OPTOELECTRONIC DEVICE FOR ON-DEMAND DEFORMATION OF A SEMICONDUCTIVE CRYSTALLINE PORTION OPTICALLY COUPLED TO A WAVEGUIDE
The optoelectronic device addresses the limitation of fixed mechanical stress in semiconductor crystalline portions by using electrical deformation to dynamically tune mechanical stress, enhancing performance in devices like laser diodes and photodiodes.
Patent Information
- Application Number
- FR2023004614
- Authority / Receiving Office
- FR · FR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-10
- Publication Date
- 2024-11-15
AI Technical Summary
Existing optoelectronic devices with semiconductor crystalline portions optically coupled to waveguides cannot control the mechanical stress on the central part on demand, limiting the optimization of device performance and functionality.
An optoelectronic device with an electrical deformation device that induces controlled and reversible deformation of the semiconductor crystalline portion via an electrical control signal, using either a piezoelectric or thermal actuator to adjust mechanical stress along a main axis.
Enables dynamic tuning of the semiconductor crystalline portion's optical and electrical properties, allowing for optimized performance and functionality in devices such as laser diodes, photodiodes, and optical modulators by adjusting mechanical stress on demand.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Title of the invention: OPTOELECTRONIC DEVICE FOR DEFORMING ON DEMAND A SEMICONDUCTOR CRYSTALLINE PORTION OPTICALLY COUPLED TO A WAVEGUIDE Technical field
[0001] The field of the invention is that of optoelectronic devices, such as emitting diodes, photodiodes and optical modulators, comprising a semiconductor crystalline portion which can be stressed on demand, in a controlled and reversible manner, by suspended arms. The invention finds an application in integrated photonic circuits, in particular in the context of so-called silicon photonic technology. STATE OF THE PRIOR ART
[0002] In various optoelectronic applications, it may be advantageous to use a semiconductor crystalline portion having a desired mechanical stress, for example in tension. This is the case in particular for certain light sources whose active zone (optical amplification or semiconductor junction) has, outside of mechanical stresses, an indirect energy band structure, this being then made direct by the application of a sufficient mechanical stress in tension. The semiconductor crystalline portion may be a germanium-based crystalline material, such as for example germanium tin Gei xSnx.
[0003] In this respect, document EP3745473A1 describes an optoelectronic device, for example a laser diode, comprising a semiconductor crystalline portion, optically coupled to a waveguide, and stressed by a deformation structure along a main axis. The deformation structure is formed of a support substrate, an interlayer thin layer, and a semiconductor thin layer. The interlayer thin layer is etched locally to form a cavity, and the semiconductor thin layer is structured to form two arms suspended above the cavity and connected to each other by a central portion. This is an optically active zone, and here forms the gain medium of the laser diode. It is located in an optical cavity delimited by two Bragg mirrors made in the structured thin layer.
[0004] In this example, the central part is tensioned by the tensioning arms along the longitudinal axis of the latter. As explained in particular in the article by Süess et al. entitled Analysis of enhanced light emission from highly strained germanium microbridges, Nature Photon. 7, 466-472 (2013), due to the shape of the arms in the plane main axis (parallel to the support substrate), the suspension of the tension arms above the support substrate leads to an increase in the residual tension of the central part of the structured thin layer. Thus, when it is made from germanium, the central part can then present sufficient mechanical tension along the main axis to make its band structure direct.
[0005] Thus, the final value of the mechanical tension undergone by the central part remains constant and cannot subsequently be adjusted. It depends essentially on the dimensions of the tensioning arms and in particular on the aspect ratio 'length to width' of the latter. It is therefore not possible to control on demand the value of the mechanical stresses undergone by the central part, which would make it possible to optimize the performance of the optoelectronic device, whether during operation of the device, or to take into account the type of optoelectronic device (emitting diode, photodiode, etc.). Statement of the invention
[0006] The invention aims to remedy at least in part the drawbacks of the prior art, and more particularly to propose an optoelectronic device suitable for deforming, on demand, in a controlled and reversible manner, a semiconducting crystalline portion optically coupled to a waveguide.
[0007] For this, the object of the invention is an optoelectronic device: - a structure for deforming a semiconductor crystalline portion, comprising a stack of: a support substrate; then a thin intercalary layer delimiting a cavity in a plane parallel to that of the support substrate; then a structured thin layer, resting on the thin intercalary layer, comprising at least two arms suspended above the cavity, extending longitudinally along the same main axis; - the semiconductor crystalline portion, resting on the two arms, and extending longitudinally along the main axis; - a waveguide, optically coupled to the semiconductor crystalline portion.
[0008] According to the invention, the optoelectronic device comprises an electrical deformation device, adapted to deform the semiconductor crystalline portion on demand along the main axis, comprising: an electrical source, adapted to generate an electrical control signal; and an electrical circuit, connected to the electrical source, and adapted to generate in the arms, in response to the electrical control signal, an electric field or a temperature field, inducing a deformation, along the main axis, of the arms and therefore of the semiconductor crystalline portion.
[0009] Some preferred but non-limiting aspects of this optoelectronic device are as follows.
[0010] The semiconductor crystalline portion may have a central portion located between two end portions which rest on the arms, the central portion having an average width less than that of the end portions.
[0011] The semiconductor crystalline portion may have a central portion located between two end portions which rest on the arms, the central portion having an average width less than that of the arms.
[0012] The support substrate can be made from silicon, and the semiconductor crystalline portion can be made from germanium.
[0013] The structured thin layer can be made of a piezoelectric material. The electrical circuit can then comprise two lower and upper electrodes, in the form of thin layers, located on either side of the arms along an axis of thickness of the structured thin layer, and connected to the electrical source to generate, in response to the electrical control signal, an electric field in the arms inducing a deformation of the latter by inverse piezoelectric effect.
[0014] The optoelectronic device may comprise a thin protective layer made of a material inert to hydrofluoric acid, covering a free surface of the arms.
[0015] The optoelectronic device may comprise two thin bonding layers, made from a metallic material, in contact with each other, and located between the semiconductor crystalline portion and the arms.
[0016] The electrical circuit may comprise metal tracks, resting on and in thermal contact with the arms, and connected to the electrical source to generate, in response to the electrical control signal, a temperature field in the arms inducing a deformation of the latter by thermal expansion.
[0017] The waveguide may rest on the arms, and be made of the same material as that of the semiconductor crystalline portion and be in physical continuity with it. Alternatively, the waveguide may be integrated into the support substrate.
[0018] The invention also relates to a method of manufacturing an optoelectronic device according to any one of the preceding characteristics, comprising the following steps: - production of a first stack comprising the structured thin layer covered by a first thin bonding layer; - production of a second stack comprising a thin crystalline semiconductor layer intended to form the crystalline semiconductor portion and covered by a second thin bonding layer; - transfer and bonding of the second stack onto the first stack, by bringing the first and second thin bonding layers into contact.
[0019] The method may comprise the following steps: - prior to the transfer step, structuring of a thin deformation layer of the first stack to form the structured thin layer and the arms; - depositing a thin protective layer, made of a material inert to an etching agent used during a subsequent step of suspending the arms, so as to cover a free surface of the arms.
[0020] The method may comprise the following step: production of a stack formed from the support substrate, then the intercalary thin layer, then a deformation thin layer intended to form the structured thin layer, then a semiconducting thin layer intended to form the semiconductor crystalline portion, the semiconductor thin layer being produced by epitaxy from the deformation thin layer.
[0021] The method may comprise the following steps: - production of a stack formed from the support substrate, then the intercalary thin layer, then the structured thin layer, then the semiconductor crystalline portion; - chemical etching of part of the thin interlayer located under the arms, so as to create a cavity above which the arms are suspended. Brief description of the drawings
[0022] Other aspects, aims, advantages and characteristics of the invention will appear better on reading the following detailed description of preferred embodiments thereof, given by way of non-limiting example, and made with reference to the appended drawings in which:
[0023] Figures 1A, 1B and 1C are schematic and partial views, respectively in longitudinal section, in top view and in perspective, of an optoelectronic device according to a first embodiment where the electromechanical actuator is of the piezoelectric type;
[0024] Figures 2A, 2B and 2C are schematic and partial views, respectively in longitudinal section, in top view and in perspective, of an optoelectronic device according to a second embodiment where the electromechanical actuator is of the thermal type;
[0025] Figures 3A to 3G illustrate different steps of a method of manufacturing an optoelectronic device similar to that illustrated in [Fig.lA] to IC;
[0026] Figures 4A to 4F illustrate different steps of a method of manufacturing an optoelectronic device similar to that illustrated in [Fig.2A] to 2C;
[0027] DETAILED DESCRIPTION OF PARTICULAR EMBODIMENTS
[0028] In the figures and in the remainder of the description, the same references represent identical or similar elements. In addition, the different elements are not shown to scale so as to enhance the clarity of the figures. Furthermore, the different embodiments and variants are not mutually exclusive and may be combined with each other. Unless otherwise indicated, the terms "substantially", "approximately", "in the order of" mean to within 10%, and preferably to within 5%. Furthermore, the terms "between ... and ..." and equivalents mean that the limits are included, unless otherwise stated.
[0029] The invention relates to an optoelectronic device adapted to deform on demand, in a controlled and reversible manner, a semiconductor crystalline portion, the latter being optically coupled to a waveguide to receive or transmit an optical mode thereto. Such an optoelectronic device may be a light source (laser diode or light-emitting diode), a photodetector, or even an optical modulator. Depending on the applications, the waveguide may belong to or be coupled to an integrated photonic circuit, or may be coupled to an external optical fiber.
[0030] Generally, the optoelectronic device comprises an electrical deformation device adapted to deform, in a controlled and reversible manner, suspended arms of a deformation structure on which the semiconductor crystalline portion rests. The electrical deformation device and the deformation structure together form an electromechanical actuator.
[0031] The deformation structure comprises a structured thin layer having two arms suspended above a support substrate, which extend longitudinally along a main axis. The semiconductor crystalline portion rests on the two arms such that the deformation of the arms along the main axis causes that of the semiconductor crystalline portion along the same axis.
[0032] The electrical deformation device comprises: an electrical source adapted to generate an electrical control signal; and an electrical circuit, connected to the electrical source, and adapted to generate, in response to the electrical control signal, an electric field or a temperature field in the arms, which causes the deformation of the arms along the main axis, and therefore of the semiconductor crystalline portion along the same axis.
[0033] The semiconductor crystalline portion then passes, in a controlled and reversible manner, from a first state at rest of mechanical constraints, in the absence of the electrical control signal, where it can be relaxed or can present residual constraints, to a second state of mechanical constraints different from the first state.
[0034] By constrained portion, we mean that the semiconductor crystalline portion undergoes mechanical stresses in tension or compression, resulting in a deformation of the meshes of its crystal lattice. Thus, the portion is constrained in tension when it undergoes a mechanical stress which tends to stretch the meshes of the network in a given direction. In the context of the invention, the semiconductor crystalline portion is intended to be more or less stressed in tension or compression, and preferably in tension, along the main axis which corresponds to the longitudinal axis of the arms.
[0035] The material of the semiconductor crystalline portion, when subjected to mechanical stresses generated by the electromechanical actuator, therefore has modified optical and / or electrical properties, for example in terms of refractive index at a given wavelength and band gap energy. In particular, in the case of a semiconductor crystalline portion made from germanium undergoing mechanical tension, the material may have a reduced band gap energy, in particular that associated with the valley F (or direct valley). The band gap energy can be estimated as a function of the tensile strain, as described in the case of a germanium layer in the publication by Guilloy et al. entitled Germanium under high tensile stress: Nonlinear dependence of direct band gap vs strain, ACS Photonics 2016, 3, 1907-1911.The tensile mechanical stress experienced by the semiconductor crystalline portion may be sufficient for the energy band structure to become direct.
[0036] By direct or substantially direct band structure, it is meant that the minimum energy EBCjl of the conduction band of the valley L (or indirect valley) is greater than or substantially equal to the minimum energy EBCF of the conduction band of the valley F (or direct valley), in other words: AE = EBCjL- EBC E > 0. The semiconductor crystalline portion can be made from germanium whose energy band structure is indirect in the relaxed state, in other words AE < 0, and becomes direct when it undergoes sufficient tensile deformation.
[0037] Note, however, that the semiconductor crystalline portion can be made of a material whose band structure is not necessarily made direct by the deformation generated by the electromechanical actuator. Thus, in the case of a photodetector, the semiconductor crystalline portion can be made of germanium whose value of the forbidden energy band varies according to the deformation generated (regardless of whether its band structure is direct or indirect). Furthermore, in the case of a light source, the semiconductor crystalline portion can be made of GebxSnx with x at least equal to 6% so that its band structure is naturally direct.
[0038] As detailed below, in a first embodiment illustrated in [Fig. 1A] to [Fig. 1C], the electromechanical actuator is of the piezoelectric type, that is to say that it ensures controlled deformation of the arms by an inverse piezoelectric effect. Furthermore, in a second embodiment illustrated in [Fig. 2A] to [Fig. 2C], the electromechanical actuator is of the thermal type, that is to say that the controlled deformation of the arms corresponds to a thermal expansion of the latter.
[0039] Figures 1A and 1B are schematic and partial views, in cross-section and in top view ([Fig.lB]), of an optoelectronic device 1 according to the first embodiment where the deformation of the arms 23.1 is obtained by an inverse piezoelectric effect. [Fig.lC] is a perspective view of the optoelectronic device 1 where certain elements are omitted for the sake of clarity.
[0040] In this example, the optoelectronic device 1 is adapted to emit coherent monochromatic light radiation (laser diode). It comprises an optical cavity oriented along the main axis and delimited by two optical reflectors 3, in which is located the gain medium formed by a central part 11 of the semiconductor crystalline portion 10. However, the optoelectronic device 1 can be a light-emitting diode, a photodiode, or even an optical modulator.
[0041] Here and for the remainder of the description, a direct three-dimensional reference frame XYZ is defined, where the XY plane (main plane) is parallel to the plane of the support substrate 21, where the X axis is oriented along the longitudinal axis of the arms 23.1 and of the semiconductor crystalline portion 10 (main axis), and where the +Z direction is oriented from the support substrate 21 in the direction of the semiconductor crystalline portion 10. Furthermore, the terms “lower” and “upper” are understood as relating to an increasing positioning when moving away from the support substrate 21 along the +Z direction.
[0042] Generally speaking, the optoelectronic device 1 comprises: the semiconductor crystalline portion 10; a waveguide 2 optically coupled thereto; and an electromechanical actuator adapted to generate a deformation along the main axis, at the request (in a controlled and reversible manner) of the arms 23.1, and therefore of the semiconductor crystalline portion 10, here by inverse piezoelectric effect.
[0043] The electromechanical actuator is formed: of a deformation structure 20 which comprises deformation arms 23.1 on which the semiconductor crystalline portion 10 rests; and of an electrical deformation device adapted to generate in the arms 23.1, in response to an electrical control signal, an electric field inducing by reverse piezoelectric effect a mechanical deformation of the latter, and therefore a deformation of the semiconductor crystalline portion 10 along the main axis.
[0044] The deformation structure 20 is formed of a stack of the support substrate 21, a thin interlayer 22, and a structured thin layer 23 made of a piezoelectric material, which comprises two arms 23.1 which extend longitudinally along the same main axis. The semiconductor crystalline portion 10 rests on these two arms 23.1 so that the deformation of the arms 23.1 (here by inverse piezoelectric effect) induces the deformation of the semiconductor crystalline portion 10. This inverse piezoelectric effect is the physical phenomenon of deformation of the crystalline structure of the piezoelectric material, in expansion or compression, in response to the application of an electric field passing through it. As is known, the stress field T in the piezoelectric material depends on the electric field E and the piezoelectric coefficient e. The stress tensor [T] can thus be written, in the absence of an applied external force: [T] = — [e][E].
[0045] The support substrate 21 provides support for the intercalary thin layer 22, the structured thin layer 23 and the semiconductor crystalline portion 10. It may be made from silicon, for example silicon and / or a silicon oxide or nitride. However, it may be made from a material chosen from sapphire, borosilicate, glass, quartz or any other suitable material. It may have a thickness of the order of a few microns to a few hundred microns. Furthermore, the support substrate 21 may include active or passive optical elements (modulators, multiplexers, coupling networks, etc.), particularly in the context of so-called silicon photonics technology.
[0046] The intercalary thin layer 22 ensures the spacing of the arms 23.1 of the structured thin layer 23 with respect to the support substrate 21, and delimits the cavity in the XY plane. It is preferably made from silicon, for example from a silicon oxide or nitride, or even from alumina A12O3, among others. It rests on the support substrate 21, and may have a thickness of the order of a few tens of nanometers to a few microns. It defines laterally, in the XY plane, a cavity above which the arms 23.1 of the structured thin layer 23 are suspended.
[0047] The structured thin layer 23 rests on the intercalary thin layer 22. It is formed of a holding part 23.2, which rests on the intercalary thin layer 22, and arms 23.1 suspended above the cavity. The arms 23.1 are elongated along the main axis X, that is to say they have an average width along the Y axis less than the length along the Z axis. They extend longitudinally, coaxially, along the main axis X, so that this axis forms the main deformation axis of the semiconductor crystalline portion 10.
[0048] The arms 23.1 have a length Lb and an average width <lb>, which is less than the width of the cavity. The width here is the dimension along the transverse axis Y. The arms 23.1 may have a shape in the XY plane that is substantially rectangular, with possibly a progressive or abrupt decrease (as illustrated in [Fig.lB] and IC) of the local width in the direction of the semiconductor crystalline portion 10. In this example, the arms 23.1 have a local width lb which passes, from the holding part 23.2, a first substantially constant value Ibl, then decreases abruptly to a second substantially constant value lb2. Preferably, to effectively induce a deformation of the portion crystalline semiconductor 10, the average value <lb>the width of the arms 23.1 is greater than the average value of the semiconductor crystalline portion 10, and preferably greater than the average value <lpc>of the width of the central part 11 of the semiconductor crystalline portion 10 (where the gain medium is located).
[0049] Note that the arms 23.1 may be physically distinct from one another along the main axis X, as illustrated in [Fig.1A] (no continuity between the arms 23.1 by the material(s) from which they are formed). As a variant (not shown), they may be connected to one another by a central portion of the structured thin layer 23, this central portion extending continuously from one arm to the other under the semiconductor crystalline portion 10 and preferably having a local width at most equal to that of the semiconductor crystalline portion 10.
[0050] In this embodiment where the on-demand deformation of the arms 23.1 is obtained by an inverse piezoelectric effect, the structured thin layer 23 is made from a piezoelectric material, preferably lead zirconate titanate PbZrTiO3 (PZT), but other materials may be used, such as BaTiO3, PAIN, ZnO, LiNbO3, Pb(NbO3)2, PbTiO3, Pb(Mg0.33Nb0.66)O3, Pb(Sc0.5Ta0.5)O3 or any other suitable piezoelectric material. It has a thickness of the order of a few microns, for example between 0.5 and 2 μm. It is a thin layer deposited on the intercalary thin layer 22 by microelectronic deposition techniques, for example by a sol-gel method or by spraying. It is therefore distinguished from piezoelectric substrates whose thickness is several hundred microns or even several millimeters.
[0051] The semiconductor crystalline portion 10 is made of at least one crystalline, and preferably monocrystalline, semiconductor material. This material may be chosen in particular from the elements of column IV of the periodic table, such as germanium Ge, silicon Si, and from the compounds formed from these elements, for example GeSn, SiGe and SiGeSn. It may also be chosen from the IILV compounds comprising elements from columns III and V of the periodic table, such as for example InP and GalnAs, or even from the II-VI compounds, such as for example CdHgTe.
[0052] Preferably, the semiconductor crystalline portion 10 is made from a semiconductor material whose band structure, in the absence of sufficient tensile deformation, is indirect. The tensile deformation of the semiconductor crystalline portion 10, induced by the electromechanical actuator, may then be sufficient to make its band structure direct. The semiconductor crystalline portion 10 is preferably made from germanium. By “made from germanium”, it is meant that the semiconductor crystalline portion 10 is formed mainly from germanium or its compounds. In this example, the crystalline portion semiconductor 10 is made of GeSn.
[0053] The semiconductor crystalline portion 10 preferably has an elongated shape along the main axis X. It rests on the arms 23.1, so that the deformation of the arms 23.1 along the main axis X causes that of the semiconductor crystalline portion 10 along the same axis. It comprises a central part 11, which here forms the gain medium of the laser diode, and two end parts 12, which rest on the arms 23.1. In this example where the arms 23.1 are distinct from each other (no continuity of material), the central part 11 is directly suspended above the support substrate 21 without resting on the arms 23.1, while the end parts 12 rest on the arms 23.1. To improve the mechanical strength of the semiconductor crystalline portion 10 on the arms 23.1 on the one hand, and to optimize the deformation thereof, the central part 11 preferably has an average width less than that of the end parts 12.Furthermore, the central part 11 here has a length Lpc and a width Ipc here substantially constant. Preferably, as indicated previously, so as to optimize the deformation induced by the arms 23.1 in the semiconductor crystalline portion 10, its average width. <lpc>is less than the average width <lb>arms 23.1. The semiconductor crystalline portion 10 has a thickness along the Z axis which can be between a few hundred nanometers and a few microns, for example between approximately 100 nm and 2 pm.
[0054] The optoelectronic device 1 comprises an electrical deformation device, adapted to generate an electric field in the arms 23.1 of the structured thin layer 23, inducing a deformation of the arms 23.1 (by inverse piezoelectric effect), and therefore of the semiconductor crystalline portion 10, along the main axis X. This electrical deformation device comprises an electrical source (not shown) and an electrical circuit adapted to generate the electric field.
[0055] The electrical source is adapted to generate an electrical control signal, for example an electrical potential difference between two electrodes 31, 32, so as to cause a deformation in compression or in tension, by inverse piezoelectric effect, of the structured thin layer 23 along the main axis X.
[0056] The electrical circuit is connected to the electrical source. It comprises two lower electrodes 31 and upper 32, which are in the form of thin conductive layers located on either side of the structured thin layer 23 along the vertical axis Z. The electrodes 31, 32 are made of an electrically conductive material, for example CrAu, Pt / TiO2, among others, and have a thickness for example of the order of 100 nm. The electrical circuit may comprise contact pads 33, 34, which ensure the connection of the lower electrodes 31 and upper electrodes 32 to the electrical source. The contact pads 34 here pass through the structured thin layer 23 to come into contact with the lower electrodes 31 (without contacting the upper electrode 32).
[0057] Finally, the optoelectronic device 1 comprises a waveguide 2 optically coupled to the semiconductor crystalline portion 10. In this example where the optoelectronic device 1 is a laser diode, the waveguide 2 is adapted to receive light radiation from the semiconductor crystalline portion 10 (see dotted arrow in [Fig. 1A]). The waveguide 2 is here a linear portion made of the same material as that of the semiconductor crystalline portion 10, and ensuring physical continuity with the latter. It may have a width different from that of the semiconductor crystalline portion 10. Note that an optical insulation dielectric layer (not shown) may be located between the waveguide 2 and the upper electrode 32 to limit optical losses and thus improve the performance of the waveguide 2.
[0058] Alternatively, as illustrated in [Fig.2A], the waveguide 2 may be an integrated waveguide located in the support substrate 21. The optical coupling is then an evanescent coupling, where the optical mode coming from the semiconductor crystalline portion 10 is coupled firstly to the underlying structured thin layer 23 and then to the integrated waveguide 2. This type of coupling is similar to that described in the document EP3462555A1.
[0059] The waveguide 2 may belong to or be optically coupled to a photonic circuit of the optoelectronic device 1, located for example at least partly in the support substrate 21. The photonic circuit may comprise active and / or passive optical elements. Alternatively or additionally, the waveguide 2 may be optically coupled to an external optical fiber via a diffraction grating.
[0060] In this example where the optoelectronic device 1 is a laser diode, two optical reflectors 3 are produced here in the semiconductor crystalline portion 10, in end parts 12 located on either side of its central part 11 where the gain medium is located. The optical reflectors 3 thus delimit the optical cavity along the main axis X. Also, one of the optical reflectors 3 has a reflectivity substantially equal to 100%, while the other optical reflector 3 (here located between the central part 11 and the waveguide 2) has a reflectivity less than 100%, so as to allow the directive emission of an optical mode at the wavelength of the optical cavity (Fabry-Pérot). In this example, the optical reflectors 3 are cube corner structures, as described in the article by Zabel et al. entitled Top-down method to introduce ultra-high elastic strain, J. Mater. Res., 2017, 32 (4), 726-736.Alternatively, they may be Bragg mirrors produced by partial or total localized etching, depending on the thickness, of the semiconductor crystalline portion 10, as described for example in the document EP3745473A1 cited above. Let us also note that it is advantageous for the optical reflectors 3 to be located in a suspended part of the semiconductor crystalline portion 10 (i.e. which are not perpendicular to the arms 23.1), so as to improve the confinement of the mode in the optical cavity.
[0061] Note that the deformation structure 20 may comprise additional thin layers. Thus, a thin protective layer 41 extends so as to cover a free surface of the arms 23.1, and extends here over the upper face and sides of the arms 23.1. It extends here over the upper electrode 32 (but it may be located between the upper face of each arm 23.1 and the upper electrode 32). It is made of a material inert here to a chemical agent used during a chemical attachment making it possible to produce the cavity and the suspension of the arms 23.2. It makes it possible to protect the arms 23.1 during this chemical attack, here with hydrofluoric acid (HF) in the vapor phase. It may be made of amorphous silicon with a thickness of approximately 60 nm, and may be deposited in a conformal manner by plasma-enhanced chemical vapor deposition (PECVD).
[0062] Furthermore, thin bonding layers 42 (42.1 and 42.2, cf. [Fig.3D]) may be located between and in contact with the semiconductor crystalline portion 10 and the arms 23.1. They may be made of a metallic material, for example aluminum, gold Au or its compounds, among others. As described below, these thin bonding layers 42 ensure the bonding (here by thermocompression) of the semiconductor crystalline portion 10 on the arms 23.1 of the structured thin layer 23.
[0063] Finally, as illustrated in [Fig.3G], a thin encapsulation layer 47 can be deposited so as to cover the semiconductor crystalline portion 10 as well as the deformation structure 20. It can be made of amorphous silicon with a thickness of a few tens of nanometers deposited by PECVD.
[0064] In operation, the electrical source generates an electrical control signal, here a bias voltage between the two lower 31 and upper 32 electrodes. An electric field is then generated within the arms 23.1 of the structured thin layer 23, the field lines of which extend substantially parallel to the vertical axis Z. The electric field induces a deformation of the arms 23.1 along the vertical axis Z, and also, by Poisson effect, a deformation in the XY plane and therefore along the main axis X due to the elongated shape of the arms 23.1 along this axis. The deformation of the arms 23.1 along the main axis X therefore causes that of the semiconductor crystalline portion 10 along the same axis. Note that the intensity of the deformation is proportional to that of the electric field and therefore to that of the electrical control signal.
[0065] Also, the electromechanical actuator is able to deform the crystalline portion semiconductor 10, on demand (in a controlled and reversible manner). The deformation range of the arms 23.1 and therefore of the semiconductor crystalline portion 10 can be significant, for example of the order of several percent, with a control voltage of the order of ten to a few tens of volts, for example of the order of 10 to 20V. The optoelectronic device 1 has an architecture allowing high integration of the different elements on a reduced surface of the support substrate 21. It also allows effective optical coupling to be achieved between the semiconductor crystalline portion 10 and the waveguide 2. All this is obtained in particular by the fact that the deformation structure 20 comprises thin layers produced by conventional microelectronic techniques (deposition, lithography, etching, etc.).Furthermore, as described below, it can be produced from a silicon-on-insulator (SOI) or germanium-on-insulator (GeOI) substrate, possibly with a transfer and bonding step (here by thermocompression).
[0066] By way of example, the arms 23.1 may have a constant width lb2 of 50 pm over a length of approximately 300 pm. The semiconductor crystalline portion 10 may have a central part 11 having a constant width Ipc of 1.5 pm over a length Lpc of approximately 8 pm. The end parts 12 which rest on the arms 23.1 may have a length of approximately 20 pm and a constant width of approximately 40 pm. The central part 11 of the semiconductor crystalline portion 10 may have non-zero tensile stresses in the absence of a control voltage applied by the electromechanical actuator (U=0V), for example of the order of -1.5% for the uniaxial deformation exx due to the residual stresses present in the materials of the stacks and which are released during under-etching.Numerical simulation studies, of the finite element method type, carried out using the COMSOL Multiphysics tool show that the central part 11 of the semiconductor crystalline portion 10 can reach tensile deformations of approximately 3% with very high deformation rates, for example here of the order of 0.2% per volt applied.
[0067] In the case here where the optoelectronic device 1 is a laser diode, the modification on demand of the state of mechanical stresses of the semiconductor crystalline portion 10, and in particular that of the central part 11, makes it possible to tune in a controlled manner the gap of the material and therefore the wavelength of the emission band. It is then possible to shift the optical gain zone over a large wavelength range and therefore to tune or detune it with the spectral distribution of the permitted modes of the cavity. Furthermore, the contribution of free carriers in the gain medium can be carried out by optical pumping or by electrical pumping. In the latter case, the central part 11 comprises a semiconductor junction, for example of the pin type, and electrodes are in electrical contact with this one.
[0068] In the case where the optoelectronic device 1 is a photodetector, the central part 11 of the semiconductor crystalline portion 10 comprises a semiconductor junction, for example of the pin type. Its deformation by the electromechanical actuator makes it possible to modulate the cut-off wavelength in a controlled manner. Due to its architecture, the optoelectronic device 1 can occupy a very small surface area, for example on a silicon substrate, much smaller than that of conventional macroscopic spectrometers. It is then possible to find the shape of the spectrum of the incident radiation on the basis of the measurement of the photoconductivity of the illuminated semiconductor crystalline portion 10 and under increasing mechanical tension.The optoelectronic device 1 then forms a spectrometer of a technology different from those of the FTIR type (analysis in the reciprocal space of the spectrum) or of the grating type (diffraction in the real space of the components of the light according to their frequency).
[0069] Finally, note that the optoelectronic device 1 may be an optical modulator. The material of the semiconductor crystalline portion 10 may be made opaque to the wavelength of the guided mode, due to a reduction in its band gap energy due to sufficient deformation by means of the electromechanical actuator. The optical modulator may behave, for example, as an optical switch, controllable by actuation of the deformation of the arms 23.1 and therefore of the semiconductor crystalline portion 10.
[0070] Figures 2A and 2B are schematic and partial views, in cross-section ([Fig.2A]) and in top view ([Fig.2B]), of an optoelectronic device 1 according to the second embodiment, where the deformation of the semiconductor crystalline portion 10 is induced by a thermal expansion of the arms 23.1 controlled by the electromechanical actuator. [Fig.2C] is a perspective view of the optoelectronic device 1 where certain elements are omitted for the sake of clarity.
[0071] In this example, the optoelectronic device 1 is also a laser diode, but the waveguide 2 is an integrated guide located in the support substrate 21. It belongs to an integrated photonic circuit comprising waveguides and possibly active and / or passive optical elements.
[0072] Here, the deformation structure 20 is similar to that of the first embodiment in that it also comprises a support substrate 21, a thin interposed layer 22 delimiting a cavity in the XY plane, and a thin structured layer 23 comprising the arms 23.1 suspended above the cavity.
[0073] The support substrate 21 is similar to that of [Fig.lA] and differs in that it comprises the integrated waveguide 2. This can be made from a thin layer of silicon, preferably monocrystalline and having a residual voltage. It is surrounded by a sheath made of a silicon oxide. The support substrate 21 can thus be formed from a strained SOI substrate. Furthermore, the intercalary thin layer 22 is here identical to that of [Fig.lA]. The stack 21, 22 and 23 can also be made from a GeOI substrate.
[0074] The structured thin layer 23 is here made of a material whose thermal expansion coefficient is sufficient to impose a desired deformation of the semiconductor crystalline portion 10. In addition, it has optical properties, for example in terms of refractive index at the wavelength of the optical mode, allowing optical coupling between the semiconductor crystalline portion 10 and the integrated waveguide 2. It can also be adapted to produce the semiconductor crystalline portion 10 by epitaxy. Thus, in this example, the semiconductor crystalline portion 10 is produced by epitaxy from the material of the structured thin layer 23. The latter can thus be made of germanium Ge, and the semiconductor crystalline portion 10 can be made of germanium tin GeSn.
[0075] The electromechanical actuator is here adapted to generate a thermal expansion of the arms 23.1, and therefore a deformation of the latter along the main axis X, which consequently induces a deformation of the semiconductor crystalline portion 10 along the same main axis X.
[0076] For this, the electrical source is here adapted to generate a control electric current, and the electrical circuit here comprises metal tracks 35 extending over and in thermal contact with the arms 23.1. These metal tracks 35 are made of a metallic material, for example Pt or TiN with a thickness of 200 nm, and are connected to the electrical source by contact pads 36. A thin layer 24 is located between the structured thin layer 23 on the one hand, and the metal tracks 35 and the electrodes 36 on the other hand. It is made of an electrically insulating and thermally conductive material, for example PAIN. The semiconductor crystalline portion 10 can be covered by it. The circulation of the electric control current in the metal tracks 35 results in heating of these by Joule effect, and therefore of the arms 23.1, which causes their thermal expansion along, in particular, the main axis X.In other words, the circulation of the control electric current generates a temperature field in the arms 23.1 which induces a thermal expansion of the latter. The thermal expansion of the arms 23.1 along the main axis X therefore causes the deformation of the semiconductor crystalline portion 10 along the same axis.
[0077] Also, in operation, the electromechanical actuator makes it possible to impose a deformation on demand, in a controlled and reversible manner, on the semiconductor crystalline portion 10 along the main axis X. Stopping the circulation of the control electric current leads to a return to the initial temperature of the arms 23.1, and therefore to their initial mechanical stress, thus canceling the deformation of the portion crystalline semiconductor 10 imposed by the electromechanical actuator.
[0078] In this example, the optoelectronic device 1 being a laser diode, the central part 11 (gain medium) of the semiconductor crystalline portion 10 is located in an optical cavity delimited by two optical reflectors 3. The latter can be Bragg mirrors (not shown) formed in the integrated waveguide 2. The optical mode (see dotted arrow in [Fig.2A]) is formed in the gain medium and oscillates in the optical cavity, i.e. in the semiconductor crystalline portion 10, then is emitted out of the optical cavity to circulate in the integrated waveguide 2.
[0079] Here, the germanium-based material of the structured thin layer 23 may not be sensitive to the chemical etching agent used to partially etch the interlayer thin layer 22 and form the cavity. Also, a protective thin layer 41 covering the free surface of the structured thin layer 23 (of the arms 23.1 in particular) is not necessary.
[0080] Figures 3A to 3G illustrate steps of an example of a method for manufacturing an optoelectronic device 1 according to the first embodiment (deformation by inverse piezoelectric effect) similar to that of [Fig. 1A] to IC. This method is given here as an example and several modifications can be made.
[0081] With reference to [Fig.3A], a first stack of continuous thin layers is produced from the support substrate 21. Here, we start with an SOI substrate, formed of a silicon substrate (support substrate 21) several hundred microns thick, a buried oxide layer (intercalary thin layer 22), and a thin silicon layer 43 (optional). A conductive thin layer 31c intended to form the lower electrode 31, for example made of CrAu, Pt, or Pt / TiO2, with a thickness of approximately 100 nm, is then deposited, then a piezoelectric thin layer 23c intended to form the structured thin layer 23, for example made of PZT with a thickness of a few microns, and finally a conductive thin layer 32c intended to form the upper electrode 32.
[0082] The thin silicon layer 43, although optional, is advantageous insofar as it makes it possible to improve the symmetry of the thin layers on either side of the piezoelectric thin layer 23, and in particular of the arms 23.1 when they are produced and suspended. Indeed, they will comprise the thin silicon layer 43 at their lower face, and a thin protective layer 41, here made of amorphous silicon, at their upper face (see [Fig.3B]). Preferably, these two thin silicon layers 41, 43 have a substantially identical thickness, for example of the order of a few tens of nanometers, for example 60nm.
[0083] With reference to [Fig.3B], a through opening is made opening onto the intermediate thin layer 22, by localized etching of the conductive thin layer on upper 32c (thus forming the upper electrode 32), the piezoelectric thin layer 23c (thus forming the structured thin layer 23 with the arms 23.1), the lower conductive thin layer 31c (thus forming the lower electrode 31), and here the silicon thin layer 43.
[0084] Here, the thin protective layer 41 is deposited conformally, by PECVD, in amorphous silicon 60nm thick, so as to cover the arms 23.1 and in particular the sides of the latter. This thin protective layer 41 will ensure protection of the piezoelectric material during the chemical etching of a part of the intercalary thin layer 22 during the production of the cavity and the suspension of the arms 23.1. The part of the thin protective layer 41 located in contact with the intercalary thin layer 22 is removed. Then, a full-plate conformal deposition of a thin bonding layer 42.1 is carried out, here a metallic material such as aluminum.
[0085] With reference to [Fig.3C], a second stack is produced comprising a buffer substrate 44, a thin seed layer 45, for example here in germanium with a thickness of a few microns, here approximately 2.5 pm, epitaxially grown from the buffer substrate 44, then a thin layer 46 intended to form the semiconductor crystalline portion 10, here in germanium tin with a thickness of between a few tens of microns to a few microns, for example here approximately 500 nm, epitaxially grown from the thin seed layer 45. A thin bonding layer 42.2 is deposited, here a metallic material such as aluminum.
[0086] With reference to [Fig.3D], the second stack is reported to bring the two thin bonding layers 42.1, 42.2 into contact with each other. The assembly of the two stacks is carried out here by thermocompression, for example at a temperature of approximately 300°C and a pressure of 5 MPa for 30 min. Another type of bonding remains possible, for example a molecular bonding of the oxide / oxide type.
[0087] With reference to [Fig.3E], the buffer substrate 44 is removed, for example by grinding, so as to free the thin seed layer 45. The grinding comprises a mechanical polishing step followed by selective wet or dry etching. The thin seed layer 45 is then removed by selective etching with etching stop on the thin semiconductor crystalline layer 46. The latter is then structured to form the semiconductor crystalline portion 10 (see [Fig.1B]), with the central part 11 and the end parts 12, as well as, here, the waveguide 2. A lateral part of the thin bonding layers, denoted here 42, located around the semiconductor crystalline portion 10 and the waveguide 2, is then freed.This part is then removed, which frees the lateral part of the thin protective layer 41 not covered by the semiconductor crystalline portion 10, as well as the part of the thin intercalary layer 22 located in the cavity.
[0088] With reference to [Fig.3F], a portion of the intercalary thin layer 22 is etched, here by chemical etching with HF in the vapor phase so as to form the cavity. This partial etching causes the arms 23.1 to be suspended. The cavity is delimited in the -Z direction by the support substrate 21 and in the XY plane by the unetched intercalary thin layer 22. The semiconductor crystalline portion 10, and in particular its central portion 11, has a first state of mechanical stress. It may be relaxed, or, as here, have a slight residual tension.
[0089] With reference to [Fig.3G], the optical reflectors 3 are produced (which may have been produced earlier), here cube corners, then a thin encapsulation layer 47 (optional) is deposited in a conformal manner, for example an oxide, covering the semiconductor crystalline portion 10. Finally, the contact pads are produced for each of the arms 23.1, with a first contact pad 33 which comes into contact with the upper electrode 32, and a second contact pad 34 which comes into contact with the lower electrode 31. The contact pads 33, 34 are connected to the electrical source. An optoelectronic device 1 is thus obtained having an integrated architecture, here in silicon technology, comprising an electromechanical actuator (here of the piezoelectric type) making it possible to deform the semiconductor crystalline portion 10 on demand, in a controlled and reversible manner, over a large deformation range.
[0090] Figures 4A to 4F illustrate steps of a method for manufacturing an optoelectronic device 1 according to the second embodiment (deformation by thermal effect) identical or similar to that of [Fig.2A] to 2C. This method is given here as an example and several modifications can be made.
[0091] With reference to [Fig.4A], a stack is produced formed of a support substrate 21, an intermediate thin layer 22, a seed thin layer 23c intended to form the structured thin layer 23, and a thin layer 46 intended to form the semiconductor crystalline portion 10. The support substrate 21 here comprises an integrated waveguide 2, which belongs to an integrated photonic circuit. This support substrate 21 may have been produced from an SOI substrate, where the waveguide 2 was formed from the thin silicon layer of the SOI. The intermediate thin layer 22 is here a layer of silicon oxide, the seed thin layer 23c is here made of germanium, and the semiconductor crystalline layer 46 is made of tin germanium.
[0092] With reference to [Fig.4B], the thin layer 46 is first structured so as to form a mask intended for the production of the arms 23.1 of the structured thin layer 23. For this, the thin layer 46 is locally etched, anisotropically, with a selective etching stop on the Ge layer 23c (or a time etching). The optical reflectors (not shown here) can be produced during this step. Note that the right part of [Fig.4B] is a top view of the stack, and that the left part is a cross-sectional view along line AA.
[0093] With reference to [Fig.4C], the layer 23c is locally etched over its entire thickness, selectively with GeSn, by isotropic dry etching. The Ge under-etching is illustrated on the right-hand side of [Fig.4C] by dotted lines. This gives the structured thin layer 23 which has arms 23.1.
[0094] With reference to [Fig.4D], the semiconductor crystalline portion 10 is then produced by anisotropic localized etching of the layer 46 over its entire thickness selectively with Ge. This produces the semiconductor crystalline portion 10 in GeSn which rests on the ends of the arms 23.1 in Ge. The optical reflectors (if any) may be located in a part of the semiconductor crystalline portion 10 which does not rest directly on the arms 23.1, thus improving the confinement of the optical mode in the optical cavity.
[0095] With reference to [Fig.4E], the contact pads 36 and the metal tracks 35 are produced on the thin layer 24 (here in AIN). The contact pads 36 are connected to the electrical source and the metal tracks are in thermal contact with the arms 23.1.
[0096] With reference to [Fig.4F], a portion of the intercalary thin layer 22 is etched, here by chemical etching with HF in the vapor phase. This partial etching results in the suspension of the arms 23.1 above a cavity delimited in the -Z direction by the support substrate 21 and in the XY plane by the unetched intercalary thin layer 22. The semiconductor crystalline portion 10, and in particular its central portion 11, has a first state of mechanical stress. It can be relaxed, or, as here, have a slight residual tension.
[0097] Thus, an optoelectronic device 1 is obtained having an integrated architecture, here in silicon technology, comprising an electromechanical actuator (here of the thermal type) making it possible to deform the semiconductor crystalline portion 10 on demand, in a controlled and reversible manner, over a large deformation range.
[0098] Particular embodiments have just been described. Different variants and modifications will appear to those skilled in the art.< / lb> < / lpc> < / lpc> < / lb> < / lb>
Claims
Claims
1. Optoelectronic device (1), comprising: • a deformation structure (20) of a semiconducting crystalline portion (10), comprising a stack of: • a support substrate (21); then • a thin interlayer (22) delimiting a cavity in a plane parallel to that of the support substrate (21); then • a structured thin layer (23), resting on the intermediate thin layer (22), comprising at least two arms (23.1) suspended above the cavity, extending longitudinally along the same main axis; • the semiconductor crystalline portion (10), resting on the two arms (23.1), and extending longitudinally along the main axis; • a waveguide (2), optically coupled to the semiconductor crystalline portion (10); • characterized in that it comprises an electrical deformation device, adapted to deform the semiconductor crystalline portion (10) on demand along the main axis, comprising: • an electrical source, suitable for generating an electrical control signal; • an electrical circuit (31, 32, 33, 34; 35, 36), connected to the electrical source, and adapted to generate in the arms (23.1), in response to the electrical control signal, an electric field or a temperature field, inducing a deformation, along the main axis, of the arms (23.1) and therefore of the semiconductor crystalline portion (10).
2. An optoelectronic device (1) according to claim 1, wherein the semiconductor crystalline portion (10) has a central portion (11) located between two end portions (12) which rest on the arms (23.1), the central portion (11) having a lower average width to that of the end parts (12).
3. Optoelectronic device (1) according to claim 1 or 2, wherein the semiconductor crystalline portion (10) has a central portion (11) located between two end portions (12) which rest on the arms (23.1), the central portion (11) having an average width less than that of the arms (23.1).
4. Optoelectronic device (1) according to any one of claims 1 to 3, in which the support substrate (21) is made from silicon, and the semiconductor crystalline portion (10) is made from germanium.
5. Optoelectronic device (1) according to any one of claims 1 to 4, in which the structured thin layer (23) is made of a piezoelectric material, and in which the electrical circuit comprises two lower (31) and upper (32) electrodes, in the form of thin layers, located on either side of the arms (23.1) along an axis of thickness of the structured thin layer (23), and connected to the electrical source to generate, in response to the electrical control signal, an electric field in the arms (23.1) inducing a deformation of the latter by inverse piezoelectric effect.
6. Optoelectronic device (1) according to claim 5, comprising a thin protective layer (41), made of a material inert to hydrofluoric acid, covering a free surface of the arms (23.1).
7. Optoelectronic device (1) according to claim 5 or 6, comprising two thin bonding layers (42.1, 42.2), made from a metallic material, in contact with each other, and located between the semiconductor crystalline portion (10) and the arms (23.1).
8. Optoelectronic device (1) according to any one of claims 1 to 4, in which the electrical circuit comprises metal tracks (35), resting on and in thermal contact with the arms (23.1), and connected to the electrical source to generate, in response to the electrical control signal, a temperature field in the arms (23.1) inducing a deformation of the latter by thermal expansion.
9. Optoelectronic device (1) according to any one of claims 1 to 8, in which the waveguide (2) rests on the arms (23.1), is made of the same material as that of the semiconductor crystalline portion (10) and is in physical continuity with the latter; or in which the waveguide (2) is integrated in the support substrate (21).
10. Method of manufacturing an optoelectronic device (1) according to one of
11.
12.
13. any of claims 5 to 7, comprising the following steps: production of a first stack comprising the structured thin layer (23) covered by a first thin bonding layer (42.1); production of a second stack comprising a thin crystalline semiconductor layer (46) intended to form the crystalline semiconductor portion (10) and covered by a second thin bonding layer (42.2); transferring and bonding the second stack onto the first stack, by bringing the first and second thin bonding layers (42.1, 42.2) into contact. Manufacturing method according to claim 10, comprising the following steps: prior to the transfer step, structuring a thin deformation layer (23c) of the first stack to form the structured thin layer (23) and the arms (23.1); depositing a thin protective layer (41), made of a material inert to an etching agent used during a subsequent step of suspending the arms (23.1), so as to cover a free surface of the arms (23.1). Method of manufacturing an optoelectronic device (1) according to any one of claims 8, comprising the following step: production of a stack formed from the support substrate (21), then from the intermediate thin layer (22), then from a thin deformation layer (23c) intended to form the structured thin layer (23), then from a thin semiconductor layer (46) intended to form the crystalline semiconductor portion (10), the thin semiconductor layer (46) being produced by epitaxy from the thin deformation layer (23c). Method of manufacturing an optoelectronic device (1) according to any one of claims 1 to 9, comprising the following steps: production of a stack formed from the support substrate (21), then the intercalary thin layer (22), then the structured thin layer (23), then the semiconductor crystalline portion (10); chemical etching of a part of the thin interlayer (22) located under the arms (23.1), so as to create a cavity above which the arms are suspended.
Citation Information
Patent Citations
Laser source with a germanium based suspended membrane and integrated waveguide contributing to forming the optical cavity
EP3462555A1
Optoelectronic device comprising a central portion stressed by tensioning according to a first axis and electrically polarised according to a second axis
EP3745473A1
Semiconductor structure comprising a tensilely stressed suspended membrane including an optical cavity
US10411434B2
Laser source with a germanium-based suspended membrane and an integrated waveguide that participates in forming the optical cavity
US10490976B2
Tunable organic VCSEL system
US20040076198A1
Cited By
Integrated optical structure and method of fabricating an integrated optical structure
EP4822430A1