Organic copolymer additive, its synthesis and its use in coke production

IN607412BActive Publication Date: 2026-10-27TATA STEEL LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202231077457
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-12-30
Publication Date
2026-10-27
Estimated Expiration
2042-12-30

AI Technical Summary

Technical Problem

The challenge is to enhance the quality of metallurgical coke produced from weak coking coal without compromising its properties, as the global supply of prime coking coal is limited and the use of non-coking coals is prevalent, requiring additives that improve coking potential without emitting pollutants.

Method used

A phenol-melamine-urea based organic copolymer is synthesized and added to the coal blend, which improves the swelling and fluidity of the coal matrix during carbonization, allowing for a higher percentage of non-coking coal to be used without deteriorating coke quality, through a pilot-scale synthesis process.

Benefits of technology

The organic copolymer significantly enhances the crucible swelling number and fluidity of semi-soft, hard, and non-coking coals, enabling the use of up to 16% non-coking coal in the blend while maintaining or improving coke strength properties, as demonstrated by carbonization studies and coke strength after reaction tests.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

PLEASE SEE ATTACHED
Need to check novelty before this filing date? Find Prior Art

Description

FIELD OF THE INVENTIONThe present disclosure relates to the formation of metallurgical coke from weak coking coal by theaddition of organic copolymer. The present disclosure provides organic polymer additive, its pilotscale synthesis and application in metallurgical coke production.BACKGROUND OF THE INVENTIONMetallurgical coke plays a crucial role for the production of pig iron in the blast furnace. It acts asa chemical reducing agent, fuel as well as crucial permeable support. Considering various roles ofcoke in the blast furnace, a coke with specific physical and chemical properties is essential forsmooth operation and high productivity in modern blast furnaces.Due to the high price and the inadequate stock of prime coking coal on global scale, usage of ahigher amount of poor coking coal in the blend is increased to form high-strength coke in steelindustry. The demand for superior quality coke with a higher percentage of non-coking coals ishigh. Substantial amount of research is going on to synthesis organic additives, which can enhancethe coke quality of non-coking coal. The impact of organic additives on the thermochemicaltransformation of coal arises through the increase in fluidity and thereby softening coal in cokemaking. During heating, polymeric additives penetrate to the organic mass of the coal grains at thecontact surface through the evolution of hydrogen followed by stabilization of the metaplast in thefluidic regime.Due to the limited reserve of prime coking coal in the world, various technologies have beenexplored to improve the coking potential of weak-coking coals. The addition of additives in thecoal blend is an effective technology to get better coke quality. The usage of blends of coals ofdifferent origin and quality is the standard practice in the coke manufacture industry. Additionalcarbonaceous materials as additives like pitch, coking plant waste materials can be used in thepreparation of industrial coal blends for metallurgical coke making. Additionally, anthracite andbituminous like materials e.g. coal tar, coal-tar pitch can be utilized in the coke oven.Nowadays, lignin (an aromatic plant polymer) is one of the most attractive renewable materialprecursors for the development of smart materials. It is an excellent candidate for chemicalmodifications and reactions due to its highly functional character (i.e., rich in phenolic andaliphatic hydroxyl groups) for the development of new bio-based materials which will improve itsbinding property as well as high thermal stability. Suopajarvi et. al. investigates the effects ofcharcoal and Kraft-lignin additions on the structure, cold compression strength, and reactivity ofbio-cokes produced from medium-volatile coal.The addition of binders like coal tar pitch to the coal blend, prior to stamping is expected to reducethe consumption of thermal energy and would impart the requisite strength and stability at lowermoisture levels. Coal-tar pitch has been recognized as a suitable active plasticizing agent duringthe co-carbonization processes. The proper chemical composition, mainly of an aromatic natureand good coking properties are all the advantages of coal-tar pitch as a blend constituent.Moreover, pitch addition improves the strength characteristics of the resultant coke derived fromcoals having weak rheological properties.Moreover, materials derived from petroleum processing have also been utilized as additives incoke production. Nomura et al. have reported that interaction between semi-soft coking coal andpetroleum-derived binder enhanced the caking property and coke strength. However, theseadditives usually contain high sulfur, emit high amount of pollutants and subsequently reduces thecoke quality. There is a demand for the coke additive which enhances coke quality withoutemission of pollutants.There are no scientific studies available on pilot scale synthesis of phenol, melamine and ureabased organic copolymer for metallurgical coke-making application. Therefore, a technologywithout compromising the coke quality of higher percentage of non-coking coals is highlydesirable. Thus, the aim of the present disclosure is to maximum utilization of poor coking coal inblend to produce metallurgical coke with addition of smart polymeric additive.OBJECTIVES OF THE INVENTIONThe main objective of the present disclosure is to provide an organic copolymer-based additive.One objective of the present disclosure is to provide a pilot-scale synthesis of the organiccopolymer-based additive.One objective of the present disclosure is to provide a blend for metallurgical coke making.One objective of the present disclosure is to provide the organic copolymer-based additive forpreparing a blend for metallurgical coke synthesis.One objective of the present disclosure is to provide a method for metallurgical coke production.Yet another objective of the present disclosure isto improve the swelling and fluidity of coal matrixby using the organic copolymer during carbonization.One objective of the present disclosure is to utilize the maximum amount of different type of noncoking coal in blend without deterioration of metallurgical coke properties.SUMMARY OF THE INVENTIONThe present disclosure provides an organic copolymer-based additive. Particularly, the presentdisclosure provides a phenol-amine based organic co-polymer-based additive. The presentdisclosure relates to the formation of metallurgical coke from weak coking coal by the addition ofan organic copolymer. Specifically, the present disclosure defines the synthesis of an organiccopolymer derived from phenol melamine and urea-based precursor in presence of formaldehydemonomer using single alkali metal catalyst and its application in metallurgical coke production.The present disclosure also provides a blend for metallurgical coke making. The present disclosureprovides the organic copolymer-based additive for preparing a blend for metallurgical cokesynthesis. The present disclosure relates to improving the swelling and fluidity of coal matrix byusing the organic copolymer during carbonization. The present disclosure provides utilization ofthe maximum amount of different type of non-coking coal in blend without deterioration ofmetallurgical coke properties.BRIEF DESCRIPTION OF THE DRAWINGSIn order that the disclosure may be readily understood and put into practical effect, reference willnow be made to exemplary embodiments as illustrated with reference to the accompanying figures.The figures together with a detailed description below, are incorporated in and form part of thespecification, and serve to further illustrate the embodiments and explain various principles andadvantages, in accordance with the present disclosure where:Fig 1 illustrates a schematic representation for the synthesis of organic copolymer.Fig 2 illustrates FTIR Spectra of organic copolymer.Fig 3 illustrates 13C NMR Spectra of organic copolymer.DETAILED DESCRIPTION OF THE INVENTIONAt the very outset of the detailed description, it may be understood that the ensuing descriptiononly illustrates a particular form of this disclosure. However, such a particular form is an onlyexemplary embodiment, and without intending to imply any limitation on the scope of thisdisclosure.While the disclosure is susceptible to various modifications and alternative forms, specific aspectthereof has been shown by way of example and will be described in detail below. It should beunderstood, however that it is not intended to limit the disclosure to the particular forms disclosed,but on the contrary, the disclosure is to cover all modifications, equivalents, and alternative fallingwithin the spirit and the scope of the invention.The Applicant would like to mention that the examples are mentioned to show only those specificdetails that are pertinent to understanding the aspects of the present disclosure so as not to obscurethe disclosure with details that will be readily apparent to those of ordinary skill in the art havingthe benefit of the description herein.The terms "comprises", "comprising", or any other variations thereof, are intended to cover a nonexclusive inclusion, such that a method that comprises a list of components does not include onlythose components but may include other components not expressly listed or inherent to suchprocess. In other words, one or more elements in a method proceeded by "comprises… a" doesnot, without more constraints, preclude the existence of other elements or additional elements inthe method.Accordingly, the main embodiment of the present disclosure provides an organic copolymer-basedadditive which is phenol-amine based co-polymer having the following chemical formula:In one embodiment, the viscosity of the copolymer is in a range of 15-50 cP.In one embodiment, the solid content of the copolymer is 50-55 weight %.In one embodiment, the present disclosure provides a method for preparing the organic copolymerwherein the method comprising the steps of:(a) treating phenol with formaldehyde monomer in presence of ammonia solution at 40-50°Ctemperature for 0.5-1 hr to obtain a reaction mixture;(b) adding an alkali metal catalyst into the reaction mixture of step (a);(c) adding melamine into the reaction mixture of step (b) at a temperature of 85-90 °C; and(d) adding urea precursor into the reaction mixture of step (c) at a temperature of 80-85 °Cfor 1-2 hr to obtain the copolymer.In one embodiment, the alkali metal catalyst is selected from sodium hydroxide and potassiumhydroxide.In one embodiment, the alkali metal catalyst is sodium hydroxide.In one embodiment, phenol is in a range of 8-12 wt %.In one embodiment, formaldehyde monomer is in a range of 58-62 wt %.In one embodiment, melamine is in a range of 14-16 wt %.In one embodiment, urea precursor is in a range of 14-16 wt %.In one embodiment, pH of the reaction mixture in presence of ammonia solution is 5.7 to 6.4.In one embodiment the ammonia solution is 25% ammonia solution.In one embodiment, pH after adding alkali metal catalyst is 8.5 to 9.In one embodiment of the disclosure, co-polymerization is occurred between phenolic moiety andmelamine unit with formaldehyde monomer and urea-based functional group. Also, H-bondinginteraction between phenolic component with amine-based functional present in melamine andamide functional group of urea precursor provides the desirable stability of the additive and formsco-polymer network structure. In one embodiment, the organic copolymer is called as Fortiset1150.In one embodiment, the present disclosure provides a blend for metallurgical coke making whereinthe blend comprises:a) one or more non-coking coal (Non-coking coal is the type of coal which do not soften,swell and resolidify during carbonization. Non-coking coal does not have any cakingproperties. Therefore, this type of coal is not suitable for coke making);b) one or more coking coal (Coking coal is the type of coal which on heating in the absenceof air undergoes a transformation into a plastic state, swells and then solidifies to formcoke); andc) the organic copolymer having the following chemical formula:In one embodiment, one or more non-coking coal is present in 5-20 wt. %.In one embodiment, one or more coking coal is present in 80-95 wt.%.In one embodiment, the organic copolymer is 0.7 - 1 wt. %.In one embodiment, the present disclosure provides a method for metallurgical coke productioncomprising the steps of:(a) preparing an organic polymer derived from phenol, melamine and urea precursor,formaldehyde-based monomer in presence of alkali metal catalyst; and(b) mixing the organic polymer in a specific dosage with specific coal blend for carbonizationstudy.The co-polymer significantly enhanced the crucible swelling number (CSN) and fluidity of semisoft, hard coking coal and non-coking coal.The additive is mixed to the coal blend for cake formation in a specific dosage (0.7-1 wt. %) duringcarbonization study. The coal blend is prepared by using different types of coal, which containssemi soft coal 45-70 wt. %, hard coking coal is 15-40 wt. % and non-coking coal 6-16 wt. %.Fortiset 1150 co-polymer enables to accommodate 6-16 wt. % different type non-coking coal inthe coal blend with improved coke strength properties.The following examples further describe and demonstrate embodiments within the scope of thepresent disclosure. The examples are given solely for the purpose of illustration and not to beconstrued as limitations of the present disclosure, as many variations are possible withoutdeparting from the spirit and scope of the disclosure.EXAMPLESSynthesis of organic copolymerIn a pilot scale reactor, phenol (8-12 wt %) is gradually mixed with formaldehyde monomer (58-62 wt %) in presence of 25% ammonia solution to neutralize the pH to 5.7-6.4 and heated at 40-50 °C for 0.5-1 hr. Sodium hydroxide solution (40%) is added to the mixture to adjust pH of thesolution to 8.5-9 and mixed it for 10-15 min. Melamine (14-16 wt %) is slowly mixed into thereaction vessel with continuous stirring and the temperature is maintained at 85-90 °C. Thereaction mixture is uniformly mixed until the water solubility of the mixture is improved. Theurea-based raw material (14-16 wt %) is added to the reaction mixture immediately and maintainedat 80-85 °C temperature till the water solubility of the material is further improved. Finally, theentire reaction mixture is gradually cooled down to 30 °C and the resultant polymeric material isdischarged from the reaction vessel. The synthesized product is obtained as organic copolymerand schematic representation is shown in Fig. 1. Herein, co-polymerization occurs betweenphenolic moiety and melamine unit with and formaldehyde monomer and urea-based functionalgroup. Also, H-bonding interaction between phenolic component with an amine-based functionalpresent in melamine and amide functional group of urea precursor provides the desired stability ofthe additive and forms co-polymer network structure.Physical and chemical characteristics of organic copolymerPhysical and chemical properties of phenol-melamine-urea based organic copolymer arementioned as follows:Appearance: Reddish Brown liquidNature: Adhesive and easily flowableSolubility: Soluble in waterSpecific gravity (at 25 °C): 1.215Viscosity (at 22 °C): 15 cPSolid: 52.43 %Molecular weight:The molecular mass of organic copolymer is measured through DLS method and its value is 5.15x 104 Da.FTIR spectra:The FTIR spectrum (Fig.2) of organic copolymer shows the symmetric and asymmetric stretchingvibrations for C-O group of aromatic sectors at 1005 cm-1 and 1155 cm-1, respectively. The peakat 1260 cm-1 is responsible for stretching vibration of C-N functional group present in melaminecomponent of polymer. The peaks at 1368 cm-1 is associated with the C-H bending vibration. The peak for aromatic C=C stretching vibration is observed at 1565 cm-1. The emerging peaks at 1660cm-1are attributed to C=O amide stretching vibration of urea component present in polymermatrix. The peak at 2960 cm-1 is due to the presence of methylene (-CH2) bridges or aliphatic -CHstretching vibration. The peaks at 3355 cm-1 is associated with the O-H and N-H stretchingvibration of phenolic / amine moiety present in co-polymer structure.13C NMR Spectra:Liquid state 13C NMR of the organic copolymer (Fig. 3) is performed in presence of D6-DMSOsolvent. Here, chemical shifts around δ 39 ppm is responsible for ortho methylene bridges ofphenol & melamine linkages of polymer. Chemical shift at δ 49 ppm is because of the carbons ofNH-CH2-NH linkages of dimethylene urea segments of polymer. The chemical shift at δ 59-64ppm is because of the presence of methylol groups (-CH2OH) of polymeric unit. The peak at δ115-132 ppm is due to the presence of substituted aromatic carbons present in phenolic &melamine unit. The chemical shift at δ 151-167 ppm is because of the phenoxy carbon of resin.Characterization of coalThe coals are characterized in terms of ash, volatile matter (VM) and category in terms of cokingpotentiality (Table 1). The details of the tests are as follows:Ash analysis:Ash is determined by following ASTM standard D 3174-11. 1 gm of 250 mm size sample is takento a weighed capsule. Then the sample is placed in a cold muffle furnace and heated gradually insuch a way that the temperature reaches from 450 °C to 500 °C by 1 hr. At the end of 2 hr. it willreach 950°C. After cooling, the weight of the sample is measured, and ash is calculated by weightdifference.VM analysis:VM is determined by following ASTM standard D 3175-11. In this test 1 gm of 250 mm sizesample is taken in a covered platinum crucible and heated in a furnace of 950 °C for 7 min. TheVM is calculated by weight difference.Table 1: Properties of different coal samplesCrucible swelling number (CSN) study:Crucible swelling number test is done by following ASTM D720-91 (2010). In which 1 gm ofsample (-0.212 mm size) is taken in a translucent squat shaped silica crucible and the sample isleveled by tapping the crucible 12 times. The crucible is covered with a lid and heated understandard conditions, either by a special type of gas burner or muffle furnace. After the test, theshape of coke button is compared with a standard chart and accordingly, the crucible swellingnumber (0 to 9) is assigned to the coal sample.Table 2 summarizes the CSN result of coal before and after the addition of organic copolymer(dosage: 5 wt. %). For all the coal samples (Semi Soft: Coal A, Hard Coking: Coal E and Noncoking: Coal J) addition of polymer makes significant improvement of swelling property of coal.Table 2: CSN value of coal before and after addition of organic copolymerFluidity study:The instrument used for fluidity determination is known as Geiseler Plastometer. Plastometermeasures the plastic properties of coal by using of a constantly applied torque on a stirrer, placedon a crucible into which the coal is charged. The ASTM standard (D2639-Plastometer) wasfollowed for this test. 5 gm sample of -0.425 mm particle size is packed around a stirrer in acylindrical steel crucible (21.5 mm ID x 35 mm length). As the coal is being heated from 300 °Cunder prescribed conditions at the rate of 3 °C / min, it begins to soften, and the torque weight causesthe stirrer to rotate in the sample. As the coal begins to soften andattained fluid state at higher temperature, the stirrer rotates more rapidly up to a maximum. As thetemperature continues to raise, the fluidity of coal starts to fall because of re-solidification of coaland subsequently the stirrer moves slowly until the coal is resolidified into coke and the stirrerstops. The speed of rotation of the stirrer in terms of dial divisions per minute (ddpm) and thecorresponding temperatures is recorded every minute.Fluidity tests have been performed with different semi soft and hard coking coal with addition of5 wt. % organic copolymer. Table 3 shows the significant improvement of coal fluidity for semisoft and hard coking coal after addition of polymeric additive.Table 3: Fluidity of coal before and after addition of polymer organic copolymerCarbonization studyA series of carbonization tests were carried to study the influence of the polymeric additive oncoke properties. Several carbonization tests were conducted in the 7-kg carbolite oven, understamp charging conditions. Water was added to the coal blend to obtain the desired value ofmoisture content. The coal cake was made inside a cardboard box keeping the bulk density 1150kg / m3. Tests were done with different blends. Initially test carried out with base blend (blend no1). Then, the hard-coking coal from the base blend is replaced by non-coking coal. Optimizedquantity of polymeric additive is mixed to maintain the coke quality. Before charging the coal cakeinto the oven, it was ensured that the empty oven temperature is 900±5°C. After 5 hr. ofcarbonization time, the hot coke was pushed out and quenched with water. The coke samples weretested for coke strength after reaction (CSR).Coke strength after reaction is studied using NSC method. In which 200 gm coke of 19-21 mmsize is heated in a reaction tube (78 mm diameter X 210 mm length) at 1100 °C for 2 hrs. and CO2is passed at a flow rate of 5 L / min. The percentage weight loss of coke during the above reactionis reported as the coke reactivity indices (CRI). This reacted coke is further tested by rotating in aI drum (127 mm diameter X 725 mm length) for 30 min at a speed of 20 rpm. The coke is thenscreened on 10 mm sieve and the % of + 10 mm fraction is reported as the coke strength afterreaction (CSR).Table 4: The blend composition and coking properties:In Table 4, blend 1 is the base blend with 16 % of non-coking coal (Coal I). In blend 2, 16 % ofnon-coking coal (Coal I) is used with addition of 0.7 % of organic copolymer. Results show thatthe CSR value is increased from 40.78 to 47. In blend 3, 16 % of non-coking coal (Coal I) is usedby addition of 1 % of organic copolymer and CSR value is increased to 50.36. Blend 4 is the baseblend with 8 % of non-coking coal (Coal J). In blend 5, 16 % of non-coking coal (Coal J) is usedwith addition of 0.7 % of organic copolymer to replace hard coking coal. Results show that theCSR value is increased from 48.31 to 49.07. In blend 6, 16 % of non-coking coal (Coal J) is usedwith addition of 1 % of organic copolymer to replace hard coking coal and CSR value is improvedto 49.43. This indicates that organic copolymer (at 0.7-1 wt % dosage) has significant potential toreplace ~ 16 % of hard coking coal by non-coking coal.Mechanism of phenol-melamine-urea based organic copolymerIt is well established that most significant range of temperature during coke making is 350-550°C. In this temperature region coal exists in the form of a plastic phase that finally resolidifies togive semi-coke. The organic copolymer plays the role of plasticizing agent which by reducing theviscosity of plastic phase facilitate the mobility and ordering of the molecules into liquid crystalsstructures leading to the development of the anisotropic texture of coke. The appropriatecharacteristics of additives are aromaticity, alkyl substitution, heteroatoms and reactive functionalgroup concentration and chemical compatibility with coal. The H-donor ability is one of theimportant characteristics of polymer for non-coking coal to coke manufacturing.In the present disclosure, effect of phenolic group and aromatic amine functional group present inpolymeric additive plays the crucial role for donation of hydrogen inside the coal matrix duringcoke carbonization process. The transferable hydrogens released from the methylene (-CH2) unitof polymeric additive plays the crucial role for polycondensation reaction of coal structure inplastic phase at 350-550 °C temperature, which is helpful for semi coke structure formation. Also,π-π stacking interaction between delocalized aromatic structure of coal and aromatic co-polymericstructure present in organic copolymer is key factor for coal-cake formation. Also, our synthesizedpolymer has amide functional moiety present in urea component of polymer, which stabilized theentire matrix through H-bonding of amide group with amine and hydroxyl functional group. Thisunique characteristic of organic copolymer is highly supportive to enhance the coal plasticproperty. This fact is established through our experimental study like CSN and fluidity test. Inaddition, organic copolymer has hydroxyl, amine and amide reached functional group, which formH-bonding site with coal structure, resulting inhibition of volatilization of small aromatic clusterspresent in poor-coking coal. Also, methylene bridge moiety present in additive structure providesdesired free radical binding site and it accelerates the re-aromatization process of coal structure atplastic phase through free radical mechanism, resulting structural ordering of semi-coke. Insummary, presence of -CH2 bridge polymeric structural chemistry, existence of phenolic -OHgroup and aromatic amine functional group of melamine unit and amide functional moiety of ureacomponent of organic copolymer plays the crucial role for carbonization of non-coking coal.

Claims

1. An organic copolymer having following chemical formula:

2. The organic copolymer as claimed in claim 1, wherein the viscosity of the copolymer is in a range of 15-50 cP.

3. The organic copolymer as claimed in claim 1, wherein the solid content of the copolymer is weight 50-55 %.

4. A method for preparing the organic copolymer as claimed in claim 1, wherein the method comprising: (a) treating phenol with formaldehyde monomer in presence of ammonia solution at 40-50°C temperature for 0.5-1 hr to obtain a reaction mixture; (b) adding an alkali metal catalyst into the reaction mixture of step (a); (c) adding melamine into the reaction mixture of step (b) at a temperature of 85-90 °C; and (d) adding urea precursor into the reaction mixture of step (c) at a temperature of 80-85 °C for 1-2 hr to obtain the copolymer.

5. The method for preparing the organic copolymer as claimed in claim 4, wherein the alkali metal catalyst is selected from sodium hydroxide and potassium hydroxide.

6. The method for preparing the organic copolymer as claimed in claim 5, wherein the alkali metal catalyst is sodium hydroxide.

7. The method for preparing the organic copolymer as claimed in claim 4, wherein phenol is in range of 8-12 wt %.

8. The method for preparing the organic copolymer as claimed in claim 4, wherein formaldehyde monomer is in a range of 58-62 wt %.

9. The method for preparing the organic copolymer as claimed in claim 4, wherein melamine is in a range of 14-16 wt %.

10. The method for preparing the organic copolymer as claimed in claim 4, wherein urea precursor is in a range of 14-16 wt %.

11. The method for preparing the organic copolymer as claimed in claim 4, wherein pH of the reaction mixture in presence of ammonia solution is 5.7 to 6.4.

12. The method for preparing the organic copolymer as claimed in claim 4, wherein pH after adding alkali metal catalyst is 8.5 to 9.

13. A blend for metallurgical coke making wherein the blend comprises: d) one or more non-coking coal; e) one or more coking coal; and f) the organic copolymer having the following chemical formula:

14. The blend as claimed in claim 13, wherein one or more non-coking coal is 5-20 wt. %.

15. The blend as claimed in claim 13, wherein one or more coking coal is 80-95 wt.%.

16. The blend as claimed in claim 13, wherein the organic copolymer is 0.7 - 1 wt. %.

17. A method for metallurgical coke production comprising the steps of: (a) preparing an organic polymer derived from phenol, melamine and urea precursor, formaldehyde-based monomer in presence of alkali metal catalyst; and (b) mixing the organic polymer in a specific dosage with specific coal blend for carbonization study.

18. The method for metallurgical coke production as claimed in claim 17, wherein organic copolymer having the following chemical formula:

19. The method for metallurgical coke production as claimed in claim 17, wherein alkali metal catalyst is sodium hydroxide or potassium hydroxide.