Packaging bag, manufacturing method of packaging bag

A paper-based packaging bag with a transparent portion and heat-sealing layer addresses the manufacturing challenge of plastic bags, enabling efficient production and reducing environmental impact.

JP2024135191APending Publication Date: 2024-10-04FUJI SEAL INC
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023045755
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-22
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Existing packaging bags made from plastic laminated films cannot be manufactured using bag-making machines that heat-seal plastic films, and there is a need for an environmentally friendly alternative that reduces greenhouse gas emissions.

Method used

A paper-based packaging bag with a transparent portion impregnated with a transparentizing agent and a heat-sealing layer formed on the inner surface, allowing it to be manufactured using a bag-making machine.

Benefits of technology

The solution enables the production of a partially transparent paper-based packaging bag that can be manufactured efficiently using conventional bag-making machines, enhancing design appeal and product visibility while reducing plastic use and greenhouse gas emissions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024135191000001_ABST
    Figure 2024135191000001_ABST
Patent Text Reader

Abstract

To provide a packaging bag which can be manufactured by a bag making machine, which is made of paper and part of which is transparent.SOLUTION: A packaging bag (100) includes: a bag body (10) constituted by a paper base material (21), and having a surface and an inner surface; a transparent part (8) in which a transparency agent is impregnated in a first region which is part of the paper base material (21); and a heat seal layer (22) in which a heat seal agent is coated at least on part of an inner surface of the paper base material (21). In order to make the packaging bag (100), the heat seal layer (22) formed in a region excluding the first region in the paper base material (21) is heat-sealed.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a packaging bag and a method for manufacturing the packaging bag. [Background technology]

[0002] There are various types of packaging bags (flat pouches, standing pouches, side gusset pouches, pillow packaging bags, etc.) that use a laminated film with a heat sealable film (sealant layer) laminated on the inner surface. These packaging bags use a transparent plastic film to allow the contents (products) to be seen through.

[0003] On the other hand, the use of paper substrates as an alternative material to plastics is being considered due to marine pollution caused by plastics, the problem of fossil fuel depletion, and environmental measures such as reducing greenhouse gases such as CO2. A transparent agent can be applied to the paper substrate to form a see-through portion. Patent Documents 1 and 2 are known as documents disclosing packaging bags using such paper substrates. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP2005-1163A [Patent Document 2] Patent Publication No. 2000-85868 Summary of the Invention [Problem to be solved by the invention]

[0005] However, the envelopes disclosed in Patent Documents 1 and 2 are manufactured by gluing, and cannot be manufactured using the widely used bag-making machines that heat-seal laminated plastic films to make bags.

[0006] In view of the above problems, the present disclosure aims to provide a paper, partially transparent packaging bag that can be produced using a bag making machine, and a method for producing such a packaging bag. [Means for solving the problem]

[0007] In order to solve the above-mentioned problems, a packaging bag according to one embodiment of the present disclosure comprises a bag body made of a paper base material and having a surface and an inner surface, a transparent portion formed by impregnating a transparentizing agent in a first region that is a part of the paper base material, and a heat seal layer formed by applying a heat sealant to at least a part of the inner surface of the paper base material, and the heat seal layer formed in an area of ​​the paper base material excluding the first region is heat sealed to produce a self-packaging bag.

[0008] A method for manufacturing a packaging bag according to one embodiment of the present disclosure includes the steps of preparing a paper base material having a surface and an inner surface that constitutes a bag body; impregnating a first region that is a part of the paper base material with a transparentizing agent to form a transparent portion; forming a heat seal layer by applying a heat sealant to at least a portion of the inner surface of the paper base material; and heat sealing the heat seal layer formed in an area of ​​the paper base material excluding the first region to form a bag. Effect of the Invention

[0009] According to the present disclosure, it is possible to provide a paper, partially transparent packaging bag that can be produced using a bag making machine, and a method for producing the packaging bag. [Brief description of the drawings]

[0010] [Figure 1] FIG. 2 is a front view of a packaging bag according to the present disclosure. [Diagram 2] FIG. 2 shows a schematic cross-sectional view of a packaging bag (a schematic cross-sectional view taken along line AA in FIG. 1). [Diagram 3] 1 shows a schematic cross-sectional view of a packaging bag according to the present disclosure. [Figure 4] 4 is a flowchart showing a method for manufacturing a packaging bag according to the present disclosure. [Diagram 5] FIG. 1 is a perspective view of a pillow packaging bag according to the present disclosure. [Figure 6] FIG. 2 is a diagram showing an example of a sheet for manufacturing a pillow packaging bag according to the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] An embodiment of the present disclosure will be described in detail below with reference to FIG. 1 and the like. FIG. 1 is a front view of a packaging bag 100 according to the present disclosure. In FIG. 1, XYZ coordinates are shown. The X-axis indicates the width direction of the packaging bag 100. The Y-axis indicates the thickness direction of the packaging bag 100. The Z-axis indicates the height direction of the packaging bag 100. The outer surface of the packaging bag 100 is defined as the "front surface" and the inner surface is defined as the "inner surface." A numerical range expressed as "lower limit value XXX to upper limit value YYY" means equal to or greater than the lower limit value XXX and equal to or less than the upper limit value YYY.

[0012] (packaging bag) The configuration of the packaging bag 100 will be described with reference to Figures 1 and 2. Figure 1 is a front view of the packaging bag 100. Figure 2 shows a schematic cross-sectional view of the packaging bag 100 (schematic cross-sectional view along line AA in Figure 1). Figures 1 and 2 show the packaging bag 100 in a state in which no contents are enclosed. In Figures 1 and 2, the packaging bag 100 has a bag body 10 and a zipper 20. The packaging bag 100 does not have to have the zipper 20, but will be described below as having the zipper 20.

[0013] First, the configuration of the packaging bag 100 according to the present disclosure will be described as follows. The packaging bag 100 includes a bag body having a front surface and an inner surface, which is made of a paper base material 21, a transparent portion 8 formed by impregnating a transparentizing agent in a first region that is a part of the paper base material 21, and a heat seal layer 22 formed by applying a heat seal agent to at least a part of the inner surface of the paper base material 21. Then, in order to manufacture the packaging bag 100, the heat seal layer 22 formed in the paper base material 21 in a region excluding the first region is heat sealed.

[0014] The bag body 10 is mainly composed of a paper base material 21, and forms the main body of the packaging bag 100. In Fig. 1, the bag body 10 is illustrated as having a vertically long rectangular shape, but in order to improve the design of the packaging bag, it may be formed in a shape having curved portions, such as a polygon (square, trapezoid, triangle, pentagon, etc.), ellipse, or gourd shape. In the following description, the bag body 10 will be described as having a vertically long rectangular shape.

[0015] The bag body 10 is composed of a first sheet 1 and a second sheet 2. The first sheet 1 and the second sheet 2 face each other and have the same shape. The first sheet 1 and the second sheet 2 are bonded to each other by heat sealing at a right end 4a and a left end 4b parallel to the Z axis and a lower end 5 parallel to the X axis direction. The bond width between the first sheet 1 and the second sheet 2 at the right end 4a, the left end 4b, and the lower end 5 is, for example, 5 to 20 mm, but may be any appropriate width as long as the bond is maintained, and the width may vary. The first sheet 1 and the second sheet 2 have an upper end 6 parallel to the X axis direction. After the bag body 10 is filled with the contents, the upper end 6 is bonded by heat sealing to seal the bag body 10.

[0016] In Fig. 1, the first sheet 1 and the second sheet 2 are bonded to each other at the lower end 5. However, before the bag body 10 is filled with the contents, the first sheet 1 and the second sheet 2 may be bonded to each other at the upper end 6, not at the lower end 5. In this case, after the bag body 10 is filled with the contents, the bag body 10 can be sealed by bonding the first sheet 1 and the second sheet 2 at the lower end 5.

[0017] The bag body 10 has four corners. The corners may be configured as either right angles or curved lines. The bag body 10 may have a bottom gusset and be configured as a freestanding type. The bag body 10 may be a side gusset type having gussets on the left and right. The paper base material 21 may also have a heat seal layer in the sheet that constitutes the bottom gusset or the side gusset.

[0018] The first sheet 1 and the second sheet 2 may be formed by folding a single sheet. In this case, the first sheet 1 and the second sheet 2 do not need to be bonded at the lower end 5, the upper end 6, the right end 4a, or the left end 4b.

[0019] The first sheet 1 and the second sheet 2 have zippers 20 at opposing positions on the inner surface. The zipper 20 is provided parallel to the X-axis from the right end 4a to the left end 4b. In Fig. 1, the zipper 20 is provided on the upper side of the packaging bag 100, but it may be provided near the center or on the lower side of the packaging bag 100. In the following description, the zipper 20 is described as being provided on the upper side of the packaging bag 100.

[0020] The packaging bag 100 may have a tear-off portion 7 below the zipper 20. The zipper 20 is made of plastic. The upper side of the packaging bag 100 including the zipper 20 can be torn off at the tear-off portion 7 or starting from the tear-off portion 7, and thus the portion of the packaging bag 100 below the tear-off portion 7 can be recycled as recyclable paper.

[0021] The tear-off portion 7 is provided on the first sheet 1 and the second sheet 2, and the tear-off portion 7 on the first sheet 1 and the tear-off portion 7 on the second sheet 2 are provided at positions facing each other. The tear-off portion 7 may be a half-cut line 7A, a notch portion 7B, or the like. The tear-off portion 7 may be any portion having a shape or structure for facilitating tearing off the upper side of the packaging bag 100 including the zipper 20.

[0022] In FIG. 1, as an example of the tear-off portion 7, a half-cut line 7A parallel to the X-axis direction and a V-shaped cutout portion 7B (a so-called V notch) are shown. The cutout portion 7B may be provided at the outer edge of the right end portion 4a and / or the outer edge of the left end portion 4b. The cutout portion 7B is formed to a size not exceeding the bonding width between the first sheet 1 and the second sheet 2 at the right end portion 4a and the left end portion 4b. In addition, when both the half-cut line 7A and the cutout portion 7B are provided, it is preferable that the cutout portion 7B is provided at the right end portion and / or the left end portion of the half-cut line 7A. The packaging bag 100 may have a cut (a so-called I notch) instead of the cutout portion 7B.

[0023] The packaging bag 100 does not have to have the tear-off portion 7. When recycling the lower portion of the zipper 20 as recyclable paper, the lower portion of the zipper 20 may be cut off using, for example, scissors. However, since the packaging bag 100 has the tear-off portion 7, the lower portion of the zipper 20 can be easily cut off without using scissors or the like.

[0024] The packaging bag 100 has a transparent portion 8 in the first sheet 1 and / or the second sheet 2. The transparent portion 8 is impregnated with a transparent agent by applying the transparent agent, and a transparent agent layer 23 (described later) is formed. The transparent portion 8 is more transparent than a portion not impregnated with the transparent agent, and the contents of the packaging bag 100 can be visually confirmed from the outside through the transparent portion 8. The transparent portion 8 is not formed on the entire surface of the paper base material 21, but is formed by impregnating a first region, which is a part of the paper base material 21, with the transparent agent. In FIG. 1, the first region is the region where the transparent portion 8 is formed.

[0025] Next, referring to FIG. 2, the first sheet 1 and the second sheet 2 each have a paper base material 21 and a heat seal layer 22 on the inner surface of the paper base material 21.

[0026] 2, the first sheet 1 has a transparentizing agent layer 23. In FIG. 2, the transparentizing agent layer 23 is formed on the front and inner surfaces of the paper base material 21 in the first sheet 1, and the transparentizing agent layer 23 is not formed on the front and inner surfaces of the paper base material 21 in the second sheet 2. However, the transparentizing agent layer 23 may be formed on the front and / or inner surfaces of the paper base material 21 in the second sheet 2. The transparentizing agent layer 23 may be formed on only one of the front and inner surfaces of the paper base material 21 in the first sheet 1 and / or the second sheet 2.

[0027] Furthermore, the first sheet 1 and / or the second sheet 2 may have a printed layer 24 on the whole or part of the surface of the paper base material 21. Although not shown in FIG. 2, the printed layer 24 may have a varnish layer formed on its upper surface.

[0028] The first sheet 1 and the second sheet 2 have zippers 20 at opposing positions on their inner surfaces. Fig. 2 shows the zipper 20 when closed. The configuration of each part will be specifically described below.

[0029] (Paper base material) The paper base material 21 is the main structure of the packaging bag 100, which gives strength to the bag body 10. The paper base material 21 may be manufactured by a known papermaking machine using natural fibers for papermaking, such as wood pulp. The papermaking conditions are not particularly limited. The natural fibers for papermaking may be wood pulp, such as softwood pulp or hardwood pulp, non-wood pulp, such as Manila hemp pulp, sisal hemp pulp, flax pulp, or pulp obtained by chemically modifying these pulps. The paper base material 21 may be selected from uncoated paper, one-side gloss kraft paper in which one side of the base material is treated, bleached kraft paper, unbleached kraft paper, and the like. In particular, from the viewpoint of improving transparency by applying a clarifying agent described later and of the printability of the surface, the paper base material 21 is preferably one-side gloss bleached kraft paper. The paper base material 21 is, for example, 30 g / m 2 ~120g / m 2 , preferably 40 g / m 2 ~100g / m 2 The basis weight may be

[0030] (Heat seal layer) The heat seal layer 22 is formed by applying a heat seal agent to at least a part of the inner surface of the paper base material 21. The heat seal layer 22 may be formed on the entire inner surface of the paper base material 21, or may be formed by overlapping on the transparentizing agent layer 23. The heat seal layer 22 does not have to be formed on the transparentizing agent layer 23. The heat seal layer 22 is formed at least in an area of ​​the inner surface of the paper base material 21 except for a first area impregnated with the transparentizing agent. The packaging bag 100 is made by heat sealing the heat seal layer 22 formed in an area except for the first area.

[0031] The heat seal layer 22 is formed by applying an aqueous coating agent to the paper base material 21 and then drying the aqueous coating agent. The aqueous coating agent is applied to the paper base material 21 in a state where a heat sealable resin or the like is dispersed in water (in a dispersion, suspension, or emulsion state). This can increase the redisintegrability of the heat seal layer 22 when the paper base material 21 to which the heat seal layer 22 is applied is recycled as paper.

[0032] As the resin component of the aqueous coating agent, one containing an olefin-based copolymer resin can be used. The olefin-based copolymer resin is preferably a polyethylene-based resin, for example, an ethylene-vinyl acetate copolymer resin, an ethylene-(meth)acrylic copolymer resin, an ethylene-vinyl chloride copolymer resin, an ethylene-vinyl acetate-vinyl chloride copolymer resin, or an ethylene-vinyl acetate-acrylic copolymer resin. The main component of the aqueous coating agent is preferably an ethylene-vinyl acetate copolymer resin. The ethylene-vinyl acetate copolymer resin may contain other polymerization components such as an acrylic acid ester or acrylic acid.

[0033] The aqueous coating agent may use an ethylene-acrylic acid copolymer as a main component, or an ionomer such as a metal salt of an ethylene-methacrylic acid copolymer, a metal salt of an ethylene-acrylic copolymer, or a metal salt of an ethylene-urethane copolymer as the main component.

[0034] The aqueous coating agent may contain, as an anti-blocking agent, pigments such as kaolin, talc, calcium bicarbonate, titanium oxide, silica, hollow beads, microcapsules, etc. The aqueous coating agent may contain, as a lubricant, synthetic waxes such as paraffin wax, polyethylene wax, fatty acid amide wax, etc., or natural waxes such as carnauba wax, etc.

[0035] Examples of the aqueous coating agent that can be used include "Chemipearl S type and V type manufactured by Mitsui Chemicals, Inc.," "Aqua TOP HS Varnish manufactured by Toyo Ink Co., Ltd.," "HYDBAR, HYDRECT manufactured by DIC Corporation," "SEIKOAT manufactured by Seiko PMC Corporation," and "Aqueous SA series manufactured by Toyo Ink Co., Ltd."

[0036] The aqueous coating agent is applied to the paper base material 21 by, for example, flexographic printing or gravure printing. By applying the aqueous heat seal agent to the paper base material 21 by the flexographic printing method, the aqueous heat seal agent can be applied appropriately with little unevenness even to the paper base material 21 having a rough surface. Furthermore, by applying the aqueous heat seal agent to the paper base material 21 by the gravure printing method, a larger amount of the aqueous coating agent can be applied to the paper base material 21 in one printing run compared to flexographic printing.

[0037] The heat seal layer 22 has, for example, a coating amount of 1 g / m after drying. 2 ~15g / m 2 The thickness is about 1 μm to 15 μm, particularly 2 μm to 15 μm. When the thickness of the heat seal layer 22 is 2 μm or more, the adhesive strength of the zipper 20 to the paper base material 21 can be kept high. The thickness of the heat seal layer 22 may be 15 μm or more, but considering the material cost of the heat seal agent or the ratio of the resin component of the packaging bag 100, the thickness is preferably 15 μm or less.

[0038] The heat seal layer 22 is not limited to an aqueous coating agent, and may be formed by applying and drying a solvent-based coating agent to the paper substrate 21. The solvent-based coating agent may be a solution in which a heat-sealable resin component exemplified in the aqueous coating agent is dissolved in an organic solvent and additives such as an anti-blocking agent and a lubricant are added.

[0039] (Clarifying agent layer) The clarifying agent layer 23 is formed by applying and impregnating the paper base material 21 with a clarifying agent. When the clarifying agent is applied to the paper base material 21, part of the agent penetrates into the gaps between the fibers of the paper base material 21, and part of the agent is formed as a surface layer. The part that penetrates into the gaps between the fibers of the paper base material 21 fills the gaps between the fibers of the paper base material 21 and improves light transmittance. The part where the surface layer is formed smoothes the surface of the paper base material 21 and suppresses diffuse reflection of light, thereby improving the transparency of the paper base material 21.

[0040] The area of ​​the paper base material 21 impregnated with the clarifying agent becomes the transparent portion 8 in FIG. 1. The transparent agent may be applied to and impregnated into both sides of the paper base material 21, as shown in FIG. 2. By impregnating from both sides, the transparent agent fills gaps between fibers in the thickness direction of the paper base material 21, improving transparency. When the inner surface of the paper base material 21 is rougher than the front surface and only one side is impregnated with the transparent agent, the transparent agent is preferably impregnated into the inner surface. This is because the transparent agent is more easily impregnated into the rough surface (inner surface) than the glossy surface (front surface), making it possible to increase the transparency of the transparent portion 8.

[0041] When the transparentizing agent layer 23 is formed on the surface side of the paper base material 21, the transparentizing agent layer 23 may be formed on the upper surface of the printed layer 24, or may be formed on the surface of the paper base material 21 on which the printed layer 24 is not formed. In addition, a varnish layer (not shown) may be formed on the upper surface of the transparentizing agent layer 23. The printed layer 24 may be formed on the upper surface (surface) of the transparentizing agent layer 23. The design is improved by overlaying a design print (printed layer 24) on the transparentizing agent layer 23.

[0042] The transparentizing agent layer 23 is formed by impregnating the paper substrate 21 with a transparentizing agent (transparentizing resin). The transparentizing resin may be, for example, a petroleum-based hydrocarbon resin, a rosin-based resin, an olefin-based resin, an acrylic resin, a polyester-based resin, a urethane-based resin, a paraffin wax, or a fluororesin, or may be used alone or in combination with two or more kinds, or may further contain additives. The transparentizing resin is applied in the form of an aqueous emulsion or an organic solvent solution. For example, the transparentizing resin may be "Clariten DC" made of an alicyclic saturated hydrocarbon resin, which is a petroleum-based hydrocarbon resin, or "LG-WR Marking Agent" made by Toyo Ink Co., Ltd. The clarifying agent layer 23 is formed by appropriately adjusting the type and / or amount of the clarifying resin to be applied so as to obtain a desired transparency. The clarifying agent layer 23 may be formed by a method of impregnating the paper base material 21 with the clarifying resin only in the necessary portions. The clarifying agent layer 23 may be formed by a method of impregnating the paper base material 21 with the clarifying resin by various printing methods (e.g., flexographic printing, inkjet printing, gravure printing, offset printing, gravure offset printing, silk screen printing).

[0043] The clarifying agent may be one that is applied and dried as an emulsion or solution, or one that is cured by ultraviolet light or electron beams. However, when the paper substrate 21 is recycled, it is preferable to use one that is applied and dried as an emulsion or solution, which has good disintegration suitability during recycling. In particular, petroleum-based hydrocarbon resins such as alicyclic saturated hydrocarbon resins are preferable. The coating method is preferably gravure printing, which is performed continuously with the heat seal agent.

[0044] The transparentizing agent layer 23 is, for example, a single-sided bleached kraft paper with a basis weight of 50 g / m 2 ~70g / m 2 In the case of , the coating amount is 2g / m2 after drying. 2 ~15g / m 2 About 3 g / m 2 ~12g / m 2If the amount of the clarifying agent applied is small, the transparency is poor. If the amount of the clarifying agent applied is large, the coating drying property is poor, the difference in thickness and / or hardness of the sheet between the coated and non-coated parts of the clarifying agent is large, and the suitability for processing such as bag making is also poor.

[0045] (Transparency) In the present disclosure, the transparentizing agent layer 23 has a transparency of "hiding power of 60% or less" so that the contents of the packaging bag can be visually confirmed. The hiding power of a certain sample is calculated as follows.

[0046] First, prepare a sample. Place the sample on top of a black reference (over black), and place a spectrophotometer (product name: X-rite RM200QC portable color difference meter, manufactured by X-rite) on top of it. Then, measure the tristimulus value YB using the spectrophotometer. Next, place the sample on top of a white reference (over white), and measure the tristimulus value YW using the spectrophotometer placed on top of the sample. Next, substitute the tristimulus value YB and the tristimulus value YW into the formula shown below to calculate the hiding power of each sample. A black and white ledger (thin material) (manufactured by Daimonji Paper Co., Ltd.) was used as the black reference and the white reference.

[0047] Opacity = (YB / YW) x 100 The hiding power will be described in more detail below with reference to Table 1. Table 1 shows the test results relating to hiding power.

[0048] [Table 1] (Comparative Examples 1 and 2) The paper base material is bleached kraft paper (one-sided gloss) "Sankayo ​​60g / m 2 (Oji Materia Co., Ltd.) and "Silver 50g / m 2 (manufactured by Nippon Paper Industries Co., Ltd.) was used. Samples in which the paper base material was not coated with a clarifying agent were designated as Comparative Examples 1 and 2, respectively.

[0049] Example 1 The paper base material is bleached kraft paper (one-sided gloss) "Sankayo ​​60g / m 2 (Oji Materia Co., Ltd.) was used. A transparentizing agent, Clariten DC (Yamato Chemical Industry Co., Ltd.), was applied to both sides (glossy and rough sides) of the paper base material using a gravure printing machine to create partially transparent paper.

[0050] (Examples 2 to 4) The paper base material is bleached kraft paper (one-sided gloss) "Silver 50g / m 2 (manufactured by Nippon Paper Industries Co., Ltd.) was used. Three types of partially transparent paper were created by applying the clarifying agent "Clariten DC (manufactured by Daiwa Chemical Industry Co., Ltd.)" to the glossy and / or rough surfaces of the paper substrate using a gravure printing machine.

[0051] Example 5 The paper base material is bleached kraft paper (one-sided gloss) "Silver 50g / m 2 A transparentizing agent "Clariten DC (manufactured by Nippon Paper Industries Co., Ltd.)" was used. A clarifying agent "Clariten DC (manufactured by Yamato Chemical Industry Co., Ltd.)" was applied to a partial area on one side of the paper base material using a gravure printing machine. Next, a heat seal agent "EA-700 (manufactured by Toyo-Morton Co., Ltd.)" was applied to almost the entire surface including the partial area on the one side. In this way, a partially transparent paper was created in which the transparentizing agent was applied to one side and the heat seal agent was applied to the transparentizing agent.

[0052] Example 6 The paper base material is bleached kraft paper (one-sided gloss) "Silver 50g / m 2 A transparentizing agent "Clariten DC (manufactured by Nippon Paper Industries Co., Ltd.)" was used. A clarifying agent "Clariten DC (manufactured by Yamato Chemical Industry Co., Ltd.)" was applied to a partial area on one side of the paper substrate using a gravure printing machine. Then, a heat seal agent "EA-700 (Toyo-Morton Co., Ltd.)" was applied to the substantially entire surface including the partial area on the one side. Then, the paper substrate was inverted on the gravure printing machine, and a transparentizing agent was applied to a partial area (a region substantially overlapping the partial area) on the opposite side of the one side, and a transparent varnish was applied to cover the surface of the transparentizing agent. In this way, a partially transparent paper was created in which the transparentizing agent was applied to both sides, the heat seal agent was applied to the transparentizing agent on one side, and the transparent varnish was applied to the transparentizing agent on the other side.

[0053] In Examples 1 to 6, the clarifying agent was about 5 g / m2 in terms of dry weight per side. 2 It is applied so that

[0054] From Table 1, the following results were obtained. In Examples 1 to 6 in which a clarifying agent was applied, the hiding power was significantly lower than in Comparative Examples 1 and 2 in which a clarifying agent was not applied. When the transparentizing agent was applied on both sides (Examples 4 and 6), the hiding power was lower than when the transparentizing agent was applied on one side (Examples 2, 3, and 5). When the transparentizing agent was applied to the rough side of the paper base material (Example 3), the hiding power was lower than when the transparentizing agent was applied to the glossy side of the paper base material (Example 2). The same paper base material "Silver 50g / m 2 Comparing Examples 1 to 4, which used "Nippon Paper Industries Co., Ltd.", with Examples 5 and 6, it was found that the hiding power was increased by applying the heat seal agent onto the transparentizing agent. The "difference (%) substrate alone - processed substrate" shown at the bottom of Table 1 indicates the value obtained by subtracting the hiding power of the Examples from the hiding power of the Comparative Examples. For example, in the case of Example 1, the hiding power of Comparative Example 1 is 74.8% and the hiding power of Example 1 is 44.4%, so the difference (%) is 30.4%. The differences are also calculated for Comparative Example 2 and Examples 2 to 4. As is clear from this difference, the hiding power is greatly reduced by applying a clarifying agent.

[0055] Thus, Table 1 shows that the hiding power changes depending on factors such as whether the transparentizing agent is applied to one side or both sides, and whether the transparentizing agent is applied to the glossy side or the rough side when applied to one side. In the present disclosure, as described above, the transparentizing agent layer 23 has a transparency of "hiding power of 60% or less" so that the contents of the packaging bag can be visually confirmed.

[0056] (Printing layer) A printing layer 24 may be formed on the surface of the paper substrate 21. The printing layer 24 may be formed by flexographic printing or gravure printing. The printing layer 24 is a layer on which a product description, various designs, or an identification code for identifying the product to be packaged in the packaging bag 100 is printed. The printing layer 24 may be color printed or black and white printed. The printing layer 24 may be formed on only one surface of the first sheet 1 or the second sheet 2. The printing layer 24 may have a transparentizing agent layer 23 and / or a varnish layer formed on its upper surface. The printing layer 24 may be formed on the upper surface of the transparentizing agent layer 23. The printing layer 24 and the varnish layer may be formed by a known method using a known material. The printing layer 24 is preferably formed by gravure printing in succession to the heat seal agent and the transparentizing agent.

[0057] (Chuck) The chuck 20 is attached to the paper substrate 21 via a heat seal layer 22. The chuck 20 is composed of, for example, a chuck protrusion 20a having a linear protrusion and a chuck groove 20b having a linear groove. The chuck protrusion 20a is attached to the inner surface of the first sheet 1, and the chuck groove 20b is attached to the inner surface of the second sheet 2.

[0058] The chuck 20 is made of a material that can be heat-sealed to the heat seal layer 22. As an example, when the heat seal layer 22 is made of a polyethylene-based resin, the chuck 20 is also made of a polyethylene-based resin. In other words, it is preferable that the material of the heat seal layer 22 and the material of the surface of the chuck 20 that is attached to the heat seal layer 22 are the same type of resin. This essentially means that the adhesive surfaces of the heat seal layer 22 and the chuck 20 have high affinity when melted or softened by heat.

[0059] 2 shows an example of the chuck 20 in which the chuck protrusions 20a and the chuck grooves 20b are simply illustrated, but various known shapes may be used for the chuck 20. The chuck 20 may have various shapes, such as a shape of interlocking protrusions and grooves, a shape with a wide adhesive surface, or a shape with two rows of protrusions and grooves.

[0060] The bag body 10 and the zipper 20 are preferably bonded by heat by pressing with a heat seal bar or the like, but may be bonded by a known method such as ultrasonic bonding.

[0061] (Anchor coat layer) The packaging bag 100 may have an anchor coat layer between the paper base material 21 and the heat seal layer 22. The anchor coat layer prevents the heat seal agent from penetrating into the paper base material 21 and improves the adhesion between the paper base material 21 and the heat seal agent, thereby making it possible to utilize the performance of the heat seal agent. The anchor coat agent may be, for example, a vinyl chloride-vinyl acetate resin, a chlorinated polyolefin resin, an acrylic resin, or the like as a main component. The anchor coat agent may be selected according to the paper base material 21 and / or the heat seal layer 22. The anchor coat agent is preferably applied to the paper base material 21 by flexographic printing, gravure printing, or the like in a state where it is dispersed in water (dispersion, suspension, or emulsion state) or dissolved in an organic solvent.

[0062] (Modification) A packaging bag 300 according to the present disclosure, which is a modified example of the packaging bag 100, will be described with reference to Fig. 3. Fig. 3 shows a schematic cross-sectional view of the packaging bag 300 according to the present disclosure. Note that the contents that have already been described will not be described again.

[0063] In the packaging bag 300, a heat seal layer 22 is formed on the inner surface of the paper base material 21. The heat seal layer 22 is formed only on a part of the inner surface of the paper base material 21. Specifically, in the packaging bag 300, the heat seal layer 22a is formed on the upper end portion 6 of the packaging bag 300, the heat seal layer 22b is formed on the lower end portion 5 of the packaging bag 300, and a part of the heat seal layer 22b is bonded by heat sealing. The heat seal layer 22 is not formed in other places.

[0064] Then, the transparentizing agent layer 23 is formed in the area on the inner surface of the paper base material 21 where the heat seal layer 22 is not formed. The transparentizing agent layer 23 is formed on the surface of the paper base material 21, the inner surface of the paper base material 21, and the upper surface of the printed layer 24 formed on the surface of the paper base material 21 in the first sheet 1. Specifically, the printed layer 24a, the printed layer 24b, and the printed layer 24c are formed on the surface of the paper base material 21 in the first sheet 1. The transparentizing agent layer 23 is not formed on the upper surface of the printed layer 24a. The printed layer 24b has the transparentizing agent layer 23 formed over the entire upper surface. The printed layer 24c has the transparentizing agent layer 23 formed on a part of the upper surface. The transparentizing agent layer 23 on the inner surface of the paper base material 21 is partially formed at a position corresponding to the application area of ​​the transparentizing agent on the surface of the paper base material 21. According to this configuration, the transparency is given shading, and the packaging bag 300 is finished to have a more impressive design.

[0065] In this way, the transparentizing agent layer 23 is provided in various forms on the packaging bag 300. Although the transparentizing agent layer 23 is formed only on the first sheet 1 side in Fig. 3, the transparentizing agent layer 23 may be formed on the second sheet 2 side.

[0066] The packaging bag according to the present disclosure has been described above. By being configured as described above, the packaging bag according to the present disclosure has the following advantages. These advantages will be described below.

[0067] First, a conventional envelope will be described. Conventional envelopes are manufactured by applying a transparent agent to a paper base material to form a see-through portion, and then gluing the paper base material to produce an envelope. Therefore, such envelope materials cannot be used in a bag-making machine or a bag-making and filling machine that heat-seals a plastic film to produce a bag.

[0068] In contrast, the packaging bag according to the present disclosure has a heat seal layer 22 formed by applying a heat sealant to at least a portion of the inner surface of the paper base material 21. Therefore, the packaging bag according to the present disclosure can be made using a bag making machine used to manufacture a wide variety of pouches, just like pouches made from plastic laminated films. The bag making machine can continuously make bags at high speed by unwinding a long wound sheet and bonding the sheets together into a bag shape using heat sealing.

[0069] Furthermore, in the packaging bag according to the present disclosure, the transparent agent may be applied to the paper substrate 21 multiple times, for example, the transparent agent is applied once to each of the surface and the inner surface of the paper substrate 21. As a result, the transparent agent is filled in the gaps between the fibers in the thickness direction of the paper substrate in the packaging bag according to the present disclosure, and the transparency of the transparent portion 8 can be increased compared to the case where the transparent agent is applied to one side. When the degree of impregnation of the transparent agent differs between the surface and the inner surface of the paper substrate 21, a contrast in transparency is obtained, and the contrast enhances the design of the packaging bag. Furthermore, by forming the transparent agent layer 23 on the surface and the inner surface of the paper substrate 21, and printing and applying one or both of the transparent agents with a pattern such as letters or a design, and partially overlapping the formed areas, the watermark pattern can be given a shading, and the packaging bag can be finished with a more impressive design. Naturally, the packaging bag according to the present disclosure can bring about a change in the design of the packaging bag by applying the transparent agent to only one of the surface and the inner surface of the paper substrate 21, more than when the transparent agent is not applied to both sides.

[0070] Also, by carefully selecting the position where the transparentizing agent is applied to the paper base material 21, the appearance of the contents (product) can be made more impressive, thereby enhancing the product's appeal. Furthermore, when the product is removed, the design printed on the back side can be seen through the transparent portion 8 formed on the front side, improving the appeal of the packaging bag alone. Such a packaging bag increases the added value of the product.

[0071] (Manufacturing method) Next, a method for producing a packaging bag according to the present disclosure will be described below. Fig. 4 is a flow chart showing a method for producing a packaging bag according to the present disclosure.

[0072] First, in S10, a paper base material 21 having a surface and an inner surface that constitute the bag body 10 is prepared. Next, in S20, a transparentizing agent is impregnated into a first region that is a part of the paper base material 21 to form a transparent portion 8. Next, a heat seal layer 22 is formed by applying a heat seal agent to at least a part of the inner surface of the paper base material 21. Finally, in S40, the heat seal layer 22 formed in the region of the paper base material 21 except the first region is heat sealed to form a bag. S20 and S30 are performed by a printing machine. S40 is performed by a bag making machine. The order of S20 and S30 may be reversed. For example, when the region to which the transparentizing agent is applied and the region to which the heat seal agent is applied do not overlap, the order of S30 and S20 may be used.

[0073] The packaging bag according to the present disclosure can be manufactured using a bag making machine. In the manufacturing process of the packaging bag, although not limited thereto, at least a part of the printing layer 24 may be printed on the paper substrate 21 before S20. The printed content may be a character or a picture, and serves as a mark that provides a reference point for the position. The number of colors may be one color or four colors. The heat seal layer 22, the transparent agent layer 23, and the printing layer 24 can be formed according to the printing position of the printing layer 24, and as a result, the heat seal layer 22, the transparent agent layer 23, and the printing layer 24 can be accurately positioned.

[0074] The printing by the printing machine may be either gravure printing or flexographic printing, but gravure printing is preferred since it can ensure a larger coating amount in one printing and can increase production efficiency.

[0075] It is preferable not to form the transparent agent layer 23 at the fold positions of the packaging bag (bottom gusset, outer edge of the packaging bag, etc.) unless a transparent portion is required at these positions. If the transparent agent layer 23 is formed at these positions, streaks due to the folds may appear in the transparent portion 8, which may impair the design of the transparent portion 8.

[0076] (Strength test) The inventors of the present application conducted a strength test when a transparentizing agent and a heat-sealing agent were applied in layers. As a result, they found that the strength was reduced when the transparentizing agent and the heat-sealing agent were applied in layers, and therefore it was preferable to impregnate the transparentizing agent in the area of ​​the paper base material where no heat sealing was performed (except for the heat-sealing position).

[0077] Table 2 shows the results of a strength test (Example) when only a heat sealant was applied to a paper substrate, and a strength test (Comparative Example) when a transparentizing agent and a heat sealant were applied to a paper substrate. This strength test measures the force (N (Newtons)) required to peel the second sheet from the first sheet after the heat sealant was heat sealed. The following conditions were set in common for both the Examples and Comparative Examples. Sample creation: Heat seal tester (Tester Sangyo Co., Ltd., model number: TP-701-B Heat seal tester) Heat sealing conditions: the temperature of the upper bar is as shown in Table 2, and the temperature of the lower bar is all 80°C. 1 second, 0.3 MPa. ·Paper base material: basis weight 50g / m 2 Pure white roll paper (Nippon Paper Industries Co., Ltd. model number: Shirogane). Autograph test: Autograph testing machine (Shimadzu Corporation, model number: AG-500NX Plus). Autograph test conditions: 200 m / min, test gap 100 mm, sample width 15 mm, T-type peel. Number of tests: 5 times each. (Example) A heat sealant (EA-700 from Toyo-Morton Co., Ltd.) was applied to the paper substrate. (Comparative example) A transparency agent (Clariten DC, manufactured by Yamato Chemical Industry Co., Ltd.) and a heat seal agent (EA-700, manufactured by Toyo-Morton Co., Ltd.) were applied to a paper substrate. Heat sealant is 2.5~5g / m 2 and the clarifying agent is 5g / m 2 Apply with.

[0078] (Test Results) The test results based on the above-mentioned test conditions are shown in Table 2. If the strength when peeling the first sheet and the second sheet is maintained at 2N or more, they will not peel off easily, but in the examples, practical test results of 3.71N or more were obtained under all conditions with the upper bar at 80°C to 140°C.

[0079] [Table 2] In contrast, in the comparative example, the first sheet and the second sheet did not bond when the upper bar was between 80°C and 120°C ("ND" in Table 2). In other words, when the upper bar was in the temperature range of 80°C to 120°C, the strength required for bonding could not be obtained even when the first sheet and the second sheet were bonded with a heat sealant. Also, it was found that in order to bond the first sheet and the second sheet, the upper bar temperature needed to be 130°C or higher, and that the temperature conditions needed to be set higher than in the examples.

[0080] From the above results, it can be seen that the adhesive strength decreases when a transparentizing agent and a heat sealing agent are applied in multiple coats, and therefore it is preferable to impregnate the transparentizing agent in areas of the paper base material that are not heat sealed (except for the heat sealing position).

[0081] Furthermore, it is preferable that the transparent portion 8 is separated from the heat seal position where the heat seal layer 22 is heat sealed. In thermal adhesion (heat sealing) by pressing with a heat seal bar, the heat of the heat seal bar can be transmitted to areas other than the area to be heat sealed. In this case, if the transparentizing resin and the heat seal position are adjacent to each other, unnecessary heat is transmitted to the transparentizing resin. Since the transparentizing resin has low heat resistance, the unnecessary heat can have a negative effect on the transparentizing resin. For this reason, a configuration in which a boundary area of ​​an appropriate width where nothing is applied is provided between the transparentizing portion 8 and the heat seal position, and the transparentizing portion 8 is separated from the heat seal position, can be said to be one of the preferable manufacturing methods for packaging bags.

[0082] (Pillow packaging bag) Next, a pillow packaging bag 500 according to the present disclosure will be described with reference to Figs. 5 and 6. Fig. 5 is a perspective view of the pillow packaging bag 500 according to the present disclosure. The figure indicated by reference numeral 501 is a front perspective view of the pillow packaging bag 500. The figure indicated by reference numeral 502 is a rear perspective view of the pillow packaging bag 500. Note that pillow packaging refers to a packaging form in which a single sheet is sealed (jointed) in a cylindrical state with its backs facing each other, and the ends are sealed and cut at a predetermined length. Description of the contents already explained will be omitted.

[0083] 5, pillow packaging bag 500 includes bag body 50, end portion 52, and transparent portion 58, and contains contents 59 (products) therein. End portion 52 is a portion formed at both ends of pillow packaging bag 500 and between both ends of pillow packaging bag 500 on the back surface, and is bonded by heat sealing. In FIG. 5, heat seal application region 56 is a region where a heat seal agent is applied to form a heat seal layer. Heat seal application region 56 is formed to be wider than the region where end portion 52 is formed. Transparent portion 58 is formed at a position and / or size that allows at least a part of contents 59 to be seen.

[0084] Fig. 6 is a diagram showing an example of a sheet 600 for manufacturing a pillow packaging bag 500 according to the present disclosure. In Fig. 6, XY coordinates are shown. The X axis indicates the direction in which the sheet 600 extends. The Y axis indicates the direction perpendicular to the X axis.

[0085] The sheet 600 is a single sheet, in which the transparentizing agent-coated areas 53, the non-coated areas 54, and the heat seal-coated areas 56 are regularly formed.

[0086] The transparentizing agent-coated regions 53 are regions where a transparentizing agent is applied to form a transparentizing agent layer on the sheet 600. The transparentizing agent-coated regions 53 are formed at regular intervals along the X-axis direction. In Fig. 6, the transparentizing agent-coated regions 53 are formed in a substantially rectangular shape, but the transparentizing agent-coated regions 53 may be formed in a shape having curved portions such as a polygon (such as a square, trapezoid, triangle, or pentagon), an ellipse, or a gourd shape.

[0087] The non-coated region 54 is a region that is formed so as to surround the periphery of the transparentizing agent coated region 53, and does not include the transparentizing agent coated region 53 or the heat seal coated region 56. In Fig. 6, the non-coated region 54 is formed with a rectangular outer edge, but the non-coated region 54 may be formed in a shape having curved portions, such as a polygon (such as a square, trapezoid, triangle, or pentagon), an ellipse, or a gourd shape.

[0088] The heat seal applied area 56 is formed in an area of ​​the sheet 600 where the transparentizing agent applied area 53 and the non-applied area 54 are not formed.

[0089] 6, lines L1 and L2 each extend parallel to the X-axis and are folds along which pillow packaging bag 500 is produced from sheet 600. Line L3 extends parallel to the Y-axis and indicates a planned cutting position after sheet 600 is heat-sealed.

[0090] The sheet 600 is folded at lines L1 and L2 to encase the contents 59 (not shown), and the overlapping portions of the folded film are heat-sealed. Then, the sheet 600 is cut along line L3 after the heat seal application area 56 formed between two adjacent non-application areas 54 is heat-sealed.

[0091] In this manner, the packaging bag according to the present disclosure can be applied to the pillow packaging bag 500 shown in FIG. 5 as an example, and such pillow packaging bag 500 can be manufactured by a bag making machine (for example, a horizontal pillow packaging machine).

[0092] Although the pillow packaging bag with the backside seam seal has been described above, the configuration according to the present disclosure can also be applied to an envelope-sealed bag manufacturing method in which the front and back sides of both ends are sealed instead of the backside seam seal. In the case of the envelope-sealed bag manufacturing method, a heat seal agent application area (heat seal layer) may be provided on the front side of the seam.

[0093] As described above with reference to FIGS. 5 and 6, the packaging bag according to the present disclosure can be applied to various types of packaging bags, such as pillow packaging bags.

[0094] 〔summary〕 The packaging bag according to aspect 1 of the present disclosure comprises a bag body made of a paper base material and having a surface and an inner surface, a transparent portion formed by impregnating a transparentizing agent in a first region that is a part of the paper base material, and a heat seal layer formed by applying a heat sealant to at least a part of the inner surface of the paper base material, and the heat seal layer formed in an area of ​​the paper base material excluding the first region is heat sealed to produce a self-packaging bag.

[0095] According to the above configuration, in the packaging bag of aspect 1 of the present disclosure, the heat seal layer formed in the area other than the first area impregnated with a transparentizing agent is heat sealed, thereby realizing a paper, partially transparent packaging bag that can be manufactured using a bag making machine.

[0096] The packaging bag according to a second aspect of the present disclosure is the same as that of the first aspect, in which the inner surface is rougher than the outer surface, and the transparentizing agent is impregnated into the inner surface.

[0097] The rough surface (inner surface) is more easily impregnated with the clarifying agent than the glossy surface (front surface), which increases the transparency of the transparent portion.

[0098] The packaging bag according to a third aspect of the present disclosure is the packaging bag according to the first or second aspect, wherein the transparentizing agent is impregnated into the surface and the inner surface.

[0099] By impregnating the transparent agent from the front and back surfaces of the paper base material, the packaging bag according to aspect 3 of the present disclosure can have improved transparency in the transparent portion.

[0100] The packaging bag according to a fourth aspect of the present disclosure is any one of the first to third aspects, wherein the transparent portion is separated from a heat seal position where the heat seal layer is heat sealed.

[0101] In thermal adhesion (heat sealing) where pressure is applied with a heat seal bar, the heat of the heat seal bar can be transferred to areas other than the area to be heat sealed. In this case, if the transparentizing resin (transparent portion) is adjacent to the heat sealing position, unnecessary heat is transferred to the transparentizing resin. Since the transparentizing resin has low heat resistance, the unnecessary heat can have a negative effect on the transparentizing resin.

[0102] The packaging bag according to the fourth aspect of the present disclosure can avoid such effects by having the above-mentioned configuration.

[0103] A method for manufacturing a packaging bag according to aspect 5 of the present disclosure includes the steps of preparing a paper base material having a surface and an inner surface that constitutes a bag body; impregnating a first region that is a part of the paper base material with a transparentizing agent to form a transparent portion; forming a heat seal layer by applying a heat sealant to at least a portion of the inner surface of the paper base material; and heat sealing the heat seal layer formed in an area of ​​the paper base material excluding the first region to form a bag.

[0104] According to the above configuration, the method for producing a packaging bag according to the fifth aspect of the present disclosure can provide the packaging bag according to the first aspect.

[0105] The present disclosure is not limited to the above-described embodiments, and various modifications are possible within the scope of the claims. The technical scope of the present disclosure also includes embodiments obtained by appropriately combining the disclosed technical means. Furthermore, new technical features can be formed by combining the disclosed technical means. [Explanation of symbols]

[0106] 1 Sheet 1 2. Second Sheet 8, 58 Transparent section 10, 50 bags 20 Chuck 21 Paper base material 22, 22a, 22b Heat seal layer 23 Clarifying agent layer 24, 24a, 24b, 24c printing layer 50g basis weight 53 Transparent agent application area 54 Non-applied area 56 Heat seal application area 100, 300 packaging bags 500 pillow packaging bags 600 seats

Claims

1. A bag body having a surface and an inner surface, the bag body being made of a paper base material; a transparent portion formed by impregnating a transparent agent in a first region that is a part of the paper base material; a heat seal layer formed by applying a heat seal agent to at least a portion of the inner surface of the paper base material; The heat seal layer formed on the paper base material in an area other than the first area is heat sealed to produce a self-packaging bag.

2. the inner surface is rougher than the front surface; The packaging bag according to claim 1 , wherein the transparent agent is impregnated into the inner surface.

3. The packaging bag according to claim 1 or 2, wherein the transparent agent is impregnated into the surface and the inner surface.

4. The packaging bag according to claim 1 or 2, wherein the transparent portion is spaced apart from a heat-sealing position where the heat-sealing layer is heat-sealed.

5. A step of preparing a paper substrate having a surface and an inner surface that constitutes a bag body; A step of impregnating a first region, which is a part of the paper base material, with a transparentizing agent to form a transparent portion; forming a heat seal layer by applying a heat seal agent to at least a portion of the inner surface of the paper base material; and heat-sealing the heat-seal layer formed in the paper base material in an area other than the first area to form a bag.

Citation Information

Patent Citations

  • Clothes packaging material and cover for packaging clothes

    JP2000085868A

  • Method and apparatus for manufacturing windowed envelope

    JP2005001163A