Deck slab and design method of deck slab

The deck slab design addresses cracking issues by optimizing reinforcing bar ratios based on load specifications, ensuring effective crack control and efficient material use.

JP2024135158APending Publication Date: 2024-10-04NIPPON STEEL METAL PROD CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2023045704
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-22
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Conventional deck slabs, particularly of the reverse and intermediate enclosing types, experience increased stress on the concrete surface layer due to thinner cross sections, leading to higher risks of cracking, as existing designs do not account for specific stress distributions and reinforcing bar specifications.

Method used

A deck slab design that incorporates reinforcing bars arranged above the beams with a reinforcing bar ratio determined by the equation y = (x-3.9)/6.4, where y is the reinforcing steel ratio and x is the generated or design load, ensuring adequate reinforcement to control cracks.

Benefits of technology

The design effectively controls cracks by optimizing the reinforcing bar ratio, reducing material usage and construction effort while maintaining deck slab quality, even in thinner concrete sections.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024135158000001_ABST
    Figure 2024135158000001_ABST
Patent Text Reader

Abstract

To provide a deck slab capable of controlling cracks by arranging a necessary and sufficient amount of reinforcing bars with respect to a predetermined generated load or a design load, and a deck slab.SOLUTION: In a deck slab 100, a reinforcement ratio of a cross section in the span direction D1 of the deck slab 100 is set to be equal to or more than a value that is given by a formula (1). In order to obtain the reinforcement rebar ratio for suppressing the crack width to a desired size with respect to the generated load or the design load of the deck slab 100, at least the required rebar ratio can be calculated by substituting the generated load or the design load x into Equation (1). It is possible to control cracks by arranging a necessary and sufficient amount of reinforcing bars with respect to a predetermined generated load or a design load, Accordingly, since the amount of reinforcement becomes a necessary minimum amount, it is possible to reduce the amount of steel material and the labor of bar arrangement construction. In addition, cracks can be appropriately controlled, and the quality of the deck slab 100 as a floor can be ensured. Y=(x-3.9) / 6.4 (1)SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a deck slab and a method for designing a deck slab. [Background technology]

[0002] A conventional deck slab is described in Non-Patent Document 1. This deck slab includes a deck plate and concrete poured on the deck plate. Reinforcement bars are placed in the concrete on the upper side of the beam. [Prior art documents] [Non-patent literature]

[0003] [Non-Patent Document 1] "Deck Plate Floor Structure Design and Construction Standards: 2018 (Supervised by the Building Research Institute, National Research and Development Agency)" Summary of the Invention [Problem to be solved by the invention]

[0004] Here, the reverse enclosing type (see Figure 2) or the intermediate enclosing type (see Figure 5(b)) may be adopted as the deck slab. In these reverse enclosing and intermediate enclosing types, the concrete thickness above the beam is thinner than that of the conventional open type (see Figure 5(a)). Therefore, the effective cross section that can bear the negative bending stress generated near the beam is smaller, so the stress of the concrete surface layer increases and the risk of cracking increases. For example, Figure 1 shows the generated moment acting on the deck slab. At the point where the deck slab is supported by the beam from below, the peak MT of the generated moment occurs on the negative side, so negative bending instead of positive bending occurs at that point, and tensile force acts on the concrete. This causes cracks CR to occur in the surface layer.

[0005] Similar issues exist not only in reverse enclosing and intermediate enclosing types, but also in open type cross sections, and measures are sometimes taken to place reinforcing steel bars on the beams. However, the amount of reinforcing bars and anchorage length follow uniform specifications, and quantitative design according to existing stresses is not carried out.

[0006] Furthermore, the deck standards do not include specifications that assume reverse-enclosed or intermediate-enclosed decks, where the concrete thickness above the beams is thin. The Japan Society of Civil Engineers' Standard Specifications for Concrete [Structural Performance Verification Edition] specifies that the allowable crack width in "general environments" is 0.005 x cmm (c: cover thickness (mm)) when deformed reinforcing bars or ordinary round steel bars are used, and for a commonly used cover thickness of 30 mm, the allowable crack width is 0.15 mm. As shown in the analysis results below, in reverse-enclosed specifications, even if reinforcement is placed with a reinforcing bar ratio exceeding 0.2%, the crack width exceeds 0.15 mm, and it was necessary to determine the appropriate amount of reinforcement.

[0007] The present invention has been made to solve such problems, and has an object to provide a deck slab and a design method for a deck slab that can control cracks by placing a necessary and sufficient amount of rebar for a specified generated load or design load. [Means for solving the problem]

[0008] The deck slab of the present invention is a deck slab having a deck plate and concrete placed on the deck plate, in which reinforcing bars are arranged inside the concrete on the upper side of the beams and around the upper periphery of the beams, and the reinforcing bar ratio of the cross section in the span direction of the deck slab is equal to or greater than the value given by the following formula (1). y=(x-3.9) / 6.4 …(1) y is the reinforcement ratio (%) and x is the generated load or design load (kN / m 2 ).

[0009] In the deck slab according to the present invention, the reinforcement ratio of the cross section in the span direction of the deck slab is set to be equal to or greater than the value given by formula (1). In this case, in order to obtain a reinforcement ratio for suppressing the crack width to a desired size for the deck slab's generated load or design load, at least the required reinforcement ratio can be calculated by substituting the generated load or design load x into formula (1). As described above, it is possible to control cracks by arranging a necessary and sufficient amount of reinforcement for a predetermined generated load or design load. This results in a minimum amount of reinforcement, which can reduce the amount of steel material and the labor required for reinforcing bar arrangement. In addition, cracks can be appropriately controlled to ensure the quality of the deck slab as a floor.

[0010] The cover thickness of rebar on beams may be up to 40mm, provided that the rebar provides adequate crack control.

[0011] The deck slab may be of the reverse enclosing type or intermediate enclosing type. Even with the reverse enclosing type or intermediate enclosing type deck plate, the necessary and sufficient amount of reinforcing bars can be obtained.

[0012] Load capacity: 8.9kN / m 2 In this case, it is possible to prevent the load from becoming too large.

[0013] The diameter of reinforcing bars on beams may be greater than D10 and the spacing may be less than 300mm. This allows the reinforcing bars to adequately control cracks.

[0014] The design method for a deck slab according to the present invention is a design method for a deck slab having a deck plate and concrete provided on the deck plate, in which reinforcing bars are arranged inside the concrete on the upper side of the beams and around the upper periphery of the beams, and the reinforcing bar ratio of the cross section in the span direction of the deck slab may be equal to or greater than the value given by the following formula (1). y=(x-3.9) / 6.4 …(1) y is the reinforcement ratio (%) and x is the generated load or design load (kN / m 2 ).

[0015] According to the deck slab design method of the present invention, it is possible to obtain the same functions and effects as those of the above-mentioned deck slab. Effect of the Invention

[0016] According to the present invention, it is possible to provide a deck slab and a method for designing a deck slab that can control cracks by arranging a necessary and sufficient amount of reinforcing bars for a specified design load. [Brief description of the drawings]

[0017] [Figure 1] FIG. 2 is a schematic cross-sectional view of a deck slab according to an embodiment of the present invention. [Diagram 2] FIG. 2 is an enlarged cross-sectional view of the deck slab as viewed from the width direction of the deck slab. [Diagram 3] 3 is a cross-sectional view in the span direction of the deck slab taken along lines IIIa-IIIa, IIIb-IIIb, and IIIc-IIIc shown in FIG. 2. [Figure 4] FIG. 2 is a top view of reinforcing steel bars. [Diagram 5] FIG. 13 is a diagram showing a model for performing verification by simulation. [Figure 6] FIG. 13 is a diagram showing a verification result by simulation. [Figure 7] FIG. 13 is a diagram showing a verification result by simulation. [Figure 8] FIG. 13 is a diagram showing a model for performing verification by simulation. [Figure 9] 1 is a table showing specifications of a model for performing verification by simulation. [Figure 10] 13 is a graph showing a verification result by simulation. [Figure 11] 13 is a graph showing a verification result by simulation. [Figure 12]13 is a table showing verification results by simulation. [Figure 13] 13 is a graph showing a verification result by simulation. [Figure 14] 13 is a graph showing a verification result by simulation. [Figure 15] 13 is a table showing an evaluation formula. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0018] Hereinafter, preferred embodiments of the present invention will be described with reference to the drawings.

[0019] Fig. 1 is a schematic cross-sectional view of a deck slab 100 according to an embodiment of the present invention. As shown in Fig. 1, the deck slab 100 is provided as a floor slab in a building. The deck slab 100 is supported at its four edges by beams 2. The beams 2 on the four sides are each supported by a column 3. Also, a beam 2 (two beams in this example) may be provided midway between the beams 2 corresponding to a pair of opposing sides.

[0020] The span direction D1 and width direction D2 of the deck slab 100 will be described. The direction in which the peaks 6a and valleys 6b of the deck plate 6 of the deck slab 100 extend is the span direction D1 of the deck slab 100, and the direction in which the peaks 6a and valleys 6b are aligned is the width direction D2 of the deck slab 100. In the following description, when simply referred to as "span direction" and "width direction", it means the span direction D1 and width direction D2 of the deck slab 100. FIG. 2 is an enlarged cross-sectional view of the deck slab 100 as viewed from the width direction D2. FIGS. 3(a), (b), and (c) are cross-sectional views along the lines IIIa-IIIa, IIIb-IIIb, and IIIc-IIIc shown in FIG. 2. As shown in FIG. 2, the deck slab 100 has a deck plate 6 and concrete 7 provided on the deck plate 6.

[0021] As shown in Figures 3(a) and (b), the deck plate 6 has alternating peaks 6a and valleys 6b in the width direction D2. The peaks 6a are provided so as to protrude upward from the bottom surfaces of the valleys 6b. The peaks 6a extend parallel to each other in the span direction D1 while being spaced apart from each other in the width direction D2. The peaks 6a form both side walls of the valleys 6b.

[0022] The concrete 7 is poured onto the deck plate 6. The concrete 7 is filled inside the valleys 6b of the deck plate 6 up to a position higher than the upper surfaces of the peaks 6a. As a result, the concrete 7 has an upper surface that extends in the span direction D1 and width direction D2 above the deck plate 6. This upper surface becomes the upper surface 100a of the deck slab 100. The thickness t of the concrete 7 on the peaks 6a of the deck plate 6 is 50 mm to 100 mm.

[0023] 2 and 3, crack expansion prevention bars 8 are arranged inside the concrete 7. The crack expansion prevention bars 8 are mesh members extending parallel to the span direction D1 and width direction D2. The crack expansion prevention bars 8 are arranged between the peaks 6a and the upper surface 100a.

[0024] As shown in FIG. 2, reinforcing bars 9 are arranged inside the concrete 7 on the upper side of the beam 2. The reinforcing bars 9 extend in the span direction D1. The reinforcing bars 9 extend so as to protrude from both sides of the beam 2 in the span direction D1. The length of the reinforcing bars 9 that protrude from the beam 2 is referred to as the anchoring length. The reinforcing bars 9 are arranged between the peaks 6a and the upper surface 100a. The reinforcing bars 9 are arranged at a predetermined pitch in the width direction D2 (see FIG. 4).

[0025] The reinforcing steel bars may be shorter than the standardized length. The standard may be, for example, a standard that conforms to "Standard Specifications for Building Construction and Commentary JASS5 Reinforced Concrete Construction 2018". For example, the length of the straight anchorage may conform to 40d (d: rebar diameter (mm)).

[0026] In the area of ​​the concrete 7 supported by the beam 2, a reduced thickness portion 12 is formed in which the concrete thickness is thinner than that of the general portion 11 in the other area E1. In this embodiment, in the area of ​​the concrete 7 supported by the beam 2 and the area E2 including the periphery of the area supported by the beam 2, the reduced thickness portion 12 is formed. The deck plate 6 includes an oblique side portion 13 provided in the span direction D1 and a flat portion 14. The oblique side portion 13 is provided on both sides of the beam 2 in the span direction D1. The oblique side portion 13 is inclined upward from the end of the general portion 11 (area E1) on the beam 2 side toward the beam 2 side in the span direction D1. The flat portion 14 is formed between the upper ends of the pair of oblique side portions 13. The flat portion 14 is disposed on the upper surface of the upper flange of the beam 2.

[0027] As shown in FIG. 3(a), the thickness of the concrete 7 in the general portion 11 is "t1". As shown in FIG. 3(b), the valley portion 6b of the oblique side portion 13 is disposed at a higher position than the valley portion 6b of the general portion 11. As a result, the thickness of the concrete 7 in the oblique side portion 13 is thinner than the thickness t1 of the concrete 7 in the general portion 11. As shown in FIG. 3(c), the flat portion 14 is disposed at a higher position than the valley portion 6b of the general portion 11. In this embodiment, the flat portion 14 is disposed at the same height as the peak portion 6a of the general portion 11. As a result, the thickness t2 of the concrete 7 in the flat portion 14 is thinner than the thickness t1 of the concrete 7 in the general portion 11 (see also FIG. 2). The deck slab 100 of this embodiment is called a reverse enclosing type.

[0028] Here, the reinforcement ratio of the cross section (cross section in FIG. 2) in the span direction D1 of the deck slab 100 may be set to be equal to or greater than the value given by the following formula (1): y is the reinforcement ratio (%), and x is the generated load or design load (kN / m 2 The reinforcing bar ratio is defined as the ratio between the cross-sectional area of ​​concrete and the cross-sectional area of ​​reinforcing bar. The upper limit of the reinforcing bar ratio y is not particularly limited, but may be greater than 0.353% and greater than 0.881%. y=(x-3.9) / 6.4 …(1)

[0029] For example, a φ6-100x100 crack expansion prevention bar (reinforced concrete cross-sectional area 282.7 mm) is installed on a deck slab with a concrete thickness of 80 mm on a beam. 2 / m) and the reinforcing steel bars on the D13 beam are 300 mm (reinforcing steel cross-sectional area 422.3 mm 2 / m), the reinforcement ratio can be calculated as y = (282.7 + 422.3) / (80 × 1000) ≒ 0.0081 (= 0.881%).

[0030] The cover thickness H1 of the reinforcing bar 9 on the beam may be 40mm or less, taking into account the standard cover thickness of 30mm for floors and a construction error of 10mm. The cover thickness H1 is determined by the vertical dimension between the top end of the reinforcing bar 9 and the top surface of the concrete 7. The thickness H1 may be set to 25mm or more, the minimum reinforcing bar clearance value in the "Guidelines for Reinforced Concrete Construction and Commentary (Architectural Institute of Japan)", or it may be set to 20mm or more, the minimum cover thickness in the "Standard Specifications for Building Construction JASS5 Reinforced Concrete Construction". The live load is 8.9kN / m 2 It may be less than 6.0 kN / m 2 It may be less than 3.0kN / m 2 It may be more than that.

[0031] The reinforcing bar diameter of the reinforcing bars 9 on the beam 2 may be greater than D10, and may be equal to or greater than D13. The reinforcing bar arrangement interval P1 (see FIG. 4) of the reinforcing bars 9 may be equal to or less than 300 mm, and may be equal to or less than 200 mm.

[0032] The deck slab 100 may have a configuration shown in Fig. 5(b). The deck slab 100 shown in Fig. 5(b) is obtained by adding an oblique side portion 26 to the upper side of the deck slab 100 in Fig. 2. The oblique side portion 26 slopes downward from the end of the general portion 11 on the beam 2 side toward the beam 2 side in the span direction D1. This type of deck slab 100 is called an intermediate encro type.

[0033] Next, the verification content for deriving the above formula (1) will be explained. In this verification, in addition to the inverted enclosing type deck plate shown in Fig. 2, an open type deck slab 100 shown in Fig. 5(a) is used. The open type in Fig. 5(a) has a configuration in which the end of the deck plate 6 without a slant portion is placed on the beam. In the open type, the concrete 7 on the beam has the same thickness as the other areas.

[0034] As shown in Fig. 6, the unreinforced deck slab and the framework (columns, girders, and sub-girders) were modeled and the design load level (6000N / m 2 Fig. 6(a) shows the results of an FEM analysis (span direction D1, surface layer stress contour diagram) when a uniformly distributed load of 100 mm (0.2 in) is applied. Fig. 6(a) shows the results for the open type, and Fig. 7(b) shows the results for the reverse-enclosed type. This model does not include the crack prevention bars 8 and the reinforcing bars 9 on the beams. It can be seen that the stress on the beams is greater for the reverse-enclosed type than for the open type (see A1 in the figure).

[0035] Next, Fig. 7 shows a graph plotting the stress values ​​of each node in the open type model and the inverted enclosing type model. The results for the open type are shown in graph GA1, and the results for the inverted enclosing type are shown in GA2. In the figures, the hatched squares indicate minor beams, and the dotted squares indicate major beams. As shown in Fig. 7, there is a large difference in the stress in the span direction D1 (open type is 4.79 N / mm 2 The effect of the smaller cross section resisting negative bending on the girder was confirmed. If the above generated stress exceeds the allowable tensile stress of the concrete 7, cracks will occur.

[0036] Next, crack prevention bars 8 and reinforcing bars on the beams 9 were added to the model, and an elastic-plastic analysis was carried out using load increments to quantitatively compare the occurrence and progression of cracks. An overview of the common models is shown in Figure 8. Figures 8(a) and (b) are overall views of the model with columns, main beams, sub-beams, and deck slabs. Figure 8(c) is an enlarged view of the frame model. The columns have beam elements, the main beams have shell elements, the sub-beams have shell elements, and the studs have beam elements. Figure 8(d) shows a model of reinforcing bars for crack prevention bars, on beams, and around columns. The reinforcing bars have truss elements, and the boundary condition is complete adhesion to the concrete.

[0037] Four models, Models No. 1 to 4, were prepared as analytical models of the deck slab 100. Model No. 1 was an open type without reinforcing bars 9. Model No. 2 was an inverted enclosed type without reinforcing bars 9. Model No. 3 was an inverted enclosed type with reinforcing bars 9. In Model No. 3, the pitch of the reinforcing bars 9 was set to 300 mm. Model No. 4 was an inverted enclosed type with reinforcing bars 9. In Model No. 4, the pitch of the reinforcing bars 9 was set to 200 mm.

[0038] Figure 9 shows the conditions of each model. In models No. 1 to 4, the thickness dimension L1 of the concrete 7 relative to the top surface of the deck plate 6 was 80 mm, the thickness dimension L2 of the deck plate 6 was 75 mm, and the cover thickness H2 of the crack expansion prevention reinforcement 8 was 30 mm (see Figure 2). In models No. 1 to 4, the crack expansion prevention reinforcement 8 was "φ6mm-100mm x 100mm". The girder was "H-700mm x 300mm x 13mm x 24mm". In model No. 3, the reinforcing bar 9 was "D13@300mm" and the cover thickness H1 (see Figure 2) was 30 mm. In model No. 4, the reinforcing bar 9 was "D13@200mm" and the cover thickness H1 (see Figure 2) was 30 mm. The length P1 (see FIG. 2) of the reinforcing bar 9 protruding from the beam 2 in the span direction D1 was set to 520 mm (= 40d = 40 × 13 (d: reinforcing bar diameter (mm)).

[0039] Figure 10 shows a graph showing the relationship between load and crack width. Note that concrete crack width is calculated by multiplying concrete crack strain (%) and element size (mm). Figure 11 shows the amount of crack strain increase per unit load increment, and the inflection point was confirmed. There was not much difference in the load value at which the inflection occurs with and without reinforcing bars, but the amount of increase was about two times higher, and it was confirmed that with reinforcing bars, the amount of increase was kept to the same level as with an open cross section.

[0040] The results thus far are summarized in Figure 12. Comparing cases without reinforcing bars (No. 2) with cases with reinforcing bars (No. 3, 4), there was no difference in the crack initiation load, and only a small difference in the crack propagation load, but a large difference was observed in the crack strain and crack width per unit incremental load. From the above, it can be seen that the introduction of reinforcing bars 9, with the specifications confirmed in this analysis (reinforcing bar ratio of 0.881% or more), suppressed the sudden decrease in rotational rigidity near the beam when a certain load was exceeded, and the eventual increase in crack width (8.9 kN / m 2 However, we were able to confirm the effect of reducing the thickness by less than 0.15 mm.

[0041] In addition, the required crack performance (the maximum allowable crack width) differs depending on the building's purpose and the environment in which the deck slab is used, so it is necessary to make a quantitative judgment from the perspective of both the required performance and cost. Below, we will derive an evaluation formula for crack width and reinforcement ratio.

[0042] Figure 13 plots the loads at which the crack widths of the reverse enclosing specifications (No. 2-4) reached 0.05 mm, 0.1 mm, and 0.15 mm, and calculates an approximate formula. The plots surrounded by B1 are the results for No. 2, the plots surrounded by B2 are the results for No. 3, and the plots surrounded by B3 are the results for No. 4. It was confirmed that it can be roughly evaluated with a linear function. It can be seen that when the rebar ratio increases beyond the minimum rebar ratio of 0.2% stipulated in the deck standards, the allowable load value for each crack width increases steadily.

[0043] An image of practical use is shown in Fig. 14. For example, a load of 6.0 kN / m 2 In the case of a deck slab, if you wish to keep the crack width to 0.15 mm or less, the specified crack performance can be ensured by keeping it in the range shown in B4 (reinforcement ratio 0.32% or more).

[0044] The evaluation formulas are summarized in Figures 15(a) and 15(b). The formula for confirming the allowable load at a certain reinforcement ratio is shown in Figure 15(a), and the formula for confirming the necessary reinforcement ratio under a certain generated load is shown in Figure 15(b). To keep the crack width to 0.15 mm or less, the reinforcement ratio of the cross section in the span direction D1 of the deck slab 100 shall be equal to or greater than the value given by the following formula (1). To keep the crack width to 0.10 mm or less, the reinforcement ratio of the cross section in the span direction D1 of the deck slab 100 shall be equal to or greater than the value given by the following formula (2). To keep the crack width to 0.05 mm or less, the reinforcement ratio of the cross section in the span direction D1 of the deck slab 100 shall be equal to or greater than the value given by the following formula (3). Here, y is the reinforcement ratio (%), and x is the generated load or design load (kN / m 2 ). y=(x-3.9) / 6.4 …(1) y=(x-3.4) / 4.2 …(2) y=(x-4.4) / 0.7 …(3)

[0045] Next, the action and effect of the deck slab 100 according to the embodiment of the present invention will be described.

[0046] In the deck slab 100 according to this embodiment, the reinforcement ratio of the cross section in the span direction D1 of the deck slab 100 is set to a value equal to or greater than that given by formula (1). In this case, in order to obtain a reinforcement ratio for suppressing the crack width to a desired size for the occurrence load or design load of the deck slab 100, the occurrence load or design load x can be substituted into formula (1) to calculate at least the required reinforcement ratio. From the above, it is possible to control cracks by arranging a necessary and sufficient amount of reinforcement for a predetermined occurrence load or design load. This results in a minimum amount of reinforcement, which can reduce the amount of steel material and the labor required for reinforcing bar construction. In addition, cracks can be appropriately controlled to ensure the quality of the deck slab 100 as a floor.

[0047] The cover thickness of the reinforcing bars 9 on the beams may be 40 mm or less. In this case, the reinforcing bars 9 can adequately control cracks.

[0048] The deck slab 100 may be of the reverse enclosing type or intermediate enclosing type. Even in the case of the deck slab 100 of the reverse enclosing type or intermediate enclosing type, a necessary and sufficient amount of reinforcing bars can be obtained.

[0049] Load capacity: 8.9kN / m 2 In this case, it is possible to prevent the load from becoming too large.

[0050] The diameter of the reinforcing bars 9 on the beam may be greater than D10, and the spacing may be 300 mm or less. This allows the reinforcing bars 9 to adequately control cracks.

[0051] The design method for the deck slab 100 according to this embodiment is a design method for the deck slab 100 having a deck plate 6 and concrete 7 provided on the deck plate 6, in which reinforcing bars 9 are arranged on the upper side of the beam inside the concrete 7, and the reinforcing bar ratio of the cross section in the span direction D1 of the deck slab 100 may be set to be equal to or greater than the value given by the following formula (1). y=(x-3.9) / 6.4 …(1) y is the reinforcement ratio (%) and x is the generated load or design load (kN / m 2 ).

[0052] According to the design method for the deck slab 100 according to this embodiment, it is possible to obtain the same functions and effects as those of the deck slab 100 described above.

[0053] The present invention is not limited to the above-described embodiments.

[0054] For example, the above-mentioned deck slab structure is merely one example, and may be modified as appropriate without departing from the spirit of the present invention. [Explanation of symbols]

[0055] 2...beam, 6...deck plate, 7...concrete, 9...rebar, 100...deck slab.

Claims

1. A deck slab having a deck plate and concrete provided on the deck plate, Inside the concrete, reinforcing bars are arranged on the upper side of the beam and around the upper periphery of the beam, A deck slab having a cross-sectional reinforcement ratio in the span direction of the deck slab that is equal to or greater than the value given by the following formula (1). y=(x-3.9) / 6.4...(1) y is the reinforcement ratio (%), and x is the generated load or design load (kN / m 2 ).

2. 2. The deck slab according to claim 1, wherein the cover thickness of the reinforcing bars on the beam is 40 mm or less.

3. 2. The deck slab of claim 1, which is of a reverse encro type or an intermediate encro type.

4. Load capacity: 8.9 kN / m 2 2. The deck slab according to claim 1, wherein:

5. 2. The deck slab according to claim 1, wherein the reinforcing bars on the beam have a diameter greater than D10 and are spaced apart at intervals of 300 mm or less.

6. A method for designing a deck slab having a deck plate and concrete provided on the deck plate, comprising: Inside the concrete, reinforcing bars are arranged on the upper side of the beam and around the upper periphery of the beam, A method for designing a deck slab, the method comprising: setting a cross-sectional reinforcement ratio of the deck slab in the span direction to a value equal to or greater than the value given by the following formula (1). y=(x-3.9) / 6.4...(1) y is the reinforcement ratio (%), and x is the generated load or design load (kN / m 2 ).