A biosensor for detection of a biochemical analyte and a method of fabrication thereof

IN606758BActive Publication Date: 2026-10-23INDIAN INST OF TECH BANARAS HINDU UNIV VARANASI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202311076099
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-11-07
Publication Date
2026-10-23
Estimated Expiration
2043-11-07

AI Technical Summary

Technical Problem

Current biosensors for detecting biochemical analytes face limitations such as complex and expensive fabrication methods, sample contamination risks, requirement of sophisticated instrumentation, long analysis durations, and environmental unfriendliness, making them difficult to operate and manage for ultrasensitive trace amount detection.

Method used

A surface-enhanced Raman scattering (SERS) biosensor using a chemically vapor deposited (CVD) three-dimensional network of vertically oriented molybdenum disulphide (MoS2) nano-films on a silicon substrate, which is easy to fabricate, cost-effective, and environmentally friendly, allowing for accurate and quick detection of biochemical analytes at lower concentrations.

Benefits of technology

The SERS-based biosensor achieves ultrasensitive detection of biochemical analytes with a detection limit of 10^-3 to 10^-8 M, providing a non-destructive, contamination-free, and chemically stable solution suitable for the health sector, with enhanced light trapping and adsorption capabilities for improved detection efficiency.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

ABSTRACT “A BIOSENSOR FOR DETECTION OF A BIOCHEMICAL ANALYTE AND A METHOD OF FABRICATION THEREOF” The present invention relates to a surface-enhanced Raman scattering (SERS) technology based on chemical vapor deposition (CVD) grown vertical oriented three-dimensional interconnected network of nano-film (2) of MoS2 over the substrate (1) for the detection of biochemical analyte such as water-soluble vitamin. The present invention provides a SERS substrate-based biosensor with detection limit of 10-3 to 10-8 M for vitamin B12. The method of fabrication of SERS substrate-based biosensor substrate and detection method is quite easy and environment friendly. The chemical stability and cost-effectiveness of CVD synthesized vertical nano-film (2) of MoS2 over Si provides a quick, accurate SERS technology suitable for the health sector. Figures 3 and 4 on sheet no. 3 of the drawings may accompany the abstract when published.
Need to check novelty before this filing date? Find Prior Art

Description

FIELD OF THE INVENTIONThe present invention relates to the field of biosensors. More particularly, the present invention relates to a biosensor for the ultrasensitive detection of a biochemical analyte in a trace amount and a method of fabrication of the biosensor thereof. BACKGROUND OF THE INVENTIONThe human body is composed of around 30 trillion cells that collectively perform the essential functions of life. The cells perform the life-sustaining tasks with the help of several biochemical analytes present in them. The biochemical analyte helps in monitoring or detecting the changes of electrolyte and acid-base status in an individual's body as well as evaluates the ability of a material in the functioning of absorption and metabolism. These biochemical analytes also detect various diseases as well as are also engaged in pharmacokinetic research studies. Additionally, the biochemical analyte is detected with the help of a biosensor technology in which the interaction of analyte is converted into a suitable output that is easily readable by the user. A biosensor helps in detecting target molecules with high accuracy, selectivity and sensitivity. Various analytical methods such as high-performance liquid chromatography, mass spectrometry, colorimetry, amperometry, fluorimetry, etc. have been used to quantify the biomolecule's concentration, but have limits in terms of sample preparation, sophisticated instrumentation, cost and time. WO2023073728A1 discloses a Raman signal enhancing substrate (sensor) for trace level detection and a method of fabrication thereof. The method for the fabrication of plasmonic substrate sensor comprises surface modification by abrasive blasting with abrasives such as aluminium oxide, glass beads or steel grits and conversion of nanostructured substrate to plasmonic substrates via coating with a nanolayer of coinage metals such as gold, silver, copper or combination by thermal evaporation or electrolysis deposition. Hence, the citation discloses a complex and expensive method of fabrication of sensor for trace level detection.CN113155807B discloses microRNA ultra-sensitive detection method based on surface enhanced Raman spectroscopy technology. The method comprises the steps of: firstly, preparing gold-clad silver core-shell structure nanoparticles with internal standard molecule and a silicon wafer with gold nanoparticles as a two dimensional substrate, preparing a capture probe through a microRNA cycle amplification system, coupling the gold-clad silver core-shell structure nanoparticles with the two-dimensional substrate by using the capture probe, obtaining a high-sensitivity SERS spectrum detection and calculating the concentration of microRNA in the solution. Although, the citation provides rapid and efficient ultra-sensitive quantitative detection method for detecting microRNA in serum, however, the method is focussed on expensive colloidal nanoparticles and complex fabrication techniques.CN113138236B discloses a method for quantitatively detecting vitamin B12 in serum and pre-treatment kit. The detection method comprises: pre-treating a serum sample by adopting a methanol and isopropanol precipitation and nitrogen blowing redissolution method; preparing reference solutions of cyanocobalamin, mecobalamin, hydroxocobalamin and cobamamide and performing high performance liquid chromatography / mass spectrometry (HPLC / MS) detection on the pretreated serum sample and the prepared reference solution. The method for determining the concentration of biomolecule sample employs the use of sophisticated instruments that requires long duration of sample run in the analytical instrument.CN115791743A discloses molybdenum disulfide film sensor based on Raman detection and manufacturing method thereof. The molybdenum disulfide film silicon wafer is prepared as: on a clean silicon wafer, pre-treating by an argon plasma gun, self-assembling molybdenum disulfide dispersion liquid and a poly diallyldimethylammonium chloride (PDDA) solution on the silicon wafer layer by layer to form a molybdenum disulfide film and activating ultrasonic molybdenum disulfide powder by using carboxyl provided by sodium cholate added when an EDC / NHS solution is used for activating the ultrasonic molybdenum disulfide powder to form the molybdenum disulfide film silicon wafer. However, the citation is environment-unfriendly.Cao Ky et al., Friction, www.springer.com / journal / 40544; doi: 10.1007 / s40544-017-0172-8 discloses friction characteristics of mechanically exfoliated and chemical vapor deposition (CVD) grown single-layer MoS2. The friction characteristics of mechanically exfoliated single-layer MoS2 and CVD-grown MoS2 at three different temperatures are systematically investigated. The surfaces of the mechanically exfoliated and CVD-grown MoS2 are flat and smooth. The Raman data showed that the crystalline qualities of CVD-grown MoS2 at 800°C and 850°C close to those of mechanically exfoliated MoS2. However, the crystalline qualities of the CVD-grown MoS2 at 900°C are lower than the mechanically exfoliated MoS2. Additionally, the friction of the CVD-grown MoS2 increased as the CVD growth temperature increased. Furthermore, the friction at the grain boundaries is larger than at the grain interior by factors of 1.5 to 3.0 due to defects at the grain boundary.David et al., https: / / doi.org / 10.1016 / j.talanta.2019.120190 discloses spectroelectrochemical elucidation of B vitamins present in multivitamin complexes by electrochemical surface-enhanced Raman scattering (EC-SERS). The development of EC-SERS procedure allows the generation of gold (Au) substrate with SERS properties and the detection and characterization of B vitamins. Furthermore, the combination of the electrochemical activation and Au SPEs offers a methodology to analyze samples of different nature. However, the high concentration 1.5 x 10-4 M of vitamin B1 hampers the interaction between vitamin B6 and Au SERS structure. Although the medium concentration of 10-5 M makes possible the detection of this vitamin as well as other vitamins present in the sample, however, the low concentration of 10-6 M is not detected in a mixture of vitamins.However, the aforementioned state of art provides detection of biochemical analyte that have limitations in terms of sample preparation, chances of sample contamination, sophisticated instrumentation, long duration of sample run in the analytical instruments, expensive methods, user-unfriendly and are difficult to operate and manage.Therefore, there is a need to develop an accurate, highly sensitive, more precise and easy technique to detect even the trace amount of biochemical analyte.OBJECT OF THE INVENTIONThe main object of the present invention is to provide a biosensor for ultrasensitive detection of a biochemical analyte.Another object of the present invention is to provide a non-destructive and contamination free, chemically stable biosensor for ultrasensitive detection of a biochemical analyte.Yet another object of the present invention is to provide a method of fabrication of a biosensor for ultrasensitive detection of biochemical analyte. Yet another object of the present invention is to provide an environment-friendly biosensor for ultrasensitive detection of biochemical analyte in a trace amount.Still another object of the present invention is to provide a biosensor for accurate and quick detection of biochemical analyte.SUMMARY OF THE INVENTIONThe present invention relates to a biosensor for ultrasensitive detection of a biochemical analyte in a trace amount by using surface-enhanced Raman scattering (SERS) technology through SERS substrate synthesized via chemical vapour deposition (CVD) method.In an embodiment, the present invention provides a biosensor for detection of a biochemical analyte, comprising of a substrate, a nano-film, a laser emitting unit, a recording unit and an output unit. The substrate is a silicon (Si) substrate, the nano-film is a three-dimensional network of molybdenum disulphide (MoS2) in the form of nanoflakes, the biochemical analyte is a water-soluble vitamin. The nano-film is vertically oriented on the substrate for detection of the biochemical analyte. The laser emitting unit emits the light on the nano-film for detecting the biochemical analyte. The recording unit records the detection of the biochemical analyte and display on the output unit. Further, the biosensor is a surface-enhanced Raman scattering (SERS)-based biosensor having 3-dimensionally interconnected and vertically oriented network of the nano-film grown over the substrate. In another embodiment, the present invention provides a method for fabrication of a biosensor for detection of a biochemical analyte, comprising, a substrate is cleaned in acetone and isopropanol by ultrasonic bath and rinsed with deionized water to obtain a clean substrate. A predefined amount of molybdenum trioxide (MoO3) powder is kept at centre with the cleaned substrate facing downwards and a predefined amount of sulfur powder is placed upstream in a single heating zone chemical vapour deposition (CVD) furnace to obtain an assembly. This assembly is subjected to vacuum and is purged with gas mixture multiple times in a quartz tube for removing residual oxygen in the single heating zone chemical vapour deposition (CVD) furnace. The temperature of the single heating zone chemical vapour deposition (CVD) furnace is raised to a temperature ranging from 745°C to 755°C with ramping rate in a range of 8°C / min to 12°C / min in a gas mixture of argon and hydrogen to obtain a vertically grown nano-film. In yet another embodiment of the present invention, the biosensor detects the biochemical analyte by preparing the biochemical analyte at predefined concentration at room temperature with ultrasonic treatment for 4-5 hours. The biochemical analyte is dropped on the nano-film followed by keeping in vacuum for 3-4 hours for drying. The nano-film is then illuminated with an excitation wavelength of 532 nm for detection of the biochemical analyte.The present invention relates to the SERS substrate-based biosensor and is a step forward in terms of easy fabrication, cost-effective, environment friendly and applicable for lower concentration detection of biochemical analyte in the health sector.The above objects and advantages of the present invention will become apparent from the hereinafter set forth brief description of the drawings, detailed description of the invention and claims appended herewith.BRIEF DESCRIPTION OF THE DRAWINGSAn understanding of the biosensor for detection of biomolecule and the method of fabrication of the present invention may be obtained by reference to the following drawings:Figure 1 is a pictorial representation of scanning electron microscopy (SEM) image of vertical MoS2 nanofilm grown over Si substrate in part (a); a pictorial representation of high resolution transmission electron microscopy (HRTEM) image of vertical MoS2 nanofilm grown over Si substrate in part (b); a graphical representation for Raman spectrum of vertical MoS2 nanofilm grown over Si substrate in part (c) and a graphical representation for photoluminescence spectrum of vertical MoS2 nanofilm grown over Si substrate in part (d), according to the present invention.Figure 2 is a graphical representation of Raman spectrum of bulk vitamin B12 biomolecules deposited over Si substrate collected using 532 nm excitation wavelength in part (a); a graphical representation of SERS spectra of vitamin B12 on MoS2 / Si substrate at different concentrations in part (b) and a graphical representation for Raman intensity versus vitamin B12 concentrations on MoS2 / Si substrate in part (c), according to the present invention.Figure 3 is a pictorial representation illustrating the SERS measurement of vitamin B12 on MoS2 nanoflakes grown over Si substrate, according to an embodiment of the present invention. Figure 4 is a pictorial representation of SERS substrate in the biosensor, according to an embodiment of the present invention.DETAILED DESCRIPTION OF THE INVENTIONThe present invention will now be described hereinafter with reference to the accompanying drawings in which a preferred embodiment of the invention is shown. This invention may, however, be embodied in many different forms and should not be construed as being limited to the embodiment set forth herein. Rather, the embodiment is provided so that this disclosure will be thorough, and will fully convey the scope of the invention to those skilled in the art.The present invention now will be described hereinafter with reference to the detailed description, in which some, but not all embodiments of the invention are indicated. Indeed, the invention may be embodied in many different forms and should not be construed as limited to the embodiments set forth herein; rather, these embodiments are provided so that this disclosure will satisfy applicable legal requirements. Like numbers refer to like elements throughout. The present invention is described fully herein with non-limiting embodiments and exemplary experimentation.The present invention relates to a surface-enhanced Raman scattering (SERS) technology based on chemical vapor deposition (CVD) grown vertical oriented three-dimensional interconnected network of MoS2 nano-film (2) over the substrate (1) for the detection of biochemical analyte (3) such as water-soluble vitamin.In a preferred embodiment, the present invention provides a biosensor for detection of a biochemical analyte (3), comprising of: a substrate (1); a nano-film (2); a laser emitting unit (4); a recording unit (5); and an output unit (6) wherein, the substrate (1) is a silicon (Si) substrate; the nano-film (2) is a three-dimensional network of molybdenum disulphide (MoS2) in the form of nanoflakes; the biochemical analyte (3) is a water-soluble vitamin; the nano-film (2) is vertically oriented on the substrate (1) for detection of the biochemical analyte (3); the laser emitting unit (4) emits the light on the nano-film (2) for detection of the biochemical analyte; the recording unit (5) records the detection of the biochemical analyte (3) and display on the output unit (6); and the biosensor is a surface-enhanced Raman scattering (SERS)-based biosensor having 3-dimensionally interconnected and vertically oriented network of the nano-film (2) grown over the substrate (1).Here, the water-soluble vitamin is vitamin B12. The nano-film (2) of MoS2 possess thickness in a range of 5 nm to 7 nm with interlayer spacing in a range of 0.65 nm to 0.70 nm. The biosensor exhibits linear variation of peak intensity in a range of 1494 cm-1 to 1500 cm-1 and excitation wavelength of 532 nm, exhibits A-exciton at 1.835 eV to 1.845 eV and B-exciton at 1.965 eV to 1.975 eV. The difference between the A-exciton peak and B-exciton peak is in a range of 0.12 eV to 0.14 eV. In another preferred embodiment, the present invention provides a method for fabrication of a biosensor for detection of a biochemical analyte (3), comprising the steps of: (a) cleaning a substrate (1) in acetone and isopropanol by ultrasonic bath followed by rinsing with deionized water to obtain a clean substrate (1); (b) keeping a predefined amount of molybdenum trioxide (MoO3) powder at centre with the cleaned substrate (1) as obtained in step (a) facing downwards and placing a predefined amount of sulfur powder upstream in a single heating zone chemical vapour deposition (CVD) furnace to obtain an assembly; (c) subjecting the assembly obtained in step (b) to vacuum and purge with gas mixture multiple times in a quartz tube for removing residual oxygen in the single heating zone chemical vapour deposition (CVD) furnace; and (d) raising temperature of the single heating zone chemical vapour deposition (CVD) furnace to a temperature ranging from 745°C to 755°C with ramping rate in a range of 8°C / min to 12°C / min in a gas mixture of argon and hydrogen to obtain a vertically grown nano-film (2) on said substrate (1). In yet another preferred embodiment of the present invention, the biosensor detects the biochemical analyte (3) by the following steps: (i) preparing the biochemical analyte (3) at a predefined concentration at room temperature with ultrasonic treatment for 4-5 hours; (ii) dropping 2 μl of said biochemical analyte (3) on said nano-film (2); (iii) keeping the biochemical analyte for 3-4 hours in vacuum for drying; and (iv) illuminating the nano-film with an excitation wavelength of 532 nm for detection of the biochemical analyte (3).Here, the biochemical analyte (3) is detected at the predefined concentration ranging from 10-3 to 10-8 M; the predefined amount of the molybdenum trioxide (MoO3) is in a range of 95 mg to 105 mg; the predefined amount of the sulfur is in a range of 695 mg to 705 mg; the biosensor is surface-enhanced Raman scattering (SERS)-based biosensor and the nano-film (2) is in the form of nanoflakes.Referring to Figure 3, a pictorial representation of the SERS measurement of vitamin B12 on MoS2 nanoflakes grown over Si substrate is illustrated.Referring to Figure 4, a pictorial representation of SERS substrate in the biosensor is depicted. The SERS based biosensor of the present invention is having 3D interconnected and vertically oriented network of MoS2 nano-film (2) grown over substrate (1). The biochemical analyte (3) is adsorbed on MoS2 / Si SERS substrate indicates strong semiconductor-biomolecule interaction rather than simple physical mixing.EXAMPLE 1Fabrication of SERS-based biosensorVertical nano-film (2) of MoS2 was fabricated on substrate (1) via chemical vapor deposition (CVD) technique. Initially, the substrate (1) was cleaned in acetone and isopropanol for 10 minutes each using ultrasonic bath and then, rinsed with deionized water. Molybdenum trioxide (MoO3) and sulfur powder (99% extra pure, Loba chemie Pvt. Ltd.) were used as precursors. The MoO3 powder was kept at the center with cleaned substrate (1) placed facing downward and the sulfur powder was placed upstream in the single heating zone CVD furnace. Vacuum and purging with gas mixture of argon and 10% hydrogen was done multiple times in quartz tube to exhaust the residual oxygen present. Then, the furnace temperature was raised to ~750°C with 10°C / min ramping rate in Ar / H2 environment having flow rate of 100 standard cubic centimeters per minute (sccm). The reaction time lasts for 10 minutes for the growth of vertically oriented nano-film (2). During the growth process, the Ar / H2 gas carries the sulfur vapors in the heating zone and partially reduces the MoO3 powder to form volatile sub-oxide MoO3-x that again sulfurizes to form MoS2. The vertical morphology is typically attributed to high S:MoO3 concentration. After the reaction time, the system was cool down naturally to room temperature under Ar / H2 atmosphere. Figure 3 shows the schematic representation of the SERS based biosensor for detecting concentration of biochemical analyte (3). In the biosensor, the SERS substrate is fabricated as 3D interconnected vertical network of MoS2 nanoflakes grown over the substrate (1). This vertical network of MoS2 nanoflakes grown over the substrate (1) enhances the light trapping efficiency and allows better adsorption of biochemical analyte (3) i.e., vitamin B12, that gives improved SERS detection. The Raman spectrum of vitamin B12 deposited on the SERS substrate is collected with Airix Corp. STR 300 spectrometer using an excitation wavelength of 532 nm with 50x objective lens and 1.2 cm-1 spectral resolution. To avoid the degradation of biochemical analyte (3) i.e., vitamin B12, a low laser power of 1.15 mW is chosen.EXAMPLE 2Characterization of SERS based biosensorScanning electron microscopyPart (a) of Figure 1 shows the scanning electron microscopy (SEM) image of MoS2 / Si illustrating the growth of interconnected vertically oriented 3D network of MoS2 nanoflakes with enriched edges. The morphology confirms the presence of large number of nucleation sites with nearly vertical morphology that provides accessible surface area for biochemical analyte (3) adsorption on MoS2 / Si SERS substrate with exposed domain edges. The greater SERS enhancement is mainly contributed from the densely stacked vertical nanoflakes.High-resolution transmission electron microscopyPart (b) of Figure 1 shows the high-resolution transmission electron microscopy (HRTEM) image of MoS2 / Si, indicating the presence of six to seven layers having thickness in a range of 5 nm - 7 nm in MoS2 nanostructures with ~0.67 nm of interlayer spacing.Raman spectroscopyThe prepared MoS2 / Si SERS substrate were also characterized using Raman spectroscopy with excitation wavelength of 532 nm as shown in part (c) of Figure 1. The presence of two intense characteristic Raman modes: E12g at ~ 381 cm-1 (in-plane vibration of Mo and S atom) and A1g at ~ 406 cm-1 (the out-of-plane vibration of S atom) shows that the synthesized MoS2 exhibits well-defined and hexagonally symmetric crystalline structure of 2H phase. The layer number of the synthesized MoS2 is estimated by observing the frequency difference between these two phonon modes of ~25 cm-1 indicating the growth of few-layer MoS2 nanoflakes over the substrate (1). Furthermore, a weak broad peak appears at ~450 cm-1 corresponding to 2LA (M) mode (second order longitudinal acoustic phonon at M point in the Brillouin zone). Also, a Si peak appears at ~520 cm-1 in the Raman spectrum of MoS2 / Si. The semiconducting feature of the synthesized MoS2 / Si SERS substrate was observed via photoluminescence (PL) study as shown in part (d) of Figure 1. Two intense PL peaks were observed at ~1.84 eV (A-exciton) and ~1.97 eV (B-exciton) and are attributed to the direct excitonic transition from splitted valence band due to spin orbit coupling, to the doubly degenerate conduction band at K-point of the Brillouin zone. The energy difference between the two excitonic peaks is ~0.13 eV. The existence of direct transition features the charge transfer between the SERS substrate and the biochemical analyte (3) showing an efficient SERS detection.Further, the probe biomolecule that is vitamin B12 is also analyzed using Raman spectroscopy. Part (a) of Figure 2 shows the Raman spectrum of biochemical analyte (3) deposited over the substrate (1) illustrating the different Raman peaks. The Raman spectrum of bare vitamin B12 are linked with corrin ring vibrational modes. The 532 nm excited Raman spectrum shows the most intense band centered at ~1500 cm-1 and was assigned to the stretching of C=C and C=N bonds of the corrin ring with some contributions from CH, CH2 and CH3 bending modes. The Raman bands at ~1164 and 1203 cm-1 were assigned to the stretching of C-C bond in addition to the CH bending, CH2 twisting and CH3 rocking modes. Also, the stretching of C-N mode contributes to the mode at ~1164 cm-1. The band at ~1348 cm-1 is assigned to vibrational stretching of N2-C6 and N3-C14 bonds with respect to the Co-C10 axis. The band at ~729 cm-1 appear due to 5, 6-dimethylbenzimidazole vibrational modes. The weak bands at ~486 and 630 cm-1 were assigned to corrin ring vibration modes and Co-CN stretching mode, respectively. At lower frequency, several modes of low Raman intensities were present and were difficult to assign.Next, the SERS signal for biochemical analyte (3) on prepared nano-film (2) are reported as shown in part (b) of Figure 2. The significant peak shift and enhanced intensity of vitamin B12 when adsorbed on MoS2 / Si SERS substrate indicates better adsorption and strong nano-film (2) biochemical analyte (3) interaction rather than simple physical mixing. With the decreasing concentration of vitamin B12, the SERS intensity decreases. The limit of detection for biochemical analyte (3) adsorbed on nano-film (2) is 10-8 M indicating SERS activity at room temperature. The linear variation of peak intensity is around ~1497 cm-1 of vitamin B12 with concentration on MoS2 / Si substrate as shown in part (c) of Figure 2. The significant intensity of the SERS peak was detected even at ten nanomolar concentration (10-8M) of vitamin B12 on MoS2 / Si substrate. The dense and edge enriched 3D network of vertical MoS2 nanoflakes grown over the substrate (1) provides good surface wettability that assures biochemical analyte (3) adsorption and enhances the light absorption and trapping resulting into enhancement in SERS signal of biomolecules.Therefore, the present invention provides a vertically oriented nano-film (2) grown over substrate (1) as a SERS substrate-based biosensor with detection limit of 10-3 to 10-8M for biochemical analyte (3). The method of fabrication of SERS substrate-based biosensor and detection method is quite easy and environment friendly. The chemical stability and cost-effectiveness of CVD synthesized vertical nano-film (2) over Si provides a quick, accurate SERS technology suitable for the health sector.Many modifications and other embodiments of the invention set forth herein will readily occur to one skilled in the art to which the invention pertain having the benefit of the teachings presented in the foregoing descriptions and the associated drawings. Therefore, it is to be understood that the invention is not to be limited to the specific embodiments disclosed and that modifications and other embodiments are intended to be included within the scope of the appended claims. Although specific terms are employed herein, they are used in a generic and descriptive sense only and not for purposes of limitation.

Claims

1. A biosensor for detection of a biochemical analyte (3), comprising of: a substrate (1); a nano-film (2); a laser emitting unit (4); a recording unit (5); and an output unit (6); wherein, said substrate (1) is a silicon (Si) substrate; said nano-film (2) is a three-dimensional network of molybdenum disulphide (MoS2) in the form of nanoflakes; said biochemical analyte (3) is a water-soluble vitamin; said nano-film (2) is vertically oriented on said substrate (1) for detection of said biochemical analyte (3); said laser emitting unit (4) emits the light on said nano-film (2) for detecting said biochemical analyte (3); said recording unit (5) records the detection of said biochemical analyte (3) and display on said output unit (6); and said biosensor is a surface-enhanced Raman scattering (SERS)-based biosensor having 3-dimensionally interconnected and vertically oriented network of said nano-film (2) grown over said substrate (1) for detection of said biochemical analyte (3).

2. The biosensor as claimed in claim 1, wherein said water-soluble vitamin is vitamin B12.

3. The biosensor as claimed in claim 1, wherein said nano-film (2) of MoS2 possess thickness in a range of 5 nm to 7 nm with interlayer spacing in a range of 0.65 nm to 0.70 nm.

4. The biosensor as claimed in claim 1, wherein said biosensor exhibits linear variation of peak intensity in a range of 1494 cm-1 ± 1500 cm-1.

5. The biosensor as claimed in claim 1, wherein said biosensor exhibits excitation wavelength of 532 nm.

6. The biosensor as claimed in claim 1, wherein said biosensor exhibits A-exciton at 1.835 eV to 1.845 eV and B-exciton at 1.965 eV to 1.975 eV.

7. The biosensor as claimed in claim 1, wherein said biosensor exhibits the difference between said A-excitonic peak and B-excitonic peak in a range of 0.12 eV to 0.14 eV.

8. A method for fabrication of a biosensor for detection of a biochemical analyte (3), comprising the steps of: (a) cleaning a substrate (1) in acetone and isopropanol by ultrasonic bath followed by rinsing with deionized water to obtain a clean substrate (1); (b) keeping a predefined amount of molybdenum trioxide (MoO3) powder at centre with said cleaned substrate (1) as obtained in step (a) facing downwards and placing a predefined amount of sulfur powder upstream in a single heating zone chemical vapour deposition (CVD) furnace to obtain an assembly; (c) subjecting said assembly obtained in step (b) to vacuum and purge with gas mixture multiple times in a quartz tube for removing residual oxygen in said single heating zone chemical vapour deposition (CVD) furnace; and (d) raising temperature of said single heating zone chemical vapour deposition (CVD) furnace to a temperature ranging from 745°C to 755°C with ramping rate in a range of 8°C / min to 12°C / min in a gas mixture of argon and hydrogen to obtain a vertically grown nano-film (2) on said substrate (1).

9. The method as claimed in claim 8, wherein said biosensor detects said biochemical analyte (3) by the following steps: i. preparing said biochemical analyte (3) at a predefined concentration at room temperature with ultrasonic treatment for 4-5 hours; ii. dropping 2 μl of said biochemical analyte (3) on said nano-film (2); iii. keeping said biochemical analyte (3) for 3-4 hours in vacuum for drying; and iv. illuminating said nano-film with an excitation wavelength of 532 nm for detection of said biochemical analyte (3).

10. The method as claimed in claim 8, wherein said biochemical analyte (3) is detected at said predefined concentration ranging from 10-3 to 10-8 M.

11. The method as claimed in claim 8, wherein said predefined amount of said molybdenum trioxide (MoO3) is in a range of 95 mg to 105 mg.

12. The method as claimed in claim 8, wherein said predefined amount of said sulfur is in a range of 695 mg to 705 mg.

13. The method as claimed in claim 8, wherein said nano-film (2) is in the form of nanoflakes.