Black bismuth tungstate photocatalyst, preparation method, and application
Patent Information
- Application Number
- GB2021005335
- Authority / Receiving Office
- GB · GB
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-09-17
- Filing Date
- 2020-09-11
- Publication Date
- 2024-11-13
- Estimated Expiration
- 2040-09-11
AI Technical Summary
Conventional bismuth tungstate photocatalysts have a high carrier recombination rate, limiting their photocatalytic efficiency, particularly in visible light utilization and CO2 reduction.
A black bismuth tungstate photocatalyst is prepared by treating white bismuth tungstate with dielectric barrier discharge plasma under different atmospheres to reduce elemental bismuth on the surface, enhancing hole-electron separation and expanding light absorption range.
The method improves photocatalytic CO2 reduction ability with mild treatment conditions, low energy consumption, and environmental friendliness, suitable for mass production and enhanced visible light absorption.
Smart Images

Figure 00000001_0000 
Figure 00000002_0000 
Figure 00000003_0000
Abstract
Description
BLACK BISMUTH TUNGSTATE PHOTOCATALYST AND PREPARATION METHOD AND USE THEREOF Technical Field The present invention relates to a preparation method of a black bismuth tungstate photocatalyst, and belongs to the technical field of preparation methods of photocatalytic materials, and specifically, is used for photocatalytic CO: reduction. Background Bismuth tungstate (B12WOs), as a photocatalyst with a certain visible light response, has been widely investigated and applied in, for example, the degradation of organic pollutants and the CO> reduction. However, since the high carrier recombination rate of the conventional bismuth tungstate catalysts affects their photocatalytic efficiency, the modification of the conventional bismuth tungstate catalysts to improve their photocatalytic efficiency becomes more and more important. The existing modification methods of the photocatalysts mainly include morphology control, deposition of precious metal, semiconductor composite, defect control and the like. In recent years, the use of plasma to modify the surface of photocatalysts can greatly improve the catalytic performance. Plasma refers to a gas that is partially or completely ionized, where the sums of the positive and negative charges carried by free electrons and ions completely counteract, so it appears to be electrically neutral on a macroscopic scale. According to the plasma temperature, the plasma can be classified into high-temperature plasma (thermonuclear fusion plasma) and low-temperature plasma. The low-temperature plasma further includes hot plasma (plasma arc, plasma torch, and the like) and cold plasma (low-pressure AC / DC, radio frequency, microwave plasma, and high-pressure dielectric barrier discharge, corona discharge, RF discharge, and the like). A large number of active particles exist in the low-temperature cold plasma and can react with the material surface with which they contact, so they are used to modify the surface of materials. The dielectric barrier discharge (DBD) is a non-equilibrium gas discharge with an insulating medium inserted in the discharge space. It is also called dielectric barrier corona discharge or silent discharge. The dielectric barrier discharge can be operated at a high pressure and in a wide frequency range, and can usually generate plasmas at normal pressure and a power frequency which may be from 50 Hz to 1 MHz. The treatment of photocatalysts with the dielectric barrier discharge plasma has characteristics such as mild treatment conditions, short reaction time and low energy consumption. Summary An objective of the present invention is to provide a black bismuth tungstate photocatalyst by treating white bismuth tungstate with plasmas generated by dielectric barrier discharge under different atmospheres to address the disadvantage of the low visible light utilization of the conventional bismuth tungstate photocatalytic materials, wherein the bismuth tungstate is reduced to elemental bismuth on a surface by plasma treatment, thereby promoting the separation of photogenerated holes from electrons, and also expanding the light absorption range, to improve the photocatalytic CO, reduction ability. In order to achieve the above objective, the following technical solutions are mainly employed. A preparation method of a black bismuth tungstate photocatalyst includes the following steps: (1) weighing white bismuth tungstate and absolute ethanol for ultrasonic dispersion to form a homogeneous mixture, and uniformly applying the mixture on a quartz sheet, followed by oven-drying; (2) placing the oven-dried quartz sheet with the white bismuth tungstate into a dielectric barrier discharge reactor, and performing plasma discharge treatment at a predetermined power for a predetermined time, wherein a reaction gas is introduced at a constant rate during the plasma discharge treatment; (3) collecting the bismuth tungstate after the first plasma treatment, re-dispersing ultrasonically the bismuth tungstate with absolute ethanol to form a homogeneous mixture, and applying the mixture uniformly on a quartz sheet, followed by oven-drying; and (4) placing the completely oven-dried quartz sheet with the bismuth tungstate into the dielectric barrier discharge reactor for secondary treatment, wherein a reaction gas is introduced at a constant rate during the treatment, so as to finally obtain the black bismuth tungstate photocatalytic material when the treatment is completed. In the above preparation method, in Step (1), the white bismuth tungstate is used in an amount of 5-20 mg; the absolute ethanol is used in an amount of 2-4 mL; the ultrasonic dispersion is performed at an ultrasonic power of 100-150 W for an ultrasonic time of 5-10 min; and the quartz sheet used has a thickness of 0.5 mm. In the above preparation method, in Step (2), the power of the dielectric barrier discharge is 50-100 W; the reaction gas is argon, ammonia or hydrogen, the plasma discharge treatment is performed for a treatment time of 1-5 min, and the reaction gas is introduced at a gas flow rate of 100-200 mL / min. In the above preparation method, in Step (3), the absolute ethanol is used in an amount of 1-2 mL; the bismuth tungstate is re-dispersed ultrasonically at an ultrasonic power of 50-100 W for an ultrasonic time of 3-5 min; and the quartz sheet used has a thickness of 0.5 mm. In the above preparation method, in Step (4), the power of the dielectric barrier discharge, the treatment time and the gas flow rate are changed, wherein the power of the dielectric barrier discharge is 100-150 W; the reaction gas is argon, ammonia or hydrogen, the treatment time is 5-15 min, and the gas flow rate is 200-300 mL / min. A black bismuth tungstate photocatalytic material is prepared by the method of the present invention. The present invention has the following beneficial effects. The present invention adopts the treatment method with the dielectric barrier discharge plasma, and has the characteristics of mild treatment conditions, short reaction time, low energy consumption and environmental friendliness. The present invention is suitable for mass production, and has certain application prospects. The surface of the black bismuth tungstate photocatalyst prepared by the present invention contains elemental bismuth, which promotes the separation of photogenerated holes from electrons, and also allows a relatively high visible light absorption, and the black bismuth tungstate photocatalyst has certain application prospects in photocatalytic CO: reduction. Brief Description of the Drawings FIG. 1 is a comparison photograph of the color of bismuth tungstate before and after plasma treatment in Example 1. FIG. 2 shows XRD patterns of bismuth tungstate before and after plasma treatment in Example 1. FIG. 3 shows UV-Vis diffuse reflectance spectra of bismuth tungstate before and after plasma treatment in Example 1. FIG. 4 is a comparison graph of the CO: reduction activity of bismuth tungstate before and after plasma treatment in Example 1. Detailed Description of the Embodiments The present invention is described below in detail in combination with particular embodiments, and is not limited thereto. Experimental methods employed in the following examples are all conventional methods unless particularly indicated. Materials, reagents, and the like employed in the following examples are all commercially available unless indicated particularly. Example 1: 10 mg of white bismuth tungstate was weighed and added into 2 mL of absolute ethanol for sonication at an ultrasonic power of 150 W for an ultrasonic time of 8 min to form a mixed solution. Then, the mixed solution was uniformly applied on a 0.5 mm thick quartz sheet, and after completely oven-dried, the quartz sheet was placed into a dielectric barrier reactor for the first treatment. Hydrogen was introduced into the reactor at a constant rate of 150 mL / min. The discharge power was 80 W, and the treatment time was 5 min. The bismuth tungstate after the treatment was re-collected and re-dispersed ultrasonically with 2 mL of absolute ethanol at an ultrasonic power of 100 W for an ultrasonic time of 5 min to form a mixed solution. The mixed solution was uniformly applied on a quartz sheet. The completely oven-dried quartz sheet was placed into the dielectric barrier reactor for the second treatment. Hydrogen was introduced into the reactor at a constant rate of 300 mL / min. The discharge power was 120 W, and the treatment time was 10 min. Therefore, the black bismuth tungstate was obtained. Example 2: 5 mg of white bismuth tungstate was weighed and added into 2 mL of absolute ethanol for sonication at an ultrasonic power of 100 W for an ultrasonic time of 5 min to form a mixed solution. Then, the mixed solution was uniformly applied on a 0.5 mm thick quartz sheet, and after completely oven-dried, the quartz sheet was placed into a dielectric barrier reactor for the first treatment. Argon was introduced into the reactor at a constant rate of 100 mL / min. The discharge power was 50 W, and the treatment time was 3 min. The bismuth tungstate after the treatment was re-collected and re-dispersed ultrasonically with 2 mL of absolute ethanol at an ultrasonic power of 50 W for an ultrasonic time of 3 min to form a mixed solution. The mixed solution was uniformly applied on a quartz sheet. The completely oven-dried quartz sheet was placed into the dielectric barrier reactor for the second treatment. Argon was introduced into the reactor at a constant rate of 300 mL / min. The discharge power was 100 W, and the treatment time was 5 min. Therefore, the black bismuth tungstate was obtained. Example 3: 20 mg of white bismuth tungstate was weighed and added into 4 mL of absolute ethanol for sonication at an ultrasonic power of 150 W for an ultrasonic time of 10 min to form a mixed solution. Then, the mixed solution was uniformly applied on a 0.5 mm thick quartz sheet, and after completely oven-dried, the quartz sheet was placed into a dielectric barrier reactor for the first treatment. Ammonia was introduced into the reactor at a constant rate of 200 mL / min. The discharge power was 100 W, and the treatment time was 5 min. The bismuth tungstate after the treatment was re-collected and re-dispersed ultrasonically with 2 mL of absolute ethanol at an ultrasonic power of 100 W for an ultrasonic time of 5 min to form a mixed solution. The mixed solution was uniformly applied on a quartz sheet. The completely oven-dried quartz sheet was placed into the dielectric barrier reactor for the second treatment. Ammonia was introduced into the reactor at a constant rate of 300 mL / min. The discharge power was 150 W, and the treatment time was 15 min. Therefore, the black bismuth tungstate was obtained. FIG. 1 is a comparison photograph of the color of white bismuth tungstate before the plasma treatment and black bismuth tungstate after the plasma treatment in Example 1. From FIG. 1, it can be seen that after the treatment, the bismuth tungstate turns from white to black in color. The structure of the prepared sample was tested on the Germany Model Bruker D8 X-ray diffractometer (XRD) (Cu-Ka ray, A=1.5418 A, range 10°-80°) at a scanning speed of 7° min". As shown in FIG. 2, when black bismuth tungstate after the treatment is compared with white bismuth tungstate before the treatment in Example 1, except for the peaks corresponding to bismuth tungstate, the other peaks appeared are all attributed to elemental bismuth, indicating that elemental bismuth was formed by reduction through plasma treatment. FIG. 3 shows UV-Vis diffuse reflectance spectra of white bismuth tungstate before the plasma treatment and black bismuth tungstate after the plasma treatment in Example 1. From FIG. 3, it can be seen that the light absorption range of the black bismuth tungstate is significantly expanded. Example 4. 10 mg of the catalyst prepared in Example 1 was weighed, and dissolved in a formulated solution (6 mL of acetonitrile, 4 mL of H,0, and 2 mL of TEOA) by sonication for 10 min. The reaction system was reacted at a temperature of 10°C and a pressure of 0.75 MPa with the irradiation of a 300 W xenon lamp (PLS-SXE 300C (BF), Perfectlight). Gaseous products were analyzed with a GC-2002 gas chromatography system and a thermal conductivity detector manufactured by Shanghai KECHUANG Chromatography Instruments Co., Ltd. Photocatalytic activity test: The photocatalytic CO: reduction performance of the synthesized sample was tested in a photocatalytic CO; reduction reaction instrument of Model Labsolar-6A manufactured by PerfectLight CO ,LTD. FIG. 4 is a comparison graph of the rate of photocatalytic CO; reduction to CO. It can be seen from FIG. 4 that the performance of the prepared black bismuth tungstate is greatly improved, compared with the untreated white bismuth tungstate. The above-disclosed contents are only preferred examples of the present invention. Without departing from the above methodological idea of the present invention, replacements and improvements based on common technical knowledge and conventional means in the art shall be all included in the protection scope of the present invention.
Claims
1. A preparation method of a black bismuth tungstate photocatalyst, characterized in that the black bismuth tungstate photocatalyst is obtained by treating white bismuth tungstate with plasmas generated by dielectric barrier discharge under different atmospheres, wherein the bismuth tungstate is reduced to elemental bismuth on a surface by plasma treatment, thereby promoting separation of photogenerated holes from electrons, and also expanding a light absorption range, to improve photocatalytic CO2 reduction ability, the method specifically comprises the following steps:(1) weighing white bismuth tungstate and absolute ethanol for ultrasonic dispersion to form a homogeneous mixture, and uniformly applying the mixture on a quartz sheet, followed by oven-drying;(2) placing the oven-dried quartz sheet with the white bismuth tungstate into a dielectric barrier discharge reactor, and performing plasma discharge treatment at a predetermined power for a predetermined time, wherein a reaction gas is introduced at a constant rate during the plasma discharge treatment;(3) collecting the bismuth tungstate after the first plasma treatment, re-dispersing ultrasonically the bismuth tungstate with absolute ethanol to form a homogeneous mixture, and applying the mixture uniformly on a quartz sheet, followed by oven-drying; and(4) placing the completely oven-dried quartz sheet with the bismuth tungstate into the dielectric barrier discharge reactor for secondary treatment, wherein a reaction gas is introduced at a constant rate during the treatment, so as to finally obtain the black bismuth tungstate photocatalytic material when the treatment is completed.
2. The preparation method of the black bismuth tungstate photocatalyst according to claim 1, characterized in that in Step (1), the white bismuth tungstate is used in an amount of 5-20 mg; the absolute ethanol is used in an amount of 2-4 mL; the ultrasonic dispersion is performed at an ultrasonic power of 100-150 W for an ultrasonic time of 5-10 min; and the quartz sheet used has a thickness of 0.5 mm.
3. The preparation method of the black bismuth tungstate photocatalyst according to claim 1, characterized in that in Step (2), the power of the dielectric barrier discharge is 50-100 W; the reaction gas is argon, ammonia or hydrogen, the plasma discharge treatment is performed for a treatment time of 1-5 min, and the reaction gas is introduced at a gas flow rate of 100-200 mL / min.
4. The preparation method of the black bismuth tungstate photocatalyst according to claim 1, characterized in that in Step (3), the absolute ethanol is used in an amount of 1-2 mL; the bismuth tungstate is re-dispersed ultrasonically at an ultrasonic power of 50-100 W for an ultrasonic time of 3-5 min; and the quartz sheet used has a thickness of 0.5 mm.
5. The preparation method of the black bismuth tungstate photocatalyst according to claim 1, characterized in that in Step (4), the power of the dielectric barrier discharge, the treatment timeand the gas flow rate are changed, wherein the power of the dielectric barrier discharge is 100-150 W; the reaction gas is argon, ammonia or hydrogen, the treatment time is 5-15 min, and the gas flow rate is 200-300 mL / min.
Citation Information
Patent Citations
Preparing method of simple substance bismuth / bismuth compound nanocomposite with oxygen vacancies
CN104874811A
Method for converting carbon dioxide
CN106890565A
Plasma-modified metal oxide and g-carbon nitride co-modified titanium dioxide nanorod composite photocatalyst, preparation and application thereof
CN109569684A
Reactor and method for production of nanostructures
US9630162B1