Decorative glass article
A lead-free decorative glass with high refractive index and low Abbe number, using specific oxides, addresses the lack of shine and iridescent glow in existing lead-free crystal glass, offering improved decorative properties.
Patent Information
- Application Number
- JP2024116770
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2019-04-05
- Filing Date
- 2024-07-22
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2040-02-28
AI Technical Summary
Lead-free crystal glass lacks sufficient shine and iridescent glow, making it less effective as a decorative item.
A decorative glass article with a refractive index of 1.9 or more and an Abbe number of 40 or less, composed of specific oxides like La2O3, Nb2O5, B2O3, Al2O3, ZrO2, and TiO2, to enhance light reflection and dispersion, thereby improving shine and fire.
The glass article achieves enhanced shine and fire, suitable for decorative uses such as jewelry and ornaments, while being lead-free and transparent.
Smart Images

Figure 2024133342000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a decorative glass article suitable for use as an ornament such as a ring, a pendant, an earring, or a bracelet. [Background technology]
[0002] According to the Japan Glass Manufacturers Association, crystal glass is defined as "glass containing lead oxide as its main component, or potassium oxide, barium oxide, titanium oxide, etc. as its main components, with high transparency, a refractive index nd of 1.52 or more, and characterized by a beautiful glossy shine and a clear tone." These crystal glasses excel in brilliance, transparency, resonance, weightiness, and workability, and are used for decorative items (jewelry, artwork, tableware, etc.).
[0003] However, since crystal glass containing lead is harmful to the human body and is easily scratched, efforts are being made to develop crystal glass that is substantially free of lead (Patent Documents 1 and 2). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent No. 2588468 [Patent Document 2] Patent No. 4950876 Summary of the Invention [Problem to be solved by the invention]
[0005] The lead-free crystal glass described in Patent Document 2 does not have sufficient shine to be used as an ornament. In addition, the rainbow-colored shine known as "fire" tends to be weak.
[0006] In view of the above, an object of the present invention is to provide a decorative glass article having excellent brilliance and fire. [Means for solving the problem]
[0007] The decorative glass article of the present invention is characterized by being substantially free of lead oxide, having a refractive index of 1.9 or more, and an Abbe number of 40 or less. Since the glass article of the present invention has a high refractive index, the difference in refractive index between the inside and outside (atmosphere) of the glass article is large, and light is easily reflected inside the glass article. As a result, it is easy to obtain sufficient brilliance as a decorative glass article. In addition, since the glass article of the present invention has a small Abbe number and high dispersion, fire is easily generated. In this specification, "substantially free of lead oxide" means that it is not intentionally contained in the glass composition, and does not exclude the inclusion of unavoidable impurities. Objectively, it means that the content is less than 0.1% in mol%.
[0008] The decorative glass article of the present invention preferably has a coloring degree λ5 of 395 or less. This allows visible light to easily pass through, so that the glass article tends to be colorless and transparent. The "coloring degree λ5" refers to the shortest wavelength (nm) at which the light transmittance is 5% in the transmittance curve at a thickness of 10 mm.
[0009] The decorative glass article of the present invention preferably contains bismuth oxide in an amount of 30% or less by mole. If bismuth oxide is contained, the glass article tends to be excessively colored and has poor fire. Therefore, by reducing the bismuth oxide content, it becomes easier to obtain a glass article with excellent fire.
[0010] The decorative glass article of the present invention contains, in mole percent, 0-63% La2O3, 0-40% B2O3, 0-50% Al2O3, 0-40% ZrO2, 50-80% Nb2O, 0-60% Gd2O3, and 50-60% Ta2O, and preferably contains 0.1-100% La2O3+Nb2O5+Ta2O5+Gd2O3. By defining the glass composition in this way, it becomes easier to obtain a glass article having the desired optical constants.
[0011] The decorative glass article of the present invention preferably further contains, in mol %, 20 to 85% of TiO.
[0012] The decorative glass article of the present invention is preferably subjected to chamfering, which makes it easier for light to be reflected inside the glass article, thereby making it possible to enhance the brilliance.
[0013] The decorative glass article of the present invention is suitable as a pseudo-jewel.
[0014] The decorative article of the present invention is characterized by comprising the decorative glass article described above. Effect of the Invention
[0015] According to the present invention, a decorative glass article having excellent brilliance and fire can be provided. [Brief description of the drawings]
[0016] [Figure 1] 1 is a plan view of Samples No. 8, 34, and 35 in the examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] The decorative glass article of the present invention has a refractive index (nd) of 1.9 or more, preferably 2.0 or more, 2.1 or more, 2.2 or more, and particularly preferably 2.25 or more. This increases the difference in refractive index between the inside and outside (atmosphere) of the glass article, making it easier for light to be reflected inside the glass article. As a result, it becomes easier to obtain sufficient brightness as a decorative glass article. There is no particular upper limit to the refractive index, but if it is too high, vitrification becomes unstable, so it is preferably 2.6 or less, 2.5 or less, and particularly preferably 2.4 or less.
[0018] The Abbe number (νd) of the decorative glass article of the present invention is preferably 42 or less, 40 or less, 35 or less, 30 or less, and particularly preferably 25 or less. In this way, the glass article becomes highly dispersed and fire is easily generated. Although there is no particular restriction on the lower limit of the Abbe number, if it is too small, vitrification becomes unstable, so it is preferably 10 or more, and particularly preferably 15 or more.
[0019] The composition of the decorative glass article of the present invention is not particularly limited as long as it has the above optical properties, but examples thereof include, in mol%, La2O30-63%, B2O30-40%, Al2O30-50%, ZrO20-40%, Nb2O50-80%, Gd2O30-60, Ta2O50-60%, and La2O3+Nb2O5+Ta2O5+Gd2O30.1-100%. The reason for limiting the glass composition in this way is explained below. In the following explanation of the content of each component, "%" means "mol%" unless otherwise specified.
[0020] La2O3 is a component that forms a glass skeleton and increases the refractive index without decreasing the transmittance. It also has the effect of improving weather resistance. The content of La2O3 is preferably 0 to 63%, 0 to 60%, and particularly preferably 1 to 55%. If the content of La2O3 is too low, it becomes difficult to obtain the above effects. On the other hand, if the content of La2O3 is too high, it becomes difficult to vitrify.
[0021] Nb2O5 is a component that has a large effect of increasing the refractive index, lowering the Abbe number and providing high dispersion. It also has the effect of widening the vitrification range. The content of Nb2O5 is 0 to 80%, preferably 1 to 78%, 5 to 75%, 10 to 73%, and particularly preferably 20 to 70%. If the content of Nb2O5 is too high, vitrification becomes difficult.
[0022] Gd2O3 is a component that increases the refractive index. It also has the effect of improving weather resistance. However, if the Gd2O3 content is too high, vitrification becomes difficult. Therefore, the Gd2O3 content is preferably 0 to 60%, 0.1 to 60%, 1 to 50%, 2 to 45%, and particularly preferably 3 to 40%.
[0023] Ta2O5 is a component that has a large effect of increasing the refractive index. However, if the content of Ta2O5 is too high, vitrification becomes difficult and the raw material cost tends to increase. Therefore, the content of Ta2O5 is preferably 0 to 60%, 0.1 to 60%, 1 to 50%, 2 to 45%, and particularly preferably 3 to 40%.
[0024] B2O3 is a component that forms a glass skeleton and expands the vitrification range. However, if the content of B2O3 is too high, the refractive index decreases and it becomes difficult to obtain the desired optical properties. Therefore, the content of B2O3 is preferably 0 to 40%, 0.1 to 40%, 1 to 30%, 2 to 25%, and particularly preferably 3 to 20%.
[0025] Al2O3 is a component that forms a glass skeleton and expands the vitrification range. However, if the content of Al2O3 is too high, the refractive index decreases and it becomes difficult to obtain the desired optical properties. Therefore, the content of Al2O3 is preferably 0 to 50%, 0.1 to 40%, 1 to 30%, 2 to 25%, and particularly preferably 3 to 20%.
[0026] ZrO2 is a component that increases the refractive index. In addition, since it forms a glass skeleton as an intermediate oxide, it has the effect of widening the vitrification range. However, if the content of ZrO2 is too high, vitrification becomes difficult and the melting temperature becomes too high. Therefore, the content of ZrO2 is preferably 0 to 40%, 0.1 to 40%, 1 to 30%, 2 to 25%, and particularly preferably 3 to 20%.
[0027] The content of La2O3+Nb2O5+Ta2O5+Gd2O3 is preferably 0.1 to 100%, more preferably 10 to 95%, and particularly preferably 20 to 90%. If the content of La2O3+Nb2O5+Ta2O5+Gd2O3 is too small, it becomes difficult to obtain the desired refractive index and Abbe number.
[0028] The decorative glass article of the present invention may contain the following components in addition to the above components.
[0029] TiO2 is a component that is highly effective in increasing the refractive index, and also has the effect of increasing chemical durability. It also has the effect of decreasing the Abbe number and increasing dispersion. The TiO2 content is preferably 0-85%, 0.1-83%, 5-80%, 10-80%, 30-77%, and particularly preferably 50-75%. If the TiO2 content is too high, the absorption edge shifts to the long wavelength side, and the transmittance of visible light (especially visible light in the short wavelength range) tends to decrease. In addition, vitrification becomes difficult.
[0030] The glass used in the decorative glass article of the present invention may contain coloring components such as transition metal oxides and rare earth oxides other than those mentioned above in order to impart a desired color tone. Specifically, transition metal oxides include Cr2O3, Mn2O3, Fe2O3, CoO, NiO, CuO, V2O5, MoO3, RuO2, etc. Rare earth oxides include CeO2, Nd2O3, Eu2O3, Tb2O3, Dy2O3, Er2O3, etc. These transition metal oxides and rare earth oxides may be contained alone or in combination of two or more. The content of these transition metal oxides and rare earth oxides (total amount when two or more are contained) is preferably 0 to 5%, 0.001 to 3%, 0.01 to 2%, and particularly 0.02 to 1%. Note that, depending on the components contained, the coloring may be too strong, the visible transmittance may decrease, and the desired brilliance and fire may not be obtained. In this case, the content of the transition metal oxides and rare earth oxides may be less than 1%, 0.5% or less, or even 0.1% or less.
[0031] In addition to the above components, the glass used in the decorative glass article of the present invention may contain SiO2, ZnO, MgO, CaO, SrO, BaO, etc., each in an amount of 10% or less, in order to broaden the range of vitrification.
[0032] However, if bismuth oxide (Bi2O3) is contained, the glass article tends to be excessively colored and have poor fire. Therefore, the content of bismuth oxide in the decorative glass article of the present invention is preferably 30% or less, 20% or less, 10% or less, and particularly preferably 1% or less, in mole percent, and most preferably is substantially free of bismuth oxide.
[0033] The decorative glass article of the present invention is substantially free of lead oxide, which is harmful to the human body.
[0034] The decorative glass article of the present invention actively contains components that expand the vitrification range, such as La2O3, Nb2O5, and B2O3, which suppresses inappropriate crystallization during glass production and makes it easy to increase the size of the glass article (for example, a diameter of 2 mm or more, 3 mm or more, 4 mm or more, and particularly 5 mm or more).
[0035] The coloring degree λ5 of the glass used in the decorative glass article of the present invention is preferably 395 or less, 390 or less, 380 or less, and particularly preferably 370 or less. This makes it easier to obtain colorless and transparent glass because visible light can easily pass through it. It also makes it easier to increase the brilliance and fire.
[0036] The higher the density of the glass used in the decorative glass article of the present invention, the more profound the appearance becomes, and the more luxurious the decorative glass article (particularly the glass article for jewelry) is, which is preferable. The density of the glass is, for example, 3 g / cm 3 More than 4g / cm 3 Above, especially 5g / cm 3 More preferably, it is equal to or greater than this.
[0037] The decorative glass article of the present invention can be used for decorative purposes such as jewelry, art, tableware, etc. For example, it can be attached as a pseudo-gemstone to ornaments (jewelry) such as rings, pendants, earrings, bracelets, etc. The shape of the decorative glass article is not particularly limited, and examples thereof include a sphere, an ellipse, a polyhedron, etc.
[0038] The decorative glass article of the present invention is preferably subjected to chamfering such as brilliant finishing, which makes it easier for light to be reflected inside the glass article, enhancing the brilliance and making it particularly suitable as a pseudo-gemstone. EXAMPLES
[0039] The decorative glass article of the present invention will be described in detail below using examples, but the present invention is not limited to the following examples.
[0040] Tables 1 to 4 show examples of the present invention (Nos. 1 to 33) and comparative examples (Nos. 34 to 35).
[0041] [Table 1]
[0042] [Table 2]
[0043] [Table 3]
[0044] [Table 4]
[0045] First, raw materials were mixed to prepare raw material batches so as to obtain the glass compositions shown in the table. The obtained raw material batches were melted until homogeneous, and then rapidly cooled to obtain glass samples. The melting temperatures were 1500 to 2000°C for samples No. 1 to 33, and 1400 to 1500°C for samples No. 34 to 35. The obtained glass samples were annealed near the glass transition temperature (450 to 700°C), and then the refractive index (nd), Abbe number (νd), and coloring degree (λ5) were measured and the appearance (brilliance, fire, and color tone) were evaluated by the following methods.
[0046] The refractive index (nd) and Abbe number (νd) were measured by polishing the glass sample at a right angle and using a KPR-2000 (Shimadzu Corporation). The refractive index (nd) was evaluated using the measured value for the d-line (587.6 nm) of a helium lamp. The Abbe number (νd) was calculated from the above-mentioned d-line refractive index and the values of the F-line (486.1 nm) and C-line (656.3 nm) of a hydrogen lamp, using the formula Abbe number (νd) = {(nd-1) / (nF-nC)}.
[0047] The coloring degree (λ5) was determined by measuring the spectral transmittance of a glass sample polished to a thickness of 10±0.1 mm, and adopting the wavelength showing a transmittance of 5% in the obtained transmittance curve. The spectral transmittance was measured using a V-670 manufactured by JASCO Corporation.
[0048] Appearance evaluation was performed as follows. First, brilliant processing was performed on each sample so that the planar shape of each sample was approximately 5 to 7 mmφ. Next, the processed glass samples were visually evaluated for brilliance and fire under a fluorescent light source. The evaluation was performed on a four-point scale as shown below. In addition, color tone was evaluated visually. Planar photographs of samples No. 8, 34, and 35 are shown in Figure 1.
[0049] [Shining] ◎: Looks shiny and has a strong shine. ○: Looks shiny. △: It looks slightly shiny. ×: Almost no shine (same as a glass window).
[0050] [fire] ◎: Iridescent (various colors) sparkle can be seen. ○: Iridescent glow is visible, but the number of colors is limited. △: A slight rainbow glow is visible. ×: The rainbow color is barely visible.
[0051] As is clear from Tables 1 to 4, the example samples Nos. 1 to 33 had refractive indices of 1.90 or more and Abbe numbers of 41.4 or less, and were good in brilliance and fire. On the other hand, the comparative sample samples Nos. 34 and 35 had low refractive indices of 1.56 or less and high Abbe numbers of 45 or more, and were therefore poor in brilliance and fire.
Claims
1. A decorative glass article, which is substantially free of lead oxide, has a refractive index of 1.9 or more, and an Abbe number of 42 or less.
2. Coloring degree λ 5 2. The decorative glass article according to claim 1, wherein the hardness is 395 or less.
3. 3. The decorative glass article according to claim 1, wherein the content of bismuth oxide is 30% or less in mole percent.
4. In mole percent, La 2 O 3 0-63%, B 2 O 3 0-40%, Al 2 O 3 0-50%, ZrO 2 0-40%, Nb 2 O 5 0-80%, Gd 2 O 3 0-60, Ta 2 O 5 0-60%, La 2 O 3 +Nb 2 O 5 +Ta 2 O 5 +Gd 2 O 3 4. The decorative glass article according to claim 1, wherein the content is 0.1 to 100%.
5. Further, in mol%, TiO 2 5. The decorative glass article according to claim 4, characterized in that it contains 0 to 85%.
6. 6. The decorative glass article according to claim 1, which is subjected to a chamfering process.
7. 7. The decorative glass article according to claim 1, which is a pseudo-gemstone.
8. A decorative article comprising the decorative glass article according to any one of claims 1 to 7.
Citation Information
Patent Citations
JP1975023842A
Microspheres comprising titania and bismuth oxide
JP2007501183A
Titanium based oxide glass and method of manufacturing the same
JP2008069047A
Methods of Making Pavement Road Markings, Reflective Elements and Microspheres
JP2009516102A
Optical glass and method for producing the same
JP2017132656A