Measuring apparatus, surface plasmon resonance sensor, wearable sensor, and manufacturing method

By integrating a light emitting element and photodiode array on a semiconductor substrate, the measuring device achieves downsizing and enhanced accuracy through surface plasmon resonance, suitable for wearable sensors.

JP2024135227APending Publication Date: 2024-10-04RICOH CO LTD
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
JP2023045807
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-22
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Existing measuring devices are not downsized effectively, limiting their miniaturization and integration capabilities.

Method used

A measuring device is designed with a semiconductor substrate that integrates a light emitting element, a measuring section, and a light receiving element, utilizing surface plasmon resonance phenomenon, where light is emitted into the substrate, reflected, and detected by a photodiode array, allowing for compact and accurate measurements.

Benefits of technology

The integration of components on a semiconductor substrate enables a downsized measuring device with improved measurement accuracy and sensitivity, suitable for wearable sensors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024135227000001_ABST
    Figure 2024135227000001_ABST
Patent Text Reader

Abstract

To provide a small-sized measuring apparatus.SOLUTION: The present invention is a measuring apparatus including: a semiconductor substrate; a light-emitting element that is formed on the semiconductor substrate and emits light into the semiconductor substrate; a measuring unit to which the light that has passed through the semiconductor substrate is made incident as incident light, and which reflects at least a part of the incident light as reflected light; and a light-receiving element that receives the reflected light that has passed through the semiconductor substrate.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a measuring device, a surface plasmon resonance sensor, a wearable sensor, and a manufacturing method. [Background technology]

[0002] Patent Document 1 discloses a surface plasmon resonance sensor device that uses a surface emitting laser as a light source, which has excellent light directionality and polarization plane controllability and is suitable for arraying, and a sensor array such as a CCD as a photodetector, and fabricates these on the same substrate, and has an optically transparent medium and a metal thin film provided or present on the substrate. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 3647267 Summary of the Invention [Problem to be solved by the invention]

[0004] The object is to provide a miniaturized measuring device. [Means for solving the problem]

[0005] A measuring device according to the present invention is characterized in that it comprises a semiconductor substrate, a light-emitting element formed on the semiconductor substrate and emitting light into the semiconductor substrate, a measuring unit receiving the light that has passed through the semiconductor substrate as incident light and reflecting at least a portion of the incident light as reflected light, and a light-receiving element that receives the reflected light that has passed through the semiconductor substrate. Effect of the Invention

[0006] A miniaturized measuring device can be provided. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a schematic diagram of a first embodiment. [Diagram 2] This is the surface plasmon resonance waveform of a surface emitting laser with a divergence angle of 2.5°. [Diagram 3] 1A is a schematic diagram (plan view) of the first embodiment, and FIG. 1B is a schematic diagram of the back surface of the first embodiment. [Figure 4] 1 is a cross-sectional view of a surface-emitting laser element and a photodiode according to a first embodiment. [Diagram 5] FIG. 2 is a cross-sectional view of a sensitive part according to the first embodiment. [Figure 6] FIG. 11 is a partial cross-sectional view of a surface-emitting laser and a photodiode according to a third embodiment. [Figure 7] FIG. 13 is a schematic view (cross-sectional view) illustrating a manufacturing method according to a third embodiment. [Figure 8] FIG. 11 is a partial cross-sectional view of a surface-emitting laser and a photodiode according to a third embodiment. [Figure 9] 1 is a schematic diagram (plan view) of a fourth embodiment, (a) the front side, and (b) the back side. [Figure 10] FIG. 13 is a schematic diagram (cross-sectional view) of a fourth embodiment. [Figure 11] FIG. 11 is a partial cross-sectional view illustrating a mirror structure according to a fourth embodiment. [Figure 12] 13 is a partial cross-sectional view illustrating a sensitive part according to a fourth embodiment. FIG. [Figure 13] The black line indicates the waveform of the generated surface plasmon resonance, and the round dots indicate the measurement points on the photodiode array. (a) Comparative example (b) This embodiment. [Figure 14] 13 is a schematic diagram (plan view) of the fifth embodiment, (a) front side, (b) back side. [Figure 15] FIG. 13 is a schematic diagram (cross-sectional view) relating to a fifth embodiment. [Figure 16] FIG. 13 is a schematic diagram (cross-sectional view) relating to a sixth embodiment. [Figure 17] FIG. 13 is a schematic diagram (cross-sectional view) according to a seventh embodiment. [Figure 18] FIG. 13 is a schematic diagram (cross-sectional view) according to an eighth embodiment. [Figure 19]FIG. 13 is a schematic diagram (cross-sectional view) of the ninth embodiment. [Figure 20] 13 is a schematic diagram of a tenth embodiment, (a) a finger ring type, (b) a wristwatch type, and (c) a contact lens type. [Figure 21] FIG. 15 is a schematic diagram of an eleventh embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the description of the drawings, the same elements are given the same reference numerals, and duplicated description will be omitted.

[0009] First Embodiment FIG. 1 is a schematic diagram of a measuring device 100 according to a first embodiment. The measuring device 100 according to this embodiment is a measuring device that utilizes the surface plasmon resonance phenomenon, also called a surface plasmon resonance sensor. The main components are a light source 104, a sensitive portion 102, a photodiode array 103, and a semiconductor substrate 101. Light 106 generated from the light source 104 propagates through the semiconductor substrate 101, is reflected by an inclined mirror structure 105, and enters the sensitive portion 102 as incident light 106. At least a part of the incident light 106 is reflected by the sensitive portion 102, and the reflected light 106' is received by the photodiode array 103. First, each of the main components will be described individually.

[0010] <Light source> A back-emitting light-emitting diode structure, a back-emitting surface-emitting laser, or the like is used as the light source 104. These light sources are formed on the semiconductor substrate 101 by metal organic chemical vapor deposition, molecular beam epitaxy, or the like.

[0011] 1, the semiconductor substrate 101 is on the XY plane, with the surface seen from the +Z direction being the front surface, and the surface seen from the -Z direction being the back surface. Hereinafter, the back surface and front surface will follow this rule. In the case of a surface-emitting laser 104 formed on the back surface (-Z surface) of the semiconductor substrate 101, the back-emitting type surface-emitting laser emits light in the +Z direction (towards the semiconductor substrate 101).

[0012] The layer structure of a light-emitting diode is composed of a lower contact layer, a light-emitting region including a carrier activation layer, and an upper contact layer on a substrate. If necessary, a multilayer structure that enhances reflectivity (for example, a Bragg reflector structure; an explanation of Bragg reflectors is given below) may be formed between the light-emitting region and the upper contact layer to facilitate emission to the back side. The layer structure of a surface-emitting laser is composed of a lower Bragg reflector, a resonant region including an active layer, and an upper Bragg reflector grown on a semiconductor substrate 101.

[0013] A Bragg reflector is a structure in which materials with different refractive indices are alternately laminated with an optical film thickness of ¼ wavelength of the emitted wavelength λ.

[0014] The feature is that light resonates between the upper and lower Bragg reflectors in a direction perpendicular to the substrate, and some of the light is emitted in a direction perpendicular to the substrate. This is a back-emitting surface-emitting laser structure in which the upper mirror is designed to have a high reflectance, so that laser light is emitted in the direction of the substrate.

[0015] This multilayered film growth structure is then shaped into a mesa shape using various semiconductor process technologies, followed by the formation of a current confinement region by selective oxidation, the formation of a passivation layer and electrodes, and so on, to complete a surface-emitting laser or light-emitting diode.

[0016] A plurality of light sources may be arranged in an array. The wavelength of the light source is selected so as not to be absorbed by the semiconductor substrate.

[0017] <Photodiode array> The growth structure of the photodiode is the same as that of the light source. When light is irradiated onto a light-emitting diode or a surface-emitting laser, light absorption occurs in the active layer, and carriers are excited. A voltage is applied to the active layer through the electrodes, and the excited carriers are extracted, and the amount of current is converted into the amount of light.

[0018] Since the photodiode array can be formed at the same time as the light source formation, with only a change in patterning, the photodiode array can be formed in one or two dimensions.

[0019] <Surface plasmon resonance> At a flat interface where two regions with different dielectric constants meet, there may be electromagnetic waves traveling along the interface. In the case of a metal-dielectric interface, free electrons in the metal create compressional waves along the interface and these waves are called surface plasmon waves, which propagate. In the dielectric near the metal surface, an electric field is formed from the electron sparse region to the electron dense region due to the compressional waves of the surface plasmon electrons. Since the electric field is formed perpendicular to the interface, p-polarized light with a perpendicular electric field is required to interact with the electric field and excite the surface plasmon.

[0020] Furthermore, because the wave number of surface plasmons is larger than that of normal light, the law of conservation of wave numbers does not hold, and surface plasmons cannot be excited. The evanescent wave that is generated when p-polarized light incident at or above the critical angle is totally reflected has an incident angle at which the wave number matches that of the surface plasmon wave. This angle is generally called the surface plasmon resonance angle, and the surface plasmon wave is strongly excited. This phenomenon is called surface plasmon resonance.

[0021] Near the resonance angle, the energy of the incident light is used to excite the surface plasmon wave via the evanescent wave, so the intensity of the reflected light decreases.

[0022] The resonance angle is greatly affected by minute changes in the refractive index in an area of ​​about 100 nm vertically from the metal surface. For example, if an antibody is immobilized on a metal surface and a fluid containing an antigen is poured onto it, the antibody captures the antigen, causing a slight change in the refractive index of the surface and causing the resonance angle to fluctuate. By utilizing this reaction and sensing the change in the resonance angle, it is possible to detect organic molecules and estimate their concentration. Such a measuring device is called a surface plasmon resonance sensor 100.

[0023] The light source may be either a light-emitting diode or a surface-emitting laser, but the incident light must be p-polarized to excite surface plasmon resonance. A surface-emitting laser can emit p-polarized light. In the case of a light-emitting diode structure, the light is unpolarized, so the waveform of the surface plasmon resonance is measured simultaneously with the reflected light of the s-polarized component, which reduces the accuracy of the surface plasmon resonance sensor 100.

[0024] Surface-emitting lasers have superior monochromaticity compared to light-emitting diodes, making it possible to obtain a sharp waveform due to wavelength dispersion of surface plasmon resonance. Therefore, the measurement accuracy of surface plasmon resonance is higher when using a surface-emitting laser.

[0025] On the other hand, since light-emitting diodes can be manufactured at low cost, it is possible to select whether a surface-emitting laser is a light-emitting diode or not, depending on the need.

[0026] <Tilted mirror structure> Light emitted from the light source is reflected by the inclined mirror structure 105 formed on the rear surface of the substrate, and travels straight through the semiconductor substrate 101 while being reflected.

[0027] The inclined mirror structure 105 is formed by grayscale exposure and etching, or etching that utilizes the difference in etching rate for each crystal orientation. The sensitive part 102 is formed on the mirror surface of the inclined mirror structure 105. The mirror structure 105 may be a curved surface, and in particular, a curved mirror having a curvature that diverges and reflects light is preferable.

[0028] <Sensing section> The sensitive part 102 is formed by using general photolithography and plasma chemical deposition, and an anti-reflection coating and a dielectric layer, and a metal layer is formed by using photolithography and techniques such as vacuum deposition and sputtering. A sensitive film for capturing a measurement target substance such as an antibody is formed on the metal layer. The sensitive film is formed by a fixation process of organic molecules such as a self-assembled monolayer or an antibody, and may be used in combination with a patterning technique such as photolithography. It may be formed on the entire surface of the wafer without using a patterning technique. The sensitive part 102 may be only a metal layer and a sensitive film, and may or may not have an anti-reflection coating or a dielectric layer. The inclined mirror structure 105 and the sensitive film are formed on the back surface of the semiconductor substrate 101 by a semiconductor process method.

[0029] Light from light source 104 has a divergence angle, and propagates through semiconductor substrate 101 (light path) while spreading. The light enters the sensitive section formed on inclined mirror structure 105 and is reflected by the metal layer. The divergence angle of the light becomes the angle of incidence on the metal layer in sensitive section 102. The intensity distribution of the reflected light is expressed as the product of the reflectance with respect to the incident angle of the surface plasmon resonance and the intensity distribution of the light with a divergence angle. As an example, Figure 2 below shows the intensity distribution of the reflected light in the case of a back-emitting surface-emitting laser with a divergence angle of 2.5 degrees. Figure 2 shows the surface plasmon resonance waveform of a surface-emitting laser with a divergence angle of 2.5 degrees.

[0030] The reflected light continues to travel straight inside the semiconductor substrate 101 and is incident on the photodiode array 103. The angular component of the reflected light is converted and detected into the coordinates of the photodiode array 103. When an organic molecule is captured by the sensitive film in the sensitive portion 102, the resonance angle shifts, and this is detected as a change in the signal coordinates in the photodiode array 103.

[0031] In reality, the waveform in Figure 2 cannot be measured continuously because it is measured at the pitch of the photodiode arrangement. Since there are fewer measurement points, especially near the resonance angle, the arrangement pitch of the photodiode array should be narrowed as much as possible, and a two-dimensional array structure may be adopted to increase spatial resolution if necessary. Also, to reduce errors such as photodiode measurement noise, measurements are taken multiple times under the same conditions and averaged. After that, the waveform is estimated to obtain the measurement results of the resonance angle change.

[0032] With this method, each element of the surface plasmon resonance sensor 100 can be formed using the integration of a semiconductor process, making it possible to create a smaller surface plasmon resonance sensor than the conventional method of mounting each element individually, or the process performed after the chip is divided.

[0033] <Detailed explanation of the measuring device> Fig. 3 is a plan view showing the measurement device of this embodiment. Note that Fig. 3 is simplified for the purpose of explaining this embodiment, and for convenience, the scale and the number of constituent elements are different from the actual configuration.

[0034] Fig. 4 is a partial cross-sectional view illustrating the surface-emitting laser 104 and the photodiode 206 according to this embodiment, and shows cross sections along the lines A-A' and B-B' in Fig. 3. Note that Fig. 4 is simplified for the purpose of explaining this embodiment, and detailed descriptions of the layer structure and the like are omitted for convenience.

[0035] Fig. 5 is a partial cross-sectional view illustrating the inclined mirror structure 105 according to this embodiment and the sensitive part 102 formed thereon, showing a cross section along the line D-D' in Fig. 3. Note that Fig. 5 is simplified for the purpose of explaining this embodiment, and detailed descriptions of the layer structure and the like are omitted for convenience.

[0036] The photosensitive part 102 shown in Fig. 3 is formed on a GaAs substrate. One or more light sources 104 are formed on the crystal growth surface side, and photodiodes 206 are formed in an array to form a photodiode array 103. When multiple light sources 104 are formed, they may be formed one-dimensionally or two-dimensionally. The photodiode array may be arrayed two-dimensionally. The positive electrode 204 and the negative electrode 207 are connected to each element individually.

[0037] An inclined mirror structure 105 and a sensitive portion 102 are formed on the back surface (the surface opposite to the crystal growth surface, as viewed from the +Z direction) of the semiconductor substrate 101. This sensitive portion 102 is formed with a chip size of approximately 1 mm or less in the longitudinal direction and approximately 100 μm in the lateral direction. Note that further miniaturization may be achieved by arranging the elements more densely within the minimum processing width of the processing for forming each element.

[0038] The following will first explain the case where the light source 104 is a back-emitting surface-emitting laser. Fig. 4 is a simplified structural cross-sectional view taken along dashed line AA' of the light source 104 and dashed line BB' of the photodiode array 103 in Fig. 3.

[0039] 3 and 4, the surface-emitting laser 104 has a mesa structure. The shape of the mesa structure as viewed from above the surface-emitting laser 104 may be circular, elliptical, square, rectangular, or the like. In the surface-emitting laser 104, laser light is emitted from the back side (opposite the crystal growth surface) of the semiconductor substrate 101 (in the direction of the arrow 320 in FIG. 4), and propagates within the GaAs substrate. A plurality of such surface-emitting lasers may be formed, and each surface-emitting laser is connected to a corresponding electrode.

[0040] In the surface-emitting laser 104, an n-type contact layer 308 is formed on the semiconductor substrate 101. The n-type contact layer is made of, for example, n-GaAs. The n-type contact layer 308 is connected to an n-electrode 309. A lower Bragg reflector 307 (hereinafter referred to as lower DBR 307) is formed on the n-type contact layer. Note that DBR is an abbreviation for Distributed Bragg Reflector.

[0041] The semiconductor substrate 101 may be, for example, a SI-GaAs substrate (semi-insulating type). The lower DBR 307 is formed by alternately laminating semiconductor materials having different refractive indices. Specifically, the lower DBR 307 is, for example, n-Al 0.16 Ga 0.84 As high refractive index layer and n-Al 0.9 Ga 0.1 The lower DBR 307 can be formed by laminating 23.5 pairs of AlGaAs low refractive index layers so that the optical film thickness of each layer is 1 / 4 wavelength. The number of pairs in the lower DBR 307 may be more or less than 23.5 pairs in order to achieve the required desired reflectance, and the composition ratio of the material system may be changed.

[0042] On the lower DBR 307, a resonator region 306 is formed, which is made of a lower spacer layer made of AlGaAs, an active layer made of a GaInAs quantum well layer / AlGaAs barrier layer, and an upper spacer layer made of AlGaAs. The resonator region 306 has an optical film thickness of one wavelength. On the resonator region 306, a first upper Bragg reflector 312 (hereinafter referred to as upper DBR 312) is formed.

[0043] The first upper DBR 312 is formed by alternately laminating semiconductor materials having different refractive indices. 0.16 Ga 0.84 As high refractive index layer and p-Al 0.9 Ga 0.1The upper DBR 312 can be formed by laminating a pair of AlGaAs low refractive index layers so that the optical film thickness of each layer is 1 / 4 wavelength. The number of pairs in the upper DBR 312 may be more or less than one pair in order to achieve the required desired reflectance, and the material system may change the composition ratio of AlGaAs.

[0044] A current confinement layer 304 made of AlAs is formed on the first upper DBR 312. The peripheral portion of the current confinement layer 304 is selectively oxidized to form a selectively oxidized region 305, and the central portion forms a current confinement region 304 that is not oxidized.

[0045] A second upper Bragg reflector 303 (hereinafter referred to as upper DBR 303) is formed on the oxide layer 304 and the selectively oxidized region 305. The second upper DBR 303 may be formed of the same material as the first upper DBR 312, and can be formed by laminating 40 pairs. Note that the number of pairs in the upper DBR 303 may be more or less than 40 pairs in order to achieve the required reflectance, and the composition ratio of AlGaAs in the material system may be changed.

[0046] A contact layer 302 is formed on the second upper DBR 303. The contact layer 302 can be made of, for example, p-GaAs. The p-type contact layer 302 is connected to a p-electrode 301.

[0047] The wavelength of the light source 104 may be any wavelength band that is not absorbed by the semiconductor substrate 101. For example, in the case of a SI-GaAs substrate, the emission wavelength may be in the 940 nm band. A longer wavelength may also be used.

[0048] In the following, a structure in which multiple layers are stacked on the substrate 310 in this manner may be referred to as a "stack" for convenience. The stack can be formed by, for example, metal-organic chemical vapor deposition (MOCVD) method. Alternatively, it may be formed by using a molecular beam epitaxial growth (MBE) method or the like.

[0049] The surface emitting laser 104 is formed with a dielectric film 311 made of silicon nitride to protect the mesa sidewall and to serve as a passivation film. The material of the dielectric film 311 may be silicon oxide or other dielectric materials other than silicon nitride. The dielectric film 311 may be formed by using, for example, plasma enhanced chemical vapor deposition or atomic layer deposition. The n-electrode 309 and p-electrode 301 may be formed by vacuum deposition or plating of an appropriate material.

[0050] It is also possible to form a surface-emitting laser structure of an intra-cavity type by forming a portion above the active layer using a dielectric material and then forming appropriate contact layers, electrodes, etc.

[0051] The above description is for a surface emitting laser, but a light emitting diode structure may also be used. In the case of a light emitting diode structure, the lower DBR 307, the oxide layer 304, the oxidized region 305, the first upper DBR 312, and the second upper DBR 303 are removed from the above structure. Also, in order to increase the efficiency of emission toward the substrate, only the upper DBR may be left.

[0052] In this embodiment, the light source is formed using materials such as AlGaAs and InGaAs on a GaAs substrate, but the semiconductor substrate may be made of materials other than GaAs that are used in general semiconductor devices, such as InP, GaN, Si, Ge, and sapphire, and any material, film thickness, and layer configuration may be used as long as the growth structure can be formed in a crystal growth state.

[0053] Photodiode 206 has the same growth structure as light source 104, and is formed by a single crystal growth. Therefore, substrate 101, passivation films 311 and 411, lower contact layers 308 and 408, lower electrodes 309 and 409, lower DBRs 307 and 407, resonator regions 306 and 406, first upper DBRs 312 and 412, current confinement layers 304 and 405, second upper DBRs 303 and 403, upper contact layers 302 and 402, and upper electrodes 301 and 401 in Fig. 3 are made of the same material and have the same film thickness.

[0054] The device structures of the photodiode 206 and the light source 104 differ only in the patterning in the semiconductor process, and are formed simultaneously in a single semiconductor process. When the light source is a surface-emitting laser, the photodiode 206 has the same growth structure (layer structure) as the surface-emitting laser 104, but the current confinement layer 405 is not selectively oxidized. When the light source is a light-emitting diode structure, the photodiode structure is the same as the light source.

[0055] Fig. 5 shows a simplified cross-sectional view of the sensitive portion 102 formed on the tilted mirror structure 105 in Fig. 3 along the dashed line D-D'. The tilted mirror structure 105 is formed on the front surface (opposite the crystal growth surface) of the GaAs substrate.

[0056] The position where the inclined mirror structure 105 is formed is the position where the light emitted from the light source 104 propagates through the GaAs substrate 101 and enters it. The mirror angle of the inclined mirror structure 105 is set at an angle at which surface plasmon resonance occurs in the sensitive part 102 .

[0057] The inclined mirror structure 105 is formed by forming a three-dimensional photoresist mask on the GaAs substrate surface (the surface opposite the crystal growth surface and seen from the +Z direction) using, for example, grayscale exposure, and forming a mirror structure using a dry etching process such as reactive ion etching or a wet etching process such as immersion in a mixture of sulfuric acid and hydrogen peroxide. Alternatively, a specific off-angle of the substrate may be selected, and a mirror structure with a desired angle may be formed by utilizing the change in etching rate for each crystal orientation.

[0058] An anti-reflective coating 604 is formed on the GaAs substrate 101. The anti-reflective coating 604 may be formed, for example, by plasma enhanced chemical vapor deposition or atomic layer deposition with an appropriate material, composition, and thickness.

[0059] A dielectric layer 603 is formed on the anti-reflection coating 604. The dielectric layer 603 is formed, for example, of silicon nitride with a thickness of about 400 nm. The material of the dielectric layer 603 may be silicon oxide or other dielectric material, and the layer structure may be a single layer or a multilayer structure. The thickness may be thicker or thinner than 400 nm. The dielectric layer 603 may be formed by plasma enhanced chemical vapor deposition or the like.

[0060] A metal layer 602 is formed on the dielectric layer 603. The metal layer 602 is formed of 40 nm of gold on 2 nm of chromium. The material of the metal layer 602 may be aluminum, platinum, titanium, or other metal materials other than chromium and gold. The metal layers of each layer may be formed by vacuum deposition, sputtering, plating, or the like. An evanescent wave that excites a surface plasmon wave is generated at the interface between the dielectric layer 603 and the metal layer 602, and the seepage length in the direction perpendicular to the substrate is about 200 to 300 nm. Therefore, the metal film is formed to a thickness less than that.

[0061] It is also possible to eliminate the anti-reflection coating 604 and the dielectric layer 603 and form the metal layer 602 so that it is in direct contact with the GaAs substrate 101. Other layers may be formed as necessary.

[0062] A sensitive film 601 is formed on the metal layer 602. The sensitive film 601 is formed from various materials and structures depending on the target to be sensed. For example, an example of forming a sensitive film used for sensing cortisol, which is generally called a stress hormone, is shown below. The sensitive film 601 is composed of two layers: a self-assembled monolayer layer and an antibody layer.

[0063] A self-assembled monolayer is formed on the metal layer 602. The self-assembled monolayer is formed by mixing a self-assembled monolayer agent in ethanol adjusted to a pH of about 2 with concentrated hydrochloric acid, immersing the wafer in the solution, and leaving it to stand in a dark room for about 48 hours. The wafer is then repeatedly washed with ethanol and dried with nitrogen.

[0064] The self-assembled monolayer agent used has a thiol group on one side and a carboxyl group on the other, and has a carbon chain of 5 or more. The gold surface of the metal layer 602 and the thiol group of the self-assembled monolayer agent form an Au-S bond, forming a self-assembled monolayer on the surface. The wafer is immersed in a mixed solution of N-hydroxysuccinimide (NHS) and 1-ethyl-3-(3-dimethylaminopropyl)carbodiimide (EDC). This activates the carboxyl groups of the self-assembled monolayer.

[0065] The antibody that captures cortisol is added to a phosphate buffer solution, stirred, and the wafer is immersed in the solution, which causes a portion of the antibody to bind to the activated carboxyl group via amine coupling, immobilizing the antibody on the substrate.

[0066] The wafer is then immersed in an ethanolamine solution. This inactivates the carboxyl groups to which the antibody has not bound. The wafer is then washed with pure water and dried with nitrogen. Using the above method, a sensitive film 601 that can be used for sensing cortisol can be formed. Alternatively, a different type of self-assembled monolayer can be used, or a film such as carboxymethyl dextran can be formed instead of the self-assembled monolayer.

[0067] For measurement targets other than cortisol, the self-assembled monolayer, antibody, etc. used may be selected to be appropriate for the measurement target and formed by an appropriate process. In addition, a method other than the antibody reaction for capturing organic molecules may be used, in which an organic substance is captured on the gold surface to change the refractive index near the gold surface.

[0068] <Features of this embodiment> The measuring device 100 of this embodiment is characterized in that a light emitting element 104, a measuring unit 102, and a light receiving element 103 are arranged on a semiconductor substrate 101 and configured as an integrated unit. The light source and surface emitting laser 104 are an example of a light emitting element. The photodiode array 103 is an example of a light receiving element. The sensitive unit 102 is an example of a measuring unit. The GaAs substrate 101 is an example of a semiconductor substrate. This allows for miniaturization by sharing the same part as the holder for the light emitting element, the light receiving element, and the measuring unit and the path for propagating light.

[0069] The measuring device 100 according to this embodiment is characterized by comprising a semiconductor substrate 101, a light emitting element 104 formed on the semiconductor substrate 101 and emitting light 106 into the semiconductor substrate, a measuring unit 102 receiving the light 106 that has passed through the semiconductor substrate 101 as incident light and reflecting at least a part of the incident light as reflected light 106', and a light receiving element that receives the reflected light 106' that has passed through the semiconductor substrate 101. This allows for miniaturization by using a light emitting element holder that also serves as a path for propagating light.

[0070] The measuring device 100 according to the present embodiment is characterized by comprising a semiconductor substrate 101, a light emitting element 104 that emits light 106 into the semiconductor substrate 101, a measuring unit that receives the light 106 that has passed through the semiconductor substrate 101 as incident light and reflects at least a part of the incident light as reflected light 106', and a light receiving element 103 that is formed on the semiconductor substrate 101 and receives the reflected light 106' that has passed through the semiconductor substrate 101. This allows for miniaturization by using a holder for the light receiving element and a path for propagating light in common.

[0071] The measuring device 100 according to this embodiment is characterized in that the light receiving element 103 is formed on the semiconductor substrate 101. This allows the light receiving element and the light emitting element to be held by a single unit, thereby making it possible to reduce the size of the device.

[0072] The measuring device 100 according to this embodiment is characterized in that the semiconductor substrate 101, the light emitting element 104, the light receiving element 103, and the measuring unit 102 are integrally configured. This allows the light emitting element and the light receiving element to be formed close to each other, and allows the main elements of the measuring device to be fabricated at high density. Since the light emitting element 104, the light receiving element 103, and the measuring unit 102 can be aligned with high accuracy, the measurement accuracy is improved.

[0073] The measuring device 100 according to this embodiment is characterized in that the light emitting element 104 and the light receiving element 103 are formed as films on the same surface of the semiconductor substrate 101. This improves the relative positional accuracy of the light emitting element and the light receiving element by a semiconductor process such as photolithography performed on the same plane, thereby improving the measurement accuracy.

[0074] The measuring device 100 according to this embodiment is a surface plasmon resonance sensor including a metal layer 602 that generates surface plasmon resonance in the measuring section, which enables extremely sensitive measurement using the surface plasmon resonance phenomenon.

[0075] The measuring device 100 according to this embodiment is characterized in that the light emitting element 104 is a surface emitting laser, which enables light to be directly incident on the semiconductor substrate 101, thereby providing a compact measuring device.

[0076] The manufacturing method of the measuring device 100 according to this embodiment is characterized by comprising the steps of forming a light emitting element 104 on a semiconductor substrate 101 so that emitted light 106 is emitted into the semiconductor substrate 101, and arranging a measuring unit 102 on the semiconductor substrate 101 so that the light 106 that has passed through the semiconductor substrate 101 is incident thereon.

[0077] The manufacturing method of the measuring device 100 in this embodiment is characterized by comprising the steps of: arranging a measuring unit 102 on a semiconductor substrate 101 so that light 106 that has passed through the semiconductor substrate 101 is incident thereon; and forming a light receiving element 103 on the semiconductor substrate so that reflected light 106' that is formed by reflecting the light 106 that has entered the measuring unit 102 and is reflected by the measuring unit 102 is incident thereon.

[0078] <Effects of this embodiment> In this method, the light source 104 constituting the surface plasmon resonance sensor can be formed by a semiconductor process on the semiconductor substrate 101 that serves as the light propagation path. With conventional miniaturization techniques, it is necessary to separately mount the light source and the medium that serves as the light propagation path, and a processing process is required for each chip. This means that there is a limit to miniaturization within the mountable and processable sizes. On the other hand, in this method, the light source 104 is formed by a semiconductor process on the semiconductor substrate 101 that serves as the light propagation path, making it possible to realize a measurement device that is smaller than conventional devices.

[0079] In addition, in this method, the photodiode array 103 constituting the surface plasmon resonance sensor can be formed by a semiconductor process on the semiconductor substrate 101 that serves as the light propagation path. This makes it possible to realize a measurement device that is smaller than conventional devices.

[0080] In addition, in this method, the light source 104 and the photodiode array 103 that constitute the surface plasmon resonance sensor can be formed by a semiconductor process on the semiconductor substrate 101, which is the light propagation path. This makes it possible to realize a measurement device that is smaller than conventional devices. Furthermore, by forming the inclined mirror structure 105 and the sensitive part 102 by a semiconductor process, individual mounting and processing for each chip, as in conventional miniaturization techniques, are no longer necessary, making it possible to realize a measurement device that is smaller and more accurate than conventional devices.

[0081] <Second embodiment> A schematic diagram of this embodiment is shown in FIG. 6. It is a partial cross-sectional view illustrating the surface-emitting laser 104 and the photodiode 220 according to this embodiment. The second embodiment employs a method of improving the performance of the surface plasmon resonance sensor by making the photodiode 220 have a layer structure different from that of the light source 104. In this embodiment, a processing process of etching only the photodiode portion may be added, and after the first crystal growth, the light source formation portion may be protected with photoresist or the like, and the photodiode portion may be removed by etching, and then a desired photodiode structure may be formed by the second crystal growth.

[0082] This makes it possible to reduce reflection at the DBR and reflection due to differences in refractive index between materials, improve the amount of light incident on the photodiode, and improve the SNR by reducing stray light, thereby improving the performance of the surface plasmon resonance sensor. A specific description of this embodiment will be given below, but this description does not limit the scope of the present invention.

[0083] The following describes some changes made to the manufacturing process of the light source and layer structure of the photodiode from the first embodiment. The other structures and manufacturing processes are the same as those of the first embodiment.

[0084] Fig. 6 is a partial cross-sectional view illustrating the surface-emitting laser 104 and the photodiode 220 according to the second embodiment, showing cross sections along the lines A-A' and B-B' in Fig. 3. Note that Fig. 6 is simplified for the purpose of explaining this embodiment, and detailed descriptions of the layer structure and the like are omitted for convenience.

[0085] The layer structure in Figure 6 is partially common to the light source, and the semiconductor substrate 101, passivation films 311 and 411, lower contact layers 308 and 408, lower electrodes 309 and 409, lower DBRs 307 and 407, resonator regions 306 and 406, first upper DBRs 312 and 412, and upper electrodes 301 and 401 are made of the same materials and have the same film thickness.

[0086] The first upper DBRs 312 and 412 are formed of a material different from that of the layers above them. For example, the layers above the first upper DBR are formed of AlAs, AlGaAs, or GaAs, and the first upper DBRs 312 and 412 are formed of GaInP, AlGaInP, or the like. The AlAs, AlGaAs, and GaAs layers can be etched with a mixture of sulfuric acid and hydrogen peroxide, while the GaInP and AlGaInP layers have the property of not being etched with a mixture of sulfuric acid and hydrogen peroxide. A layer having such etching selectivity may be referred to as an etch stop layer below.

[0087] Therefore, after the crystal growth, the light source part is protected with a photomask or the like, and then etching is selectively performed up to the interface between the first upper DBRs 312 and 412 and the selective oxidation layer 305. Thereafter, the photodiode 220 is formed by performing a processing process similar to that of the first embodiment.

[0088] The material of the first upper DBR and the layer structure above it may be different materials as long as the etching selectivity can be ensured. The mixed liquid used for etching may be, for example, a mixed liquid of phosphoric acid and hydrogen peroxide, or another mixed liquid as long as the etching selectivity can be ensured. The layer having etching selectivity may be formed in a place other than the first upper DBR, for example, in the middle of the second upper DBR, or in another layer.

[0089] Similarly, even when the light source has a light emitting diode structure, a layer having etching selectivity may be provided at any desired location.

[0090] The light emitting element 104 in the measuring device 100 according to this embodiment includes a first upper contact layer 302, a first carrier excitation layer 306, and a first lower contact layer 308 closer to the semiconductor substrate 101 than the first upper contact layer 302, and the light receiving element 103 includes a second upper contact layer 402, a second carrier excitation layer 406, and a second lower contact layer 408 closer to the semiconductor substrate 101 than the second upper contact layer 402, and is characterized in that at least the first lower contact layer 308 and the second lower contact layer 408 are made of the same material. This allows a low-cost manufacturing method to be adopted by simultaneously growing crystals, and a low-cost, small-sized measuring device can be provided.

[0091] The method for manufacturing the measuring device of this embodiment is characterized by comprising a step of simultaneously growing crystals of the light emitting element 104 and the light receiving element 103 on the semiconductor substrate 101, and a step of removing a part of the light receiving element 103 by selective etching.

[0092] <Effects of this embodiment> In this embodiment, the amount of light incident on the photodiode is improved by removing a portion of the photodiode layer in a processing process. For example, by removing the upper DBR 303, the reflectance can be reduced and the amount of light incident on the photodiode can be improved. In addition, the reduction in unnecessary reflected light reduces stray light components, improving the signal-to-noise ratio of detection. This improves the measurement accuracy of the surface plasmon resonance sensor.

[0093] <Third embodiment> In this embodiment, a photodiode 206 is subjected to a processing process and a second crystal growth, so that the layer structure is partially different from that of the light source 104. The other structures and processing processes not described below are the same as those of the first embodiment.

[0094] 7 shows a simplified cross-sectional view of a region where a light source and a photodiode are formed according to the third embodiment, and a processing flow. Note that FIG. 7 is simplified for the purpose of explaining the present embodiment, and for convenience, detailed descriptions of layer configurations and the like are omitted.

[0095] Fig. 8 is a partial cross-sectional view illustrating the surface-emitting laser 104 and the photodiode 206 according to the third embodiment, and shows cross sections along the lines A-A' and B-B' in Fig. 3. Note that Fig. 8 is simplified for the purpose of explaining this embodiment, and detailed descriptions of the layer structure and the like are omitted for convenience.

[0096] 7(a) is a simplified diagram of the layer structure after the first crystal growth is performed on a GaAs substrate 101. An etch stop layer 801 is formed on the GaAs substrate 101. The etch stop layer 801 is formed of, for example, GaInP or AlGaInP. A layer of another material may be used as long as it has etching selectivity.

[0097] A light source layer 802 that forms the structure of the light source is formed on the etch stop layer 801. The light source layer 802 is formed of, for example, an AlGaAs, AlAs, GaAs, InGaAs, AlInGaAs, GaAsP layer, etc. In the light source layer 802 of a surface emitting laser structure, necessary layers such as a DBR layer, a resonance region, and a contact layer are formed, and in the light emitting diode structure, necessary layers such as a contact layer and a light emitting layer are formed.

[0098] An etch stop layer 803 is formed on the light source layer 802. The etch stop layer 803 is formed of, for example, GaInP or AlGaInP, etc. A layer of another material may be used as long as it has etching selectivity.

[0099] 7(b) is a simplified diagram of the layer structure after photolithography and selective etching. A photoresist 804 is formed in the light source formation region by, for example, photolithography, and selective etching is performed on the etch stop layer 803, the light source layer 802, and the etch stop layer 801. The etch stop layers 803 and 801 are selectively etched with, for example, diluted hydrochloric acid, and the light source layer 802 is selectively etched with, for example, a mixture of sulfuric acid and hydrogen peroxide. Other chemicals may be used for etching as long as they are capable of selective etching.

[0100] FIG. 7(c) is a simplified diagram of the layer structure after the second crystal growth is performed after the photoresist is stripped off. The photoresist 804 is stripped off, for example, using a stripping solution. In addition to the stripping solution, an organic solvent such as acetone may be used. After that, the wafer is again introduced into the crystal growth apparatus, and a photodiode layer 806 and an etch stop layer 805 are formed by the second crystal growth. The photodiode layer 806 includes a layer that absorbs light and excites carriers, and is formed of, for example, an AlGaAs, GaAs, InGaAs, or GaInAsP layer. Other materials may be used as long as they can function as a photodiode. The etch stop layer 805 is formed of the same material as the etch stop layers 801 and 803.

[0101] 7(d) is a simplified diagram of the layer structure after photolithography and selective etching. For example, photoresist 809 is formed in the photodiode formation region by photolithography, and selective etching is performed on the etch stop layer 805 and the photodiode layer 806. The selective etching of each layer is performed in the same manner as the selective etching of the light source layer 802 and the etch stop layers 801 and 803.

[0102] 7(e) is a simplified diagram of the layer structure after selective etching is performed after removing the photoresist. The photoresist 809 is removed in the same manner as the photoresist 804. The etch stop layers 803 and 806 are selectively etched in the same manner as the etch stop layers 801 and 803.

[0103] After carrying out the above processing, the light source 104 and the photodiode 206 are formed in the light source forming region 807 and the photodiode forming region 808 by the same processing process as in the first embodiment. Furthermore, the light source 104 and the photodiode 206 may be formed by separate processing processes as necessary.

[0104] Furthermore, a GaInP or AlGaInP layer may be used as part of the light source layer 802, and in that case, a processing step such as selective etching may be appropriately added as required.

[0105] 8 shows the light source 104 and the photodiode 230 of this embodiment. The structure of the light source 104 is a surface emitting laser, as in the first embodiment. The photodiode 230 will be described below.

[0106] An n-type contact layer 408 is formed on the GaAs substrate 101. The n-type contact layer 408 is made of, for example, n-GaAs.

[0107] A carrier excitation layer 450 is formed on the n-type contact layer 408. The carrier excitation layer 450 is formed of, for example, InGaAs. Other material systems may be used as long as light absorption occurs at the wavelength to be used and carrier excitation can be achieved. A p-type contact layer 412 is formed on the carrier excitation layer 450. The p-type contact layer is formed of, for example, p-GaAs.

[0108] The method for manufacturing the measuring device of this embodiment is characterized by including a step of forming a light emitting element 104 on a semiconductor substrate 101 and a step of forming a light receiving element 103 on the semiconductor substrate 101.

[0109] The light emitting element 104 and the light receiving element 103 in the measuring device 100 according to this embodiment are characterized in that the carrier excitation layers (306, 450) are made of different thicknesses or different materials. This allows the lower contact layers to be grown simultaneously, and a low-cost manufacturing method can be selected, while the light receiving elements, which are grown individually as crystals, are made of the optimum thickness and material for light reception, thereby improving the light receiving sensitivity. Highly sensitive light receiving elements enable highly accurate measurements.

[0110] The method for manufacturing the measuring device of this embodiment is characterized by comprising a step of simultaneously growing crystals of the light emitting element 104 and the light receiving element 103 on the semiconductor substrate 101, and a step of removing a part of the light receiving element 103 by selective etching.

[0111] <Effects of this embodiment> In this method, the material and film thickness of the carrier excitation layer 450 of the photodiode 206 can be formed in a layer structure different from that of the light source 104. Therefore, for example, it is possible to increase the film thickness of the carrier excitation layer to increase the carrier generation efficiency, reduce the refractive index difference up to the carrier excitation layer, reduce unintended reflection when light is incident on the photodiode, increase the amount of light, and reduce stray light. This makes it possible to achieve high accuracy of the surface plasmon resonance sensor.

[0112] <Fourth embodiment> This embodiment is illustrated in Figures 9 and 10. The propagation distance in the GaAs substrate is increased to improve measurement accuracy. The propagation distance in the optical path may be increased after surface plasmon resonance is generated in the sensitive part. Since the light from the light source has a divergence angle, the area of ​​the reflected waveform projected on the photodiode array increases as the propagation distance increases. The number of photodiodes contributing to the measurement increases, improving the estimation accuracy and the performance of the surface plasmon sensor.

[0113] Furthermore, by increasing the propagation distance, the change in the coordinates of the light incident on the photodiode array caused by the change in the resonance angle when the organic molecule is captured by the sensitive portion increases, improving the accuracy of the surface plasmon resonance sensor.

[0114] If necessary, the mirror structure and the sensitive part may be separated, or multiple mirror structures may be formed to reflect the light multiple times within the substrate and increase the propagation distance. In the present invention, in which the semiconductor substrate is used as the light path, it is more difficult to increase the propagation distance than in the conventional method of making the light incident on a large-volume light-transmitting medium. Depending on the detection efficiency and spatial resolution of the photodiode array, the desired performance as a surface plasmon resonance sensor may not be achieved. In that case, it is possible to improve the performance of the sensor by reflecting the light multiple times within the substrate and increasing the propagation distance.

[0115] The present embodiment will be described in detail below, but the description is not intended to limit the scope of the present invention.

[0116] This embodiment is an example in which the first tilted mirror structure 105 and the photosensitive portion 102 are formed separately, and the second mirror structure 709 is formed between the light source and the photodiode array, as shown in Fig. 10. Other structures and processing steps not described below are the same as those of any of the first to third embodiments.

[0117] Fig. 9 is a plan view illustrating a measuring device 100 (surface plasmon resonance sensor) according to a fourth embodiment. Note that Fig. 9 is simplified for the purpose of explaining the present embodiment, and differs from the actual configuration in terms of scale, number of constituent elements, etc., for convenience.

[0118] Fig. 10 is a schematic diagram of the configuration of a surface plasmon resonance sensor proposed by the present invention when a back-emission type surface-emitting laser according to the fourth embodiment is used. Note that Fig. 10 is simplified for the purpose of explaining this embodiment, and for convenience, the scale and the number of constituent elements are different from the actual configuration.

[0119] Fig. 11 is a partial cross-sectional view illustrating an inclined mirror structure 105 according to the fourth embodiment, showing a cross section along line E-E' in Fig. 9. Note that Fig. 11 is simplified for explaining the present embodiment, and detailed descriptions of the layer configuration and the like are omitted for convenience.

[0120] Fig. 12 is a partial cross-sectional view illustrating the sensitive part 102 according to the fourth embodiment, showing a cross section along the line F-F' in Fig. 9. Fig. 12 is simplified for explaining the present embodiment, and detailed descriptions of the layer structure and the like are omitted for convenience. Fig. 13 is a simplified diagram of a signal waveform projected on the photodiode according to the third embodiment, and is simplified for convenience.

[0121] 9 shows the structure of the fourth embodiment. In this embodiment, a light source 104, an inclined mirror structure 105, a second mirror structure 709, a sensitive portion 102, and a photodiode 206 are arranged in an array on a semiconductor substrate. The light source and the photodiode are connected to individual electrodes, a p-electrode 204 and an n-electrode 207, respectively. A plurality of light sources may be arranged in an array. The photodiode array may be arranged two-dimensionally.

[0122] 10 is reflected by the inclined mirror structure 105 and travels straight through the substrate. It is then reflected by the second mirror structure 709 and enters the sensitive portion 102. Surface plasmon resonance occurs in the sensitive portion 102 and is detected by the photodiode array.

[0123] 11 is formed at a position where light emitted from light source 104 is incident, and the mirror angle is set at an angle at which surface plasmon resonance occurs in the sensitive area. A three-dimensional photoresist mask is formed on the back side (opposite the crystal growth surface) of GaAs substrate 101 by, for example, grayscale exposure, and a mirror structure is formed by a dry etching process such as reactive ion etching or a wet etching process such as immersion in a mixture of sulfuric acid and hydrogen peroxide.

[0124] Alternatively, a mirror structure with a desired angle may be formed by selecting a specific off-angle for the substrate and utilizing the change in etching rate for each crystal orientation. A reflective metal layer 501 for increasing reflectance, for example, is formed on the mirror structure. The reflective metal layer 501 may be made of a material used when forming the sensitive portion, in which case it can be formed simultaneously with the formation of the sensitive portion.

[0125] The reflective metal layer 501 may be formed of an appropriate dielectric material instead of metal, a single layer film with an appropriate thickness, or a multilayer film structure. Alternatively, nothing may be formed on the inclined mirror structure 105, and a mirror utilizing the refractive index difference with air may be used. Alternatively, the inclined mirror structure 105 may be shaped like a diffraction grating.

[0126] A parallel plate semiconductor substrate 101 has an inclined mirror structure (reflecting surface) 105 at an arbitrary angle. By inclining this reflecting surface, it is possible to bend the light emitted perpendicularly (Z direction) to the semiconductor substrate 101. This makes it possible to efficiently guide the light to the second mirror and the sensitive part 102 without wasting the light. Ultimately, the light can be incident on the light receiving part with a large light intensity. This improves the sensitivity of the sensitive part 102, making it possible to provide a highly accurate measuring device.

[0127] 12 shows a simplified cross-sectional view of the sensitive portion 102. In the sensitive portion 102, an anti-reflection coating 604 is formed on a GaAs substrate 101. The anti-reflection coating 604 is formed by a plasma enhanced chemical vapor deposition method, an atomic layer deposition method, or the like, with an appropriate material, composition, and thickness.

[0128] A dielectric layer 603 is formed on the anti-reflection coating 604. The dielectric layer 603 is formed, for example, of silicon nitride with a thickness of about 400 nm. The material of the dielectric layer 603 may be silicon oxide or other dielectric material, and the layer structure may be a single layer or a multilayer structure. The thickness may be thicker or thinner than 400 nm. The dielectric layer 603 may be formed by plasma enhanced chemical vapor deposition or the like.

[0129] A metal layer 602 is formed on the dielectric layer 603. The metal layer 602 is formed of 40 nm of gold on 2 nm of chromium. The material of the metal layer 602 may be aluminum, platinum, titanium, or other metal materials other than chromium and gold. The metal layers of each layer may be formed by vacuum deposition, sputtering, plating, or the like. An evanescent wave that excites a surface plasmon wave is generated at the interface between the dielectric layer 603 and the metal layer 602, and the seepage length in the direction perpendicular to the substrate is about 200 to 300 nm. Therefore, the metal film is formed to a thickness less than that.

[0130] The metal layer 602 may be formed so as to be in direct contact with the GaAs substrate 101 without the anti-reflection coating 604 and the dielectric layer 603 .

[0131] The second mirror structure 709 has a metal layer formed thereon. The metal layer may be made of the same material as that used when forming the electrodes of the light source and photodiode, and can be formed at the same time as forming the electrodes. Also, instead of metal, an appropriate dielectric material, a single layer film with an appropriate thickness, or a multilayer film structure may be formed. Alternatively, nothing may be formed, and a mirror may be formed that utilizes the refractive index difference with air. Alternatively, a structure in which the lower DBR remains during the processing of the surface-emitting laser may be used as a mirror.

[0132] The light source and the photodiode may have the same structure as described in the first embodiment, or may have different layer configurations as described in the second or third embodiment.

[0133] <Effects of this embodiment>

[0134] The measuring apparatus 100 of this embodiment is characterized in that the light 106, 106' emitted from the light emitting element 104 is reflected on the surface of the semiconductor substrate 101 at least two times.

[0135] Depending on the arrangement pitch of the photodiode array, the light may not spread sufficiently on the photodiode array. This may result in the measurement coordinate interval being small compared to the signal waveform, making it impossible to estimate the waveform sufficiently, resulting in reduced measurement accuracy. Figure 13(a) shows the case where, after reflection at the sensitive area, the light enters the photodiode array without ever being reflected within the GaAs substrate (when the propagation distance is short). Figure 13(b) shows the case where the light is reflected by the inclined mirror structure and the second mirror structure, causing the area projected onto the photodiode to expand (when the propagation distance is long). A comparison of these two figures is provided below.

[0136] The black line in FIG. 13 indicates the waveform of the generated surface plasmon resonance, and the round dots indicate the measurement points on the photodiode array.

[0137] When the propagation distance is short, depending on the arrangement pitch of the photodiode array, there are few measurement points for the entire waveform, and when the propagation distance is long, there are more measurement points for the entire waveform. Fitting and other procedures are performed from these measurement points to estimate the waveform and calculate the change in resonance angle. The longer the propagation distance, the greater the number of measurement points that are effective for estimating the waveform for the entire waveform, improving the estimation accuracy. As a result, by increasing the propagation distance, the performance of the surface plasmon resonance sensor is improved.

[0138] <Fifth embodiment> 14 and 15 are schematic diagrams of a measuring device 100 according to this embodiment. In this embodiment, an inclined mirror structure 105 and a sensitive portion 102 are formed separately, the sensitive portion 102 is formed between a light source and a photodiode array, and a second mirror structure 709 is formed on the rear surface side of a semiconductor substrate 101. Other structures and processing processes not described in this embodiment are the same as those of any of the first to fourth embodiments.

[0139] 14 and 15 are simplified for the purpose of explaining this embodiment, and for the sake of convenience, the scale and the number of constituent elements are different from the actual configuration.

[0140] In this embodiment, a light source 104, an inclined mirror structure 105, a sensitive portion 102, a second mirror structure 709, and a photodiode 206 are formed in an array on a semiconductor substrate 101. The light source and the photodiode are connected to individual electrodes, a p-electrode 204 and an n-electrode 207, respectively. A plurality of light sources may be arranged in an array. The photodiode array may be arranged two-dimensionally.

[0141] Sixth embodiment Fig. 16 is a schematic diagram of the configuration of a measurement device 100 according to the sixth embodiment. Note that Fig. 16 is simplified for the purpose of explaining this embodiment, and for convenience, the scale and the number of constituent elements are different from the actual configuration.

[0142] In this embodiment, the reflected light caused by surface plasmon resonance in the photosensitive part 102 travels straight through the substrate, is reflected by the second mirror structure 709 provided on the rear surface of the substrate, and is reflected multiple times by the third mirror structure 907 before entering the photodiode array. In order to increase the propagation distance, the light is reflected multiple times within the substrate. The third mirror structure may be the same as or different from the second mirror structure.

[0143] In this embodiment, the sensitive part 102 may be formed on the rear side of the substrate as in the fourth embodiment, or may be formed on the mirror structure as in the first embodiment, and may be realized by forming a second mirror structure and a third mirror structure at positions where the reflected light can be reflected multiple times within the substrate.

[0144] The measuring apparatus 100 of this embodiment is characterized in that the light 106, 106' emitted from the light emitting element 104 is reflected on the surface of the semiconductor substrate 101 at least two times.

[0145] <Effects of the Fifth and Sixth Embodiments> In this embodiment, the reflected light caused by surface plasmon resonance in the sensitive part 102 propagates a longer distance in the substrate than in the first to fourth embodiments. The change in the resonance angle caused by the organic molecules captured in the sensitive part increases the amount of change in the coordinates incident on the photodiode array as the propagation distance increases, and is detected. This improves the performance of the surface plasmon resonance sensor. In this method, although the limitations of the processing process, mounting form, cost, etc. are greater than those of the first to fourth embodiments, it is sufficient to set the optimal number of reflections within an acceptable range.

[0146] Seventh embodiment 17 is a schematic diagram of the configuration of the measuring device 100 according to this embodiment. A method of improving the measurement accuracy by extracting light from the semiconductor substrate 101 to the transparent substrate 603 and then returning it to the semiconductor substrate 101 will be described. As shown in the fourth embodiment, after surface plasmon resonance is generated, the propagation distance is increased, so that the change in the resonance angle can be expanded as a change in coordinates on the photodiode array. This improves the measurement accuracy.

[0147] In this embodiment, light is incident on a transparent substrate having a larger volume than the semiconductor substrate. Surface plasmon resonance is generated in a sensitive portion formed on the transparent substrate, and the light is returned to the semiconductor substrate 101. A specific description of this embodiment will be given below, but this description does not limit the scope of the present invention.

[0148] 17 is simplified for the purpose of explaining this embodiment, and differs from the actual configuration in terms of scale, number of constituent elements, etc. Other structures and processing processes not described in this embodiment are the same as any of the first to sixth embodiments.

[0149] <Eighth embodiment>

[0150] Fig. 18 is a schematic diagram of the configuration of a measuring device 100 according to this embodiment. Note that Fig. 18 is simplified for the purpose of explaining this embodiment, and differs from the actual configuration in terms of scale and the number of constituent elements for convenience. Other structures and processing processes not described in this embodiment are the same as those of any of the first to seventh embodiments.

[0151] A light source 104 and a photodiode array 103 are formed by crystal growth and semiconductor processes on a GaAs substrate 101. An anti-reflection coating 604 is formed on the back surface (opposite the crystal growth surface) of the GaAs substrate.

[0152] A glass substrate 603, which is a transparent member, is in contact with the anti-reflection coating 604. The glass substrate 603 is fixed, for example, by lamination or adhesion. The glass substrate may be made of resin or other materials as long as they are light-transmitting. The glass substrate 603 may be formed as a part of the microchannel.

[0153] An inclined mirror structure 105 is formed on the glass substrate 603. The inclined mirror structure 105 is formed by polishing, grayscale exposure, etching, or the like. The angle of the inclined mirror structure 105 is set so that surface plasmon resonance occurs in the sensitive portion. A metal or dielectric multilayer film structure may be formed on the surface of the inclined mirror structure 105 in order to increase the reflectance. A metal layer 602 is formed on a glass substrate 603. Surface plasmon resonance occurs in the metal layer 602. A sensitive film 601 is formed on the metal layer 602.

[0154] As a modified example, the inclined mirror structure 105 may be formed on the GaAs substrate 101. The inclined mirror structure 105 is formed by the same method as in any one of the first to sixth embodiments. The semiconductor substrate (in a wafer state) 101 on which the light source 104, the photodiode array 103, the inclined mirror structure 105, and the anti-reflection coating 604 are formed may be bonded to a glass substrate on which the metal layer 602 and the sensitive film 601 are formed, to complete the wafer state. In this case, the glass substrate 603 can be bonded without the need for highly accurate alignment. A microchannel may be formed in the glass substrate 603.

[0155] <Effects of the Seventh and Eighth Embodiments> In the measuring apparatus 100 of this embodiment, a transparent substrate 603 is bonded to a semiconductor substrate 101. It is characterized in that the metal layer is formed on the surface of a transparent substrate 603 .

[0156] In this embodiment, the performance of the surface plasmon resonance sensor is improved by increasing the propagation distance as in the fourth embodiment. Since the light-transmitting medium can be used as a flow path as it is, there is a possibility that the cost can be reduced as a result compared to the first to third embodiments.

[0157] In addition, in the seventh and eighth embodiments, since the photodiode array and the reflective surface formed on the semiconductor substrate are close to each other, the reflected light in unintended directions increases due to the flatness of the mirror surface depending on the processing method, which may cause stray light and reduce the performance of the surface plasmon resonance. Within the constraints of cost and required performance, the optimal method can be selected from the method of this embodiment or the methods of the first to sixth embodiments.

[0158] <Ninth embodiment> Fig. 19 is a schematic diagram of a systemized measurement device 100 according to the ninth embodiment. The measurement device (surface plasmon resonance sensor) 100 according to any one of the first to eighth embodiments is connected to a microchannel equipped with a reverse iontophoresis mechanism to form a system. Note that Fig. 19 is simplified for the purpose of explaining this embodiment, and for convenience, the scale, arrangement of components, number, etc. differ from the actual configuration.

[0159] A measuring device (surface plasmon resonance sensor) 100 according to any one of the first to eighth embodiments is fixed to a microchannel for use. The microchannel is formed on glass, resin, a Si substrate, or the like by photolithography and etching. The width of the channel is about several tens to several hundreds of μm. A liquid sample is sent to a sensitive portion of the surface plasmon resonance sensor using the microchannel. A micropump, a microvalve, or the like is formed in the microchannel using MEMS technology or the like, making it possible to control the movement of the required liquid. When using capillary action in the microchannel, a micropump, a microvalve, or the like is not required.

[0160] When sweat is the measurement target, for example, reverse iontophoresis technology is applied for active sampling. Reverse iontophoresis technology is a technology in which electrodes are placed in contact with the skin and current is passed through the skin to cause sweat components to seep out onto the skin. Electrodes are provided in a part of the microchannel, and active sampling of sweat is performed by passing a current through the electrodes. Note that if active sampling is not required, there is no need to apply reverse iontophoresis technology. In that case, any sampling method may be used, and any method may be used as long as the sample can be brought into contact with the sensitive part.

[0161] The flow path is connected to an area where an appropriate chemical solution is stored to assist in the transfer of the sample and to protect the sensitive part. The chemical solution is, for example, a phosphate buffer solution, but other suitable chemical solutions such as pure water may also be selected. The chemical solution is periodically replenished. Alternatively, it does not have to be connected to an area where the chemical solution is stored all the time, and may be connected from the outside as needed.

[0162] The flow path is connected to a region that stores a regenerant that removes organic molecules captured on the surface of the sensing part and regenerates the function of the sensor. The regenerant is periodically replenished. Alternatively, it does not have to be connected to a region that stores regenerant all the time, and it can be connected from the outside and used as needed.

[0163] The flow path is connected to an area for storing the measured sample, and the measured sample is temporarily stored and periodically discarded. Alternatively, it does not have to be connected to an area for constantly storing the sample, and may be discharged to the outside each time. The sample may be other than sweat, such as saliva, plasma, urine, or tears.

[0164] The configuration of this embodiment will be described with reference to Fig. 19. A sensitive part 102 of a measuring device (surface plasmon resonance sensor) 100 is connected to a microchannel 1001. Organic molecules passing through the microchannel 1001 are captured by the sensitive part 102 on the way, causing a change in the resonance angle.

[0165] A first electrode 1002 and a second electrode 1002 are provided in the microchannel 1001. For example, when the electrodes are brought into contact with the skin and a current is passed through them, it is possible to make sweat seep out of the skin by reverse iontophoresis technology. The exuded sweat is guided to a sensing part and sensed. The electrodes for reverse iontophoresis may be rectangular or circular pad-shaped, and an electrode of one polarity may be arranged so as to surround the electrode of the other polarity. Alternatively, the electrodes may be arranged in a way that allows efficient sampling.

[0166] When collecting saliva, plasma, etc. separately, the application of reverse iontophoresis technology is not necessary, and only the microchannel is sufficient. The microchannel 1001 is formed with a micropump and a microvalve mechanism, and is configured to enable the necessary fluid control within the microchannel.

[0167] The microchannel 1001 is connected to an area 1008 in which a chemical solution is stored to assist in liquid transfer and protect the sensitive membrane. The organic molecules to be measured that seep into the microchannel 1001 near the electrode 1003 are transferred to the sensitive section using, for example, a phosphate buffer solution. The chemical solution used may be other than phosphate buffer solution, and an appropriate one may be used depending on the material of the sensitive membrane, etc.

[0168] Depending on the sensitive film, impurities may adhere to the sensitive film surface during exposure to the atmosphere or drying, resulting in a decrease in performance or loss of function as a surface plasmon resonance sensor. For this reason, the sensitive film is always immersed in a chemical solution to protect the surface, or the sensitive film is designed so that the chemical solution flows continuously over the sensitive film surface. Alternatively, a drying process may be performed that prevents impurities from adhering. Alternatively, the area 1008 in which the chemical solution is stored may be eliminated, and the chemical solution may be directly supplied from the outside at the required timing.

[0169] The microchannel 1001 is connected to an area 1009 that stores a regenerant for removing organic molecules captured by the sensitive membrane 601. When organic molecules are captured by the sensitive membrane 601, they usually remain captured, adversely affecting the next measurement. For this reason, it is necessary to remove the organic molecules with a regenerant for each measurement. For example, when an antibody that captures cortisol is used as the sensitive membrane, a 10 mM HCL glycine buffer solution with a pH of 2.5 is used. Other appropriate chemical solutions may also be selected. Also, the area 1009 where the regenerant is stored may be eliminated, and the regenerant may be directly supplied from the outside at the required timing.

[0170] The microchannel 1001 is connected to an area 1005 where the measured sample, buffer solution, etc. are temporarily stored as waste liquid. All waste liquid is collected here and discarded at an appropriate time. It is also possible to eliminate the area 1005 where the waste liquid is stored and release it to the outside.

[0171] The surface plasmon resonance sensor 100, the microchannel 1001, the areas 1005, 1008, and 1009 for storing each drug and waste liquid, and the electrodes 1002 and 1003 for reverse iontophoresis are all mounted together in a single PKG or the like, and have a structure that can be incorporated into various systems. Alternatively, each element may be mounted individually as necessary.

[0172] The measuring device 100 of this embodiment is characterized in that at least a part of the transparent substrate 603 serves as a flow path for sending the analyte to the metal layer 602 .

[0173] The measuring device 100 of this embodiment is characterized in that electrodes 1002 and 1003 are formed on the surface of a transparent substrate 603 .

[0174] <Effects of this embodiment> By using a microchannel equipped with electrodes for reverse iontophoresis, the system size can be prevented from increasing and real-time measurement by active sampling can be performed.

[0175] <Tenth embodiment> A schematic diagram of this embodiment is shown in Fig. 20. This embodiment is an example of various wearable devices capable of real-time monitoring of biomolecules to which the measuring device (surface plasmon resonance sensor) 100 according to any one of the first to eighth embodiments or the system 1102 thereof is applied.

[0176] The surface plasmon resonance sensor 100 is smaller than conventional ones, being less than 1 mm in size, and has a chip shape. Even with a flow path etc., it can be fabricated with a system size of about several mm, making it applicable to various wearable devices.

[0177] A wearable device that comes into contact with the skin can measure sweat, enabling real-time, constant monitoring of, for example, cortisol. In addition to cortisol, it can also monitor glucose and various other bioorganic molecules in real time. This can be used for quantitative monitoring of stress by real-time quantification of cortisol, a stress hormone, which has been difficult to achieve until now, non-invasive real-time monitoring of blood glucose levels, and real-time monitoring of other biomolecules important in the vital and social activities of humans and animals. Examples are given below to provide a specific explanation of the tenth embodiment, but this embodiment does not limit the scope of the present invention.

[0178] Fig. 20 is a diagram illustrating a ring type device, a wristwatch type device, and a contact lens type device to which the surface plasmon resonance sensor 100 according to this embodiment is applied. Note that Fig. 20 is simplified for the purpose of explaining this embodiment, and differs from the actual configuration for convenience. Fig. 20(a) is a simplified cross-sectional view of the ring type device, Fig. 20(b) is a simplified cross-sectional view of the wristwatch type device, and Fig. 20(c) is a simplified overhead view of the contact lens type device.

[0179] A surface plasmon resonance sensor system 1102 is mounted on the inside of a ring-shaped device 1101 in Fig. 20(a). A reverse iontophoresis electrode is formed on the part that comes into contact with the skin, and active sweat sampling is performed, enabling constant monitoring of the concentration of biomolecules such as cortisol contained in sweat. Other necessary control ICs, batteries, etc. are also built into the ring-shaped device 1101.

[0180] Similarly, a surface plasmon resonance sensor system 1102 is formed in the area of ​​a wristwatch type device 1103 in FIG. 20(b) that comes into contact with the skin. The surface plasmon resonance sensor system 1102 may be formed in the band portion instead of on the back of the dial. Similarly, a surface plasmon resonance sensor system 1102 is formed in a contact lens type device 1104 in FIG. 20(c). In this case, the sample is tears instead of sweat. The electrodes for reverse iontophoresis may be eliminated. The present invention can also be applied to other items that are in contact with the skin for long periods of time, such as glasses, VR goggles, necklaces, earrings, piercings, and shoes.

[0181] The wearable devices (1101, 1103, 1104) according to the present embodiment are characterized by including a measuring device 100 (1102). This makes it possible to provide a wearable sensor that is compact and comfortable to wear while enabling highly accurate detection.

[0182] <Effects of this embodiment> The health and stress state of an organism are correlated with changes in the concentration of various biomolecules present inside the organism. For example, in the case of cortisol, a so-called stress hormone, these changes vary over a period of several minutes to several tens of minutes. With conventional hormone analysis methods (such as ELISA), frequent measurements at intervals of several minutes are not realistic.

[0183] As shown in this embodiment, by applying a small surface plasmon resonance sensor to equipment that is in contact with the skin for long periods of time, such as a wearable device, and performing active sampling using reverse iontophoresis technology or the like, it becomes possible to continuously monitor the concentration of biomolecules, which was not possible before.

[0184] <Eleventh embodiment> A schematic diagram of this embodiment is shown in Fig. 21. The measuring device 100 of this embodiment is characterized by having a measuring unit 108 that employs the ATR (Attenuated Total Reflection) method. The light emitting element 104 and the light receiving element 103 are formed as films on a semiconductor substrate 110, and the light 106, 106' propagates within the semiconductor substrate, making this a very small measuring device using the ATR method. This is an example of a wearable device that can monitor biomolecules in real time.

[0185] Molecular analysis using infrared light is a molecular structure analysis technique that takes advantage of the property of molecules absorbing light of specific wavelengths due to molecular vibration. Generally, absorption occurs with light in the mid-infrared region, so a light source that emits broadband mid-infrared light is used. Light from the light source is irradiated onto the sample, and the transmitted light is detected after dispersion using a spectroscope or similar device to obtain a transmission spectrum (or absorption spectrum). The obtained spectral shape is used to identify the molecule and analyze its concentration, etc. There is also an analytical technique in which an interference system is constructed, the sample is irradiated with interfered infrared light, and the transmitted interference light is Fourier transformed to obtain an absorption spectrum. This is a molecular structure spectroscopic analysis technique called FT-IR.

[0186] There is a spectroscopic analysis technology that uses near-infrared light instead of mid-infrared light. When near-infrared light is used, it can be used with the same optical system as the infrared spectroscopy technology mentioned above. In particular, when an analysis similar to FT-IR is performed using near-infrared light, it is called FT-NIR.

[0187] The ATR method is a spectroscopic analysis technique that utilizes evanescent waves generated when a sample is placed in close contact with a prism and light is totally reflected at the prism surface. It can be used in conjunction with analysis techniques such as the FT-IR mentioned above. Total reflection occurs when light is incident from the prism to the interface of the sample at an angle equal to or greater than the critical angle. At that time, the incident light penetrates the sample for a few hundred nm (evanescent wave) before being reflected. Absorption occurs in the evanescent wave that penetrates the sample in a manner that depends on the molecular structure of the sample, and molecular analysis is performed by detecting the reflected light. Generally, glass, germanium, ZnSe, etc. are used as materials for the prism, but other materials are also acceptable.

[0188] When using a single-wavelength light source such as a laser rather than a broadband mid-infrared light source, a light source that emits light at a wavelength that provides a characteristic absorption peak in the molecular absorption spectrum is used. The correlation between major molecules and characteristic absorption wavelengths is summarized in Table 1. Note that there are characteristic wavelengths other than those described below, so any wavelength can be used.

[0189] [Table 1]

[0190] It is said that blood glucose levels can be estimated by capturing signal changes at a certain depth in cross-sectional images in OCT (optical coherence tomography), and an example has been shown in which blood glucose levels were estimated from signals pinpoint measured in skin tissue (dermal tissue) 200 to 600 μm below the skin surface using an OCT device that uses near-infrared light of 1300 nm.It has also been shown that changes in the measured OCT signal were measured as changes in scattering coefficient associated with changes in glucose concentration in the skin tissue, and that there was a maximum change of 2.8% for a glucose concentration change of 10 mg / dL (Non-Patent Document 1). [Non-Patent Document 1] KVLarin, MMMotamedi, MSEledrisi, ROEsenaliev,“Noninvasive Blood Glucose Monitoring With Optical Coherence Tomography”,Diabetes Care,25,12,2263-2267

[0191] In the first to tenth embodiments, for example, a back-emitting light-emitting diode or a back-emitting surface-emitting laser is exemplified as the light source. The emission wavelength band of these light sources is generally from visible light to near infrared light of 2,000 nm due to the characteristics of the material. Therefore, they can be used in near infrared spectroscopy. On the other hand, the wavelength suitable for molecular analysis in infrared spectroscopy such as FT-IR is generally mid-infrared light of 2,000 nm to 20,000 nm, so it is necessary to form a light source capable of emitting mid-infrared light.

[0192] A quantum cascade surface-emitting laser (QC-VCSEL) is an example of a light source that can emit mid-infrared light and can emit light in the direction of the substrate. In this configuration, a QC-VCSEL structure is grown on a semiconductor substrate using an MOCVD or MBE device, and the structure is formed using an appropriate semiconductor process, allowing it to be used as a light source of mid-infrared light that emits light in the direction of the substrate.

[0193] In the case of infrared spectroscopy using near-infrared light, the light receiving element can use a photodiode array as in the first to tenth embodiments. On the other hand, it is difficult to detect mid-infrared light using, for example, a QC-VCSEL with a normal photodiode structure. Therefore, when forming a light receiving element using selective etching and recrystallization growth technology as in the third embodiment, it is necessary to design the material of the carrier generation layer sensitive to mid-infrared light and the film thickness of each layer. An example of the material of the carrier generation layer sensitive to mid-infrared light is InAsSb.

[0194] In addition, when a superlattice structure of InAs and GaSb is grown with appropriate thickness for each layer, minibands with narrow energy intervals are formed, which absorb mid-infrared radiation and cause carrier transitions between the minibands. This optical absorption can be used to function as a mid-infrared light receiving element. These materials can be formed by crystal growth techniques such as MOCVD and MBE. The carrier generation layer may be formed of materials other than InAsSb, InAs, and GaSb. In addition, mid-infrared detectors such as bolometers, MCTs, pyroelectric sensors, and quantum dot sensors may be used as necessary.

[0195] Conventional optical systems for molecular analysis by infrared spectroscopy using the ATR method require a spectrometer, an interference system, and other optical elements such as mirrors and lenses, which results in the device becoming larger. In contrast, by using the substrate itself as a substitute for the ATR prism without evaporating metal on the sensitive portion of the first to tenth embodiments, it is possible to make the device smaller than conventional infrared spectroscopic analysis devices using the ATR method.

[0196] The light source 104 in FIG. 21 is a surface-emitting laser 10 with a wavelength of 1300 nm formed on an InP substrate by crystal growth techniques such as MOCVD and MBE. In this embodiment, a surface-emitting laser 11 with a wavelength of 1400 nm is also provided adjacent to the laser, and is used as a reference light when the blood glucose level is relatively quantified from the amount of light absorption. By having two wavelengths, it is possible to correct fluctuations in external factors such as the amount of moisture as an environmental change and the contact condition of the measurement part with the skin. This correction enables continuous stable measurement, and the relative change over time in the blood glucose level and the like can be visualized in a graph. The manufacturing method for forming two-wavelength surface-emitting lasers on the same substrate may be the method described in the third embodiment, and is described in detail in Patent Document 2, etc., so it will not be described here. [Patent Document 2] JP 2020-161800 A

[0197] The semiconductor substrate 110 is an InP substrate, and is transparent at wavelengths of 1300 nm and 1400 nm used in this embodiment, so that the light 106 is incident on the measurement unit 108 without attenuation. At this time, the inclined mirror 105 is arranged in the propagation path, and the propagating light 106 is incident on the measurement unit 108 at an incident angle designed for the measurement unit 108, and the ATR method using the total reflection angle is realized. The surface viewed from the -Z direction is a second mirror structure 709 so that the light propagating through the semiconductor substrate 110 causes multiple reflections. By multiple reflections, the light 106 is incident on the measurement unit 108 many times, thereby achieving high sensitivity. The light 106' reflected from the measurement unit 108 is incident on the light receiving element 103 via the inclined mirror 109 and detected. In this embodiment, the light that is reflected last among the multiple reflections at the measurement unit 108 and heads toward the light receiving element 103 is referred to as the reflected light 106'.

[0198] The measuring device 100 of this embodiment uses the 1300 nm band, which is said to be correlated with blood glucose levels, so it is possible to read changes in blood glucose levels over time by continuously measuring. In this embodiment, the device is small, measuring just a few mm, so it can be fixed in the oral cavity via a mucosal patch. Since the skin in the oral cavity is thin, it is said that there is a correlation with the blood glucose level near the dermis measured by the ATR method (Patent Document 3). Alternatively, the thin skin in the oral cavity contains a lot of interstitial fluid, improving detection accuracy. [Patent Document 3] JP 2021-067652 A

[0199] Even a small measuring device such as that of this embodiment can be powered by batteries for several days, making it suitable as a wearable sensor for detecting changes over time.

[0200] As described above, one embodiment of the present invention is as follows.

[0201] <1> The measuring device 100 according to the present embodiment is characterized by comprising a semiconductor substrate 101, a light emitting element formed on the semiconductor substrate and emitting light 106 into the semiconductor substrate, a measuring unit 102 receiving the light 106 that has passed through the semiconductor substrate as incident light and reflecting at least a part of the incident light as reflected light 106', and a light receiving element that receives the reflected light that has passed through the semiconductor substrate 100. This allows for miniaturization by using the same unit as both a holder for the light emitting element and a light propagation path.

[0202] <2> The measuring device 100 according to the present embodiment is characterized by comprising a semiconductor substrate 101, a light emitting element 104 that emits light 106 into the semiconductor substrate 101, a measuring unit that receives the light 106 that has passed through the semiconductor substrate 101 as incident light and reflects at least a part of the incident light as reflected light 106', and a light receiving element 103 that is formed on the semiconductor substrate and receives the reflected light 106' that has passed through the semiconductor substrate. This allows for miniaturization by using the same unit as a holder for the light receiving element and a light propagation path.

[0203] <3> The measuring device 100 according to this embodiment is characterized in that the light receiving element 103 is formed on the semiconductor substrate 101. <1> In this way, the light receiving element and the light emitting element are held by a single unit, thereby making it possible to reduce the size of the measuring device.

[0204] <4> The measuring device 100 according to this embodiment is characterized in that the semiconductor substrate 101, the light emitting element 104, the light receiving element 103, and the measuring unit 102 are integrally configured. <1> ~ <3> This allows the light emitting element and the light receiving element to be formed close to each other, and the main elements of the measuring device can be fabricated at high density. The light emitting element 104, the light receiving element 103, and the measuring unit 102 can be aligned with high accuracy, improving the measurement accuracy.

[0205] <5> The measuring device 100 according to the present embodiment is characterized in that the light emitting element 104 and the light receiving element 103 are formed as films on the same surface of the semiconductor substrate 101. <1> ~ <4> This improves the relative positional accuracy of the light emitting element and the light receiving element by a semiconductor process such as photolithography carried out on the same plane, thereby improving the measurement accuracy.

[0206] <6> The measuring device 100 according to this embodiment is characterized in that the light emitting element 104 is a surface emitting laser. <1> ~ <5> This makes it possible to directly input light to the semiconductor substrate 101, and thus provides a compact measuring device.

[0207] <7> The light-emitting element 104 in the measuring device 100 according to this embodiment includes a first upper contact layer 302, a first carrier excitation layer 306, and a first lower contact layer 308 closer to the semiconductor substrate 101 than the first upper contact layer 302, and the light-receiving element 103 includes a second upper contact layer 402, a second carrier excitation layer 406, and a second lower contact layer 408 closer to the semiconductor substrate 101 than the second upper contact layer 402, and is characterized in that at least the first lower contact layer 308 and the second lower contact layer 408 are made of the same material. <1> ~ <6> This allows for simultaneous crystal growth, making it possible to employ a low-cost manufacturing method and provide a low-cost, small-sized measuring device.

[0208] <8> The light emitting element 104 and the light receiving element 103 in the measuring device 100 according to this embodiment are characterized in that the carrier excitation layers (306, 450) have different thicknesses or are made of different materials. <1> ~ <7> This allows the lower contact layer to be grown simultaneously, and therefore the light receiving sensitivity can be improved by selecting a manufacturing method that realizes low cost while also making the light receiving element, which is grown as a crystal, into an optimal film thickness and material for light reception. This enables highly accurate measurement using the highly sensitive light receiving element.

[0209] <9> The measuring apparatus 100 according to the present embodiment is characterized in that the light is reflected at least two times within the semiconductor substrate 101. <1> ~ <8> This makes it possible to increase the distance that light propagates while maintaining a small size, thereby improving detection accuracy.

[0210] <10> The wearable devices (1101, 1103, 1104) according to this embodiment are: <1> ~ <9> The present invention is characterized in that it is equipped with the measuring device 100 (1102) described in 2. This makes it possible to provide a wearable sensor that is compact and capable of highly accurate detection while maintaining comfort.

[0211] <11> The manufacturing method of the measuring device 100 according to this embodiment is characterized by comprising the steps of forming a light emitting element 104 on a semiconductor substrate 101 so that emitted light 106 is emitted into the semiconductor substrate 101, and arranging a measuring unit 102 on the semiconductor substrate so that the light 106 that has passed through the semiconductor substrate 101 is incident thereon. This makes it possible to provide a miniaturized measuring device.

[0212] <12> The manufacturing method of the measuring device 100 according to this embodiment is characterized by comprising the steps of arranging a measuring unit 102 on a semiconductor substrate 101 so that light 106 passing through the semiconductor substrate 101 is incident thereon, and forming a light receiving element 103 on the semiconductor substrate so that reflected light 106' resulting from reflection of the light 106 incident on the measuring unit 102 by the measuring unit 102 is incident thereon. This makes it possible to provide a miniaturized measuring device.

[0213] <13> The measuring device 100 according to this embodiment includes a metal layer 602 that generates surface plasmon resonance in the measuring section. <1> ~ <12> This surface plasmon resonance sensor has the characteristics described in 2. This makes it possible to perform extremely sensitive measurements using the surface plasmon resonance phenomenon. [Explanation of symbols]

[0214] 100 Surface plasmon resonance sensor (an example of a measuring device) 101 GaAs substrate (an example of a semiconductor substrate) 102 Sensing part (an example of a measuring part) 103 Photodiode array (an example of a light receiving element) 104 Surface-emitting laser (light-emitting element, an example of a light source) 105 Inclined mirror structure 106 Light (an example of incident light) 106' Light (Example of reflected light) 206 Photodiode (an example of a light receiving element) 220 Photodiode (an example of a photodetector with the upper DBR removed) 230 Photodiode (an example of a photodetector with an optimized carrier excitation layer) 307 Lower contact layer (light emitting device) 306 Carrier excitation layer (photodetector) 302 Upper contact layer (photodetector) 407 Lower contact layer (photodetector) 406 Carrier excitation layer (photodetector) 402 Upper contact layer (photodetector) 450 Carrier excitation layer (material and thickness optimized for light receiving performance) 601 Sensitive membrane 602 Metal layer 603 Dielectric film, glass substrate (an example of a transparent substrate) 709 Second mirror structure 907 Third Mirror Structure 1001 Channel 1002 First electrode 1003 Second electrode 1101 Ring-type wearable sensor 1102 Surface plasmon resonance sensor system (an example of a measuring device) 1103 Wristwatch-type wearable sensor 1104 Contact lens type wearable sensor

Claims

1. Semiconductor substrate and a light emitting element formed on the semiconductor substrate and emitting light into the semiconductor substrate; a measurement unit that receives the light that has passed through the semiconductor substrate as incident light and reflects at least a portion of the incident light as reflected light; a light receiving element that receives the reflected light that has passed through the semiconductor substrate; A measuring device comprising:

2. Semiconductor substrate and a light emitting element that emits light into the semiconductor substrate; a measurement unit that receives the light that has passed through the semiconductor substrate as incident light and reflects at least a portion of the incident light as reflected light; a light receiving element formed on the semiconductor substrate, the light receiving element receiving the reflected light having passed through the semiconductor substrate; A measuring device comprising:

3. 2. The measuring apparatus according to claim 1, wherein said light receiving element is formed on said semiconductor substrate.

4. The semiconductor substrate, the light emitting element, the light receiving element, and the measuring unit are integrally configured.

2. The measuring device according to claim 1 .

5. The light emitting element and the light receiving element are formed by film formation on the same surface of the semiconductor substrate.

5. The measuring device according to claim 3 or 4.

6. The light emitting device is a surface emitting laser.

2. The measuring device of claim 1.

7. the light emitting element includes a first upper contact layer, a first carrier excitation layer, and a first lower contact layer closer to the semiconductor substrate than the first upper contact layer; the light receiving element includes a second upper contact layer, a second carrier excitation layer, and a second lower contact layer closer to the semiconductor substrate than the second upper contact layer; At least the first lower contact layer and the second lower contact layer are made of the same material.

6. The measuring device according to claim 5.

8. The light emitting element and the light receiving element are The carrier excitation layer is made of different thicknesses or different materials.

6. The measuring device according to claim 5.

9. The light is reflected at least two times inside the semiconductor substrate.

2. The measuring device according to claim 1 .

10. A wearable device comprising the measuring device according to claim 1.

11. forming a light emitting element on the semiconductor substrate such that emitted light is emitted into the semiconductor substrate; and arranging a measurement unit on the semiconductor substrate so that the light having passed through the semiconductor substrate is incident thereon. A method for manufacturing a measuring device.

12. a step of arranging a measurement unit on the semiconductor substrate so that the light having passed through the semiconductor substrate is incident thereon; forming a light receiving element on the semiconductor substrate so that the light incident on the measurement unit is reflected by the measurement unit and the reflected light is incident on the light receiving element. A method for manufacturing a measuring device.

13. 3. The surface plasmon resonance sensor according to claim 1, further comprising a metal layer for generating surface plasmon resonance in the measurement section.

Citation Information

Patent Citations

  • Miniature real-time on-line offshore oil spill detection system

    CN104713851A

  • Surface plasmon resonance sensor

    JP1998019768A

  • Surface plasmon resonance sensor device using surface emitting laser

    JP1999344437A

  • Surface plasmon resonance sensor

    JP2005156415A

  • Mobile / Wearable devices that capture the lspr sensor

    JP2017538917A