Lignin-silica (SIO2) nanocomposite for sensing of water impurities and method for synthesis thereof

IN605632BActive Publication Date: 2026-10-12GNA UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202311012061
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-02-22
Publication Date
2026-10-12
Estimated Expiration
2043-02-22
Patent Text Reader

Abstract

A lignin-Silica (SiO2) nanocomposite for sensing of water impurities, comprising: i) lignin and silica dioxide (SiO2) in a ratio of 1:1. A method for synthesis comprising of following steps: i) mixing wheat straw with aqueous ethanol and H2SO4 in hydrothermal autoclave, followed by stirring to obtain mixture, ii) filtering mixture using nylon filter to obtain pulp and black liquor, iii) washing pulp with ethanol solution and mixing with black liquor, followed by addition of water to obtain solution, iv) subjecting obtained solution to centrifugation at of 15-25oC followed by filtration to obtain lignin precipitate, v) suspending obtained lignin precipitate in demineralized water followed by stirring utilizing magnetic stirrer at 10-14 h to obtain solution, vi ) adding silica solution and using HCl, followed by stirring to obtain a lignin-silica co-precipitate, and vii) washing obtained lignin-silica co-precipitate with demineralized water, followed by drying at 40-60oC to obtain lignin-silica nanocomposite.
Need to check novelty before this filing date? Find Prior Art

Description

FIELD OF THE INVENTION

[0001] The present invention relates to a lignin-silica (SiO2) nanocomposite forsensing of water impurities and method for synthesis thereof composed from anenvironmentally safe biomaterial (wheat straw) which is environmental friendly,sustainable and scalable utilized for self-cleaning surfaces as well as utilized inwide range of applications such as in solar panel surfaces, marine surfaces, glasssurfaces and in water treatment.BACKGROUND OF THE INVENTION

[0002] The appearance, maintenance, enhancement, and protection of varioussurfaces from contaminants, air oxidation, and moisture corrosion. Althoughsimilar products are widely available in the market, they frequently require rinsingwith water after use and typically rely on a temporary hydrophilic surface. Watermarks, smears, or spots are typically left behind when water dries from the surfacedue to mineral deposits that were present as dissolved solids in water. Whencleaning glass, painted surfaces, steel, alloy, plastic, or ceramic surfaces, this issuebecomes apparent. One method for resolving this well-known problem in theliterature is to dry water from surface by using the cloth. However, the dryingprocess requires lot of time along with manual efforts.

[0003] When the products are tested, they produced unsuitable coatings whenapplied to substrates. For example, it was discovered that the resulting coating isinitially super-hydrophobic and may remain so for long periods of time indoors.However, when exposed to outdoor UV light, rubbed even slightly, or otherwiseexposed to weather, the coating loses super-hydrophobicity within days or insome cases, becomes hydrophilic. Therefore, there is a need of solution.

[0004] EP3009558A2 discloses about a self-cleaning composite material capableof removing contaminants, in particular stains or spots, of solid structures afteractivation. Thus, the present invention describes self-cleaning structures,particularly rigid, flexible or mixed structures, and processes for producing suchself-cleaning structures, especially indicated for clothing and textile articles. Thereferred self-cleaning composite material, by activation, comprises a substrate, aplurality of nanocomposites; wherein each nanocomposite comprises in its coreSiO2 particles coated with TiO2 particles, wherein the nanocomposite iscovalently linked to the substrate, in particular by the linkage of a silane group toa hydroxyl group.

[0005] WO2010078649A2 discloses about two methods for synthesizing noveltitania-polyurethane (nTiO2-PU) nanocomposites for self-cleaning coatings, one apolymer functionalization method ("grafting to") and the other, a monomerfunctionalization method ("grafting from"). Here, 2, 2 bis(hydroxymethyl)propionic acid (HMPA) was used as the coordination agent, which was reactedwith n-TiO2 (50:50 anatase / rutile) to form nTiO2-HMPA, then polymerized in themonomer functionalization method. In the polymer functionalization method,HMPA was reacted with a pre-polymer to form the PU, and then subsequentlyreacted with n-TiO2 to form the polymer nanocomposite. The photocatalyticcleanability of the nanocomposites was investigated when exposed to ultravioletradiation using additional unreacted HMPA or stearic acid as the model "dirt"compounds. Nanocomposites prepared using both strategies showed similar selfcleaning behavior, although the monomer technique gave less substratedegradation.

[0006] Conventionally, synthesized nano composite sensing water imputiries inan effective manner However, these Nano-composite become hydrophilic whenexposed to Ultraviolet solar radiations for longer period of time as well as losestheir super-hydrphobilicity, thereby effecting the sensing of water impurities.

[0007] In order to overcome the aforementioned drawbacks, there is a need tosynthesize a nanocomposite by utilizing environmentally safe biomaterial suchlignin which is principally present in nature in biomass as source of wheat straw,thereby preventing the harmful effects on the environment caused due to theburning of biomass.OBJECTS OF THE INVENTION

[0008] The principal object of the present invention is to overcome thedisadvantages of the prior art.

[0009] An object of the present invention is to synthesize a nanocompositeutilized for self-cleaning surfaces as well as in wide range of applications such asin solar panel surface etc.

[0010] Another object of the present invention is to synthesize a nanocompositewhich is mechanically stable, environmental friendly, sustainable and scalable andsynthesized by the use of biomaterial (Lignin) which is principally present innature in biomass, our source is wheat straw.

[0011] Another object of the present invention is to synthesize a nanocompositein a cost effective manner by converting waste biomass in to valuable product,mainly wheat straw that gives very harmful effects on environment due to stubbleburning.

[0012] Yet another object of the present invention is to synthesize nanocompositewhich is used for wide range of applications such as in solar panel surfaces,marine surfaces, glass surfaces and in water treatment.

[0013] The foregoing and other objects, features, and advantages of the presentinvention will become readily apparent upon further review of the followingdetailed description of the preferred embodiment as illustrated in theaccompanying drawings.SUMMARY OF THE INVENTION

[0014] The present invention relates to a lignin-silica (SiO2) nanocomposite forsensing of water impurities and method for synthesis thereof with the use ofenvironmental friendly biomaterial, coatings that is utilized for water purificationapplications.

[0015] According to an embodiment of the present invention, a lignin-silica(SiO2) nanocomposite for sensing of water impurities and method for synthesisthereof comprises of lignin and silica dioxide (SiO2) in a ratio of 1: 1.

[0016] According to another embodiment of the present invention, the method forsynthesis of a lignin-Silica (SiO2) nanocomposite for sensing of water impuritiescomprising of following steps: i) wheat straw is mixed with aqueous ethanol andsulfuric acid (H2SO4) in a hydrothermal autoclave, followed by stirring for a timeduration in the range of 1.5-2.5 h at a temperature in the range of 140-180°C andsubsequent cooling to obtain a mixture, ii) the obtained mixture is filtered using anylon filter to obtain a pulp and black liquor, iii) the pulp is washed with aqueousethanol solution at a time duration in the range of 50-70°C and mixing with blackliquor, followed by addition of water to obtain a solution, iv) the obtained solutionis subjected to centrifugation at a temperature in the range of 15-25°C at a rpm inthe range of 4900-5000 rpm for a time duration in the range of 15-25 minfollowed by filtration under vacuum using Whatman No 1 filters to obtain ligninprecipitate, v) the obtained lignin precipitate is suspended in demineralized waterand adjusting the pH to 12 using NaOH (Sodium hydroxide), followed by stirringutilizing magnetic stirrer at room temperature for a time duration in the range of10-14 h to obtain a solution, vi) the silica solution is added to the obtain solutionand adjusting the pH to 2 using HCl (Hydrochloric acid), followed by stirring atroom temperature for a time duration in the range of 10-14 h to obtain a ligninsilica co-precipitate, vi) the obtained lignin-silica co-precipitate is washed withdemineralized water, followed by drying at a temperature in the range of 40-60°Cfor a time duration in the range of 5-10 days to obtain the lignin-silicananocomposite, and vii) the obtained lignin precipitate is washed with water anddried at a temperature of 50°C for 72 h.

[0017] According to another embodiment of the present invention, the ligninsilica nanocomposite is fabricated on glass and steel substrate by dip coating (L-bL) technique, followed by coating SDS (sodium dodecyl sulphate) on the coatingfor sensing of water impurities.

[0018] While the invention has been described and shown with particularreference to the preferred embodiment, it will be apparent that variations might bepossible that would fall within the scope of the present invention.BRIEF DESCRIPTION OF THE DRAWINGS

[0019] These and other features, aspects, and advantages of the present inventionwill become better understood with regard to the following description, appendedclaims, and accompanying drawings where:Figure 1 illustrates a schematic illustration of synthesized lignin-Silica (SiO2)nanocomposite and fabrication of coating;Figure 2 illustrates a photographic images of coating of synthesized lignin-Silica(SiO2) nanocomposite over glass substrate and steel panels;Figure 3 (a) and (b) illustrates a microscopic image of scanning electronmicroscopy (SEM) of synthesized lignin-Silica (SiO2) nanocomposite;Figure 4 illustrates a graphical representation of Fourier transform infrared(FTIR) spectroscopy of SiO2 nanoparticle sol;Figure 5 illustrates a graphical representation of Fourier transform infrared(FTIR) spectroscopy of synthesized lignin-Silica (SiO2) nanocomposite;Figure 6 illustrates a photographic image of contact angle measurement ofsynthesized lignin-Silica (SiO2) nanocomposite;Figure 7 illustrates a graphical representation of stability of the coating / contactangle of synthesized lignin-Silica (SiO2) nanocomposite; andFigure 8 illustrates a graphical representation of UV-visible spectroscopy ofsynthesized lignin-Silica (SiO2) nanocomposite.DETAILED DESCRIPTION OF THE INVENTION

[0020] The following description includes the preferred best mode of oneembodiment of the present invention. It will be clear from this description of theinvention that the invention is not limited to these illustrated embodiments but thatthe invention also includes a variety of modifications and embodiments thereto.Therefore, the present description should be seen as illustrative and not limiting.While the invention is susceptible to various modifications and alternativeconstructions, it should be understood, that there is no intention to limit theinvention to the specific form disclosed, but, on the contrary, the invention is tocover all modifications, alternative constructions, and equivalents falling withinthe spirit and scope of the invention as defined in the claims.

[0021] In any embodiment described herein, the open-ended terms "comprising,""comprises," and the like (which are synonymous with "including," "having" and"characterized by") may be replaced by the respective partially closed phrases"consisting essentially of," consists essentially of," and the like or the respectiveclosed phrases "consisting of," "consists of, the like.

[0022] As used herein, the singular forms "a," "an," and "the" designate both thesingular and the plural, unless expressly stated to designate the singular only.

[0023] The present invention relates to a lignin-silica (SiO2) nanocomposite forsensing of water impurities and method for synthesis thereof by utilizingenvironmentally safe biomaterial that is extracted from biomass in a cost effectivemanner used for water purification application.

[0024] According to an embodiment of the present invention, a lignin-silica(SiO2) nanocomposite for sensing of water impurities and method for synthesisthereof comprises of lignin and silica dioxide (SiO2) in a ratio of 1: 1.

[0025] According to another embodiment of the present invention, the methodfor synthesis of a lignin-Silica (SiO2) nanocomposite for sensing of waterimpurities comprising of following steps: i) mixing wheat straw with aqueousethanol and sulfuric acid (H2SO4) in a hydrothermal autoclave, followed bystirring for a time duration in the range of 1.5-2.5 h at a temperature in the rangeof 140-180°C and subsequent cooling to obtain a mixture, ii) filtering the obtainedmixture using a nylon filter to obtain a pulp and black liquor, iii) washing the pulpwith aqueous ethanol solution at a time duration in the range of 50-70°C andmixing with the black liquor, followed by addition of water to obtain a solution,iv) subjecting the obtained solution to centrifugation at a temperature in the rangeof 15-25°C at a rpm in the range of 4900-5000 rpm for a time duration in therange of 15-25 min followed by filtration under vacuum using Whatman No 1filters to obtain lignin precipitate, v) suspending the obtained lignin precipitate indemineralized water and adjusting the pH to 12 using NaOH (Sodium hydroxide),followed by stirring utilizing magnetic stirrer at room temperature for a timeduration in the range of 10-14 h to obtain a solution, vi ) adding silica solution tothe obtain solution and adjusting the pH to 2 using HCl (Hydrochloric acid),followed by stirring at room temperature for a time duration in the range of 10-14h to obtain a lignin-silica co-precipitate, and vii) washing the obtained ligninsilica co-precipitate with demineralized water, followed by drying at atemperature in the range of 40-60°C for a time duration in the range of 5-10 daysto obtain the lignin-silica nanocomposite.

[0026] The lignin-silica nanocomposite used herein is fabricated on glass andsteel substrate by dip coating (L-b-L) technique, followed by coating SDS(sodium dodecyl sulphate) on said coating for sensing of water impurities.EXAMPLE

[0027] Referring to Figure 1, a schematic illustration of synthesized lignin-Silica(SiO2) nanocomposite and fabrication of coating. The method for synthesis of alignin-Silica (SiO2) nanocomposite for sensing of water impurities comprising offollowing steps: i) 40 gm of wheat straw is mixed with 1.25 L aqueous ethanol(EtOH 65%, H2O 35%) and 8 mmol L-1 catalyst sulfuric acid (H2SO4) in a 2 Lhydrothermal autoclave, followed by stirring for a time duration for 2 h at atemperature in the range of 1605°C and subsequent cooling to obtain a mixture, ii)the obtained mixture is filtered using a nylon filter to obtain a pulp and blackliquor, iii) the pulp is washed with 300 ml of aqueous ethanol solution at a timeduration of 60°C and mixing with black liquor, followed by addition of water toobtain a solution, iv) the obtained solution is subjected to centrifugation at atemperature of 20°C at a rpm of 4950 rpm for a time duration of 20 min followedby filtration under vacuum using Whatman No. 1 filters to obtain ligninprecipitate, v) the obtained lignin precipitate is suspended in demineralized waterand adjusting the pH to 12 using 30% of NaOH (Sodium hydroxide), followed bystirring utilizing magnetic stirrer at room temperature for a time duration of 1 h toobtain a solution, vi) the silica solution is added to the obtain solution andadjusting the pH to 2 using 0.1 M HCl (Hydrochloric acid), followed by stirring atroom temperature for a time duration of 12 h to obtain a lignin-silica coprecipitate, vi) the obtained lignin-silica co-precipitate is washed withdemineralized water, followed by drying at a temperature in the range of 50°C fora time duration of 7 days to obtain the lignin-silica nanocomposite, and vii) theobtained lignin precipitate is washed with water and dried at a temperature of50°C for 72 h.

[0028] The obtained lignin-silica co-precipitate is prepared by mixing Ligninsilica ratio in 0.3, 0.6, 1.4 reached by mixing 3, 4, 5 gm of lignin with 30, 20 and10 ml of silica sol. The coating were fabricated on glass and steel substrate by asprepared lignin-silica nanocomposite by facile and sustainable dip coating (L-b-L)technique. After the deposition of one layer the coating were air dried at roomtemperature. The second layer was deposited by same procedure. After thedeposition of lignin-silica nanocomposite on the substrate 2% of surfactant (SDSsodium dodecyl sulphate was coated on the coating to facilitate the final layer ofcoating. The coating reached the angle 164°C by contact angle measurement byapplying a final layer of NUVA-2114, it is a commercially available low surfaceenergy compound basically used in textile industry to make fabrics hydrophobic& self-cleaning.

[0029] Referring to Figure 2, a photographic images of coating of synthesizedlignin-Silica (SiO2) nanocomposite over glass substrate and steel panels isillustrated.

[0030] The synthesized lignin-Silica (SiO2) nanocomposite were subjected tofollowing type of analysis which includes: i) Scanning electron microscopy(SEM), ii) Fourier transform infrared (FTIR) spectroscopy, and iii) contact anglemeasurement.i) Scanning electron microscopy (SEM):

[0031] Referring to Figure 3 (a) and 3 (b), a microscopic image of scanningelectron microscopy (SEM) of synthesized lignin-Silica (SiO2) nanocomposite isillustrated. The size of the synthesized nanocomposite lies in the range of 200 nm.The self-cleaning superhydrophobic surface exhibits rough surface with a micro / nanohierarchical structure of lignin-Silica (SiO2) nanocomposite, which is thebasic framework for the superhydrophobic surface. The silica sols were firmlyimmobilized by lignin biopolymer, which guarantee the mechanical stability andpreserve the superhydrophobic property over long-term use at harsh conditions.ii) Fourier transform infrared (FTIR) spectroscopy:

[0032] Referring to Figure 4 and 5, a graphical representation of Fouriertransform infrared (FTIR) spectroscopy of SiO2 nanoparticle sol and synthesizedlignin-Silica (SiO2) nanocomposite is illustrated respectively. The interactionsbetween different layers of coating and to confirm the formation of synthesizedlignin-Silica (SiO2) nanocomposite IR spectra were recorded. IR spectra of ligninSilica (SiO2) nanocomposite, SDS coated surface and final superhydrophobicsurface coated with NUVA -2114 shows in Figure 5. Characteristics peaks ofSiO2 nanoparticle sol (800 cm-1), low-intensity peaks of SDS (819 cm-1) wasobserved while characteristic peaks of NUVA (1706 cm-1, 1450 cm-1) appearprominent in IR spectra. The characteristics of FTIR peaks of -Si-O, -C=O, -CH2,confirm the interactions between different layers of coating and hence establishedmechanical stability in as fabricated self-cleaning superhydrophobic surface.iii) Contact angle measurement:

[0033] Referring to Figure 6, a photographic image of contact angle measurementof synthesized lignin-Silica (SiO2) nanocomposite is illustrated. Water contactangles of the coatings were measured using optical contact angle goniometer(model SL150) with a drop shape analyzer at ambient temperature the drops ofwater on the sensor surface are perfect spherical water droplets formed with a CAof 163.3°, illustrating the super hydrophobic nature of the self-cleaning sensorsurface. Low surface energy and micro / nanostructures are two essential physicalingredients to prepare the superhydrophobic surface.

[0034] Referring to Figure 7, a graphical representation of stability of thecoating / contact angle of synthesized lignin-Silica (SiO2) nanocomposite isillustrated. To evaluate the mechanical robustness, the tape peeling test for thesensor film is conducted. As shown in Figure 6, after 10 cycles of tape peeling,ignorable effects in superhydrophobicity occurred. The (CA) contact angle of thesensor film slightly declines from 163.3° to 160.7°, and the sliding angle (SA)slightly increases from 2° to 4°. It seems that the increases of (SA) sliding angleare related to the decreases of (CA) contact angle. Continuing to 40 cycles, thesensor still reserves its superhydrophobicity.

[0035] The surface properties of the superhydrophobic sensor film aftercontinuous tape peeling shows resistance to these external destructions, even inexceptionally harsh conditions, is important in real applications. The currentmajor challenge for practical application is its poor mechanical robustness.APPLICATION

[0036] Referring to Figure 8, a graphical representation of UV-visiblespectroscopy of synthesized lignin-Silica (SiO2) nanocomposite is illustrated.Photocatalytic activity is the most essential practical aspect of the hydrophilicself-cleaning coatings. A methylene blue (MB) dye for the determination ofphotocatalytic activity of SiO2 / TiO2 composite coating under ultraviolet (UV-Vis)and visible light irradiations. As shown in Figure 8, the degradation of MB byTiO2 coating and degradation curve are not able to show significant degradationafter 5 min of illumination. As shown in Figure 8, SiO2@TiO2 composite coatingon glass substrate, after 5 min of UV-Vis light illumination it clearly shows thedegradation curve shows fast decrease, demonstrating that self -degradation waspossibly happen within this period. After 5 min the degradation rate staysimmediate constant and after 120 min of illumination under UV-Vis light, about82.79 % of MB degraded by SiO2@TiO2 nanocomposite coating. As theillumination time increases, the degradation curve shows smooth decrease andtends to flatten ,the coating degrade 92.55 % of MB dye solution after 90 min ofillumination. The superhydrophobicity of as prepared composite coating was notshowing decrement after the UV-irradiation, exemplify that the preparedcomposite coating had a UV irradiation resistance.

[0037] Although the field of the invention has been described herein with limitedreference to specific embodiments, this description is not meant to be construed ina limiting sense. Various modifications of the disclosed embodiments, as well asalternate embodiments of the invention, will become apparent to persons skilled inthe art upon reference to the description of the invention.

Claims

1. A lignin-Silica (SiO2) nanocomposite for sensing of water impurities, comprising: i) lignin and silica dioxide (SiO2) in a ratio of 1:1.

2. A method for synthesis of said nanocomposite, comprising the steps of: a) mixing wheat straw with aqueous ethanol and sulfuric acid (H2SO4) in a hydrothermal autoclave, followed by stirring for a time duration in the range of 1.5-2.5 h at a temperature in the range of 140-180°C and subsequent cooling to obtain a mixture; b) filtering said obtained mixture using a nylon filter to obtain a pulp and black liquor; c) washing said pulp with aqueous ethanol solution at a time duration in the range of 50-70°C and mixing with said black liquor, followed by addition of water to obtain a solution; d) subjecting said obtained solution to centrifugation at a temperature in the range of 15-25°C at a rpm in the range of 4900-5000 rpm for a time duration in the range of 15-25 min followed by filtration under vacuum using Whatman No 1 filters to obtain lignin precipitate; e) suspending said obtained lignin precipitate in demineralized water and adjusting the pH to 12 using NaOH (Sodium hydroxide), followed by stirring utilizing magnetic stirrer at room temperature for a time duration in the range of 10-14 h to obtain a solution; f) adding silica solution to said obtain solution and adjusting the pH to 2 using HCl (Hydrochloric acid), followed by stirring at room temperature for a time duration in the range of 10-14 h to obtain a lignin-silica co-precipitate; and g) washing said obtained lignin-silica co-precipitate with demineralized water, followed by drying at a temperature in the range of 40-60°C for a time duration in the range of 5-10 days to obtain said lignin-silica nanocomposite.

3. The method as claimed in claim 3, wherein said obtained lignin precipitate in washed with water and dried at a temperature of 500°C for 72 h.

4. The method as claimed in claim 3, wherein said lignin-silica nanocomposite is fabricated on glass and steel substrate by dip coating (L-b-L) technique, followed by coating SDS (sodium dodecyl sulphate) on said coating for sensing of water impurities.