the metal part 24 described above is only one possible example among many conventional processes which are generally less expensive than composite manufacturing processes. The advantage obtained in the overall manufacturing process of the fan blade (or generally of any other part) lies in the fact that a part of the blade is made in a bi-composite (or even multi-composite) structure with the first zone in a metallic composite structure and that the other metallic part complementary to the first zone is made by another process in order to obtain an external surface condition of this other metallic part of very good quality, that is to say without uncontrolled excessive roughness, as would be the case if the blade were manufactured only in a bi-composite (or even multi-composite) structure.

[0070] The metal part 24 is thus brought closer to the first composite zone 10a', as indicated by the arrow, in order to be assembled with it. The assembly method can take several forms.

[0071] By way of example, the part 24 can be welded by one, denoted 24a, of its two opposite ends, to the free end 10a'1 of the first composite zone 10a'. Insofar as the part 24 is cylindrical, the welding step can be carried out by carrying out friction welding between the part 24 and the free end 10a'1 of the first composite zone 10a'.

[0072] According to another example illustrated in [Fig.2B], the metal part 24' is mechanically assembled to the first metal composite zone 10a”, preferably using one or more added assembly members.

[0073] In this example, the metal part 24' has been previously shaped at its end 24a' intended for assembly by reducing the diameter of the part from a peripheral zone forming a shoulder and which connects the portion of the part of non-reduced diameter to the end of reduced diameter 24a'. The first metal composite zone 10a”, for its part, has been hollowed out at its free end 10a” 1, in the central part thereof, so as to form a cavity of a shape complementary to that of the end of reduced diameter 24a' in order to be able to cooperate perfectly with it.

[0074] As shown in [Fig.2B], the end 24a' is inserted axially into the cavity of the free end 10a' ' 1 opposite it so as to completely match its shapes. An assembly member 26, such as a pin, is placed transversely relative to the insertion axis and passes through the wall of the free end 10a” 1 which externally borders the cavity and the reduced diameter end 24a' in order to secure the two parts together. Other types of mechanical assembly are of course conceivable by shaping the two parts to be assembled differently and by using one or more added assembly members.

[0075] [Fig. 3] represents the final part 26 (fan blade) after manufacture. The blade thus manufactured comprises, on the one hand, a blade root comprising a first part 10a' formed from a composite structure made from a metal matrix (CMM) and a second part 24 formed from the metal part assembled with the first zone 10a' of the preform and, on the other hand, a blade 10b' forming a composite structure made from an organic matrix (CMO).

[0076] According to an alternative embodiment, the assembly of the metal part 24 with the first zone 10a' of the preform can take place at another time in the overall manufacturing process of the composite part of the blade.

[0077] Thus, the assembly can be carried out by insertion during the low-pressure molding of the metal composite structure 10a, as described above in relation to FIGS. 1B and 1C. In this example, the metal part 24 can be used as an insert at the time of low-pressure casting in the mold 12.

[0078] For this purpose, figures 4A to 4E illustrate this variant embodiment which applies from the preform 10 shown in [Fig.1A] described above.

[0079] The metal part 24 described above is thus inserted into the bottom 30a of a mold 30 which is shaped in a suitable manner to receive it ([Fig.4A]) and comprises, for example, a bowl for receiving the part 24.

[0080] In the following step ([Fig.4B]), the preform 10 is placed in the mold 30, above the part 24. Here too, the bottom 30a has a shape adapted to house the preform 10 above the part 24, for example on the peripheral edges of the bowl.

[0081] In the next step ([Fig.4C]), the metal matrix M is introduced by low pressure casting or by gravity into the mold 30, as already described in relation to [Fig.1C], then the metal thus introduced is waited for to harden ([Fig.4D]).

[0082] At the end of this step, the preform obtained comprises in the lower part a first part forming a metallic composite structure 10a”' which has been secured to a second metallic part (part 24) by connection with the molten metal. The assembly of these two parts thus assembled forms the root of the blade in the final part. The preform is then removed from the mold (demolding; [Fig.4E]) and placed on a support 32 where it can be deburred, machined, retouched, etc., before carrying out the other steps IG and 1H already described above.

[0083] Everything described above applies generally, regardless of the processing method used to produce each composite structure, regardless of the part to be manufactured and the number of zones and, therefore, the number of composite structures to be manufactured.

[0084] It will be noted that the preform may comprise several types of fibers, possibly with several lengths and diameters. For example, the preform may comprise carbon fibers and glass fibers.

[0085] [Fig. 5] illustrates an exemplary embodiment of a turbomachine (turboreactor) 30 (here shown shrouded although it may be unshrouded) comprising a fan 32 which incorporates fan blades 34 manufactured according to the method described above. It will be noted that the blades manufactured by the method described above may be blades of a rotor of a turbomachine which is not necessarily a fan.

[0086] [Fig.6] illustrates an example of a fan blade 34 used in the fan 32 of [Fig.5].

[0087] According to another embodiment, the method can be used to manufacture a part made of composite material comprising three distinct zones with heterogeneous functionalities.

[0088] For example, such a part may be a turboprop propeller.

[0089] The preform of such a propeller comprises three distinct zones, namely a first zone corresponding to a part of the root of the propeller, a second zone corresponding to the leading edge of the propeller which is subjected to abrasive erosion and a third zone corresponding to the rest of the part which must be as light as possible. In such a preform a part of the reinforcing fibers of the first zone extends into the second zone adjacent to the first zone and another part of the reinforcing fibers of the first zone extends into the third zone adjacent to the first zone and to the second zone. Thus, the first and second zones are spatially connected to each other by a part of the reinforcing fibers and the first and third zones are spatially connected to each other by another part of the reinforcing fibers.

[0090] In this example, the reinforcing fibers of the preform are made of silicon carbide (SiC). The first area of ​​the root portion may be treated to produce a metal matrix composite structure, for example using an aluminum matrix. The second area of ​​the leading edge may be treated to produce a metal matrix composite structure, for example using a Ti-6Al-4V matrix. The third area may be treated to produce an organic matrix composite (OMC) structure, for example using an epoxy matrix.

[0091] In this embodiment, again, the order of treatment of the zones is carried out according to the decreasing order of the temperatures applied during the production of each composite structure in order to treat the first zone by the method requiring the highest temperature and proceeding in an identical manner for the following zones. Thus, the second zone of the titanium leading edge will be treated first (temperature of 1660°C), then the first zone of the aluminum root part (temperature of 660°C) and lastly the third zone for the rest of the blade in CMO (temperature of 150 / 200°C). The metal parts or zones are preferably treated by gravity by carrying out a casting operation of the metal matrices with the area of ​​interest located in the lower part. What has been described above with reference to Figures 1A-H and 4A-E can also be applied here, possibly with some adjustments within the reach of those skilled in the art.

[0092] The method can be used to manufacture a part with a greater number of heterogeneous areas to be treated than the numbers envisaged above.

[0093] It will be noted that everything described above in relation to figures 1A-H, 4A-E and 2A-B applies here to produce the other part of the propeller root in metal, separately from the manufacturing process of the rest of the propeller.

[0094] We thus obtain a turboprop propeller which comprises: - a propeller foot comprising a first part formed from a composite structure made from a metal matrix (CMM) and a second part formed from the metal part assembled with the first zone of the preform, - a leading edge (second zone) formed from a metal matrix composite structure, -the remaining part of the blade (third zone) formed from an organic matrix composite (OMC) structure.

[0095] Although the present description refers to specific exemplary embodiments, modifications may be made to these examples without departing from the general scope of the invention as defined by the claims. Furthermore, individual features of the various embodiments illustrated or mentioned may be combined in additional embodiments. Therefore, the description and drawings should be considered in an illustrative rather than restrictive sense.

Claims

Claims

1. A method of manufacturing a part (26) from a preform (10) comprising reinforcing fibers (f1, f2) and which comprises several zones, the preform comprising at least two adjacent zones (10a, 10b) which are such that at least some reinforcing fibers (f1) of the preform have a length which extends in said at least two adjacent zones so as to ensure continuity of the reinforcing fibers from one zone to the other, the method comprising the production of a separate composite structure for each of said at least two adjacent zones of the preform, by firstly producing a first metallic composite structure (10a') of a first (10a) of these zones, then a second composite structure (10b') of a second zone (10b) adjacent to this first zone, and so on for each possible additional adjacent zone, the first metallic composite structure (10a') being produced, on the one hand,by introducing a metallic composite matrix into the first zone (10a) and, on the other hand, by applying to this zone operating conditions, in particular temperature conditions, suitable for producing the composite structure from the reinforcing fibers of the zone and the composite matrix introduced, the different zones of said at least two adjacent zones of the preform being treated in an order which corresponds to the decreasing order of temperatures used in the operating conditions applied to producing the separate composite structures, characterized in that the method also comprises the assembly of a metallic part (24) with the first zone (10a) of the preform.,

2. Manufacturing method according to claim 1, characterized in that the metal part is a part of revolution.

3. Manufacturing method according to claim 1 or 2, characterized in that the assembly is carried out by choice: - by insertion of the metal part during low-pressure or gravity molding of the metal composite structure (10a'; 10a'”); - by welding; - by mechanical assembly, preferably using at least one added assembly member.

4. Manufacturing method according to claim 3, characterized in that the metal part (24) is inserted at the bottom of a mold (30), the preform (10) is introduced into the mold above the metal part (24) and a metal composite matrix is introduced into the mold in order to carry out the low pressure or gravity molding of the metal composite structure (10a”') and the joining of the latter with the metal part (24).

5. Manufacturing method according to one of the preceding claims, characterized in that the preform (10) comprises two distinct adjacent zones (10a, 10b), the matrix introduced into the second zone (10b) being different from that of the first zone (10a) and chosen from an organic matrix and a ceramic matrix.

6. Manufacturing method according to one of the preceding claims, characterized in that the reinforcing fibers comprise carbon fibers, silicon carbide fibers, glass fibers, boron fibers, alumina fibers.

7. Manufacturing method according to one of the preceding claims, characterized in that the preform is formed in one piece.

8. Part, characterized in that it comprises several distinct composite structures produced by the method according to one of the preceding claims.

9. Part according to claim 8, characterized in that the separate composite structures are each intended to be subjected to a field of mechanical and / or temperature stresses distinct from one zone to another.

10. Part according to one of the preceding claims, characterized in that the part is a rotor blade (34) of a turbomachine.

11. Part according to claim 10, characterized in that the rotor blade (34) comprises, on the one hand, a blade root comprising a first part formed from a composite structure made from a metal matrix (CMM) and a second part formed from the metal part assembled with the first zone (10a) of the preform and, on the other hand, a blade forming a composite structure made from an organic matrix (CMO).

12. Part according to claim 8 or 9, characterized in that the part is a turboprop propeller.

13. Turbomachine rotor, characterized in that it comprises a plurality of parts according to one of claims 8 to 12.

14. A turbomachine comprising a turbomachine rotor according to claim 13.

Citation Information

Patent Citations

  • Device and method for mounting a root of a blade of a turbomachine and a turbomachine with such a device

    EP1777371A1

  • A composite material fan blade integrating large clearance

    EP3578760A1

  • METHOD FOR MANUFACTURED A PART FROM COMPOSITE MATERIAL AND THE PART THUS MANUFACTURED

    FR3124422A1