"Thermal expansion compensation unit for fiber optic lines"

The thermal expansion compensation box addresses the issue of fiber breakage by integrating a cylindrical metal envelope with adjustable fiber entrances and exits, compensating for differential expansion, ensuring fiber integrity in extreme environments.

FR3148848A1Pending Publication Date: 2024-11-22SEDI ATI FIBERS OPTIQUES
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
FR2023004813
Authority / Receiving Office
FR · FR
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-15
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Existing optical fibers in extreme environments suffer from breakage due to differential thermal expansion between the metal protective tubes and silica fibers, as the metal tubes expand more than the fibers, leading to mechanical stress and failure.

Method used

A thermal expansion compensation box with a cylindrical metal envelope is integrated into the optical fiber line, featuring a diameter that is between 4 to 15 times the fiber diameter, with offset fiber entrances and exits, and is welded or brazed to the tube faces, allowing the fiber to wind and unwind based on environmental expansion, maintaining the fiber within its nominal curvature radius.

Benefits of technology

The solution effectively compensates for differential thermal expansion, preventing fiber breakage by allowing the fiber to adjust its length according to environmental changes, ensuring longevity and reliability in high-temperature, high-pressure, and radiation-exposed conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The present invention relates to a thermal expansion compensation housing for optical fiber lines, characterized in that it comprises a cylindrical metallic casing (1) defining an inner surface of diameter DB, closed by two front faces (6, 7) and a winding of at least one optical fiber (2) of outer diameter dF, the diameter DB being between 4 times the outer diameter dF of said at least one optical fiber (2) and 15 times the outer diameter dF of said at least one optical fiber (2). Abstract figure: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: "Thermal expansion compensation box on fiber optic lines" Technical field of the invention

[0001] The present invention relates to the field of protection of optical fibers used in high temperature, high pressure or high radiation environments, for example in a nuclear reactor vessel, a boiler, a furnace, a combustion chamber.

[0002] The invention relates in particular to optical fiber-based sensors or detectors for objects, position, IR radiation, or temperature, by the Raman effect or other nonlinear optical effects, introduced into extreme environments (high temperature, high pressure, strong radiation) where active detectors and their electronics cannot be present. Prior art

[0003] The demand for the use of optical sensors is increasing in extreme environments. This is only possible by using optical fiber lines protected by metallic tubes with sensor ends or connectors.

[0004] Prior art is known in the United States patent US7865044B2 concerning remote sensing in an environment with temperatures exceeding 300 °C, using an optical fiber comprising a core, a cladding, and a metallic protective coating on the cladding to protect a surface of the cladding. The cladding has a diameter greater than 150 µm and a thickness of at least 50 µm. A metal conduit encapsulates the sensing fiber, and a pump allows evacuation of the conduit to reduce hydrogen loss. Ceramic splice protectors are used.

[0005] European patent EP3362834B1 relates to an optical fiber comprising a core and a cladding. A metallic sheath surrounds the cladding, the metallic sheath extending over the entire axial length of the optical fiber. A powder is applied as a coating to the outer surface of the metallic sheath, the powder being a mineral powder, a ceramic powder, or a carbon powder.

[0006] Korean patent KR0150915 proposes a metal / carbon coated optical fiber using invar.

[0007] Patent application CN202119938 or patent application CN202563117 also describes a temperature-compensated high-strength optical fiber having an envelope made of a negative-expansion coating at the fiber core, of the sheath, with a high-temperature resistant coating and a high-strength protective layer. Disadvantages of prior art

[0008] Prior art solutions are unsatisfactory because at very high temperatures the metal tube, which has a higher coefficient of expansion than silica, will expand more than the fiber. This difference in expansion will cause breakage of the optical fiber, given that it is fixed to the tube at its ends.

[0009] For example, the coefficient of expansion of a 316L stainless steel tube: 17.5 x 10⁶ °K⁻¹ (from 20°C to 500°C)

[0010] The coefficient of expansion of a silica optical fiber: 4.8 x 10⁷ °K⁻¹ (from 0°C to 900°C)

[0011] For a distance of 10 m (measured at 25°C), the tube expands, in the embodiments of the state of the art, 50 mm longer than the 360° optical fiber. Description of the invention

[0012] The present invention aims to address these drawbacks. To this end, the invention relates, in its most general scope, to a thermal compensation housing characterized in that it comprises a metallic cylindrical envelope defining an internal surface of diameter DB, closed by two front faces and a winding of at least one optical fiber of outside diameter dF, the diameter DB being between 4 times the outside diameter dF of said at least one optical fiber and 15 times the outside diameter dF of said at least one optical fiber.

[0013] The object of the present invention may also have one or a compatible combination of the following characteristics: - The cylindrical casing is preferably between 7.5 times the outside diameter dF of said optical fiber and 10 times the outside diameter dF of said optical fiber - the faces of the cylinder have optical fiber inputs and outputs that are radially offset with respect to the axis of the cylinder - the faces of the cylinder (6, 7) have optical fiber inputs and outputs (1) that are not longitudinally aligned

[0014] The invention also relates to a method of installing a line of at least one optical fiber protected by a metallic tube in a high temperature environment characterized in that at least one thermal compensation box is integrated on said line comprising a metallic cylindrical envelope defining an inner surface of diameter DB, closed by two front faces and a winding of at least one optical fiber of outside diameter dF, the diameter DB being between 4 times the outside diameter dF of said at least one optical fiber (2) and 15 times the outside diameter dF of said at least one optical fiber.

[0015] Preferably said tubes (4, 5) are welded or brazed onto the faces (6, 7) of said cylinder.

[0016] Advantageously, said optical fiber tube lines are assembled and sealed in production at room temperature.

[0017] Description of non-limiting examples of embodiment

[0018] The present invention will be better understood upon reading the following description, concerning a non-limiting example of an embodiment illustrated by the accompanying drawings where:

[0019] [Fig-1] [Fig. 1] shows a perspective view of a compensation unit according to the invention

[0020] [Fig.2] Fig.2 represents a longitudinal cross-sectional view of a compensation housing according to the invention

[0021] [Fig.3] Fig.3 represents a transparent cross-sectional view of a compensation housing according to the invention. General principle of the invention

[0022] The invention relates to the compensation of the differential expansion occurring between the optical fiber and the metallic protective envelope by a thermal expansion compensation box (1) intercalated on a line of optical fibers protected by metallic tubes (4), operating at high temperature high pressure under radiation.

[0023] This compensation box (1) is integrated in the middle of a line of optical fibers protected by tubes. The tubes are welded or brazed to the box, and the fibers (2) are wound around the inner face (3) of the cylinder before exiting into the tubes (4). The number of turns (3) is calculated according to the length of the tubes and their thermal expansion. The box (1) and the tubes (4, 5) are welded or brazed together and are therefore sealed.

[0024] The ends of the optical fibers are attached to connectors or probe heads, which are brazed or welded to the metal tubes (4, 5).

[0025] The compensation housing (1) according to the invention is a cylinder with an inner diameter significantly greater than the break radius of the optical fiber (2) and less than or equal to the nominal bend radius. This nominal bend radius is recommended by the fiber manufacturer.

[0026] In the absence of a manufacturer's recommendation, the nominal bending radius, without a tensile load, corresponds to 10 times the cable's outside diameter, and, under tension or with a "loaded" cable, the nominal bending radius is 15 times the cable's outside diameter. A reference nominal bending radius will typically be 12 times the cable's outside diameter.

[0027] This nominal radius of curvature is typically between 2 and 25 millimeters.

[0028] The radius of breakage is the minimum permissible radius that can bend the fiber The radius of curvature, which determines the optical properties without damaging, bending, or shortening the lens's lifespan, is between 4 and 7.5 times the outer diameter.

[0029] The optical fiber (2) is wound several times around the inner face of the cylinder. The number of turns depends on the difference in expansion between the tube (4, 5) and the optical fiber (2), i.e., the length of the optical line tube. Thus, the volume of this housing (1) allows the fiber to wind or unwind according to the expansion of the tubes (temperature of the environment).

[0030] The optical fiber tube lines (4, 5) are assembled and sealed during production at room temperature. Their high-temperature applications require a transfer housing (1) to absorb the difference in expansion between the metal tubes and the optical fibers.

[0031] The material and thickness of the cylindrical housing are designed to resist pressure and thermal expansion.

[0032] Optical lines in metallic tubing can contain a single optical fiber or a group of optical fibers (a bundle). The compensation box (1) can accommodate several fibers at the input and output.

[0033] It is also possible to put several compensation boxes (1) on a long optical fiber line protected by a tube.

[0034] The optical fibers (1) have their inputs and outputs through the faces of the cylinder (6, 7). These inputs and outputs are off the longitudinal axis (9) of the cylinder and never face each other in order to push the fibers (1) to wind inside.

Claims

Claims

1. Thermal compensation box characterized in that it comprises a metallic cylindrical casing (1) defining an interior surface of diameter DB, closed by two front faces (6, 7) and a winding of at least one optical fiber (2) of external diameter dF, the diameter DB being between 4 times the external diameter dF of said at least one optical fiber (2) and 15 times the external diameter dF of said at least one optical fiber (2).

2. Thermal compensation box according to claim 1 characterized in that it comprises a cylindrical envelope and preferably between 7.5 times the external diameter dF of said at least one optical fiber (2) and 10 times the external diameter dF of said at least one optical fiber (2).

3. Thermal compensation box according to claim 1 or 2 characterized in that said front faces (6, 7) have inputs and outputs of the optical fibers (2) offset radially relative to the axis (9) of said cylindrical casing (1).

4. Thermal compensation box according to claim 1 or 2 characterized in that said front faces (6, 7) of said cylindrical casing (1) have inputs and outputs of the optical fibers (2) which are not aligned longitudinally.

5. Method for installing a line of at least one optical fiber protected by a metal tube in a high temperature environment characterized in that at least one thermal compensation box is integrated on said line comprising a metallic cylindrical casing (1) defining an inner surface of diameter DB, closed by two front faces (6, 7) and a winding of at least one optical fiber of outer diameter dF, the diameter DB being between 4 times the outer diameter dF of said at least one optical fiber and 15 times the outer diameter dF of said at least one optical fiber.

6. Method of installing a line of at least one optical fiber protected by a metal tube according to claim 5 characterized in that tubes (4, 5) are welded or brazed on said front faces (6, 7).

7. Method of installing a line of at least one optical fiber protected by a metal tube according to claim 5 characterized in that said lines of optical fiber tubes are assembled and sealed in production at room temperature.

Citation Information

Patent Citations

  • High-strength high-temperature compensation optical fiber

    CN202119938U

  • Anti-radiation high-temperature compensation optical fiber

    CN202563117U

  • Optical fibers and cables for high temperature applications

    EP3362834B1

  • Metal(INVAR) / cabon hermetic coating optical fiber and making method